A control system and method for preparing anti-corrosion, anti-wax and anti-fouling coating

By introducing a control system of inspection items, processes, risk assessment and adjustment modules in the paint preparation process, the complex process and inspection problems in paint sample preparation are solved, timely positioning and correction are achieved, and data accuracy and safety are improved.

CN118485310BActive Publication Date: 2024-10-22甘肃衍河石油管道涂层有限公司
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
CN202410824530.1
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2024-06-25
Publication Date
2024-10-22
Estimated Expiration
2044-06-25

AI Technical Summary

Technical Problem

In the preparation process of modified paint samples, due to the large number of inspection items and complex process steps, the proportions and parameter adjustments are complicated, and problems with the inspection items cannot be located in time, resulting in inaccurate test data and inaccurate prediction results, which affects preparation safety.

Method used

Provide a control system, including inspection project module, process module, risk assessment module and adjustment module. By setting the sampling cycle and risk level assessment, the sampling frequency of the process period is adjusted, process problems are discovered and corrected in a timely manner, and data accuracy and safety are improved. sex.

Benefits of technology

It achieves timely location of inspection project problems, avoids inaccurate prediction results, improves preparation safety, and ensures coating quality and process stability.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118485310B_ABST
    Figure CN118485310B_ABST
Patent Text Reader

Abstract

The present application provides a control system and method for preparing anti-corrosion, anti-wax and anti-fouling coatings, including an inspection item module, a process module, a risk assessment module and an adjustment module; wherein the inspection item module includes inspection items for inspecting and evaluating samples; the process module includes processes and process periods when preparing samples, and a sampling period is set in the process period; wherein a process with a certain degree of association with the inspection item is set as an associated process of the inspection item, and when the inspection item fails the inspection assessment, the associated process of the inspection item is used as a risk process; the risk assessment module is used to assess the degree of danger of the risk process and obtain the danger level of the risk process; the adjustment module adjusts the sampling period in the process period of the risk process according to the danger level of the risk process. The present application improves the safety and stability of preparation.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present application relates to the field of coating preparation for petroleum oil pipes, and in particular to a control system and method for preparing anti-corrosion, anti-wax and anti-fouling coatings. Background Art

[0002] Existing oil pipe coatings are generally based on epoxy resin. Since epoxy resin has good adhesion to metal surfaces and has excellent alkali resistance, chemical resistance and flexibility, it is a coating with good performance. However, in some extreme or harsh use environments, such as when used in oil pipes deep underground, higher requirements are placed on the performance stability, shrinkage and yield of the coating. Therefore, the inspection indicators of the coating samples in terms of anti-corrosion, anti-wax and anti-fouling performance are also more stringent. In order to meet the above requirements, phenolic resin will be used to adjust the epoxy resin, that is, epoxy phenolic resin is used as the base material, and pigments, fillers, solvents, additives and other materials are added. After grinding to the required fineness, the material is filtered out in a proportion. The modified coating film obtained after the addition of phenolic resin retains the advantages of strong adhesion, high flexibility and good alkali resistance of epoxy resin, and has the excellent water resistance, solvent resistance and acid resistance of phenolic resin, which can improve the overall anti-corrosion, anti-wax and anti-fouling effects of the coating. During the preparation of modified coating samples, due to the adjustments to the preparation process steps, the test ratio, parameter adjustment, and final inspection items become more complicated. Therefore, when problems occur in some of the inspection items, it is often impossible to locate which process step caused the problem in time, and it is impossible to determine whether it is caused by improper process operation. This will make the data acquisition of the test samples inaccurate, the results of predicting the sample quality inaccurate, and it is impossible to promptly discover and correct the corresponding process problems and equipment problems in advance, and the safety of the preparation is also affected. Summary of the invention

[0003] The following description is used to disclose the present invention so that those skilled in the art can implement the present invention. The preferred embodiments described below are only examples, and those skilled in the art can think of other obvious variations. The basic principles of the present invention defined in the following description can be applied to other embodiments, variations, improvements, equivalents, and other technical solutions that do not deviate from the spirit and scope of the present invention.

[0004] To solve the technical problem, the present application provides a control system for preparing an anti-corrosion, anti-wax and anti-fouling coating, comprising an inspection project module, a process module, a risk assessment module and an adjustment module;

[0005] Wherein, the inspection item module includes inspection items for inspecting and evaluating samples;

[0006] The process module includes a sample process and a process period, and a sampling period is set in the process period;

[0007] Wherein, a process with a certain degree of association with the inspection item is set as an associated process of the inspection item, and when the inspection item fails the inspection assessment, the associated process of the inspection item is used as a risk process;

[0008] The risk assessment module is used to assess the risk level of the risk process and obtain the risk level of the risk process;

[0009] The adjustment module adjusts the sampling period in the process period of the risk process according to the risk level of the risk process;

[0010] The risk process is sampled using the adjusted sampling cycle, and the hazard level of the risk process is re-evaluated based on the sampling results.

[0011] Among them, preferably, the inspection items for inspection and evaluation of the anti-corrosion, anti-wax and anti-fouling coating samples include: hardness, bending strength, corrosion resistance, adhesion, heat resistance, wear resistance, bending resistance and impact resistance.

[0012] Among them, preferably, the environmental temperature for inspection and evaluation of the anti-corrosion, anti-wax and anti-fouling coating samples is 200°C, the pH value is 1-13, the upper limits of H2S and CO2 gas content are 10% and 95% respectively, and the internal pressure of the environment is 7MPa.

[0013] The present application also provides a control method for a control system for preparing an anti-corrosion, anti-wax and anti-fouling coating as described above, comprising the following steps:

[0014] S1, set the inspection and evaluation of the prepared samples to include n types of inspection items, and the preparation process of the prepared samples includes k preparation processes W = [W1, W2, W3, ..., W k ], where the i-th preparation process is W i , W i The process period is △T i , process period △T i Including θ i Sampling period;

[0015] Among them, the preparation process associated with the inspection item is set as an associated process;

[0016] S2: If the inspection items of the prepared sample do not meet the inspection requirements, the associated process of the inspection item is taken as a risk process and added to the risk process list H; set W i The total count in the risk process list H is NUM i , where W i Associated with the r-type non-conforming inspection item EB, EB = [EB1, EB2, EB3, ..., EBr ], among which the jth category non-conforming inspection item EB j The basic evaluation value is δ j , E.B. j Preparation process W i The correlation degree is ω j ;

[0017] S3, set up inspection items EB j The test value of is δ1, according to its basic evaluation value δ j , get the non-standard project EB i The test value δ1 and the basic assessment value δ j The difference between j , and obtain △δ j The normalized value of △δ j ';

[0018] Get the risk process W i Risk Assessment Score

[0019] S4, set up risk process W i The risk assessment score threshold interval (F i-min , F i-max );

[0020] When F i <F i-min When the risk process W i The risk level is set to low risk and the process proceeds to the low risk sampling step;

[0021] F i-min ≤F i ≤F i-max When setting the risk process W i The risk level is medium risk, and the medium risk sampling step is carried out;

[0022] F i >F i-max When setting the risk process W i The risk level is high risk, and the process proceeds to high-risk sampling.

[0023] Among them, in step S4, the low-risk sampling step includes:

[0024] In the risk process i Process period △T i The sampling is performed with a sampling period of θ1, where θ1<θ i , in the process period △T i In the above example, sampling is performed with a sampling period of θ1, and a total of f1 samples are obtained, of which c1 samples fail to meet the standards, and the sampling qualification rate μ1=(f1-c1) / f1;

[0025] Set the low-risk sampling pass rate threshold to A1;

[0026] When μ1 ≥ A1, the risk process W is maintained i The risk level is low risk;

[0027] When μ1<A1, the risk process W is improved i The risk level of the risk process W i The risk level was adjusted to medium risk.

[0028] Among them, in step S4, the medium-risk sampling step includes:

[0029] In the risk process i Process period △T i The sampling is performed with a sampling period of θ2, where θ2 < θ1, and a total of f2 samples are obtained, of which c2 samples fail to meet the standards, and the sampling qualification rate μ2 = (f2-c2) / f2;

[0030] Set the risk sampling pass rate threshold to A2, where A2<A1;

[0031] When μ2 ≥ A1, the risk reduction process W i The risk level of the risk process W i The risk level of the company was adjusted to low risk;

[0032] When A2<μ2<A1, maintain the risk process W i The risk level is medium risk;

[0033] When μ2≤A2, improve the risk process W i The risk level of the risk process W i The risk level was adjusted to high risk.

[0034] Among them, in step S4, the high-risk sampling step includes:

[0035] In the risk process i Process period △T i In the example, the sampling period θ3 is used for sampling, where θ3 < θ2, and a total of f3 samples are obtained, of which c3 samples fail to meet the requirements, and the sampling qualification rate μ3 = (f3-c3) / f3 is obtained; wherein the high-risk sampling qualification rate threshold is set to A3, where A3 < A2;

[0036] When μ3 ≥ A2, the risk reduction process W i The risk level of the risk process W i The risk level of the company was adjusted to medium risk;

[0037] When A3<μ2<A2, maintain the risk process W i The risk level is high risk;

[0038] When μ3≤A3, for risk process W i Issue abnormal alarm.

[0039] Among them, in step S3, the non-compliant project EB i The test value δ1 and the basic assessment value δ j The difference between j The normalized value of

[0040] The beneficial effects achieved by this application are as follows:

[0041] The present application overcomes the situation in which, during the preparation process of modified coating samples, there are many inspection items, many process steps, and the adjustment of proportions and parameters is relatively complicated. It can timely locate the problems of inspection items to the relevant process steps, provide guidance and reminders to the staff, avoid the problem of inaccurate prediction results of the data analysis model for predicting the quality of the finished product, and can also timely discover and correct process problems and equipment problems in advance, thereby improving the safety of coating preparation. BRIEF DESCRIPTION OF THE DRAWINGS

[0042] In order to more clearly illustrate the embodiments of the present application or the technical solutions in the prior art, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are only some embodiments recorded in the present application. For those skilled in the art, other drawings can also be obtained based on these drawings.

[0043] Figure 1 The present invention is a flow chart of an embodiment of a control method for preparing an anti-corrosion, anti-wax and anti-fouling coating according to the present application. DETAILED DESCRIPTION

[0044] The following is a clear and complete description of the technical solutions in the embodiments of the present application in conjunction with the drawings in the embodiments of the present application. Obviously, the described embodiments are part of the embodiments of the present application, rather than all of the embodiments. Based on the embodiments in the present application, all other embodiments obtained by those skilled in the art without making creative work are within the scope of protection of the present application. It should be noted that the terms "first", "second", etc. in the specification and claims of the present application and the above-mentioned drawings are used to distinguish similar objects, and do not have to be used to describe a specific order or sequence. In addition, the terms "including" and "having" and any of their variations, for example, a process, method, system, product or device comprising a series of steps or units is not necessarily limited to those steps or units clearly listed, but may include other steps or units that are not clearly listed or inherent to these processes, methods, products or devices.

[0045] In the existing oil pipe technology, epoxy resin-based coatings are generally used. Since epoxy resin has good adhesion to the metal surface and has excellent alkali resistance, chemical resistance and flexibility, it is recognized as the best anti-corrosion coating. However, since the oil pipe involved in this application is used for underground petroleum oil and gas, the actual application temperature usually reaches about 200°C, the pH value is 1-13, the upper limit of H2S and CO2 gas content is as high as 10% and 95% respectively, and the environmental internal pressure is 7MPa. In the above application scenarios, the requirements for the anti-corrosion materials used are more stringent, and more inspection indicators need to be achieved. Therefore, higher requirements are put forward for the performance stability, shrinkage and yield of epoxy resin. In order to meet the above application requirements, the modification function of epoxy phenolic type coating is adopted, and phenolic resin is used to adjust epoxy resin to obtain a better coating product that meets the inspection indicators. Among them, the coating is based on epoxy phenolic resin, and pigments, fillers, solvents, additives and other materials are added. Under different fluidity, specific surface area and temperature and pressure environments, after grinding to the required fineness, the material is filtered out in a proportion. The addition of phenolic resin causes a cross-linking reaction between the active functional groups of the two resins. The resulting modified coating film has the advantages of strong adhesion, high flexibility and good alkali resistance of epoxy, as well as the excellent water resistance, solvent resistance and acid resistance of phenolic resin, achieving the effects of anti-corrosion, anti-wax and anti-fouling.

[0046] In order to ensure the anti-corrosion, anti-wax and anti-fouling effects of the coating, the modified coating finally obtained must undergo various inspection tests. The sample mass is about 5 mg. It is heated at a specified rate of high-purity ammonia and prepared by KBr tableting and KBr wafer coating. The inspection items include: hardness (determined according to the GB / T6739-2006 coating hardness pencil test method); bending strength (determined according to GB / T6742-1986); chemical corrosion resistance (determined according to GB / T18593-2001); salt spray test (determined according to GB / T1771-1991); adhesion test (determined according to the standard SY / T0315-2005 issued by the Ministry of Petroleum); comprehensive thermal test (differential scanning calorimetry, using The test was carried out by SDTQ600 comprehensive thermal analyzer of ThermoEl-emental Company of the United States); water absorption test of epoxy free film (the degree of reduction in water absorption of epoxy free film after adding phenolic resin in distilled water at 100°C); fineness ≤100μm (GB / T1724-2019 standard); drying time: 4h for surface / 24h for entity at 25±2°C (GB / T1728-2020 standard); non-volatile matter ≥80% (the loss of material in a flat-bottomed dish under heating is <20%, GB / T1725-2007 standard); wear resistance ≤120mg (mg loss of CS-17 abrasive at 1kg / 1000r, GB / T1768-2006 standard). Adhesion ≥4A (on-site tape method, SY / T6717-2016 standard); Hardness: no scratches on the surface with a 2H pencil (GB / T6739-2006 standard); Chemical corrosion resistance: no change in the coating after 72 hours in acid, alkali and 80°C crude oil (SY / T6717-2016 standard); Bending resistance: no cracks in the coating at a constant temperature of 25°C and an angle of 1.5° (SY / T0442-2018 standard); Impact resistance: no leakage in the coating under a constant temperature of 25°C and an impact of 8J (SY / T0442-2018 standard).

[0047] Based on the above-mentioned inspection standards, the present application provides a control system for preparing anti-corrosion, anti-wax and anti-fouling coatings, comprising an inspection item module, a process module, a risk assessment module and an adjustment module; wherein the inspection item module includes inspection items for inspecting and evaluating samples; the process module includes processes and process periods when samples are taken, and a sampling period is provided in the process period; wherein a process having a certain degree of correlation with the inspection item is set as an associated process of the inspection item, and when the inspection item fails the inspection and assessment, the associated process of the inspection item is used as a risk process; the risk assessment module is used to evaluate the degree of danger of the risk process and obtain the danger level of the risk process; the adjustment module adjusts the sampling period in the process period of the risk process according to the danger level of the risk process; the risk process is sampled and acquired with the adjusted sampling period, and the danger level of the risk process is re-evaluated according to the sampling results.

[0048] Specifically, in one embodiment, the sample inspection and evaluation includes n types of inspection items, and the sample preparation process includes k processes W=[W1, W2, W3, ..., W k ], where the i-th process is W i , W i The process period is △T i , process period △T i Including θ i Sampling period;

[0049] Among them, the process associated with the inspection item is set as the associated process;

[0050] If the inspection item does not meet the inspection requirements, the associated process of the inspection item will be taken as a risk process and added to the risk process list H;

[0051] The risk process list H records all the inspection items that do not meet the inspection requirements and their associated processes; among them, set W i The total count in the risk process list H is NUM i , W i Associated with r types of non-conforming inspection items EB (r<n), EB=[EB1,EB2,EB3,…,EB r ], among which the jth category non-conforming inspection item EB j The basic evaluation value is δ j , E.B. j With process W i The correlation degree is ω j ;

[0052] Set up inspection project EB j The test value of is δ1, according to its basic evaluation value δ j, get the non-standard project EB i The test value δ1 and the basic assessment value δ j The difference between j , where the different magnitudes of each item may have a significant impact on the calculation results, so the data is first normalized to eliminate the impact of different magnitudes of different parameters, and then the calculation is performed. The specific calculation method is: EB of the non-compliant items i The test value δ1 and the basic assessment value δ j The difference between j The normalized value of

[0053]

[0054] Get the risk process W i Risk Assessment Score

[0055] Setting up risk processW i The risk assessment score threshold interval (F i-min , F i-max );

[0056] When F i <F i-min When the risk process W i The risk level of the risk process W is set to low risk. i Perform low-risk spot check procedures;

[0057] F i-min ≤F i ≤F i-max When setting the risk process W i The risk level of the risk process is medium risk. i Perform medium-risk sampling steps;

[0058] F i >F i-max When setting the risk process W i The risk level is high risk, and the risk process W i Perform high-risk spot check steps.

[0059] Among them, the low-risk sampling steps are: in the risk process W i Process period △T i The sampling period is θ1 (θ1<θ i ) to obtain the sample data, and then analyze the process EC based on the sampled data. z The risk level can be further judged; specifically, in this embodiment, in the process period △T iIn the above example, sampling is performed with a sampling period of θ1, and a total of f1 samples are obtained, of which c1 samples fail to meet the requirements, and the sampling pass rate μ1 = (f1-c1) / f1 is obtained; wherein, the low-risk sampling pass rate threshold is set to A1;

[0060] When μ1 ≥ A1, the risk process W is maintained i The risk level is low risk;

[0061] When μ1<A1, the risk process W is improved i The risk level of the risk process W i The risk level was adjusted to medium risk.

[0062] The steps for medium-risk sampling are: i Process period △T i In the above example, the sampling period θ2 (θ2<θ1) is used for sampling, and a total of f2 samples are obtained, of which c2 samples fail to meet the requirements, and the sampling qualification rate μ2=(f2-c2) / f2 is obtained; wherein, the threshold of the risk sampling qualification rate is set to A2 (A2<A1);

[0063] When μ2 ≥ A1, the risk reduction process W i The risk level of the risk process W i The risk level of the risk process W is adjusted to low risk. i Perform low-risk spot check procedures;

[0064] When A2<μ2<A1, maintain the risk process W i The risk level is medium risk;

[0065] When μ2≤A2, the risk process W is improved i The risk level of the risk process W i The risk level of the risk process W is adjusted to high risk. i Perform high-risk spot check steps.

[0066] The high-risk sampling steps are: i Process period △T i In the above example, the sampling period θ3 (θ3<θ2) is used for sampling, and a total of f3 samples are obtained, of which c3 samples fail to meet the requirements, and the sampling qualification rate μ3=(f3-c3) / f3 is obtained; wherein, the high-risk sampling qualification rate threshold is set to A3 (A3<A2);

[0067] When μ3 ≥ A2, the risk reduction process W i The risk level of the risk process W i The risk level of the risk process W is adjusted to medium risk. i Perform medium-risk sampling steps;

[0068] When A3<μ2<A2, maintain the risk process W i The risk level is high risk;

[0069] When μ3≤A3, for risk process W i In case of abnormal alarm, it is recommended to enter the equipment maintenance process.

[0070] In one specific embodiment, process W i When preparing epoxy phenolic coating, in order to make the raw materials mix more evenly during the experiment, the raw materials are first coarsely crushed to 50 mesh before use, and then the raw materials are weighed in proportion, mixed evenly and melted at 70-80°C for 20 minutes, cooled to room temperature, and then crushed and sieved to 180 mesh to obtain the finished product for use. Process W i It is associated with multiple inspection items, such as hardness, corrosion resistance, bending resistance and impact resistance. If any of the inspection items fail to meet the requirements, the process W i Sampling inspection is carried out on the molten mixed raw materials to identify abnormal risks in the process.

[0071] Further, it should be understood that since the setting of each module is only for illustrating the functional units of the device of the present invention, the physical devices corresponding to these modules can be the processor itself, or a part of the software in the processor, a part of the hardware, or a part of the combination of software and hardware. Therefore, the number of each module in the figure is only schematic.

[0072] Those skilled in the art will appreciate that the various modules in the device may be adaptively split or merged, and such splitting or merging of specific modules will not cause the technical solution to deviate from the principles of the present invention. Therefore, the technical solutions after splitting or merging will fall within the protection scope of the present invention.

[0073] It is understood by those skilled in the art that all or part of the processes in the method for implementing the above-mentioned embodiments of the present invention can also be completed by instructing the relevant hardware through a computer program, and the computer program can be stored in a computer-readable storage medium, and when the computer program is executed by a processor, the steps of each of the above-mentioned method embodiments can be implemented. Among them, the computer program includes computer program code, and the computer program code can be in source code form, object code form, executable file or some intermediate form, etc. The computer-readable storage medium may include: any entity or device, medium, U disk, mobile hard disk, disk, optical disk, computer memory, read-only memory, random access memory, electric carrier signal, telecommunication signal and software distribution medium, etc., which can carry the computer program code.

[0074] The computer device may be a terminal, and the computer device includes a processor, a memory, a communication interface, a display screen and an input device connected via a system bus. The processor of the computer device is used to provide computing and control capabilities. The memory of the computer device includes a non-volatile storage medium and an internal memory. The non-volatile storage medium stores an operating system and a computer program. The internal memory provides an environment for the operation of the operating system and the computer program in the non-volatile storage medium. The communication interface network of the computer device, NFC (near field communication) or other technical implementations. The display screen of the computer device may be a liquid crystal display or an electronic ink display screen, and the input device of the computer device may be a touch layer covering the display screen, or a button, trackball or touchpad provided on the housing of the computer device, or an external keyboard, touchpad or mouse, etc.

[0075] Those skilled in the art will appreciate that the various modules in the device may be adaptively split or merged, and such splitting or merging of specific modules will not cause the technical solution to deviate from the principles of the present invention. Therefore, the technical solutions after splitting or merging will fall within the protection scope of the present invention.

Claims

1. A control method for a control system for preparing an anti-corrosion, anti-wax and anti-fouling coating, characterized in that: The following steps are involved: S0, provides a control system for preparing anti-corrosion, anti-wax and anti-fouling coatings, including an inspection project module, a process module, a risk assessment module and an adjustment module; wherein the inspection project module includes inspection items for inspecting and evaluating samples; the process module includes processes and process periods when samples are used, and a sampling period is set in the process period; wherein a process with a certain degree of correlation with the inspection project is set as an associated process of the inspection project, and when the inspection project fails to pass the inspection and assessment, the associated process of the inspection project is used as a risk process; the risk assessment module is used to assess the degree of danger of the risk process and obtain the risk level of the risk process; the adjustment module adjusts the sampling period in the process period of the risk process according to the risk level of the risk process; the risk process is sampled and obtained with the adjusted sampling period, and the risk level of the risk process is re-evaluated according to the sampling results; S1, set the inspection and evaluation of the prepared samples to include n types of inspection items, and the preparation process of the prepared samples includes k preparation processes W=[W1, W2, W3, ..., W k ], where the i-th preparation process is W i , W i The process period is △T i , process period △T i Including θ i Sampling period; Among them, the preparation process associated with the inspection item is set as an associated process; S2: If the inspection items of the prepared sample do not meet the inspection requirements, the associated process of the inspection item is taken as a risk process and added to the risk process list H; set W i The total count in the risk process list H is NUM i , where W i Associated with the r-type non-conforming inspection item EB, EB=[EB1, EB2, EB3, …, EB r ], among which the jth category of non-compliant inspection items EB j The basic evaluation value is δ j , E.B. j Preparation process W i The correlation degree is ω j ; S3, set up inspection items EB j The test value of is δ1, according to its basic evaluation value δ j , get the non-standard project EB i The test value δ1 and the basic assessment value δ j The difference between j , and obtain △δ j The normalized value of △δ j '; Get the risk process W i Risk Assessment Score ; S4, set up risk process W i The risk assessment score threshold interval (F i-min , F i-max ); When F i <F i-min When the risk process W i The risk level is set to low risk and the process proceeds to the low risk sampling step; F i-min ≤F i ≤ F i-max When setting the risk process W i The risk level is medium risk, and the medium risk sampling step is carried out; F i >F i-max When setting the risk process W i The risk level is high risk, and the process proceeds to the high-risk sampling step.

2. The control method of the control system for preparing an anti-corrosion, anti-wax and anti-fouling coating according to claim 1, characterized in that: The inspection items for testing and evaluation of the anti-corrosion, anti-wax and anti-fouling coating samples include: hardness, bending strength, corrosion resistance, adhesion, heat resistance, wear resistance, bending resistance and impact resistance.

3. The control method of the control system for preparing anti-corrosion, anti-wax and anti-fouling coatings according to claim 2, characterized in that: The environmental temperature for the inspection and evaluation of the anti-corrosion, anti-wax and anti-fouling coating samples is 200°C, the pH value is 1-13, the upper limits of H2S and CO2 gas content are 10% and 95% respectively, and the internal pressure of the environment is 7MPa.

4. The control method of the control system for preparing the anti-corrosion, anti-wax and anti-fouling coating according to claim 1, characterized in that: In step S4, the low-risk sampling step includes: In the risk process i Process period △T i The sampling is performed with a sampling period of θ1, where θ1<θ i , in the process period △T i In the above example, sampling is performed with a sampling period of θ1, and a total of f1 samples are obtained, of which c1 samples fail to meet the standards, and the sampling qualification rate μ1=(f1-c1) / f1 is obtained; Set the low-risk sampling pass rate threshold to A1; When μ1 ≥ A1, the risk process W is maintained i The risk level is low risk; When μ1<A1, the risk process W is improved i The risk level of the risk process W i The risk level was adjusted to medium risk.

5. The control method of the control system for preparing the anti-corrosion, anti-wax and anti-fouling coating according to claim 1, characterized in that: In step S4, the medium-risk sampling step includes: In the risk process i Process period △T i The sampling is performed with a sampling period of θ2, where θ2 < θ1, and a total of f2 samples are obtained, of which c2 samples fail to meet the standards, and the sampling qualification rate μ2 = (f2-c2) / f2 is obtained; Set the risk sampling pass rate threshold to A2, where A2<A1; When μ2 ≥ A1, the risk reduction process W i The risk level of the risk process W i The risk level of the company was adjusted to low risk; When A2<μ2<A1, maintain the risk process W i The risk level is medium risk; When μ2≤A2, improve the risk process W i The risk level of the risk process W i The risk level was adjusted to high risk.

6. The control method of the control system for preparing the anti-corrosion, anti-wax and anti-fouling coating according to claim 1, characterized in that: In step S4, the high-risk sampling step includes: In the risk process i Process period △T i In the example, the sampling period θ3 is used for sampling, where θ3<θ2, and a total of f3 samples are obtained, of which c3 samples fail to meet the standards, and the sampling pass rate μ3=(f3-c3) / f3 is obtained; the high-risk sampling pass rate threshold is set to A3, where A3<A2; When μ3 ≥ A2, the risk reduction process W i The risk level of the risk process W i The risk level of the company was adjusted to medium risk; When A3<μ2<A2, maintain the risk process W i The risk level is high risk; When μ3≤A3, for risk process W i Issue abnormal alarm.

7. The control method of the control system for preparing the anti-corrosion, anti-wax and anti-fouling coating according to claim 1, characterized in that: In step S3, the non-compliant items EB i The test value δ1 and the basic assessment value δ j The difference between j The normalized value of .

Citation Information

Patent Citations

  • Method and equipment for detecting and evaluating inner drag-reducing coating of natural gas pipeline

    CN103198210A

  • Iterative project risk identification alarm method, system and equipment and storage medium

    CN116307735A

  • Information security audit method, system and computer readable storage medium for storing thereof

    US20140130170A1

  • Food safety risk assessment method, apparatus, device, and storage medium

    WO2021232588A1

  • KR20210119138A