A method for improving battery cycle life based on dynamically adjusting stacked stress
By dynamically adjusting the contact area between the internal electrodes and the electrolyte of the battery, and utilizing an elastic pressure device and internal resistance control technology, the lifespan and safety issues caused by increased contact resistance at the battery interface are solved, achieving long battery life and high safety in use.
Patent Information
- Application Number
- CN202311163142.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2023-09-11
- Publication Date
- 2026-11-17
- Estimated Expiration
- 2043-09-11
AI Technical Summary
Existing technologies have failed to effectively maintain minimum resistance by changing the contact area between the internal electrodes and the electrolyte of the battery, resulting in increased contact resistance at the battery interface, which affects battery life and safety.
By setting up an elastic pressure device, the contact area between the internal electrodes and electrolyte of the battery can be dynamically adjusted. Using an internal resistance controller, force sensor and electric spring, the pressure is calculated and adjusted according to the current change to keep the battery internal resistance within a minimum range, thus achieving flexible adjustment of the battery interface contact area.
It improves battery life and safety, reduces the risk of battery thermal runaway and circuit noise, extends battery cycle life, and improves output power and electrical safety.
Smart Images

Figure CN117199562B_ABST
Abstract
Description
Technical Field
[0001] This invention belongs to the field of battery technology, and in particular relates to a method for improving battery cycle life based on dynamically adjusting stacking stress. Background Technology
[0002] Batteries have gained widespread attention worldwide as a sustainable energy storage system. On the one hand, they are the power source for new energy vehicles and portable electronic products in daily life; on the other hand, they can also serve as energy storage devices to store electricity generated by renewable energy sources (such as wind or solar power) and play a role in peak shaving and valley filling for smart grids, thereby improving their quality.
[0003] The internal resistance of a battery mainly comes from two parts. One part is the battery resistance formed by the positive and negative electrode materials and the electrolyte itself. This part of the resistance depends on the conductivity of the electrode materials, the electrode structure, and the permeability of the electrolyte. The other part is the battery interface contact resistance, which is the contact interface resistance formed between the internal electrodes and the electrolyte. This part of the resistance is affected by the contact area between the internal electrodes and the electrolyte. During the charge-discharge cycle, the battery volume changes, and these volume changes cause changes in the battery interface contact resistance. After multiple charge-discharge cycles, the battery volume changes significantly, which is the common phenomenon of "battery bulging" in daily life. Battery bulging causes a sharp increase in the battery interface contact resistance, thereby affecting the battery's lifespan and safety.
[0004] To improve battery cycle life, patent documents CN113078363A and CN111864859A disclose technologies for enhancing the cycle life of lithium-ion batteries. Both technologies effectively improve cycle life. However, neither discloses a method to maintain minimum battery resistance by altering the contact area between the internal electrodes and electrolyte, thereby ensuring long battery life and high safety. Therefore, it is necessary to provide another new technology to address the aforementioned technical problems. Summary of the Invention
[0005] This invention proposes a method to improve battery cycle life based on dynamically adjusting stacked stress. This method applies dynamically changing pressure to the battery, altering the contact area between the internal electrodes and electrolyte, thereby maintaining minimum battery resistance, thus improving battery life and ensuring high-safety battery use. This solves the technical problem that existing technologies still cannot effectively improve battery life.
[0006] To achieve the above objectives, the technical solution adopted by the present invention is as follows: A method for improving battery cycle life based on dynamically adjusting stacked stress, characterized by comprising the following steps: Step 1: Set up an elastic pressure device, which can apply different pressures to the battery according to the different currents passing through it; Step 2: Collect the pressure value applied to the battery by the elastic pressure device at time step intervals, and calculate the pressure change value of the battery at the current time step based on the pressure value at the current time step and the pressure value at the previous time step; Step 3: Calculate the battery interface contact area at the current time step based on the battery's initial interface contact resistance and the pressure change value at the current time step, and calculate the battery internal resistance change value at the current time step based on the battery interface contact area at the current time step and the battery's comprehensive influence constant. Step 4: Calculate the dynamic change current value that should be supplied to the elastic pressure device at the current time step based on the change value of the battery internal resistance at the current time step and the initial interface contact resistance of the battery. Step 5: The elastic pressure application device applies corresponding pressure to the battery based on the dynamically changing current value; Step 6: Reacquire the pressure value applied to the battery by the elastic pressure device at the current time step, and recalculate the change in battery internal resistance at the current time step; Step 7: Determine whether the change in battery internal resistance at the current time step meets the set conditions; Step 8: If the set conditions are met, maintain the dynamic change current value that should be applied in the current time step, and repeat steps 2 to 7 at the beginning of the next time step until the charging / discharging ends; if the set conditions are not met, recalculate the dynamic change current value that should be applied to the elastic pressure device in the current time step based on the battery internal resistance change value that does not meet the set conditions, and repeat steps 5 to 7 until the set conditions are met.
[0007] The elastic pressure application device includes an internal resistance controller, a force sensor, and an electric spring. The electric spring is used to apply pressure to the battery. The force sensor is used to collect the pressure value applied by the electric spring to the battery. The internal resistance controller is used to read the pressure value collected by the force sensor and to calculate the pressure change value, battery interface contact area, battery internal resistance change value, and dynamic current change value, respectively. It is used to control the electric spring to apply corresponding pressure to the battery according to the dynamic current change value, and to determine whether the battery internal resistance change value meets the set conditions.
[0008] The number of electric springs is at least one. When the number of electric springs exceeds one, the pressure values collected at each time step are average values.
[0009] In step two, the time step is calculated as follows: t=T / n In the formula, t represents the time step, T represents the total time for the battery to perform one charge / discharge cycle, and n ranges from 5 to 100.
[0010] In step two, the method for calculating the pressure change value of the battery at the current time step is as follows: ΔF=F t -F t-1 In the formula, ΔF represents the pressure change value of the battery at the current time step, F t F represents the pressure value of the battery at the current time step. t-1 This indicates the pressure value at the previous time step of the battery.
[0011] In step three, the method for calculating the change in battery internal resistance at the current time step is as follows: ΔR = k / ΔS in, ΔS=R t0 exp(ΔF) In the formula, ΔR represents the change in battery internal resistance at the current time step, ΔS represents the battery interface contact area at the current time step, and k is a constant representing the combined influence of the resistivity of the battery internal materials and the battery geometry; R t0 This indicates the initial interface contact resistance of the battery.
[0012] In step four, the method for calculating the dynamically changing current value at the current time step is as follows: I t =(lnΔR / R t0 )x)+I t-1 In the formula, I t I represents the dynamically changing current value at the current time step. t-1 This represents the dynamic change in current value at the previous time step. x is a constant that is related to the material properties of the electric spring.
[0013] In step five, the calculation method for the elastic pressure application device to apply corresponding pressure to the battery based on the dynamically changing current value is as follows: F=I t x In the formula, F represents the corresponding pressure applied to the battery by the elastic pressure device.
[0014] In step seven, determining whether the change in battery internal resistance at the current time step meets the set condition means determining whether the change in battery internal resistance satisfies ΔR < mR0, where m ∈ [0.0001, 0.5].
[0015] The advantages of using this invention are: 1. This invention applies dynamically changing pressure to the battery, which allows for flexible adjustment of the contact area between the internal electrodes and the electrolyte, ensuring that the battery maintains minimum resistance. This improves the battery's lifespan and ensures its safe operation, solving the technical problem that existing technologies cannot effectively improve battery lifespan.
[0016] 2. This invention can dynamically monitor the battery interface contact area throughout the battery's entire life cycle, and can meet the requirements of long battery life and high safety in single charge-discharge cycles and full life cycle cycles.
[0017] 3. This invention can achieve rational adjustment of the battery interface contact resistance, select the most suitable applied pressure through feedback verification technology, and thus maintain the minimum interface contact resistance of the battery.
[0018] 4. This invention can reduce losses and improve battery output power by maintaining minimum contact resistance. By maintaining minimum contact resistance, the loss of battery current during the output process can be reduced, thereby improving battery output power.
[0019] 5. This invention reduces the risk of battery thermal runaway and extends battery life by maintaining minimum contact resistance: When a battery is charging and discharging, due to the presence of contact resistance, some electrical energy is converted into heat energy, causing the battery temperature to rise. This not only reduces battery life but may also lead to overheating or even explosion. Maintaining minimum contact resistance can effectively reduce this overheating risk and extend battery life.
[0020] 6. This invention maintains minimum contact resistance, which also reduces circuit noise and minimizes battery hazards: Contact resistance introduces circuit noise, which can interfere with other electronic devices or sensors. Maintaining minimum contact resistance reduces this noise and improves circuit reliability and accuracy.
[0021] 7. By maintaining minimum contact resistance, the present invention can reduce arcing in the circuit, thereby reducing the risk of fire and electric shock and improving electrical safety. Attached Figure Description
[0022] Figure 1 This is a flowchart of the present invention; Figure 2 A flowchart for determining whether the change in battery internal resistance at the current time step meets the set conditions. Figure 3 This is a schematic diagram of the elastic pressure application device in this invention; Figure 4 A graph showing the dynamic changes in the battery interface contact resistance and the applied current value of the electric spring. Figure 5 This is a comparison chart of battery health status (SOH) during the verification of this invention.
[0023] The diagram is labeled as follows: 1. Force sensor, 2. Electric spring. Detailed Implementation
[0024] Example 1 This invention provides a method for improving battery cycle life based on dynamically adjusting stacking stress. This method is suitable for improving the cycle life of both ordinary batteries and various types of lithium batteries. Furthermore, while this method is applicable throughout the battery's entire lifespan, since the battery's volume changes significantly only during charging / discharging, and is negligible during non-charging / discharging, this method is particularly suitable for dynamically adjusting the stacking stress of the battery during charging / discharging to maintain minimum internal resistance and effectively improve battery cycle life.
[0025] The following section provides a detailed explanation of this solution in conjunction with the battery charging / discharging process.
[0026] like Figure 1 , 2 As shown, the method includes the following steps: Step 1: Set up an elastic pressure device that can apply different pressures to the battery depending on the current flowing through it.
[0027] Specifically, such as Figure 3 As shown, the elastic pressure application device includes an internal resistance controller, a force sensor 1, and an electric spring 2. The electric spring 2 applies pressure to the battery. The force sensor 1 collects the pressure value applied to the battery by the electric spring at time intervals. The internal resistance controller reads the pressure value collected by the force sensor 1 at each time step, calculates the pressure change value at each time step based on the collected pressure value, calculates the battery interface contact area at each time step, calculates the battery internal resistance change value at each time step, calculates the dynamic current change value at each time step, controls the electric spring 2 to apply corresponding pressure to the battery according to the calculated dynamic current change value, and determines whether the battery internal resistance change value meets the set conditions, etc.
[0028] The number of electric springs 2 is at least one. When the number of electric springs 2 exceeds one, the pressure value collected at each time step is the average value of the electric springs 2. Preferably, the number of electric springs 2 is two and they are symmetrically arranged on both sides of the battery.
[0029] It should be noted that the electric spring 2 is a conventional technology. For example, according to the research of Su et al., the extension and contraction of the spring can be controlled by the magnitude of the current. Such springs are made of piezoelectric materials (Su Y, Li Q, Amagat J, et al. 3Dspring-based piezoelectric energy generator[J]. Nano Energy, 2021, 90:106578.) It can apply different pressures to the battery depending on the magnitude of the input current. The pressure exerted by the electric spring 2 on the battery (the spring force) can be calculated using the following formula: F=Ix In the formula, F is the spring force of the electric spring, I is the current, and x is a constant.
[0030] The value of x is related to the material properties of the electric spring and can be obtained through experiments. Specifically, apply an arbitrary current I1 to the electric spring and measure the spring force F1. Then, select an arbitrary current I2 of a different magnitude than I1 and measure the corresponding spring force F2. Based on this, x = (F1 - F2) / (I1 - I2) can be calculated. Electric springs made of the same type of material have the same value of x.
[0031] In addition to the internal resistance controller, force sensor 1, and electric spring 2, the elastic pressure device can also be equipped with corresponding frames, support frames, and other structural components to fix the electric spring 2 and force sensor 1, in order to ensure that the force of the electric spring 2 can be accurately applied to the battery and that the force sensor 1 can accurately collect the pressure value applied by the electric spring 2 to the battery.
[0032] Step Two: First, the internal resistance controller sets the time step based on the total charging / discharging time of the battery. The calculation method for the time step is as follows: t=T / n In the formula, t represents the time step, T represents the total time for the battery to perform one charge / discharge cycle, and n ranges from 5 to 100.
[0033] Secondly, the internal resistance controller controls the force sensor to collect the pressure value applied to the battery by the electric spring at time step intervals, and calculates the pressure change value of the battery at the current time step based on the pressure value at the current time step and the pressure value at the previous time step.
[0034] Specifically, the method for calculating the pressure change value of the battery at the current time step is as follows: ΔF=F t -F t-1 In the formula, ΔF represents the pressure change value of the battery at the current time step, F tF represents the pressure value of the battery at the current time step. t-1 This indicates the pressure value at the previous time step of the battery.
[0035] Step 3: The internal resistance controller calculates the battery interface contact area at the current time step based on the battery's initial interface contact resistance and the pressure change value at the current time step, and calculates the battery internal resistance change value at the current time step based on the battery interface contact area at the current time step and the battery's comprehensive influence constant.
[0036] Specifically, the method for calculating the change in battery internal resistance at the current time step is as follows: ΔR = k / ΔS in, ΔS=R t0 exp(ΔF) In the formula, ΔR represents the change in battery internal resistance at the current time step, ΔS represents the battery interface contact area at the current time step, and k is a constant representing the combined influence of the resistivity of the battery internal materials and the battery geometry; R t0 This indicates the initial interface contact resistance of the battery. The initial interface contact resistance of the battery is marked on the battery at the factory.
[0037] It should be noted that the constant k can be obtained experimentally. Specifically, the method is to measure the battery's internal resistance R at any time t1. t1 And the spring force F at this time t1 The battery internal resistance R is measured at any time t2 different from t1. t2 And the spring force F at this time t2 It can be calculated that: k=(R t1 -R t2 ) / ((R0) exp(F t1 -F t2 )) In the formula, R0 represents the battery resistance formed by the positive and negative electrode materials and the electrolyte itself. The battery resistance is marked on the battery when it leaves the factory; the constant k is the same for batteries of the same type.
[0038] Step 4: The internal resistance controller calculates the dynamic change current value that should be applied to the elastic pressure device at the current time step based on the change value of the battery's internal resistance at the current time step and the battery's initial interface contact resistance.
[0039] Specifically, the calculation method for the dynamically changing current value at the current time step is as follows: I t =(lnΔR / R t0 )x)+I t-1 In the formula, I t I represents the dynamically changing current value at the current time step. t-1 This represents the dynamic change in current value at the previous time step. x is a constant that is related to the material properties of the electric spring.
[0040] Step 5: The internal resistance controller controls the electric spring in the elastic pressure device to input a dynamically changing current value. By changing the input current of the electric spring, the electric spring applies pressure to the battery corresponding to the dynamically changing current value.
[0041] Specifically, the calculation method for the electric spring applying corresponding pressure to the battery based on the dynamically changing current value is as follows: F=I t x In the formula, F represents the corresponding pressure applied by the electric spring to the battery.
[0042] Step 6: The internal resistance controller controls the force sensor to re-acquire the pressure value applied to the battery by the electric spring at the current time step, and recalculates the change in battery internal resistance at the current time step.
[0043] Step 7: Determine whether the change in battery internal resistance at the current time step meets the set conditions. Specifically, determining whether the change in battery internal resistance at the current time step meets the set conditions means: determining whether the change in battery internal resistance satisfies ΔR < mR0, where m ∈ [0.0001, 0.5].
[0044] Step 8: If the set conditions are met, maintain the dynamically changing current value I that should be applied at the current time step. t Then, at the beginning of the next time step, steps two through seven are repeated until the charging / discharging ends; if the set conditions are not met, the dynamic change current value that should be supplied to the elastic pressure device in the current time step is recalculated based on the battery internal resistance change value that does not meet the set conditions, and steps five through seven are repeated until the set conditions are met.
[0045] It should be noted that the method described in this invention mainly maintains the internal resistance of the battery by dynamically adjusting the electric spring to apply different pressures to the battery. The stacking stress on the battery is equal to the pressure applied by the electric spring divided by the area on which the force is applied. Adjusting the pressure on the electric spring is actually adjusting the stacking stress on the battery surface. Since the electric spring acts on a surface, and the surface area of different types of batteries varies greatly, the physical quantity of pressure divided by the area on which the force is applied is used to represent the stacking stress.
[0046] The present invention can achieve the interface contact resistance R through the above method. t The dynamic changes of both the electric spring and the applied current I are as follows: Figure 4 As shown, when the interface contact resistance R tWhen the pressure increases, the internal resistance controller will control the current I to increase accordingly, thereby increasing the pressure F. The stacking stress P increases accordingly, causing the interface contact area S to increase, leading to R t Reduce. To avoid applying excessive pressure F to the battery for extended periods, which could cause severe wear on the contact surfaces and lead to interface contact failure, the interface contact resistance R is reduced. t As the current decreases, the current I also decreases. This is because the current I on the electric spring and the contact resistance R at the battery interface decrease during a single charge / discharge process. t A process of dynamic change.
[0047] In summary, this invention applies dynamically varying pressure to the battery, allowing for flexible adjustment of the contact area between the internal electrodes and the electrolyte. This maintains the battery at its minimum resistance, thereby improving battery lifespan and ensuring safe operation. It solves the technical problem that existing technologies cannot effectively improve battery lifespan.
[0048] Example 2 This embodiment verifies the method of the present invention as follows: Under the same conditions, the same group of batteries was subjected to approximately 1200 charge / discharge cycles using the method of this invention and without the method of this invention, resulting in the following... Figure 5 The battery health status (SOH) comparison chart shown indicates that the battery using the method of this invention exhibits a smaller overall change in resistance, and the battery SOH remains above 80%. In contrast, the battery without the method of this invention shows a larger change in internal resistance, and the battery SOH drops to approximately 60%. It is evident that the method of this invention has a significant effect on reducing battery internal resistance and increasing battery SOH, thereby significantly improving the battery's cycle life.
[0049] The above description is merely a specific embodiment of the present invention. Any feature disclosed in this specification may be replaced by other equivalent or similar features unless otherwise specified. All features or steps in the disclosed methods or processes may be combined in any way, except for mutually exclusive features and / or steps.
Claims
1. A method for improving battery cycle life based on dynamically adjusting stacked stress, characterized in that, Includes the following steps: Step 1: Set up an elastic pressure device, which can apply different pressures to the battery according to the different currents passing through it; Step 2: Set the time step according to the total charging / discharging time of the battery, collect the pressure value applied to the battery by the elastic pressure device at time step intervals, and calculate the pressure change value of the battery at the current time step based on the pressure value of the current time step and the pressure value of the previous time step. In step two, the time step is calculated as follows: t=T / n In the formula, t represents the time step, T represents the total time for the battery to perform one charge / discharge cycle, and n ranges from 5 to 100. In step two, the method for calculating the pressure change value of the battery at the current time step is as follows: ΔF=F t -F t-1 In the formula, ΔF represents the pressure change value of the battery at the current time step, F t F represents the pressure value of the battery at the current time step. t-1 This indicates the pressure value of the battery at the previous time step; Step 3: Calculate the battery interface contact area at the current time step based on the battery's initial interface contact resistance and the pressure change value at the current time step, and calculate the battery internal resistance change value at the current time step based on the battery interface contact area at the current time step and the battery's comprehensive influence constant. In step three, the method for calculating the change in battery internal resistance at the current time step is as follows: ΔR = k / ΔS in, ΔS=R t0 exp(ΔF) In the formula, ΔR represents the change in battery internal resistance at the current time step, ΔS represents the battery interface contact area at the current time step, and k is a constant representing the combined influence of the resistivity of the battery internal materials and the battery geometry; R t0 Indicates the initial interface contact resistance of the battery; Step 4: Calculate the dynamic change current value that should be supplied to the elastic pressure device at the current time step based on the change value of the battery internal resistance at the current time step and the initial interface contact resistance of the battery. In step four, the method for calculating the dynamically changing current value at the current time step is as follows: I t =((lnΔR / R t0 )x)+I t-1 In the formula, I t I represents the dynamically changing current value at the current time step. t-1 This represents the dynamically changing current value at the previous time step, where x is a constant related to the material properties of the electric spring. Step 5: The elastic pressure application device applies corresponding pressure to the battery based on the dynamically changing current value; In step five, the calculation method for the elastic pressure application device to apply corresponding pressure to the battery based on the dynamically changing current value is as follows: F=I t x In the formula, F represents the corresponding pressure applied to the battery by the elastic pressure application device; Step 6: Reacquire the pressure value applied to the battery by the elastic pressure device at the current time step, and recalculate the change in battery internal resistance at the current time step; Step 7: Determine whether the change in battery internal resistance at the current time step meets the set conditions; In step seven, determining whether the change in battery internal resistance at the current time step meets the set condition means determining whether the change in battery internal resistance satisfies ΔR < mR0, where m ∈ [0.0001, 0.5]. Step 8: If the set conditions are met, maintain the dynamic change current value that should be applied in the current time step, and repeat steps 2 to 7 at the beginning of the next time step until the charging / discharging ends; if the set conditions are not met, recalculate the dynamic change current value that should be applied to the elastic pressure device in the current time step based on the battery internal resistance change value that does not meet the set conditions, and repeat steps 5 to 7 until the set conditions are met.
2. The method for improving battery cycle life based on dynamically adjusting stacking stress according to claim 1, characterized in that: The elastic pressure application device includes an internal resistance controller, a force sensor, and an electric spring. The electric spring is used to apply pressure to the battery. The force sensor is used to collect the pressure value applied by the electric spring to the battery. The internal resistance controller is used to read the pressure value collected by the force sensor and to calculate the pressure change value, battery interface contact area, battery internal resistance change value, and dynamic current change value, respectively. It is used to control the electric spring to apply corresponding pressure to the battery according to the dynamic current change value, and to determine whether the battery internal resistance change value meets the set conditions.
3. The method for improving battery cycle life based on dynamically adjusting stacking stress according to claim 2, characterized in that: The number of electric springs is at least one. When the number of electric springs exceeds one, the pressure values collected at each time step are average values.
Citation Information
Patent Citations
Lithium battery pack service life prolonging system and method with constant-current and constant-voltage charging and discharging
CN111864859A
Method for prolonging cycle life of lithium ion battery
CN113078363A
Device and method for detecting response time of magneto-rheological elastomer
CN110940586A
Corrosion rate measuring device and method based on slide rheostat
CN114199748A