By employing a multi-layer structure in the plastic pipe, with an outer layer of PVC or CPVC and an inner layer of polycarbonate, and adding glass filler, the problems of high cost and insufficient thermal stability of existing pipes are solved, achieving a cost-effective improvement in thermal stability.

CN117355381BActive Publication Date: 2026-11-17ENGINEERED PROFILES LLC
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
CN202280036809.2
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Priority Date
2021-05-05
Filing Date
2022-05-05
Publication Date
2026-11-17
Estimated Expiration
2042-05-05

AI Technical Summary

Technical Problem

Existing plastic pipe materials such as PVC and CPVC are expensive and lack thermal stability, necessitating a cost-effective alternative that provides improved or similar thermal stability.

Method used

It adopts a multi-layer structure, with the outer layer being PVC or CPVC and the inner layer being polycarbonate. Glass filler can be added to enhance thermal stability. The pipe is manufactured through extrusion or co-extrusion processes.

Benefits of technology

It achieves significant improvement in the thermal stability and other mechanical and chemical properties of pipelines while reducing costs, and is suitable for both pressurized and non-pressurized applications.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN117355381B_ABST
    Figure CN117355381B_ABST
Patent Text Reader

Abstract

A multilayer pipe includes at least a first layer and a second layer, wherein the first layer is composed of a first polymer having a first thermal stability, and the second layer is composed of a second polymer having a second thermal stability improved relative to the first thermal stability. In one exemplary embodiment, the first layer is composed of PVC or CPVC, and the second layer is composed of polycarbonate.
Need to check novelty before this filing date? Find Prior Art

Description

[0001] This application claims priority to U.S. Provisional Application No. 63 / 184303, filed May 5, 2021, the entire contents of which are incorporated herein by reference. Technical Field

[0002] Exemplary embodiments of the present invention generally relate to pipelines. Background Technology

[0003] Plastic pipes are typically made of polyvinyl chloride (PVC) or chlorinated polyvinyl chloride (CPVC). PVC or CPVC provides beneficial properties for pipes, such as corrosion resistance and degradability. Both materials have good heat resistance. Specifically, PVC can have a maximum functional temperature of about 140°F, and CPVC can have a maximum functional temperature of about 200°F. However, both PVC and CPVC are expensive, with CPVC typically costing significantly more than PVC. Therefore, there is a need for a cost-effective alternative to PVC and CPVC, particularly for plastic pipes, that offers improved or similar thermal stability compared to PVC and CPVC, especially those used in conventional plastic pipes.

[0004] Other types of pipes can be made of polyethylene, polypropylene, or other polymers. These other polymers may also be expensive and / or lack thermal stability. Therefore, there is a need for a cost-effective alternative to any of these polymers, while also having improved or similar thermal stability compared to those polymers. Summary of the Invention

[0005] Exemplary embodiments can address some or all of the disadvantages of known technologies. In an exemplary embodiment, the conduit includes at least a first layer and a second layer, wherein the first layer is composed of a first polymer having a first thermal stability, and the second layer is composed of a second polymer having a second thermal stability that is improved relative to the first thermal stability.

[0006] In at least one exemplary embodiment, at least the first layer may include PVC, CPVC, acrylonitrile butadiene styrene (ABS), polyethylene, polypropylene, or other similar or suitable materials. The second layer may include polycarbonate, acrylic acid, acrylonitrile styrene acrylate, acrylonitrile butadiene acrylate, ABS, CPVC, nylon, or other similar or suitable materials that have improved thermal stability relative to the polymer of the first layer. Some exemplary embodiments may also include at least a third layer. For example, as an example, a particularly useful embodiment may include PVC or CPVC as an outer layer, polycarbonate as an intermediate layer, and PVC or CPVC as an inner layer. In one example, compared to other similar conventional components that only include the aforementioned first layer and / or do not have the aforementioned second layer, the embodiment may provide improved thermal stability characteristics. In another example, compared to other similar conventional components that only include the aforementioned first layer and / or do not have the aforementioned second layer, the embodiment may provide the same, similar, or improved thermal stability characteristics at a reduced cost.

[0007] In one exemplary embodiment, the plastic conduit includes at least one layer (preferably an outer layer) made of PVC or CPVC and at least one layer (preferably an intermediate or inner layer) made of polycarbonate. While plastic conduits are typically made of PVC or CPVC, other exemplary embodiments of the invention may have at least one layer (preferably an outer layer) made of polyethylene or polypropylene and at least one layer (preferably an intermediate or inner layer) made of nylon. In any of these embodiments, the resulting plastic conduit may have improved thermal stability properties or the same, similar, or improved thermal stability properties at a reduced cost compared to other similar components made solely of PVC, CPVC, polyethylene, or polypropylene.

[0008] In an exemplary embodiment, the first, second, and / or any additional layer may have at least one additional filler, additive, or dopant material mixed with the polymer material. Some types of fillers include, but are not limited to, glass, talc, fibrous materials, chemicals, metals, other mineral fillers, and other organic or inorganic materials. If desired, other materials or material layers may be used, and they must be compatible with at least one of the aforementioned layers.

[0009] The filler, additive, or dopant can be any material compatible with the material of the layer in which the filler is placed. Additionally, the user can select which fillers, additives, or dopants to use based on the properties that will enhance or be added to the final material. One or more fillers may be used.

[0010] In particular, additives, fillers, or dopants may be desired to improve (or at least not impair) the thermal stability of the piping. Thermal stability refers to a material's resistance to permanent qualitative changes caused solely by heat. Heat distortion temperature (HDT), coefficient of linear thermal expansion (CLTE), and shrinkage rate are some commonly used metrics for assessing thermal stability. Exemplary embodiments of the invention may improve the thermal stability described above or otherwise, as used herein with respect to "improvements," etc.

[0011] Additionally, exemplary embodiments of the final material may have improved thermal deformation, improved thermal motion, improved surface finish, or improved impact resistance. Exemplary embodiments of the final material may also provide better structural stability, be manufactured at a lower cost, or provide improved physical, electrical, or other properties as needed.

[0012] In addition to the novel features and advantages described above, other advantages will become apparent from the following description of the accompanying drawings and exemplary embodiments. Attached Figure Description

[0013] Figure 1 This is a side view of an exemplary embodiment of the pipe of the present invention.

[0014] Figure 2 Examples of graphs showing the linear coefficient of thermal expansion and shrinkage (and other properties) of various examples of multilayer pipes comprising PVC or CPVC layers and polycarbonate layers are provided. For comparison, sample 19 of a conventional CPVC pipe is also shown.

[0015] Figure 3 yes Figure 2 Examples of graphs showing the linear coefficient of thermal expansion for various examples.

[0016] Figure 4 yes Figure 2 Examples of various examples of collapsed exemplary charts.

[0017] Figure 5 Is with Figure 2 Exemplary diagrams relating the adhesion between layers in various examples.

[0018] Figure 6 This is a side view of an exemplary embodiment of the pipe of the present invention. Detailed Implementation

[0019] This disclosure describes exemplary embodiments of pipes that can be manufactured by extrusion or co-extrusion processes, wherein the pipes can have improved thermal stability. Additionally, depending on the materials and fillers used, the pipes can have improved mechanical, chemical, electrical, or other properties. Desired properties can be achieved using combinations of materials. For example, combinations of materials can be selected to reduce costs while increasing thermal stability and other properties, and also to impart a high-quality appearance to the pipe material.

[0020] The tubing may comprise at least two layers of different polymer materials, wherein fillers, additives, or dopants may be incorporated into the respective polymer materials. Tubing is typically manufactured using known extrusion or co-extrusion processes. However, other suitable manufacturing processes may be employed.

[0021] Various combinations of materials can be selected based on the conditions the pipeline needs to withstand and the mechanical, thermal, chemical, or other properties it requires. For example, pressurized applications that may experience high temperatures may require certain materials with sufficient thermal stability, while non-pressurized applications may allow for a wider range of materials.

[0022] Figure 1 Exemplary embodiments of the conduit of the present invention are shown, in which any of the above considerations may be applied. In this exemplary embodiment, conduit 100 includes at least one layer (preferably outer layer 102) made of a polymer having a first or basic thermal stability, and at least one layer (preferably inner layer 104) made of another polymer having improved thermal stability relative to the polymer of the first layer. For example, as an alternative to conventional PVC or CPVC conduit, conduit 100 may include at least one layer (preferably outer layer 102) made of PVC or CPVC, and at least one layer (preferably inner layer 104) made of polycarbonate. As an alternative to or supplement to PVC or CPVC, other exemplary embodiments of the present invention may have at least one layer (preferably outer layer) made of polyethylene or polypropylene, and at least one layer (preferably inner layer) made of polycarbonate. However, in other exemplary embodiments, PVC, CPVC, polyethylene, or polypropylene may form an intermediate or inner layer, and / or polycarbonate may form an intermediate or outer layer. Some exemplary embodiments may also include other material layers required or desired for a particular application. In all such exemplary embodiments, the pipes may have improved thermal stability characteristics or the same, similar or improved thermal stability characteristics at a reduced cost compared to other similar pipes made only of PVC, CPVC, polyethylene or polypropylene.

[0023] In some exemplary embodiments of the conduit 100, the inventors have found that the inner layer 104 may include glass filler in an amount up to about 35 wt% of the inner layer 104, more preferably between about 9 wt% and 30 wt% of the inner layer 104. Glass filler can further enhance thermal stability and also contribute to further cost reduction. However, as with the previous embodiments herein, the outer layer 102 (or an additional layer in other embodiments) may include glass filler in addition to or as an alternative to the inner layer 104. Furthermore, other fillers, additives, or dopants designed to further improve the thermal, electrical, chemical, or other properties of the conduit 100 may be used. In addition to glass filler, the user may select other suitable fillers, additives, or dopants, and their concentrations, based on the desired characteristics of the conduit 100. The amount and type of filler added will depend on the physical or other properties that can be imparted to the conduit 100.

[0024] Figure 2-6 Different examples of pipe 100 with a polycarbonate inner layer 104 are shown. In samples or items 1-12 and 20-22, the outer core polymer is PVC. In samples or items 13-18, the outer core polymer is CPVC. Figure 2-6 The sample or item 19 in the examples is compared to conventional CPVC pipes. In each of these exemplary embodiments, pipe 100 has a total thickness of approximately 0.060 inches, and inner layer 104 is approximately 0.015 inches to 0.030 inches thick. Other exemplary embodiments may have other total thicknesses, as well as inner, outer, and / or other layers with other thicknesses, as may be required or advantageous for a particular application.

[0025] The CPVC comparison sample or item 19 has a heat shrinkage rate of 0.31% at 230°F and a linear coefficient of thermal expansion (CLTE) of approximately 4.02 × 10⁻⁶ at 230°F. -5 in / in-°F. In samples or articles 10-12 without glass filler, the PVC examples have similar or improved heat shrinkage rates between about 0.06% and 0.35% at 230°F, and at 3.42 × 10⁻⁶. -5 in / in-°F and 3.73×10 -5 Improved CLTE between in / in-°F, all of which offer significantly reduced costs compared to conventional CPVC pipes. Similarly, in samples or articles 13-15 without glass filler, the CPVC examples exhibit similar or improved heat shrinkage rates between about 0.22% and 0.30% at 230°F, and at about 3.84 × 10⁻⁶. -5 in / in-°F and 4.06×10 -5Similar to or improved CLTE between in / in-°F, it also offers a significant cost reduction compared to conventional CPVC pipes.

[0026] The inventors have discovered that the addition of glass filler can further improve heat shrinkage rate and CLTE compared to conventional CPVC pipes (and extended to conventional PVC pipes), while providing a significant cost reduction. In samples or items 1-3 with 9 wt% glass filler in the polycarbonate layer 104, the PVC examples exhibited a significantly improved heat shrinkage rate between about 0.08% and 0.10% at 230°F, and a CLTE of about 3.05 × 10⁻⁶. -5 in / in-°F and 3.36×10 -5 Significantly improved CLTE between in / in-°F. In samples or items 4-6 with 20 wt% glass filler in polycarbonate layer 104, the PVC examples exhibited a significantly improved heat shrinkage rate between about 0.05% and 0.07% at 230°F, and at about 2.51 × 10⁻⁶. -5 in / in-°F and 2.85×10 -5 A significantly improved CLTE was observed between in / in-°F. Furthermore, in samples or items 20-22 containing 20 wt% glass filler in the polycarbonate layer 104, the PVC examples exhibited a significantly improved heat shrinkage rate between approximately 0.07% and 0.08% at 230°F, and a shrinkage rate of approximately 2.56 × 10⁻⁶. -5 in / in-°F and 2.63×10 -5 CLTE is significantly improved between in / in-°F. Furthermore, in samples or items 16-18 with 20 wt% glass filler in the polycarbonate layer 104, the CPVC examples exhibit even more significantly improved heat shrinkage rates between approximately 0.04% and 0.07% at 230°F, and approximately 2.31 × 10⁻⁶. - 5 in / in-°F and 2.98×10 -5 CLTE showed even more significant improvements between in / in-°F. Similarly, significant improvements were observed when the amount of glass filler in polycarbonate layer 104 was increased to 30 wt%. Indeed, in samples or items 7-9, such PVC embodiments exhibited improved heat shrinkage rates between approximately 0.07% and 0.09% at 230°F, and at approximately 2.23 × 10⁻⁶. -5 in / in-°F and 2.68×10 -5CLTE with even further improvements between in / in-°F. Based on the foregoing examples, similar benefits are expected for embodiments with a PVC or CPVC outer layer, and for embodiments with a polyethylene or polypropylene outer layer relative to conventional polyethylene or polypropylene pipes, for different amounts of glass filler content up to about 35 wt%. Furthermore, significant improvements in heat distortion temperature (HDT) can be achieved (e.g., Figure 2 Samples 13-18).

[0027] Figure 6 An example of a pipe with at least one additional layer is shown. This exemplary embodiment of the pipe can be similar to the example of pipe 100, except for the addition of at least one other layer. For example, certain standards or regulations may only allow certain pre-approved materials to be used as the innermost layer of the pipe. In this case, at least one additional layer may be positioned inside the aforementioned second layer to contact any fluid that can flow through the pipe. Other examples may also have at least one additional layer positioned outside the aforementioned first layer, or between the aforementioned first and second layers. Furthermore, as mentioned above, in other exemplary embodiments, the layers may be rearranged in other ways according to the needs or expectations of a particular application.

[0028] exist Figure 6 In this example, the conduit 200 includes a first polymer layer 202 having a first thermal stability, a second polymer layer 204 having a second thermal stability improved relative to the first thermal stability, and a third polymer layer 206 having thermal stability between the first and second thermal stability. In this exemplary embodiment, the first layer 202 may be made of PVC or CPVC, and the second layer 204 may be made of polycarbonate. Furthermore, in this exemplary embodiment, the third layer 206 may be the innermost layer made of the same polymer as the first layer. However, other exemplary embodiments may have a third layer made of a different polymer than the first layer, and / or may be positioned in other locations relative to the aforementioned first and second layers, such as may be necessary or desired for certain applications.

[0029] Other exemplary embodiments may include other polymers suitable for the application. The examples described above may be particularly suitable for pressurized applications (e.g., involving high heat), while also being applicable to non-pressurized applications. Other polymers may be suitable for other applications (e.g., non-pressurized applications). For example, some other exemplary embodiments may have a first layer made of PVC, CPVC, ABS, polyethylene, or polypropylene, and a second layer made of polycarbonate or ABS. Furthermore, other exemplary embodiments may have at least one additional layer made of PVC, CPVC, ABS, polyethylene, polypropylene, or another polymer having thermal stability between that of the first and second polymers. Finally, other exemplary embodiments may include other additives and fillers in any layer, such as those that may be suitable or desired for any application.

[0030] The foregoing examples describe some possible alternatives to conventional types of piping. Based on the aforementioned principles, other variations are possible to improve the thermal stability of the piping and / or reduce its cost. In exemplary embodiments, the first layer can be a polymer, copolymer, or other material with desired properties. The first layer can be any material that is chemically compatible with or otherwise bondable (e.g., using a bonding layer) to the polymeric material of the second layer. In exemplary embodiments, the material in the first layer can include PVC, CPVC, ABS, high-density polyethylene (HDPE), low-density polyethylene (LDPE), polypropylene, or other similar or suitable materials.

[0031] In another exemplary embodiment of a pipe with a total thickness of 0.040 to 0.060 inches, the first layer may be 0.001 inches to 0.050 inches thick. More preferably, in such an embodiment, the first layer may be 0.005 inches to 0.030 inches thick, and even more preferably, the first layer may be 0.015 inches to 0.025 inches thick. In yet another exemplary embodiment with a total thickness of 0.5 inches, the first layer may be 0.002 inches to 0.200 inches thick. Other exemplary embodiments may have other total thicknesses and first layers with other total thicknesses, as may be necessary or beneficial for a particular pipe.

[0032] The second layer can be a polymer, copolymer, or other material that is chemically compatible with or otherwise can be attached to the first layer. Additionally, the material of the second layer can include fillers, additives, or dopants to create a composite material. In exemplary embodiments, the primary component of the second layer can typically be polycarbonate (PC), acrylic acid, acrylonitrile styrene acrylate (ASA), acrylonitrile butadiene acrylate (ABA), acrylonitrile butadiene styrene (ABS), CPVC, nylon, or other similar or suitable materials.

[0033] While some examples of materials used for different layers have been mentioned above, many other types of materials can be implemented in various other embodiments. For example, standard plastics, engineering plastics, advanced engineering materials, and imidized materials can be used for any layer, which may be amorphous or crystalline, where the materials of adjacent layers may or may not be compatible. For example, in the case of incompatible layers, a bonding layer can be used to bond adjacent layers together. In the progression from standard plastics, engineering plastics, advanced engineering materials to imidized materials, the properties of the materials can generally be transformed from: 1) versatility, lower stress tolerance, good adhesion, and good formability; 2) engineering or structural grade, and good abrasion resistance; 3) higher temperature resistance, higher steam resistance, higher abrasion resistance, and higher chemical resistance. Examples of standard plastics include, but are not limited to, polystyrene (PS), acrylonitrile butadiene styrene (ABS), PVC, CPVC, polypropylene (PP), HDPE, and low-density polyethylene (LDPE). Examples of engineering plastics include, but are not limited to, polyphenylene oxide (PPO), acrylic acid, PC, acetal, polyoxymethylene (POM), polyethylene terephthalate (PTEP), ultra-high molecular weight polyethylene (UHMW PE), nylon, and polyamide (PA). Examples of advanced engineering materials include, but are not limited to, polysulfone (PSU), polyphenylene sulfone (PPSU), polyetherimide (PEI), polyphenylene sulfide (PPS), polyether ether ketone (PEEK), and polytetrafluoroethylene (PTFE). Finally, examples of imidized materials include, but are not limited to, polyimide (PI), polybenzimidazole (PBI), and polyamide-imide (PAI). Specific materials can be selected for each layer of multilayer piping to achieve desired physical properties (e.g., thermal stability). However, other factors may also be considered in material selection, such as material availability, material cost, and manufacturability.

[0034] As described above, the first or second layer (or an additional layer in other embodiments) may comprise fillers, additives, or dopants designed to improve the thermal, electrical, chemical, or other properties of the conduit. Users can select appropriate fillers, additives, or dopants, and their concentrations, based on the desired properties of the final conduit. The amount and type of filler added may depend on the physical or other properties imparted to the conduit. In one exemplary embodiment, the amount of filler added may be 10 wt% to 45 wt% of the weight of the second layer, and more preferably, 30 wt% to 40 wt% of the weight of the second layer. In yet another exemplary embodiment, the amount of filler added may be 0 wt% to 70 wt% of the weight of the second layer, and more preferably, between 0.5 wt% and 70% of the weight of the second layer. Other exemplary embodiments may have other filler contents, such as those described herein, or may be additionally required or beneficial to a particular conduit material or its intended use.

[0035] For example, a user may decide that the pipe may require further enhanced thermal stability. In this case, in addition to the thermal stability of the polymer described above, glass or fiber fillers can be added to the first or second layer to further improve the thermal stability of the pipe. Fillers can be added to the polymer material during compounding or extrusion processes and are typically mixed into the polymer in a homogeneous or non-homogeneous manner. Talc, chemicals, metals, other mineral fillers, or other organic or inorganic fillers can also be used alone or in combination with glass or fiber fillers to improve thermal stability (or other physical properties).

[0036] In another embodiment, the second layer may be 0.001 inches to 0.030 inches thick. More preferably, the second layer may be 0.008 inches to 0.025 inches thick, and even more preferably, the second layer may be 0.012 inches to 0.018 inches thick. However, the thicknesses of the first and second layers can vary to take into account the total thickness of the conduit, the specific type of conduit or its intended use, specific materials, or other considerations. For example, in another embodiment with a total thickness of 0.500 inches, the first layer may have a thickness of 0.100 inches to 0.480 inches, and the second layer may have a thickness of 0.020 inches to 0.400 inches. Additionally, the second layer may more preferably be composed of an acrylonitrile butadiene acrylate and a chlorinated polyvinyl chloride copolymer with fibrous glass filler.

[0037] Besides thermal stability, other fillers can be used alone or in combination with other fillers to achieve one or more other performance improvements. For example, if the pipeline requires improved electrical conductivity, aluminum powder, carbon fiber, or graphite can be used. If the pipeline requires improved structural strength, boron, carbon, carbon fiber, or Kevlar can be used. TM Or other fibrous materials. To improve fire resistance, the addition of chlorine, bromine, phosphorus, or metal salts may be useful. Other additives and properties can be modified by adding other materials not mentioned herein but generally known in the art.

[0038] The percentages of mixtures and combinations of different pipes may vary when the design requires it (e.g., the amount of thermal stability or other material properties required for the final application).

[0039] In one example, polyvinyl chloride (PVC) can be used as the first layer. A blend of acrylonitrile styrene acrylate, acrylonitrile butadiene acrylate (e.g., ABS), or a polycarbonate copolymer can be used as the second layer. The second layer may contain glass or other fillers in a homogeneous mixture with the aforementioned polymers. Furthermore, a third layer containing PVC can be added to the other side of the second layer. In an exemplary embodiment of a pipe having a total thickness of 0.060 inches, the first layer may be 0.001 inches to 0.050 inches thick. More preferably, in this example, the first layer may be 0.005 inches to 0.030 inches thick, and even more preferably, the first layer may be 0.015 inches to 0.025 inches thick. Other exemplary embodiments may have fewer or more layers, be composed of different materials, or have different thicknesses, such as taking into account a particular type of pipe or its use, specific materials, or other considerations.

[0040] In the above examples, polyvinyl chloride (PVC) can serve to smooth the surface and form a thin decorative cap. Other exemplary embodiments may utilize other materials or layers to achieve the desired surface (e.g., an aesthetically pleasing or durable surface).

[0041] For example, in another exemplary embodiment, the conduit may include a fourth layer. In an exemplary embodiment of a conduit with a total thickness of 0.060 inches, the fourth layer may be an ultraviolet (UV) light protection layer. The UV protection layer may be 0.001 inches to 0.010 inches thick. More preferably, the UV protection layer may be 0.003 inches to 0.008 inches thick, and even more preferably, the UV protection layer may be 0.004 inches to 0.006 inches thick. Similarly, other exemplary embodiments may have fewer or more layers, be made of different materials, or have different thicknesses, such as taking into account a particular type of conduit or its use, specific materials, or other considerations.

[0042] Any embodiment of the present invention may include any optional or preferred features of other embodiments of the invention. The exemplary embodiments disclosed herein are not intended to be exhaustive or unnecessarily limiting of the scope of the invention. Exemplary embodiments have been selected and described to explain some principles of the invention, enabling those skilled in the art to practice it. Having shown and described exemplary embodiments of the invention, those skilled in the art will recognize that many variations and modifications can be made to the invention. Many of these variations and modifications will provide the same results and fall within the spirit of the invention. Therefore, the invention is intended to be limited only to what is indicated by the scope of the claims.

Claims

1. A pipe, comprising an outermost layer and a second layer, wherein: The outermost layer is made of polyvinyl chloride material; The second layer is adjacent to and inside the outermost layer, and the second layer is selected from the group consisting of chlorinated polyvinyl chloride materials and polycarbonate materials; The outermost polyvinyl chloride material and the second layer of chlorinated polyvinyl chloride material or polycarbonate material were not foamed; The pipe is formed by extrusion and has a smooth outer surface; Compared to pipes of the same shape and size made solely of the polyvinyl chloride material, the pipes have improved thermal stability, making them more resistant to permanent energy changes caused solely by heat.

2. The pipe according to claim 1, wherein, The second layer of chlorinated polyvinyl chloride or polycarbonate material includes glass filler, the amount of which is up to 35 wt% of the second layer.

3. The pipe according to claim 2, wherein, The second layer of chlorinated polyvinyl chloride material or polycarbonate material includes the glass filler, the amount of which is between 9 wt% and 30 wt% of the second layer.

4. The pipe according to claim 1, wherein, Compared to pipes of the same shape and size made solely of the polyvinyl chloride material, the pipe has a lower coefficient of linear thermal expansion.

5. The pipe according to claim 1, wherein, Compared to pipes of the same shape and size made solely of the polyvinyl chloride material, the pipe has a smaller rate of thermal shrinkage.

6. The pipe according to claim 1, wherein, Compared to pipes of the same shape and size made solely of the polyvinyl chloride material, the pipe has a higher heat distortion temperature.

7. The pipe according to claim 1, wherein, Compared to pipes of the same shape and size made solely of the polyvinyl chloride material, the pipe has a smaller thermal shrinkage rate and a higher heat distortion temperature.

8. The pipe according to claim 1, wherein, Compared to pipes of the same shape and size made solely of the polyvinyl chloride material, the pipes have a lower coefficient of linear thermal expansion and a higher temperature of heat distortion.

9. The pipe according to claim 1, wherein, Compared to pipes of the same shape and size made solely of the polyvinyl chloride material, the pipe has a lower coefficient of linear thermal expansion and a smaller rate of thermal shrinkage.

10. The pipe according to claim 1, wherein, Compared to pipes of the same shape and size made solely of the polyvinyl chloride material, the pipes have a lower linear coefficient of thermal expansion, a smaller rate of thermal shrinkage, and a higher temperature of thermal distortion.

11. The pipe according to claim 1, wherein, The second layer is composed of the polycarbonate material.

12. The pipe according to claim 1, wherein, The second layer is composed of the chlorinated polyvinyl chloride material.

13. The pipe according to claim 11, wherein, The second layer of polycarbonate material contains glass filler, the content of which is up to 35% by weight of the second layer.

14. The pipe according to claim 13, wherein, The polycarbonate material of the second layer contains glass filler at a content of 9% to 30% of the weight of the second layer.

Citation Information

Patent Citations

  • Filled polycarbonate compositions with modified resilience

    CN101541873A

  • Fiber reinforced polyvinyl chloride and copolyester compositions and articles made using these compositions

    CN110997798A

  • Vinyl chloride resin pipe and method for constructing vinyl chloride resin pipe

    JP2021028507A

  • Double wall corrugated pipe having end protection ring

    KR101534600B1