A density safety detection method for concrete-filled steel tubes based on stress level
By considering the stress level in steel pipe concrete components, the problem of inaccurate density testing in traditional detection methods is solved, and the accuracy of detection and reliability of safety evaluation is improved.
Patent Information
- Application Number
- CN202310957550.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2023-08-01
- Publication Date
- 2024-11-26
- Estimated Expiration
- 2043-08-01
AI Technical Summary
Traditional steel pipe concrete density detection fails to take into account the impact of detection time and stress on compactness, resulting in inaccurate test results.
The stress level-based detection method is adopted, including conducting compactness detection when the steel pipe concrete member is not loaded, monitoring its strain and blind hole stress, and then detecting compactness changes under different load ratios to evaluate component safety.
The accuracy of density test and the reliability of the results are improved, and the safety of the components is reasonably evaluated by combining density and loading conditions, ensuring the safety of the structure.
Smart Images

Figure CN117091990B_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the technical field of nondestructive testing of composite structures, and in particular to a method for testing the density safety of steel tube concrete based on stress levels. Background Art
[0002] The traditional steel tube concrete density test process does not take into account the test time and the impact of different stresses on the density of steel tube concrete components. When steel tube concrete is under pressure, it will cause the internal concrete to expand and the density to increase, but the existing technology does not consider the impact of concrete expansion on density. Summary of the invention
[0003] In view of this, the present invention proposes a density safety detection method of steel tube concrete based on stress level, aiming to solve the problem of inaccurate density test results of existing steel tube concrete.
[0004] The present invention proposes a method for detecting the density safety of steel tube concrete based on stress level, which comprises the following steps:
[0005] Step 1, after the steel tube concrete component is cast, when there is no load on the upper part, a density test is performed on it to determine the density of the steel tube concrete component when there is no load on the upper part;
[0006] Step 2, taking another steel tube concrete component, and performing strain monitoring and blind hole stress testing on the interior and surface of the steel tube concrete component after the concrete pouring is completed, so as to determine the load ratio of the steel tube concrete component;
[0007] Step 3, testing the density of concrete inside the steel tube concrete component with different load ratios, so as to obtain the density change of the steel tube concrete component under different load ratios, so as to evaluate the safety of the steel tube concrete component.
[0008] Furthermore, in the above stress level-based steel tube concrete density safety detection method, in step 2, after the steel tube concrete is poured, the density of the concrete inside the steel tube concrete component is detected under a preset load ratio.
[0009] Furthermore, in the above-mentioned stress level-based steel tube concrete density safety detection method, the preset load ratio is 0.2, 0.4, 0.6 or 0.8.
[0010] Furthermore, in the above stress level-based steel tube concrete density safety detection method, the safety of the steel tube concrete component is evaluated as follows:
[0011] Even if the steel tube concrete component has defects, but the upper load is small, the steel tube concrete component is safe at this time; even if the steel tube concrete component has defects, but the impact on its bearing capacity is small, then the steel tube concrete component is also safe.
[0012] The stress level-based steel tube concrete density safety detection method of the present invention takes into account the influence of stress on the internal density of steel tube concrete, which is beneficial to improving the accuracy of the steel tube concrete density test results. The density of steel tube concrete is detected under different stresses, and the safety status of the component is reasonably evaluated in combination with the density and load conditions, thereby improving the reliability of the judgment results and ensuring the safety of the structure. BRIEF DESCRIPTION OF THE DRAWINGS
[0013] Various other advantages and benefits will become apparent to those of ordinary skill in the art by reading the detailed description of the preferred embodiments below. The accompanying drawings are only for the purpose of illustrating the preferred embodiments and are not to be considered as limiting the present invention. Moreover, the same reference symbols are used throughout the accompanying drawings to represent the same components. In the accompanying drawings:
[0014] Figure 1 A schematic flow chart of a method for detecting the density safety of concrete-filled steel tubes based on stress levels provided in an embodiment of the present invention;
[0015] Figure 2 Another schematic flow chart of a method for detecting the density safety of concrete-filled steel tubes based on stress levels provided by an embodiment of the present invention;
[0016] Figure 3 It is a schematic diagram of the state change of the density of an embodiment of the present invention as the construction and load increase;
[0017] Figure 4 This is a void ratio-bearing capacity analysis diagram provided in an embodiment of the present invention. DETAILED DESCRIPTION
[0018] Exemplary embodiments of the present disclosure will be described in more detail below with reference to the accompanying drawings. Although exemplary embodiments of the present disclosure are shown in the accompanying drawings, it should be understood that the present disclosure can be implemented in various forms and should not be limited by the embodiments set forth herein. On the contrary, these embodiments are provided in order to enable a more thorough understanding of the present disclosure and to be able to fully convey the scope of the present disclosure to those skilled in the art. It should be noted that, in the absence of conflict, the embodiments of the present invention and the features described in the embodiments can be combined with each other. The present invention will be described in detail below with reference to the accompanying drawings and in combination with the embodiments.
[0019] See also Figure 1 and Figure 2The method for detecting the density safety of concrete-filled steel tubes based on stress level in an embodiment of the present invention comprises the following steps:
[0020] Step 1: After the steel tube concrete component is cast, when there is no load on the upper part, a density test is performed on it to determine the density of the steel tube concrete component when there is no load on the upper part.
[0021] Specifically, an initial steel tube concrete component can be taken and its density can be tested. Since there is no load on the initial steel tube concrete component, the density obtained by the test can be used as the density of the steel tube concrete component under an ideal state.
[0022] Step 2: Take another steel tube concrete component, and after the concrete pouring is completed, perform strain monitoring and blind hole stress testing on the interior and surface of the steel tube concrete component to determine the load ratio of the steel tube concrete component.
[0023] In specific implementation, since the load on the components will gradually increase as the floors are added, another group of steel tube concrete components are taken. After the concrete is poured, strain detection and stress detection are performed on them to determine the load ratio of the steel tube concrete components.
[0024] Step 3, testing the density of concrete inside the steel tube concrete component with different load ratios, so as to obtain the density change of the steel tube concrete component under different load ratios, so as to evaluate the safety of the steel tube concrete component.
[0025] Specifically, after the steel tube concrete is poured, the density of the concrete inside the steel tube concrete component is tested under a preset load ratio, that is, the density of the same steel tube concrete component under different load ratios is tested.
[0026] The preset load ratio is 0.2, 0.4, 0.6 or 0.8.
[0027] See also Figure 3 It can be seen that although the load ratio gradually increases, the density of the steel tube concrete component is also increasing, and the two are positively correlated.
[0028] Specifically, the safety of the steel tube concrete member is evaluated as follows:
[0029] Even if the steel tube concrete component has defects, but the upper load is small, the steel tube concrete component is safe at this time; even if the steel tube concrete component has defects, but the impact on its bearing capacity is small, then the steel tube concrete component is also safe.
[0030] In this embodiment, the bearing capacity of the component corresponding to different void defect areas is calculated, and the obtained bearing capacity changes with the void rate as shown in the following figure, where the bearing capacity coefficient SI = Nt / Nh, Nh is the theoretical calculated value of the healthy component bearing capacity Nt; the void rate is the defect area divided by the component cross-sectional area. The area void rate limit is determined by reducing the theoretical calculated value of the bearing capacity to 95% of the theoretical calculated value of the healthy component bearing capacity, see Figure 4 , the limit of voiding for cylindrical spherical cap is 1.09%, the limit of voiding for cylindrical ring is 0.16%, the limit of voiding for square spherical cap is 3.58%, and the limit of voiding for square ring is 0.37%. The calculation also obtained the corresponding area voiding rate that the concrete expansion can completely fill inside the steel pipe. Below this area voiding rate, the core concrete can gradually fill the voids as the load increases.
[0031] The stress level-based steel tube concrete density safety detection method provided by the present invention takes into account the influence of stress on the internal density of steel tube concrete, which is beneficial to improving the accuracy of steel tube concrete density test results, detects the density of steel tube concrete under different stresses, and reasonably evaluates the safety status of the component in combination with the density and load conditions, thereby improving the reliability of the results and ensuring the safety of the structure.
[0032] Obviously, those skilled in the art can make various changes and modifications to the present invention without departing from the spirit and scope of the present invention. Thus, if these modifications and variations of the present invention fall within the scope of the claims of the present invention and their equivalents, the present invention is also intended to include these modifications and variations.
Claims
1. A method for detecting the density safety of steel tube concrete based on stress level, characterized in that: The following steps are involved: Step 1, after the steel tube concrete component is cast, when there is no load on the upper part, a density test is performed on it to determine the density of the steel tube concrete component when there is no load on the upper part; Step 2, taking another steel tube concrete component, and performing strain monitoring and blind hole stress testing on the interior and surface of the steel tube concrete component after the concrete pouring is completed, so as to determine the load ratio of the steel tube concrete component; Step 3, testing the density of concrete inside the steel tube concrete component with different load ratios, so as to obtain the change of density of the steel tube concrete component under different load ratios, so as to evaluate the safety of the steel tube concrete component; the judgment of the safety evaluation of the steel tube concrete component is as follows: even if the steel tube concrete component has defects, but the upper load is small, the steel tube concrete component is safe at this time; even if the steel tube concrete component has defects, but the impact on its bearing capacity is small, then the steel tube concrete component is also safe.
2. The method for detecting the density safety of steel tube concrete based on stress level according to claim 1 is characterized in that In, In the step 3, after the pouring of the steel tube concrete is completed, the density of the concrete inside the steel tube concrete component is tested under a preset load ratio.
3. The method for detecting the density safety of steel tube concrete based on stress level according to claim 2 is characterized in that In, The preset load ratio is 0.2, 0.4, 0.6 or 0.8.