Operation method of hollow fiber membrane module

By controlling the flow rate and viscosity ratio of the stock solution to the filtrate in external pressure cross-flow filtration, combined with countercurrent cleaning and appropriate hollow silk membrane structure, the problem of pressure difference between the membrane caused by the difference in viscosity between the stock solution and the filtrate is solved, and the pressure difference between the membrane is achieved. Stable operation and low cleaning frequency of hollow silk film.

CN118019573BActive Publication Date: 2024-11-22TORAY INDUSTRIES INC
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202280065495.9
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Priority Date
2021-09-30
Filing Date
2022-09-29
Publication Date
2024-11-22
Estimated Expiration
2042-09-29

AI Technical Summary

Technical Problem

In the external pressure cross-flow filtration, the pressure difference between the membrane caused by the difference in viscosity between the stock solution and the filtrate becomes larger, resulting in the speed of occlusion of the hollow wire membrane and the increase in the cleaning frequency. The prior art has not effectively suppressed this problem.

Method used

By controlling the flow rate ratio of the stock solution to the filtrate to 0.02≤vp/vf≤0.3, and the ratio of the viscosity μf of the stock solution to the viscosity μp of the filtrate is ≥1.5 in the filtration process, combining the countercurrent cleaning process and an appropriate hollow silk film Structural design reduces the pressure difference between membranes and suppresses the occlusion speed.

Benefits of technology

It effectively suppresses the occlusion speed of the hollow silk film, reduces the cleaning frequency, ensures the stability of the filtrate flow rate and the reduction of filtration cost.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118019573B_ABST
    Figure CN118019573B_ABST
Patent Text Reader

Abstract

The operation method of the hollow fiber membrane module of the present invention includes a filtration step, wherein the filtration step is a step of performing cross-flow filtration by supplying a raw liquid to the outer surface side of the hollow fiber membrane. In the filtration step, the viscosity μ of the raw liquid is f The viscosity of the filtrate μ p The ratio is μ f / μ p ≥1.5, and the flow rate of the filtrate v p The flow rate v of the stock solution f The flow rate ratio is 0.02≤v p / v f ≤0.3.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to an operating method of a hollow fiber membrane module for filtration. Background Art

[0002] In recent years, membrane filtration using separation membranes has been expanding its application to various fields, including fermentation with the cultivation of microorganisms and cultured cells, medicine, and food and beverages, in addition to water treatment fields such as drinking water production, water purification, and wastewater treatment. Among separation membranes, membrane filtration using hollow fiber membrane modules is used in many fields because of its large water treatment volume and easy cleaning.

[0003] In the field of water treatment, relatively clear raw liquid is often filtered. In contrast, in the fields of fermentation, medicine, food and beverage, raw liquid with high turbidity and viscosity is often handled. In the case of high turbidity and high viscosity, if the full-volume filtration operation, which is more commonly used in the field of water treatment, is to be applied, the occlusion of the hollow fiber membrane and the so-called scaling will progress very quickly. Therefore, in these fields, cross-flow filtration operation is performed to reduce scaling. The so-called cross-flow filtration operation is a method of always making the raw liquid flow parallel to the surface of the hollow fiber membrane and filtering part of it.

[0004] In this method, due to the effect of the flow parallel to the surface of the hollow fiber membrane, it is possible to operate while preventing the accumulation of turbid matter on the surface of the hollow fiber membrane, so that scaling can be greatly reduced. As the application of separation membranes expands, the demand for technology that can stably operate a stock solution with high turbidity and viscosity through cross-flow filtration is increasing.

[0005] When a stock solution with high turbidity and viscosity is subjected to cross-flow filtration, either an external pressure type in which the stock solution is introduced to the outer surface side of the hollow fiber membrane or an internal pressure type in which the stock solution is introduced to the inner surface side of the hollow fiber membrane can be used. For example, Patent Documents 1 and 2 disclose a method of filtering a high viscosity liquid by internal pressure cross-flow filtration using an ultrafiltration membrane.

[0006] However, when filtering a stock solution with high turbidity and viscosity by internal pressure cross flow filtration, since the flow path size of the stock solution is smaller than that of the external pressure type, there is a situation where the flow path is blocked and the pressure loss caused by the flow of the stock solution increases. As a countermeasure, it is necessary to increase the inner diameter of the hollow fiber membrane. As a result, the membrane area of ​​the hollow fiber membrane module becomes smaller and the filtration amount of the hollow fiber membrane module decreases. Therefore, external pressure cross flow filtration is more suitable for such stock solutions.

[0007] Patent Document 3 discloses a method of applying external pressure cross flow filtration for oil-water separation, and Patent Document 4 discloses a method of applying external pressure cross flow filtration to a yeast culture solution. Patent Document 3 states that it is preferable to make the average size of the hollow fiber membranes larger in order to suppress clogging of the flow path in the external pressure cross flow filtration.

[0008] Prior art literature

[0009] Patent Literature

[0010] Patent Document 1: Japanese Patent Application Publication No. 2020-146645

[0011] Patent Document 2: Japanese Patent Application Laid-Open No. 10-42851

[0012] Patent Document 3: Japanese Patent Application Publication No. 2010-36183

[0013] Patent Document 4: International Publication No. 2017 / 209150 Summary of the invention

[0014] Problems to be solved by the invention

[0015] In the case of cross-flow filtration of a high-viscosity liquid under external pressure, a difference is generated between the viscosity of the raw liquid side and the viscosity of the filtrate side due to the thickening component being blocked by the separation membrane, and the difference between the membrane differential pressure on the raw liquid inlet side and the membrane differential pressure on the raw liquid outlet side of the hollow fiber membrane module (hereinafter referred to as the membrane differential pressure difference) becomes larger. As a result, the hollow fiber membrane on the raw liquid inlet side with a larger membrane differential pressure is blocked earlier, and the time until the upper limit of the membrane differential pressure of the entire hollow fiber membrane module is reached is shortened, resulting in the problem of increased cleaning frequency. Therefore, in the case where a viscosity difference occurs between the raw liquid side and the filtrate side, it is desired to reduce the membrane differential pressure difference to suppress the occlusion speed.

[0016] Patent document 1 discloses a method for suppressing the clogging of hollow fiber membranes caused by the increase in viscosity of the stock solution, returning the back pressure cleaning drainage to the stock solution, and thereby maintaining the filtration flow rate at a high level. Patent document 2 discloses a method for controlling the Reynolds number during circulation filtration in order to suppress the pore blockage of the hollow fiber and obtain a larger permeation flux. Patent document 3 describes that when an external pressure circulation type is set, the dirt on the membrane surface of the hollow fiber membrane can be peeled off by the flow of the treated liquid, and even if the non-water-soluble oil content and the concentration of suspended matter in the treated liquid are high, the filtration can continue while suppressing the dirt on the membrane surface and the pore blockage. Patent document 4 describes that when a yeast culture solution is subjected to external pressure cross-flow filtration, it is possible to operate without the breakage of the hollow fiber membrane by using a high-strength hollow fiber membrane.

[0017] However, no patent document discloses a method for reducing the differential pressure between membranes caused by the viscosity difference between the raw liquid and the filtrate. Therefore, the subject of the present invention is to provide a method for operating a hollow fiber membrane module that can reduce the differential pressure between membranes when a viscosity difference occurs between the raw liquid and the filtrate in external pressure cross-flow filtration, thereby suppressing the occlusion rate and reducing the cleaning frequency.

[0018] Means used to solve problems

[0019] In order to achieve the above-mentioned object, the present invention provides the following method for operating a hollow fiber membrane module.

[0020] <1> A method for operating a hollow fiber membrane module, characterized in that it includes a filtration step, wherein the filtration step is a step of cross-flow filtration by supplying a raw liquid to the outer surface side of the hollow fiber membrane, and in the filtration step, the viscosity of the raw liquid is μ f The viscosity of the filtrate μ p The ratio is μ f / μ p ≥1.5, and the flow rate of the filtrate v p The flow rate v of the stock solution f The flow rate ratio is 0.02≤v p / v f ≤0.3.

[0021] <2> like <1> The method for operating the hollow fiber membrane module is characterized in that, in the filtration step, the viscosity of the stock solution is μ f It is 3.0 mPa·s or more.

[0022] <3> like <1> or <2> The operating method of the hollow fiber membrane module is characterized in that, in the filtration step, the dissolved organic carbon concentration of the stock solution is greater than or equal to 1000 mg / L and less than or equal to 100000 mg / L.

[0023] <4> like <1> ~ <3> The method for operating a hollow fiber membrane module according to any one of the preceding claims is characterized in that the hollow fiber membrane is an ultrafiltration membrane.

[0024] <5> like <1> ~ <4> The operating method of any one of the hollow fiber membrane modules is characterized in that the load at break of the hollow fiber membrane is 500 gf / filament or more.

[0025] <6> like <1> ~ <5> The method for operating a hollow fiber membrane module according to any one of the preceding claims, wherein in the filtering step, the viscosity of the stock solution is μ f The flow rate v of the above stock solution f Satisfy v f ≤-0.135μ f +3.0 relationship.

[0026] <7> like <1> ~ <6> The method for operating a hollow fiber membrane module according to any one of the preceding claims is characterized in that the inner diameter D of the hollow fiber membrane is i 300μm≤D i ≤1000μm.

[0027] <8> like <1> ~ <7> The method for operating a hollow fiber membrane module according to any one of the preceding claims, wherein the filling rate of the hollow fiber membrane module is 25% to 45%.

[0028] <9> like <1> ~ <8> The method for operating a hollow fiber membrane module according to any one of the preceding claims, wherein the membrane length of the hollow fiber membrane is not less than 0.50 m and not more than 2.00 m.

[0029] <10> like <1> ~ <9> The method for operating a hollow fiber membrane module as described in any one of the preceding claims is characterized in that it further comprises a countercurrent cleaning step of causing a cleaning liquid to flow from the inner surface of the hollow fiber membrane toward the outer surface; the pore size of the outer surface of the hollow fiber membrane for The pore size of the inner surface of the hollow fiber membrane The aperture of the outer surface The ratio is

[0030] Effects of the Invention

[0031] According to the present invention, when a viscosity difference occurs between the raw liquid and the filtrate in external pressure cross flow filtration, the inter-membrane differential pressure difference can be reduced to suppress the blocking speed and reduce the cleaning frequency. BRIEF DESCRIPTION OF THE DRAWINGS

[0032] Figure 1 This is a schematic diagram showing one embodiment of the hollow fiber membrane module of the present invention.

[0033] Figure 2 This is a schematic flow chart showing one embodiment of a membrane filtration unit to which cross-flow filtration is applied.

[0034] Figure 3 This is a schematic diagram showing a model for simulating the pressure distribution in the hollow fiber membrane module.

[0035] Figure 4 This is a schematic flow chart showing one embodiment of viscosity measurement using a capillary viscometer.

[0036] Figure 5 This is a schematic flow chart showing one form of a membrane filtration unit used to verify the simulation. DETAILED DESCRIPTION

[0037] Below, while referring to the attached Figure 1 Although the embodiments of the present invention have been described in detail, the present invention is not limited to these embodiments.

[0038] Figure 1 1 is a schematic diagram showing one form of the hollow fiber membrane module of the present invention. In the following, in this specification, directions such as "up" and "down" are based on the states shown in the drawings for the sake of convenience. Figure 1 In the description, the filtrate outlet 3 side is set as the upper side and the stock solution inlet 2 side is set as the lower side.

[0039] The hollow fiber membrane module 10 of the present invention is filled with a hollow fiber membrane 5 in a container 1 having a stock solution inlet 2, a filtrate outlet 3, and a stock solution outlet 4. Both ends of the hollow fiber membrane 5 are embedded by a first potting portion 8 and a second potting portion 9, and the first potting portion 8 and the second potting portion 9 are fixed to the container 1. The lower end of the hollow fiber membrane 5 embedded by the first potting portion 8 is closed. In addition, the first potting portion 8 has a plurality of through holes for circulating the stock solution introduced from the stock solution inlet 2. On the other hand, the upper end of the hollow fiber membrane 5 embedded by the second potting portion 9 is embedded in an open state.

[0040] The stock liquid inlet 2, the filtrate outlet 3, and the stock liquid outlet 4 are cylindrical nozzles for connecting the container 1 to a pipe (not shown), and are fixed to the container 1, which is also cylindrical, in an open state. The stock liquid inlet 2 is connected to the lower end of the container 1, and the filtrate outlet 3 is connected to the upper end. The stock liquid outlet 4 is connected to the side of the container 1 and is provided near the second potting part 9. The raw materials thereof may be either resin or metal.

[0041] The hollow fiber membrane 5 filled in the container 1 is a hollow filamentary membrane having a liquid separation function. The hollow fiber membrane 5 is filled so that the axial direction of the container 1 is parallel to the axial direction of the hollow fiber membrane 5. The axial direction refers to the longitudinal direction of the container 1 and the longitudinal direction of the hollow fiber membrane 5.

[0042] The first potting part 8 and the second potting part 9 to which the plurality of hollow fiber membranes are fixed by adhesive are the parts where the gaps between the bundled hollow fibers are filled with so-called adhesive, i.e., a potting agent mainly composed of a potting resin. The potting part is preferably formed at the end of the hollow fiber membrane bundle.

[0043] The potting resin as the main component of the potting agent is preferably an epoxy resin, polyurethane resin or silicone resin having excellent adhesion to the hollow fiber membrane, heat resistance and chemical durability. In addition, the potting agent may also include additives such as silicon dioxide, talc, mica, clay, calcium carbonate, glass or rubber in addition to the potting resin.

[0044] The first potting portion 8 is formed at the end of the stock solution inlet side of the hollow fiber membrane 5. The end of the stock solution inlet side of the hollow fiber membrane 5 is preferably closed. By closing the end of the stock solution inlet side, the filtrate flowing in the hollow portion flows in one direction, and a pressure difference can be generated between the end of the stock solution inlet side and the end of the filtrate outlet side on the filtrate side of the hollow fiber membrane 5. Here, the so-called closing is a state in which the liquid flowing inside the hollow fiber membrane 5 is not led out from the closed end.

[0045] The first potting part 8 is fixed to the container 1, but has a plurality of through holes for circulating the stock solution introduced from the stock solution inlet 2, and the stock solution is introduced into the hollow fiber membrane 5 through the through holes. The shape and number of the through holes are not specified, and they are appropriately set according to the flow rate of the circulating stock solution to suppress the generation of resistance and flow unevenness.

[0046] The first potting part 8 only needs to be fixed in position so that the first potting part 8 does not float due to the flow of the stock solution, and may be bonded and fixed to the container 1 or made into a detachable cartridge structure. The method of position fixing is not particularly specified, and a structure for fixing the position between the container 1 and the first potting part 8, a structure for fixing the position between the second potting part 9 and the first potting part 8, etc. may be appropriately selected.

[0047] In addition, as long as the end of the stock solution inlet side of the hollow fiber membrane 5 is sealed, the first potting part 8 is not necessary, and it can also be a free end that is not fixed by a potting agent instead of a so-called fixed end in which the hollow fiber membrane bundle is fixed to each other with a potting agent. The so-called free end is a state in which the hollow fiber membranes are not fixed to each other with a potting agent and can move freely. In this case, as a method for sealing the end of the stock solution inlet side of the hollow fiber membrane 5, a method of injecting a potting agent into the hollow part of the hollow fiber membrane 5 and sealing it, a method of sealing the end by heat welding, etc. can be applied.

[0048] Next, the second potting portion 9 is formed at the end of the filtrate outlet side of the hollow fiber membrane 5 and fixed in a state where the end of the filtrate outlet side of the hollow fiber membrane 5 is opened. The so-called open state is a state where the liquid flowing inside the hollow fiber membrane is discharged from the open end.

[0049] The second potting part 9 is fixed to the container 1, but as long as the raw liquid and the filtrate can be separated liquid-tightly, the second potting part 9 and the container 1 can be bonded and fixed or made into a structure that allows the hollow fiber membrane to be detachable as in the so-called cylindrical type. In the case of the cylindrical type, the second potting part 9 and the container 1 can also be connected via an O-ring or the like.

[0050] In the hollow fiber membrane module having the above structure, the interior of the container 1 is separated by the hollow fiber membrane 5 and the second potting part 9 into a raw liquid side space 6 filled with raw liquid and a filtrate side space 7 filled with filtrate. The raw liquid side space 6 becomes the space in contact with the outer surface of the hollow fiber membrane 5, and the filtrate side space 7 becomes the space in contact with the inner surface of the hollow fiber membrane 5.

[0051] The present invention is applied to a so-called external pressure type hollow fiber membrane module in which the raw liquid inlet 2 and the raw liquid outlet 4 are connected to the raw liquid side space 6 and the filtrate outlet 3 is connected to the filtrate side space 7 .

[0052] Next, use Figure 2 For use Figure 1 The operation method of the hollow fiber membrane module shown is described below.

[0053] Figure 2 1 is a flow chart of a membrane filtration unit. The raw liquid is supplied from a raw liquid tank 12 to a container 1 by a supply pump 14. The raw liquid introduced into the container 1 from the raw liquid inlet 2 passes through Figure 1 The through-hole of the first potting part 8 shown is fed into the stock solution side space 6 in a flow parallel to the axial direction of the hollow fiber membrane 5 , and then is discharged from the container 1 through the stock solution outlet 4 .

[0054] Cross-flow filtration operation is an operation method that can prevent membrane-blocking components from the raw liquid from accumulating on the membrane surface by circulating at a flow rate of about 10 to 30 times the filtration flow rate, using the shear effect of the flow, and can perform stable filtration. It is an operation method that is particularly suitable for filtering raw liquid with a large amount of blocking components accumulated on the membrane surface.

[0055] In addition, the operation is often performed so that the filtrate flow rate observed by the filtrate flowmeter 32 becomes constant. In the cross-flow filtration operation, the difference between the average value of the raw liquid inlet pressure P1 and the raw liquid outlet pressure P2 observed by the raw liquid inlet pressure gauge 41 and the raw liquid outlet pressure gauge 42 and the filtrate outlet pressure P3 observed by the filtrate outlet pressure gauge 43 is called the average membrane differential pressure, and the operation is continued until the average membrane differential pressure reaches a specified pressure.

[0056] During the external pressure cross-flow filtration operation, the raw liquid flows in the raw liquid side space 6, and a high pressure loss is generated in the raw liquid side space 6. Therefore, a high raw liquid side pressure acts on the raw liquid inlet side end of the hollow fiber membrane 5, so the load of this part becomes higher. On the other hand, regarding the filtrate side space 7 inside the hollow fiber membrane, the filtrate also produces a pressure loss. Although the filtrate flows slower than the raw liquid, since the flow path of the filtrate side space 7 is smaller than that of the raw liquid side space 6, a relatively high pressure loss is also generated in the filtrate side space 7. As a result, there are the following characteristics: at the raw liquid inlet side end of the hollow fiber membrane 5, both the raw liquid side pressure and the filtrate side pressure become higher, thereby being able to suppress the increase of the differential pressure between the membranes.

[0057] However, when the viscosity of the stock solution and the filtrate is different, especially when the thickening component in the stock solution is retained by the separation membrane in the stock solution side space and the viscosity of the filtrate is smaller than that of the stock solution, the pressure loss in the filtrate side space 7 is smaller than the pressure loss in the stock solution side space 6. As a result, at the end of the stock solution inlet side of the hollow fiber membrane 5, the pressure on the stock solution side becomes higher and the pressure on the filtrate side becomes lower, and the differential pressure between the membranes at this part tends to increase. Therefore, at the end of the stock solution inlet side of the hollow fiber membrane 5, the excess liquid is filtered compared to the end of the filtrate outlet side, which becomes a major cause of promoting scaling.

[0058] We have conducted intensive research on this issue and found that in a hollow fiber membrane module performing external pressure cross-flow filtration, by controlling the flow rate on the raw liquid side and the flow rate on the filtrate side within a specified range, the axial pressure difference between the membranes of the hollow fiber membrane can be suppressed, thereby achieving the invention of the operation method of the hollow fiber membrane module.

[0059] That is, in the operation method of the hollow fiber membrane module of the present invention, when cross flow filtration is performed by supplying a raw liquid to the outer surface side of the hollow fiber membrane as a filtration step, the operation is performed so that when the viscosity μ of the raw liquid is f The viscosity of the filtrate μ p The ratio is μ f / μ p ≥1.5, the flow rate of the filtrate v p The flow rate v of the stock solution f The flow rate ratio becomes 0.02≤v p / v f ≤0.3.

[0060] If the viscosity of the stock solution is μ f The viscosity of the filtrate μ p Ratio (viscosity μ of stock solution f Relative to the viscosity of the filtrate μ p Ratio of)μ f / μ pWhen the flow velocity v of the filtrate is 1.5 or more, the pressure loss in the filtrate side space 7 becomes smaller than the pressure loss in the raw liquid side space 6. p The flow rate v of the stock solution f The flow rate ratio (the flow rate of the filtrate v p Flow rate v relative to the stock solution f The ratio of) is controlled to 0.02≤v p / v f ≤0.3, it is possible to ensure the required filtrate flow rate and suppress the filtration cost, and at the same time, make the pressure loss on the raw liquid side and the filtrate side uniform, and suppress the progress of scaling.

[0061] In more detail, by p / v f ≥0.02, even in μ f / μ p When v is 1.5 or more, the difference between the pressure loss on the raw liquid side and the pressure loss on the filtrate side can be reduced, and the increase in the differential pressure between the membranes can be suppressed. As a result, scaling can be suppressed. p / v f ≥0.02, the filtrate flow rate will not be excessively reduced, and the required filtrate flow rate can be ensured, so the number of membranes can be reduced and the filtration cost can be suppressed. p / v f ≤0.3, which can prevent the circulation flow rate of the raw liquid from becoming excessively small compared to the filtrate flow rate, so that the required raw liquid flow can be ensured to prevent the membrane clogging components from the raw liquid from accumulating on the membrane surface. As a result, the progression of scaling can be prevented. Preferably, 0.02≤v p / v f ≤0.2, more preferably 0.03≤v p / v f ≤0.15.

[0062] based on Figure 1 , Figure 2 The flow rate v of the stock solution f and the flow rate of the filtrate v p The flow rate v of the stock solution is f The concentrate flow rate Q measured by the concentrate flow meter 31 c Divide by the flow path area S of the raw liquid side space 6 of the hollow fiber membrane module 10 f The flow path area S of the raw liquid side space is calculated. f It is the value obtained by subtracting the total cross-sectional area of ​​the hollow fiber membrane 5 inserted in the container 1 from the cross-sectional area of ​​the container 1. If the inner diameter of the container 1 is D c , the outer diameter of the hollow fiber membrane 5 is set to D o, assuming that the number of hollow fiber membranes 5 is N, the following formula (1) is used for calculation.

[0063] [Formula 1]

[0064]

[0065] Filtrate flow rate v p The filtrate flow rate Q measured by the filtrate flow meter 32 p Divide by the flow path area S of the filtrate side space 7 p If the inner diameter of the hollow fiber membrane 5 is set to D i , then the flow path area S of the filtrate side space 7 is p Calculate using the following formula (2).

[0066] [Formula 2]

[0067]

[0068] About the flow rate v of the stock solution f , can also replace the concentrate flow Q c , and a supply liquid flow meter is set between the raw liquid inlet 2 and the supply pump 14, and the supply liquid flow rate Q measured is used f In this case, the flow rate v of the stock solution is calculated in the same way. f .

[0069] Viscosity of stock solution μ f and the viscosity of the filtrate μ p Since its value changes greatly depending on the temperature, it is preferable to measure the viscosity at the stock solution temperature measured by the stock solution temperature meter 51. Furthermore, since the viscosity may change due to shearing caused by the flow of the stock solution or the filtrate, it is preferable to measure the viscosity when the shearing rate γ caused by the flow during operation is applied.

[0070] The shear velocity γ depends on the flow velocity v and the flow path diameter D e The following formula (3) can be used to calculate the flow path diameter D of the filtrate side space 7: e The inner diameter D of the hollow fiber membrane 5 is i On the other hand, the flow path diameter D of the raw liquid side space 6 is e Due to the complex shape, the equivalent diameter calculated by the following formula (4) is used as the flow path diameter D e .

[0071] [Formula 3]

[0072]

[0073] [Formula 4]

[0074]

[0075] Regarding the viscosity measurement method, the viscosity measured by using a capillary viscometer at the same temperature and shear rate as in actual operation is used as the viscosity in the present invention. v Inner diameter of pipe D v , tube length L v The viscosity μ is measured by using the following formula (5) based on the inlet pressure P1 and outlet pressure P2 of the capillary tube. Using the above formula (3), the flow velocity v in the capillary tube is set v , so that the shear rate during actual operation is the same as the shear rate in the capillary viscometer, and the viscosity is measured.

[0076] [Formula 5]

[0077]

[0078] The capillary tube viscometer is not particularly limited as long as it can control the temperature of the tube and measure the pressure at the tube inlet and outlet, and any commercially available or homemade device may be used.

[0079] In addition, the viscosity may change as the operation continues, but it is preferred that the viscosity μ of the stock solution at least at the beginning of the operation is f The viscosity of the filtrate μ p The ratio is μ f / μ p ≥1.5. The so-called initial operation is the time when the stock solution is introduced into the new hollow fiber membrane module to start filtering, the time when the hollow fiber membrane module that is blocked during filtering is cleaned with the drug solution to restore the water permeability, and the stock solution is reintroduced to start filtering. In the case of a viscosity difference at the initial operation, in order to suppress the progress of hole clogging, it is preferred to operate so that the flow rate of the filtrate v p The flow rate v of the stock solution f The flow rate ratio becomes 0.02≤v p / v f ≤0.3.

[0080] In addition, it is preferred that the flow rate v of the stock solution is f 0.30m / s≤v f ≤1.80m / s. By v f ≥0.30m / s, can inhibit the accumulation of turbid matter on the surface of the hollow fiber membrane caused by the flow of the stock solution, and can inhibit the progress of scaling. f ≤1.80m / s, the pressure loss in the raw liquid side space 6 can be suppressed, so the raw liquid side pressure acting on the raw liquid inlet side end of the hollow fiber membrane 5 can be suppressed. As a result, the load on this part can be reduced, and as a result, the progress of scaling can be suppressed. The flow rate v of the raw liquidf Preferably 0.50m / s≤v f ≤1.50m / s, more preferably 0.70m / s≤v f ≤1.30m / s.

[0081] Filtrate flow rate v p Preferably 0.006m / s≤v p ≤0.30m / s. By v p ≥0.006m / s, the pressure loss in the filtrate side space 7 can be increased, and the pressure loss difference with the raw liquid side space 6 can be reduced. Furthermore, the filtration flux itself can also be increased, so the number of membrane modules required can be reduced. p ≤0.30m / s, which can prevent the pressure loss in the filtrate side space 7 from becoming excessively high and reduce the pressure loss difference with the raw liquid side space 6. Flow rate v of the filtrate p Preferably 0.01m / s≤v p ≤0.25m / s, more preferably 0.03m / s≤v p ≤0.20m / s.

[0082] During the entire period of cross-flow filtration operation of the stock solution using the hollow fiber membrane module, it is preferred to control the flow rate v of the filtrate. p The flow rate v of the stock solution f The flow rate ratio is 0.02≤v p / v f ≤0.3, but it is particularly preferred to control it within this range at the beginning of operation. As scaling progresses with continued operation, the axial inter-membrane pressure difference of the hollow fiber membrane 5 is relaxed. p The flow rate v of the stock solution f When the flow rate is outside the above range from the start of operation, the clogging will occur earlier and the relaxation speed will also be faster. Therefore, in order to suppress scaling, the flow rate of the filtrate v is controlled especially at the beginning of operation. p The flow rate v of the stock solution f The flow rate ratio becomes important.

[0083] The flow rate of the stock solution v f and the flow rate of the filtrate v p The flow rate v of the raw liquid can be controlled by adjusting the supply pump 14, the concentrate valve 21, and the filtrate valve 22. f It can be adjusted by the speed of the supply pump 14 and the concentrate valve 21. The flow rate v of the filtrate pAffected by the differential pressure between membranes and the flow rate of the raw liquid. Since the differential pressure between membranes is the pressure difference between the raw liquid side space 6 and the filtrate side space 7, it can be controlled by adjusting the speed of the supply pump 14, the opening of the concentrate valve 21, and the filtrate valve 22. By performing PID control (Proportional-Integral-Differential control) on the supply pump 14, the concentrate valve 21, and the filtrate valve 22, the raw liquid flow rate and the filtrate flow rate can be kept constant.

[0084] Next, the operation method of the hollow fiber membrane module of the present invention is preferably applied to the viscosity μ of the stock solution. f In the case of a clear filtrate, the viscosity of the filtrate is about 1.0 mPa·s, so in the stock solution of 3.0 mPa·s or more, a viscosity μ of the filtrate is generated. p On the other hand, if the viscosity of the stock solution is μ f If it is too high, the pressure loss in the liquid side space 6 will increase and the operation will become difficult, so it is better to apply to the liquid below 100.0 mPa·s. It is more preferably applied to the liquid below 30.0 mPa·s, and more preferably applied to the liquid below 10.0 mPa·s.

[0085] The stock solution to which the method for operating the hollow fiber membrane module of the present invention is applied is not particularly limited, and the viscosity μ of the stock solution that can be applied is f The viscosity of the filtrate μ p The ratio of μ f / μ p It is preferably used for various stock solutions with a DOC concentration of 1.5 or more, but preferably has a dissolved organic carbon (DOC) concentration of 1000 mg / L or more and 100,000 mg / L or less. When the DOC concentration is 1000 mg / L or more, the stock solution contains more thickening components and has a higher inhibitory effect on scaling by applying the operation method of the hollow fiber membrane module of the present invention. It is preferably used for stock solutions with a DOC concentration of 5000 mg / L or more, and more preferably used for stock solutions with a DOC concentration of 10,000 mg / L or more.

[0086] The DOC concentration is obtained by measuring the total organic carbon (TOC) concentration of the liquid after filtering the sample with a membrane filter with a pore size of 0.45 μm. The TOC concentration can be measured using the TC-IC method, which calculates the TOC concentration by subtracting the inorganic carbon (IC) from the total carbon (TC), or the NPOC method, which calculates the TOC concentration by adding an acid to the sample and aerating it, and measuring the total carbon of the aerated liquid. In the case where the stock solution contains more volatile organic carbon, it is preferred to use the TC-IC method for measurement.

[0087] In addition, as for the hollow fiber membrane 5 mounted in the hollow fiber membrane module of the present invention, as long as separation can be performed so that the viscosity of the stock solution is μ f The viscosity of the filtrate μ p The ratio of μ f / μ p It can be 1.5 or more without being particularly limited. It can be applied to various membranes such as precision filtration membrane, ultrafiltration membrane, nanofiltration membrane, reverse osmosis membrane, etc. from the larger pore size. However, in nanofiltration membrane and reverse osmosis membrane, the pressure loss when the stock solution passes through the membrane becomes extremely large compared with the pressure loss caused by the flow of the stock solution and the flow of the filtrate, and the influence of the pressure loss of the stock solution side space 6 and the filtrate side space 7 becomes small, so it is preferable to use precision filtration membrane and ultrafiltration membrane. In addition, since the thickening component that increases the viscosity of the stock solution is often a high molecular weight component dissolved in the stock solution, it is preferable to use an ultrafiltration membrane that can separate the dissolved high molecular weight component.

[0088] There are various definitions of precision filtration membrane and ultrafiltration membrane, but in the present invention, they are defined as follows. That is, a separation membrane having a pore size of 0.1 μm or more and 10 μm or less is defined as a precision filtration membrane, a separation membrane having a pore size smaller than 0.1 μm and a molecular weight cutoff of 1000 Da or more is defined as an ultrafiltration membrane, and a separation membrane having a molecular weight cutoff smaller than 1000 Da is defined as a nanofiltration membrane or a reverse osmosis membrane.

[0089] Next, the hollow fiber membrane 5 used in the present invention preferably has a strength (load at break) of 500 gf / filament or more. Figure 1 As shown, after the stock solution is introduced into the hollow fiber membrane module 10 from the stock solution introduction port 2 of the hollow fiber membrane module 10, it is discharged from the stock solution outlet 4, but the flow of the stock solution changes by 90 degrees when it is discharged from the stock solution outlet 4. Therefore, near the stock solution outlet 4, a shear force perpendicular to the length direction of the hollow fiber membrane 5 is applied to the hollow fiber membrane 5.

[0090] The present invention has found that the force passing through the hollow fiber membrane 5 is 500 gf / filament or more, and that fiber breakage, membrane damage, and the like can be suppressed against shearing caused by the cross-flow velocity assumed in the present application.

[0091] The so-called strength is the load (gf) applied when the hollow fiber membrane 5 is stretched in the axial direction by a tensile tester or the like and breaks. The measurement temperature at this time is the actual stock solution temperature during operation. The strength of the hollow fiber membrane 5 is preferably 600 gf / root or more, and more preferably 700 gf / root or more.

[0092] The method for measuring strength is not particularly limited. For example, the strength can be measured by using a tensile testing machine that can control the ambient gas temperature, stretching a sample with a measuring length of 50 mm at a tensile speed of 50 mm / min, changing the sample and performing the test more than 5 times, and calculating the average strength.

[0093] Furthermore, in the method for operating the hollow fiber membrane module of the present invention, it is preferred that the flow rate v of the stock solution is f Viscosity μ of the original solution f Satisfy v f ≤-0.135μ f +3.0. The flow rate of the stock solution v f The value calculated by formula 1 is in m / s. The viscosity of the stock solution is μ f It is the viscosity at the actual operating temperature, and the unit is mPa·s.

[0094] The flow rate v of the original solution is f ≤-0.135μ f +3.0 can prevent the shear force applied to the hollow fiber membrane 5 by the flow of the stock solution near the stock solution outlet 4 from increasing, and can reduce the risk of fiber breakage and membrane damage. f ≤-0.135μ f +2.5, preferably v f ≤-0.135μ f +2.3.

[0095] Regarding the size of the hollow fiber membrane 5 loaded in the hollow fiber membrane module 10, the outer diameter D o Preferably 600μm≤D o ≤2000μm. Pass D o ≤2000μm, the membrane area of ​​each hollow fiber membrane module will not be excessively reduced, and the filtrate flow rate of each module can be ensured. o ≥600 μm, the contact area between the stock solution and the hollow fiber membrane increases, thereby preventing the pressure loss in the stock solution side space from becoming excessively high. o Preferably 900μm≤D o ≤1800μm, more preferably 1000μm≤D o ≤1500μm.

[0096] The inner diameter D of the hollow fiber membrane 5 i Preferably 300μm≤D i ≤1000μm. Pass 300μm≤D i ≤1000 μm, the pressure loss of the filtrate side space 7 can be controlled within an appropriate range, and the inter-membrane pressure difference in the longitudinal direction of the hollow fiber membrane 5 can be reduced. Preferably, 400 μm≤D i≤900μm, more preferably 500μm≤D i ≤800μm.

[0097] About the outer diameter D of the hollow fiber membrane 5 o , inner diameter D i , the hollow fiber membrane 5 is cut with a single blade or the like with a surface perpendicular to the axial direction, and the cross section is observed with a microscope or the like to measure the diameter of the outer circle and the inner circle. When the outer circle or the inner circle is flat, the length of the longest diameter part (major diameter) and the length of the shortest diameter part (minor diameter) are measured, and the two are averaged to calculate. Preferably, the hollow fiber membrane 5 loaded into the hollow fiber membrane module 10 is arbitrarily cut, and the outer diameter and inner diameter of more than 10 hollow fiber membranes are averaged.

[0098] The filling rate M of the hollow fiber membrane 5 loaded into the hollow fiber membrane module 10 is preferably 25% ≤ M ≤ 45%. By setting it to 25% ≤ M ≤ 45%, the pressure loss on the raw liquid side can be controlled within an appropriate range while ensuring the membrane area of ​​each module. The filling rate M is preferably 28% ≤ M ≤ 42%, and more preferably 30% ≤ M ≤ 40%.

[0099] The filling rate M depends on the inner diameter D of the container 1 c , the outer diameter D of the hollow fiber membrane 5 o , the number N of hollow fiber membranes 5 is calculated using the following formula (6). When there is a component in the raw liquid side space 6 in addition to the hollow fiber membranes 5 in the container 1, the cross-sectional area of ​​the component perpendicular to the axial direction of the container 1 is calculated and added to the exclusive area S of the hollow fiber membranes 5. p Calculate in.

[0100] [Formula 6]

[0101]

[0102] The membrane length L is the length of the portion actually used for filtration when the hollow fiber membrane 5 is filled in the container 1, that is, the portion where the outer surface of the hollow fiber membrane 5 contacts the raw liquid in a direction parallel to the container 1. Figure 1 In the figure, the length of the hollow fiber membrane is the length from the second potting portion side end surface of the first potting portion 8 to the first potting portion side end surface of the second potting portion 9 in the hollow fiber membrane 5. The length of the hollow fiber membrane embedded in the first potting portion 8 and the second potting portion 9 is not considered here.

[0103] In the present invention, the membrane length L is preferably 0.50m≤L≤2.00m. By setting it to 0.50m≤L≤2.00m, it is possible to ensure the membrane area of ​​the hollow fiber membrane module while suppressing excessive increase in pressure loss in the raw liquid side space 6, thereby preventing the progression of scaling. The membrane length L is preferably 0.70m≤L≤1.50m, and more preferably 0.80m≤L≤1.20m.

[0104] In the case of a hollow fiber membrane module in which the hollow fiber membrane 5 is filled in a so-called U-shape and is embedded only by the second potting part 9 with both ends open, the membrane length L becomes half of the length of the hollow fiber membrane actually used for filtration, that is, half of the length of the part where the outer surface of the hollow fiber membrane contacts the raw liquid.

[0105] When there is no first potting section 8 and the end of the hollow fiber membrane 5 on the stock solution inlet side is a free end, the length is from the portion of the free end that has not been sealed with an adhesive or heat to the end surface of the second potting section 9 on the stock solution inlet side.

[0106] When the hollow fiber membrane 5 is curled or twisted, the membrane length L may be measured as the length of the portion of the hollow fiber membrane actually used for filtration, that is, the portion where the outer surface of the hollow fiber membrane contacts the raw liquid, in a direction parallel to the container 1 .

[0107] Next, the operation method of the hollow fiber membrane module of the present invention preferably further comprises a countercurrent washing step of causing the washing liquid to flow from the inner surface side to the outer surface side of the hollow fiber membrane in addition to the above-mentioned filtration step, and preferably, the surface pore size of the outer surface of the hollow fiber membrane is for The pore size of the inner surface of the hollow fiber membrane Surface aperture with outer surface The ratio is

[0108] Generally, during the filtration operation, components larger than the pores on the surface of the hollow fiber membrane are deposited on the surface of the hollow fiber membrane 5. In addition, components contained in the stock solution that are smaller than the pores on the surface of the hollow fiber membrane enter the pores. As a result, pores on the membrane surface and inside the membrane are clogged. In the external pressure cross flow filtration, the components deposited on the membrane surface are removed by the flow generated by the cross flow filtration operation.

[0109] In order to eliminate the clogging of the pores inside the membrane, it is preferred to perform a backflow cleaning process in which the cleaning liquid flows from the inner surface side to the outer surface side of the hollow fiber membrane. The backflow cleaning process is, for example, a process in which the cleaning liquid is circulated from the filtrate tank 13 to the filtrate side space 7 of the hollow fiber membrane module 10 using compressed gas, a pump, etc., and the cleaning liquid flowing out to the raw liquid side space 6 is discharged to the outside of the hollow fiber membrane module 10.

[0110] However, it is difficult to completely remove the components that have penetrated into the membrane by backflow cleaning alone. During long-term operation, the membrane pores become clogged and need to be cleaned with chemicals. Cleaning with chemicals can cause the strength of the membrane to deteriorate, which hinders the long-term use of the membrane.

[0111] Furthermore, when the viscosity of the filtrate becomes lower than that of the raw liquid as in the present invention, the pore-clogging components in the raw liquid are particularly retained by the hollow fiber membrane in the raw liquid side space and adhere to the membrane surface, whereby the pore-clogging components are mainly easily accumulated on the membrane surface and in the pores near the surface.

[0112] We have conducted intensive research on this issue and found that in a hollow fiber membrane module performing external pressure cross-flow filtration, by using a hollow fiber membrane in which the pore size of the outer surface of the hollow fiber membrane and the ratio of the pore size of the inner surface to the outer surface are controlled, the effect of backflow cleaning is particularly evident, and stable filtration can be performed for a long time.

[0113] The pore size of the outer surface of the hollow fiber membrane Preferably By While having a pore size that can ensure the required amount of filtrate, it can also prevent pore-clogging components from invading the interior of the membrane. More preferably Particularly preferred

[0114] The surface pore size in the present invention is obtained by the following method. Using the free software "ImageJ", the image of the outer surface and inner surface of the hollow fiber membrane observed by a scanning electron microscope (SEM) or a transmission electron microscope (TEM) is binarized. When binarization is performed, set it to 1 pixel in Subtract Background and perform Create Background, and then select the condition in Threshold: Renyi Entropy. In the obtained binary image, by selecting Area in Analyze Particles, the area of ​​each hole is obtained, and the diameter is calculated by assuming that each hole is a circle. The surface pore size is obtained by averaging the pore size of more than one hundred holes.

[0115] In addition, when the surface is uneven and difficult to pass through the binary screening hole, the surface pore size can also be obtained from the cross-sectional pore size described below. In this case, the cross-sectional pore size within a depth of 20 μm from the surface is set as the surface pore size.

[0116] In addition, the pore size of the inner surface of the hollow fiber membrane that contacts the filtrate is The surface in contact with the stock solution, i.e. the outer surface The ratio of the pore size (the pore size of the inner surface Relative to the outer surface ratio of the aperture) Preferably By The flow rate of the cleaning liquid near the membrane surface can be increased, and the cleaning effect near the surface can be particularly improved even in the stock solution where pore-clogging components are easily accumulated on the membrane surface and in the pores near the surface, and there is a viscosity difference between the stock solution and the filtrate. Particularly preferred also, The larger the value, the higher the cleaning recovery of the hollow fiber membrane by backflow cleaning becomes. Therefore, the upper limit is not particularly limited, but is, for example, 1000 or less, and preferably 700 or less.

[0117] The cleaning liquid used in the backflow cleaning process is preferably pure water, filtrate, or other liquid with a lower viscosity than the original liquid, which is easy to achieve the cleaning effect. The backflow cleaning process can be performed after the cross-flow filtration operation is stopped, and the frequency can be appropriately set according to the operating conditions.

[0118] The hollow fiber membrane 5 of the present invention may also be a single-layer hollow fiber membrane, but a composite hollow fiber membrane having two or more layers stacked together is easy to In this case, the transmittance coefficient Lp of the layer on the outer surface side is o and the permeability Lp of the inner surface layer i , preferably Lp i ≥Lp o . The permeability coefficient Lp is an indicator of the ease with which water passes through, and is expressed by the following formula (7), which means that the larger the permeability coefficient, the easier it is for water to pass through, and the smaller the permeability coefficient, the more difficult it is to pass through. Formula (7) is recorded, for example, in the Journal of Chemical Engineering of Japan (Vol. 15, No. 3 (1982) pp. 200-205). In the above-mentioned literature, the cross-sectional pore size is expressed not by diameter but by radius, and the porosity is expressed by opening ratio, but they are used in the same meaning. In addition, the pure water permeability performance K described later is also an indicator of the ease with which water passes through, but the pure water permeability performance K is calculated based on the measurement results of water permeability, while the permeability coefficient Lp is calculated based on the microscopic structure of the separation membrane. The permeability coefficient Lp is only used to compare the ease with which water passes through each layer.

[0119] [Formula 7]

[0120]

[0121] here, is the cross-sectional pore size (μm), A is the porosity (-), μ is the viscosity of water (Pa·s), and H is the thickness (μm).

[0122] Transmission coefficient Lp of the layer on the inner surface side i The transmittance coefficient Lp of the layer on the outer surface sideo When backflow cleaning is performed, the pressure loss of the cleaning liquid passing through the inner surface layer can be reduced, and the pressure acting on the outer surface layer where pore clogging components are easily accumulated can be increased, thereby improving the cleaning effect.

[0123] The cross-sectional pore size of the present invention can be obtained by the following method. The cross-sectional sample for observation is obtained by using a frozen ultrathin slicer to slice the porous membrane with a thickness of 100 nm at low temperature, and vacuum drying it at room temperature overnight. The cross-sectional area of ​​the hollow fiber membrane is observed with a scanning electron microscope (SEM) or a transmission electron microscope (TEM) to obtain images of each layer. If the structure of the layer is symmetrical in the direction of the membrane thickness, an image of the central part of the layer is obtained. If the structure of the layer is asymmetrical in the direction of the membrane thickness, an image of the area with the densest pore size is obtained. Then, the free software "ImageJ" is used for binarization. When binarization is performed, the condition "Minimum" is selected in Threshold (binarization threshold). In the obtained binary image, the area of ​​each hole is obtained by selecting Area in Analyze Particles (analyzed particles), and the diameter is calculated by assuming that each hole is a circle. The cross-sectional pore diameter is obtained by averaging the pore diameters of one hundred or more pores.

[0124] The porosity A can also be obtained from the above-mentioned binary image of the hollow fiber membrane cross section, and the porosity is calculated by dividing the total value of the calculated pore areas by the total area including the hollow fiber membrane in the observed image.

[0125] In addition, the permeability coefficient Lp in the present invention is calculated in the region with an interval of 10 μm in the film thickness direction, and the cross-sectional pore size and voids also use the values ​​calculated in the region with an interval of 10 μm. In addition, when the structure of each layer is symmetrical in the film thickness direction, the permeability coefficient Lp calculated in the region located at the center of each layer in the film thickness direction is set as the Lp of the layer; when the structure of each layer is asymmetrical in the film thickness direction, the permeability coefficient Lp calculated in the region with the densest cross-sectional pore size in the film thickness direction is set as the Lp of the layer.

[0126] In addition, the thickness H of the layer with a smaller permeability on the outer surface side is o , the thickness H of the layer with a larger permeability on the inner surface side i Preferably H o / H i ≤1.0. By H o / H i≤1.0, the pressure loss in the layer with a small permeability coefficient can be reduced. As a result, the pressure acting on the layer on the outer surface side where the pore-clogging components are likely to accumulate can be increased, and the cleaning effect becomes higher. o / H i If the value is too small, the separation function of the thickening component will be reduced, so it is preferably 0.04≤H o / H i ≤0.5, more preferably 0.1≤H o / H i ≤0.4.

[0127] As the layer on the outer surface side with a smaller pore size and a smaller permeability coefficient, a three-dimensional mesh structure layer that is easy to form fine holes is preferred. On the other hand, as the layer on the inner surface side with a larger pore size and a larger permeability coefficient, a spherical structure layer that is easy to form thick holes and has a higher strength is preferred. Therefore, as a composite hollow fiber membrane composed of two layers, it is preferred to set the spherical structure layer on the inner surface side and set the three-dimensional mesh structure layer on the outer surface side.

[0128] In a composite hollow fiber membrane having a spherical structure layer on the inner surface side and a three-dimensional mesh structure layer on the outer surface side, from the viewpoint of the above-mentioned cleaning effect and the blocking property of the thickening component, the thickness of the three-dimensional mesh structure layer is preferably 20 μm to 120 μm, and more preferably 30 μm to 80 μm. When the thickness of the three-dimensional mesh structure layer is less than 20 μm, there is a possibility that the blocking rate of the thickening component decreases. When it is thicker than 120 μm, the permeation resistance becomes too large, which may cause a decrease in the cleaning effect and a decrease in water permeability.

[0129] From the viewpoint of the above-mentioned cleaning effect, the strength of the hollow fiber membrane, and the water permeability, the thickness of the spherical structural layer is preferably 120 μm to 500 μm, and more preferably 200 μm to 300 μm.

[0130] The three-dimensional network structure layer may be formed by the liquid-liquid thermally induced phase separation method or the non-solvent induced phase separation method described below, and the spherical structure layer may be formed by the solid-liquid thermally induced phase separation method.

[0131] As the polymer of the material of the hollow fiber membrane 5, for example, polyethylene, ethylene-propylene copolymer, ethylene-ethyl acrylate copolymer, ethylene-vinyl acetate copolymer, ionomer, polypropylene or poly-4-methylpentene-1 and other olefin polymers, polytetrafluoroethylene, polytrifluorochloroethylene, polyvinylidene fluoride, tetrafluoroethylene-ethylene copolymer or tetrafluoroethylene-perfluoroalkyl vinyl ether copolymer and other fluorine-containing polymers, cellulose polymers such as cellulose acetate, polyvinyl chloride, acrylonitrile polymers, silicone polymers, polyamide, polyimide, polyethersulfone, polysulfone, polyphenylene ether, polyphenylene sulfide, polyarylate, polyetheretherketone, polyetherimide, polycarbonate or polyvinyl alcohol polymers can be cited. In order to improve the heat resistance, physical strength and chemical durability of the obtained hollow fiber membrane, fluororesin polymers, polyethersulfone or polysulfone are preferred, but in the hollow fiber membrane module for cross-flow filtration with a large load on the membrane, fluororesin polymers with excellent strength are preferred.

[0132] In addition, in order to reduce the scaling of the hollow fiber membrane 5, a hydrophilic polymer may also be included. Specifically, polymers including vinyl alcohol, ethylene glycol, vinyl pyrrolidone, methacrylic acid, allyl alcohol, cellulose, and vinyl acetate may be cited. Furthermore, as copolymer polymers containing hydrophilic groups, polyvinyl alcohol having a saponification degree of less than 99%, vinyl pyrrolidone-vinyl acetate copolymers, vinyl pyrrolidone-vinyl caprolactam copolymers, and vinyl pyrrolidone-vinyl alcohol copolymers may be cited.

[0133] Hereinafter, the method for producing the hollow fiber membrane module of the present invention will be described.

[0134] (Method for producing hollow fiber membrane)

[0135] Regarding the method for producing the hollow fiber membrane in the present invention, a method for producing the hollow fiber membrane using a fluororesin polymer is described as an example. As a method for producing the hollow fiber membrane using a fluororesin polymer, various methods such as a thermally induced phase separation method and a non-solvent induced phase separation method can be used. The following is a method for producing the hollow fiber membrane using the thermally induced phase separation method.

[0136] A fluororesin polymer solution (ie, a film-forming stock solution containing a fluororesin polymer) is prepared by dissolving the fluororesin polymer in a poor solvent or a good solvent for the fluororesin polymer at a relatively high temperature above the crystallization temperature.

[0137] If the polymer concentration in the membrane stock solution is high, a porous hollow fiber membrane with high strength can be obtained. On the other hand, if the polymer concentration is low, the porosity of the porous hollow fiber membrane becomes larger and the pure water permeability is improved. Therefore, the concentration of the fluororesin polymer is preferably 20% by weight or more and 60% by weight or less, and more preferably 30% by weight or more and 50% by weight or less.

[0138] In this specification, a poor solvent is a solvent that cannot dissolve fluororesin polymers by 5% or more at low temperatures below 60°C, but can dissolve fluororesin polymers by 5% or more at high temperatures above 60°C and below the melting point of the fluororesin polymer (for example, about 178°C when the polymer is composed of vinylidene fluoride homopolymer alone). A good solvent is a solvent that can dissolve fluororesin polymers by 5% or more at low temperatures below 60°C, and a non-solvent is defined as a solvent that neither dissolves nor swells the fluororesin polymer up to the melting point of the fluororesin polymer or the boiling point of the solvent.

[0139] Here, as the poor solvent of fluororesin polymer, cyclohexanone, isophorone, γ-butyrolactone, methyl isoamyl ketone, propylene carbonate, dimethyl sulfoxide, etc. and their mixed solvents can be enumerated. As the good solvent, N-methyl-2-pyrrolidone, dimethylacetamide, dimethylformamide, methyl ethyl ketone, acetone, tetrahydrofuran, tetramethylurea, trimethyl phosphate, etc. and their mixed solvents can be enumerated. As the non-solvent, water, hexane, pentane, benzene, toluene, methanol, ethanol, carbon tetrachloride, o-dichlorobenzene, trichloroethylene, ethylene glycol, diethylene glycol, triethylene glycol, propylene glycol, butanediol, pentanediol, hexanediol, aliphatic hydrocarbons such as polyethylene glycol of low molecular weight, aromatic hydrocarbons, aliphatic polyols, aromatic polyols, chlorinated hydrocarbons, or other chlorinated organic liquids and their mixed solvents can be enumerated.

[0140] In the process of forming the hollow fiber membrane, the hollow fiber membrane is obtained from the membrane-forming stock solution containing the fluororesin polymer by using the heat-induced phase separation method that induces phase separation by temperature change. In the heat-induced phase separation method, two phase separation mechanisms are mainly used. One is a liquid-liquid phase separation method in which a polymer solution that is uniformly dissolved at high temperature is separated into a polymer-rich phase and a polymer-diluted phase due to the decrease in the solubility of the solution when the temperature is lowered, and then the structure is fixed by crystallization. The other is a solid-liquid phase separation method in which a polymer solution that is uniformly dissolved at high temperature undergoes polymer crystallization when the temperature is lowered and phase-separates into a polymer solid phase and a solvent phase.

[0141] In the former method, a three-dimensional mesh structure is mainly formed, and in the latter method, a spherical structure composed of spherical tissue is mainly formed. There is no particular specification in the manufacture of the hollow fiber membrane of the present invention, but as a hollow fiber membrane for cross-flow filtration with required strength, it is preferred to utilize the latter phase separation mechanism. Thus, the polymer concentration and solvent that induce solid-liquid phase separation are selected.

[0142] As a specific method, the above-mentioned membrane-forming stock solution is ejected from the outer tube of a double-layer tubular spinneret (orifice) for spinning a porous hollow fiber membrane, and the hollow portion forming liquid is ejected from the inner tube of the double-layer tubular spinneret. The membrane-forming stock solution ejected in this way is cooled and solidified in a cooling bath to obtain a porous hollow fiber membrane.

[0143] Next, a cooling bath for cooling the fluororesin polymer solution ejected from the spinneret is described. In the cooling bath, it is preferred to use a mixed liquid consisting of a poor solvent or a good solvent with a concentration of 50 to 95% by weight and a non-solvent with a concentration of 5 to 50% by weight. Furthermore, as a poor solvent, it is preferred to use the same poor solvent as the polymer solution. In addition, in the hollow portion forming liquid, as in the cooling bath, it is preferred to use a mixed liquid consisting of a poor solvent or a good solvent with a concentration of 50 to 95% by weight and a non-solvent with a concentration of 5 to 50% by weight. Furthermore, as a poor solvent, it is preferred to use the same poor solvent as the polymer solution. The hollow fiber membrane composed of the fluororesin polymer obtained by the above method can also be stretched. The stretching ratio and the stretching temperature are appropriately selected according to the desired pore size, size, and pure water permeability.

[0144] In the case of obtaining a hollow fiber membrane filled in the hollow fiber membrane module of the present invention, the inner and outer diameters of the hollow fiber membrane can be mainly controlled by adjusting the spinneret diameter of the double-layer tubular spinneret, the ejection amount of the membrane stock solution and the hollow portion forming liquid. That is, a hollow fiber membrane with a larger inner and outer diameter is obtained by using a double-layer tubular spinneret with a larger diameter or increasing the ejection amount of the membrane stock solution and the hollow portion forming liquid. In addition, the size can also be adjusted by changing the stretching ratio and the stretching temperature.

[0145] As methods for obtaining a composite hollow fiber membrane, there are methods for forming multiple layers simultaneously and methods for sequentially forming other layers on a single-layer hollow fiber membrane. As the former, for example, there is a method of using a multilayer tubular spinneret to compositely mold multiple resin solutions. In addition, as the latter, for example, there is a method of applying a resin solution forming other layers to the hollow fiber membrane obtained after the above-mentioned process, scraping it off with a nozzle or a slit coater, or spraying the resin solution forming other layers. Among them, the method of applying the resin solution forming other layers and then scraping it off to form and solidify it is simpler and is preferred.

[0146] In the manufacture of the composite separation membrane using the above method, the resin solution forming the other layer is not particularly limited, but in the case of modifying and densifying the surface of the separation membrane, it is preferred to use a three-dimensional mesh structure. In the case of a composite separation membrane composed of a spherical structure and a three-dimensional mesh structure, a non-solvent induced phase separation method can be used to form a three-dimensional mesh structure. Here, the so-called non-solvent induced phase separation is a phase separation in which the resin solution is solidified by contacting it with a non-solvent.

[0147] In the case of using the non-solvent induced phase separation method, the solvent of the resin solution is preferably a good solvent for the resin. For example, as a good solvent for polyvinylidene fluoride resin, N-methyl-2-pyrrolidone, dimethylacetamide, dimethylformamide, methyl ethyl ketone, acetone, tetrahydrofuran and other lower alkyl ketones, esters, amides and mixed solvents thereof can be cited. Here, the so-called good solvent is a solvent that can dissolve 5% by weight or more of the polyvinylidene fluoride resin even at a low temperature of less than 60°C.

[0148] In addition, the non-solvent is defined as a solvent that neither dissolves nor swells the polyvinylidene fluoride resin up to the melting point of the polyvinylidene fluoride resin or the boiling point of the solvent. Here, examples of the non-solvent for the polyvinylidene fluoride resin include water, hexane, pentane, benzene, toluene, methanol, ethanol, carbon tetrachloride, o-dichlorobenzene, trichloroethylene, ethylene glycol, diethylene glycol, triethylene glycol, propylene glycol, butanediol, pentanediol, hexanediol, aliphatic hydrocarbons such as low molecular weight polyethylene glycol, aromatic hydrocarbons, aliphatic polyols, aromatic polyols, chlorinated hydrocarbons, or other chlorinated organic liquids and mixed solvents thereof.

[0149] (Manufacturing of hollow fiber membrane modules)

[0150] Hollow fiber membrane modules are classified into container-integrated modules in which container 1 and hollow fiber membranes 5 are fixed with adhesive, and cylindrical modules in which container 1 and hollow fiber membranes 5 are not fixed with adhesive and hollow fiber membranes 5 are detachable from container 1 .

[0151] In the container-integrated module, a plurality of hollow fiber membranes 5 are inserted into a container 1, and the ends of the hollow fiber membranes 5 and the container 1 are fixed with adhesive. In the cartridge module, the hollow fiber membranes are inserted into a dedicated jig or the like and the membranes are bonded to each other with adhesive, but not fixed to the container 1.

[0152] In either method, the hollow fiber membrane 5 is inserted into a fixture, a container, or both for fixing, and the adhesive is flowed in to fix. As a method for filling the gap between the hollow fiber membranes with the adhesive, for example, a centrifugal potting method in which the potting agent is infiltrated by centrifugal force, or a static potting method in which the adhesive is infiltrated by natural flow can be cited. In addition, the adhesive can also be injected into a mold for injection molding to fill the gap between the hollow fiber membranes.

[0153] In the case where the end of the hollow fiber membrane fixed with an adhesive is opened, the end of the hollow fiber membrane 5 is sealed in advance so that the adhesive does not flow into the hollow part of the hollow fiber membrane when the adhesive flows in, and fixed with the adhesive. As a sealing method, a method of injecting an adhesive only into the hollow part, welding by heat or solvent, etc. can be cited. After the hollow fiber membrane 5 with the sealed end is fixed with an adhesive, it can be opened by cutting the other end side closer to the sealed part in the cross-sectional direction of the hollow fiber membrane 5. If the end of the hollow fiber membrane is not sealed and fixed with an adhesive, the end is sealed because the adhesive flows into the hollow part of the hollow fiber membrane 5.

[0154] In the present invention, a method of fixing both ends of the hollow fiber membrane 5 with an adhesive may be adopted, but the end of the hollow fiber membrane 5 on the stock solution introduction port side may be a free end not fixed with an adhesive.

[0155] (Simulation of pressure distribution in hollow fiber membrane module)

[0156] In order to verify the effect of the method for operating the hollow fiber membrane module of the present invention, the pressure distribution in the hollow fiber membrane module was simulated to study the range that could not be studied by experiments.

[0157] exist Figure 3 The model outline used for the simulation is shown in Figure 3 (a) shows one hollow fiber membrane 5 and the flow of the raw liquid and the filtrate. Figure 3 In the figure, the raw liquid is represented by a shaded arrow, and the filtrate is represented by a hollow arrow. The end of the raw liquid inlet side of the hollow fiber membrane 5 is set to n=0, and the position of the end of the filtrate outlet side is set to n=k. The end of the raw liquid inlet side of the hollow fiber membrane 5 is closed, and the end of the filtrate outlet side is open, and the filtrate is completely discharged from the end of the filtrate outlet side. Here, Figure 3 (b) shows the flow of liquid in micro-segment n when the hollow fiber membrane 5 is meshed every Δl in the axial direction. n is an integer greater than 0, and k is a natural number greater than 1. In micro-segment n, the filtrate derived from micro-segment n-1 merges with the filtrate filtered by the membrane in micro-segment n. As a result, the filtrate flow rate Q derived from micro-segment n is i,n , if the amount of filtrate derived from the small interval n-1 is set to Q i,n-1 , the amount of filtrate after membrane filtration in the small interval n is set as Q p,n , then it becomes the following formula (8). In addition, there is no Q i,-1 , for Q i,0 =Q p,0 k is preferably 50 or more, and more preferably 100 or more. In addition, the membrane length from the end of the stock solution inlet to the micro-interval n is set to ln . is l0=0, is l k =L.

[0158] [Formula 8]

[0159] Q i,n =Q i,n-1 +Q p,n …(8)

[0160] The filtrate flow rate Q in the small interval n p,n , according to the raw liquid side pressure P in the small interval n o,n and the filtrate side pressure P i,n , membrane area A n 、Membrane filtration resistance R n and the viscosity μ of the filtrate at the filtration temperature p , calculated using the following formulas (9) to (11). n Based on the filtration flux J (= permeation (m 3 ) / filtration time (hr) / effective membrane area (m 2 ))、Differential pressure between membranes ΔP m The viscosity μ is calculated assuming that the viscosity μ is the same in the axial direction of the hollow fiber membrane 5 at the beginning of filtration.

[0161] [Formula 9]

[0162]

[0163] [Formula 10]

[0164] A n =πD0Δl…(10)

[0165] [Formula 11]

[0166]

[0167] Regarding the pressure P of the raw liquid in the small interval n o,n , considering the original liquid introduction pressure P o,0 And the pressure loss ΔP0×l generated by the raw liquid flow n , calculated using the following formula (12). In fact, since part of the raw liquid is filtered by the membrane, the circulation flow rate changes in the axial direction of the hollow fiber membrane 5, but since the filtered flow rate is small relative to the circulation flow rate, it can be ignored. Therefore, in this model, the pressure loss per unit length of the axial direction generated by the raw liquid flow is ΔP o It is calculated to be constant regardless of the position.

[0168] [Formula 12]

[0169] Po,n =P o,0 -ΔP o l n …(12)

[0170] Pressure loss per unit length ΔP o , according to the equivalent diameter D of the raw liquid side space 6 e 、The viscosity of the stock solution μ f , use the following formulas (13) to (14) to calculate the pressure loss ΔP o In addition, ρ is the stock solution density, D c is the diameter of the inner circle of the container 1, and τ is the shape correction coefficient of the flow path on the raw liquid side.

[0171] [Formula 13]

[0172]

[0173] [Formula 14]

[0174]

[0175] The filtrate side pressure P in the small interval n i,n , calculated from the pressure loss when the filtrate flows inside the hollow fiber membrane 5. Here, the Reynolds number Re of the filtrate flowing inside the hollow fiber membrane 5 is calculated. i,n Calculate the pressure loss from the small interval n to the end of the filtrate outlet side by integrating it. p,n is the flow rate of the filtrate in the micro-interval n. Here, the calculation method is represented by the following equations (15) and (16) when the flow flowing inside is assumed to be a laminar flow.

[0176] [Formula 15]

[0177]

[0178] [Formula 16]

[0179]

[0180] Here, for convenience, let P i,k =0, by adjusting P o,0 The filtrate flow rate Q obtained by the hollow fiber membrane 5 is i,k The pressure distribution on the raw liquid side and the filtrate side of the hollow fiber membrane 5 is calculated by satisfying the following formula (17). t Indicates the set filtering flux.

[0181] [Formula 17]

[0182]

[0183] According to the pressure distribution calculated in this way, the raw liquid side pressure P in the small interval n o,n With P i,n The difference is the membrane pressure difference ΔP in this interval m,n In the method for operating the hollow fiber membrane module of the present invention, the inter-membrane pressure difference in the axial direction of the hollow fiber membrane 5, ΔP m,k -ΔP m,0 It is preferably 50 kPa or less.

[0184] Example

[0185] The present invention will be described below with reference to specific examples, but the present invention is not limited to these examples. In addition, various parameters related to the present invention were measured using the above-mentioned methods.

[0186] (Measurement of pure water permeability)

[0187] A small module consisting of three hollow fiber membranes with a membrane length of 0.1 m was made, and the pure water permeability K was measured. Under the conditions of temperature 25°C and filtration differential pressure 16 kPa, the reverse osmosis membrane filtered water was filtered under external pressure for 10 minutes, and the permeation rate (m 3 ). By taking the permeation amount (m 3 ) is converted to per unit time (h) and effective membrane area (m 2 ) is multiplied by (50 / 16) times to convert it to a value at a pressure of 50 kPa, thereby obtaining the pure water permeability K. In the present invention, the effective membrane area is the area of ​​the portion of the outer surface of the hollow fiber membrane 5 that is used for filtration during implementation.

[0188] (Strong measurement)

[0189] The strength was tested five or more times using a tensile tester (TENSILON (registered trademark) / RTM-100, manufactured by Toyo Baldwin Co., Ltd.) with a measuring length of 50 mm in an atmosphere of 25°C at a tensile speed of 50 mm / min, and the average value was calculated.

[0190] (Viscosity measurement)

[0191] use Figure 4 The viscosity is measured by the device shown. The stock liquid tank 12 and the capillary tube 16 are set in the constant temperature water tank 15 and connected with a fluorine tube so that the stock liquid can be sent to and returned to the capillary tube 16. The capillary tube 16 uses a fluorine tube with an inner diameter of 2.0 mm and a tube length of 1.0 m. The tube inlet pressure gauge 45 and the tube outlet pressure gauge 46 are connected to both ends of the capillary tube. Water is filled in the constant temperature water tank 15 to adjust the temperature of the stock liquid to the same temperature as that during actual operation.

[0192] Then, according to the flow path diameter D of the hollow fiber membrane module used in actual operation e The shear rate is calculated by the flow rate v and the flow rate v of the stock solution fed into the capillary tube. v , so as to achieve a shear velocity equal to the actual module shear velocity γ. v The stock solution is fed in, and the viscosity is calculated using equation (5) based on the measured tube inlet pressure P1 and tube outlet pressure P2.

[0193] (Aperture measurement)

[0194] After the hollow fiber membrane was vacuum dried at 25°C overnight, it was observed using SEM (S-5500, manufactured by Hitachi High-Technologies Co., Ltd.) at a magnification of 30,000 to 100,000 times. The image obtained by observing the surface of the porous membrane by SEM was binarized using the free software "ImageJ". When binarizing, set 1 pixel in Subtract Background and perform Create Background, and then select the condition Renyi Entropy in Threshold. In the obtained binary image, the area of ​​each hole is determined by selecting Area in Analyze Particles, and the diameter is calculated by assuming that each hole is a circle. The surface pore diameter is calculated by averaging the pore diameters of more than one thousand holes.

[0195] Regarding the cross-sectional pore size, the hollow fiber membrane embedded with a commercially available embedding medium for frozen tissue sectioning (OCT Compound, manufactured by Tissue Tech) was sliced ​​with a thickness of 100 nm at -40°C in a direction perpendicular to the surface using a cryo-ultra-thin slicer (FC7, manufactured by Leica), and vacuum dried at room temperature overnight. The cross section of the hollow fiber membrane was observed using a SEM (S-5500, manufactured by Hitachi High-Technologies Corporation) or a TEM (JEM-1400Plus, manufactured by JEOL Ltd.), and the image was obtained and binarized using the free software "ImageJ". When binarizing, select the condition "Minimum" in Threshold (binarization threshold). In the obtained binary image, the area of ​​each hole was determined by selecting Area in Analyze Particles, and the diameter was calculated by assuming each hole to be a circle. The cross-sectional pore size was determined by averaging the pore sizes of more than one thousand holes.

[0196] (Manufacturing of hollow fiber membranes)

[0197] (Reference Example 1)

[0198] First, 39 wt % of a vinylidene fluoride homopolymer having a weight average molecular weight of 417,000 (KF1300 manufactured by Kureha Corporation, weight average molecular weight: 417,000, number average molecular weight: 221,000) and 61 wt % of γ-butyrolactone were dissolved at 150° C. to obtain a polymer solution as a raw material solution.

[0199] In the pressurization and ejection of the obtained polymer solution, a device having a double-layer tubular spinneret, a pipe connected to the spinneret, and two gear pumps arranged on the pipe is used. In the pipe between the gear pumps, the above-mentioned raw material liquid is pressurized to 2.5 MPa while being retained at 100-103°C for 15 seconds. Then, while ejecting an 85% by weight aqueous solution of γ-butyrolactone from the inner tube of the double-layer tubular spinneret, the raw material liquid is ejected from the outer tube. The raw material liquid is retained for 20 seconds in a cooling bath of 5°C composed of an 85% by weight aqueous solution of γ-butyrolactone and solidified. Next, the hollow fiber membrane obtained above is stretched to 1.5 times in water at 95°C to obtain a supporting layer.

[0200] The composite membrane was obtained by coating the support layer obtained above with a functional layer. In the functional layer, 12 wt% of a vinylidene fluoride homopolymer having a weight average molecular weight of 284,000, 7.2 wt% of cellulose acetate (CA435-75S, Eastman Chemical Company), and 80.8 wt% of N-methyl-2-pyrrolidone were mixed and dissolved at a temperature of 95°C to prepare a polymer solution.

[0201] The membrane-making stock solution was evenly applied to the surface of the hollow fiber membrane composed of a spherical structure, and immediately coagulated in a coagulation bath composed of 100% water to produce a hollow fiber membrane with a three-dimensional mesh structure layer formed on the spherical structure layer. The obtained hollow fiber membrane had an outer diameter of 1.30 mm, an inner diameter of 0.75 mm, a pure water permeability of 0.4 m / hr, and a strength of 1010 g / filament. In addition, the pore size of the outer surface was The pore size on the inner surface was calculated to be 0.006 μm based on the binary SEM image. The cross-sectional aperture was calculated to be 0.6 μm. is 100.

[0202] In addition, the thickness Li of the spherical structural layer is 0.225 mm.

[0203] (Reference Example 2)

[0204] In Reference Example 1, the temperature of the coagulation bath for coagulating the functional layer membrane stock solution was adjusted to produce a hollow fiber membrane with an outer surface pore size of 0.010 μm. At this time, the outer diameter was 1.30 mm, the inner diameter was 0.75 mm, the pure water permeability coefficient was 0.6 m / hr, and the strength was 1010 g / filament. is 60.

[0205] (Reference Example 3)

[0206] 12 wt% of a vinylidene fluoride homopolymer having a weight average molecular weight of 284,000, 7.2 wt% of cellulose acetate (CA435-75S, Eastman Chemical Company), and 80.8 wt% of N-methyl-2-pyrrolidone were mixed and dissolved at 95°C to prepare a polymer solution.

[0207] While the injection liquid composed of 100% water was ejected from the inner tube of the double-layered tubular spinneret, the adjusted polymer solution was coagulated in a coagulation bath composed of 100% water from the outer tube of the double-layered tubular spinneret to produce a hollow fiber membrane composed of a layer of a three-dimensional mesh structure. The obtained hollow fiber membrane has an outer diameter of 1.30 mm, an inner diameter of 0.75 mm, a pure water permeability of 0.5 m / hr, a strength of 230 g / filament, and an outer surface pore size of 1.30 mm. 0.008μm, is 1.13.

[0208] (Manufacturing of hollow fiber membrane modules)

[0209] The obtained hollow fiber membrane 5 was cut into pieces with a length of 1.2 m, immersed in a 30% by mass glycerol aqueous solution for 1 hour, and then air-dried. Then, the holes at the end of the filtrate outlet side of the hollow fiber membrane were blocked with a silicone adhesive (made by Dow Corning Toray, SH850A / B, two agents were mixed in a mass ratio of 50:50).

[0210] Then, if Figure 1 As shown, the hollow fiber membrane 5 is filled in a container 1 (inner diameter 97.6 mm, length 1100 mm) so that the blocked end of the filtrate outlet side is close to the filtrate outlet 3. A raw liquid outlet 4 is provided on the side of the container 1 on the filtrate outlet 3 side.

[0211] Next, a first potting part-forming jig is installed on the side of the stock liquid inlet 2 of the container 1, and a second potting part-forming jig is installed on the side of the filtrate outlet 3. In order to open the through hole for introducing the stock liquid into the stock liquid side space 6, a pin with a diameter of 7 mm and a length of 100 mm is inserted into the first potting part-forming jig in the same direction as the axial direction of the hollow fiber membrane 5.

[0212] As a potting agent, bisphenol F epoxy resin (LST868-R14 manufactured by Huntsman Corporation) and aliphatic amine curing agent (LST868-H14 manufactured by Huntsman Corporation) were mixed in a mass ratio of 100:30, and a total of 800 g (400 g per end) was charged into a potting agent dispenser.

[0213] Next, the centrifugal molding machine was rotated to fill the potting agent into the first potting part forming jig and the second potting part forming jig at both ends, and the first potting part 8 and the second potting part 9 were formed to solidify the potting agent. The temperature in the centrifugal molding machine was set to 35°C, the rotation speed was set to 300 rpm, and the centrifugal time was set to 5 hours.

[0214] After solidification, the first potting part forming clamp, the second potting part forming clamp and the pin are pulled out, and after being solidified at room temperature for 24 hours, the end of the second potting part 9 is cut with a tip saw-type rotary knife (チップソー-type revolving blade) to open the end face on the filtrate outlet side of the hollow fiber membrane 5.

[0215] Next, a lower cap with a raw liquid inlet 2 and an upper cap with a filtrate outlet 3 were installed on the container 1 to prepare a hollow fiber membrane module. At this time, the hollow fiber membrane had a membrane length L of 1.0 m, a filling rate M of 40%, and a membrane area of ​​9.2 m 2 .

[0216] (Filtration test)

[0217] In the filtration test using the hollow fiber membrane module obtained above, Figure 2 The filtration unit shown. The volume of the raw liquid tank 12 is 200L. The supply pump 14 is operated to introduce the raw liquid into the hollow fiber membrane module, a part of it is filtered, and the filtrate is sent to the filtrate tank 13. The raw liquid that has not been filtered is all returned to the raw liquid tank 12 from the raw liquid outlet 4. The filtrate sent to the filtrate tank 13 is returned to the raw liquid tank 12 by a pump each time, and the water level of the raw liquid tank is controlled so that it does not decrease.

[0218] The filtration is performed at a constant flow rate, and the membrane differential pressure increases as the membrane is blocked. In addition, the membrane differential pressure here is calculated by subtracting the filtrate outlet pressure measured by the filtrate outlet pressure gauge 43 from the average of the raw liquid inlet pressure measured by the raw liquid inlet pressure gauge 41 and the raw liquid outlet pressure measured by the raw liquid outlet pressure gauge 42. The filtrate outlet pressure is fixed at 20 kPa and the rising speed of the membrane differential pressure is set to rise to the filtration amount per membrane area (m 3 / m 2 ) becomes 0.1m 3 / m 2 The pressure difference between the membranes up to 0.1m 3 / m 2 The obtained value (unit is kPa / m, expressed below).

[0219] (Reference Example 4)

[0220] The simulations represented by the above equations (8) to (17) verified how accurately the pressure distribution of the actual hollow fiber membrane module can be predicted.

[0221] In the verification, another hollow fiber membrane module different from the above was prepared using the hollow fiber membrane obtained above. A fluorine tube with an inner diameter of 6 mm was used as the container 1, and the 15 hollow fiber membranes obtained above were potted in a state where both ends were open in such a way that the membrane length L became 1.0 m. The filling rate M at this time was 32%. Figure 5 As shown, the stock solution inlet 2 and the stock solution outlet 4 are connected to the side of the tube, and the stock solution introduced from the stock solution inlet 2 flows in the container 1 in a direction parallel to the axial direction of the hollow fiber membrane 5 and is discharged from the stock solution outlet 4. At this time, the pressure measured by the stock solution introduction pressure gauge 41 is set as the stock solution introduction pressure P o,0 The pressure measured by the raw liquid outlet pressure gauge 42 is set as the raw liquid outlet pressure P o,k .

[0222] On the other hand, on the filtrate side, pressure gauges are connected to both ends of the opening, and the pressure measured by the filtrate outlet pressure gauge 43 provided on the piping connected to the filtrate tank 13 is referred to as the filtrate outlet pressure P. i,k The pressure measured by the filtrate introduction pressure gauge 44 at the other end is set as the filtrate introduction pressure P i,0 .

[0223] In the hollow fiber membrane module 10 of the present application, Figure 1 As shown in FIG. 1 , the end of the hollow fiber membrane 5 on the filtrate outlet side is open, and the end on the raw liquid inlet side is closed. Therefore, in the P shown in formula (16), i,n The filtrate introduction pressure P at the position n=0 cannot be measured. i,0 Therefore, as a verification of this simulation, a small module with both ends open was made and P i,0 In addition, measure P i,0 The space connected to the filtrate introduction pressure gauge 44 is closed, and the filtrate is not led out to the filtrate introduction pressure gauge 44 side, so the pressure distribution of the small module and the pressure distribution of the hollow fiber membrane module 10 show the same distribution.

[0224] The filtration test was conducted using this small module. In the test, a 0.3 wt% aqueous solution obtained by dissolving polyethylene glycol (molecular weight 2,000,000, manufactured by Fujifilm Wako Pure Chemical Industries, Ltd.) in distilled water was used as the stock solution. The stock solution was stirred overnight with a stirrer to dissolve it, and the viscosity of the stock solution after dissolution was measured at 25°C, and the viscosity was 5.0 mPa·s.

[0225] The stock solution is supplied to the small module by the supply pump 14 for cross-flow filtration. The operating conditions at this time are that the flow rate of the stock solution is 1.0 m / s and the flow rate of the filtrate is 0.045 m / s (equivalent to a filtration flux of 0.4 m / d). In addition, the temperature of the stock solution is 25°C. Filtration is started under this operating condition, and the pressures after the filtration are measured to calculate ΔP m,0 , ΔP m,k The viscosity of the filtrate recovered in this experiment was also measured in the same manner and was 1.0 mPa·s.

[0226] Furthermore, using equations (8) to (17), ΔP is also calculated from simulations. m,0 , ΔP m,k Various parameters of the hollow fiber membrane 5 used in the production of the small module were input into the simulation. In addition, regarding the filtrate extraction pressure P o,k , calculated using the measured values ​​obtained from the test of the small module. In addition, Δl was set to 10 mm, and the shape correction coefficient τ of the raw liquid side flow path was set to 1.0.

[0227] Comparing the measured values ​​with the simulated values, the results are shown in Table 1. m , 0, ΔP m , k showed similar values, confirming that the present simulation can accurately predict the differential pressure between membranes.

[0228] [Table 1]

[0229] Measured calculate <![CDATA[ΔP m,0 [kPa]]]> 67 69 <![CDATA[ΔP m,k [kPa]]]> 25 25 <![CDATA[ΔP m,0 -ΔP m,k [kPa]]]> 42 44

[0230] (Example 1)

[0231] The hollow fiber membrane module loaded with the hollow fiber membrane of Reference Example 1 was filtered using a polyethylene glycol aqueous solution. The polyethylene glycol aqueous solution was prepared by adjusting polyethylene glycol (molecular weight 2,000,000, manufactured by Fujifilm Wako Pure Chemical Industries, Ltd.) in distilled water to 0.3 wt % as a stock solution. The stock solution at this time had a temperature of 25° C. and a viscosity of 5.0 mPa·s.

[0232] Adjust so that the flow rate of the stock solution v f becomes 1.0m / s, and the flow rate of the filtrate v p The pressure was 0.03 m / s (equivalent to 0.3 m / d as a filtration flux), and filtration was started. As shown in Table 2, the rate of increase of the differential pressure between membranes was 230 kPa / m, and the operation was able to suppress the increase of the differential pressure between membranes. In addition, the viscosity of the filtrate was 1.0 mPa·s immediately after the filtration started.

[0233] [Table 2]

[0234]

[0235] In parallel with the actual filtration test, the pressure distribution in the module was calculated by simulation. The calculation method was the same as that described in Reference Example 1. As a result, the cross-membrane pressure difference ΔP in the axial direction of the hollow fiber membrane 5 was m,0 -ΔP m,k The lower value is 43 kPa.

[0236] (Example 2)

[0237] In addition to changing the filtrate flow rate v p A filtration test and a simulation of the pressure distribution in the module were carried out in the same manner as in Example 1 except that the pressure was adjusted to 0.05 m / s (corresponding to 0.5 m / d as a filtration flux).

[0238] As a result, as shown in Table 2, the rate of increase of the differential pressure between membranes was 250 kPa / m, and the operation was possible while suppressing the increase of the differential pressure between membranes. m,0 -ΔP m,k The lower value is 43 kPa.

[0239] (Example 3)

[0240] In addition to changing the filtrate flow rate v p A filtration test and a simulation of the pressure distribution in the module were carried out in the same manner as in Example 1 except that the pressure was adjusted to 0.11 m / s (corresponding to 1.0 m / d as a filtration flux).

[0241] As a result, as shown in Table 2, the rate of increase of the differential pressure between membranes was 265 kPa / m, and the operation was possible while suppressing the increase of the differential pressure between membranes. m,0 -ΔP m,k The lower value is 41 kPa.

[0242] (Example 4)

[0243] The same hollow fiber membrane module as in Example 1 was used to filter using a polyethylene glycol aqueous solution. The polyethylene glycol aqueous solution was prepared by adjusting polyethylene glycol (molecular weight 2,000,000, manufactured by Fujifilm Wako Pure Chemical Industries, Ltd.) in distilled water to 0.45 wt % as a stock solution. The stock solution at this time had a temperature of 25° C. and a viscosity of 10.0 mPa·s.

[0244] Adjust so that the flow rate of the stock solution v f becomes 0.5m / s, and the flow rate of the filtrate v pThe pressure was 0.05 m / s (equivalent to 0.5 m / d as a filtration flux), and filtration was started. As shown in Table 2, the rate of increase of the differential pressure between membranes was 260 kPa / m, and the operation was able to suppress the increase of the differential pressure between membranes. In addition, the viscosity of the filtrate immediately after the start of filtration was 1.4 mPa·s.

[0245] In parallel with the actual filtration test, the pressure distribution in the module was calculated by simulation. The calculation method was the same as that described in Reference Example 1. As a result, the cross-membrane pressure difference ΔP in the axial direction of the hollow fiber membrane 5 was m,0 -ΔP m,k The lower value is 42 kPa.

[0246] (Example 5)

[0247] The same hollow fiber membrane module as in Example 1 was used to filter the gelatin aqueous solution. The gelatin aqueous solution was adjusted to a gelatin concentration of 0.4 wt % with respect to distilled water to prepare a stock solution. The stock solution had a temperature of 60° C. and a viscosity (μ f ) is 3.5mPa·s.

[0248] Adjust so that the flow rate of the stock solution v f becomes 1.0m / s, and the flow rate of the filtrate v p The filtration was started after the pressure difference between the membranes reached 0.03 m / s (equivalent to 0.3 m / d as the filtration flux). As a result, as shown in Table 3, the rate of increase of the differential pressure between the membranes was 260 kPa / m, and the filtration was able to operate while suppressing the increase of the differential pressure between the membranes. In addition, the viscosity of the filtrate immediately after the filtration was started was 1.1 mPa·s, μ f / μ p is 3.2.

[0249] When the pressure difference between membranes reached 1.5 times the initial pressure, the filtration was terminated, and pure water was pressurized at 200 kPa from the filtrate side for 15 seconds of backflow washing. f is 1.0m / s, the flow rate of the filtrate v p After filtering the gelatin aqueous solution at a flow rate of 0.03 m / s (corresponding to 0.3 m / d as a filtration flux), the differential pressure between membranes recovered to 1.1 times the initial ratio, and the effect of the backflow cleaning could be confirmed.

[0250] [Table 3]

[0251]

[0252] (Example 6)

[0253] A hollow fiber membrane module loaded with the hollow fiber membrane of Reference Example 2 was prepared, and filtration was performed using a gelatin aqueous solution. The gelatin aqueous solution used was the same as that of Example 5.

[0254] Adjust so that the flow rate of the stock solution v f becomes 1.0m / s, and the flow rate of the filtrate v p The filtration was started after the pressure difference between the membranes reached 0.03 m / s (equivalent to 0.3 m / d as the filtration flux). As a result, as shown in Table 3, the rate of increase of the differential pressure between the membranes was 280 kPa / m, and the filtration was able to operate while suppressing the increase of the differential pressure between the membranes. In addition, the viscosity of the filtrate immediately after the filtration was started was 1.2 mPa·s, μ f / μ p is 2.9.

[0255] When the pressure difference between membranes reached 1.5 times the initial pressure, the filtration was terminated, and pure water was pressurized at 200 kPa from the filtrate side for 15 seconds of backflow washing. f is 1.0m / s, the flow rate of the filtrate v p After filtering the gelatin aqueous solution at a flow rate of 0.03 m / s (corresponding to 0.3 m / d as a filtration flux), the differential pressure between membranes recovered to 1.1 times the initial ratio, and the effect of the backflow cleaning could be confirmed.

[0256] (Example 7)

[0257] A hollow fiber membrane module loaded with the hollow fiber membrane of Reference Example 3 was prepared, and filtration was performed using a gelatin aqueous solution. The gelatin aqueous solution used was the same as that of Example 5.

[0258] Adjust so that the flow rate of the stock solution v f becomes 1.0m / s, and the flow rate of the filtrate v p The filtration was started after the pressure difference between the membranes reached 0.03 m / s (equivalent to 0.3 m / d as the filtration flux). As a result, as shown in Table 3, the rate of increase of the differential pressure between the membranes was 290 kPa / m, and the filtration was able to operate while suppressing the increase of the differential pressure between the membranes. In addition, the viscosity of the filtrate immediately after the filtration was started was 1.1 mPa·s, μ f / μ p is 3.2.

[0259] When the pressure difference between membranes reached 1.5 times the initial pressure, the filtration was terminated, and pure water was pressurized at 200 kPa from the filtrate side for 15 seconds of backflow washing. f is 1.0m / s, the flow rate of the filtrate v pAfter filtering the gelatin aqueous solution at a flow rate of 0.03 m / s (equivalent to 0.3 m / d), the membrane pressure difference increased to 1.4 times the initial ratio, and the effect of backwashing could not be confirmed. The smaller the size, the less effective the backflow cleaning will be.

[0260] (Comparative Example 1)

[0261] In addition to adjusting the flow rate v of the stock solution f The flow rate of the filtrate is 0.5 m / s. p A filtration test and a simulation of the pressure distribution in the module were carried out in the same manner as in Example 1 except that the pressure was 0.16 m / s (corresponding to 1.5 m / d as the filtration flux).

[0262] As a result, as shown in Table 2, the rising speed of the differential pressure between membranes was 420 kPa / m, which was a result that the rising speed of the differential pressure between membranes was fast. m,0 -ΔP m,k Although 10 kPa is a relatively low value, it is conceivable that the raw liquid flow rate is slower than the filtrate flow rate, and the accumulation of fouling on the membrane surface progresses, causing the increase in the differential pressure between membranes to occur earlier.

[0263] (Comparative Example 2)

[0264] In addition to adjusting the flow rate v of the stock solution f The flow rate of the filtrate is 2.0 m / s. p A filtration test and a simulation of the pressure distribution in the module were carried out in the same manner as in Example 1 except that the pressure was 0.10 m / s (corresponding to 0.1 m / d as the filtration flux).

[0265] As a result, as shown in Table 2, the increasing speed of the differential pressure between membranes was 370 kPa / m, which was high. m,0 -ΔP m,k The higher pressure was 87 kPa, which is estimated to be a reverse filtration in which part of the filtrate flows back to the raw liquid side, which is a poor filtration efficiency. In addition, the filtration flux is small, and it is calculated that three times the number of hollow fiber membrane modules is required compared to Example 1, which is a condition that increases the filtration cost.

[0266] Although the present invention has been described in detail and with reference to specific embodiments, it will be apparent to one skilled in the art that various changes and modifications can be made without departing from the spirit and scope of the present invention.

[0267] In addition, this application is based on the Japanese patent application (Japanese Patent Application No. 2021-160479) filed on September 30, 2021, the entirety of which is incorporated by reference.

[0268] Industrial Applicability

[0269] The operation method of the hollow fiber membrane module of the present invention has been preferably applied to membrane filtration of raw liquids in the fermentation field accompanied by cultivation of microorganisms and cultured cells, the medical field, the food and beverage field, etc. in recent years, in addition to water treatment fields such as drinking water production, water purification or wastewater treatment.

[0270] Description of Reference Numerals

[0271] 1 Container

[0272] 2 Stock solution inlet

[0273] 3 Filtrate outlet

[0274] 4. Liquid outlet

[0275] 5 Hollow fiber membrane

[0276] 6. Liquid side space

[0277] 7 Filtrate side space

[0278] 81st potting department

[0279] 9Second potting section

[0280] 10Hollow fiber membrane module

[0281] 12 original liquid tank

[0282] 13 Filter liquid tank

[0283] 14 Supply pump

[0284] 15 constant temperature water tank

[0285] 16 capillaries

[0286] 21 Concentrate valve

[0287] 22 Filter liquid valve

[0288] 31 Concentrate flow meter

[0289] 32 Filtrate flow meter

[0290] 41 Stock liquid introduction pressure gauge

[0291] 42 stock liquid export pressure gauge

[0292] 43 Filtrate export pressure gauge

[0293] 44 Filtrate introduction pressure gauge

[0294] 45 tube inlet pressure gauge

[0295] 46 pipe outlet pressure gauge

[0296] 51 stock thermometer

Claims

1. A method for operating a hollow fiber membrane module, characterized in that: The filtration step includes a filtration step in which a raw liquid is supplied to the outer surface side of the hollow fiber membrane to perform cross-flow filtration. In the filtration step, the viscosity of the raw liquid is μ f The viscosity of the stock solution is 3.0 mPa·s or more and 10.0 mPa·s or less. f The viscosity of the filtrate μ p The ratio is μ f / μ p ≥1.5, and the flow rate of the filtrate v p The flow rate v of the stock solution f The flow rate ratio is 0.02≤v p / v f ≤0.

3.

2. The method for operating a hollow fiber membrane module according to claim 1, characterized in that: In the filtration step, the dissolved organic carbon concentration of the stock solution is 1,000 mg / L or more and 100,000 mg / L or less.

3. The method for operating a hollow fiber membrane module according to claim 1 or 2, characterized in that: The aforementioned hollow fiber membrane is an ultrafiltration membrane.

4. The method for operating a hollow fiber membrane module according to claim 1 or 2, characterized in that: The load at break of the hollow fiber membrane is 500 gf / filament or more.

5. The method for operating a hollow fiber membrane module according to claim 1 or 2, characterized in that: In the above filtration step, the viscosity of the above stock solution is μ f The flow rate v of the above stock solution f Satisfy v f ≤-0.135μ f +3.0 relationship.

6. The method for operating a hollow fiber membrane module according to claim 1 or 2, characterized in that: The inner diameter D of the hollow fiber membrane i 300μm≤D i ≤1000μm.

7. The method for operating a hollow fiber membrane module according to claim 1 or 2, characterized in that: The filling rate of the hollow fiber membrane module is 25% or more and 45% or less.

8. The method for operating a hollow fiber membrane module according to claim 1 or 2, characterized in that: The hollow fiber membrane has a membrane length of 0.50 m to 2.00 m.

9. The method for operating a hollow fiber membrane module according to claim 1 or 2, characterized in that: The method further comprises a backflow cleaning step of causing a cleaning liquid to flow from the inner surface to the outer surface of the hollow fiber membrane; The pore size of the outer surface of the hollow fiber membrane for The pore size of the inner surface of the hollow fiber membrane The aperture of the outer surface The ratio is