A quantitative deposition method for GTAW arc additive manufacturing
By using a quantitative deposition method that controls the amount of filler wire, droplet transfer, and welding speed, the problem of unstable material deposition in GTAW additive manufacturing was solved, thereby improving welding quality and weld uniformity.
Patent Information
- Application Number
- CN202410457995.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2024-04-16
- Publication Date
- 2026-11-10
- Estimated Expiration
- 2044-04-16
AI Technical Summary
In GTAW additive manufacturing, unstable material deposition leads to problems such as collapse, overflow, and uneven weld beads, and there is a lack of effective control methods.
By controlling the filler wire amount, droplet transfer, and welding speed, a quantitative deposition control method and system are adopted, including a quantitative deposition control center, a filler wire system, and a filler wire height adjustment mechanism, to achieve quantitative deposition control of the GTAW arc additive manufacturing process.
It improves welding quality, solves the problem of unstable material deposition, reduces collapse and overflow, and ensures weld uniformity.
Smart Images

Figure CN118204599B_ABST
Abstract
Description
Technical Field
[0001] This invention relates to the field of GTAW (Ground-Touch Aluminum Arc Additive Manufacturing) and is a quantitative deposition method for GTAW. Technical Background
[0002] Additive manufacturing is widely used in aerospace, medical, and manufacturing industries due to its economic efficiency and flexibility. GTAW (Ground-Tracked Aluminum Additive Manufacturing) based on filler wire improves the stability of the additive manufacturing process and the quality performance of the products. However, in GTAW additive manufacturing, unstable material deposition can lead to defects such as collapse and overflow, as well as uneven weld beads. Currently, there is no method for controlling the amount of metal deposited during the GTAW additive manufacturing process. To address the problem of unstable material deposition in GTAW additive manufacturing, this invention discloses a quantitative deposition method for GTAW arc additive manufacturing. By controlling the filler wire amount, droplet transfer, and welding speed during the GTAW arc additive manufacturing process, quantitative deposition control is achieved, thereby improving weld quality. Summary of the Invention
[0003] like Figure 1 As shown, a quantitative deposition method for GTAW (Glass Wire Arcade) additive manufacturing is disclosed, used to control the amount of material deposited during the GTAW process. The method is characterized by comprising a quantitative deposition control method and a quantitative deposition control system. The quantitative deposition control method includes a filler wire amount control method, a droplet transfer control method, and a welding speed control method. The filler wire amount is controlled using the filler wire amount control method, the droplet transfer control method is controlled using the droplet transfer control method, and the welding speed control method is controlled using the welding speed control method. The quantitative deposition control system includes a quantitative deposition control center, a filler wire system, and a filler wire height adjustment mechanism. Figure 2 As shown, the wire feeding system includes a wire feeder, a wire guide tube, a clamping device, and a filling nozzle. The wire feeder includes a wire feed reel and a central shaft. The wire feed reel is used to hold the welding wire roll. The wire feed reel is driven to rotate and feed the welding wire out. The wire guide tube is used to guide the fed welding wire to a specific position. The clamping device is used to clamp the filling nozzle to fix the welding wire filling position and angle. The filling nozzle feeds the welding wire into the welding position.
[0004] The quantitative deposition control center receives wire feed tray quality data and preset input data, processes the wire feed tray quality data and preset input data, and outputs wire filler height adjustment control signals, wire feed speed adjustment control signals, and welding torch movement control signals. The quantitative deposition control center also receives preset target deposition amount data. and actual wire feed data The received data is processed according to the quantitative deposition control method, and then outputs a wire feed speed adjustment control signal and a wire filling height adjustment control signal to control the wire filling system and the wire filling height adjustment mechanism. The wire filling system adjusts the wire feed speed according to the wire feed speed adjustment control signal to change the actual wire feed amount. The filler height adjustment mechanism changes the filler height according to the filler height adjustment control signal. The aforementioned filler wire height This refers to the vertical distance between the tip of the welding wire fed into the welding position and the substrate.
[0005] The quantitative deposition method for GTAW arc additive manufacturing is characterized in that: the filler wire amount control method is based on the target deposition amount. and actual wire feed To correct the deviation, adjust the wire feeding speed. This results in the actual wire feeding amount Equal to the target deposition amount, that is, when When, decrease ;when At that time, increase ;when At that time, keep Unchanged; the target deposition amount The desired wire deposition quality is preset; the actual wire feed rate is... To ensure the actual quality of the welding wire fed by the wire feeding system, a quality monitoring device is installed inside the central shaft of the wire feeding reel. This quality monitoring device acquires the quality data of the wire feeding reel in real time. The data is then transmitted to the quantitative deposition control center, which uses the wire feed tray quality data for analysis. The actual wire feed amount is calculated from the changes. .
[0006] The quantitative deposition method for GTAW arc additive manufacturing is characterized by the following conditions for droplet transition: the droplet grows to contact the molten pool, the droplet is approximately spherical during growth, and the diameter of the sphere is [missing information] when the droplet contacts the molten pool. equal to filler wire height The volume of the deposited droplet is the same as the volume of the sphere; the droplet transition control method is based on the droplet transition conditions and the material density of the welding wire. Target sediment volume and formula Calculate the amount of sediment to achieve the target. Corresponding droplet sphere diameter Target filler height First, calibrate the zero point of the filler wire height: Move the welding torch to the welding position, drive the welding wire so that the tip of the welding wire is in the same vertical line as the tungsten electrode, control the filler wire height adjustment mechanism to drive the clamping device to move downwards in the vertical direction until the tip of the welding wire contacts the workpiece, and record the current position information of the clamping device as the zero point of the filler wire height, denoted as . The quantitative deposition control center outputs a control signal based on the target deposition amount, and, starting from the zero point of the filler wire height, drives the clamping device to move vertically upward a certain distance using the filler wire height adjustment mechanism. At this time, the filler wire height Remember the current clamping device position information; before welding, use the remembered clamping device position information as the adjustment target, and adjust the filler wire height through the filler wire height adjustment mechanism to make the filler wire height equal to the target filler wire height, i.e. This allows for control of the droplet size when it comes into contact with the molten pool, thereby enabling control of the droplet transition during the welding process.
[0007] The quantitative deposition method for GTAW arc additive manufacturing is characterized by a welding speed control method that controls the movement of the welding torch based on a torch movement control signal. The welding speed control method keeps the welding torch stationary (i.e., welding speed is 0) during droplet transfer at the target position, and stops wire feeding and controls the torch movement distance after the target deposition amount is achieved at the target position. Upon reaching the new target position, the movement stops, and wire filling begins at the current target position, simultaneously completing droplet transfer to achieve the target deposition amount. This process is repeated until welding is complete. The distance mentioned... These are preset values. The timing diagram for the welding torch and filler wire system during welding is as follows: Figure 3 As shown.
[0008] Beneficial effects of the invention:
[0009] This invention relates to the field of GTAW (Glass Craft Artificial) additive manufacturing, and specifically to a quantitative deposition method for GTAW additive manufacturing. It utilizes a droplet deposition volume monitoring method to detect droplet deposition quality, a droplet transition control method to control droplet deposition volume, and a welding speed control method to control welding speed, thereby achieving quantitative deposition in GTAW additive manufacturing. Attached Figure Description
[0010] Figure 1 This is a schematic diagram of a quantitative deposition method for GTAW arc additive manufacturing.
[0011] Figure 2 This is a system schematic diagram of a quantitative deposition method for GTAW arc additive manufacturing.
[0012] In the diagram: 1 - Fill height 2-Electric arc, 3-Welding wire, 4-Welding gun, 5-Workpiece, 6-Filling nozzle, 7-Filling height adjustment mechanism, 8-Clamping device, 9-Wire guide tube, 10-Wire feeder, 11-Central shaft, 12-Wire feeder, 13-Quantitative deposition control center, 14-Quantitative deposition algorithm.
[0013] Figure 3 This is a sequence diagram of the operation of the filler wire height adjustment mechanism, the filler wire system, and the welding torch.
[0014] In the picture: - One work cycle, - Working time of the filler system within one work cycle - Welding torch working time within a work cycle
[0015] Figure 4 This is a flowchart of a quantitative deposition method for GTAW arc additive manufacturing. Detailed Implementation
[0016] To better illustrate the technical solution and beneficial effects of the present invention, the present invention will be further described in detail below with reference to the accompanying drawings and embodiments. The implementation methods of the present invention are not limited thereto.
[0017] like Figure 4 The diagram shows a flowchart of a quantitative deposition method for GTAW arc additive manufacturing technology.
[0018] Step 1: Input prerequisite parameters
[0019] Input welding wire material density Set the target deposition amount for a single movement. welding torch movement parameters ;
[0020] Step 2: Calculate the target filler wire height and record the position information of the clamping device at the target filler wire height.
[0021] Based on the material density of the welding wire Target sediment volume and formula Calculate the amount of sediment to achieve the target. Corresponding target filler wire height First, calibrate the zero point of the filler wire height: Move the welding torch to the welding position, drive the welding wire so that the tip of the welding wire is in the same vertical line as the tungsten electrode, and control the filler wire height adjustment mechanism to drive the clamping device to move downwards in the vertical direction until the tip of the welding wire contacts the workpiece. Record the current position information of the clamping device as the zero point of the filler wire height, denoted as _____. The quantitative deposition control center outputs a control signal based on the target deposition amount, and, starting from the zero point of the filler wire height, drives the clamping device to move vertically upward a certain distance using the filler wire height adjustment mechanism. At this time, the filler wire height Remember the current position information of the clamping device;
[0022] Step 3: Arc Initiation
[0023] Adjust the welding torch to the arc-starting height and start the arc;
[0024] Step 4: Welding torch position and filler wire height are ready.
[0025] Adjust the welding torch to the welding height, according to the filler wire height recorded in step 2. Based on the position information of the clamping device, after adjusting the filler wire height to the target filler wire height, welding begins.
[0026] Step 5: Filler wire, droplet transfer
[0027] by Figure 3 The timing sequence shown employs a filler wire amount control method to fill the welding wire while simultaneously performing droplet transfer.
[0028] Step 6: Move the welding torch a certain distance along the welding direction. Then stop
[0029] Step 7: Repeat steps 5 and 6 until the welding is complete.
Claims
1. A quantitative deposition method for GTAW arc additive manufacturing, used to control the amount of material deposited during the GTAW arc additive manufacturing process, characterized in that: The quantitative deposition method for GTAW arc additive manufacturing comprises a quantitative deposition control method and a quantitative deposition control system. The quantitative deposition control method includes a filler wire amount control method, a droplet transfer control method, and a welding speed control method. The filler wire amount control method controls the filler wire amount, the droplet transfer control method controls the droplet deposition amount, and the welding speed control method controls the welding speed. The quantitative deposition control system includes a quantitative deposition control center, a filler wire system, and a filler wire height adjustment mechanism. The quantitative deposition control center receives wire feed reel quality data and preset input data, processes the wire feed reel quality data and preset input data, and outputs filler wire height adjustment control signals, wire feed speed adjustment control signals, and welding torch movement control signals. The filler wire system includes a wire feeder, a wire guide tube, a clamping device, and a filler nozzle. The wire feeder includes a wire feed reel and a central shaft. The wire feed reel is used to hold the welding wire roll and is driven to rotate. The welding wire is fed out; the wire guide tube is used to guide the fed welding wire to a specific position; the clamping device is used to fix the welding wire filling position and angle; the filling nozzle feeds the welding wire into the welding position; the filling wire height adjustment mechanism is used to adjust the filling wire height; the filling wire height refers to the vertical distance between the tip of the welding wire fed into the welding position and the substrate; the condition for droplet transition is that the droplet grows to contact the molten pool; during the droplet growth process, the droplet is approximately spherical, and when the droplet contacts the molten pool, the diameter of the sphere is equal to the filling wire height, and the amount of droplet deposition is the volume of the sphere; the droplet transition control method is based on the droplet transition condition, and adjusts the filling wire height through the filling wire height adjustment mechanism to change the size of the droplet when it contacts the molten pool, thereby achieving control of droplet transition; the filling wire height adjustment mechanism receives the filling wire height adjustment control signal and controls the filling wire height adjustment mechanism to adjust the filling wire height so that the amount of droplet deposition during droplet transition is equal to the target deposition amount.
2. The quantitative deposition method for GTAW arc additive manufacturing according to claim 1, characterized in that: The wire feed control method adjusts the wire feeding speed according to the deviation between the target deposition amount and the actual wire feed amount, so that the actual wire feed amount equals the target deposition amount. The target deposition amount is the deposition amount required for welding in a pre-set manner. The actual wire feed amount is the quality of the welding wire actually fed by the wire feed system. There is a quality monitoring device in the central shaft of the wire feed reel. The quality monitoring device acquires the quality data of the wire feed reel in real time and transmits it to the quantitative deposition control center, which calculates the actual wire feed amount.
3. The quantitative deposition method for GTAW arc additive manufacturing according to claim 1, characterized in that: The welding speed control method described herein controls the movement of the welding torch based on the torch movement control signal from the quantitative deposition control center. During droplet transfer at the target position, the welding torch is kept stationary (i.e., the welding speed is 0). After the target deposition amount is achieved at the target position, wire feeding is stopped, and the welding torch movement is controlled by setting a predetermined distance. Upon reaching the new target position, the movement stops, and wire filling begins at the current target position, simultaneously completing the droplet transfer to achieve the target deposition amount. This process is repeated until welding is completed. This is a preset value.
Citation Information
Patent Citations
Device and method for achieving non-consumable electrode arc high-precision additive forming through real-time fine adjustment wire feeding
CN115194293A
GTAW process droplet transition frequency control method based on arc sensing
CN115383260A