A method for judging the prefabricated cracks passing through the bonding interface of layered elastomer based on Abaqus
Abaqus simulation software is used to establish models without cracks and with prefabricated cracks in the layered structure of elastomer materials, obtain the changing relationship between fracture energy and fracture tensile, and determine whether the prefabricated cracks cross the bonding interface, solving the difficulties in the existing technology. The problem of predicting the direction of cracks enables effective evaluation and optimization of the fracture properties of elastomer materials.
Patent Information
- Application Number
- CN202410127030.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2024-01-30
- Publication Date
- 2024-10-29
- Estimated Expiration
- 2044-01-30
AI Technical Summary
The existing technology fails to provide a method for judging whether surface cracks in the layered structure of elastomer materials are deflected to the interface or penetrate into the matrix after forming channels along the film, making it difficult to predict the crack direction and fracture performance.
Abaqus simulation software was used to establish layered elastomer structural models without cracks and with prefabricated cracks. The relationship between fracture energy and fracture tensile changes was obtained through pure shear tests, and the prefabricated crack development path and energy release rate of the bonding interface were set. , the functional relationship between the development path length and the energy release rate is fitted, and the maximum value of the energy release rate is defined as the crossing critical condition to determine whether the prefabricated crack crosses the bonding interface.
It provides a method to determine the critical conditions for prefabricated cracks in the layered structure of elastomer materials to cross the bonding interface, improves the accuracy of material testing and modeling efficiency, and can determine that interface debonding is equivalent to crack propagation, forming a type II crack, and Improve fracture performance.
Smart Images

Figure CN118258706B_ABST
Abstract
Description
Technical Field
[0001] The present application belongs to the technical field of elastomer materials, and specifically relates to a method for judging, based on Abaqus, that prefabricated cracks pass through the bonding interface of a layered elastomer. Background Art
[0002] Common elastomer materials include rubber, silicone, hydrogel, etc. As stretchable materials, elastomer materials have been widely used in emerging fields such as tissue engineering, soft robotics, and stretchable electronic devices. Stretchable devices are usually composed of elastomer materials in the form of layered structures to form membrane and matrix structures. When the membrane-matrix structure is under tension, surface cracks penetrate the membrane, then form channels along the membrane, deflect to the interface, or penetrate into the matrix, depending on the critical condition that the path reaches first.
[0003] Layered elastomers are a type of elastomer structure with a bonding interface and composed of at least two different elastomer materials. The prior art has given the crack propagation mode of thin films in layered structures. Reasonable design of the strength of the bonding interface in the layered elastomer structure can change the crack direction to improve its fracture performance. However, the prior art still does not provide a relevant judgment method for whether the surface crack will deflect to the interface or penetrate into the matrix after forming a channel along the film. Summary of the invention
[0004] The invention provides a method for judging whether a prefabricated crack passes through a layered elastomer bonding interface based on Abaqus, and provides a method for judging whether a prefabricated crack passes through a layered elastomer bonding interface.
[0005] The technical solution of the present invention is as follows:
[0006] A method for judging whether a prefabricated crack crosses a layered elastomer bonding interface based on Abaqus comprises the following steps:
[0007] S1) Establish a crack-free layered elastomer structure model in Abaqus and conduct a pure shear test to obtain the relationship between fracture energy and fracture elongation;
[0008] S2) establishing a layered elastomer structure model with prefabricated cracks in Abaqus, and setting a set of specific values of fracture energy and fracture stretch for the layered elastomer structure model with prefabricated cracks according to the change relationship obtained in step S1);
[0009] S3) specifying in Abaqus the bonding interface of the layered elastomer structure model with prefabricated cracks as the development interface of the prefabricated cracks in the pure shear test, and setting the length of the development path of the prefabricated cracks in the bonding interface;
[0010] S4) drawing a ring-shaped grid around the prefabricated crack development path set in step S3);
[0011] S5) Perform pure shear simulation test on the layered elastomer structure model with prefabricated cracks to check the mesh around the prefabricated cracks. J The integral result is J The integral result is the energy release rate of the prefabricated crack along the development path;
[0012] S6) controlling the fracture elongation to remain unchanged, changing the length of the development path of the prefabricated crack, repeating steps S3) to S5) several times, and fitting the functional relationship between the length of the development path and the energy release rate based on the test results of several times;
[0013] S7) selecting the maximum value of the energy release rate in the function relationship fitted in step S6), and defining the ratio of the maximum value of the energy release rate to the fracture energy set in step S2) as the crossing critical condition; when the ratio of the debonding energy to the fracture energy of the bonding interface is greater than the crossing critical condition, the prefabricated crack passes through the bonding interface; when the ratio of the debonding energy to the fracture energy of the bonding interface is less than or equal to the crossing critical condition, the prefabricated crack develops at the bonding interface.
[0014] Furthermore, the geometric parameters of the crack-free layered elastomer structure model in step S1) and the layered elastomer structure model with prefabricated cracks in step S2) are the same, the layered elastomer structure model is a combination of two elastomer materials with different shear moduli, and the prefabricated cracks are located in the elastomer material with a relatively small shear modulus.
[0015] Furthermore, in step S3), a two-dimensional line is drawn in the bonding interface, and the two-dimensional line is used as a development path of the prefabricated crack using the specified crack command in the Abaqus interaction module.
[0016] Further, in step S4), the step of drawing the ring-shaped mesh is: cutting two ring-shaped areas around the prefabricated crack tip at the normal plane of the bonding interface, drawing the mesh in the inner ring area using a sweep command, and drawing the mesh between the inner ring area and the outer ring area using a structured mapping command.
[0017] Due to the adoption of the above technical solution, the beneficial effects of this application are as follows:
[0018] 1. Based on Abaqus, this application provides a critical condition judgment method for the prefabricated cracks in the layered elastomer structure to cross the bonding interface. This method can be applied to actual material tests to determine whether the prefabricated cracks cross the bonding interface. In a high-elastic layered structure, the influencing factors of the debonding of the bonding interface are related to the debonding length, fracture stretch, modulus ratio between the matrix and thickness ratio function. For a given elastomer layered structure in actual engineering, except for the debonding length, the remaining parameters are specific values related to the material itself (which can be determined). Therefore, for a given layered elastomer structure, after specifying its fracture stretch, the energy release rate of the prefabricated crack along the bonding interface is only related to the debonding length. Furthermore, this application equates interface debonding to crack extension, that is, interface debonding can be considered as a type II crack formed by the extension of the prefabricated crack along the bonding interface.
[0019] 2. This application obtains the changing relationship between fracture energy and fracture stretch by establishing a crack-free layered elastomer structure, and then uses this changing relationship to determine the specific value of the energy release rate corresponding to the fracture stretch within a certain range. In simulation experiments with multiple fracture stretch requirements, this changing relationship can be reused, which can significantly improve the modeling efficiency. BRIEF DESCRIPTION OF THE DRAWINGS
[0020] The drawings described herein are used to provide a further understanding of the present application and constitute a part of the present application. The illustrative embodiments of the present application and their descriptions are used to explain the present application and do not constitute an improper limitation on the present application. In the drawings:
[0021] Figure 1 A flowchart of a method for judging that a prefabricated crack passes through a layered elastomer bonding interface based on Abaqus provided in this application;
[0022] Figure 2 is a graph showing the relationship between the fracture energy and the fracture elongation of the first embodiment;
[0023] Figure 3 A functional relationship diagram of the length of the development path and the energy release rate for the second embodiment;
[0024] Figure 4 A prefabricated crack development path diagram of the third embodiment;
[0025] Figure 5 A prefabricated crack development path diagram of the fourth embodiment;
[0026] Figure 6 This is a prefabricated crack development path diagram of the fifth embodiment. DETAILED DESCRIPTION
[0027] As described in the background technology, the layered elastomer can change the crack direction by reasonably designing the bonding strength to improve the fracture performance, and when the crack expands along the interface direction to form a type II crack, the fracture performance effect is better. Therefore, when the critical conditions for crossing the prefabricated cracks of the layered elastomer are obtained, it can be determined whether it can form a type II crack under a certain specific stretch, and then whether it can be used as a material that can improve the fracture performance. The present application provides a method for judging whether the prefabricated crack crosses the bonding interface of the layered elastomer based on Abaqus, comprising the following steps:
[0028] S1) A crack-free layered elastomer structure model was established in Abaqus and a pure shear test was performed to obtain the relationship between fracture energy and fracture elongation.
[0029] The structural model established by Abaqus can be a three-dimensional model. For structures that can be converted into plane stress problems, two-dimensional modeling can also be used. This application can use a three-dimensional model or a two-dimensional model when it is specifically implemented. It should be noted that Abaqus modeling is a well-known technical means in the art, and the material definition, selection of material constitutive relations, contact settings, boundary conditions, and loading methods of pure shear tests included therein do not affect the implementation of this method. It should be understood that after inputting material parameters and setting loading-related parameters, the resulting change relationship between fracture energy and fracture stretch is a change relationship of a class of materials. In different fracture stretches of this model, fracture energy is a change value. Furthermore, after adding a prefabricated crack in this structural model, the above-mentioned change relationship is not changed, but after determining the fracture energy, the energy required for expansion during the crack development process is called the energy release rate. Fracture energy and energy release rate are two similar concepts. Fracture energy reflects material properties, while energy release rate is an indicator for evaluating the crack development process.
[0030] S2) establishing a layered elastomer structure model with prefabricated cracks in Abaqus, and setting a set of specific values of fracture energy and fracture stretch for the layered elastomer structure model with prefabricated cracks according to the variation relationship obtained in step S1).
[0031] The elastomer structure model with prefabricated cracks is established based on S1, and the present application does not limit the specific loading method or crack location. In order to facilitate the setting of the relevant conditions for the simulation test loading, the prefabricated crack can be designed in the middle position of the matrix with a relatively small shear modulus, and the applied load can be set on the upper surface of the layered elastomer. In the specific implementation, the energy release rate corresponding to the required fracture stretch is determined according to S1). The fracture stretch is defined as the ratio of the height of the structure after deformation to the original height when the crack begins to expand. The fracture energy is defined as the energy required per unit area for crack expansion.
[0032] S3) specifying in Abaqus the bonding interface of the layered elastomer structure model with prefabricated cracks as a development interface of the prefabricated cracks in a pure shear test, and setting the length of the development path of the prefabricated cracks in the bonding interface.
[0033] In Abaqus, the crack development path can be specified to solve the relevant parameters of the crack development along this path, which is contrary to actual material testing. The development path of the prefabricated crack is set within the bonding interface of the matrix in order to make the debonding effect equivalent to the crack extension, that is, the crack tearing the matrix along the bonding interface can be regarded as the prefabricated crack becoming a type II crack during the formation process. After determining the fracture tensile strength of the layered elastomer structure, the development of the prefabricated crack in the bonding interface is related to the length of the development path. In theory, the energy release rate required for crack extension will quickly reach the maximum value at the beginning when the development path is 0 and gradually increases. Therefore, when setting several development path lengths as described below, relatively dense reference points should be set within the development range of the shorter crack path.
[0034] S4) Drawing a ring-shaped grid around the prefabricated crack development path set in step S3).
[0035] In Abaqus, whether the grid division is reasonable is an important factor affecting the simulation accuracy and calculation efficiency. When using J integral to calculate the energy release rate in Abaqus, it has special requirements for the grid division method of the structure. Therefore, the area around the crack tip should be appropriately divided to meet the requirements of J integral calculation. In this application, two annular areas are cut around the prefabricated crack tip at the normal plane of the bonding interface, and the sweep command is used to draw the grid in the inner ring area, and the structured mapping command is used to draw the grid between the inner ring area and the outer ring area. After drawing, the number of grids can be optimized through the seed editing module.
[0036] S5) Perform pure shear simulation test on the layered elastomer structure model with prefabricated cracks to check the mesh around the prefabricated cracks. J The integral result is J The integral result is the energy release rate of the pre-crack along the development path.
[0037] After setting the corresponding loading conditions, a pure shear simulation test is carried out. J Integration is a concept in elastic-plastic fracture mechanics that provides a method to quantify and analyze the stress-strain field at the crack tip. In Abaqus, J The integral can be selected in the test output data and can be viewed directly after the simulation is completed. J The result of the integration is the energy release rate in this application.
[0038] S6) controlling the fracture elongation to remain unchanged, changing the length of the development path of the prefabricated crack, repeating steps S3) to S5) several times, and fitting the functional relationship between the length of the development path and the energy release rate based on the test results of several times.
[0039] In layered elastomer structures, the factors affecting debonding at the bonding interface are related to the debonding length, fracture elongation, modulus ratio between the matrix and thickness ratio function. For a given high elastic layered structure in actual engineering, except for the debonding length, the remaining parameters are specific values related to the material itself (which can be determined). Therefore, for a given layered elastomer structure, after specifying its fracture elongation, the energy release rate of the prefabricated crack along the bonding interface is only related to the debonding length. To find the critical condition, it is necessary to determine the maximum value of the energy release rate, so several simulation tests are required to improve the accuracy of the simulation. The method for determining the development path length has been given above.
[0040] S7) selecting the maximum value of the energy release rate in the function relationship fitted in step S6), and defining the ratio of the maximum value of the energy release rate to the fracture energy set in step S2) as the crossing critical condition; when the ratio of the debonding energy to the fracture energy of the bonding interface is greater than the crossing critical condition, the prefabricated crack passes through the bonding interface; when the ratio of the debonding energy to the fracture energy of the bonding interface is less than or equal to the crossing critical condition, the prefabricated crack develops at the bonding interface.
[0041] The interfacial debonding energy is the energy required for the interface between different layers in the layered elastomer structure to overcome the molecular forces to separate the unit area. After defining the critical crossing condition, the interfacial debonding energy and the fracture energy can be used to determine whether the material can form a type II crack.
[0042] This application specifically illustrates the application process of this method through the following four embodiments.
[0043] First embodiment:
[0044] In this embodiment, the neo-Hookean model is used in Abaqus to define the elastomer material and establish a three-dimensional layered elastomer structure model. The total length of the structure is L = 50 mm, the height is H = 10 mm, the width is d = 0.1 mm, and the shear modulus of the left film is =5kpa, length L1=20mm, right side matrix shear modulus =10kpa, length L2=30mm, vertical displacement is applied on the upper surface of the structure and the horizontal displacement is fixed, a fixed horizontal displacement constraint is applied on the lower surface of the structure, and the grid is divided into C3D20RH units.
[0045] As attached Figure 2 As shown, the first embodiment obtains the changing relationship between the breaking energy and the breaking elongation.
[0046] Second embodiment:
[0047] The second embodiment adds a prefabricated crack on the basis of the first embodiment. The prefabricated crack is located in the middle of the left film. The prefabricated crack extends symmetrically upward and downward at the bonding interface. The fracture tensile strength of the second embodiment is set to =1.2, according to Figure 2 It can be seen that the corresponding fracture energy at this time is =4.92J / m 2 .
[0048] As attached Figure 3 As shown, the maximum energy release rate J / m 2 It should be noted that refer to Figure 3 The maximum value of the energy release rate of interfacial debonding at different debonding lengths. The following is the reasoning for crossing the critical condition:
[0049] The critical condition for interface debonding, i.e. the formation of mode II crack, is:
[0050] ;
[0051] In the formula, is the maximum value of the energy release rate of interfacial debonding at different debonding lengths; is the interfacial debonding energy between the film and the substrate in the layered elastomer structure.
[0052] The critical condition for the film crack to enter the substrate and form a mode I crack is:
[0053] ;
[0054] For the layered elastomer structure, before the left film crack enters the right substrate to form a type I crack, the crack must propagate along the bonding interface between the film and the substrate to form a type II crack. hour, ,
[0055] and then:
[0056] ;
[0057] Therefore, when the crack of the second embodiment propagates along the bonding interface and peels off the material:
[0058] ;
[0059] Crossing critical condition.
[0060] Therefore, by obtaining α crThe value of can determine the crack propagation path and the crack propagation along the bonding interface to form a type II crack. α , thereby eliminating the influence of the initial defects on the left film on the substrate, reforming the layered elastomer structure into a crack-free structure, and protecting the right substrate.
[0061] Third embodiment:
[0062] The third embodiment is based on the second embodiment, except that the vusdfle subroutine is used to define the damage control crack of the material in the horizontal direction, simulating the effect of the left film crack entering the right substrate, and cohesive contact is used to connect the left and right sides above the crack in the vertical direction at the crack tip to simulate the interface debonding effect in the layered elastomer structure under actual conditions. The crack propagation path is changed by changing the fracture energy of the cohesive contact.
[0063] As attached Figure 4 As shown, the third embodiment of .
[0064] when When the prefabricated cohesive contact is used, it does not affect the crack propagation from the film through the substrate.
[0065] Fourth embodiment:
[0066] The fourth embodiment differs from the third embodiment in that .
[0067] As attached Figure 5 As shown, when When it is close to 0.23, the cohesive contact set in the vertical direction also separates while the crack expands in the horizontal direction, indicating that the expansion resistance of the crack in the horizontal and vertical directions is close to its driving force. This also verifies the critical value for the crack to deflect in the vertical direction. The theoretical correctness.
[0068] Fifth embodiment:
[0069] The fifth embodiment is different from the third embodiment in that .
[0070] As attached Figure 6 As shown, when When the stretching reaches 1.26, the crack will first extend in the vertical direction, and when it is stretched to 1.26, the fracture will still occur in the horizontal direction.
[0071] The above embodiments are comprehensively judged to prove that the critical crossing condition determined by the method shown in this application is reasonable.
[0072] Anything not described in this application can be achieved by adopting or drawing on existing technologies.
[0073] The above is only an embodiment of the present application and is not intended to limit the present application. For those skilled in the art, the present application may have various changes and variations. Any modification, equivalent replacement, improvement, etc. made within the spirit and principle of the present application should be included in the scope of the claims of the present application.
Claims
1. A method for judging whether a prefabricated crack crosses a layered elastomer bonding interface based on Abaqus, characterized in that: The following steps are involved: S1) Establish a crack-free layered elastomer structure model in Abaqus and conduct a pure shear test to obtain the relationship between fracture energy and fracture elongation; S2) establishing a layered elastomer structure model with prefabricated cracks in Abaqus, and setting a set of specific values of fracture energy and fracture stretch for the layered elastomer structure model with prefabricated cracks according to the change relationship obtained in step S1); S3) specifying in Abaqus the bonding interface of the layered elastomer structure model with prefabricated cracks as the development interface of the prefabricated cracks in the pure shear test, and setting the length of the development path of the prefabricated cracks in the bonding interface; S4) drawing a ring-shaped grid around the prefabricated crack development path set in step S3); S5) Perform pure shear simulation test on the layered elastomer structure model with prefabricated cracks to check the mesh around the prefabricated cracks. J The integral result is J The integral result is the energy release rate of the prefabricated crack along the development path; S6) controlling the fracture elongation to remain unchanged, changing the length of the development path of the prefabricated crack, repeating steps S3) to S5) several times, and fitting the functional relationship between the length of the development path and the energy release rate based on the test results of several times; S7) selecting the maximum value of the energy release rate in the function relationship fitted in step S6), and defining the ratio of the maximum value of the energy release rate to the fracture energy set in step S2) as the crossing critical condition; when the ratio of the debonding energy to the fracture energy of the bonding interface is greater than the crossing critical condition, the prefabricated crack passes through the bonding interface; when the ratio of the debonding energy to the fracture energy of the bonding interface is less than or equal to the crossing critical condition, the prefabricated crack develops at the bonding interface.
2. The method for judging whether a prefabricated crack crosses the bonding interface of a layered elastomer based on Abaqus according to claim 1, characterized in that: The geometric parameters of the crack-free layered elastomer structure model in step S1) and the layered elastomer structure model with prefabricated cracks in step S2) are the same. The layered elastomer structure model is a combination of two elastomer materials with different shear moduli, and the prefabricated cracks are located in the elastomer material with a relatively small shear modulus.
3. The method for judging whether a prefabricated crack crosses a layered elastomer bonding interface based on Abaqus according to claim 1, characterized in that: In step S3), a two-dimensional line is drawn in the bonding interface, and the two-dimensional line is used as the development path of the prefabricated crack using the specified crack command in the Abaqus interaction module.
4. The method for judging whether a prefabricated crack crosses a layered elastomer bonding interface based on Abaqus according to claim 1, characterized in that: In step S4), the step of drawing the ring-shaped mesh is: cutting two ring-shaped areas around the prefabricated crack tip at the normal plane of the bonding interface, drawing the mesh in the inner ring area using a sweep command, and drawing the mesh between the inner ring area and the outer ring area using a structured mapping command.
Citation Information
Patent Citations
Method for simulating fracture toughness of layered rock based on extended finite elements
CN111488703A
Critical energy release rate test method for interface II type crack
CN112710566A