A method for removing calcium and magnesium ions from brine used in chlor-alkali electrolysis process

Through the two-stage reaction treatment and hypochlorite ion-assisted method, the calcium and magnesium ion content in the chlor-alkali industrial brine was successfully reduced, solving the problem of high calcium and magnesium ion content, and improving the quality of the raw material liquid and the life of the equipment.

CN118026379BActive Publication Date: 2024-10-18JIANGXI SELON INDAL
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
CN202410365430.7
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2024-03-28
Publication Date
2024-10-18
Estimated Expiration
2044-03-28

AI Technical Summary

Technical Problem

In the existing chlor-alkali industry, the calcium and magnesium ions in the brine are relatively high, which leads to an increase in the operating load of the chelating resin tower and unstable raw material liquid quality, affecting the normal operation of the ion membrane electrolyzer.

Method used

A two-stage reaction treatment method is adopted. First, calcium carbonate and magnesium hydroxide are generated in a high-temperature primary reaction tank, and then calcium hydrogen phosphate and magnesium hydrogen phosphate are generated in a low-temperature secondary reaction tank. The excess reaction of disodium hydrogen phosphate is further carried out. Reduce the content of calcium and magnesium ions, and use hypochlorite ions to efficiently remove organic matter during the salt preparation process.

Benefits of technology

It effectively reduces the calcium and magnesium ion content in the brine, reduces the adsorption load of the chelating resin tower, improves the quality of the raw material liquid, and extends the regeneration cycle and service life of the equipment.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118026379B_ABST
    Figure CN118026379B_ABST
Patent Text Reader

Abstract

The invention provides a method for removing calcium and magnesium ions in brine used in a chlor-alkali electrolysis process, comprising: S1, mixing water with solid raw salt to obtain saturated crude brine; S2, sending the saturated crude brine, sodium carbonate and sodium hydroxide into a primary reaction tank, so that they fully react to generate calcium carbonate solid and magnesium hydroxide colloid; S3, sending disodium hydrogen phosphate and a mixed solution in the primary reaction tank into a secondary reaction tank, so that the remaining calcium and magnesium ions fully react to generate calcium hydrogen phosphate and magnesium hydrogen phosphate solids; S4, sending the mixed solution in the secondary reaction tank into a filter for filtration, sending the filtered clear liquid into a brine regulating tank, adding hydrochloric acid to make the pH of the clear liquid 9-10, and then pumping the clear liquid into a primary brine tank; the invention can fully reduce the content of calcium / magnesium ions in the brine, improve the removal effect of calcium / magnesium ions, help to reduce the adsorption load of a chelating resin tower, and improve the quality of the raw material liquid sent to a subsequent ion membrane electrolyzer.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to a method for treating primary brine of ion membrane caustic soda, in particular to a method for removing calcium and magnesium ions from brine used in a chlor-alkali electrolysis process, mainly to removing calcium and magnesium ions from brine. Background Art

[0002] The main processes used by my country's chlor-alkali industry to treat brine are the traditional Doyle clarification process and the inorganic / organic membrane process. The calcium and magnesium ion content (calculated as calcium) of brine treated by the traditional Doyle clarification process is between 1000 and 3000 PPb, and the calcium and magnesium ion content (calculated as calcium) of brine treated by the inorganic / organic membrane process is between 500 and 2000 PPb. However, the calcium / magnesium ion content of the primary brine in these two process flows is still relatively high, which increases the operating load of the chelating resin tower while the calcium / magnesium adsorption capacity of the resin tower remains unchanged. At the same time, the brine quality at the outlet of the resin tower is also unstable, affecting the normal operation of the subsequent ion membrane electrolyzer.

[0003] With the continuous development of the chlor-alkali industry, the prior art has made certain improvements to the traditional process, such as patent CN1868878A, which first uses sodium hydroxide, sodium carbonate and other refining agents to fully react with calcium / magnesium ions for precipitation, and then filters through a filter to obtain primary brine. However, the existing refining agents such as sodium hydroxide and sodium carbonate often cannot ensure the complete precipitation of calcium / magnesium ions, which leads to the calcium / magnesium ion content of the primary brine in the prior art is still relatively high, making it difficult to further reduce the adsorption load of the chelating resin tower, and is not conducive to further improving the quality of the raw liquid sent to the subsequent ion membrane electrolyzer. Summary of the invention

[0004] In view of this, the present invention aims to provide a method for removing calcium and magnesium ions from brine used in a chlor-alkali electrolysis process, so as to solve the problem that the calcium / magnesium ion content of primary brine in the prior art is still relatively high.

[0005] To achieve the above object, the technical solution of the present invention is achieved as follows:

[0006] A method for removing calcium and magnesium ions from brine used in a chlor-alkali electrolysis process comprises: S1, mixing water with solid raw salt to obtain saturated crude brine; S2, sending the saturated crude brine, sodium carbonate and sodium hydroxide into a primary reaction tank, so that they fully react to generate solid calcium carbonate and colloid magnesium hydroxide; S3, sending disodium hydrogen phosphate and a mixed solution in the primary reaction tank into a secondary reaction tank, so that the remaining calcium and magnesium ions fully react to generate solid calcium hydrogen phosphate and magnesium hydrogen phosphate; S4, sending the mixed solution in the secondary reaction tank into a filter for filtration, sending the filtered clear liquid into a brine regulating tank, adding hydrochloric acid to make the pH of the clear liquid 9-10, and then pumping the clear liquid into a primary brine tank.

[0007] Furthermore, the water in step S1 at least includes dechlorinated salt water containing hypochlorite ions returned from the downstream ion membrane electrolysis process.

[0008] Furthermore, the hypochlorite ion concentration in the dechlorinated brine is 5-40 mg / L, and the chlorate ion concentration in the mixed solution at the outlet of the secondary reaction tank is lower than 1-3 mg / L, so that the organic matter content in the mixed solution at the outlet of the secondary reaction tank is ≤10 ppm.

[0009] Furthermore, in step S2, based on the unit volume of saturated crude brine, the amount of sodium carbonate over-alkali is 300-500 mg / L, and the amount of sodium hydroxide over-alkali is 100-300 mg / L.

[0010] Furthermore, the temperature of the mixed liquid in the primary reaction tank is not less than 55°C.

[0011] Furthermore, a plurality of steam heating pipes are evenly arranged in the first-stage reaction tank, and the steam heating pipes have steam outlets for directly conveying steam into the first-stage reaction tank.

[0012] Furthermore, in step S3, based on the residual calcium and magnesium ion contents in the mixed solution fed into the secondary reaction tank, the amount of disodium hydrogen phosphate added exceeds the theoretical amount required for the reaction by 10-20 ppm.

[0013] Furthermore, the temperature of the mixed liquid in the secondary reaction tank is 10-20°C.

[0014] Furthermore, in step S4, the filter is a polytetrafluoroethylene tubular filter membrane filter.

[0015] Compared with the prior art, the method for removing calcium and magnesium ions from brine used in chlor-alkali electrolysis process described in the present invention has the following advantages:

[0016] The method for removing calcium and magnesium ions from salt water used in a chlor-alkali electrolysis process of the present invention first utilizes the dechlorinated light salt water returned from the downstream ion membrane electrolysis process and utilizes the hypochlorite ions therein to efficiently remove natural organic matter such as bacteria, algae, humic acid, etc. in the salt water at the stage of preparing saturated crude salt water by salt conversion. Not only does it not require the additional addition of sodium hypochlorite, it reduces the additional agent injection and eliminates the corresponding agent injection equipment, but it can also effectively reduce the organic matter content on the basis of minimizing the residual hypochlorite ions, avoid interference with the calcium and magnesium element removal process, avoid the organic matter carried in the water from affecting the normal working environment of the chelating resin tower, and improve the quality of the raw material liquid sent to the subsequent ion membrane electrolyzer.

[0017] At the same time, the present application performs at least two-stage reaction treatment on the brine, using a relatively high temperature primary reaction tank to perform a first-stage reaction to remove calcium / magnesium ions, and then using a relatively low temperature secondary reaction tank to perform a second-stage reaction to remove the remaining calcium / magnesium ions in the brine, thereby achieving two-stage removal of calcium / magnesium ions, which can fully reduce the calcium / magnesium ion content in the brine, improve the removal effect of calcium / magnesium ions, help reduce the adsorption load of the chelating resin tower, improve the quality of the raw material liquid sent to the subsequent ion membrane electrolyzer, and help extend the regeneration cycle or service life of downstream equipment such as the resin tower and the ion membrane electrolyzer. BRIEF DESCRIPTION OF THE DRAWINGS

[0018] The accompanying drawings constituting a part of the present invention are used to provide a further understanding of the present invention. The exemplary embodiments of the present invention and their descriptions are used to explain the present invention and do not constitute an improper limitation of the present invention. In the accompanying drawings:

[0019] Figure 1 A process block diagram of a method for removing calcium and magnesium ions from brine used in a chlor-alkali electrolysis process according to an embodiment of the present invention;

[0020] Figure 2 Another process block diagram of a method for removing calcium and magnesium ions from brine used in a chlor-alkali electrolysis process according to an embodiment of the present invention;

[0021] Figure 3 It is a schematic diagram of the structure of the cross-flow filter according to an embodiment of the present invention;

[0022] Figure 4 This is a simplified structural diagram of a driving device in a cross-flow filter according to an embodiment of the present invention;

[0023] Figure 5 It is a schematic diagram of the structure of the gear assembly in the driving device according to an embodiment of the present invention.

[0024] Description of reference numerals:

[0025] 1. Shell; 2. Inner core; 21. Central axis; 3. Outer core; 31. Outer sleeve; 4. Driving device; 5. Brine chamber; 6. First filter chamber; 61. Liquid extraction tube; 7. Second filter chamber; 71. Liquid outlet; 81. Central gear; 82. Planetary gear; 83. Driven gear ring; 84. Planetary carrier; 85. Box; 91. Rotor; 92. Stator. DETAILED DESCRIPTION

[0026] The inventive concepts of the present disclosure will be described below using terms commonly used by those skilled in the art to convey the essence of their work to other persons skilled in the art. However, these inventive concepts can be embodied in many different forms and should not be considered limited to the embodiments described herein.

[0027] It should be noted that, in the absence of conflict, the embodiments of the present invention and the features in the embodiments may be combined with each other.

[0028] The present invention will be described in detail below with reference to the accompanying drawings and in conjunction with embodiments.

[0029] In order to solve the problem that the calcium / magnesium ion content of primary brine in the prior art is still relatively high, this embodiment proposes a method for removing calcium and magnesium ions from brine used in a chlor-alkali electrolysis process, as shown in the attached Figure 1-2 As shown, the method includes:

[0030] S1, mixing water and solid raw salt to obtain saturated crude brine;

[0031] The water in step S1 at least includes dechlorinated brine containing hypochlorite ions returned from the downstream ion membrane electrolysis process, so that in the process of preparing saturated crude brine by salt treatment, there is no need to add additional sodium hypochlorite, which reduces the amount of additional reagents and can also achieve efficient removal of natural organic matter such as bacteria, algae, humic acid, etc. in the brine.

[0032] Specifically, the concentration of hypochlorite ions in the dechlorinated light salt water is 5-40 mg / L (with the dechlorinated light salt water as a reference), and the concentration of chlorate ions in the mixed solution at the outlet of the secondary reaction tank should be ensured to be lower than 1-3 mg / L (with the mixed solution at the outlet of the secondary reaction tank as a reference), preferably lower than 1 mg / L. Accordingly, the natural organic matter such as algae and humic acid in the salt water is removed by relatively slightly excessive hypochlorite ions, so that the organic matter content in the mixed solution at the outlet of the secondary reaction tank is ≤10ppm. Thus, without the need to add additional sodium hypochlorite and reduce the dosage of the agent, by further regulating the concentration of hypochlorite ions, the organic matter content can be effectively reduced on the basis of leaving no residual hypochlorite ions as far as possible, which can not only avoid interference with the removal process of calcium and magnesium elements, but also avoid the organic matter carried in the water from affecting the normal working environment of the chelating resin tower, and can also improve the quality of the raw liquid sent to the subsequent ion membrane electrolyzer.

[0033] In addition, the water may include industrial water, filtrate from a plate and frame filter press, miscellaneous water from diaphragm electrolysis, etc., in addition to the dechlorinated brine containing hypochlorite ions returned from the downstream ion membrane electrolysis process. The specific process of step S1 is roughly as follows: water is pumped into a water bucket, and then pumped from the water bucket into a salt tank as a solvent; solid raw salt is unloaded from a salt unloader to a salt field, and then sent to a salt tank by a crane; saturated crude brine is obtained by dissolving the raw salt in the salt tank, and the saturated crude brine in the salt tank overflows into a crude brine receiving bucket, and then is pumped to a brine receiving tank in the factory by a crude brine pump.

[0034] S2, sending saturated crude brine, sodium carbonate and sodium hydroxide into a primary reaction tank to fully react to generate solid calcium carbonate and colloid magnesium hydroxide;

[0035] Among them, based on the unit volume of saturated crude brine, the amount of sodium carbonate is 300-500 mg / L, and the amount of sodium hydroxide is 100-300 mg / L, so that the amount of sodium carbonate and sodium hydroxide added exceeds the theoretical amount required for the reaction and tries not to exceed the water quality standard required for production. Among them, sodium carbonate and sodium hydroxide can be added to the crude brine in solid form, or they can be prepared in advance into solutions of appropriate concentrations and added to the crude brine, such as: sodium carbonate and sodium hydroxide are prepared into saturated solutions respectively, and added to the crude brine respectively.

[0036] In order to increase the reaction rate in the primary reaction tank, the primary reaction tank is provided with a heating device so that the temperature of the mixed liquid in the primary reaction tank is not less than 55°C; preferably, the heating device is steam heating, and a plurality of steam heating pipes are evenly arranged in the primary reaction tank, and the steam heating pipes have a steam outlet for directly conveying steam into the primary reaction tank. While improving the heating efficiency and the reaction rate, the influx of steam into the mixed brine can also increase the turbulence of the brine, avoid the appearance of static dead zones of different densities in the brine, and allow the materials to fully mix and react, which is beneficial to further improve the removal effect of calcium / magnesium ions.

[0037] S3, sending the mixed solution of disodium hydrogen phosphate and the primary reaction tank into the secondary reaction tank, so that the remaining calcium and magnesium ions fully react to form calcium hydrogen phosphate and magnesium hydrogen phosphate solids;

[0038] The amount of disodium hydrogen phosphate added is slightly excessive, and based on the residual calcium and magnesium ion content in the mixed solution fed into the secondary reaction tank, the amount of disodium hydrogen phosphate added exceeds the theoretical amount required for the reaction by 10-20ppm. Similarly, disodium hydrogen phosphate can be added in solid form, or it can be added after being prepared in advance into a solution of appropriate concentration.

[0039] The temperature of the mixed solution in the secondary reaction tank is 10-20°C, that is, the mixed solution in the secondary reaction tank is room temperature (such as conventional 20°C) or slightly lower than room temperature, so that the secondary reaction tank maintains a relatively low temperature reaction environment, and the calcium and magnesium ions remaining in the brine can be further removed in the form of calcium hydrogen phosphate and magnesium hydrogen phosphate solids, and the dissolution trend of solids (especially slightly soluble substances) can also be suppressed, avoiding insufficient precipitation of some solids due to high temperature, which is conducive to further improving the removal effect of calcium / magnesium ions. Specifically, a baffle groove is set between the primary reaction tank and the secondary reaction tank, and the baffle groove preferably has a sufficient length, so that the mixed solution of the relative height in the primary reaction tank can be cooled by the baffle groove and then flow into the secondary reaction tank, so as to ensure that the temperature of the mixed solution in the secondary reaction tank is near room temperature. In addition, preferably, a cooling coil is provided in the secondary reaction tank. When the temperature of the mixed liquid in the secondary reaction tank is high, a low-temperature medium (such as low-temperature carbon dioxide, low-temperature Freon, etc.) can be transported into the cooling coil, and the temperature of the mixed liquid in the secondary reaction tank is near or below room temperature through the coil heat exchange.

[0040] S4. Send the mixed liquid in the secondary reaction tank to the filter for filtration, send the filtered clear liquid to the brine adjustment tank, add hydrochloric acid to make the pH of the clear liquid 9-10, and then pump the clear liquid into the primary brine tank.

[0041] Among them, the brine in the primary brine tank can be regarded as brine after the calcium and magnesium ions are removed, which can be used in downstream processes or for secondary treatment.

[0042] Therefore, the present application firstly utilizes the dechlorinated light brine returned from the downstream ion membrane electrolysis process, and utilizes the hypochlorite ions therein to efficiently remove natural organic matter such as bacteria, algae, humic acid, etc. in the brine at the stage of preparing saturated crude brine by salt conversion. Not only does it not require the additional addition of sodium hypochlorite, it reduces the additional agent dosage and eliminates the corresponding agent dosage equipment, but it can also effectively reduce the organic matter content on the basis of minimizing the residual hypochlorite ions, which can not only avoid interference with the calcium and magnesium element removal process, but also avoid the organic matter carried in the water from affecting the normal working environment of the chelating resin tower, and can also improve the quality of the raw liquid sent to the subsequent ion membrane electrolyzer.

[0043] At the same time, the present application performs at least two-stage reaction treatment on the brine, using a relatively high temperature primary reaction tank to perform a first-stage reaction to remove calcium / magnesium ions, and then using a relatively low temperature secondary reaction tank to perform a second-stage reaction to remove the remaining calcium / magnesium ions in the brine, thereby achieving two-stage removal of calcium / magnesium ions, which can fully reduce the calcium / magnesium ion content in the brine, improve the removal effect of calcium / magnesium ions, help reduce the adsorption load of the chelating resin tower, improve the quality of the raw material liquid sent to the subsequent ion membrane electrolyzer, and help extend the regeneration cycle or service life of downstream equipment such as the resin tower and the ion membrane electrolyzer.

[0044] In this application, after sampling and testing the corresponding salt water, each material can be added quantitatively by manual or automatic dosing device. Taking automatic dosing as an example, the concentration signal of the specific component in the salt water detected can be converted into an electrical signal and input into the automatic control system through the online detector. Through the control of the automatic control system, the dosing pump can adjust the flow rate and addition amount of the agent in real time. In view of the fact that the technologies such as quantitative dosing and automatic dosing can refer to the existing technology or analytical chemistry technology, this application will not elaborate on them.

[0045] The sodium carbonate and sodium hydroxide used in this application often do not exceed the water quality standards required for production, but the use of disodium hydrogen phosphate often leads to excessive total phosphorus content in the water body, which not only easily induces eutrophication of the water body and causes microbial growth, but also causes certain inconveniences to the treatment of downstream water bodies (such as harmless treatment of wastewater). For this reason, this application sets a pretreatment process between steps S1 and S2, that is, after executing step S1, the pretreatment process is executed, and then step S2 is executed;

[0046] The pretreatment process includes: feeding saturated crude brine, sodium hydroxide, and a magnetized modifying agent into a pretreatment tank, stirring them sufficiently, and then feeding them into a magnetic sedimentation tank, using magnetic force to adsorb the magnetized modifying agent, and using the supernatant as saturated crude brine after pretreatment for use in step S2;

[0047] Wherein, the magnetized modification agent is a magnetic chitosan microsphere with sodium polyacrylate grafted on the surface. Based on the unit volume of saturated crude brine, a magnetized modification agent with a particle size of 400-800 microns is taken, and the usage amount of the magnetized modification agent is 30-100 particles / L; the amount of sodium hydroxide added is such that the pH value of the saturated crude brine is 7.2-8.0. Thus, in a weakly alkaline environment, by adding magnetic chitosan microspheres with sodium polyacrylate grafted on the surface into the saturated crude brine, the calcium / magnesium ions in the saturated crude brine are treated and attached to the surface of the microspheres, so as to achieve pretreatment of the saturated crude brine, which can effectively reduce the content of calcium / magnesium ions sent to the primary reaction tank. Correspondingly, after being treated in the primary reaction tank, the content of calcium / magnesium ions entering the secondary reaction tank is further reduced, which can effectively reduce the amount of sodium hydrogen phosphate added in the secondary reaction tank, which is beneficial to reduce the total phosphorus content in the water body.

[0048] The preparation process of the magnetized modifying agent is as follows:

[0049] B1, taking an acetic acid solution with a volume fraction of 2%-4%, dissolving chitosan powder in the acetic acid solution to obtain a chitosan solution with a mass fraction of 2.5%-3.0%;

[0050] B2, adding nickel powder with a particle size of 100-200 microns to the chitosan solution, stirring evenly, dripping the chitosan solution into a curing bath to solidify into balls, and filtering to obtain magnetic chitosan microspheres;

[0051] The mass ratio of nickel powder to chitosan is 0.01-0.05. The curing bath is an ethanol solution containing sodium hydroxide, the volume fraction of ethanol is 10%-40%, and the mass fraction of sodium hydroxide is 5%-15%;

[0052] B3, take a 4% sodium bisulfite solution, heat it to 55-65°C, add magnetic chitosan microspheres under stirring, and then drop acrylic acid monomer and ammonium persulfate solution into the sodium bisulfite solution at the same time;

[0053] The mass ratio of acrylic acid monomer to magnetic chitosan microspheres is 0.3-0.6, and the mass ratio of ammonium persulfate to acrylic acid monomer is 1:200-400.

[0054] B4. After the addition is completed, the reaction is kept warm for 2-4 hours, and then sodium hydroxide solution is added to adjust the pH to 7.2-7.6. After filtering, magnetic chitosan microspheres with sodium polyacrylate grafted on the surface are obtained.

[0055] Therefore, the present application utilizes magnetic chitosan microspheres as a matrix and grafts them with sodium polyacrylate. On the one hand, since both chitosan and sodium polyacrylate have good heavy metal ion treatment capabilities, the removal effect of calcium / magnesium ions in the pretreatment process can be improved, and the burden of treating calcium / magnesium ions in subsequent processes can be reduced. On the other hand, the precipitates formed by calcium / magnesium ions will mainly adhere to the surface of the microspheres, and then in the magnetic sedimentation tank, as the magnetized modified treatment agent quickly settles under the action of magnetic force, the separation efficiency of the supernatant and the solid matter is greatly improved.

[0056] For the magnetic sedimentation tank, an electromagnetic generating device, such as an electromagnet, is arranged at the bottom of the magnetic sedimentation tank to generate magnetic force under the action of electricity, and magnetically adsorb the magnetized modified treatment agent entering the magnetic sedimentation tank, so that the magnetized modified treatment agent carries the calcium and magnesium precipitates attached to its surface for rapid sedimentation, which is beneficial to improving the separation efficiency of the supernatant and also improving the production efficiency.

[0057] For the filter, the present application can use a Kai membrane filter, wherein the Kai membrane filter uses a polytetrafluoroethylene (PTFE) tubular filter membrane filter, the pore size of the filter membrane in the Kai membrane filter is 0.22-0.5 μm, and the flow rate of a single Kai membrane filter is about 120 cubic meters per hour, which is a large flux filter that can meet large-scale brine treatment processes. In order to maintain a high filtration capacity and a low filtration pressure, the filter needs to be chemically regenerated with a 15% hydrochloric acid solution after running for a certain period of time.

[0058] However, considering that the magnesium hydroxide generated during the removal of calcium / magnesium ions has colloidal properties to a certain extent, it is easy to cause clogging of the filter membrane and affect the continuity of production. For this reason, the filter in this application is preferably a cross-flow filter, such as the attached Figure 3 As shown, the cross-flow filter includes a shell 1, an outer core 3 and an inner core 2 are arranged inside the shell 1, and the outer core 3 and the inner core 2 are both cylindrical filter structures with closed bottoms, and conventional tubular filter membranes or other tubular filter materials can be used; the inner core 2 is arranged inside the outer core 3, and the inner core 2 and the outer core 3 are arranged coaxially, and the inner core 2 has a first filter chamber 6 inside, a salt water chamber 5 is formed between the inner core 2 and the outer core 3, and a second filter chamber 7 is formed between the shell 1 and the outer core 3, and the inner core 2 and the outer core 3 can at least rotate in the opposite direction to each other. The opposite rotation includes at least one of the following states: when the inner core 2 rotates forward, the outer core 3 rotates backward accordingly, when the inner core 2 rotates backward, the outer core 3 rotates forward accordingly, and when the inner core 2 rotates forward and reverse alternately, the outer core 3 rotates forward and reverse alternately.

[0059] Thus, the mixed liquid in the secondary reaction tank is injected into the salt water chamber 5. As the inner core 2 and the outer core 3 rotate, a part of the salt water enters the first filter chamber 6 after being filtered by the inner core 2, and a part of the salt water enters the second filter chamber 7 after being filtered by the outer core 3. The filter residue blocked by the inner core 2 and the outer core 3 will be continuously washed by the salt water in the salt water chamber 5 as the inner core 2 and the outer core 3 rotate, and will be separated from the inner core 2 and the outer core 3 to form an internal and external bidirectional cross-flow filtration, which not only increases the filtration area, but also prevents the filter residue from adhering to the surface of the filter core, preventing the clogging of the filter core, maintaining the continuous operation of the filtration, and improving the filtration efficiency. At the same time, due to the mutual reverse rotation between the inner core 2 and the outer core 3, the turbulence degree of the water flow in the salt water chamber 5 is aggravated, the force of the salt water washing the surface of the filter core is increased, and the water flow dead zone in the salt water chamber 5 is avoided, which can further improve the filtration efficiency.

[0060] For the rotation of the inner core 2 and the outer core 3, the cross-flow filter includes a driving device 4, a central axis 21 is arranged at the bottom of the inner core 2, an outer shaft sleeve 31 is arranged at the bottom of the outer core 3, the outer shaft sleeve 31 is sleeved on the outside of the central axis 21 and is coaxially arranged with the central axis 21, the central axis 21 and the outer shaft sleeve 31 can rotate relative to each other, and the central axis 21 and the outer shaft sleeve 31 are respectively connected to the driving device 4, so that the inner core 2 and the outer core 3 can at least rotate in opposite directions to each other.

[0061] When the center shaft 21 and the outer sleeve 31 are set, a water seal is set between the center shaft 21 and the bottom of the outer core 3 or the outer sleeve 31, and a water seal is set between the outer sleeve 31 and the bottom of the shell 1. Therefore, on the basis of setting the center shaft 21 and the outer sleeve 31 and ensuring their rotation, corresponding water seals are set to perform sealing treatment to prevent brine from leaking directly from the bottom of the outer core 3 into the shell 1, and to prevent brine from leaking directly from the bottom of the shell 1 into the external environment.

[0062] Regarding the specific content of driving the inner core 2 and the outer core 3 to rotate in opposite directions, two driving implementation forms are proposed in this application:

[0063] 1. The driving device 4 includes two independent motors, which are respectively denoted as the first motor and the second motor. The central shaft 21 is directly connected to the first motor, and the outer sleeve 31 is driven by the second motor through a pulley; thus, by adjusting the rotation direction of the two motors, various rotation forms such as reverse rotation and same-direction rotation between the inner core 2 and the outer core 3 can be achieved.

[0064] 2. The drive device 4 is provided with only one motor, as shown in the attached Figure 4 , 5 As shown, specifically, the driving device 4 includes a motor and a gear box. A gear assembly is arranged inside the housing 85 of the gear box. The gear assembly includes a central gear 81, a planetary gear 82, a driven gear ring 83, and a planet carrier 84. The driven gear ring 83 surrounds the outside of the central gear 81 and the planetary gear 82. The planetary gear 82 is located between the central gear 81 and the driven gear ring 83. The planetary gear 82 meshes with the central gear 81 and meshes with the inner teeth of the driven gear ring 83. The planetary gear 82 is fixedly connected to the housing 85 through the planet carrier 84. One side of the central gear 81 is connected to the central shaft 21, and the other side is connected to the motor. The outer sleeve 31 is connected to the driven gear ring 83. For the motor, it includes a rotor 91 and a stator 92. The central gear 81 is connected to the rotor 91.

[0065] Thus, by setting up a gear box and a motor, through the rotation of the motor (either forward or reverse), while the motor drives the center gear 81 and the center shaft 21 to rotate, the planetary gear 82 rotates in the opposite direction relative to the center gear 81. Since the planetary carrier 84 is fixed, the planetary gear 82 only transmits and drives the driven ring gear 83 to rotate in the opposite direction relative to the center gear 81. The outer sleeve 31 rotates with the driven ring gear 83, so that the center shaft 21 and the outer sleeve 31 can generate relative rotation in the opposite direction, and accordingly, the inner core 2 and the outer core 3 can rotate in the opposite direction.

[0066] For the injection or discharge of the mixed liquid in the secondary reaction tank and the discharge of the filtrate after filtration, corresponding material pipelines can be set in the cavities corresponding to the first filter chamber 6, the brine chamber 5, and the second filter chamber 7 to provide for the flow of materials, for example, a liquid injection pipeline and a liquid extraction pipeline are set in the brine chamber 5, a liquid extraction pipe 61 is set in the first filter chamber 6, and a liquid outlet 71 connected to the second filter chamber 7 is set in the shell 1. In addition, the liquid extraction pipe 61 can also be omitted, and the central axis 21 can be changed into a hollow axis with a cavity, and the cavity is connected to the first filter chamber 6, so that the filtrate in the first filter chamber 6 can flow along the cavity to the outside of the cross-flow filter, thereby realizing the gravity self-drainage of the first filter chamber 6.

[0067] Example 1

[0068] A1. Salting. Mix water and solid raw salt to obtain saturated crude brine;

[0069] A2. Pretreatment. Saturated crude brine, sodium hydroxide, and magnetized modifying agent are sent to the pretreatment tank, stirred thoroughly, and then sent to the magnetic sedimentation tank. The magnetized modifying agent is adsorbed by magnetic force, and the supernatant is used as the saturated crude brine after pretreatment; the magnetized modifying agent is magnetic chitosan microspheres with surface grafted sodium polyacrylate, and the magnetized modifying agent with a particle size of 400-800 microns can be used. The usage amount is 60 particles per liter of saturated crude brine, and the amount of sodium hydroxide added is such that the pH value of the saturated crude brine is 7.2-8.0;

[0070] A3, primary reaction. The saturated crude brine after pretreatment, excess sodium carbonate, and excess sodium hydroxide are sent to the primary reaction tank to fully react to generate solid calcium carbonate and colloid magnesium hydroxide; based on the unit volume of saturated crude brine, the amount of sodium carbonate is 400 mg / L, and the amount of sodium hydroxide is 200 mg / L; the temperature of the primary reaction tank is 60°C;

[0071] A4. Secondary reaction. The sodium hydrogen phosphate and the mixed solution in the primary reaction tank are sent to the secondary reaction tank, so that the remaining calcium and magnesium ions react fully to form calcium hydrogen phosphate and magnesium hydrogen phosphate solids; the amount of sodium hydrogen phosphate added exceeds the theoretical amount required for the reaction by 10ppm; the temperature of the secondary reaction tank is room temperature;

[0072] A5. Send the mixed liquid in the secondary reaction tank to the filter for filtration, and send the filtered clear liquid to the brine adjustment tank. Add hydrochloric acid to make the pH of the clear liquid 9-10, and then pump the clear liquid into the primary brine tank.

[0073] The calcium and magnesium ion (calculated as calcium) contents of the brine in the primary brine tank were tested, and the results are shown in Table 1.

[0074] Example 2

[0075] This embodiment omits the pre-treatment process of step A2 in embodiment 1, and the operations of the remaining steps are completely consistent with those of embodiment 1. The calcium and magnesium ion contents (calcium) of the brine in the primary brine tank were tested, and the results are shown in Table 1.

[0076] Comparative Example 1

[0077] This embodiment adopts the existing technology, and utilizes the process principle of obtaining primary brine by filtering after sodium hydroxide, sodium carbonate and calcium / magnesium ions fully react and precipitate, and the specific operation process is: retaining the operation process of steps A1, A3, and A5 of embodiment 1, omitting the pretreatment process of step A2 and the secondary reaction process of step A4. The calcium and magnesium ion (calculated as calcium) content of the brine in the primary brine tank is detected, and the results are shown in Table 1.

[0078] It should be noted that the specific steps in Example 1, Example 2, and Comparative Example 1 are consistent with the relevant contents in the specific implementation manner of this application. In order to avoid redundancy, this application briefly describes the relevant contents in Example 1, Example 2, and Comparative Example 1.

[0079] Table 1 Calcium and magnesium ion (calculated as calcium) content test results

[0080]

[0081] It can be seen from Table 1 that when Example 1 and Example 2 are compared with Comparative Example 1, since the present application uses disodium hydrogen phosphate to remove the residual calcium / magnesium ions in the brine in a relatively low temperature secondary reaction tank after the first-stage reaction, the calcium / magnesium ion content in the brine is significantly reduced, and the removal effect of calcium / magnesium ions is improved. In addition, by comparing Example 1 with Example 2, the present application uses a magnetized modified treatment agent to pre-treat the saturated crude brine, which can further reduce the calcium / magnesium ion content in the brine, and can also effectively reduce the amount of disodium hydrogen phosphate added in the secondary reaction tank, which is beneficial to reducing the total phosphorus content in the water body.

[0082] The above description is only a preferred embodiment of the present invention and is not intended to limit the present invention. Any modifications, equivalent substitutions, improvements, etc. made within the spirit and principle of the present invention should be included in the protection scope of the present invention.

Claims

1. A method for removing calcium and magnesium ions from brine used in a chlor-alkali electrolysis process, characterized in that: The method comprises: S1, mixing water and solid raw salt to obtain saturated crude brine; S2, sending saturated crude brine, sodium carbonate and sodium hydroxide into a primary reaction tank to fully react to generate solid calcium carbonate and colloid magnesium hydroxide; S3, sending the mixed solution of disodium hydrogen phosphate and the primary reaction tank into the secondary reaction tank, so that the remaining calcium and magnesium ions fully react to form calcium hydrogen phosphate and magnesium hydrogen phosphate solids; S4, sending the mixed liquid in the secondary reaction tank to the filter for filtration, sending the filtered clear liquid to the brine adjustment tank, adding hydrochloric acid to make the pH of the clear liquid 9-10, and then pumping the clear liquid into the primary brine tank; The temperature of the mixed liquid in the primary reaction tank is not less than 55°C; a plurality of steam heating pipes are evenly arranged in the primary reaction tank, and the steam heating pipes have a steam outlet for directly conveying steam into the primary reaction tank; the temperature of the mixed liquid in the secondary reaction tank is 10-20°C; After executing step S1, the method performs a pre-processing process, and then executes step S2; The pretreatment process includes: sending saturated crude brine, sodium hydroxide, and a magnetized modifying agent into a pretreatment tank, stirring them sufficiently, and then sending them into a magnetic sedimentation tank, using magnetic force to adsorb the magnetized modifying agent, and using the supernatant as the saturated crude brine after pretreatment for use in step S2; wherein the magnetized modifying agent is a magnetic chitosan microsphere with sodium polyacrylate grafted on the surface.

2. A method for removing calcium and magnesium ions from brine used in a chlor-alkali electrolysis process according to claim 1, characterized in that: The water in step S1 at least includes dechlorinated salt water containing hypochlorite ions returned from the downstream ion membrane electrolysis process.

3. A method for removing calcium and magnesium ions from brine used in a chlor-alkali electrolysis process according to claim 2, characterized in that: The hypochlorite ion concentration in the dechlorinated brine is 5-40 mg / L, and the chlorate ion concentration in the mixed solution at the outlet of the secondary reaction tank is lower than 1-3 mg / L, so that the organic matter content in the mixed solution at the outlet of the secondary reaction tank is ≤10 ppm.

4. A method for removing calcium and magnesium ions from brine used in a chlor-alkali electrolysis process according to claim 1, characterized in that: In step S2, based on the unit volume of saturated crude brine, the amount of sodium carbonate over-alkali is 300-500 mg / L, and the amount of sodium hydroxide over-alkali is 100-300 mg / L.

5. A method for removing calcium and magnesium ions from brine used in chlor-alkali electrolysis process according to claim 1, characterized in that: In step S3, based on the residual calcium and magnesium ion contents in the mixed solution fed into the secondary reaction tank, the amount of disodium hydrogen phosphate added exceeds the theoretical amount required for the reaction by 10-20 ppm.

6. A method for removing calcium and magnesium ions from brine used in chlor-alkali electrolysis process according to claim 1, characterized in that: In step S4, the filter is a polytetrafluoroethylene tubular filter membrane filter.

Citation Information

Patent Citations

  • Method of refining salt by membrane filtration

    CN1868878A

  • Method for reducing content of calcium and magnesium ions in primary brine

    CN103449479A

  • Device for carrying out impurity removal treatment on crude brine for electrolysis and treatment method using same

    CN104030485A

  • Method of prolonging regeneration period of ionic membrane caustic soda resin column, and apparatus by using the method

    CN108517535A