A kind of anticorrosion heat preservation pipeline and its production equipment

By designing fixing mechanisms and rotary casting systems with different diameters, the problem of difficulty in efficiently producing insulation pipes of different diameters is solved in existing equipment, the production efficiency and forming rate are improved, and the failure rate and construction difficulty are reduced.

CN118254328BActive Publication Date: 2024-11-01CANGZHOU RUNXINGDA THERMAL INSULATION ENGINEERING CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202410684847.X
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2024-05-30
Publication Date
2024-11-01
Estimated Expiration
2044-05-30

AI Technical Summary

Technical Problem

The existing insulation pipeline production equipment is single, making it difficult to efficiently produce insulation pipelines of different diameters, resulting in low production efficiency and increased costs.

Method used

A production equipment including a bracket, a casting mechanism, a fixing mechanism and a rotating mechanism is designed to adapt the pipe body and the anti-corrosion layer body through multiple fixing grooves and barrier parts of the fixing mechanism, and to utilize the rotating mechanism and a casting mechanism. Ensure uniform pouring of polyurethane foam to reduce deformation caused by foam expansion.

Benefits of technology

The production efficiency and forming rate of insulation pipes are improved, the unqualified rate is reduced, and efficient production of pipes of different diameters is achieved, reducing construction difficulty.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118254328B_ABST
    Figure CN118254328B_ABST
Patent Text Reader

Abstract

The invention relates to an anti-corrosion thermal insulation pipe and production equipment thereof, and relates to the technical field of thermal insulation pipes. The anti-corrosion thermal insulation pipe comprises a steel pipe, a thermal insulation layer and an anti-corrosion layer; the thermal insulation layer is made of polyurethane foam poured between a pipe body and an anti-corrosion layer body; the production equipment comprises a bracket, a pipe body, an anti-corrosion layer body, a pouring mechanism, a fixing mechanism and a rotating mechanism, the pipe body and the anti-corrosion layer body are both fixed on the bracket by the fixing mechanism, the pouring mechanism is used to pour polyurethane foam between the pipe body and the anti-corrosion layer body, and the rotating mechanism is used to drive the bracket to rotate; since the lengths of both ends of the steel pipe in the produced thermal insulation pipe exceed the lengths of the thermal insulation layer and the anti-corrosion layer by twenty centimeters, it is not necessary to peel off the two ends of the thermal insulation pipe to expose the steel pipe and then weld it during the construction of the thermal insulation pipe, thereby reducing the difficulty of construction.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of thermal insulation pipes, in particular to an anti-corrosion thermal insulation pipe and production equipment thereof. Background Art

[0002] The insulated pipe is used for insulation and cold preservation projects in heating, cooling, hot oil transportation, chemical industry and other industries. It consists of a working steel pipe for conveying the medium, a glass wool insulation layer, an aluminum foil reflective layer, a stainless steel fastening belt, a sliding guide bracket, an air insulation layer, an outer protective steel pipe, and an outer anti-corrosion layer that are combined outward in sequence through equipment.

[0003] At present, when producing insulated pipes, the production equipment is single. When it is necessary to produce insulated pipes of different diameters, different production equipment needs to be provided, which leads to low production efficiency of the insulated pipes and increased production costs. Summary of the invention

[0004] In order to solve the problems mentioned in the background technology, the present invention provides an anti-corrosion and heat-insulating pipeline and a production equipment thereof.

[0005] In the first aspect, the present invention provides an anti-corrosion and thermal insulation pipeline, comprising a steel pipe, an insulation layer and an anti-corrosion layer, the insulation layer is arranged between the anti-corrosion layer and the steel pipe, the steel pipe is the pipeline body; the anti-corrosion layer is the anti-corrosion layer body; the length of the insulation layer is the same as the length of the anti-corrosion layer, and the lengths of both ends of the steel pipe exceed the lengths of the insulation layer and the anti-corrosion layer; the insulation layer is made of polyurethane foam cast between the pipeline body and the anti-corrosion layer body.

[0006] In a second aspect, the present invention provides a production device for anti-corrosion and heat-insulating pipes, which adopts the following technical solution:

[0007] A production equipment for anti-corrosion and thermal insulation pipes includes a bracket, a pouring mechanism, a fixing mechanism and a rotating mechanism, the bracket is arranged on the rotating mechanism, the rotating mechanism is used to drive the bracket to rotate, the fixing mechanism includes a first fixing block, a second fixing block and a baffle, the first fixing block is arranged on one end of the bracket, the first fixing block is provided with a plurality of first fixing grooves, the second fixing block is slidably arranged on the other end of the bracket, the second fixing block is provided with a plurality of second fixing grooves, the baffle includes a first blocking part and a second blocking part, a plurality of third fixing grooves are provided on the baffle, the first blocking part and the second blocking part are both movably arranged on the first fixing block, one end of the pipeline body is passed through the first fixing groove provided on the first fixing block, the other end of the pipeline body is passed through the second fixing groove provided on the second fixing block, one end of the anti-corrosion layer body is passed through the third fixing groove provided on the baffle, and the other end of the anti-corrosion layer body is passed through the second fixing groove provided on the second fixing block.

[0008] By adopting the above technical scheme, when producing the insulated pipe, the anti-corrosion layer body is sleeved on the pipe body, the length of the anti-corrosion layer body is smaller than the length of the pipe body, so that both ends of the pipe body protrude from the anti-corrosion layer body by 20 centimeters, the pipe body and the anti-corrosion layer body are driven to move by the lifting equipment, one end of the pipe body is inserted into the first fixed groove, the first blocking part and the second blocking part of the baffle are sleeved on the pipe body, and the first blocking part and the second blocking part are connected by bolts, so that one end of the baffle abuts against the first fixed block, and then the second fixed block is slid to move in the direction close to the first fixed block, so that the other end of the pipe body is inserted into the second fixed groove, and the second fixed block is continued to slide so that the second fixed block and the light pipe body slide relative to each other, and the second fixed block pushes the anti-corrosion layer body to slide, so that the end of the anti-corrosion layer body close to the first fixed block is inserted into the third fixed groove opened on the baffle, and when the pipe After the pipe body and the anti-corrosion layer body are fixed, the rotating mechanism drives the bracket to rotate so that the pipe body and the anti-corrosion layer body are in a vertical state, and the pouring mechanism pours polyurethane foam between the pipe body and the anti-corrosion layer body. Because when the polyurethane foam is poured, one end of the pipe body is inserted into the first fixed groove and the other end is inserted into the second fixed groove, so that the length of the polyurethane pouring is the same as the length of the anti-corrosion layer body, so that when using the insulated pipe, there is no need to peel off the insulation layer and the anti-corrosion layer for a certain length, thereby improving the production efficiency of the insulated pipe; when it is necessary to produce insulated pipes of different diameters, since there are multiple first fixed grooves and multiple second fixed grooves, pipe bodies of different diameters can be inserted into the first fixed groove and the second fixed groove, and since there are multiple third fixed grooves, anti-corrosion layer bodies of different diameters can be inserted into the third fixed groove, thereby realizing the production of insulated pipes of different diameters.

[0009] Optionally, the fixing mechanism also includes a fixing plate, which includes a first fixing portion and a second fixing portion, one end of the first fixing portion is arranged on the bracket, one end of the second fixing portion is arranged on the bracket, one end of the first fixing portion away from the bracket is connected to one end of the second fixing portion away from the bracket, and the inner circumferential surface of the fixing plate abuts against the anti-corrosion layer body.

[0010] By adopting the above technical solution, after the anti-corrosion layer body is coaxially connected to the bracket with the pipeline body, the first fixing part is connected to the bracket by bolts, one end of the second fixing part is connected to the bracket by bolts, and the ends of the first fixing part and the second fixing part close to each other are connected by bolts, so that the fixing plate fixes the anti-corrosion layer body to the bracket, thereby reducing the probability of movement of the anti-corrosion layer body when filling with polyurethane foam, thereby improving the molding rate of the thermal insulation pipeline.

[0011] Optionally, the fixing mechanism further comprises a wedge block, the wedge block is arranged on the fixing plate, an arc-shaped surface is formed on the wedge block, and one end of the wedge block with the arc-shaped surface abuts against the anti-corrosion layer body.

[0012] Since the polyurethane foam expands and solidifies when it comes into contact with air, by adopting the above-mentioned technical solution, the wedge block is arranged on the fixed plate, and the end of the wedge block with an arc-shaped surface abuts against the anti-corrosion layer body so that there is no gap between the anti-corrosion layer body and the fixed plate, thereby reducing the probability of deformation of the anti-corrosion layer body due to the expansion of the polyurethane foam when filling the polyurethane foam, thereby reducing the probability of the insulation pipe being unqualified.

[0013] Optionally, the pouring mechanism includes a sliding rod, a sliding rail, a compressor, a connecting pipe and a sliding assembly, the second fixed block is provided with a through hole, the sliding rail is arranged on the bracket, the sliding rail is provided with a sliding groove, the sliding rod is slidably connected in the sliding groove, the sliding rod is provided with a channel, the compressor is arranged on the bottom surface, one end of the connecting pipe is connected to the compressor, a channel is provided inside the sliding rod, the other end of the connecting pipe is connected to the sliding rod, a nozzle is provided at the end of the sliding rod away from the connecting pipe, and the sliding assembly is used to drive the sliding rod to slide on the sliding rail.

[0014] By adopting the above technical scheme, after the pipeline main body and the anti-corrosion layer main body are fixed on the bracket, the driving component drives the slide rod to slide on the slide rail, so that the slide rod is vertical and one end of the nozzle passes through the through hole opened on the second fixed block and moves toward the first fixed block until the nozzle approaches the baffle. After the rotating mechanism drives the bracket to rotate so that the pipeline main body and the anti-corrosion layer main body are in a vertical state, the compressor starts to spray the polyurethane foam through the connecting pipe and the channel opened on the slide rod through the nozzle to the pipeline main body and the anti-corrosion layer main body, filling the pipeline limbs and the anti-corrosion layer main body. When the nozzle sprays polyurethane foam, the driving component drives the slide rod to move so that the nozzle moves away from the first fixed block until the nozzle approaches the second fixed block and stops spraying polyurethane foam.

[0015] Optionally, a plurality of nozzles are provided, and the orientation of the nozzles is the same as the length direction of the pipe body.

[0016] By adopting the above technical solution, since the gap filled by the polyurethane is annular, multiple vertical nozzles can allow the polyurethane to quickly fill the pipeline body and the anti-corrosion layer body.

[0017] Optionally, the sliding assembly includes a first drive motor, a gear and a rack, the first drive motor is arranged on a bracket, the gear key is connected to a production shaft of the first drive motor, the rack is arranged on a sliding rod, and the gear is meshed with the rack for transmission.

[0018] By adopting the above technical solution, when the sliding rod is driven to slide, the first driving motor drives the gear to rotate, and the gear engages with the rack on the sliding rod to drive the sliding rod to slide on the sliding rail, thereby driving the nozzle to move between the pipeline body and the anti-corrosion layer body.

[0019] Optionally, the rotating mechanism includes a support, a rotating shaft, a reduction gearbox and a second drive motor, wherein the support, the reduction gearbox and the second drive motor are all arranged on the ground, the rotating shaft is rotatably connected to the support, the bracket is arranged on the rotating shaft, the output end of the second drive motor is transmission-connected to the input end of the reduction gearbox, and the output end of the reduction gearbox is transmission-connected to the rotating shaft.

[0020] By adopting the above technical solution, after the pipeline body and the anti-corrosion layer body are fixed on the bracket, the output end of the second drive motor transmits power to the reduction gearbox, thereby driving the rotating shaft to rotate, and the rotating shaft drives the bracket to rotate, thereby making the pipeline body and the anti-corrosion layer body on the bracket in a vertical state, thereby reducing the probability of polyurethane foam leakage when filling polyurethane foam.

[0021] In summary, the present invention includes at least one of the following beneficial technical effects:

[0022] 1. When the polyurethane foam is poured, one end of the pipe body is inserted into the first fixed groove and the other end is inserted into the second fixed groove, so that the length of the polyurethane pouring is the same as the length of the anti-corrosion layer body, so that when using the insulated pipe, there is no need to peel off a section of the insulation layer and the anti-corrosion layer, thereby improving the production efficiency of the insulated pipe; when it is necessary to produce insulated pipes of different diameters, since there are multiple first fixed grooves and the second fixed grooves, pipe bodies of different diameters can be inserted into the first fixed groove and the second fixed groove, and since there are multiple third fixed grooves, anti-corrosion layer bodies of different diameters can be inserted into the third fixed groove, thereby realizing the production of insulated pipes of different diameters.

[0023] 2. The wedge block is arranged on the fixed plate, and one end of the wedge block with an arc surface abuts against the main body of the anti-corrosion layer so that there is no gap between the main body of the anti-corrosion layer and the fixed plate, thereby reducing the probability of deformation of the main body of the anti-corrosion layer due to expansion of the polyurethane foam when filling the polyurethane foam, thereby reducing the probability of failure of the insulation pipe.

[0024] 3. After the anti-corrosion layer body and the pipeline body are coaxially connected to the bracket, the first fixing part is connected to the bracket by bolts, one end of the second fixing part is connected to the bracket by bolts, and the end close to the first fixing part and the second fixing part is connected by bolts, so that the fixing plate fixes the anti-corrosion layer body on the bracket, thereby reducing the probability of movement of the anti-corrosion layer body when filling with polyurethane foam, thereby improving the molding rate of the thermal insulation pipeline. BRIEF DESCRIPTION OF THE DRAWINGS

[0025] Figure 1 is a schematic diagram of the overall structure of an embodiment of the present invention;

[0026] Figure 2 This is a schematic diagram of the overall structure of another state of an embodiment of the present invention;

[0027] Figure 3 It is a schematic diagram of the fixed mechanism structure;

[0028] Figure 4 for Figure 3 Section view in the AA direction;

[0029] Figure 5 for Figure 4 Enlarged view of middle part B;

[0030] Figure 6 for Figure 4 Enlarged view of middle C;

[0031] Figure 7 for Figure 2 Enlarged view of the middle D part;

[0032] Figure 8 is a schematic diagram of the fixed plate structure;

[0033] Fig. 9 This is a schematic diagram of the insulation pipe structure.

[0034] Description of reference numerals: 100, bracket; 200, pipeline body; 300, anti-corrosion layer body; 400, fixing mechanism; 410, first fixing block; 411, first fixing groove; 420, second fixing block; 421, second fixing groove; 422, through hole; 430, fixing plate; 431, first fixing portion; 432, second fixing portion; 440, wedge block; 450, baffle; 451, first blocking portion; 452, second blocking portion; 453, first Three fixed grooves; 500, pouring mechanism; 510, sliding rod; 511, nozzle; 512, channel; 520, sliding rail; 530, compressor; 540, connecting pipe; 550, sliding assembly; 551, first drive motor; 552, gear; 553, rack; 600, rotating mechanism; 610, pillar; 620, rotating shaft; 630, reduction gear box; 640, second drive motor; 700, steel pipe; 800, insulation layer; 900, anti-corrosion layer. DETAILED DESCRIPTION

[0035] The following is combined with Figure 1 -Attached Fig. 9 The present invention is described in further detail.

[0036] The embodiment of the present invention discloses an anti-corrosion and heat-insulating pipeline, comprising a steel pipe 700, an insulation layer 800 and an anti-corrosion layer 900, wherein the insulation layer 800 is arranged between the anti-corrosion layer 900 and the steel pipe 700, and the steel pipe 700 is the pipeline body 200; the anti-corrosion layer 900 is the anti-corrosion layer body 300; the length of the insulation layer 800 is the same as that of the anti-corrosion layer 900, and the lengths of both ends of the steel pipe 700 exceed the lengths of the insulation layer 800 and the anti-corrosion layer 900; the insulation layer 800 is made of polyurethane foam cast between the pipeline body 200 and the anti-corrosion layer body 300.

[0037] The anti-corrosion and heat-insulating pipe of the present invention is produced by the following production equipment. Figure 1-Figure 9 A corrosion-resistant and heat-insulating pipe and its production equipment include a bracket 100, a pouring mechanism 500, a fixing mechanism 400 and a rotating mechanism 600. The pipe body 200 and the anti-corrosion layer body 300 are fixed on the bracket 100 by the fixing mechanism 400. The pouring mechanism 500 is used to inject polyurethane foam between the pipe body 200 and the anti-corrosion layer body 300. The rotating mechanism 600 is used to drive the bracket 100 to rotate.

[0038] Reference Figure 1-Figure 6 , Figure 8The fixing mechanism 400 includes a first fixing block 410, a second fixing block 420, a fixing plate 430, a wedge block 440 and a baffle 450. The first fixing block 410 is arranged on one end of the bracket 100. The first fixing block 410 is provided with a plurality of first fixing grooves 411. The second fixing block 420 is slidably arranged on the other end of the bracket 100. The second fixing block 420 is provided with a plurality of second fixing grooves 421. The baffle 450 includes a first blocking portion 451 and a second blocking portion 452. The baffle 450 is provided with a plurality of third fixing grooves 453. The first blocking portion 451 and the second blocking portion 452 are both movably arranged on the first fixing block 410. One end of the pipe body 200 is inserted into the first fixing groove 411 provided on the first fixing block 410. The other end of the pipe body 200 is inserted into the second fixing groove 411 provided on the second fixing block 410. In the second fixing groove 421 opened on the fixed block 420, one end of the anti-corrosion layer body 300 is inserted into the third fixing groove 453 opened on the baffle 450, and the other end of the anti-corrosion layer body 300 is inserted into the second fixing groove 421 opened on the second fixing block 420. The fixing plate 430 includes a first fixing portion 431 and a second fixing portion 432. One end of the first fixing portion 431 is connected to the bracket 100 by bolts, and one end of the second fixing portion 432 is connected to the bracket 100 by bolts. The end of the first fixing portion 431 away from the bracket 100 is connected to the end of the second fixing portion 432 away from the bracket 100 by bolts. The wedge block 440 is connected to the fixing plate 430 by bolts. An arcuate surface is opened on the wedge block 440, and one end of the wedge block 440 with an arcuate surface abuts against the anti-corrosion layer body 300.

[0039] When producing the insulated pipe, the anti-corrosion layer body 300 is sleeved on the pipe body 200. The length of the anti-corrosion layer body 300 is less than the length of the pipe body 200, so that both ends of the pipe body 200 protrude from the anti-corrosion layer body 300 by 20 centimeters. The pipe body 200 and the anti-corrosion layer body 300 are moved by the lifting equipment, and one end of the pipe body 200 is inserted into the first fixing groove 411. The first blocking portion 451 and the second blocking portion 452 of the baffle 450 are sleeved on the pipe body 200, and the first blocking portion 451 and the second blocking portion 452 are connected by bolts so that one end of the baffle 450 abuts against the first fixing block 410, and then the second fixing block 420 is slid closer to the second fixing block 420. The first fixing block 410 moves in the direction of the first fixing block 410, so that the other end of the pipeline body 200 is inserted into the second fixing groove 421, and the second fixing block 420 is continued to slide so that the second fixing block 420 and the main body slide relative to each other, and the second fixing block 420 pushes the anti-corrosion layer main body 300 to slide, so that the end of the anti-corrosion layer main body 300 close to the first fixing block 410 is inserted into the third fixing groove 453 opened on the baffle 450. When the anti-corrosion layer main body 300 and the pipeline main body 200 are coaxially connected to the bracket 100, the first fixing part 431 is connected to the bracket 100 by bolts, and one end of the second fixing part 432 is connected to the bracket 100 by bolts, and the ends of the first fixing part 431 and the second fixing part 432 close to each other are connected by bolts. The bolt connection allows the fixing plate 430 to fix the anti-corrosion layer body 300 on the bracket 100, and then the second fixing block 420 is slid to move in a direction away from the pipe body 200, and the end of the pipe body 200 away from the first fixing block 410 is still in the second fixing groove 421, thereby reducing the probability of the anti-corrosion layer body 300 moving when filling with polyurethane foam, thereby improving the molding rate of the insulation pipe. Since the polyurethane foam expands and solidifies when it contacts the air, the wedge block 440 is arranged on the fixing plate 430, and the end of the wedge block 440 with an arc surface abuts against the anti-corrosion layer body 300, so that there is no gap between the anti-corrosion layer body 300 and the fixing plate 430, thereby reducing the movement of the anti-corrosion layer body 300 due to the polyurethane foam when filling. The expansion of the polyurethane foam reduces the probability of deformation of the anti-corrosion layer body 300, thereby reducing the probability of failure of the thermal insulation pipe. The rotating mechanism 600 drives the bracket 100 to rotate so that the pipe body 200 and the anti-corrosion layer body 300 are in a vertical state. The pouring mechanism 500 pours polyurethane foam between the pipe body 200 and the anti-corrosion layer body 300. During the polyurethane foaming, one end of the pipe body 200 is inserted into the first fixing groove 411, and the other end is inserted into the second fixing groove 421, so that the length of the polyurethane pouring is the same as the length of the anti-corrosion layer body 300, so that when using the thermal insulation pipe, there is no need to peel off a section of the thermal insulation layer 800 and the anti-corrosion layer 900, thereby improving the production efficiency of the thermal insulation pipe.When it is necessary to produce insulated pipes of different diameters, since the first fixing groove 411 and the second fixing groove 421 are provided with a plurality of them, the pipe bodies 200 of different diameters can be inserted into the first fixing groove 411 and the second fixing groove 421, and since the third fixing groove 453 is provided with a plurality of them, the anti-corrosion layer bodies 300 of different diameters can be inserted into the third fixing groove 453, thereby realizing the production of insulated pipes of different diameters. ;

[0040] Reference Figure 7 The pouring mechanism 500 includes a slide bar 510, a slide rail 520, a compressor 530, a connecting pipe 540 and a sliding assembly 550. The second fixing block 420 is provided with a through hole 422. The slide rail 520 is arranged on the bracket 100. The slide rail 520 is provided with a slide groove. The slide bar 510 is slidably connected in the slide groove. The slide bar 510 is provided with a channel 512. The compressor 530 is connected to the bottom surface by bolts. One end of the connecting pipe 540 is connected to the compressor 530. The slide bar 510 is provided with a channel 512. The other end of the connecting pipe 540 is connected to the compressor 530. It is connected to the slide rod 510, and one end of the slide rod 510 away from the connecting pipe 540 is connected to a nozzle 511 by bolts. There are multiple nozzles 511, and the direction of the nozzles 511 is the same as the length direction of the pipeline body 200. The sliding assembly 550 includes a first driving motor 551, a gear 552 and a rack 553. The first driving motor 551 is connected to the ground by bolts, and the gear 552 is keyed to the production shaft of the first driving motor 551. The rack 553 is fixedly connected to the slide rod 510, and the gear 552 is meshed with the rack 553 for transmission.

[0041] After the pipeline body 200 and the anti-corrosion layer body 300 are fixed on the bracket 100, the driving component drives the slide bar 510 to slide on the slide rail 520, so that the slide bar 510 is vertically moved with one end of the nozzle 511 passing through the through hole 422 opened on the second fixed block 420 toward the first fixed block 410 until the nozzle 511 approaches the baffle 450. The rotating mechanism 600 drives the bracket 100 to rotate so that the pipeline body 200 and the anti-corrosion layer body 300 are in a vertical state. The compressor 530 is started to spray the polyurethane foam through the connecting pipe 540 and the channel 512 opened on the slide bar 510 through the nozzle 511 to the space between the pipeline body 200 and the anti-corrosion layer body 300. , filling the space between the pipeline body 200 and the anti-corrosion layer body 300. When the nozzle 511 sprays polyurethane foam, when the driving slide bar 510 slides, the first driving motor 551 drives the gear 552 to rotate, and the gear 552 engages with the rack 553 on the slide bar 510 to drive the slide bar 510 to slide on the slide rail 520, driving the slide bar 510 to move so that the nozzle 511 moves away from the first fixed block 410 until the nozzle 511 approaches the second fixed block 420 and stops spraying polyurethane foam. Since the gap filled with polyurethane foam is annular, multiple vertical nozzles 511 can quickly fill the space between the pipeline body 200 and the anti-corrosion layer body 300 with polyurethane.

[0042] Reference Figure 4 The rotating mechanism 600 includes a support 610, a rotating shaft 620, a reduction box 630 and a second driving motor 640. The support 610, the reduction box 630 and the second driving motor 640 are all arranged on the ground. The rotating shaft 620 is rotatably connected to the support 610. The bracket 100 is arranged on the rotating shaft 620. The output end of the second driving motor 640 is transmission-connected to the input end of the reduction box 630. The output end of the reduction box 630 is transmission-connected to the rotating shaft 620. When the pipeline body 200 and the anti-corrosion layer body 300 are fixed on the bracket 100, the output end of the second driving motor 640 transmits power to the reduction box 630, thereby driving the rotating shaft 620 to rotate. The rotating shaft 620 drives the bracket 100 to rotate, thereby making the pipeline body 200 and the anti-corrosion layer body 300 on the bracket 100 in a vertical state, thereby reducing the probability of polyurethane foam leakage when filling polyurethane foam.

[0043] Reference Fig. 9An anticorrosion heat preservation pipeline includes a steel pipe 700, a heat preservation layer 800 and an anticorrosion layer 900. The heat preservation layer 800 is arranged between the anticorrosion layer 900 and the steel pipe 700. The lengths of the heat preservation layer 800 and the anticorrosion layer 900 are both shorter than the length of the steel pipe 700. Since the lengths of both ends of the steel pipe 700 are both 15 cm longer than the lengths of the heat preservation layer 800 and the anticorrosion layer 900, it is not necessary to peel off both ends of the heat preservation pipeline to expose the steel pipe 700 and then weld them during the construction of the heat preservation pipeline, thereby reducing the construction difficulty.

[0044] The implementation principle of an anti-corrosion and heat-insulating pipeline and its production equipment in an embodiment of the present invention is as follows:

[0045] When producing the insulated pipe, the anti-corrosion layer body 300 is sleeved on the pipe body 200. The length of the anti-corrosion layer body 300 is smaller than the length of the pipe body 200, so that both ends of the pipe body 200 protrude from the anti-corrosion layer body 300 by 20 centimeters. The pipe body 200 and the anti-corrosion layer body 300 are moved by the lifting equipment, and one end of the pipe body 200 is inserted into the first fixing groove 411. The first blocking part 451 and the second blocking part 452 of the baffle 450 are sleeved on the pipe body 200, and the first blocking part 451 and the second blocking part 452 are connected by bolts so that one end of the baffle 450 abuts against the first fixing block 410. Then, the second fixing block 420 is slid toward the direction close to the first fixing block 410, so that the other end of the pipe body 200 is inserted into the second fixing groove 421, and the second fixing block 420 is continued to slide so that the second fixing block 420 and the light pipe body slide relative to each other, and the second fixing block 420 pushes the anti-corrosion layer body 300 to slide, so that the end of the anti-corrosion layer body 300 close to the first fixing block 410 is inserted into the third fixing groove 453 provided on the baffle 450. When the anti-corrosion layer body 300 and the pipe body 200 are coaxially connected to the bracket 100, the first fixing part 431 is connected to the bracket 100 by bolts, and one end of the second fixing part 432 is connected to the bracket 100 by bolts. On the bracket 100, the first fixing portion 431 and the second fixing portion 432 are connected at one end thereof by bolts, so that the fixing plate 430 fixes the anti-corrosion layer body 300 on the bracket 100, thereby reducing the probability of the anti-corrosion layer body 300 moving when the polyurethane foam is filled, thereby improving the molding rate of the heat-insulating pipe. Since the polyurethane foam expands and solidifies when it contacts the air, the wedge block 440 is arranged on the fixing plate 430, and the end of the wedge block 440 with an arc surface abuts against the anti-corrosion layer body 300 so that there is no gap between the anti-corrosion layer body 300 and the fixing plate 430, thereby reducing the anti-corrosion layer body 300 caused by the expansion of the polyurethane foam when the polyurethane foam is filled. 0 deformation probability, thereby reducing the probability of unqualified insulation pipes, the rotating mechanism 600 drives the bracket 100 to rotate so that the pipe body 200 and the anti-corrosion layer body 300 are in a vertical state, and the pouring mechanism 500 pours polyurethane foam between the pipe body 200 and the anti-corrosion layer body 300; because when the polyurethane foam is poured, one end of the pipe body 200 is inserted into the first fixing groove 411, and the other end is inserted into the second fixing groove 421, so that the length of the polyurethane pouring is the same as the length of the anti-corrosion layer body 300, so that when using the insulation pipe, there is no need to peel off a section of the insulation layer 800 and the anti-corrosion layer 900, thereby improving the production efficiency of the insulation pipe;When it is necessary to produce insulated pipes of different diameters, since the first fixing groove 411 and the second fixing groove 421 are provided with a plurality of them, the pipe bodies 200 of different diameters can be inserted into the first fixing groove 411 and the second fixing groove 421, and since the third fixing groove 453 is provided with a plurality of them, the anti-corrosion layer bodies 300 of different diameters can be inserted into the third fixing groove 453, thereby realizing the production of insulated pipes of different diameters. Since the length of both ends of the steel pipe 700 in the produced insulated pipe exceeds the length of the insulation layer 800 and the anti-corrosion layer 900 by fifteen centimeters, it is not necessary to peel off both ends of the insulated pipe to expose the steel pipe 700 and then weld them during the construction of the insulated pipe, thereby reducing the construction difficulty. ;

[0046] The above are all preferred embodiments of the present invention, and are not intended to limit the protection scope of the present invention. Therefore, any equivalent changes made based on the structure, shape, and principle of the present invention should be included in the protection scope of the present invention.

Claims

1. A production device for an anti-corrosion and heat-insulating pipeline, the anti-corrosion and heat-insulating pipeline comprising a pipeline body (200), a heat-insulating layer (800) and an anti-corrosion layer body (300), the heat-insulating layer (800) being arranged between the anti-corrosion layer body (300) and the pipeline body (200), characterized in that: The length of the thermal insulation layer (800) is the same as that of the anti-corrosion layer body (300), and the lengths of both ends of the pipeline body (200) exceed the lengths of the thermal insulation layer (800) and the anti-corrosion layer body (300); the thermal insulation layer (800) is made of polyurethane foam cast between the pipeline body (200) and the anti-corrosion layer body (300); the production equipment comprises a bracket (100), a casting mechanism (500), a fixing mechanism (400) and a rotating mechanism (600); the bracket (100) is arranged on the rotating mechanism (600), the rotating mechanism (600) is used to drive the bracket (100) to rotate, the fixing mechanism (400) comprises a first fixing block (410), a second fixing block (420) and a baffle (450); the first fixing block (410) is arranged on one end of the bracket (100), a plurality of first fixing grooves (411) are provided on the first fixing block (410), and the second fixing block (420) The baffle (450) is slidably arranged on the other end of the bracket (100), the second fixing block (420) is provided with a plurality of second fixing grooves (421), the baffle (450) includes a first blocking portion (451) and a second blocking portion (452), the baffle (450) is provided with a plurality of third fixing grooves (453), the first blocking portion (451) and the second blocking portion (452) are both movably arranged on the first fixing block (410), one end of the pipeline body (200) is inserted into the first fixing groove (411) provided on the first fixing block (410), the other end of the pipeline body (200) is inserted into the second fixing groove (421) provided on the second fixing block (420), one end of the anti-corrosion layer body (300) is inserted into the third fixing groove (453) provided on the baffle (450), and the other end of the anti-corrosion layer body (300) is inserted into the second fixing groove (421) provided on the second fixing block (420).

2. The production equipment for anti-corrosion and heat-insulating pipes according to claim 1 is characterized in that: The fixing mechanism (400) further includes a fixing plate (430), wherein the fixing plate (430) includes a first fixing portion (431) and a second fixing portion (432), wherein one end of the first fixing portion (431) is disposed on the bracket (100), and one end of the second fixing portion (432) is disposed on the bracket (100), and one end of the first fixing portion (431) away from the bracket (100) is connected to one end of the second fixing portion (432) away from the bracket (100), and an inner peripheral surface of the fixing plate (430) abuts against the anti-corrosion layer body (300).

3. The production equipment for anti-corrosion and heat-insulating pipes according to claim 2 is characterized in that: The fixing mechanism (400) further comprises a wedge block (440), wherein the wedge block (440) is arranged on the fixing plate (430), an arcuate surface is formed on the wedge block (440), and one end of the wedge block (440) having the arcuate surface abuts against the anti-corrosion layer body (300).

4. The production equipment for anti-corrosion and heat-insulating pipes according to claim 1 is characterized in that: The pouring mechanism (500) comprises a sliding rod (510), a sliding rail (520), a compressor (530), a connecting pipe (540) and a sliding assembly (550); a through hole (422) is provided on the second fixed block (420); the sliding rail (520) is arranged on the bracket (100); a sliding groove is provided on the sliding rail (520); the sliding rod (510) is slidably connected in the sliding groove; The slide bar (510) is provided with a channel (512), the compressor (530) is arranged on the ground, one end of the connecting pipe (540) is connected to the compressor (530), the other end of the connecting pipe (540) is communicated with the slide bar (510), a nozzle (511) is arranged at one end of the slide bar (510) away from the connecting pipe (540), and the sliding assembly (550) is used to drive the slide bar (510) to slide on the slide rail (520); the nozzle (511) is provided with a plurality of nozzles, The orientation of the nozzle (511) is parallel to the length direction of the pipe body (200); the sliding assembly (550) comprises a first driving motor (551), a gear (552) and a rack (553); the first driving motor (551) is arranged on the bracket (100); the gear (552) is key-connected to the output shaft of the first driving motor (551); the rack (553) is arranged on the sliding rod (510); the gear (552) and the rack (553) are meshed for transmission.

5. The production equipment for anti-corrosion and heat-insulating pipes according to claim 1 is characterized in that: The rotating mechanism (600) comprises a support (610), a rotating shaft (620), a reduction gearbox (630) and a second driving motor (640); the support (610), the reduction gearbox (630) and the second driving motor (640) are all arranged on the ground; the rotating shaft (620) is rotatably connected to the support (610); the bracket (100) is arranged on the rotating shaft (620); the output end of the second driving motor (640) is drivingly connected to the input end of the reduction gearbox (630); and the output end of the reduction gearbox (630) is drivingly connected to the rotating shaft (620).