A spray structure, device and working method for passivation coating of cell slice sections
By setting two gas paths and setting the spacing between nozzles in the cut surface passivation coating process of the battery cell, we ensure that the gas forms a dense coating on the cut surface, and solving the problem of non-density and waste of coatings caused by the advance mixing of gases in the prior art, and realizing the More efficient coating process.
Patent Information
- Application Number
- CN202410931201.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-12
- Publication Date
- 2024-12-03
- Estimated Expiration
- 2044-07-12
AI Technical Summary
In the prior art, the reaction gas is mixed in advance in the air in the passivation coating process after battery slice, resulting in the problem that the coating is not dense enough and wastes raw materials.
Design a spray structure for passivation coating on the cutting surface of the battery cell. By setting two gas paths, the jets of passivating agent gas and oxidizing agent gas are respectively transported, and the spacing is set between the nozzles to ensure that the gas falls before falling to the cutting surface. They do not meet each other, thus forming a dense multi-layer coating on the cut surface.
It effectively avoids gas encounter and mixing in the air, improves the density of the coating, reduces waste of raw materials, and improves the quality and efficiency of the coating.
Smart Images

Figure CN118480868B_ABST
Abstract
Description
Technical Field
[0001] The present invention mainly relates to the technical field of photovoltaic cells, and in particular to a spray structure, a device and a working method for passivation coating of a cell section. Background Art
[0002] Photovoltaic cells are the core components of solar cell modules. Their quality and efficiency directly affect the power generation efficiency and life of the entire solar cell module. The current of photovoltaic cells flows along their surface, while the voltage is generated between the electrodes. When the area of photovoltaic cells is large, the route through which the current flows is extended, the resistance will increase, and thus a part of the electric energy will be lost, affecting the conversion efficiency. By cutting photovoltaic cells, reducing the area of a single cell, reducing the resistance of the current on the surface of the cell and the electron travel, the conversion efficiency of photovoltaic cells can be improved. For example, if the cell is cut in half and then connected in series, the current is reduced to half of the original. According to Joule's law, Q=I²Rt, so the electric loss caused by the resistance is 1 / 4 of the original. Therefore, after the photovoltaic cells are cut into small pieces, the resistance loss of the current on the surface of the cell is reduced, and the conversion efficiency of the solar cell is improved. It also reduces costs and improves yield.
[0003] At the same time, cutting photovoltaic cells can also reduce the scrap rate, reduce material waste, and thus reduce manufacturing costs.
[0004] In addition, dividing large-area photovoltaic cells into small pieces makes it easier to use them in different application scenarios and increases the flexibility of solar cell modules.
[0005] At present, the methods of dividing solar cells in industrial applications generally include laser scribing plus mechanical cracking, thermal laser low-damage cracking, etc. However, after the cell is divided, the section damage will occur, and the surface recombination rate on the cracked section of the cell is very large. That is, the section damage will produce a large recombination, resulting in a part of the power loss, which will have a great impact on the electrical performance of the solar cell. For example, after the Topcon solar cell is divided into two by laser scribing, the conversion efficiency of the half-cell will be reduced by 0.2-0.3% due to the increase in section recombination; the open circuit voltage of the heterojunction solar cell is higher, and the efficiency is reduced more after laser cracking. The reduction in solar cell efficiency caused by cutting will directly lead to a reduction in the power of the entire system including the sliced cells.
[0006] In order to reduce or remove the power loss caused by the cut surface damage, metal oxides such as aluminum oxide coating can be used to passivate the damaged area caused by the cut surface cutting. Specifically, the passivation coating refers to the formation of a passivation film on the end face of the silicon wafer of the side cut surface of the cell by deposition, thereby reducing minority carrier recombination, providing field passivation effect, and reducing reflectivity. As the quality of N-type silicon wafers and battery efficiency are getting higher and higher, the loss of cutting is also getting greater. Therefore, it is more important to perform passivation coating on the cut surface of the cell after slicing.
[0007] In the prior art, the process of passivation coating after battery slicing mostly adopts Chemical Vapor Deposition (CVD). Specifically, the passivator and oxidant, such as TMA (Trimethyl Aluminum) and water or ozone, are introduced into and contacted with the substrate surface to be coated, such as the cut surface, in a gaseous state, and then an atomic layer deposition (ALD) chemical reaction occurs on the substrate surface to generate a thin film and form a dense coating, such as an aluminum oxide coating. Existing passivation coating equipment, such as an aluminum oxide coating equipment, usually has two nozzles, which simultaneously spray TMA gas and oxidant gas to the battery slice placed on the plane below, and fall on the cut surface to generate a coating reaction to generate an aluminum oxide coating. However, because the cut surface has a certain length, the TMA nozzle and the oxidant nozzle need to be staggered. Therefore, before landing on the cut surface, the gaseous TMA and oxidant usually meet, mix, and react chemically in the air to generate aluminum oxide particles, which fall on the cut surface. This makes the passivation film produced not dense enough and wastes raw materials.
[0008] It can be seen that the current process of coating after battery slicing still has great deficiencies. Therefore, the existing technology needs to be further improved and enhanced. Summary of the invention
[0009] In view of the above-mentioned defects of the prior art, the object of the present invention is to provide a spray structure, device and working method for passivation coating of battery cell sections, so as to solve the technical problem in the current technology that the reaction gases are mixed in advance in the air during passivation coating of battery slices, resulting in insufficient density of the coating and waste.
[0010] The technical solution of the present invention is as follows:
[0011] The present invention first discloses a spray structure for passivation coating of a cell section, wherein the spray structure is arranged in a reaction chamber for accommodating a coating reaction, and is used to spray reaction gas toward the section of at least one cell, wherein the cell is loaded in a cell carrier box, and the cell carrier box is movable in the reaction chamber;
[0012] It includes two gas paths: a first gas path and a second gas path; wherein:
[0013] Each of the gas paths is provided with at least one nozzle, and the nozzle opens on and / or is suspended on the inner wall surface of the reaction chamber;
[0014] The first gas path is used to connect to an external passivator gas source / oxidant gas source, and includes a first nozzle for spraying a jet of passivator gas / oxidant gas toward the cut surface;
[0015] The second gas path is used to connect to an external oxidant gas source / passivant gas source, and includes a second nozzle for spraying a jet of oxidant gas / passivant gas toward the cut surface;
[0016] The first nozzle and the second nozzle are separately arranged and separated by at least a set distance;
[0017] The set interval is used to separate the jets ejected from the first nozzle and the second nozzle from each other before falling on the cut surface.
[0018] The spray structure for passivation coating of a cell section of the present invention is provided with two gas paths for conveying jets of a passivating agent gas and a jet of an oxidizing agent gas respectively, and the nozzles of the two gas paths are separately provided at a set interval to ensure that the jets of reactive gases ejected from all nozzles between the two gas paths will not meet in the air, so that no oxidation reaction will occur before falling on the section. At the same time, a wafer carrier is provided to carry the cell across at least one group of nozzles to move back and forth, so that the section receives the passivating agent gas and the oxidizing agent gas ejected from each nozzle in batches successively, so that a coating reaction can occur after the temperature conditions are met, and a dense multi-layer coating is produced. The present invention separates the nozzles of the two gas paths by at least a set spacing, and uses a wafer carrier to carry the battery cells across the nozzles, so that the cut surface receives the passivator jet and the oxidant jet successively, thereby ensuring that the passivator gas and the oxidant gas do not meet and mix in the air before falling on the cut surface, thereby avoiding chemical reactions in the air, generating oxide particles, and falling on the cut surface, resulting in reduced density of the coating on the cut surface and waste.
[0019] Preferably, the nozzle is a circular nozzle, and the set spacing satisfies the formula:
[0020]
[0021] in, h is the vertical distance from the nozzle to the section, is the turbulence coefficient, which is determined by experiments. The turbulence coefficient is related to the nozzle size and the jet velocity, and is preferably determined by experiments. Therefore, as long as the turbulence coefficient is determined by the nozzle size and the jet velocity (determined by the air supply pressure), for example, by experiments, the set spacing can be calculated based on the vertical distance between the nozzle and the section. d , and then arrange each of the first nozzles and each of the second nozzles, and keep them at least spaced by the set distance d , the arrangement of the nozzles can be completed to prevent the passivator gas and the oxidant gas from meeting in the air.
[0022] Preferably, the first gas circuit comprises a first main pipe with a hollow pipe inside, the first main pipe is connected to an external passivating agent gas source / oxidizing agent gas source, and at least one first gas outlet is opened on a side of the first main pipe; and further comprises a group of first branch pipes with hollow pipes inside, respectively connected to the first gas outlets; the first nozzle opens on the first branch pipe and is distributed along the axial direction of the first branch pipe;
[0023] The second gas circuit includes a second main pipe with a hollow pipe inside, the second main pipe is connected to an external oxidant gas source / passivating agent gas source, and at least one second gas outlet is opened on the side of the second main pipe; and also includes a group of second branch pipes with hollow pipes inside, which are respectively connected to each of the second gas outlets; the second nozzle opens on the second branch pipe and is distributed along the axial direction of the second branch pipe;
[0024] The first branch pipe and the second branch pipe are arranged substantially in parallel and substantially perpendicular to the moving direction of the slide box.
[0025] Specifically, the first branch pipe and the second branch pipe are arranged inside the reaction chamber, or close to the inner wall of the reaction chamber; and the first main pipe and the second main pipe can be arranged inside or outside the reaction chamber, and then the first branch pipe and the second branch pipe arranged roughly in parallel are respectively connected through the first air outlet or the second air outlet to form a centipede-shaped structure. This greatly simplifies the design of the entire spray structure, improves the stability of the connection between the branch pipe and the main pipe, and is more reliable. In addition, as long as the number, size, number of groups and intervals of the openings are controlled, the flow rate of the reaction gas entering the reaction chamber can be adjusted, the thickness of the generated coating layer can be controlled, and it is ensured that the oxidant gas and the passivator gas will not meet in the air. The first branch pipe and the second branch pipe are arranged roughly in parallel, which also helps to arrange as many groups of branches as possible in the reaction chamber, helping to form a denser oxide layer.
[0026] Further preferably, the first trunk pipe and the second trunk pipe are roughly parallel to the length direction of the reaction chamber; the first branch pipe and the second branch pipe are roughly perpendicular to the length direction of the reaction chamber; the wafer carrier box moves back and forth at a uniform speed along the length direction of the reaction chamber. Arranging the wafer carrier box to move back and forth at a uniform speed along the length direction of the reaction chamber can reduce the number of round trips compared to the width direction of the reaction chamber, and correspondingly reduce the inertial force caused by the switching of the moving direction to interfere with the reaction liquid layer on the cut surface; and the uniform motion can also prevent the ALD reactant from being disturbed by acceleration. Reducing the disturbance to the ALD reaction is more conducive to the generation of uniform and dense coatings. To control the thickness of the oxide layer or the coating, it is only necessary to adjust the number of branch pipes / air outlets. The roughly vertical connection facilitates the arrangement of the entire spray structure, and allows each part in the length direction of the cut surface to pass through each group of nozzles at the same time and receive reactants at the same time, so it also helps to maintain the consistency of each layer of coating on the cut surface in the length direction of the cut surface.
[0027] More preferably, the cut surface is placed parallel to the first branch pipe and the second branch pipe. Because the cell moves back and forth along the length direction of the two main pipes along with the cell carrier, placing the cell cut surface parallel to the branch pipes can ensure that all parts of the cut surface along the length direction of the cut surface are in contact with the gas ejected from each nozzle on the branch pipe at the same time, thereby ensuring that the coating thickness of each part of the cut surface is the same.
[0028] In one embodiment, the first trunk is set as one, the second trunk is set as two, the first trunk is located between the two second trunks; the first trunk is provided with the first air outlet on both sides of the left and right sides of the second trunk; the second air outlet is provided on the side of the second trunk facing the first trunk. In this embodiment, one trunk is placed in the middle and the other trunk is placed on both sides. Obviously, the left and right sides of the middle trunk can be kept in one-to-one correspondence with the first branch and the second branch, and accordingly, the first air outlet and the second air outlet can be ensured to be one-to-one corresponding, which makes it convenient for the cross section of the battery cell to receive the passivator gas and the oxidant gas uniformly in turn. Among them, the flow rate in the two trunks is determined by the specific reactants according to the reaction equation, but basically, the flow rate of the trunk located in the middle needs to be twice the pre-reaction coefficient of the corresponding reactant in the reaction equation.
[0029] In one embodiment, one end of the first branch pipe is a first open end connected to the hollow pipe inside the first branch pipe, and after the first open end is pluggably inserted into the first air outlet, the first branch pipe is connected to the first main pipe; and / or
[0030] One end of the second branch pipe is a second open end connected to the hollow pipe inside the second branch pipe. After the second open end is pluggably inserted into the second air outlet, the second branch pipe is connected to the second main pipe.
[0031] The open end and the air outlet are matched, and the two main pipes and the corresponding branch pipes are connected by a pluggable movable connection method, which is convenient for installation and disassembly, making the operation simpler and more convenient. Because the branch pipe is provided with a nozzle, and the nozzle opening is usually small, it is easy for sediment to accumulate in the branch pipe. After a period of use, it needs to be disassembled for cleaning. The pluggable structure is very convenient for installation and maintenance.
[0032] In one embodiment, the first open end is connected with the first air outlet by snapping: the first open end is provided with a first raised ring with a diameter slightly larger than the inner diameter of the first air outlet at a position adjacent to the terminal opening, the first raised ring is provided with a first contraction portion with an outer diameter slightly smaller than the inner diameter of the first air outlet and a length slightly larger than the thickness of the first air outlet on a side away from the terminal opening, and the first contraction portion is covered with a first elastic sealing ring; after the first open end is inserted into the first air outlet, the first sealing ring is squeezed to close the connection between the first air outlet and the first branch pipe; and / or
[0033] The second open end is snap-fittedly connected with the second air outlet: the second open end is provided with a second raised ring with a diameter slightly larger than the inner diameter of the second air outlet at a position adjacent to the terminal opening, and the second raised ring is provided with a second contraction portion with an outer diameter slightly smaller than the inner diameter of the second air outlet and a length slightly larger than the thickness of the second air outlet on the side away from the terminal opening, and an elastic second sealing ring is sleeved on the second contraction portion; after the second open end is inserted into the second air outlet, the second sealing ring is squeezed to close the connection between the second air outlet and the second branch pipe.
[0034] That is, a contraction part and a sealing ring are arranged at the open end of the branch pipe, and the sealing ring is made of an elastic material, such as rubber. When the raised ring is inserted into the air outlet, the contraction part follows and enters the cylindrical cavity of the air outlet. After the raised ring is inserted into the internal cavity of the main pipe, the sealing ring will produce a sealing effect due to being squeezed and deformed. Specifically, the sealing ring can block the air outlet from the outside of the air outlet or the inside of the air outlet along the radial direction. For example, the sealing ring is thinner and has a larger outer diameter. It is arranged at a section of the contraction part away from the raised ring. In this way, when inserted into the air outlet, the sealing ring remains outside the air outlet, and the sealing ring needs to be slightly squeezed so that the raised ring can completely enter the internal cavity of the main pipe. Then the sealing ring rebounds and pulls the raised ring outward, but the raised ring is blocked by the wall of the main pipe inside the air outlet, so that the sealing ring remains squeezed and deformed outside the air outlet, thereby blocking the air outlet. Alternatively, the sealing ring has a larger thickness and a smaller outer diameter, and is slightly inclined to wrap around the contraction portion, so that when inserted into the open end, the sealing ring follows the contraction portion and is inserted into the cylindrical cavity of the air outlet until the raised ring is inserted into the inner cavity of the main pipe. The sealing ring can completely block the opening hole radially due to rebound expansion. Of course, it is better that the sealing ring has a larger thickness, but the outer diameter of the sealing ring near the raised ring is small, while the outer diameter of the sealing ring away from the raised ring is larger, resulting in only the front half of the sealing ring following the contraction portion and inserted into the air outlet, and the rear half is retained outside. In this way, the sealing performance of the connection between the branch pipe and the main pipe is fully guaranteed.
[0035] More preferably, the section of the first raised ring / the second raised ring along the axial direction of the first branch pipe / the second branch pipe is close to a triangle, including an outer edge facing the end opening and an inner edge facing away from the end opening; the intersection of the outer edge and the inner edge is elastic, and the angle between the outer edge and the axial direction of the branch pipe is smaller than the angle between the inner edge and the axial direction of the branch pipe. Because the outermost circle diameter of the raised ring is slightly larger than the inner diameter of the air outlet, there will be a certain degree of difficulty when inserting the branch pipe into the main pipe. Usually, thermal expansion and contraction can be used to solve this problem. However, it is preferred to set at least the outermost circle, that is, the intersection of the outer edge and the inner edge, to be elastic, so that when plugging and unplugging, the intersection can be squeezed to reduce the maximum diameter of the raised ring. Setting the inclination of the outer edge smaller than the inclination of the inner edge will make it easier to insert, and additional force will be required to pull it out after insertion. This is also conducive to ensuring the firmness of the branch pipe after insertion and convenient daily operation.
[0036] In one embodiment, the reaction chamber is provided with a plurality of rollers arranged side by side, the wafer carrier is placed on the rollers, and driven to move in a linear manner by the rotation of the rollers, and passes through each of the first nozzles and the second nozzles in sequence. A row of rollers is provided in the lower part of the reaction chamber, for example, near the bottom, and the wafer carrier placed thereon is driven to move in a linear manner along the direction of rotation by the synchronous rotation of the rollers. This allows multiple wafer carriers to be placed at the same time, and can ensure that each wafer carrier performs the same translation action, thereby ensuring the consistency of the coating on the cut surface. At this time, each of the nozzles can be provided below the top wall of the reaction chamber, and correspondingly, the cut surface is placed in the wafer carrier facing upward. That is, the upper surface of the wafer carrier is vacant, and the cut surface is exposed upward; each of the nozzles can also be provided on the left and right side walls of the wafer carrier moving direction in the reaction chamber, and the cut surface is placed in the wafer carrier facing the left and right sides of the moving direction. That is, correspondingly, the surface of the wafer carrier on the left or right side of the moving direction is missing, and the cut surface is exposed and faces the inner wall of the reaction chamber on the left and right sides of the moving direction of the wafer carrier, so as to pass directly through each of the nozzles. At this time, the roller can only be provided with at most two rows of carrier boxes on the left and right sides along the length direction of the roller, and the missing surfaces on the carrier boxes are respectively facing the nozzles on the inner wall surface on the same side of the reaction chamber.
[0037] In one embodiment, a guide plate is further included which covers the first branch pipe and / or the second branch pipe, and the guide plate is provided with a guide groove along the axial direction of the branch pipe, and the first nozzle and / or the second nozzle is located in the guide groove. The provision of the guide plate is equivalent to reducing the distance between the nozzle and the cut surface, and further restricting the gas ejected from each nozzle to move forward in a straight line through the guide groove, which helps to further shorten the diffusion width of the ejected gas, and prevents the passivator gas and the oxidant gas ejected from the nozzles on the two adjacent branches from meeting before falling on the cut surface, causing an oxidation reaction, generating oxide particles, and falling on the cut surface to contaminate the coating on the cut surface.
[0038] The present invention also discloses a device for passivation coating of a cell section, comprising the reaction chamber, the inner wall surface of the reaction chamber being provided with a spray structure as described above, and the reaction chamber being further provided with a carrier for driving the wafer carrier box to translate along each nozzle;
[0039] A vacuum suction port is provided on the wall surface of the reaction chamber for sucking gas to reduce the gas pressure in the reaction chamber to near vacuum;
[0040] It also includes a heat radiation device for heating the cut surface to a reaction temperature by radiation, so that a coating reaction occurs and a dense coating layer is formed on the cut surface.
[0041] Adding a vacuum suction port and maintaining the reaction chamber near vacuum can help reduce the diffusion width of the nozzle jet, thereby reducing the set spacing, so that more groups of first nozzles and second nozzles can be arranged, thereby increasing the number and thickness of coating layers and further ensuring the quality of coating. By using the radiation heating method and the reaction chamber's internal environment close to vacuum, only the cut surface can reach the reaction temperature, ensuring that the coating reaction occurs on the cut surface. At the same time, even if the reaction gases meet in the air, the oxidation reaction cannot occur because the temperature is not high enough.
[0042] The present invention also discloses a working method of the device for passivation coating of a cell section, which comprises the steps of:
[0043] A. the first nozzle ejects a jet of passivator gas / oxidant gas;
[0044] B. the second nozzle ejects a jet of oxidant gas / passivator gas;
[0045] C. The carrier drives the wafer carrier to move and sequentially passes through at least one group of the first nozzle and the second nozzle;
[0046] D. the passivator gas and the oxidant gas fall on the cut surface;
[0047] E. After the heat radiation device heats the cut surface to a reaction temperature, a coating reaction occurs on the cut surface;
[0048] Step A and step B are performed simultaneously.
[0049] That is, the spray structure of the present invention is provided with two groups of nozzles, and the two groups of nozzles are separated by a set interval, and the cut surface is arranged to translate and cross each nozzle, and the reaction gas jet injected from each nozzle is received, and the cut surface is heated to the reaction temperature by the heat radiation device at the same time, and the coating reaction occurs. This avoids the oxidation reaction occurring in advance due to the reaction gas flow meeting in the air, and the generated oxide solid particles fall on the cut surface, which affects the coating quality.
[0050] The present invention will be explained in detail below with reference to the accompanying drawings and specific embodiments. BRIEF DESCRIPTION OF THE DRAWINGS
[0051] Figure 1 This is the overall system diagram of the cell section passivation coating machine;
[0052] Figure 2 The schematic diagram of the system after the cell is placed in the cell carrier box;
[0053] Figure 3 Setting the spacing in the spray structure for passivation coating of the cell section of the present invention d Schematic diagram of calculation;
[0054] Figure 4 It is a schematic diagram of the overall structure of the gas path in the spray structure used for the passivation coating of the cell section of the present invention;
[0055] Figure 5 It is a schematic diagram of the structure of the branch pipe in the spray structure used for the passivation coating of the cell section of the present invention;
[0056] In the figure: 10-reaction chamber, 11-passivator tube, 12-oxidant tube, 13-motor, 14-roller, 15-carrier plate, 16-suction tube, 20-carrier box, 21-opening groove, 22-battery cell, 23-section, 25-nozzle, 27-air inlet, 100-chamber inner wall, 110-first main pipe, 115-first branch pipe, 120-second main pipe, 125-second branch pipe, 130-guide plate, 135-guide groove, 250-nozzle plate, 261-branch pipe groove, 262-sealing ring, 263-raised ring. DETAILED DESCRIPTION
[0057] To facilitate understanding of the present invention, the present invention will be described more comprehensively below with reference to the relevant drawings. Several embodiments of the present invention are given in the drawings, but the present invention can be implemented in different forms and is not limited to the embodiments described in the text. On the contrary, these embodiments are provided to make the content disclosed in the present invention more thorough and comprehensive.
[0058] It should be noted that when an element is considered to be "connected" to another element, it may be directly connected to another element or there may be a central element at the same time. The terms "vertical", "positive", "negative" and similar expressions used in this article are based on the direction or position relationship shown in the drawings. This is only for the convenience of description, and does not indicate or imply that the system or element must have a specific orientation, be constructed and operated in a specific orientation. Therefore, it cannot be understood as a limitation on this application. In addition, the terms "first", "second", "third" and "fourth" are used for descriptive purposes only and cannot be understood as indicating or implying relative importance.
[0059] In addition, it should be noted that in the description of this application, unless otherwise clearly specified and limited, the terms "installed", "connected", and "connected" should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection or an indirect connection through an intermediate medium, or it can be the internal communication of two components. For those skilled in the art, the specific meanings of the above terms in this application can be understood according to the specific circumstances.
[0060] Unless otherwise defined, all technical and scientific terms used herein have the same meaning as commonly associated with those skilled in the art to which the invention belongs. The terminology used in the specification of the present invention is for the purpose of describing specific embodiments and is not intended to limit the present invention.
[0061] The present invention discloses a spray structure, device and working method for passivation coating of cell sections. Usually, the TMA oxidation method is generally used for coating of cell sections. Here, the technical solution of the present invention is described in detail by taking the oxidation of TMA to generate aluminum oxide for coating of silicon wafers as an example. But it is obvious that the use of other reactants is similar. The spray structure of the present invention is arranged in a reaction chamber in a coating device for accommodating the occurrence of coating reactions. Among them, an embodiment of the coating device has an overall structure as follows Figure 1 As shown, it includes a reaction chamber 10 for accommodating the occurrence of the coating reaction, a passivator tube 11 and an oxidant tube 12 for connecting an external passivator gas source and an oxidant gas source, and at least two nozzles are arranged on the inner wall surface of the reaction chamber 10 or suspended near the inner wall surface, and the passivator gas jet and the oxidant gas jet are respectively sprayed into the reaction chamber 10. A vacuum suction port is arranged on the wall surface of the reaction chamber 10, which is connected to an external vacuum source through a suction pipe 16 to suck the gas inside the reaction chamber 10 to maintain a near-vacuum low pressure of about 10-100 Pascal in the reaction chamber 10.
[0062] In the reaction chamber 10, a carrier is provided to drive the objects thereon to move in translation, for example Figure 1 A row of rollers 14 in the conveyor belt rotates in the same direction at the same time under the driving system, such as the rotation of the motor 13 and the transmission drive of the conveyor belt, and drives the items thereon, such as the film carrier box 20, to translate together. A stack of battery cells 22 is inserted into the film carrier box 20, and the cut surface 23 to be coated in the battery cell 22 faces outward and is perpendicular to the injection direction of the nozzle 25. Specifically, the roller 14 rotates in situ, driving the film carrier box 20 placed on the roller 14 to translate across the roller 14. And when the film carrier box 20 translates to close to the wall, the motor 13 rotates in the opposite direction. That is, the motor 13 drives the film carrier box 20 to reciprocate along the plane. In order to ensure the stability of the movement of the film carrier box 20, the film carrier box 20 needs to keep in contact with at least two rollers 14 at the same time during the movement, that is, the spacing between the rollers 14 should be less than half the length of the bottom of the film carrier box 20. Or more preferably, a larger carrier plate 15 is placed on the roller 14, and each carrier box 20 is arranged in a similar posture on the carrier plate 15. In this way, because the carrier plate 15 can contact multiple rollers 14 at the same time, the translation of the carrier box 20 is more stable, ensuring that the reaction gas received by the cut surface 23 is more uniform.
[0063] Specifically, in one embodiment, the nozzles 25 are divided into two categories, one for spraying oxidant gas jets, and the other for spraying passivant gas jets. Each type of nozzle is connected to the corresponding main pipe through at least one branch pipe, and then connected to the passivator pipe 11 or the oxidant pipe 12 through the main pipe to connect to the external passivator gas source or oxidant gas source. Preferably, each type of nozzle 25 includes a plurality of nozzles, which are dispersed and arranged in an array. In this embodiment, the overall structure of the spray structure is designed to include at least two gas paths, a first gas path and a second gas path, which are used to transport passivator gas and oxidant gas, respectively. Specifically, each gas path includes at least one main pipe and at least one branch pipe that opens / connects a group of nozzles, and the branch pipes of the same gas path are connected to the main pipe. In particular, each branch pipe is arranged in parallel and side by side in the shape of a centipede leg, and is inserted roughly vertically into the air outlet opened on the side of the corresponding main pipe. The branch pipes of the spray structure and the nozzles disposed on the branch pipes are disposed on the inner wall surface 100 of the reaction chamber 10, or suspended near the inner wall surface 100 of the chamber. The main pipe is then connected to the passivator pipe 11 or the oxidant pipe 12 to connect to the corresponding external gas source. In one embodiment, Figure 1 As shown, the passivator tube 11 and the oxidant tube 12 are both arranged on the outer surface of the reaction chamber 10 to facilitate the connection with the external gas source, so that the oxidant gas or the passivator gas is respectively introduced into the corresponding main tubes, and then transported to the corresponding branch pipes dispersedly arranged inside the reaction chamber 10, and then sprayed into the reaction chamber 10 from the corresponding nozzles, and fell on the moving section 23. After the section 23 meets the temperature conditions, a multi-level coating reaction occurs. In a more preferred embodiment, the battery cell 22 is arranged parallel to the axis of the branch pipe, so that during the movement, each part of the section 23 in the length direction of the battery cell section moves to face each branch pipe at the same time, and receives the gas sprayed from the nozzle on each branch pipe at the same time, so as to ensure that each part of the section 23 along the branch pipe axis is uniformly coated.
[0064] The specific structure of the slide box 20 is as follows Figure 2As shown, one side of the wafer carrier 20 is provided with an opening groove 21, and the battery cells 22, especially a plurality of battery cells, are closely attached to each other to form a cuboid, inserted into the opening groove 21, and the opening groove 21 is blocked to prevent the oxidant gas and / or passivating agent gas such as TMA fed from the nozzle from entering the wafer carrier 20, thereby preventing the occurrence of unwanted coating on the front and / or back of the battery cell 22. In a more preferred embodiment, the wafer carrier 20 may also be provided with a (group of) air inlets 27, such as on the bottom or side surface, through which a gas that does not chemically react with the reaction gas fed from the nozzle, such as an inert gas or nitrogen, is sprayed into the wafer carrier 20 to increase the internal air pressure of the wafer carrier 20, or the reaction gas that enters between the battery cells 22 is directly blown out, so as to further prevent the oxidant gas and / or passivating agent gas fed from the nozzle from entering the wafer carrier 20, resulting in the occurrence of wrap-around plating. Furthermore, the gas injected from the air inlet 27 can also cool the front and back sides of the battery cell 22 adjacent to the cut surface 23 so that the reaction temperature cannot be reached.
[0065] The battery cells 22 are very thin, with a thickness of about 120 microns, so they are usually inserted in a stack at a time, 100-1000 pieces, with a thickness of 12 mm-12 cm. When inserting multiple battery cells, the battery cells 22 are neatly arranged and stacked into a rectangular parallelepiped, with the cut surface 23 to be coated facing the same side, and then neatly inserted into the opening groove 21, leaving the cut surface 23 on the outside facing outward, while the whole stack of battery cells 22 blocks the opening groove 21. In a more preferred embodiment, the opening length of the opening groove 21 can be adjusted to accommodate the stacking of battery cells 22 with different numbers of layers and thicknesses. For example, through a system such as a spring, a movable edge of the opening groove 21 is pushed or pulled to change the length of the opening groove 21, and the movable edge is kept always in contact with the battery cell 22 with a certain pressure, especially the slightly raised grid lines on each battery cell 22 are completely in contact with each other. Although the protrusion height of the grid lines is only about 10-20 microns, they are close to each other, which can better ensure that the opening groove 21 is blocked and prevent the gas injected from the nozzle from entering the carrier box 20.
[0066] It should be noted that the gas injected into the wafer carrier 20 from the air inlet 27 preferably flows in the lateral direction of each cell 22, that is, parallel to the length direction of the cut surface 23, while the reaction gas flow injected from each nozzle is in the vertical direction facing the cut surface 23. In this way, the two airflow directions are kept as perpendicular to each other as possible to avoid airflow collision, which can minimize the interference with the reaction gas flow after it contacts the cut surface 23 and heats up, and the coating reaction occurs. Of course, limiting the airflow injected from the air inlet 27 to have a smaller momentum can also reduce the interference.
[0067] The wafer carrier 20 with the cell 22 placed thereon can be placed on the carrier in the reaction chamber 10, and driven by the carrier to move back and forth, crossing each branch pipe in turn. When passing through the nozzles 25 provided on each branch pipe, the exposed cut surface 23 receives the injected reactant gas, such as TMA and ozone, successively. After the temperature of the cut surface 23 reaches the reaction temperature, a passivation coating reaction occurs. The nozzles 25 can be provided on the inner wall surface of the top surface of the reaction chamber 10, and the gas is sprayed downward toward the carrier, at which time the cut surface 23 is exposed on the upper surface of the wafer carrier 20; the nozzles 25 can also be provided on the inner wall surfaces on the left and right sides of the translation direction of the wafer carrier 20 in the reaction chamber 10, or suspended near the left and right inner wall surfaces, and the reaction gas is sprayed horizontally toward the wafer carrier 20. At this time, the wafer carrier 20 is placed so that the opening grooves 21 face the inner wall surfaces on the left and right sides, and the cut surface 23 is also exposed to the nozzles 25.
[0068] In a more preferred embodiment, if Figure 1 As shown, a larger carrier plate 15 can be added to contact more rollers 14 at the same time to further ensure the stability of translation. The smaller carrier boxes 20 are arranged in an array on the carrier plate 15, so that when the carrier plate 15 is driven to translate by the carrier, it will carry the multiple carrier boxes 20 placed on it to translate back and forth. At this time, because the carrier box 20 lies flat on the carrier plate 15, the battery cell 22 stands upright in the carrier box 20 with the cut surface 23 facing upward. At this time, each nozzle 25 is installed or suspended on the inner side of the top cover above the reaction chamber 10. The cut surface 23 can always remain facing the injection direction of the nozzle 25 to receive the oxidant gas (such as water vapor or ozone) and passivator gas (such as TMA) injected from each nozzle. The carrier plate 15 is set up, and the number of rollers 14 that are simultaneously contacted and supported at the bottom is increased through a larger bottom area, which further ensures the stability of the movement of the carrier box 20, thereby ensuring the uniformity of the coating on the cut surface 23.
[0069] Of course, the carrier may also adopt any common transmission method in the prior art, such as a conveyor belt, etc., as long as it can drive the wafer carrier box 20 to translate stably and the cut surface 23 remains stably facing the nozzle 25.
[0070] Because the wafer carrier 20 is translated across the branches, the reaction gas ejected from the nozzles 25 falls on the cut surface 23 in sequence, and a multi-layer coating reaction can occur at the reaction temperature. d , it should be ensured that the oxidant gas and the passivant gas do not meet in the air before falling on the cut surface 23, so as to avoid oxidation reaction, which will waste materials on the one hand, and on the other hand, the generated oxide particles will fall on the cut surface 23, which will affect the quality of the coating. In one embodiment, the nozzle is a circular nozzle, and the set spacingd The calculation diagram is as follows Figure 3 As shown, at this time, the set spacing d Satisfy the formula:
[0071]
[0072] in, h is the vertical distance from the nozzle 25 to the cut surface 23, The turbulence coefficient is related to the nozzle and the jet velocity and can be determined by experiment. In theory, the turbulence coefficient is related to the size and shape of the nozzle, the flow velocity, viscosity, density, etc. of the jet, so after selecting the nozzle, it is preferably determined by experiment. h is the vertical distance from the nozzle 25 to the cut surface 23, h The larger the jet diffusion angle is, the greater the width of the jet diffusion is, because the jet diffusion angle remains basically unchanged. Accordingly, a larger set spacing is required between adjacent nozzles 25. d , in order to ensure that the jets do not meet in the air and undergo oxidation reaction before falling on the cut surface 23. If the pressure in the reaction chamber 10 is usually controlled to be low, the diffusion will be less under the same conditions, that is, at the same distance h At this point, the width of the jet diffusion will become smaller, so the spacing between the corresponding nozzles 25 on the two branches is d It can also be smaller accordingly.
[0073] During the movement of the wafer carrier 20, the spraying direction of the nozzles 25 is perpendicular to the translation direction of the wafer carrier 20, so that the cut surface 23 facing the nozzles can pass through each group of nozzles in sequence, receive the gas sprayed by the nozzles 25, and generate a coating reaction. In addition, nozzles 25 are dispersedly arranged on the entire translation path of the wafer carrier 20 to ensure that the coating has sufficient layers and thickness.
[0074] In one embodiment, Figure 4As shown, three main pipes are provided, and the three main pipes are extended in parallel along the length direction of the reaction chamber 10. The first main pipe 110 is located at the middle position of the width of the inner wall surface 100 of the reaction chamber 10, and air outlets for connecting the branch pipes are opened on the left and right sides, and a row of first branch pipes 115 are connected nearly vertically through the air outlets; and the second main pipe 120 is located at the left and right side surfaces of the width of the inner wall surface 100 of the chamber, and only the side facing the middle position of the width of the inner wall surface 100 of the chamber has an air outlet for connecting the branch pipes, and a row of second branch pipes 125 are connected nearly vertically through the air outlets. At the same time, on the left and right sides of the first main pipe 110, a first branch pipe 115 and a second branch pipe 125 are alternately arranged. Correspondingly, the first nozzle and the second nozzle on each branch pipe also correspond one to one, that is, the connecting line between the corresponding two nozzles is parallel to the main pipe, but the spacing is maintained at least d In this way, the battery cell 22 passes through each group of nozzles during the movement, and receives the passivation gas and the oxidant gas on the cut surface 23 in turn, and when the temperature reaches the reaction temperature, the coating reaction occurs.
[0075] Specifically, the passivating agent is TMA, the oxidizing agent is ozone or water vapor, and the nozzle is a circular opening with an aperture of 0.5 mm. The first nozzles on the first branch pipe 115 are spaced 4 mm apart; the second nozzles on the second branch pipe 125 are also spaced 4 mm apart; the first branch pipe 115 and the second branch pipe 125 are spaced 4 cm apart, that is, d At this time, the translation direction of the wafer carrier 20 is along the main pipe, and the translation speed is 10 cm per second. The total flow of the first nozzle / the second nozzle, that is, the flow in the oxidant tube 12 / the passivator tube 11, exceeds 2 liters per second.
[0076] The specific structure of the branch pipe is as follows Figure 5As shown, it is a hollow polygonal column or cylinder, including an open end for inserting and connecting the outlet hole to introduce the passivator / oxidant gas; and a nozzle surface provided with or connected to multiple nozzles 25 in the same group to spray out the passivator gas jet / oxidant gas jet. In one embodiment, the open end is pluggable and connected to the outlet hole. Specifically, the open end is provided with a raised ring 263 near the terminal opening, the outer diameter of the raised ring 263 is slightly larger than the inner diameter of the outlet hole, and the open end is provided with a contraction portion with an outer diameter slightly smaller than the inner diameter of the outlet hole and a length slightly larger than the thickness of the outlet hole on the side of the raised ring 263 away from the terminal opening; the contraction portion is at least in a section away from the raised ring 263, and is covered with a sealing ring 262 made of elastic material such as rubber. When the open end is inserted into the vent, the raised ring 263 is inserted into the vent and enters the internal channel of the main pipe. At this time, the sealing ring 262 is pressed against the outer wall of the main pipe / vent and is squeezed and deformed, thereby achieving the technical effect of sealing the vent. Specifically, in one embodiment, the sealing ring 262 is arranged at the root of the contraction part away from the open end, and the thickness is relatively thin, but the outer diameter is larger than the opening diameter of the vent. In this way, when the open end is inserted into the vent, the sealing ring 262 will not enter the vent, but the sealing ring 262 needs to be slightly squeezed to deform before the raised ring 263 can be completely inserted and engaged with the inner wall of the vent. Then the sealing ring 262 rebounds under elasticity and pulls the raised ring 263 outward. However, because the maximum diameter of the raised ring 263 is slightly larger than the inner diameter of the vent, the outer side of the vent and the end of the contraction part together keep squeezing the sealing ring 262, thereby blocking the vent. In another embodiment, the sealing ring 262 can also be designed to be thicker and be sleeved on the contraction portion along the axial direction of the branch pipe, with a slight cone shape, so that it follows the raised ring 263 to be inserted or partially inserted into the air outlet and is pressed to seal the air outlet.
[0077] Because the outermost diameter of the raised ring 263 is slightly larger than the inner diameter of the air outlet, it is difficult to insert the branch pipe into the main pipe. If the raised ring 263 is made of hard material, the insertion problem can be solved by methods such as thermal expansion and contraction. In a more preferred embodiment, the section of the raised ring 263 along the axial direction of the branch pipe can be close to a triangle, consisting of an outer edge, an inner edge and a bottom edge, wherein the outer edge is located on the side of the end opening, the inner edge is located on the side of the sealing ring 262, and the bottom edge is along the axial direction of the branch pipe, and the angle between the outer edge and the bottom edge is smaller than the angle between the inner edge and the bottom edge, and at least at the vertex, it has a certain elasticity. In particular, the whole of the raised ring 263 is a triangular ring structure made of an elastic sheet with a certain strength, such as a metal sheet. In this way, when inserting the air outlet at the open end, because the inclination of the outer edge is low and it has a certain elasticity at least at the height close to the vertex, it is easy to insert the air outlet. However, after insertion, because the inner edge angle is greater than the outer edge angle, the inner edge is more inclined and closer to the vertical position, so extra force is required to pull it out. This is also conducive to ensuring the firmness of the branch pipe after insertion and facilitating daily plug-in and pull-out operations.
[0078] In a more preferred embodiment, for the convenience of manufacturing, each group of nozzles 25 can be separately arranged on a nozzle plate 250. Among them, a branch pipe groove 261 connected to the open end is opened on the side of the branch pipe. When the nozzle plate 250 is covered on the branch pipe groove 261, all nozzles on the nozzle plate 250 are in the branch pipe groove 261 in a horizontal position. In order to ensure that the airflow direction ejected from the nozzle is perpendicular to the branch pipe to reduce diffusion and mutual mixing in the air, in a more preferred embodiment, a guide plate 130 is also covered on the nozzle 25. The guide plate 130 has a narrow and long guide groove 135. After covering the nozzle 25, the nozzle 25 falls into the guide groove 135 in the horizontal direction. This can be achieved by adjusting the thickness of the guide groove 135 and shortening the distance between the nozzle 25 and the cut surface 23, thereby reducing the diffusion width of the ejected gas in the air and preventing the gases ejected from different branches from contacting and mixing with each other before falling on the cut surface 23, causing chemical reactions and producing fixed precipitates that fall on the cut surface 23 and affect the strength of the coating.
[0079] Usually, in order to reduce the diffusion width and increase the gas flow rate, the distance between the nozzle 25 and the cut surface 23 can be set very small, such as only a few millimeters, and the gas flow rate can be several liters per second, thereby accelerating the efficiency of the passivation coating.
[0080] When the gas falls on the cut surface 23, the oxidant gas and the passivating agent gas will undergo a coating reaction at the reaction temperature, and the product will be deposited on the exposed cut surface 23 to achieve a coating effect. For example, ozone and TMA gases are sent into the reaction chamber 10 through their respective nozzles, and fall on the cut surface 23 successively, or because the temperature of the gas itself has exceeded the reaction temperature, or the temperature of the cut surface 23 is raised to exceed the reaction temperature by a heating device, a coating reaction will occur, and aluminum oxide will be deposited on the cut surface 23 to achieve a passivation coating. Among them, the heating device, considering that the interior of the reaction chamber 10 is close to a vacuum and cannot be heated by gas conduction or gas convection, is preferably a heat radiation device, and heats by heat radiation, such as an infrared heater that emits light toward the cut surface 23. More preferably, considering that the wafer carrier 20 is in motion, a motion device can be added to drive the heat radiation device to move or rotate synchronously with the wafer carrier 20, and keep the radiation direction of the heat radiation device always pointing to the cut surface 23.
[0081] During the entire coating reaction process, the vacuum suction port is connected to an external vacuum source through the suction tube 16 to keep sucking the gas in the reaction chamber 10 and maintain the reaction chamber 10 at an extremely low pressure close to vacuum, for example, only tens of Pascals, so as to reduce the jet diffusion width of the reaction gas and prevent the jet from heating up in the air.
[0082] The above is an exemplary description of the present invention in conjunction with the accompanying drawings. It is obvious that the specific implementation of the present invention is not limited to the above-mentioned method. As long as such non-substantial improvements are made by adopting the method concept and technical solution of the present invention, or the concept and technical solution of the invention are directly applied to other occasions without improvement, they are all within the protection scope of the present invention.
Claims
1. A device for passivation coating of a cell section, characterized in that: It comprises a reaction chamber for accommodating the occurrence of a coating reaction, wherein a spray structure is arranged on the inner wall surface of the reaction chamber, and the spray structure is used to spray a reaction gas toward a cut surface of at least one battery cell, wherein the battery cell is loaded in a carrier box, and the carrier box is movable in the reaction chamber; It includes two gas paths: a first gas path and a second gas path; wherein: Each of the gas paths is provided with at least one nozzle, and the nozzle opens on and / or is suspended on the inner wall surface of the reaction chamber; The first gas path is used to connect to an external passivating agent gas source, and includes a first nozzle, which is used to spray a jet of the passivating agent gas toward the cut surface; The second gas path is used to connect to an external oxidant gas source, and includes a second nozzle for spraying a jet of oxidant gas toward the cut surface; The first nozzle and the second nozzle are separately arranged and separated by at least a set distance; The set interval is used to make the jets ejected from the first nozzle and the second nozzle separate from each other before falling on the cut surface; The reaction chamber is also provided with a carrier for driving the wafer carrier box to move along each nozzle; A vacuum suction port is provided on the wall surface of the reaction chamber for sucking gas to reduce the gas pressure in the reaction chamber to vacuum; Also included is a heat radiation device for heating the cut surface to a reaction temperature by radiation.
2. The device according to claim 1, characterized in that The nozzle is a circular nozzle, and the set spacing satisfies the formula: in, h is the vertical distance from the nozzle to the section, is the turbulence coefficient, determined by experiment.
3. The device according to claim 1 or 2, characterized in that: The first gas path includes a first main pipe with a hollow pipe inside, the first main pipe is connected to an external passivating agent gas source, and at least one first gas outlet is opened on the side of the first main pipe; and also includes a group of first branch pipes with hollow pipes inside, which are respectively connected to the first gas outlets; the first nozzle opens on the first branch pipe and is distributed along the axial direction of the first branch pipe; The second gas circuit includes a second main pipe with a hollow pipe inside, the second main pipe is connected to an external oxidant gas source, and at least one second gas outlet is opened on the side of the second main pipe; and also includes a group of second branch pipes with hollow pipes inside, which are respectively connected to the second gas outlets; the second nozzles are opened on the second branch pipes and distributed along the axial direction of the second branch pipe; The first branch pipe and the second branch pipe are arranged in parallel and perpendicular to the moving direction of the slide box.
4. The device according to claim 3, characterized in that The first main pipe and the second main pipe are parallel to the length direction of the reaction chamber; the first branch pipe and the second branch pipe are perpendicular to the length direction of the reaction chamber; the wafer carrier box translates back and forth at a uniform speed along the length direction of the reaction chamber.
5. The device according to claim 3, characterized in that: One end of the first branch pipe is a first open end connected to the hollow pipe inside the first branch pipe, and after the first open end is pluggably inserted into the first air outlet, the first branch pipe is connected to the first main pipe; and / or One end of the second branch pipe is a second open end connected to the hollow pipe inside the second branch pipe. After the second open end is pluggably inserted into the second air outlet, the second branch pipe is connected to the second main pipe.
6. The device according to claim 5, characterized in that: The first opening end is connected with the first air outlet by snapping: the first opening end is provided with a first raised ring with a diameter larger than the inner diameter of the first air outlet at the terminal opening, the first raised ring is provided with a first contraction portion with an outer diameter smaller than the inner diameter of the first air outlet and a length larger than the thickness of the first air outlet on the side away from the terminal opening, and the first contraction portion is covered with an elastic first sealing ring; after the first opening end is inserted into the first air outlet, the first sealing ring is squeezed to close the plug-in connection between the first air outlet and the first branch pipe; and / or The second open end is snap-fittedly connected with the second air outlet: the second open end is provided with a second raised ring with a diameter larger than the inner diameter of the second air outlet at the terminal opening, and the second raised ring is provided with a second contraction portion with an outer diameter smaller than the inner diameter of the second air outlet and a length larger than the thickness of the second air outlet on the side away from the terminal opening, and the second contraction portion is covered with an elastic second sealing ring; after the second open end is inserted into the second air outlet, the second sealing ring is squeezed to close the connection between the second air outlet and the second branch pipe.
7. The device according to claim 6, characterized in that The cross-section of the first raised ring along the axial direction of the first branch tube is a triangle, and / or the cross-section of the second raised ring along the axial direction of the second branch tube is a triangle, and the triangle includes an outer edge facing the end opening and an inner edge facing away from the end opening; the intersection of the outer edge and the inner edge is elastic, and the angle between the outer edge and the axial direction of the branch tube is smaller than the angle between the inner edge and the axial direction of the branch tube.
8. The device according to claim 3, characterized in that It also includes a guide plate covering the first branch pipe and / or the second branch pipe, wherein the guide plate has a guide groove along the axial direction of the branch pipe, and the first nozzle and / or the second nozzle is located in the guide groove.
9. A working method of the device for passivation coating of a cell section according to any one of claims 1 to 8, characterized in that: Includes steps: A. the first nozzle ejects a jet of passivating agent gas; B. the second nozzle ejects a jet of oxidant gas; C. The carrier drives the wafer carrier to move and sequentially passes through at least one group of the first nozzle and the second nozzle; D. the passivator gas and the oxidant gas fall on the cut surface; E. After the heat radiation device heats the cut surface to a reaction temperature, a coating reaction occurs on the cut surface; Step A and step B are performed simultaneously.