Silicon carbide MOSFET devices and fabrication methods that eliminate the need for N+ source region photolithography
By using oxide spacer and contact pit etching processes, the high cost problem caused by photolithography in the fabrication of silicon carbide MOSFET devices was solved, and self-aligned etching of the N+ source region was achieved, reducing process costs.
Patent Information
- Application Number
- CN202410046605.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2024-01-12
- Publication Date
- 2026-11-17
- Estimated Expiration
- 2044-01-12
AI Technical Summary
In existing silicon carbide MOSFET device fabrication processes, the size of the N+ source region depends on photolithography, resulting in high process costs.
By employing oxide spacer and contact pit etching processes, the N+ source region photolithography process is eliminated. The etching width of the N+ source region is determined by selective etching of the oxide layer and the definition of the contact pits.
This effectively reduced process costs by eliminating the need for photolithography, thus enabling the fabrication of N+ source junctions.
Smart Images

Figure CN117832092B_ABST
Abstract
Description
Technical Field
[0001] This invention relates to the field of silicon carbide MOSFET device manufacturing technology, specifically to silicon carbide MOSFET devices and fabrication methods that eliminate the need for N+ source region photolithography. Background Technology
[0002] Silicon carbide (SiC) is a typical representative of third-generation wide-bandgap semiconductor materials. Its high critical breakdown electric field strength, high thermal conductivity, and high carrier saturation drift velocity make it an ideal material for fabricating high-power, radiation-resistant, high-temperature, and high-frequency devices. However, dopants of any kind are difficult to diffuse in silicon carbide. Therefore, for silicon carbide devices, multiple dopant implantations at different implantation energies are required to form a junction in the epitaxial layer of silicon carbide. This characteristic of silicon carbide makes it difficult to introduce self-aligned processes. Because the P-well junction is very deep, after P-well implantation, in existing processes, photolithography is usually required to etch away part of the N+ source region after N+ source region implantation, retaining the corresponding size of the N+ source region to form the N+ source junction (i.e., photolithography is needed to define the width of the etched N+ source region), which leads to high process costs. Summary of the Invention
[0003] The purpose of this invention is to address the problem that the size setting of the N+ source junction in existing processes relies on photolithography to define, resulting in high costs for the entire silicon carbide MOSFET device fabrication process. This invention provides a silicon carbide MOSFET device fabrication method that eliminates the need for photolithography of the N+ source region. Since this method eliminates the process of defining the etching width of the N+ source region after implantation using photolithography, it can effectively reduce process costs.
[0004] To solve the above problems, the present invention is achieved through the following technical solution: A method for fabricating silicon carbide MOSFET devices that eliminates the need for photolithography of the N+ source region is provided. The method includes the following steps: S1. Provide an N+ type silicon carbide substrate, and grow an N-type epitaxial layer on one side of the N+ type silicon carbide substrate; S2. A first oxide layer is deposited on the surface of the epitaxial layer; S3. Perform N-type doping implantation to form a JFET region in the epitaxial layer below the first oxide layer; S4. Perform polysilicon deposition to form a first polysilicon layer on the surface of the first oxide layer; S5. Perform photolithography to remove part of the first polysilicon layer and the first oxide layer, thereby forming several first channels; S6. Perform P-type doping implantation to form a P-well in the JFET region at the bottom of the first channel; S7. Continue depositing the oxide layer to form a second oxide layer covering the first polysilicon layer and the first channel; S8. Perform selective etching, retaining only a portion of the second oxide layer in the first trench and removing the rest; S9. Perform N-type doping implantation and annealing to form an N+ source region in the P-well region; S10, Remove all of the first polysilicon layer and the second oxide layer; S11. Perform photolithography and implantation to form a PSD region in the P-well region, and the PSD region is formed below the N+ source region. The PSD region is used to increase the breakdown voltage of the device. S12. The oxide layer and polysilicon are deposited sequentially to form a third oxide layer and a second polysilicon layer. The materials of the third oxide layer and the second polysilicon layer are the same as those of the first oxide layer and the first polysilicon layer, respectively. S13. Photolithography is performed on the second polysilicon layer to form a second channel that partially exposes the third oxide layer, specifically exposing the third oxide layer at the bottom of the second channel; S14. Continue to deposit an oxide layer to form a fourth oxide layer covering the second polysilicon layer and the second channel. The material of the fourth oxide layer is the same as that of the first oxide layer. S15. Photolithography removes a portion of the fourth oxide layer in the second channel to form a contact pit in the fourth oxide layer, thereby partially exposing the N+ source region. After the contact pit is formed by photolithography in this step, only a portion of the fourth oxide layer in the second channel is removed, but the fourth oxide layer still covers the second polysilicon layer. The bottom of the contact pit is in contact with the N+ source region. S16. Etch away the exposed N+ source region to expose the underlying PSD region, thereby forming an N+ source junction; S17. A source electrode is formed on the epitaxial layer, and a drain electrode is formed on the other side of the N+ type silicon carbide substrate, thus completing the fabrication of the silicon carbide MOSFET device.
[0005] Specifically, based on the characteristic that any kind of dopant is difficult to diffuse in silicon carbide materials, making it difficult to introduce self-alignment processes, the preparation method provided by the present invention can realize self-alignment processes after N+ source region implantation by using oxide (oxide layer) spacing processes and contact pit etching processes.
[0006] Furthermore, in step S1, an epitaxial layer of corresponding thickness is grown according to the voltage withstand requirement of the silicon carbide MOSFET device. The two are positively correlated, that is, the higher the voltage withstand requirement of the MOSFET device, the greater the thickness of the epitaxial layer.
[0007] Further, in step S5, polysilicon photolithography is performed to form gaps between the first polysilicon layer and the first oxide layer, thereby forming a plurality of first channels, the bottom of which is the JFET region.
[0008] Further, in step S6, P-type doping is performed at an angle perpendicular to the JFET region, thereby forming the P-well in the JFET region at the bottom of the first channel.
[0009] Further, in step S8, isotropic etching is performed to selectively etch the second oxide layer, retaining only a portion (the required portion) of the second oxide layer in the first channel, while removing the remainder. Specifically, after isotropic etching, the second oxide layer at the desired locations on the bottom and sidewalls of the first channel is retained.
[0010] Furthermore, in step S9, the annealing temperature is 850–900°C, and the annealing time is 90–120 minutes.
[0011] A silicon carbide MOSFET device that eliminates the need for N+ source region photolithography is fabricated using the above-described method.
[0012] The beneficial effects of this invention are: Because the P-well junction is relatively deep, in existing processes, after implanting the N+ source region in the P-well region, a photolithography process is usually required to define the etching width of the N+ source region. The portion of the N+ source region retained after photolithography is used to form the N+ source junction. This additional photolithography process for the N+ source region leads to higher process costs. To address this problem, this invention provides a new fabrication method. First, an oxide spacer process is used to define the implanted width of the N+ source region. Simultaneously, an oxide etching process is used to form contact pits of a certain width, and the width of these contact pits is used as the reference for the etching width of the N+ source region. By combining the oxide spacer process and the contact pit etching process, the photolithography process is replaced, thus enabling the fabrication of the N+ source junction without the need for the N+ source region photolithography process. The method of this application saves one photolithography process, which can effectively reduce process costs. Attached Figure Description
[0013] To more clearly illustrate the technical solutions of the embodiments of the present invention, the drawings used in the following description of the embodiments will be briefly introduced. Obviously, the drawings described below are only some embodiments of the present invention. For those skilled in the art, other drawings can be obtained based on these drawings without creative effort.
[0014] Figure 1 This is a schematic diagram of the structure after growing an epitaxial layer on an N+ type silicon carbide substrate in step S1 of Embodiment 1 of the present invention; Figure 2This is a schematic diagram of the structure after the first oxide layer is deposited on the epitaxial layer in step S2 of embodiment 1 of the present invention; Figure 3 This is a schematic diagram of the structure after the JFET region is formed in the epitaxial layer in step S3 of embodiment 1 of the present invention; Figure 4 This is a schematic diagram of the structure after the first polycrystalline silicon layer is deposited on the surface of the first oxide layer in step S4 of Embodiment 1 of the present invention; Figure 5 This is a schematic diagram of the structure of the first polysilicon layer and the first oxide layer after photolithography in step S5 of embodiment 1 of the present invention; Figure 6 This is a schematic diagram of the structure after P-well injection in step S6 of embodiment 1 of the present invention; Figure 7 This is a schematic diagram of the structure after the second oxide layer is deposited in step S7 of Embodiment 1 of the present invention; Figure 8 This is a schematic diagram of the structure after isotropic etching in step S8 of Embodiment 1 of the present invention; Figure 9 This is a schematic diagram of the structure after the N+ source region is formed in step S9 of embodiment 1 of the present invention; Figure 10 This is a schematic diagram of the structure after removing the first polysilicon layer and the second oxide layer in step S10 of Embodiment 1 of the present invention; Figure 11 This is a schematic diagram of the structure after the PSD region is formed in step S11 of Embodiment 1 of the present invention; Figure 12 This is a schematic diagram of the structure after the formation of the third oxide layer and the second polycrystalline silicon layer in step S12 of Embodiment 1 of the present invention; Figure 13 This is a schematic diagram of the structure formed after photolithography of the second polysilicon layer in step S13 of Embodiment 1 of the present invention; Figure 14 This is a schematic diagram of the structure formed in step S14 of Embodiment 1 of the present invention to form the fourth oxide layer; Figure 15 This is a schematic diagram of the contact pit formed after photolithography of the fourth oxide layer in step S15 of Embodiment 1 of the present invention; Figure 16 This is a schematic diagram of the structure of the N+ source junction formed after etching the N+ source region in step S16 of Embodiment 1 of the present invention.
[0015] The markings in the diagram are: 1-N+ type silicon carbide substrate, 2-epitaxy layer, 3-first oxide layer, 4-JFET region, 5-first polysilicon layer, 6-first channel, 7-P-well, 8-second oxide layer, 9-N+ source region, 10-PSD region, 11-third oxide layer, 12-second polysilicon layer, 13-second channel, 14-fourth oxide layer, 15-contact pit, 16-N+ source junction. Detailed Implementation
[0016] The technical solutions of the embodiments of the present invention will be clearly and completely described below with reference to the accompanying drawings. Obviously, the described embodiments are only some embodiments of the present invention, and not all embodiments. The following description of at least one exemplary embodiment is merely illustrative and is in no way intended to limit the present invention or its application or use. All other embodiments obtained by those skilled in the art based on the embodiments of the present invention without creative effort are within the scope of protection of the present invention.
[0017] In the description of this invention, it should be understood that the terms "upper," "lower," "left," "right," "top," and "bottom," etc., indicating orientation or positional relationships, are merely for the convenience of describing the invention and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific orientation, or be constructed and operated in a specific orientation, and therefore should not be construed as a limitation of the invention. Furthermore, the terms "first" and "second" are used for descriptive purposes only and should not be construed as indicating or implying relative importance or implicitly specifying the number of indicated technical features. Thus, a feature defined with "first" and "second" may explicitly or implicitly include one or more of that feature. Moreover, the terms "first," "second," etc., are used to distinguish similar objects and are not necessarily used to describe a specific order or sequence. It should be understood that such data can be interchanged where appropriate so that the embodiments of the invention described herein can be implemented in orders other than those illustrated or described herein. Example
[0018] A method for fabricating silicon carbide MOSFET devices that eliminates the need for N+ source region photolithography, the method comprising the following steps: S1. Provide an N+ type silicon carbide substrate 1, and grow an N-type epitaxial layer 2 on one side of the substrate, such as... Figure 1 As shown; Among them: the epitaxial layer of corresponding thickness is grown according to the voltage withstand requirement of the silicon carbide MOSFET device. The two are positively correlated, that is, the higher the voltage withstand requirement of the MOSFET device, the larger the thickness of the epitaxial layer 2 is set. S2. A first oxide layer 3 is deposited on the surface of the epitaxial layer 2 using a high-temperature furnace tube growth process, such as... Figure 2 As shown; the material of the first oxide layer 3 is silicon dioxide; S3. Perform N-type doping implantation to form a JFET region 4 in the epitaxial layer 2 below the first oxide layer 3, such as... Figure 3 As shown; S4. Perform polysilicon deposition to form a first polysilicon layer 5 on the surface of the first oxide layer 3, such as... Figure 4As shown; S5. Perform polysilicon photolithography etching to create gaps between the first polysilicon layer 5 and the first oxide layer 3, thereby forming a plurality of first channels 6. The bottom of the first channel 6 is the JFET region 4. Figure 5 As shown; S6. Perform P-type doping implantation at an angle perpendicular to the JFET region 4 to form a P-well 7 in the JFET region 4 at the bottom of the first channel 6, as shown. Figure 6 As shown; S7. Continue depositing the oxide layer to form a second oxide layer 8 covering the first polysilicon layer 5 and the first trench 6, such as... Figure 7 As shown; the material of the second oxide layer 8 is silicon dioxide; S8. Perform isotropic etching to selectively and directionally etch the second oxide layer 8, retaining only the required portion of the second oxide layer 8 in the first channel 6, and removing the rest. Wherein: the required portion of the second oxide layer 8 refers to: the second oxide layer 8 at the required positions on the bottom and sidewalls of the first channel 6, and the second oxide layer 8 at the positions corresponding to the original first oxide layer 3, such as Figure 8 As shown; S9. Perform N-type doping implantation and annealing to form an N+ source region 9 in the region of the P-well 7, such as... Figure 9 As shown; annealing temperature 850-900℃, time 90-120 minutes; S10, Remove all of the first polysilicon layer 5 and the second oxide layer 8, such as Figure 10 As shown; S11. Perform photolithography, implantation, and advancement to form a PSD region 10 in the P-well 7 region. The PSD region 10 is formed below the N+ source region 9. The width of the PSD region 10 is smaller than that of the N+ source region 9. The PSD region 10 is used to increase the breakdown voltage of the device, such as... Figure 11 As shown; S12, the oxide layer and polycrystalline silicon are deposited sequentially to form the third oxide layer 11 (made of silicon dioxide) and the second polycrystalline silicon layer 12, as follows. Figure 12 As shown; the third oxide layer 11 is also made of silicon dioxide; S13. Photolithography is performed on the second polysilicon layer 12 to form a second channel 13 that partially exposes the third oxide layer 11; specifically, the third oxide layer 11 at the bottom of the second channel 13 is exposed, such as... Figure 13 As shown; S14. Continue depositing the oxide layer to form a fourth oxide layer 14 covering the second polysilicon layer 12 and the second channel 13, such as... Figure 14 As shown; the fourth oxide layer 14 is also made of silicon dioxide; S15. Perform photolithography to remove a portion of the fourth oxide layer 14 in the second channel 13 to form a contact pit 15, thereby partially exposing the N+ source region 9 (i.e., the width of the contact pit 15 is smaller than the implantation width of the N+ source region 9), such as... Figure 15 As shown; After photolithography in step S15, only part of the fourth oxide layer 14 in the second channel 13 is removed, but the fourth oxide layer 14 still wraps the second polysilicon layer 12. The bottom of the formed contact pit 15 contacts the N+ source region 9, thereby exposing a part of the N+ source region 9. S16. The etching length of the N+ source region 9 is defined by the width of the contact pit 15, thereby etching away the exposed portion of the N+ source region 9 at the bottom of the contact pit 15. The etching width of the N+ source region does not need to be determined through photolithography; it can be determined solely by the width of the contact pit 15. After the N+ source region 9 is partially etched, the underlying PSD region 10 is exposed, thus forming the N+ source junction 16. Figure 16 As shown; S17. A source electrode is formed on the epitaxial layer 2, and a drain electrode is formed on the other side of the N+ type silicon carbide substrate 1, thus completing the fabrication of the silicon carbide MOSFET device.
[0019] In the typical fabrication process of silicon carbide MOSFET devices, multiple photolithography steps are performed, resulting in high photolithography costs. However, the method provided in this application can eliminate one photolithography process for the N+ source region. The method of this application does not require photolithography to determine the width of the N+ source region to be etched away. This application mainly achieves this by isotropically etching the deposited second oxide layer 8 immediately after deposition of the second oxide layer 8 in step S7. This ensures that a second oxide layer 8 of appropriate thickness is retained at the bottom and sidewalls of the first channel 6 after etching. At this time, the width inside the first channel 6 is related to the thickness of the second oxide layer 8 on its sidewalls. This allows the formation width of the N+ source region 9 to be controlled during the N-type doping implantation process in the subsequent step S9 (at this time, the width inside the first channel 6 is the formation width of the N+ source region 9). These retained second oxide layers 8 can then be used for self-aligned N+ source region 9 implantation. Meanwhile, in step 15 of this application, a contact pit 15 of a certain width (the contact pit 15 is smaller than the second channel 13) is formed in the second channel 13 by photolithography of the fourth oxide layer 14. The width of the contact pit 15 is used as the reference for the etching width of the N+ source region 9, and the excess N+ source region 9 in the middle is further etched away to form N+ source junctions 16 on both sides. Therefore, it can be seen that the method provided in this application fabricates the N+ source junction 16 without a photolithography process, that is, the method of this application can fabricate the N+ source junction 16 without the photolithography process of the N+ source region 9. Since the method of this application reduces one photolithography process, it can effectively reduce process costs.
[0020] The above-described preferred embodiments of the present invention are for illustrative purposes only and are not intended to limit the scope of the invention. Any obvious variations or modifications derived from the technical solutions of the present invention are still within the protection scope of the present invention.
Claims
1. A method for fabricating a silicon carbide MOSFET device that eliminates the need for N+ source region photolithography, characterized in that, The method includes the following steps: S1. Provide an N+ type silicon carbide substrate (1) and grow an N type epitaxial layer (2) on one side of the substrate. S2, deposit a first oxide layer (3) on the surface of the epitaxial layer (2); S3. Perform N-type doping implantation to form a JFET region (4) in the epitaxial layer (2) below the first oxide layer (3). S4. Perform polysilicon deposition to form a first polysilicon layer (5) on the surface of the first oxide layer (3); S5. Perform photolithography to form several first channels (6). S6. Perform P-type doping implantation to form a P-well (7) in the JFET region (4) at the bottom of the first channel (6). S7. Continue to deposit an oxide layer to form a second oxide layer (8) covering the first polysilicon layer (5) and the first trench (6). S8. Perform selective etching, retaining only a portion of the second oxide layer (8) in the first trench (6) and removing the rest; S9. Perform N-type doping implantation and annealing to form an N+ source region (9) in the P-well (7) region. S10, Remove all of the first polysilicon layer (5) and the second oxide layer (8); S11. Perform photolithography and implantation to form a PSD region (10) in the P-well (7) region, and the PSD region (10) is formed below the N+ source region (9); S12. The oxide layer and polysilicon are deposited sequentially to form the third oxide layer (11) and the second polysilicon layer (12). S13. Photolithography is performed on the second polysilicon layer (12) to form the second channel (13). S14. Continue the deposition of the oxide layer to form a fourth oxide layer (14) covering the second polysilicon layer (12) and the second channel (13). S15, Photolithography forms contact pits (15) to partially expose the N+ source region (9); S16. Etch away the exposed N+ source region (9) to expose the underlying PSD region (10), thereby forming an N+ source junction (16). S17. A source electrode is formed on the epitaxial layer (2), and a drain electrode is formed on the other side of the N+ type silicon carbide substrate (1) to complete the fabrication of the silicon carbide MOSFET device.
2. The method for fabricating a silicon carbide MOSFET device that eliminates the need for N+ source region photolithography according to claim 1, characterized in that, Step S1: Grow an epitaxial layer of appropriate thickness according to the voltage withstand requirements of the silicon carbide MOSFET device (2), and the two are positively correlated.
3. The method for fabricating a silicon carbide MOSFET device that eliminates the need for N+ source region photolithography according to claim 1, characterized in that, Step S5: Perform polysilicon photolithography etching to form gaps in the first polysilicon layer (5) and the first oxide layer (3), thereby forming a plurality of first channels (6), the bottom of the first channel (6) being the JFET region (4).
4. The method for fabricating a silicon carbide MOSFET device that eliminates the need for N+ source region photolithography according to claim 1, characterized in that, Step S6: Perform P-type doping implantation at an angle perpendicular to the JFET region (4) to form the P-well (7) in the JFET region (4) at the bottom of the first channel (6).
5. The method for fabricating a silicon carbide MOSFET device that eliminates the need for N+ source region photolithography according to claim 1, characterized in that, Step S8: Perform isotropic etching.
6. The method for fabricating a silicon carbide MOSFET device that eliminates the need for N+ source region photolithography according to claim 1, characterized in that, Step S9: Annealing temperature is 850-900℃, and annealing time is 90-120 minutes.
7. A silicon carbide MOSFET device that eliminates the need for N+ source region photolithography, characterized in that, It is prepared by the preparation method according to any one of claims 1 to 6.
Citation Information
Patent Citations
Method for manufacturing current monitoring unit integrated circuit based on JFET (Junction Field Effect Transistor) device
CN117198998A
Performance silicon carbide power devices
US11183566B1