Preparation method of magnesium mineral inorganic fiberboard for assembled integrated fire resistance limit air duct
By using magnesium oxide, magnesium sulfate and other raw materials to prepare magnesium inorganic fiber boards, it solves the problems of low compressive and seismic strength and poor environmental protection of existing fireproof air duct materials, achieving efficient and environmentally friendly fireproof performance and production efficiency, and has excellent Impact resistance and compression resistance, in line with fireproof and non-combustible level A1.
Patent Information
- Application Number
- CN202410072154.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2024-01-18
- Publication Date
- 2024-10-11
- Estimated Expiration
- 2044-01-18
AI Technical Summary
Existing fireproof air duct materials have problems such as low compressive and seismic strength, low fire resistance limit, poor environmental protection, low production efficiency and inconvenient assembly. In particular, magnesium fireproof boards are prone to frost and deformation during the production process, and magnesium chloride is used. As a result, it is difficult to meet environmental protection requirements.
Magnesium oxide and magnesium sulfate are used as raw materials to prepare magnesium inorganic fiber boards. Through mixing, roll forming, natural oxidation and curing processes, a unique natural pore structure is formed. Combined with wood fiber and other auxiliary materials, it improves impact resistance, compression resistance and tensile resistance. and fracture resistance, and improve production efficiency through specific maintenance procedures and transportation methods.
It realizes the good fire resistance, stability and environmental protection of mineral magnesium inorganic fiber board. It can not burn or deform at high temperatures, has excellent impact resistance and pressure resistance, meets the fire protection and non-combustibility level A1, and reduces production costs and Environmental impact.
Smart Images

Figure CN118205292B_ABST
Abstract
Description
Technical Field
[0001] The invention relates to a layered product, that is, a flat or non-flat thin layer, and more particularly to a method for preparing a mineral magnesium inorganic fiberboard for an assembled integrated fire resistance limit air duct. Background Art
[0002] In the existing technology of fireproof air ducts, it is more common to use galvanized iron air ducts. The production of galvanized iron air ducts requires high-power equipment, consumes energy, has low assembly efficiency, and requires more than 30 square meters per person. The metal air ducts will resonate during operation, rust, corrode and breed various bacteria. The iron air ducts are spliced with bite folds, have low compressive and seismic strength, low fire resistance, and poor insulation effect. If you want to meet national standards, you must coat the iron air duct skeleton with fireproof and thermal insulation materials, which requires secondary installation, which is labor-intensive and expensive, and greatly increases the product cost. Assembly is inconvenient, the materials are not environmentally friendly, and the strength is low. So there is magnesite fireproof board, which is a fireproof board made of magnesium oxide and magnesium chloride as raw materials, supplemented by glass fiber cloth, wood chips and perlite and other reinforcing materials. It has the three advantages of fireproof, waterproof and environmental protection. However, due to the complex process conditions, the product R&D investment is small, the unqualified rate is high, and it is easy to cause halogen frosting, deformation, etc.
[0003] The main raw materials of magnesia fireproof board are active magnesium oxide, magnesium chloride hexahydrate, water and other auxiliary materials. Chemical reactions occur during the production process to form 5-phase and 3-phase products. The current measures to prevent magnesium fireproof duct boards from returning brine and frosting can be found in the paper "Research Progress of Magnesia Fireproof Board" published by Li Fuhua in "Salt Science and Chemical Engineering" Volume 49, Issue 4, April 2020. It mentions that when the active magnesium oxide content is large (>70% or more), the hydration time is short, the liquid pH value increases, and the magnesium oxide MgCl 2 .6H 2 O formation can aggravate the return of brine and the decrease of water resistance, ensuring that MgO and MgCl 2 In the appropriate ratio. On the other hand, the use of modified admixtures and water repellents can not only slow down the reaction speed and ensure that magnesium oxide fully reacts, but also form complexes with chloride ions to solidify them within a certain range, thereby limiting their active freedom and solving the problem of halogen return and frosting. However, free chloride ions are still unavoidable, which makes it difficult for the environmental protection of magnesium fireproof duct boards to meet the requirements.
[0004] Patent with publication number CN1415884: A magnesium oxychloride cement fireproof smoke exhaust air duct and its manufacturing method, which uses magnesium oxide, magnesium chloride, and wood fiber as raw materials, phosphoric acid as an admixture, and is made into clay by mechanical mixing, and the clay and refractory fiber cloth are coated on the pre-made air duct mold. After coating to a thickness of 2mm-10mm, a layer of refractory heat-insulating material is covered on the clay, and then the clay and fiber cloth 2mm-10mm are coated on the refractory heat-insulating material. After curing and demolding, the required fireproof smoke exhaust air duct is made. The magnesium oxychloride cement fireproof smoke exhaust air duct produced by this manufacturing method has been tested by the national testing department, and all performance indicators are better than those of imported products from abroad. However, since magnesium chloride is still used, it is difficult to meet the environmental protection standards.
[0005] In addition, the production efficiency of magnesium fireproof board for air duct is not high at present, and the working hours are long. In addition to the most time-consuming maintenance, it is also necessary to wait for the cutting into boards to be transported to the transfer rack, and it also takes time to transport from the conveying mechanism to the curing room. Summary of the invention
[0006] The purpose of the present invention is to overcome the defects existing in the prior art and provide a method for preparing a magnesium mineral inorganic fiberboard for an assembled integrated fire resistance limit air duct. Since magnesium oxide and magnesium sulfate are used as raw materials, the magnesium mineral inorganic fiberboard can form a unique natural pore structure and can absorb a large amount of heat energy during combustion. The performance of the magnesium mineral inorganic fiberboard is always stable and is not affected by condensed water droplets and humid air. It performs well in impact resistance, compression resistance, tensile resistance and fracture resistance.
[0007] To achieve the above purpose, the technical solution of the present invention is to design a preparation method of mineral magnesium inorganic fiberboard for assembled integrated fire resistance limit air duct, including the following preparation steps in sequence: raw material mixing, production board, entering the primary oxidation room, demoulding, entering the secondary oxidation room, cutting board, cutting into corresponding specifications, surface polishing, natural oxidation for 3 days, packaging and storage, and finished product delivery. Mineral magnesium inorganic fiberboard has good fire resistance and is a non-combustible board. The flame continues to burn for zero time, does not burn at 800℃, and has no flames at 1200℃. It reaches the fireproof and non-combustible level A1. The partition system made with excellent keels has a fire resistance limit of more than 3 hours. It can absorb a large amount of heat energy during the combustion process of fire and delay the increase of the surrounding temperature. In dry, cold and humid weather, the performance of mineral iron inorganic fiberboard is always stable and consistent, and is not affected by condensed water droplets and humid air. Even if it is soaked in water for several days and then taken out and dried naturally, it will not deform or soften, and can be used normally. It has been tested by the National Building Materials Testing Center and has no water droplets and no moisture. Since magnesium oxide and magnesium sulfate are used as raw materials, the mineral magnesium inorganic fiberboard can form a unique natural pore structure, which can absorb a large amount of heat energy during the combustion process. The performance of the mineral iron inorganic fiberboard is always stable and is not affected by condensed water droplets and humid air. It performs well in impact resistance, compression resistance, tensile resistance and fracture resistance.
[0008] A further technical solution is that the raw materials are magnesium oxide, magnesium chloride, magnesium sulfate, wood fiber, calcium powder, phosphoric acid, foaming agent, modifier, instant glue powder and perlite; the raw materials are stirred for 4 to 5 minutes at room temperature. Although the mineral inorganic fiberboard is light in weight, it has a compact structure, good stability, no deformation, and has the toughness of wood. It performs well in impact resistance, compression resistance, tensile resistance and fracture resistance, and has both rigidity and toughness. The bending strength reaches 322kgf / cm 2 (vertical) and 216kgf / cm 2 (level), the impact strength can reach 25MPa. Foaming agent and modifier are used to improve hardness and coagulation. Pearl salt and calcium powder work together to ensure that the inorganic fiberboard made by the present invention does not return to halogen and does not frost; instant glue powder plays a bonding role;
[0009] A further technical solution is that the production process of the board is as follows: a layer of non-woven fabric is laid on the template and then a layer of glass fiber cloth is laid, then the mixed raw materials are evenly distributed on the template, and then a layer of glass fiber cloth is laid and then a layer of non-woven fabric is laid on the top layer of glass fiber cloth, and then after two roll forming, it naturally heats up and reacts to form a board. The roll-formed inorganic fiberboard is used for the inorganic fireproof layer of the air duct. The cross-sectional structure of the air duct can also include a color steel plate, and at least one side of the inorganic fireproof layer is fixed with a color steel plate. The color steel plate can be used or not according to different grades; if the fire resistance level is higher or other special requirements such as longer fire resistance time are required, galvanized steel plate or metal aluminum protective layer can be used to replace the color steel plate. The mineral magnesium inorganic fiberboard does not contain asbestos, formaldehyde, benzene and harmful radioactive elements, and is smokeless, non-toxic and odorless when exposed to fire. The materials used in production are natural mineral powder and plant fiber. The production process is naturally maintained, consumes less energy, does not emit any sewage, is energy-saving and environmentally friendly, and the board surface does not shed powder during use. Its unique natural pore structure can regulate the indoor temperature, making living and office spaces more comfortable.
[0010] The inorganic mineral powder material constitutes the anti-shock, anti-bacteria, anti-insect and anti-termite functions of the magnesium mineral inorganic fiberboard, which meets the anti-shock standards of building materials in European and American countries.
[0011] Magnesium mineral inorganic fiberboard has stable and reliable quality, high cost performance, light weight and high energy, moderate price, excellent processing and installation performance, can be pasted, cut, nailed, drilled, painted, planed, easy to carry, excellent toughness, not easy to break, and can be easily installed using self-tapping nails, gun nails and straight nails.
[0012] A further technical solution is to enter the curing room for a 24-hour constant temperature curing process, with the temperature controlled at 37-38°C. Humidity adjustment is based on climate temperature, and the relative humidity should not exceed 70%. In addition, normal temperature curing is generally sufficient in summer, and the ideal temperature of the product itself is 20°C in winter.
[0013] A further technical solution is to enter the secondary curing room process for constant temperature curing for 12 hours. The secondary curing controls the temperature and humidity, reacts naturally, and cures for 12 hours. The second curing mainly allows the board to fully react and increase the flexibility and hardness of the board.
[0014] A further technical solution is that the mass ratio of the components in the raw materials is: magnesium oxide: magnesium sulfate: wood fiber: perlite: magnesium chloride: calcium powder: instant glue powder: foaming agent: modifier is (15-22): (16-20): (4-5): 1: 83: 30: 10: 10: 0.375; the amount of phosphoric acid used is 90-110 ml.
[0015] A further technical solution is that between the production plate making process and the process of entering the primary oxidation room, there is a process for the finished plate to enter the curing extension room; in the production plate making process, there is a cutting and conveying process after the two roll forming processes to form the plate, and the cut finished plate is conveyed to the transfer rack on the rail car by a conveying mechanism and then conveyed to the curing room by the rail car, and a curing extension room is provided between the conveying mechanism and the curing room. In this way, uniform heating and constant temperature can be achieved before entering the constant temperature curing room; or in other words, constant temperature curing can be achieved almost immediately after the finished plate is cut, and curing is also carried out during the conveying process, and the curing is extended to the conveying station, which is equivalent to utilizing the conveying time, reducing the curing time, improving efficiency, and achieving earlier curing and output of the plate. After entering the curing extension room, the car drives in a circle at a uniform speed to avoid the problem of the plate not being able to fully react due to uneven temperature in the curing room.
[0016] A further technical solution is that the maintenance extension room covers the entire track area of the rail car;
[0017] The track is annular, and a portion of the track is arranged perpendicular to the board conveying direction of the conveying mechanism, and the aforementioned portion is the portion of the track located on one side of the conveying mechanism;
[0018] The curing extension room is connected to the curing room. A rubber curtain is set on one side of the curing extension room facing the conveying mechanism. An opening is set on the conveying end of the rubber curtain facing the conveying mechanism to receive the cut magnesium mineral inorganic fiberboard delivered by the conveying mechanism. The track is nearly ring-shaped, but the whole ring has a gap to avoid the pit; or the track is a closed ring, and the pit is set on one side of the ring track. After the transfer rack in the pit is filled with finished boards, the transfer rack is moved to the rail car on the track. The rubber curtain, plastic film, and rubber sheet are made of materials with certain elasticity but also certain hardness, such as rubber or plastic. Two rectangular plastic films or two rectangular rubber sheets are arranged up and down and partially overlapped, and the lower end of the upper rectangular plastic film or rectangular rubber sheet overlaps the upper end of the lower rectangular plastic film or rectangular rubber sheet to better ensure the constant temperature and heat preservation of the curing extension room. Only when the mineral magnesium inorganic fiberboard is transported into the curing extension room, part of the heat of the curing extension room is dissipated from the opening, and the temperature change of the curing room (including the curing extension room) is avoided as much as possible. A circle is formed, and the car keeps running between the curing room and the curing extension room to avoid the problem that the board cannot fully react due to uneven temperature in the curing room; and because of the continuous driving, the heat transfer between the connected curing room and the curing extension room is also promoted, effectively ensuring the constant temperature state of the entire curing room and the curing extension room to achieve constant temperature curing. Two rectangular plastic films or two rectangular rubber sheets are arranged at the opening of the rubber curtain. The two rectangular plastic films or two rectangular rubber sheets are arranged up and down and the shape formed by the combination is adapted to the opening. The upper end of the rectangular plastic film or rectangular rubber sheet located above is fixedly connected to the top wall inside the opening, and the lower end of the rectangular plastic film or rectangular rubber sheet located below is fixedly connected to the bottom wall inside the opening.
[0019] A further technical solution is that the curing room starts working after the transfer rack starts receiving finished boards, and the heating components in the curing extension room also start working when the curing room is working; the rail car starts after the transfer rack is full of finished boards, and the rail car travels one circle along the track to complete a maintenance to achieve full coverage of the transportation process and the waiting process; the time for the rail car to travel one circle is 24 hours. This can avoid the reciprocating forward and reverse rotation and start and stop of the motor driving the rail car, avoid the problem of too short service life of the entire rail car system, and avoid premature damage to the motor due to frequent forward and reverse rotation and start and stop; the time waiting for the transfer rack to be full of finished boards is also equivalent to the time for incorporating maintenance, which improves efficiency and almost eliminates waiting time.
[0020] The advantages and beneficial effects of the present invention are: the mineral magnesium inorganic fiberboard has good fireproof performance, is a non-combustible board, the flame continues to burn for zero time, does not burn at 800℃, and has no flames at 1200℃, reaching the fireproof and non-combustible level A1. The partition system made with excellent keels has a fire resistance limit of more than 3 hours. It can absorb a large amount of heat energy during the combustion process and delay the increase in the ambient temperature. In dry, cold and humid weather, the performance of the mineral iron inorganic fiberboard is always stable and is not affected by condensed water droplets and humid air. Even if it is soaked in water for several days and then taken out and dried naturally, it will not deform or soften and can be used normally. It has been tested by the National Building Materials Testing Center to be free of water droplets and moisture.
[0021] Although the mineral fiberboard is light in weight, it has a compact structure, good stability, no deformation, and has the toughness of wood. It performs well in impact resistance, compression resistance, tension resistance and fracture resistance. It has both rigidity and toughness, with a bending strength of 322kgf / cm2 (vertical) and 216kgf / cm2 (horizontal), and an impact strength of up to 25MPa.
[0022] Mineral magnesium inorganic fiberboard does not contain asbestos, formaldehyde, benzene and harmful radioactive elements. It is smokeless, non-toxic and odorless when exposed to fire. The production materials are natural mineral powder and plant fiber. The production process is naturally maintained, with low energy consumption, no sewage discharge, energy saving and environmental protection. The board surface does not fall off during use. Its unique natural pore structure can adjust the indoor temperature and make the living room and office more comfortable.
[0023] The inorganic mineral powder material constitutes the anti-shock, anti-bacteria, anti-insect and anti-termite functions of the magnesium mineral inorganic fiberboard, which meets the anti-shock standards of building materials in European and American countries.
[0024] Magnesium mineral inorganic fiberboard has stable and reliable quality, high cost performance, light weight and high energy, moderate price, excellent processing and installation performance, can be pasted, cut, nailed, drilled, painted, planed, easy to carry, excellent toughness, not easy to break, and can be easily installed using self-tapping nails, gun nails and straight nails.
[0025] Achieve uniform heating and constant temperature before entering the constant temperature curing room; or achieve constant temperature curing almost immediately after the plate is cut, and also carry out curing during the transportation process, extending the curing to the transportation station, which is equivalent to utilizing the transportation time, reducing the curing time, improving efficiency, and achieving earlier curing and board delivery.
[0026] Since magnesium oxide and magnesium sulfate are used as raw materials, the mineral magnesium inorganic fiberboard can form a unique natural pore structure, which can absorb a large amount of heat energy during the combustion process. The performance of the mineral iron inorganic fiberboard is always stable and is not affected by condensed water droplets and humid air. It performs well in impact resistance, compression resistance, tensile resistance and fracture resistance.
[0027] It can avoid the reciprocating forward and reverse rotation and start and stop of the motor driving the rail car, avoid the problem of too short service life of the entire rail car system, and avoid premature damage of the motor due to frequent forward and reverse rotation and start and stop; the time waiting for the transfer rack to be filled with finished boards is also equivalent to the maintenance time, which improves efficiency and has almost no waiting time. BRIEF DESCRIPTION OF THE DRAWINGS
[0028] Figure 1 It is a specific friction test curve diagram of an air duct made of a mineral magnesium inorganic fiberboard prepared by a method for preparing a mineral magnesium inorganic fiberboard for an assembled integrated fire resistance limit air duct of the present invention;
[0029] Figure 2 yes Figure 1 Photos of the samples being tested;
[0030] Figure 3 It is a physical schematic diagram of a mineral magnesium inorganic fiberboard prepared by a method for preparing a mineral magnesium inorganic fiberboard for an assembled integrated fire resistance limit air duct according to the present invention;
[0031] Figure 4 yes Figure 3 Schematic diagram of application scenarios;
[0032] Figure 5 It is a schematic diagram of a curing station and a conveying station involved in a method for preparing a mineral magnesium inorganic fiberboard for an assembled integrated fire resistance limit air duct according to the present invention;
[0033] Figure 6 is Figure 5 On the basis of the above, a schematic diagram of the maintenance extension room is added;
[0034] Figure 7 yes Figure 6 Schematic diagram of the extended maintenance room;
[0035] Figure 8 yes Figure 5 A magnified schematic diagram of the mid-track vehicle;
[0036] Fig. 9 yes Figure 8 Bottom view after placing the transfer rack;
[0037] Fig.10 It is a schematic diagram of the transfer rack and the lifting mechanism located in the pit of the present invention.
[0038] In the figure: 1. Conveying mechanism; 2. Rail car; 3. Transfer frame; 4. Maintenance room; 5. Extension maintenance room; 6. Pit; 7. Track; 8. Partial section; 9. Loading plate; 10. Lifting mechanism. DETAILED DESCRIPTION
[0039] The specific implementation of the present invention is further described below in conjunction with the accompanying drawings and embodiments. The following embodiments are only used to more clearly illustrate the technical solution of the present invention, and cannot be used to limit the protection scope of the present invention.
[0040] The present invention is a method for preparing a mineral magnesium inorganic fiberboard for an assembled integrated fire resistance limit air duct, comprising the following preparation steps in sequence: raw material mixing, board production, entering a primary oxidation room, demoulding, entering a secondary oxidation room, cutting boards, cutting into corresponding specifications, surface polishing, natural oxidation for 3 days, packaging and storage, and finished product delivery. The raw materials are magnesium oxide, magnesium sulfate, wood fiber and perlite; the raw material mixing time is 4 to 5 minutes, and the mixing temperature is room temperature. The production board making process is: laying a layer of non-woven fabric on the template and then laying a layer of glass fiber cloth, then evenly distributing the stirred raw materials on the template, and then laying a layer of glass fiber cloth and then laying a layer of non-woven fabric on the top layer of glass fiber cloth, and then after two roll forming, naturally heating and reacting to form a board. Enter the first curing room 4 process for constant temperature curing for 24 hours, and the temperature is controlled at 37-38°C. Enter the secondary curing room 4 process for constant temperature curing for 12 hours. The mass of each component in the raw materials is: 150kg of magnesium oxide, 200kg of magnesium sulfate, 83kg of magnesium chloride, 100ml of 30% phosphoric acid, 10kg of instant glue powder, 30kg of calcium powder, 10kg of foaming agent, 0.375kg of modifier, 40kg of wood fiber and 10kg of perlite; the foaming agent is ATF foaming agent with a solid content greater than 65%, and its Baume concentration is 25; the modifier includes citric acid, sodium dihydrogen phosphate and potassium aluminum sulfate, and the mass ratio of citric acid, sodium dihydrogen phosphate and potassium aluminum sulfate is 6:7:2; in dry, cold and humid weather, the performance of the ore iron inorganic fiberboard is always stable and is not affected by condensed water droplets and humid air. Even if it is soaked in water for several days and then taken out and dried naturally, it will not deform or soften and can be used normally. It has been inspected by the Building Environment and Energy Testing Institute of Jianke Huanneng Technology Co., Ltd., the National Air Conditioning Equipment Quality Inspection and Testing Center (such as Figure 1 , Figure 2 As shown, the non-flammability, chloride ion content, formaldehyde emission limit, etc. were specifically tested; Figure 1 This is the comparative friction test curve, and the corresponding test conditions are as shown in the following table) There are no water drops and no moisture.
[0041]
[0042] Figure 2 The following are photos of the tested samples. The corresponding test results are shown in the following table:
[0043]
[0044] like Figures 3 to 10 As shown (for ease of illustration, Figure 5A curing and extension room, a transfer rack, and a lifting mechanism are not shown). Between the plate production process and the process of entering the primary oxidation room, there is a process in which the finished plate enters the curing and extension room 5. In the plate production process, after the plates are formed by two roll forming processes, there is a cutting and conveying process. The cut plates are conveyed by the conveying mechanism 1 to the transfer rack 3 on the rail car 2 and then to the curing room 4 by the rail car 2. A curing and extension room 5 is provided between the conveying mechanism 1 and the curing room 4. A transfer rack 3 is arranged at the conveying end of the conveying mechanism 1, and the transfer rack 3 is arranged in a pit 6. A lifting mechanism is arranged in the pit 6 to complete each conveyance of a board to the empty carrying plate 9 of the transfer rack 3 and then rise a short distance to ensure that the subsequently conveyed magnesium ore inorganic fiberboard will not be placed on the surface of the previous magnesium ore inorganic fiberboard but will be placed on the empty carrying plate 9 of the transfer rack 3 (the pit 6 and the lifting mechanism are existing technologies and will not be repeated); after the magnesium ore inorganic fiberboard is received on the carrying plate 9 at the bottom of the transfer rack 3, the moving mechanism under the entire lifting mechanism moves to make the transfer rack 3 leave the pit 6 and reach the rail car 2 on the track 7. The moving mechanism can be a screw-nut mechanism, and a pair of vertical plates for rotating the screw are fixedly arranged on the bottom wall of the pit 6. When in action, the nut moves along the screw, and the slider fixedly connected to the nut moves, driving the lifting mechanism arranged above the slider to move; the lifting mechanism 10 can be a parallelogram lifting mechanism, {the structure of the parallelogram telescopic door is used to realize the lifting of the liftable table surface}, and the parallelogram adjustment mechanism includes a number of parallelogram rod assemblies hinged to each other. The lifting and lowering can be achieved by setting an articulated oil cylinder, and the piston rod of the oil cylinder is hinged to the parallelogram rod assembly. This is a prior art and will not be described in detail. The maintenance extension room 5 is covered on the pit 6 and the transfer frame 3 (or the maintenance extension room 5 covers the pit 6 and the transfer frame 3). The maintenance extension room 5 covers the entire area of the track 7 of the rail car 2 and the pit 6. The track 7 is annular, and a partial section 8 of the track 7 is arranged perpendicular to the board conveying direction of the conveying mechanism 1. The aforementioned partial section 8 is the part of the track 7 located on one side of the conveying mechanism 1. The maintenance extension room 5 is connected to the maintenance room 4, and a rubber curtain is arranged on one side of the maintenance extension room 5 facing the conveying mechanism 1, and an opening is arranged at the conveying end of the rubber curtain facing the conveying mechanism 1 for receiving the cut magnesium mineral inorganic fiberboard conveyed by the conveying mechanism 1. After the transfer rack 3 starts to receive the finished boards, the curing room 4 starts to work. When the curing room 4 is working, the heating components in the curing extension room 5 also start to work at the same time. After the transfer rack 3 is full of finished boards, the rail car 2 starts. The rail car 2 travels one circle along the track 7 to complete one maintenance to achieve full coverage of the transportation process and the waiting process. The time for the rail car 2 to travel one circle is 24 hours.
[0045] After entering the curing extension room 5, the car drives in a circle at a constant speed to avoid the problem of the plate not being able to fully react due to the uneven temperature in the curing room 4; [the process is that the cut plates are placed one by one on the carrying plate 9 of the transfer rack 3, and the transfer rack 3 is transferred from the rail car 2 to the curing room 4 (it also passes through the curing extension room 5 in this process) and continues to drive until it drives out of the curing room 4 and arrives at the curing extension room 5; this process is also constant temperature curing; combined with the rail car 2, it keeps driving; it is fully automatic and does not require manual labor]
[0046] A circle is formed, which keeps running between the curing room 4 and the curing extension room 5, so as to avoid the problem that the plate cannot fully react due to the uneven temperature in the curing room 4; and because it keeps running, it also promotes the heat transfer between the connected curing room 4 and the curing extension room 5, effectively ensuring the constant temperature state of the entire curing room 4 and the curing extension room 5 to achieve constant temperature curing; and because the transfer rack 3 keeps running with the rail car 2, it can reach a constant temperature more quickly after the curing room 4 starts working (promoting the heat transfer between the connected curing room 4 and the curing extension room 5), and realize the working condition of uniform temperature in various places in the room (referring to the curing room 4 and the curing extension room 5) more quickly; the curing extension room 5 is also provided with a heating component, and the heating component in the curing extension room 5 also works at the same time when the curing room 4 is working;
[0047] And because the track 7 of the rail car 2 is nearly a ring, unlike the previous rail car 2 that reciprocates between the maintenance room 4 and the conveying end of the conveying mechanism 1 (that is, the pit 6), it can avoid the reciprocating forward and reverse rotation and start and stop of the motor driving the rail car 2, avoid the problem of too short service life of the entire rail car 2 system, and avoid premature damage of the motor due to frequent forward and reverse rotation and start and stop; in addition, because it is a circle travel (the travel process is intermittently paused to wait for the next transfer rack 3 to be full of finished plates), the length of the track 7 can be set in advance according to the cutting speed and the conveying speed of the conveying mechanism 1, and the speed of the rail car 2 can be set in coordination (due to one time The curing time is 24h, so the speed of the rail car 2 is relatively slow), so that the rail car 2 can be transported from the transfer rack 3 to the curing room 4 and then continue to travel to the side of the conveying mechanism 1, so that the finished boards on the next transfer rack 3 (or the next few transfer racks 3) are just full. In this way, the time waiting for the transfer rack 3 to be full of finished boards is also equivalent to the time for curing, which improves the efficiency and there is almost no waiting time (it is said that there is almost no waiting time because the rail car 2 returns to the side of the conveying mechanism 1 after traveling a circle. At this time, the finished boards on the transfer rack 3 on the rail car 2 need to be taken down and demolded, so there is still time to take the boards);
[0048] Several rail cars 2 can be set up, one next to the other on the track 7. When a transfer rack 3 is full (the magnesium mineral inorganic fireproof fiberboard is placed on the transfer rack 3, and the transfer rack 3 is gradually lifted up from the pit 6 through the lifting mechanism), the finished boards are moved to the empty rail car 2 on the track 7 through the moving mechanism; the rail car 2 is started after receiving the transfer rack 3, and the next rail car 2 is started for a short time so that this rail car 2 is located on the side of the pit 6 again to receive the next fully loaded transfer rack 3; the rail car is provided with a driving motor to drive it to move along the track.
[0049] The above is only a preferred embodiment of the present invention. It should be pointed out that for ordinary technicians in this technical field, several improvements and modifications can be made without departing from the technical principles of the present invention. These improvements and modifications should also be regarded as the scope of protection of the present invention.
Claims
1. A method for preparing a magnesium mineral fiberboard for assembled integrated fire resistance limit air duct, characterized in that: The preparation steps include the following steps: mixing raw materials, producing boards, entering the primary curing room, demoulding, entering the secondary curing room, cutting boards, cutting into corresponding specifications, surface polishing, natural curing for 3 days, packaging and storage, and finished product delivery; The raw materials are magnesium oxide, magnesium chloride, magnesium sulfate, wood fiber, calcium powder, phosphoric acid, foaming agent, modifier, instant glue powder and perlite; the raw materials are stirred for 4 to 5 minutes at room temperature; The production process of the board is as follows: a layer of non-woven fabric is laid on the template, and then a layer of glass fiber cloth is laid, and then the mixed raw materials are evenly distributed on the template, and then a layer of glass fiber cloth is laid, and then a layer of non-woven fabric is laid on the top layer of glass fiber cloth, and then after two roll pressings, the board is formed by natural heat reaction; The process of entering the primary curing room is to perform constant temperature curing for 24 hours, and the temperature is controlled at 37-38°C; The process of entering the secondary curing room is to perform constant temperature curing for 12 hours; The mass ratio of the components in the raw materials is: magnesium oxide: magnesium sulfate: wood fiber: perlite: magnesium chloride: calcium powder: instant glue powder: foaming agent: modifier is (15-22): (16-20): (4-5): 1: 83: 30: 10: 10: 0.375; the amount of phosphoric acid used is 90-110 ml; Between the production and board making process and the process of entering the primary curing room, there is also a process of the finished board entering the curing extension room; in the production and board making process, after the boards are formed by the two roll forming processes, there is also a cutting and conveying process, and the cut finished boards are conveyed to the transfer rack on the rail car by the conveying mechanism and then conveyed to the curing room by the rail car, and a curing extension room is also provided between the conveying mechanism and the curing room; The maintenance extension room covers the entire track area of the railcar; The track is annular, and a portion of the track is arranged perpendicular to the board conveying direction of the conveying mechanism, and the aforementioned portion is the portion of the track located on one side of the conveying mechanism; The curing extension room is connected with the curing room. A rubber curtain is arranged on one side of the curing extension room facing the conveying mechanism. An opening is arranged on the conveying end of the rubber curtain facing the conveying mechanism to receive the cut magnesium mineral inorganic fiberboard delivered by the conveying mechanism. The curing room starts to work after the transfer rack starts to receive the finished boards, and the heating components in the curing extension room also start to work at the same time when the curing room is working.
2. The method for preparing the mineral magnesium inorganic fiberboard for assembled integrated fire resistance limit air duct according to claim 1, characterized in that: After the transfer rack is full of finished panels, the rail car starts. The rail car travels one circle along the track to complete a maintenance to achieve full coverage of the transportation process and the waiting process; the time for the rail car to travel one circle is 24 hours.