A device and method for removing inclusions from molten steel in a tundish
By using a diversion blowing dish device in the tundish, using the guide cone and blowing tube structure to form small bubbles, entraining the inclusions to float, the problem of poor removal effect of small-sized inclusions in the existing technology is solved, and a high-efficiency, low-cost solution is achieved. Low-cost liquid steel purification, suitable for a variety of steel types.
Patent Information
- Application Number
- CN202311779247.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2023-12-22
- Publication Date
- 2024-10-22
- Estimated Expiration
- 2043-12-22
AI Technical Summary
The existing technology has limited effect in removing small-sized inclusions in molten steel, especially the purification effect of low-content molten steel. Moreover, the equipment is complex and the operation is difficult, and it cannot meet the high cleanliness requirements of most steel types, resulting in the use of The cost is high and not suitable for large-scale promotion.
Design a diversion blowing dish device in the tundish. Through the guide cone and blowing tube structure, argon gas is blown into the molten steel to form small bubbles, increase the number of bubbles, entrain inclusions to float up and integrate into the covering agent, achieving An efficient method for removing inclusions.
It improves the removal efficiency of inclusions, has a simple structure and is easy to maintain, and has low cost of use. It is suitable for various steel types, especially the purification of low-content molten steel, and reduces the inclusion content of steel.
Smart Images

Figure CN117862430B_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of metal refining in iron and steel metallurgy, and in particular to a device and method for removing inclusions in molten steel in a tundish. Background Art
[0002] The molten steel contains high melting point inclusions such as aluminum oxide, most of which are less than 50 microns in size. Such small inclusions are not easy to float. Although various methods are used in refining, the inclusion content in the molten steel is usually still high during pouring, which not only sometimes causes the blockage of the pouring nozzle, but more seriously, the inclusions seriously reduce the performance of the steel and even cause the steel to be scrapped. Especially for some steel types that have very strict requirements on the type and content of inclusions, it is very difficult to control the inclusions. Therefore, how to reduce the inclusion content in the molten steel to an ideal level has always been the main research content of metallurgical workers.
[0003] Currently, methods for removing non-metallic inclusions from molten steel in the continuous casting tundish are to use dams and weirs in the tundish, which have limited effectiveness, and thus more process methods for removing inclusions from molten steel in the tundish are needed.
[0004] The announcement number is CN1082618A, and the name of the invention patent is "Removal of inclusions in continuous casting molten steel by adsorption filtration". It is characterized by a method for removing non-metallic inclusions in molten steel by adsorption filtration in a continuous casting tundish. Fillers with chemical reaction activity are densely piled between two vertical retaining walls in the tundish to form a fixed bed of fillers. When the molten steel flows through, the inclusions therein are removed by the chemical and physical adsorption and mechanical barrier effect of the bed. This method is particularly suitable for purifying molten steel with large processing volume and high impurity content. The announcement number is CN2623382, and the name of the invention patent is "Metal Liquid Inclusion Cleaner", which includes a main body and an electromagnetic stirrer; the main body is divided into a first container and a second container by a partition wall, and a channel is provided therebetween to connect the two containers; the electromagnetic stirrer is arranged in a ring on the outer end side of the first container, and applies a tangential electromagnetic induction force to the metal liquid in the first container, so that the liquid metal rotates horizontally, and non-metallic inclusions will migrate to the middle of the melt, gather and grow, and be absorbed into the covering agent, and the rest will be adsorbed on the outer wall of the immersion discharge pipe and discharged as the discharge pipe is pulled out; the metal liquid after stirring and purification flows into the second container and finally flows into the crystallizer; it can basically remove large-sized non-metallic inclusions, such as deoxidation products with particles larger than 10μm, slag and refractory inclusions.
[0005] The shortcomings of the above patents are: "adsorption filtration method for removing inclusions in continuous casting molten steel" can only purify molten steel with a high impurity content to a limited extent, and cannot further purify molten steel with a low inclusion content. In addition, the filler is quickly heated to the temperature of the molten steel, and the ability to adsorb inclusions will be greatly reduced. In addition, the filler cannot be reused, resulting in high cost of use. The "metal liquid inclusion cleaner" can only remove deoxidation products, slag and refractory inclusions with particles larger than 50μm, and has the disadvantages of complex equipment, difficult operation and difficult implementation. Both are not suitable for steel grades with high cleanliness requirements, and most of the current steel grades require steel to have a low inclusion content. Therefore, both are not suitable for most steel grades and are not worth large-scale promotion. Summary of the invention
[0006] The purpose of the present invention is to provide a device and method for removing inclusions from molten steel in a tundish, which can conveniently and effectively remove inclusions from molten steel in a tundish.
[0007] To achieve the above object, the present invention is implemented through the following technical solutions:
[0008] A device for removing inclusions in molten steel in a tundish comprises a guide blowing dish, which has a cavity structure and is arranged below a long water outlet of the tundish. The bottom of the guide blowing dish is fixedly connected to the tundish, the top of the guide blowing dish is open, and the central axis of the long water outlet of the tundish coincides with the central axis of the guide blowing dish.
[0009] A guide cone is fixedly connected to the inner bottom of the guide blowing dish. The guide cone has a quadrangular pyramid structure. The central axis of the guide cone coincides with the central axis of the guide blowing dish. Blowing pipes are evenly distributed around the guide cone. The blowing pipes penetrate the guide cone and the tundish and are connected to the argon source.
[0010] The top angle of the guide cone is 30° to 170°, and the vertical height of the guide cone is 10 to 500 mm.
[0011] The external height of the guide blowing dish is 100-600 mm, the length is 200-900 mm, the width is 200-800 mm, the wall thickness of the guide blowing dish is 10-150 mm, and the length of the top opening of the guide blowing dish is 300-700 mm.
[0012] A method for removing inclusions from molten steel in a tundish, comprising the following steps:
[0013] S1, argon gas is blown in through the blowing pipe;
[0014] S2, continuous casting starts, the molten steel flows through the long nozzle of the tundish, and under the action of the guide cone, flows over the top of the blowing pipe;
[0015] S3. Under the impact of steel flow, bubbles are broken into small bubbles, which are dispersed in the molten steel to form a "molten steel bubble flow". Small bubbles float to the liquid surface with inclusions and merge into the covering agent. Bubbles aggregate in the covering agent to form large bubbles and are discharged;
[0016] S4. The purified molten steel flows out through the submerged water outlet of the tundish.
[0017] Compared with the prior art, the present invention has the following beneficial effects:
[0018] 1. The central axis of the long shroud of the tundish coincides with the central axis of the guide blowing dish. A guide cone is fixedly connected to the inner bottom of the guide blowing dish. The guide cone is a quadrangular pyramid structure. The central axis of the guide cone coincides with the central axis of the guide blowing dish, so that the injection flow through the long shroud of the tundish is guided to the surroundings and flows through the top of the blowing pipe;
[0019] 2. During the pouring process, under the action of the guide cone and the air blowing pipe, the bubbles are broken by the impact of the steel flow to form small bubbles dispersed in the molten steel. The number of bubbles increases several times, and the probability of contact with inclusions increases. The small bubbles float to the liquid surface with the inclusions and blend into the covering agent, which improves the removal of molten steel inclusions. The structure is simple, easy to maintain, and the use cost is low. BRIEF DESCRIPTION OF THE DRAWINGS
[0020] Figure 1 It is a schematic diagram of the structure of a device for removing inclusions from molten steel in a tundish.
[0021] Figure 2 It is a schematic diagram of the structure of the guide blowing dish.
[0022] In the figure: 1- flow guide blowing dish 2- blowing pipe 3- guide cone 4- air bubble 5- covering agent 6- long water nozzle 7- tundish 8- immersed water nozzle. DETAILED DESCRIPTION
[0023] The present invention is described in detail below in conjunction with the accompanying drawings, but it should be noted that the implementation of the present invention is not limited to the following embodiments.
[0024] A device for removing inclusions from molten steel in a tundish, comprising a guide blowing dish 1, Figure 1 ,See Figure 2The shape is a rectangular parallelepiped. The top opening of the guide blowing dish 1 is used to receive the injection flow. The guide blowing dish 1 is arranged below the long water inlet 6 of the tundish. The bottom of the guide blowing dish 1 is fixedly connected to the tundish 7. The top of the guide blowing dish 1 is open. The central axis of the long water inlet 6 of the tundish coincides with the central axis of the guide blowing dish 1. The inner bottom of the guide blowing dish 1 is fixedly connected with a guide cone 3. The guide cone 3 is a quadrangular pyramid structure. The central axis of the guide cone 3 coincides with the central axis of the guide blowing dish 1. The guide cone 3 and the guide blowing dish 1 The blowing pipe 2 is evenly arranged between the four walls, and the blowing pipe 2 passes through the guide cone 3 and the tundish 7. The external height of the guide blowing dish 1 is 100-600 mm, the external length is 200-900 mm, the external width is 200-800 mm, the wall thickness of the guide blowing dish 1 is 10-150 mm, and the length of the opening of the guide blowing dish 1 is 300-700 mm; the top angle of the guide cone 3 is 30°-170°, and the vertical height of the guide cone 3 is 10-500 mm.
[0025] A method for removing inclusions from molten steel in a tundish 7, specifically comprising the following steps:
[0026] S1, connect the argon gas source to the blowing pipe 2, and blow argon gas into the blowing pipe 2;
[0027] S2, continuous casting begins, the molten steel flows through the long shroud 6 of the tundish, and under the action of the guide cone 3, flows over the top of the blowing pipe 2;
[0028] S3, under the impact of steel flow, bubbles 4 are broken into small bubbles 4, which are dispersed in the molten steel to form a "molten steel bubble 4 flow". Small bubbles 4 float to the liquid surface with inclusions and merge into the covering agent 5. Bubbles 4 aggregate in the covering agent 5 to form large bubbles 4 and are discharged;
[0029] S4. The purified molten steel flows out through the submerged nozzle 8 of the tundish 7 and is continuously cast to obtain a continuously cast billet.
[0030] Working process:
[0031] The guide blowing dish 1 is built at the bottom of the tundish 7, and the blowing pipe 2 is connected to the argon gas source, and argon is blown in through the blowing pipe 2. During the pouring process, the injection flow from the long water nozzle 6 of the tundish flows through the top of the blowing pipe 2 under the action of the guide cone 3. The bubbles 4 are broken by the impact of the steel flow to form small bubbles 4 dispersed in the molten steel, forming a "molten steel bubble 4 flow". Because the number of bubbles 4 increases several times, the probability of contact with inclusions is greatly increased; the molten steel flowing out of the guide blowing dish 1 flows to the liquid surface, and these small bubbles 4 float to the liquid surface with the steel flow; the small bubbles 4 float to the liquid surface with the inclusions and melt into the covering agent 5, and the bubbles 4 aggregate in the covering agent 5 to form large bubbles 4 and are discharged.
[0032] The following examples are implemented on the premise of the technical solution of the present invention, and provide detailed implementation methods and specific operation processes, but the protection scope of the present invention is not limited to the following examples. The methods used in the following examples are conventional methods unless otherwise specified.
[0033] [Example 1]
[0034] The tundish 7 purification treatment of heavy rail steel U71Mn is as follows:
[0035] 1. Prepare a guide blowing dish 1, build it at the bottom of the tundish 7, and bake the tundish 7; the outer height of the guide blowing dish 1 is 300 mm, the outer length and width are both 700 mm, the wall thickness of the guide blowing dish 1 is 100 mm, and the side length of the opening of the guide blowing dish 1 is 380 mm; the cone top angle of the guide cone is 100°, and the height of the guide cone is 50 mm;
[0036] 2. Connect the blowing tube 2 to the argon gas source;
[0037] 3. When continuous casting starts, the injection flow from the long shroud 6 of the tundish flows through the top of the blowing pipe 2 under the action of the guide cone 3;
[0038] 4. Bubbles 4 are broken into small bubbles 4 under the impact of steel flow, which are dispersed in the molten steel. The small bubbles 4 float to the liquid surface with inclusions and merge into the covering agent 5. The bubbles 4 aggregate in the covering agent 5 to form large bubbles 4 and are discharged;
[0039] 5. The purified molten steel flows out of the tundish 7 and is continuously cast to obtain continuous casting billets.
[0040] It has been found that the total oxygen content, which indicates the purity of the ingot, is lower than that of the conventional casting method.
[0041] [Example 2]
[0042] The tundish 7 purification treatment of plain carbon steel Q235B is as follows:
[0043] 1. Prepare a guide blowing dish 1, build it at the bottom of the tundish 7, and bake the tundish 7; the outer height of the guide blowing dish 1 is 350 mm, the outer length and width are both 780 mm, the wall thickness of the guide blowing dish 1 is 90 mm, and the side length of the opening of the guide blowing dish 1 is 4000 mm; the cone vertex angle of the guide cone is 110°, and the cone height is 40 mm;
[0044] 2. Connect the blowing tube 2 to the argon gas source;
[0045] 3. When continuous casting starts, the injection flow from the long shroud 6 of the tundish flows through the top of the blowing pipe 2 under the action of the guide cone 3;
[0046] 4. Bubbles 4 are broken into small bubbles 4 under the impact of steel flow, which are dispersed in the molten steel. The small bubbles 4 float to the liquid surface with inclusions and merge into the covering agent 5. The bubbles 4 aggregate in the covering agent 5 to form large bubbles 4 and are discharged;
[0047] 5. The purified molten steel flows out of the tundish 7 and is continuously cast to obtain a continuous casting billet.
[0048] It has been found that the total oxygen content, which indicates the purity of the ingot, is lower than that of the conventional casting method.
[0049] The central axis of the long water nozzle of the tundish of the present invention coincides with the central axis of the flow-guiding blowing dish, the inner bottom of the flow-guiding blowing dish is fixedly connected with a guide cone, the guide cone is a quadrangular pyramid structure, the central axis of the guide cone coincides with the central axis of the flow-guiding blowing dish, so that the injection flow passing through the long water nozzle of the tundish is guided to the surroundings and flows over the top of the blowing pipe; during the pouring process, under the action of the guide cone and the blowing pipe, bubbles are broken under the impact of the steel flow to form small bubbles dispersed in the molten steel, the number of bubbles increases several times, the probability of contact with inclusions is increased, the small bubbles float to the liquid surface with the inclusions, and are dissolved in the covering agent, so as to improve the removal of molten steel inclusions, the structure is simple, easy to maintain, and the use cost is low.
Claims
1. A device for removing inclusions from molten steel in a tundish, characterized in that: The guide blowing plate comprises a flow-guiding and blowing plate, which is in a cavity structure, is arranged below the long water port of the tundish, and the bottom of the guide blowing plate is fixedly connected to the tundish, the top of the guide blowing plate is open, and the central axis of the long water port of the tundish coincides with the central axis of the guide blowing plate; The inner bottom of the guide blowing dish is fixedly connected with a guide cone, which is a quadrangular pyramid structure. The central axis of the guide cone coincides with the central axis of the guide blowing dish. Blowing pipes are evenly distributed around the guide cone. The blowing pipes penetrate the guide cone and the tundish, and are connected to the argon source. The top angle of the guide cone is 30° to 170°, and the vertical height of the guide cone is 10 to 500 mm; The method for removing inclusions from molten steel in a tundish by using the device specifically comprises the following steps: S1, argon gas is blown in through the blowing pipe; S2, continuous casting starts, the molten steel flows through the long nozzle of the tundish, and under the action of the guide cone, flows over the top of the blowing pipe; S3. Under the impact of steel flow, bubbles are broken into small bubbles, which are dispersed in the molten steel to form "molten steel bubble flow". Small bubbles float to the liquid surface with inclusions and merge into the covering agent. Bubbles aggregate in the covering agent to form large bubbles and are discharged; S4. The purified molten steel flows out through the submerged water outlet of the tundish.
2. The device for removing inclusions from molten steel in a tundish according to claim 1, characterized in that: The external height of the guide blowing dish is 100-600mm, the length is 200-900mm, the width is 200-800mm, the wall thickness of the guide blowing dish is 10-150mm, and the length of the top opening of the guide blowing dish is 300-700mm.