A thin film bulk acoustic wave resonator and a method for preparing the same

By setting up an inclined protective wall structure and release holes in the base layer of the thin-film bulk acoustic wave resonator, the problem of corrosive gas or liquid leakage during the release process is solved, and the stability of the device and reliable production of the device are achieved Sex improvement.

CN118074655BActive Publication Date: 2024-11-05WUHAN MEMSONICS TECH CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202410275988.6
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2024-03-11
Publication Date
2024-11-05
Estimated Expiration
2044-03-11

AI Technical Summary

Technical Problem

The existing first cavity type thin film bulk acoustic wave resonator may leak laterally during the release process, resulting in device damage, and the chemical mechanical polishing process is difficult and the effect is unstable.

Method used

A first protective wall and an inclined second protective wall are provided in the base layer. The second protective wall is located above the first protective wall and is inclined in a direction close to the first cavity to form an inclined structure surrounding the first cavity to prevent corrosion The gas or liquid leaks transversely and the base material in the protective wall is removed by forming a release hole on the substrate layer into the corrosion gas or liquid.

Benefits of technology

It effectively prevents lateral leakage of corrosive gas or liquid during the first cavity release process, avoids lateral corrosion damage caused by unblocking protection walls, and improves device stability and production reliability.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118074655B_ABST
    Figure CN118074655B_ABST
Patent Text Reader

Abstract

The present application provides a thin film bulk acoustic wave resonator and a preparation method thereof, and relates to the field of resonator preparation technology. The thin film bulk acoustic wave resonator includes: a substrate layer, a bottom electrode layer, a piezoelectric layer and a top electrode layer stacked in sequence on the substrate layer, a first cavity, a first protective wall and a second protective wall surrounding the first cavity are provided in the substrate layer, the second protective wall is located above the first protective wall, and the second protective wall is inclined from the first protective wall to the direction close to the first cavity. The thin film bulk acoustic wave resonator can prevent the corrosive gas or corrosive liquid from leaking laterally from above the protective wall during the release of the first cavity by arranging the first protective wall and the inclined second protective wall in the substrate layer, thereby avoiding lateral corrosion damage to the device caused by the inability of the protective wall to block it.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present application relates to the technical field of resonator preparation, and in particular to a thin film bulk acoustic wave resonator and a preparation method thereof. Background Art

[0002] The ultra-high-speed development of wireless communication technology and the multifunctionality of communication terminals have put forward higher performance requirements for frequency devices working in the radio frequency band. Compared with traditional dielectric ceramic filters and SAW filters, film bulk acoustic wave resonators (FBARs) can work well in the range of several hundred MHz to 5-7 GHz. Especially in high-frequency applications, FBAR has a very large advantage. Therefore, FBAR occupies most of the application fields of wireless communications.

[0003] So far, thin film bulk acoustic wave resonators mainly include two types: back cavity thin film type and first cavity type resonator, and the production is mainly based on the first cavity type resonator. The existing preparation process of the first cavity type resonator is usually to etch a groove on the substrate to fill the sacrificial layer to form a protective wall, and then release the substrate material in the protective wall as the first cavity of the resonator. However, due to the difficulty of the chemical mechanical polishing process used to form the protective wall, the effect cannot be guaranteed. During the release process of the first cavity, there is a possibility that corrosive gas or corrosive liquid will leak laterally from above the protective wall, thereby causing lateral corrosion to damage the device. Summary of the invention

[0004] The purpose of the present application is to provide a thin film bulk acoustic wave resonator and a preparation method thereof to address the deficiencies in the above-mentioned prior art, which can prevent corrosive gas or corrosive liquid from leaking laterally from above the protective wall during the release process of the first cavity, thereby avoiding lateral corrosion damage to the device caused by the inability of the protective wall to block it.

[0005] To achieve the above purpose, the technical solution adopted in the embodiment of the present application is as follows:

[0006] According to one aspect of an embodiment of the present application, a thin film bulk acoustic wave resonator is provided, comprising: a base layer, a bottom electrode layer, a piezoelectric layer and a top electrode layer stacked in sequence on the base layer, a first cavity, a first protective wall and a second protective wall surrounding the first cavity are provided in the base layer, the second protective wall is located above the first protective wall, and the second protective wall is inclined from the first protective wall toward the first cavity.

[0007] Optionally, the second protective wall has a horizontal portion and a first inclined portion connected to an end of the horizontal portion, the horizontal portion is arranged in close contact with the first protective wall, and the first inclined portion is inclined from the first protective wall toward a direction close to the first cavity.

[0008] Optionally, the second protective wall further has a second inclined portion, the second inclined portion is connected to an end of the horizontal portion away from the first inclined portion, and the second inclined portion is inclined from the first protective wall toward a direction away from the first cavity.

[0009] Optionally, an acoustic reflection structure is provided between the bottom electrode layer and the piezoelectric layer, and the acoustic reflection structure is used to reflect sound waves.

[0010] Optionally, the base layer includes a substrate layer and a seed layer arranged on the substrate layer, the bottom electrode layer is located above the seed layer, the first protective wall is located in the substrate layer, the second protective wall is located in the substrate layer and the seed layer, and the substrate layer, the first protective wall, the second protective wall and the seed layer enclose a first cavity.

[0011] On the other hand, an embodiment of the present application provides a method for preparing a thin film bulk acoustic wave resonator, including: providing a substrate layer, and forming a first protective wall and a second protective wall in the substrate layer, wherein the second protective wall is located above the first protective wall, and at least a portion of the second protective wall is inclined from the first protective wall toward the inner side of the first protective wall; forming a bottom electrode layer, a piezoelectric layer and a top electrode layer in sequence on the substrate layer; forming a release hole above the substrate layer, wherein the bottom of the release hole extends to the substrate layer, and the top of the release hole is connected to the outside; and introducing a corrosive gas and / or a corrosive liquid into the release hole to remove the substrate layer in the first protective wall and the second protective wall.

[0012] Optionally, a base layer is provided, and a first protective wall and a second protective wall are formed in the base layer, wherein the second protective wall is located above the first protective wall, and at least a portion of the second protective wall is inclined from the first protective wall toward the inner side of the first protective wall. The method includes: providing a base layer, and forming a second groove on the surface of the base layer, wherein the longitudinal section of the second groove is an inverted trapezoid; forming a first groove at the bottom of the second groove, wherein the longitudinal section of the first groove is a rectangle; filling the first groove with protective material to form a first protective wall; and filling the second groove with protective material to form a second protective wall.

[0013] Optionally, providing a base layer, and forming a first protective wall and a second protective wall in the base layer, wherein the second protective wall is located above the first protective wall, and at least a portion of the second protective wall is inclined from the first protective wall to the inner side of the first protective wall, comprises: providing a substrate layer, and forming a second groove on the surface of the substrate layer, wherein the longitudinal section of the second groove is an inverted trapezoid; forming a first groove at the bottom of the second groove, wherein the longitudinal section of the first groove is a rectangle; filling the first groove with a protective material to form a first protective wall; forming a seed layer on the substrate layer and the first protective wall; etching the seed layer to Exposing the second groove; filling the second groove with protective material to form a second protective wall; forming a release hole above the base layer, wherein the bottom of the release hole extends to the base layer, and the top of the release hole is connected to the outside world, including: forming a release hole above the base layer, wherein the bottom of the release hole extends to the substrate layer, and the top of the release hole is connected to the outside world; introducing corrosive gas and / or corrosive liquid into the release hole to remove the base layer in the first protective wall and the second protective wall, including: introducing corrosive gas and / or corrosive liquid into the release hole to remove the substrate layer in the first protective wall and the second protective wall.

[0014] Optionally, filling the second trench with protective material to form a second protective wall includes: uniformly depositing the protective material on the surface of the seed layer and in the second trench to form a second protective layer, wherein the thickness of the second protective layer is equal to the thickness of the seed layer; etching the second protective layer to form a second protective wall in the second trench and the seed layer.

[0015] Optionally, forming a bottom electrode layer, a piezoelectric layer and a top electrode layer in sequence on the substrate layer includes: forming a bottom electrode layer on the seed layer, wherein the bottom electrode layer covers the second protective wall and forms a third groove above the second protective wall; filling the third groove with a sacrificial layer material to form a sacrificial layer, wherein the acoustic impedance of the sacrificial layer is not equal to the acoustic impedance of the bottom electrode layer; and forming a piezoelectric layer and a top electrode layer in sequence on the bottom electrode layer and the sacrificial layer.

[0016] Optionally, a release hole is formed above the base layer, wherein the bottom of the release hole extends to the substrate layer and the top of the release hole is connected to the outside world, including: forming a release hole above the base layer, wherein the release hole passes through the sacrificial layer and extends to the substrate layer, and the top of the release hole is connected to the outside world; introducing corrosive gas and / or corrosive liquid into the release hole to remove the substrate layer within the first protective wall and the second protective wall, including: introducing corrosive gas and / or corrosive liquid into the release hole to remove the sacrificial layer, and the substrate layer within the first protective wall and the second protective wall.

[0017] Optionally, forming a bottom electrode layer, a piezoelectric layer and a top electrode layer in sequence on the base layer includes: forming a bottom electrode layer on the base layer; forming a piezoelectric layer on the bottom electrode layer, and etching the piezoelectric layer to form a bottom electrode lead-out hole; forming a bottom electrode lead-out structure and a top electrode layer on the piezoelectric layer, wherein the bottom electrode lead-out structure fills the bottom electrode lead-out hole and is bonded to the bottom electrode; and forming metal electrode plates on the bottom electrode lead-out structure and the top electrode layer, respectively.

[0018] The beneficial effects of this application include:

[0019] The present application provides a thin film bulk acoustic wave resonator, comprising: a substrate layer, a bottom electrode layer, a piezoelectric layer and a top electrode layer stacked in sequence on the substrate layer, a first cavity, a first protective wall and a second protective wall surrounding the first cavity are arranged in the substrate layer, the second protective wall is located above the first protective wall, and the second protective wall is inclined from the first protective wall to the direction close to the first cavity. The thin film bulk acoustic wave resonator can prevent the corrosive gas or corrosive liquid from leaking laterally from above the protective wall during the release process of the first cavity by arranging the first protective wall and the inclined second protective wall in the substrate layer, thereby avoiding the lateral corrosion damage to the device caused by the inability of the protective wall to block it. BRIEF DESCRIPTION OF THE DRAWINGS

[0020] In order to more clearly illustrate the technical solutions of the embodiments of the present application, the drawings required for use in the embodiments will be briefly introduced below. It should be understood that the following drawings only show certain embodiments of the present application and therefore should not be regarded as limiting the scope. For ordinary technicians in this field, other related drawings can be obtained based on these drawings without paying creative work.

[0021] Figure 1 One of the structural schematic diagrams of the thin film bulk acoustic resonator provided in the embodiment of the present application;

[0022] Figure 2 The second structural schematic diagram of the thin film bulk acoustic wave resonator provided in the embodiment of the present application;

[0023] Figure 3 One of the flow charts of the method for preparing a thin film bulk acoustic wave resonator provided in an embodiment of the present application;

[0024] Figure 4 One of the schematic diagrams of the preparation process of the thin film bulk acoustic wave resonator provided in the embodiment of the present application;

[0025] Figure 5 The second schematic diagram of the preparation process of the thin film bulk acoustic wave resonator provided in the embodiment of the present application;

[0026] Figure 6 The third schematic diagram of the preparation process of the thin film bulk acoustic wave resonator provided in the embodiment of the present application;

[0027] Figure 7 The third structural diagram of the thin film bulk acoustic wave resonator provided in the embodiment of the present application;

[0028] Figure 8 Flow chart 2 of the method for preparing a thin film bulk acoustic wave resonator provided in an embodiment of the present application;

[0029] Fig. 9 A fourth schematic diagram of the preparation process of the thin film bulk acoustic wave resonator provided in an embodiment of the present application;

[0030] Fig.10 A fifth schematic diagram of the preparation process of the thin film bulk acoustic wave resonator provided in an embodiment of the present application;

[0031] Fig.11 Schematic diagram six of the preparation process of the thin film bulk acoustic wave resonator provided in the embodiment of the present application;

[0032] Fig.12 Schematic diagram of the preparation process of the thin film bulk acoustic wave resonator provided in the embodiment of the present application seven;

[0033] Fig.13 Schematic diagram eight of the preparation process of the thin film bulk acoustic wave resonator provided in an embodiment of the present application;

[0034] Fig.14 Flow chart three of the method for preparing a thin film bulk acoustic wave resonator provided in an embodiment of the present application;

[0035] Fig.15 Flow chart 4 of the method for preparing a thin film bulk acoustic wave resonator provided in an embodiment of the present application;

[0036] Fig.16 Flow chart 5 of the method for preparing a thin film bulk acoustic wave resonator provided in an embodiment of the present application;

[0037] Fig.17 A ninth schematic diagram of the preparation process of a thin film bulk acoustic wave resonator provided in an embodiment of the present application;

[0038] Fig.18 A tenth schematic diagram of the preparation process of the thin film bulk acoustic wave resonator provided in an embodiment of the present application;

[0039] Fig.19 11 is a schematic diagram of the preparation process of the thin film bulk acoustic wave resonator provided in an embodiment of the present application;

[0040] Fig. 20 A twelfth schematic diagram of the preparation process of the thin film bulk acoustic wave resonator provided in an embodiment of the present application;

[0041] Fig.21Thirteenth schematic diagram of the preparation process of the thin film bulk acoustic wave resonator provided in an embodiment of the present application;

[0042] Fig. 22 Flow chart six of the method for preparing a thin film bulk acoustic wave resonator provided in an embodiment of the present application;

[0043] Fig.23 Flow chart seven of the method for preparing a thin film bulk acoustic wave resonator provided in an embodiment of the present application.

[0044] Icon: 10-thin film bulk acoustic wave resonator; 11-base layer; 111-substrate layer; 1111-bottom silicon layer; 1112-buried oxide layer; 1113-top silicon layer; 112-seed layer; 113-second groove; 1131-first side wall; 1132-second side wall; 114-first groove; 12-bottom electrode layer; 121-third groove; 13-piezoelectric layer; 131-bottom electrode lead-out hole; 14-top electrode layer; 151-first cavity; 152-second cavity; 161-first protective wall; 162-second protective wall; 17-release hole; 18-sacrificial layer; 19-bottom electrode lead-out structure; 20-metal electrode plate. DETAILED DESCRIPTION

[0045] In order to make the purpose, technical solution and advantages of the embodiments of the present application clearer, the technical solution in the embodiments of the present application will be clearly and completely described below in conjunction with the drawings in the embodiments of the present application. Obviously, the described embodiments are part of the embodiments of the present application, rather than all the embodiments. The components of the embodiments of the present application described and shown in the drawings here can be arranged and designed in various different configurations.

[0046] It should be understood that although the terms first, second, etc. can be used to describe various elements in this article, these elements should not be limited by these terms. These terms are only used to divide an element from another element. For example, without departing from the scope of the present disclosure, the first element can be referred to as the second element, and similarly, the second element can be referred to as the first element. As used herein, the term "and / or" includes any and all combinations of one or more of the associated listed items.

[0047] It should be understood that when an element (such as a layer, region or substrate) is referred to as "on another element" or "extending onto another element", it can be directly on another element or directly extended onto another element, or there can also be an intervening element. On the contrary, when an element is referred to as "directly on another element" or "directly extending onto another element", there is no intervening element. Similarly, it should be understood that when an element (such as a layer, region or substrate) is referred to as "on another element" or "extending onto another element", it can be directly on another element or directly extended onto another element, or there can also be an intervening element. On the contrary, when an element is referred to as "directly on another element" or "extending directly onto another element", there is no intervening element. It should also be understood that when an element is referred to as "connected" or "coupled" to another element, it can be directly connected or coupled to another element, or there can be an intervening element. On the contrary, when an element is referred to as "directly connected" or "directly coupled" to another element, there is no intervening element.

[0048] Unless otherwise defined, all terms (including technical and scientific terms) used herein have the same meaning as those commonly understood by those skilled in the art to which the present disclosure belongs. It should also be understood that the terms used herein should be interpreted as having the same meaning as they do in the context of this specification and the relevant art, and should not be interpreted in an idealized or overly formal sense, unless clearly defined in this article.

[0049] In one aspect of the embodiment of the present application, referring to Figure 1 A thin film bulk acoustic wave resonator 10 is provided, comprising: a substrate layer 11, a bottom electrode layer 12, a piezoelectric layer 13 and a top electrode layer 14 stacked in sequence on the substrate layer 11, a first cavity 151, a first protective wall 161 and a second protective wall 162 surrounding the first cavity 151 are provided in the substrate layer 11, the second protective wall 162 is located above the first protective wall 161, and the second protective wall 162 is inclined from the first protective wall 161 to a direction close to the first cavity 151.

[0050] The base layer 11 is used as a supporting structure, and is mainly used to sequentially form a bottom electrode layer 12, a piezoelectric layer 13, and a top electrode layer 14 thereon. A first cavity 151 is provided inside the base layer 11, and the top of the first cavity 151 may be directly in contact with the bottom electrode layer 12 or may not be in contact with the bottom electrode layer 12. The area where the orthographic projections of the bottom electrode layer 12, the piezoelectric layer 13, and the top electrode layer 14 overlap at the bottom of the first cavity 151 together constitutes the effective area of ​​the thin film bulk acoustic wave resonator 10, and the bulk acoustic wave is formed in the effective area and reflected back and forth in the effective area to form an oscillation.

[0051] The formation of the first cavity 151 on the substrate 11 requires the release of part of the substrate 11 material. The release method is to process the release hole 17 on the thin film bulk acoustic wave resonator 10 so that the release hole 17 extends all the way to the surface or the inside of the substrate 11, and then introduce a corrosive gas or a corrosive liquid into the release hole 17 to corrode and dissolve the substrate 11 material. In order to define the boundary of the first cavity 151 and prevent the leakage of the corrosive gas or the corrosive liquid, a first protective wall 161 and a second protective wall 162 are also provided in the substrate 11, and the lower surface of the second protective wall 162 is connected to the upper surface of the first protective wall 161. The first protective wall 161 and the second protective wall 162 are annular, and the substrate 11 material in the enclosed area formed by the two is used to release to form the first cavity 151. After the first cavity 151 is formed, the first protective wall 161 and the second protective wall 162 are both arranged around the first cavity 151, wherein at least a portion of the second protective wall 162 is arranged obliquely relative to the stacking direction of each film layer, and the oblique direction is gradually approaching the first cavity 151 from bottom to top, so that the top of the first cavity 151 shows a shrinking trend. The structure of the first protective wall 161 and the second protective wall 162 can prevent the corrosive gas or corrosive liquid from leaking laterally from above the protective wall during the release process of the first cavity 151, thereby avoiding lateral corrosion damage to the device caused by the inability of the protective wall to block it.

[0052] Optionally, in one achievable method of an embodiment of the present application, the second protective wall 162 has a horizontal portion and a first inclined portion connected to the end of the horizontal portion, the horizontal portion is arranged in close contact with the first protective wall 161, and the first inclined portion is inclined from the first protective wall 161 toward a direction close to the first cavity 151.

[0053] The second protection wall 162 is connected to the first protection wall 161 through the horizontal portion, thereby forming a continuous protection wall to prevent the corrosion gas or liquid from leaking between the first protection wall 161 and the second protection wall 162. At the same time, the horizontal portion of the second protection wall 162 also provides support for the first inclined portion, so that the first inclined portion can be inclined from bottom to top toward the direction where the first cavity 151 is located.

[0054] Optionally, in one achievable method of an embodiment of the present application, the second protective wall 162 also has a second inclined portion, the second inclined portion is connected to an end of the horizontal portion away from the first inclined portion, and the second inclined portion is inclined from the first protective wall 161 in a direction away from the first cavity 151.

[0055] The second inclined portion and the first inclined portion are respectively inclined upward from the ends of the horizontal portion and gradually move away from each other. This arrangement can make the second protective wall 162 easier to process, and can also form a bridge structure in the subsequent process of forming a resonator sandwich structure to reflect sound waves, thereby improving the performance and quality factor of the thin film bulk acoustic wave resonator 10.

[0056] Optionally, in an achievable manner of the embodiment of the present application, the base layer 11 includes a substrate layer 111 and a seed layer 112 disposed on the substrate layer 111, the bottom electrode layer 12 is located above the seed layer 112, the first protective wall 161 is located in the substrate layer 111, the second protective wall 162 is located in the substrate layer 111 and the seed layer 112, and the substrate layer 111, the first protective wall 161, the second protective wall 162 and the seed layer 112 enclose a first cavity 151. The seed layer 112 can induce the crystal growth of the bottom electrode layer 12 and the piezoelectric layer 13 in the vertical direction, so that the bottom electrode layer 12 and the piezoelectric layer 13 form a good crystal orientation, thereby improving the film quality of the bottom electrode layer 12 and the piezoelectric layer 13, and optimizing the performance of the thin film bulk acoustic resonator 10.

[0057] Furthermore, the seed layer 112 has a middle portion and a peripheral portion surrounding the middle portion and separated from the middle portion, the second protective wall 162 has a first inclined portion, a horizontal portion, and a second inclined portion connected in sequence, the first inclined portion is connected to the middle portion, the second inclined portion is connected to the peripheral portion, and the middle portion and the peripheral portion are connected through the second protective wall 162. Preferably, the thickness of the second protective wall 162 and the seed layer 112 is uniform, and the thickness of the second protective wall 162 is equal to the thickness of the seed layer 112. In this way, there is no step at the connection between the second protective wall 162 and the seed layer 112, thereby preventing the subsequent formed film from being broken.

[0058] Optionally, in one implementable manner of the embodiment of the present application, an acoustic reflection structure is provided between the bottom electrode layer 12 and the piezoelectric layer 13 , and the acoustic reflection structure is used to reflect sound waves.

[0059] Please refer to Figure 2 The acoustic reflection structure can be a second cavity 152 formed between the bottom electrode layer 12 and the piezoelectric layer 13, or a sacrificial layer 18 sandwiched between the bottom electrode layer 12 and the piezoelectric layer 13. The difference in acoustic impedance between the air or the sacrificial layer 18 and the surrounding materials is utilized to reflect the acoustic waves, thereby improving the performance and quality factor of the thin film bulk acoustic resonator 10.

[0060] Optionally, in one implementable manner of an embodiment of the present application, the thin film bulk acoustic wave resonator 10 also includes a release hole 17, which extends along the stacking direction of each film layer, and the top of the release hole 17 is located on the upper surface of the top electrode layer 14, and the bottom is located on the upper surface of the substrate layer 11 or the middle of the substrate layer 11, and the orthographic projection of the release hole 17 on the substrate layer 11 is located within the inner boundary of the orthographic projection of the second protective wall 162 on the substrate layer 11, and the release hole 17 is used to release the substrate layer 11 material surrounding the first protective cavity and the second protective wall 162.

[0061] Optionally, in an achievable manner of an embodiment of the present application, the base layer 11 includes a bottom silicon layer 1111, a buried oxide layer 1112 and a top silicon layer 1113 stacked in sequence on the bottom silicon layer 1111, and a first protective wall 161 and a second protective wall 162 are arranged in the top silicon layer 1113 and penetrate the upper and lower surfaces of the top silicon layer 1113 together. The top silicon layer 1113 material inside the first protective wall 161 and the second protective wall 162 is released to form a cavity. At this time, the first protective wall 161 and the second protective wall 162 define the side boundaries of the cavity, the buried oxide layer 1112 defines the bottom boundary of the cavity, and the film layer covering the top silicon layer 1113 defines the top boundary of the cavity.

[0062] Preferably, the material of the top silicon layer 1113 is Si (111) with a thickness of 1 μm to 2.5 μm, so as to grow a film layer structure with better quality in subsequent processes.

[0063] Optionally, in one achievable method of an embodiment of the present application, a bottom electrode lead-out hole 131 is provided on the piezoelectric layer 13, and a conductive material is filled in the bottom electrode lead-out hole 131 to form a bottom electrode lead-out structure 19, and the bottom electrode lead-out structure 19 is bonded to the bottom electrode, thereby leading the bottom electrode out from under the piezoelectric layer 13.

[0064] Furthermore, metal electrode plates 20 are provided on the upper surfaces of the bottom electrode lead-out structure 19 and the top electrode layer 14, respectively. The metal electrode plates 20 can reduce resistance and electrode loss, facilitate device testing, and be used in subsequent packaging processes.

[0065] Please refer to Figure 3 This embodiment also provides a method for preparing a thin film bulk acoustic wave resonator, comprising:

[0066] S100: providing a base layer, and forming a first protection wall and a second protection wall in the base layer, wherein the second protection wall is located above the first protection wall, and at least a portion of the second protection wall is inclined from the first protection wall toward the inner side of the first protection wall.

[0067] Please note that, please refer to Figure 4 , the inner side of the first protective wall 161 refers to the direction of the area enclosed by the first protective wall 161. In this embodiment, the structures of the first protective wall 161 and the second protective wall 162 are not limited, as long as a vertical first protective wall 161 and an inclined second protective wall 162 can be formed in the base layer 11.

[0068] S200: forming a bottom electrode layer, a piezoelectric layer and a top electrode layer in sequence on the substrate layer.

[0069] Please refer to Figure 5In order to subsequently form an effective resonance region of the thin film bulk acoustic wave resonator 10, the bottom electrode layer 12, the piezoelectric layer 13 and the top electrode layer 14 should have a three-layer overlap region in the stacking direction, that is, form a sandwich structure.

[0070] S300: forming a release hole above the base layer, wherein the bottom of the release hole extends to the base layer, and the top of the release hole is connected to the outside.

[0071] Please refer to Figure 6 After forming the top electrode layer 14, it is necessary to form a release hole 17 on the top of the base layer 11. The bottom of the release hole 17 extends to the upper surface or the middle of the base layer 11, and the top of the release hole 17 is connected to the outside to facilitate the introduction of the corrosive gas and / or the corrosive liquid into the release hole 17. For example, the top of the release hole 17 is located on the top electrode layer 14, that is, the release hole 17 is formed by processing the upper surface of the top electrode layer 14 as the processing surface. In other embodiments, please refer to Figure 7 The top of the release hole 17 may also be located on the piezoelectric layer 13, that is, the release hole 17 is formed by processing the upper surface of the piezoelectric layer 13 as the processing surface. The number of the release hole 17 may be one, or two or more.

[0072] S400: Introducing a corrosive gas and / or a corrosive liquid into the release hole to remove the base layer in the first protective wall and the second protective wall.

[0073] Please refer to Figure 1 , a corrosive gas and / or a corrosive liquid is introduced into the release hole 17 to corrode and dissolve the material of the base layer 11 in the first protective wall 161 and the second protective wall 162, and a portion of the base layer 11 is removed, thereby forming a first cavity 151 for reflecting sound waves inside the first protective wall 161 and the second protective wall 162.

[0074] The above-mentioned method for preparing the thin film bulk acoustic wave resonator forms a vertical first protective wall 161 and an inclined second protective wall 162 in the base layer 11, thereby preventing the corrosive gas or corrosive liquid from leaking laterally from above the protective wall during the release of the first cavity 151, thereby avoiding lateral corrosion that cannot be blocked by the protective wall to damage the device.

[0075] Optionally, in one possible implementation of the present application, please refer to Figure 8 , providing a base layer, and forming a first protection wall and a second protection wall in the base layer, wherein the second protection wall is located above the first protection wall, and at least a portion of the second protection wall is inclined from the first protection wall to the inner side of the first protection wall, including:

[0076] S110: providing a base layer, and forming a second groove on a surface of the base layer, wherein a longitudinal section of the second groove is in an inverted trapezoidal shape.

[0077] Please refer to Fig. 9 , a second annular groove 113 is formed on the upper surface of the base layer 11, and the second groove 113 is used to form a second protective wall 162 in a subsequent process. The longitudinal section of the second groove 113 parallel to the stacking direction is an inverted trapezoid, and the second groove 113 has a first side wall 1131 and a second side wall 1132 surrounding the first side wall 1131, wherein the first side wall 1131 is inclined, and the second side wall 1132 can be inclined or vertical. When processing the second groove 113, the etching angle can be controlled by photolithography and etching, thereby forming the slope of the side wall of the second groove 113.

[0078] S120: forming a first groove at the bottom of the second groove, wherein a longitudinal section of the first groove is rectangular.

[0079] Please refer to Fig.10 The second groove 113 also has a groove bottom connecting the first side wall 1131 and the second side wall 1132. An annular first groove 114 is formed at the groove bottom of the second groove 113. The first groove 114 is used to form a first protection wall 161 in a subsequent process. The longitudinal section of the first groove 114 parallel to the stacking direction is rectangular. Preferably, the width of the first groove 114 is equal to the width of the groove bottom of the second groove 113.

[0080] S130: Filling the first trench with a protective material to form a first protective wall.

[0081] S140: Filling the second trench with a protective material to form a second protective wall.

[0082] Please refer to Figures 11 to 13 , Figure 4 , respectively fill the first trench 114 and the second trench 113 with protective materials (such as silicon dioxide) to form a first protective wall 161 and a second protective wall 162. In this embodiment, a trench is first formed on the base layer 11, and then the corresponding protective wall is formed by filling the trench, which is simple and convenient to operate.

[0083] Optionally, in one possible implementation of the present application, please refer to Fig.14 , providing a base layer, and forming a first protection wall and a second protection wall in the base layer, wherein the second protection wall is located above the first protection wall, and at least a portion of the second protection wall is inclined from the first protection wall to the inner side of the first protection wall, including:

[0084] S150: providing a substrate layer, and forming a second groove on a surface of the substrate layer, wherein a longitudinal section of the second groove is in an inverted trapezoidal shape.

[0085] S120: forming a first groove at the bottom of the second groove, wherein a longitudinal section of the first groove is rectangular.

[0086] S130: Filling the first trench with a protective material to form a first protective wall.

[0087] S160: forming a seed layer on the substrate layer and the first protective wall.

[0088] S170: etching the seed layer to expose the second trench.

[0089] S140: Filling the second trench with a protective material to form a second protective wall.

[0090] In this embodiment, the base layer 11 includes a substrate layer 111 and a seed layer 112. Figures 9 to 11 After forming the second trench 113 and the first trench 114 in the substrate layer 111, the first trench 114 is first filled with a protective material (for example, by deposition), and then the excess protective material outside the first trench 114 is removed, thereby forming a first protective wall 161 in the first trench 114 with the same shape as the first trench 114. Fig.12 After the first protective wall 161 is formed, a seed layer 112 is first prepared, and the seed layer 112 covers the upper surface of the substrate layer 111 and the first protective wall 161. The seed layer 112 can be formed by growing high-quality single-crystal aluminum nitride using organic metal chemical vapor deposition (MOCVD) technology. The provision of the seed layer 112 can induce the crystal growth of the bottom electrode layer 12 and the piezoelectric layer 13 in the vertical direction, so that the bottom electrode layer 12 and the piezoelectric layer 13 form a good crystal orientation, thereby improving the film quality of the bottom electrode layer 12 and the piezoelectric layer 13, and optimizing the performance of the thin film bulk acoustic wave resonator 10. Please refer to Fig.13 After the seed layer 112 is formed, the second trench 113 is covered. Therefore, the seed layer 112 needs to be etched to remove part of the seed layer 112 so that the second trench 113 is exposed again to prepare for subsequent filling of the protective material. Figure 4 After the second trench 113 is completely exposed, a protective material is filled into the second trench 113 (for example, by deposition), thereby forming a second protective wall 162 .

[0091] Illustratively, the substrate layer 111 includes a bottom silicon layer 1111 , a buried oxide layer 1112 and a top silicon layer 1113 sequentially stacked on the bottom silicon layer 1111 , and the second trench 113 and the first trench 114 are formed in the top silicon layer 1113 of the substrate layer 111 .

[0092] A release hole is formed above the base layer, wherein the bottom of the release hole extends to the base layer and the top of the release hole is connected to the outside world, including:

[0093] S310: forming a release hole above the base layer, wherein the bottom of the release hole extends to the substrate layer, and the top of the release hole is connected to the outside.

[0094] Introducing a corrosive gas and / or a corrosive liquid into the release hole to remove the base layer in the first protective wall and the second protective wall comprises:

[0095] S410: Introduce a corrosive gas and / or a corrosive liquid into the release hole to remove the substrate layer in the first protective wall and the second protective wall.

[0096] Please refer to Figure 6 and Figure 1 Since the first protection wall 161 and the second protection wall 162 are both formed on the substrate layer 111 , the bottom of the release hole 17 needs to extend to the upper surface or the inside of the substrate layer 111 , so as to corrode and remove part of the substrate layer 111 to form the first cavity 151 .

[0097] Optionally, in one possible implementation of the present application, please refer to Fig.15 Filling the second trench with a protective material to form a second protective wall includes:

[0098] S141: uniformly depositing a protective material on the surface of the seed layer and in the second groove to form a second protective layer, wherein the thickness of the second protective layer is equal to the thickness of the seed layer.

[0099] S142: Etching the second protection layer to form a second protection wall in the second trench and the seed layer.

[0100] Please refer to Fig.13 and Figure 4 , uniformly deposit the protective material, and remove the excess protective material, thereby forming a second protective wall 162 in the second groove 113 and the seed layer 112. The thickness of the second protective wall 162 is equal to the thickness of the seed layer 112, so that there is no step at the connection position between the second protective wall 162 and the seed layer 112, which is conducive to the subsequent growth of the thin film. At the same time, since the thickness of the second protective wall 162 is uniform, the upper surface of the second protective wall 162 is recessed in the direction of the first protective wall 161. When the bottom electrode layer 12 is subsequently formed, this feature can be replicated on the upper surface of the bottom electrode layer 12, thereby forming an acoustic reflection structure at the recessed position.

[0101] Optionally, in one possible implementation of the present application, please refer to Fig.16 , sequentially forming a bottom electrode layer, a piezoelectric layer and a top electrode layer on the substrate layer comprises:

[0102] S210: forming a bottom electrode layer on the seed layer, wherein the bottom electrode layer covers the second protection wall and forms a third trench above the second protection wall.

[0103] Please refer to Fig.17For example, a bottom electrode material is uniformly deposited on the seed layer 112, and excess bottom electrode material is removed by etching to form a bottom electrode layer 12. Since the bottom electrode material is uniformly deposited, the depression on the upper surface of the second protection wall 162 can be directly replicated on the bottom electrode layer 12 to form a third groove 121.

[0104] S220: Filling a sacrificial layer material into the third trench to form a sacrificial layer, wherein the acoustic impedance of the sacrificial layer is not equal to the acoustic impedance of the bottom electrode layer.

[0105] Please refer to Fig.18 , fill the third groove 121 with sacrificial layer 18 material, thereby forming a sacrificial layer 18 of a bridge structure in the third groove 121. The acoustic impedance of the sacrificial layer 18 is not equal to the acoustic impedance of the bottom electrode layer 12, so it can suppress the lateral leakage of the acoustic wave energy. The upper surface of the sacrificial layer 18 can be flush with the upper surface of the substrate layer 111, or it can protrude from the upper surface of the substrate layer 111, thereby forming an upward convex structure. When depositing the sacrificial layer 18, the structure of the sacrificial layer 18 can be achieved by controlling the deposition thickness. Please refer to Figure 1 After forming the piezoelectric layer 13 and the top electrode layer 14, the sacrificial layer 18 can also be removed to form a second cavity 152 at the position of the third groove 121. By utilizing the fact that the acoustic impedance of air is unequal to that of the bottom electrode layer 12, the lateral leakage of the acoustic wave energy can also be suppressed.

[0106] S230: forming a piezoelectric layer and a top electrode layer in sequence on the bottom electrode layer and the sacrificial layer.

[0107] Please refer to Figures 19 to 21 After the sacrificial layer 18 is formed, the piezoelectric layer 13 and the top electrode layer 14 can be formed. For example, a piezoelectric material is uniformly deposited on the bottom electrode layer 12 to form the piezoelectric layer 13. Furthermore, a high-quality single-crystal aluminum nitride is grown on the surface of the bottom electrode layer 12 by using an organic metal chemical vapor deposition (MOCVD) technique to form the piezoelectric layer 13, or a piezoelectric material (such as aluminum nitride, scandium-doped aluminum nitride, etc.) is grown on the surface of the bottom electrode layer 12 by other methods.

[0108] For example, a top electrode material is uniformly deposited on the piezoelectric layer 13 , and excess top electrode material is removed by etching, thereby forming the top electrode layer 14 .

[0109] Optionally, in one possible implementation of the present application, please refer to Fig. 22 , forming a release hole above the base layer, wherein the bottom of the release hole extends to the substrate layer, and the top of the release hole is connected to the outside world, including:

[0110] S320: forming a release hole above the base layer, wherein the release hole passes through the sacrificial layer and extends to the substrate layer, and the top of the release hole is connected to the outside.

[0111] Introducing a corrosive gas and / or a corrosive liquid into the release hole to remove the substrate layer in the first protective wall and the second protective wall comprises:

[0112] S420: Introduce a corrosive gas and / or a corrosive liquid into the release hole to remove the sacrificial layer and the substrate layer in the first protection wall and the second protection wall.

[0113] Please refer to Figure 2 The release hole 17 passes through the sacrificial layer 18 and the substrate layer 111 located within the first protective wall 161 and the second protective wall 162, and a corrosive gas and / or corrosive liquid is introduced into the release hole 17, so that a second cavity 152 can be formed at the position of the sacrificial layer 18, and a first cavity 151 is formed in the first protective wall 161 and the second protective wall 162 at the same time.

[0114] Optionally, in one possible implementation of the present application, please refer to Fig.23 , sequentially forming a bottom electrode layer, a piezoelectric layer and a top electrode layer on the substrate layer comprises:

[0115] S240: forming a bottom electrode layer on the base layer.

[0116] S250: forming a piezoelectric layer on the bottom electrode layer, and etching the piezoelectric layer to form a bottom electrode lead-out hole.

[0117] S260: forming a bottom electrode lead-out structure and a top electrode layer on the piezoelectric layer, wherein the bottom electrode lead-out structure fills the bottom electrode lead-out hole and is bonded to the bottom electrode.

[0118] S270: forming metal electrode plates on the bottom electrode lead-out structure and the top electrode layer respectively.

[0119] Please refer to Fig. 20 , Fig.21 and Figure 5 For example, a top electrode material is deposited on the piezoelectric layer 13, and the top electrode material naturally fills the bottom electrode lead-out hole 131. A portion of the top electrode material is removed by etching, thereby simultaneously forming a bottom electrode lead-out structure 19 and a top electrode layer 14. The bottom electrode lead-out structure 19 is used to lead the bottom electrode layer 12 out from under the piezoelectric layer 13. Then, metal electrode plates 20 are formed on the upper surfaces of the bottom electrode lead-out structure 19 and the top electrode, respectively, and the metal electrode plates 20 are used to transfer electrons and cooperate to form an alternating electric field. The metal electrode plate 20 can be formed by a photolithography-deposition-stripping method, or by a deposition-photolithography-etching method.

[0120] The above description is only the preferred embodiment of the present application and is not intended to limit the present application. For those skilled in the art, the present application may have various modifications and variations. Any modification, equivalent replacement, improvement, etc. made within the spirit and principle of the present application shall be included in the protection scope of the present application.

Claims

1. A thin film bulk acoustic resonator, characterized in that: include: A base layer, a bottom electrode layer, a piezoelectric layer and a top electrode layer stacked in sequence on the base layer, wherein a first cavity is provided in the base layer, and a first protection wall and a second protection wall surrounding the first cavity, the second protection wall is located above the first protection wall, and the second protection wall is inclined from the first protection wall toward the first cavity; A second cavity is formed between the bottom electrode layer and the piezoelectric layer, and the second cavity is located above the second protective wall.

2. The thin film bulk acoustic wave resonator according to claim 1, characterized in that The second protection wall comprises a horizontal portion and a first inclined portion connected to an end of the horizontal portion. The horizontal portion is arranged in close contact with the first protection wall. The first inclined portion is inclined from the first protection wall toward the first cavity.

3. The thin film bulk acoustic wave resonator according to claim 2, characterized in that: The second protection wall further has a second inclined portion, which is connected to an end of the horizontal portion away from the first inclined portion, and the second inclined portion is inclined from the first protection wall toward a direction away from the first cavity.

4. The thin film bulk acoustic wave resonator according to claim 1, characterized in that: The base layer includes a substrate layer and a seed layer arranged on the substrate layer, the bottom electrode layer is located above the seed layer, the first protective wall is located in the substrate layer, the second protective wall is located in the substrate layer and the seed layer, and the substrate layer, the first protective wall, the second protective wall and the seed layer enclose to form the first cavity.

5. A method for preparing a thin film bulk acoustic wave resonator, characterized in that: include: Providing a base layer, and forming a first protection wall and a second protection wall in the base layer, wherein the second protection wall is located above the first protection wall, and at least a portion of the second protection wall is inclined from the first protection wall to the inner side of the first protection wall; forming a bottom electrode layer on the base layer, wherein the bottom electrode layer covers the second protection wall, and forming a third groove above the second protection wall; Filling a sacrificial layer material into the third groove to form a sacrificial layer, wherein the acoustic impedance of the sacrificial layer is not equal to the acoustic impedance of the bottom electrode layer; forming a piezoelectric layer and a top electrode layer on the bottom electrode layer and the sacrificial layer in sequence; forming a release hole above the base layer, wherein the bottom of the release hole extends to the base layer, and the top of the release hole is connected to the outside; Corrosive gas and / or corrosive liquid is introduced into the release hole to remove the base layer in the first protective wall and the second protective wall.

6. The method for preparing a thin film bulk acoustic wave resonator according to claim 5, characterized in that: The step of providing a base layer and forming a first protection wall and a second protection wall in the base layer, wherein the second protection wall is located above the first protection wall, and at least a portion of the second protection wall is inclined from the first protection wall toward the inner side of the first protection wall, comprises: Providing a base layer, and forming a second groove on a surface of the base layer, wherein a longitudinal section of the second groove is in an inverted trapezoidal shape; A first groove is formed at the groove bottom of the second groove, wherein the longitudinal section of the first groove is rectangular; Filling the first trench with a protective material to form a first protective wall; The second trench is filled with the protection material to form a second protection wall.

7. The method for preparing a thin film bulk acoustic wave resonator according to claim 5, characterized in that: The step of providing a base layer and forming a first protection wall and a second protection wall in the base layer, wherein the second protection wall is located above the first protection wall, and at least a portion of the second protection wall is inclined from the first protection wall toward the inner side of the first protection wall, comprises: Providing a substrate layer, and forming a second groove on a surface of the substrate layer, wherein a longitudinal section of the second groove is in an inverted trapezoidal shape; A first groove is formed at the groove bottom of the second groove, wherein the longitudinal section of the first groove is rectangular; Filling the first trench with a protective material to form a first protective wall; forming a seed layer on the substrate layer and the first protective wall; etching the seed layer to expose the second groove; Filling the second trench with the protective material to form a second protective wall; The step of forming a release hole above the base layer, wherein the bottom of the release hole extends to the base layer and the top of the release hole is connected to the outside world, comprises: forming a release hole above the base layer, wherein the bottom of the release hole extends to the substrate layer, and the top of the release hole is connected to the outside; The step of introducing a corrosive gas and / or a corrosive liquid into the release hole to remove the base layer in the first protective wall and the second protective wall comprises: Corrosive gas and / or corrosive liquid is introduced into the release hole to remove the substrate layer in the first protection wall and the second protection wall.

8. The method for preparing a thin film bulk acoustic wave resonator according to claim 7, characterized in that: Filling the second trench with the protective material to form a second protective wall comprises: Uniformly depositing the protective material on the surface of the seed layer and in the second groove to form a second protective layer, wherein the thickness of the second protective layer is equal to the thickness of the seed layer; The second protection layer is etched to form a second protection wall in the second trench and the seed layer.

9. The method for preparing a thin film bulk acoustic wave resonator according to claim 8, characterized in that: The sequentially forming a bottom electrode layer, a piezoelectric layer and a top electrode layer on the substrate layer comprises: forming a bottom electrode layer on the seed layer, wherein the bottom electrode layer covers the second protection wall and forms a third groove above the second protection wall; Filling a sacrificial layer material into the third groove to form a sacrificial layer, wherein the acoustic impedance of the sacrificial layer is not equal to the acoustic impedance of the bottom electrode layer; A piezoelectric layer and a top electrode layer are sequentially formed on the bottom electrode layer and the sacrificial layer.

10. The method for preparing a thin film bulk acoustic wave resonator according to claim 9, characterized in that: Forming a release hole above the base layer, wherein the bottom of the release hole extends to the substrate layer and the top of the release hole is connected to the outside world comprises: forming a release hole above the base layer, wherein the release hole passes through the sacrificial layer and extends to the substrate layer, and the top of the release hole is connected to the outside; Introducing a corrosive gas and / or a corrosive liquid into the release hole to remove the substrate layer in the first protective wall and the second protective wall comprises: Corrosive gas and / or corrosive liquid is introduced into the release hole to remove the sacrificial layer and the substrate layer within the first protection wall and the second protection wall.

11. The method for preparing a thin film bulk acoustic wave resonator according to claim 5, characterized in that: The sequentially forming a bottom electrode layer, a piezoelectric layer and a top electrode layer on the substrate layer comprises: forming a bottom electrode layer on the base layer; forming a piezoelectric layer on the bottom electrode layer, and etching the piezoelectric layer to form a bottom electrode lead-out hole; forming a bottom electrode lead-out structure and a top electrode layer on the piezoelectric layer, wherein the bottom electrode lead-out structure fills the bottom electrode lead-out hole and is bonded to the bottom electrode; Metal electrode plates are formed on the bottom electrode lead-out structure and the top electrode layer, respectively.