A precision alloy resistor adjustment process
Through the rolling composite process and multi-row trench design, the problem of precision alloy resistors in the small packaging field is solved, and the packaging size customization and precision alloy resistor manufacturing with high power and low temperature drift are realized. Improves product performance and utilization.
Patent Information
- Application Number
- CN202311483681.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2023-11-08
- Publication Date
- 2024-11-22
- Estimated Expiration
- 2043-11-08
AI Technical Summary
The existing precision alloy resistance processing technology has problems such as packaging size limitations, low material utilization and high cost, which is difficult to achieve in the field of small packaging and the manufacturing of high-power and low-resistance products.
The composite plate is processed using the rolling composite process, designed a multi-row groove structure, filled with insulating medium and solidified, and the separation and resistance adjustment of multi-row resistance strips are achieved through machining and laser cutting, and combined with the application of electroplating layer, the packaging size is customized. and high material utilization.
It realizes precision alloy resistance manufacturing without the limitation of package size, improves material utilization and product power and surge resistance, and maintains stability in low temperature drift and high power scenarios.
Smart Images

Figure CN117393257B_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of precision alloy resistors, and in particular to a resistance adjustment process of precision alloy resistors. Background Art
[0002] Precision alloy resistors, also known as sampling resistors, shunts, etc., are mainly used to measure and monitor the current or voltage of the circuit in the feedback circuit to ensure the safe and stable operation of the circuit. They are mainly used in white goods, new energy, automotive electronics, industrial control, energy storage, electricity and other fields that require monitoring, measurement, and early warning of the safety and stability of the circuit.
[0003] At present, there are several types of precision alloy resistor processing:
[0004] 1. Use vacuum electron beam welding technology to achieve welding and compounding of copper pins and resistor alloys, and then use punching to achieve single particle production (such as Figure 1 As shown in the figure, the alloy resistor includes a resistor body 11 and copper electrodes 12 respectively welded to both ends of the resistor body 11, and a weld 13 is formed between the copper electrode 12 and the resistor body 11. However, this process can only be used for products with a package size greater than or equal to 1206, and is not applicable to products with a package size of 0805 and below, thereby limiting its application in the field of small packages. In addition, due to the need to consider the impact of the punching process edge, the material utilization rate is very low. The process route is generally strip alloy / strip copper welding, punching single grains, resistance value sorting, resistance adjustment, surface treatment, and packaging.
[0005] 2. Coat / print resistor paste on the ceramic substrate, then apply surface plastic sealing insulation glue or ink, and then electroplate on both sides to form conductive pins and electroplate pins, and then cut the ceramic to achieve single particle molding (such as Figure 2 As shown), this alloy resistor includes a ceramic substrate 21 and a resistor body 22, an insulating adhesive layer 23 is formed between the resistor body 22 and the ceramic substrate 21, and a protective solder mask 24 is coated on the other board surface of the resistor body 22. This process can expand the packaging of precision resistors to 0201 or even 01005, and the process can realize the simultaneous processing of multiple rows of products, reduce the proportion of process edges, and have a high material utilization rate. However, this process is suitable for processing ohms or greater resistance values, products with low power, cannot withstand large current shocks, and are difficult to achieve milliohm-level low resistance. The process route is generally ceramic processing, ceramic surface treatment, coating / printing slurry, coating surface insulation layer, electroplating pins, cutting single particles, resistance testing, and packaging.
[0006] 3. Another processing method that has been developed in recent years is to compound the copper pins and the resistance alloy together through the rolling composite process to make copper / resistance alloy or copper / resistance alloy / copper composite plates, and then use mechanical, chemical or electrochemical methods to remove the single-sided or double-sided copper, and then fill the gap with insulating glue or ink, and use stamping or CNC and other mechanical and laser cutting methods to achieve single-particle molding, and then electroplating nickel / electroplating the pins on both sides, and finally perform resistance testing and packaging (such as Figure 3 As shown). This alloy resistor includes a resistor body 31 and copper electrodes 32 located at both ends of the resistor body 31. Due to the good contact and conduction between the upper and lower copper and the resistor alloy, the resistance adjustment of multiple rows of products interferes with each other. Therefore, single-row processing, single-piece resistance adjustment or no resistance adjustment has been used for processing, resulting in low product yield, low material utilization and high cost. The process route is: copper / resistor alloy or copper / resistor alloy / copper composite molding, copper removal, gap filling with insulating medium, single-particle processing, electroplating pins, resistance value testing, and packaging. Summary of the invention
[0007] The purpose of the present invention is to overcome the deficiencies in the prior art and provide a precision alloy resistor adjustment process that is not limited by package size.
[0008] The objective of the present invention is achieved through the following technical solutions:
[0009] A precision alloy resistor adjustment process includes the following steps:
[0010] Obtaining a composite panel having two panels A and B disposed back to back;
[0011] A plurality of first grooves arranged in an interval manner are provided along the X-axis direction of the A panel;
[0012] Filling the insulating medium into the first grooves and solidifying the insulating medium;
[0013] A plurality of second grooves corresponding to the plurality of first grooves are formed along the X-axis direction of the B panel, wherein the depth of each of the second grooves reaches the insulating medium of the corresponding first groove, thereby obtaining a plurality of rows of resistor strips spaced apart from each other;
[0014] A plurality of third grooves arranged at intervals are provided along the Y-axis direction of the A panel, or a plurality of third grooves arranged at intervals are provided along the Y-axis direction of the B panel, or a plurality of third grooves arranged at intervals are provided along the Y-axis direction of the A panel and along the Y-axis direction of the B panel, so that a plurality of resistor monomers are formed on each row of the resistor strips;
[0015] Performing a resistance test on the resistor monomer;
[0016] Filling the insulating medium into the plurality of third grooves and solidifying the insulating medium;
[0017] The composite board is cut along the X-axis direction and the Y-axis direction to separate each resistor monomer therefrom.
[0018] In one embodiment, an insulating medium is filled into a plurality of the second grooves and solidified.
[0019] In one of the embodiments, the side surfaces of the resistor monomer are coated with an electroplating layer.
[0020] In one embodiment,
[0021] The composite plate comprises a resistance alloy layer and a copper layer bonded to each other, wherein the surface of the resistance alloy layer is panel A, and the surface of the copper layer is panel B;
[0022] A plurality of third grooves arranged at intervals from each other are formed along the Y-axis direction of the surface of the copper layer.
[0023] In one of the embodiments, an insulating medium is coated on the surface of the resistance alloy layer.
[0024] In one embodiment,
[0025] The composite plate comprises a resistance alloy layer and a copper layer bonded to each other, the surface of the copper layer is panel A, and the surface of the resistance alloy layer is panel B;
[0026] A plurality of third grooves arranged at intervals from each other are formed along the Y-axis direction of the surface of the copper layer.
[0027] In one of the embodiments, an insulating medium is coated on the surface of the resistance alloy layer.
[0028] In one embodiment,
[0029] The composite plate comprises a first copper layer, a resistance alloy layer, and a second copper layer which are laminated in sequence, wherein the surface of the first copper layer is panel A, and the surface of the second copper layer is panel B;
[0030] A plurality of the third grooves arranged at intervals from each other are opened along the Y-axis direction of the surface of the first copper layer, and a plurality of the third grooves arranged at intervals from each other are opened along the Y-axis direction of the surface of the second copper layer. BRIEF DESCRIPTION OF THE DRAWINGS
[0031] In order to more clearly illustrate the technical solutions of the embodiments of the present invention, the drawings required for use in the embodiments are briefly introduced below. It should be understood that the following drawings only show certain embodiments of the present invention and therefore should not be regarded as limiting the scope. For ordinary technicians in this field, other related drawings can be obtained based on these drawings without creative work.
[0032] Figure 1 It is a schematic diagram of the structure of the alloy resistor of Example 1 of the prior art;
[0033] Figure 2 It is a structural schematic diagram of an alloy resistor according to Example 2 of the prior art;
[0034] Figure 3 It is a schematic diagram of the structure of the alloy resistor of Example 3 of the prior art;
[0035] Figure 4 This is a schematic structural diagram of a composite coil according to Embodiment 1 of the present invention;
[0036] Figure 5 This is a schematic structural diagram of a composite coil according to a second embodiment of the present invention;
[0037] Figure 6 This is a three-dimensional structural diagram of a composite board of the present invention;
[0038] Figure 7 For Figure 6 A schematic diagram of a composite plate having a first groove formed on panel A shown;
[0039] Figure 8 for Figure 7 Cross-sectional view along AA direction;
[0040] Fig. 9 For Figure 8 A schematic diagram of filling a plurality of first trenches with an insulating medium based on the present invention;
[0041] Fig.10 For Figure 6 A schematic diagram of a second groove being provided on the B panel of the composite plate shown;
[0042] Fig.11 For Fig.10 A schematic diagram of filling a plurality of second trenches with an insulating medium based on the present invention;
[0043] Fig.12 A schematic diagram of preparing to open a third groove on the composite plate;
[0044] Fig.13 A schematic diagram showing a third groove having been opened on the composite plate;
[0045] Fig.14 for Fig.13 Cross-sectional view along direction BB;
[0046] Fig.15 A schematic diagram of opening a third groove on a composite board to obtain a plurality of resistor monomers;
[0047] Fig.16 For Fig.14 A schematic diagram of filling a plurality of third trenches with insulating medium based on the present invention;
[0048] Fig.17 A schematic diagram of cutting the composite plate along the X-axis direction and the Y-axis direction to obtain a single resistor monomer;
[0049] Fig.18 For Fig.17 Schematic diagram of the resistor monomer after electroplating based on the above;
[0050] Fig.19 The present invention is a flowchart of the steps of the precision alloy resistor adjustment process. DETAILED DESCRIPTION
[0051] In order to facilitate the understanding of the present invention, the present invention will be described more fully below with reference to the relevant drawings. The preferred embodiments of the present invention are given in the drawings. However, the present invention can be implemented in many different forms and is not limited to the embodiments described herein. On the contrary, the purpose of providing these embodiments is to make the disclosure of the present invention more thoroughly understood.
[0052] It should be noted that when an element is referred to as being "fixed to" another element, it may be directly on the other element or there may be a central element. When an element is considered to be "connected to" another element, it may be directly connected to the other element or there may be a central element at the same time. The terms "vertical", "horizontal", "left", "right" and similar expressions used herein are for illustrative purposes only and do not represent the only implementation method.
[0053] Unless otherwise defined, all technical and scientific terms used herein have the same meaning as those commonly understood by those skilled in the art of the present invention. The terms used herein in the specification of the present invention are only for the purpose of describing specific embodiments and are not intended to limit the present invention. The term "and / or" used herein includes any and all combinations of one or more related listed items.
[0054] The present invention discloses a precision alloy resistor adjustment process (please refer to Fig.19 ), comprising the following steps:
[0055] [Step 1: Using rolling technology to obtain an infinitely extended composite coil;]
[0056] The composite coil has the following two specifications: Figure 4 As shown, one composite coil 40 includes a resistance alloy layer 41 and a copper layer 42 bonded to each other. Figure 5 As shown, another composite coil 50 includes a first copper layer 51, a resistance alloy layer 52, and a second copper layer 53 which are sequentially attached, that is, copper is attached to both sides of the resistance alloy in the middle;
[0057] [Step 2: Obtain a composite board, which has two panels A and B arranged back to back (such as Figure 6 shown);]
[0058] According to the design requirements, the composite coil is cut to obtain the required length of the plate, and then the obtained plate is leveled by a leveling machine to ensure that the plate surface is flat without warping, bending, etc., so as to obtain the required composite plate (such as Figure 6 shown);
[0059] The composite board includes the following two forms: Figure 4 As shown, one of the composite plates includes a resistance alloy layer 41 and a copper layer 42 bonded to each other. Figure 5 As shown, another composite plate includes a first copper layer 51, a resistance alloy layer 52, and a second copper layer 53 which are sequentially attached, that is, copper is attached to both sides of the resistance alloy in the middle;
[0060] like Figure 6 As shown, since the composite board has the above two specifications, in order to express it more clearly and methodically, the two oppositely disposed board surfaces of the composite board are respectively referred to as panel A and panel B; in addition, for the convenience of expression, the concept of a plane rectangular coordinate system is introduced, and the plane rectangular coordinate system has an X-axis and a Y-axis perpendicular to each other, the X-axis is parallel to one side of the composite board, and the Y-axis is parallel to the other side of the composite board;
[0061] [Step 3: A plurality of first grooves 100 (such as Figure 7 as shown);]
[0062] According to the product packaging specification requirements, a plurality of first grooves 100 spaced apart from each other are opened along the X-axis direction of the A panel by machining (CNC, CNC machine tools, milling machines and other machining equipment), laser or etching processing technology. Generally, the depth of the first groove is required to be greater than 1 / 2 of the total thickness of the composite board. Of course, the depth of the first groove can also be freely selected according to actual conditions. In principle, the composite board cannot be cut through.
[0063] The spacing between the first grooves can be adjusted to any size and quantity, achieving ultra-high compatibility of package size, quantity and efficiency, and having effects that cannot be achieved by molds and other methods;
[0064] like Figure 8 As shown, a composite plate including a resistance alloy layer 41 and a copper layer 42 bonded to each other is used as an example. In this embodiment, the surface of the resistance alloy layer 41 is the A panel, and the first groove 100 is opened on the resistance alloy layer 41. Of course, in other embodiments, the surface of the copper layer 42 can also be the A panel, and the first groove 100 is opened on the copper layer 42. It can also be understood that no matter whether the first groove 100 is opened on the A panel first or the B panel first, the same effect can be obtained in the end.
[0065] [Step 4: Fill the insulating medium 60 into the first grooves 100 and solidify it;]
[0066] like Fig. 9 As shown, the insulating medium 60 (for example, epoxy resin material of the prior art) is filled into the first groove 100 by using a glue dispenser or glue injection process. The insulating medium is required to have sufficient bonding strength and rigidity, and solidify at room temperature or under heating and pressure conditions. It is usually required that the insulating medium fills the first groove and makes the insulating medium flush with the two side planes of the first groove at the same height;
[0067] [Step 5: A plurality of second grooves 200 (such as Fig.10 As shown in FIG. 1 ), the depth of each second groove reaches the insulating medium of the corresponding first groove, thereby obtaining multiple rows of resistor strips 70 spaced apart from each other (as shown in FIG. 1 ). Fig.12 as shown);]
[0068] In this step, it can be selected whether to fill the second trench with an insulating medium according to the actual situation, while filling the first trench with an insulating medium is necessary (e.g. Fig.10 As shown); due to the mutual penetration of the plurality of first grooves and the plurality of second grooves, multiple rows of mutually spaced resistor bars are obtained, and the insulating medium in the first grooves ensures that the multiple rows of mutually spaced resistor bars are not easy to shake after the mutual penetration, and the multiple rows of mutually spaced resistor bars form a stable connection through the insulating medium, which plays an important role in the stability of subsequent processing;
[0069] It should be noted that if it is necessary to fill the second groove with an insulating medium, the operation method is the same as the operation method for filling the first groove with an insulating medium, for example, a dispensing machine or a glue injection process is used to fill the second groove with an insulating medium 60 (such as Fig.11As shown), the insulating medium is required to have sufficient bonding strength and rigidity to solidify the insulating medium at room temperature or under heating and pressurizing conditions. It is usually required that the insulating medium fills the second groove and makes the insulating medium flush with the two side planes of the second groove at the same height;
[0070] This also confirms what has been said before, whether the first groove 100 is opened on the A panel first or the B panel first, the same effect can be obtained in the end, and the first groove and the second groove realize the mutual spacing of multiple rows of resistor strips.
[0071] [Step 6, a plurality of third grooves 300 are arranged at intervals along the Y-axis direction of the A panel, or a plurality of third grooves are arranged at intervals along the Y-axis direction of the B panel, or a plurality of third grooves are arranged at intervals along the Y-axis direction of the A panel and along the Y-axis direction of the B panel, so that a plurality of resistor monomers are formed on each row of resistor strips;]
[0072] like Fig.12 , Fig.13 and Fig.14 As shown, if the composite plate includes a resistance alloy layer 41 and a copper layer 42 bonded to each other, the surface of the resistance alloy layer 41 is the A panel, and the surface of the copper layer 42 is the B panel, then a plurality of the third grooves 300 spaced apart from each other are provided along the Y-axis direction of the surface of the copper layer 42; it should be particularly noted that in order to clearly understand how the third grooves 300 are provided, Fig.12 In particular, the third groove 300 is separated from the composite plate, so that by looking at the Fig.13 It is possible to more clearly and intuitively understand how the third groove 300 (shown by the thick line) is opened;
[0073] Similarly, if the composite plate includes a resistance alloy layer and a copper layer bonded to each other, the surface of the copper layer is the A panel, and the surface of the resistance alloy layer is the B panel, then a plurality of third grooves spaced apart from each other are provided along the Y-axis direction of the surface of the copper layer;
[0074] If the composite plate includes a first copper layer, a resistance alloy layer, and a second copper layer laminated in sequence, and the surface of the first copper layer is an A panel, and the surface of the second copper layer is a B panel, then a plurality of the third grooves arranged at intervals from each other are provided along the Y-axis direction of the surface of the first copper layer, and a plurality of the third grooves arranged at intervals from each other are provided along the Y-axis direction of the surface of the second copper layer;
[0075] It can be seen from this that no matter what specifications or forms the composite plate is in, the third groove is always opened on the copper layer.
[0076]
Step 7: Test the resistance of the resistor monomer;
[0077] After the third trench is formed, a plurality of resistor monomers 80 (such as Fig.15 The dashed box shows the range of the frame);
[0078] Use a resistance trimmer to test the resistance of the resistor monomer; according to the resistance requirements, use mechanical milling or laser stripping to remove the thickness of the resistor alloy to adjust the resistance from small to large, thereby improving the resistance qualification rate of the product;
[0079] [Step 8, filling a plurality of third grooves with an insulating medium and solidifying the insulating medium;]
[0080] The third groove is filled with an insulating medium 60 (such as Fig.16 As shown), the insulating medium is required to have sufficient bonding strength and rigidity, and then the insulating medium is solidified at room temperature or under heating and pressure conditions, and the insulating medium is required to be flush with the copper surfaces on both sides of the third groove or lower than the copper surfaces on both sides to form a solder resist surface;
[0081] [Step 9: If the composite plate includes a resistance alloy layer 41 and a copper layer 42 bonded to each other, an insulating medium 60 (such as Fig.16 As shown), to ensure surface insulation; it can be understood that if the composite plate includes a first copper layer, a resistance alloy layer, and a second copper layer laminated in sequence, it is not necessary to coat the surface of the resistance alloy layer with an insulating medium;]
[0082] [Step 10: Cut the composite board along the X-axis direction and the Y-axis direction to separate each resistor monomer 80 (such as Fig.15 and Fig.17 shown) separated therefrom;】
[0083] When the composite board is cut along the X-axis direction and the Y-axis direction, it is preferred to retain the insulating medium on the side of the resistor monomer (the insulating medium here refers to the medium filled in the first groove or the second groove), so as to achieve a better solder resistance effect;
[0084] [Step 11: electroplating the side of the single resistor monomer, such as copper plating, nickel plating and tin plating, so that the side of the resistor monomer is coated with an electroplating layer 90 (such as Fig.18 as shown);]
[0085] [Step 12: Test the resistance of a single resistor;]
[0086]
Step 13: Packaging.
[0087] Here, it should be noted that the order of the above steps 5 and 6 can be interchanged. For example, after the first groove is opened, the third groove is opened immediately, and after the third groove is opened, the second groove is opened. It can be seen that after the second groove is opened, multiple rows of resistor strips spaced from each other are obtained. Since the third groove has been opened, a number of resistor monomers are formed on each row of resistor strips, and then the resistance value test and subsequent operations are performed on the resistor monomers.
[0088] It should be noted that since the purpose of opening the first groove and the second groove is to form a number of resistor strips spaced apart from each other, the groove width of the first groove and the second groove should be as small as possible to improve the utilization rate of the material. The spacing distance between the first grooves (the spacing distance between the second grooves) needs to be able to accommodate a resistor monomer, that is, the distance between the first grooves or the second grooves needs to be adaptively adjusted according to the actual size of the resistor monomer. The groove width and depth of the third groove, as well as the spacing distance between the third grooves, are determined according to the package size of the product and the resistance value of the product.
[0089] The present invention adopts the process of rolling composite copper / resistance alloy or copper / resistance alloy / copper composite to process composite plates and strips, and then uses machining (CNC, numerical control machine tools, milling machines and other machining equipment) or etching processing technology for three times to realize groove design (first groove, second groove, third groove) on the front and back sides of the composite plate, and realizes multi-row structural layout for the product, realizes the design of the common process edge of the entire plate surface, and improves the utilization rate of materials; then fills the first groove with insulating medium (the second groove can freely choose whether to fill the insulating medium), realizes the disconnected layout of the multi-row resistors, and uses a resistance trimmer to perform resistance value test on the multi-row non-conductive whole board resistors one by one or row by row; according to the resistance value requirement, the resistance value is adjusted from small to large by mechanical milling or laser stripping to remove the thickness of the resistance alloy, so as to improve the resistance value qualification rate of the product; then, the insulating medium is coated on the surface of the resistance alloy; then, the single particle molding is realized by machining or laser cutting technology; then, the single product is plated with copper, nickel and tin, etc.; finally, the resistance value is tested and packaged.
[0090] This process can achieve customized design and processing of different packages (0201 / 0603 / 0805...) without being limited by the resistor package size, with high power (taking 0805 as an example, it can reach 1.5W, and 0402 can reach 1W), low temperature drift (can be controlled within ±50PPM / ℃, or even within ±10PPM / ℃), and excellent anti-surge performance. It can also ensure high power, anti-pulse performance and low temperature drift of the product on the basis of improving product utilization and yield.
[0091] The above-mentioned embodiments only express several implementation methods of the present invention, and the descriptions thereof are relatively specific and detailed, but they cannot be understood as limiting the scope of the invention patent. It should be pointed out that, for ordinary technicians in this field, several variations and improvements can be made without departing from the concept of the present invention, and these all belong to the protection scope of the present invention. Therefore, the protection scope of the patent of the present invention shall be subject to the attached claims.
Claims
1. A precision alloy resistor adjustment process, characterized in that: The steps include: A composite plate is obtained, wherein the composite plate has two face plates A and B arranged back to back; the composite plate includes a resistance alloy layer and a copper layer laminated to each other, or the composite plate includes a first copper layer, a resistance alloy layer, and a second copper layer laminated in sequence; A plurality of first grooves arranged in an interval manner are provided along the X-axis direction of the A panel; Filling the insulating medium into the first grooves and solidifying the insulating medium; A plurality of second grooves corresponding to the plurality of first grooves are formed along the X-axis direction of the B panel, wherein the depth of each of the second grooves reaches the insulating medium of the corresponding first groove, thereby obtaining a plurality of rows of resistor strips spaced apart from each other; A plurality of third grooves arranged at intervals are provided along the Y-axis direction of the A panel, or a plurality of third grooves arranged at intervals are provided along the Y-axis direction of the B panel, or a plurality of third grooves arranged at intervals are provided along the Y-axis direction of the A panel and along the Y-axis direction of the B panel, so that a plurality of resistor monomers are formed on each row of the resistor strips; Performing a resistance test on the resistor monomer; Filling the insulating medium into the plurality of third grooves and solidifying the insulating medium; The composite board is cut along the X-axis direction and the Y-axis direction to separate each resistor monomer therefrom.
2. The precision alloy resistor trimming process according to claim 1, characterized in that: An insulating medium is filled into the plurality of the second grooves and solidified.
3. The precision alloy resistor trimming process according to claim 1, characterized in that: The side surfaces of the resistor monomer are coated with an electroplating layer.
4. The precision alloy resistor trimming process according to claim 1, characterized in that: The composite plate comprises a resistance alloy layer and a copper layer bonded to each other, wherein the surface of the resistance alloy layer is panel A, and the surface of the copper layer is panel B; A plurality of third grooves arranged at intervals from each other are formed along the Y-axis direction of the surface of the copper layer.
5. The precision alloy resistor trimming process according to claim 4, characterized in that: An insulating medium is coated on the surface of the resistance alloy layer.
6. The precision alloy resistor trimming process according to claim 1, characterized in that: The composite plate comprises a resistance alloy layer and a copper layer bonded to each other, the surface of the copper layer is panel A, and the surface of the resistance alloy layer is panel B; A plurality of third grooves arranged at intervals from each other are formed along the Y-axis direction of the surface of the copper layer.
7. The precision alloy resistor trimming process according to claim 6, characterized in that: An insulating medium is coated on the surface of the resistance alloy layer.
8. The precision alloy resistor trimming process according to claim 1, characterized in that: The composite plate comprises a first copper layer, a resistance alloy layer, and a second copper layer which are laminated in sequence, wherein the surface of the first copper layer is panel A, and the surface of the second copper layer is panel B; A plurality of the third grooves arranged at intervals from each other are opened along the Y-axis direction of the surface of the first copper layer, and a plurality of the third grooves arranged at intervals from each other are opened along the Y-axis direction of the surface of the second copper layer.
Citation Information
Patent Citations
Precise electric current sensing resistor and manufacturing method thereof
CN106356168A
Low resistivity resistor and manufacturing process thereof
CN109346255A
Ultralow-resistance chip resistor and manufacturing method thereof
CN110706873A
Current sensing resistor and manufacturing method thereof
CN116741482A
Resistor, its mounting method, and its manufacture
JP2000114009A