Preparation method and application of polyaluminium chloride composite material
Polyacrylamide is synthesized by modifying chitosan and acrylamide/modified chitosan hydrogel is combined with polyaluminum chloride to form a porous structure composite material, which solves the problem of the existing technology that is difficult to remove bacteria, viruses and cysts from water problem, achieving efficient sewage treatment and antibacterial effects.
Patent Information
- Application Number
- CN202410953896.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-17
- Publication Date
- 2024-10-18
- Estimated Expiration
- 2044-07-17
AI Technical Summary
Existing polyaluminum chloride is difficult to effectively remove bacteria, viruses, cysts and other pollutants in water, and cannot meet the higher demands in the field of sewage treatment.
Modified chitosan and acrylamide are used to synthesize polyacrylamide/modified chitosan hydrogel through specific steps, and are mixed with polyaluminum chloride and processed through a three-dimensional motion mixer to form a composite material with a porous structure. Adsorption and flocculation properties.
It significantly improves the adsorption performance and flocculation performance of the material for heavy metal ions, enhances the antibacterial performance, improves the adsorption capacity of pollutants, has stable and efficient adsorption and sterilization effects, and is suitable for sewage treatment.
Smart Images

Figure SMS_4
Abstract
Description
Technical Field
[0001] The invention belongs to the technical field of composite materials, and specifically relates to a preparation method and application of a polyaluminium chloride composite material. Background Art
[0002] Water purification technology is rapidly becoming an essential aspect of modern life as conventional water resources become increasingly scarce in recent years, the quality of drinking water deteriorates over time due to various activities such as the development of manufacturing and agriculture, water pollution caused by additives and toxic heavy metals, and increased water use depletes and causes salt water pollution.
[0003] Polyaluminium chloride (PAC) is an inorganic substance, referred to as polyaluminium. It is a water-soluble inorganic high molecular polymer between AlCl3 and Al(OH)3, with a general chemical formula of [Al2(OH) n Cl 6-n ] m , where m represents the degree of polymerization, and n represents the neutrality of the PAC product. Solid PAC is usually white, light gray, light yellow or brown crystals or powder, while liquid PAC is colorless, light gray, light yellow or translucent liquid with a certain viscosity. Its structure contains highly charged polymerized ring chains, which have a strong electrical neutralization effect on colloidal substances in water, and the hydrolyzate has an excellent bridging adsorption effect on suspended matter in water, and a selective adsorption effect on soluble substances. It has a fast flocculation and sedimentation speed, a wide range of applicable pH values, is non-corrosive to pipeline equipment, has a significant water purification effect, and can effectively remove color SS, COD, BOD and heavy metal ions such as arsenic and mercury in water. Due to its outstanding performance, it has been used as an emerging water purification material in recent years and is widely used in drinking water, industrial water and sewage treatment.
[0004] Polyaluminum chloride can remove heavy metal ions in sewage, but it is difficult to remove other pollutants in the water, such as bacteria, viruses and cysts, which pollute the water quality. Therefore, it is urgent to invent a polyaluminum chloride composite material with bactericidal properties to meet the higher demands in the field of sewage treatment. Summary of the invention
[0005] The purpose of the present invention is to overcome the defects of the prior art and provide a preparation method and application of a polyaluminium chloride composite material.
[0006] The purpose of the present invention can be achieved through the following technical solutions:
[0007] A method for preparing a polyaluminium chloride composite material comprises the following steps:
[0008] A1. Add modified chitosan to an acetic acid aqueous solution (6% by mass), place in a 60°C water bath and stir until the modified chitosan is completely dissolved, add acrylamide and 2-mercaptobenzoic acid (MBA), stir thoroughly until dissolved, place in an ice water bath to cool, then add ammonium persulfate and tetramethylethylenediamine in sequence, mix quickly and transfer to a -20°C environment, continue to react for 48 hours, and after polymerization is completed, add sodium hydroxide aqueous solution (5% by mass) to neutralize excess acetic acid, wash with deionized water, and freeze-dry to obtain polyacrylamide / modified chitosan hydrogel;
[0009] A2. Mixing polyaluminium chloride and polyacrylamide / modified chitosan hydrogel together by a mixer to prepare a polyaluminium chloride composite material.
[0010] Furthermore, in step A1, the ratio of the amount of acetic acid aqueous solution, modified chitosan, acrylamide, 2-mercaptobenzoic acid, ammonium persulfate, and tetramethylethylenediamine is 100 mL: 5 g: 20 g: 1.5 g: 0.4 g: 0.6 g.
[0011] Furthermore, the raw materials in step A2 are calculated in parts by weight as follows: 80-100 parts of polyaluminium chloride, 50-60 parts of polyacrylamide / modified chitosan hydrogel.
[0012] Furthermore, in step A2, a three-dimensional motion mixer is used as the mixer, the rotation speed of the mixer is set to 15-25 rpm, and the mixing time is 6-12 hours.
[0013] Polyalumina can effectively remove heavy metals from water and improve the material's adsorption performance for heavy metal ions; the molecular structure of polyacrylamide contains a large number of active functional groups, which further enhances the adsorption performance for heavy metal ions and improves the flocculation performance of the material; using the freeze-polymerization method, the monomer acrylamide is squeezed by ice crystals during the polymerization and cross-linking process and dispersed in the unfrozen micro-areas at the grain boundaries or between ice crystals. After the ice crystals melt, voids are left behind to obtain a hydrogel with a porous structure, which enhances the adsorption capacity for pollutants.
[0014] Furthermore, the modified chitosan is prepared by the following steps:
[0015] S1. Stearic acid, diethylenetriamine and xylene were mixed in a three-necked flask equipped with a stirring reflux device, stirred vigorously at room temperature, and the temperature was raised to 150°C. After reflux reaction for 2 hours, a water separator was connected and the temperature was continued to be raised to 200°C until no water was generated. After the reaction was completed, the intermediate 1 was obtained by distillation under reduced pressure. The ratio of stearic acid, diethylenetriamine and xylene was 28.4g:11.2g:100mL.
[0016] Stearic acid first undergoes an amidation reaction with diethylenetriamine, and then a cyclization reaction occurs after the temperature is raised. By controlling the molar ratio of stearic acid to diethylenetriamine to be close to 1:1 and a slight excess of diethylenetriamine, only one amino group on diethylenetriamine participates in the reaction to obtain intermediate 1. The specific reaction process is as follows:
[0017] ;
[0018] S2. In a three-necked flask equipped with a stirring device, the intermediate 1, glutaraldehyde, piperidine (condensing agent) and toluene were stirred and mixed uniformly, the reaction temperature was controlled to be 50° C., and the reaction was kept warm for 6 hours. After the reaction was completed, it was naturally cooled, and part of the solvent was removed by rotary evaporation. Then, it was purified by column chromatography (the eluent was a mixed solvent of petroleum ether / ethyl acetate, and the volume ratio of the two was 4:1), and the eluent was removed by rotary evaporation to obtain intermediate 2; the ratio of the amount of intermediate 1, glutaraldehyde, piperidine and toluene was 35.1 g:11.4 g:10 mL:100 mL;
[0019] Under the action of the condensing agent, the amino group on the intermediate 1 condenses with the aldehyde group on the glutaraldehyde to form an imine group (C=N Schiff base structure), and by controlling the molar ratio of the two to be close to 1:1 and a slight excess of glutaraldehyde, only one aldehyde group on the glutaraldehyde participates in the reaction to obtain the intermediate 2; the specific reaction process is as follows:
[0020] ;
[0021] S3, in a three-necked flask equipped with a stirring device, the intermediate 2, methyl iodide and toluene were mixed and stirred uniformly, the reaction temperature was controlled at 80°C, the reaction was carried out for 6 hours, and the reaction was completed, and the intermediate 3 was obtained by rotary evaporation; the ratio of the intermediate 2, methyl iodide and toluene was 44.8g:14.1g:100mL;
[0022] The tertiary amino group on intermediate 2 undergoes an alkylation reaction with methyl iodide to obtain intermediate 3 (quaternary ammonium product); the structure of intermediate 3 is shown below:
[0023] ;
[0024] S4. Add chitosan to a mixed solution of acetic acid and toluene (the mass fraction of acetic acid is 28%), stir until completely dissolved, then add intermediate 3 and piperidine, stir and react at room temperature for 1 hour, add sodium hydroxide solution dropwise to adjust the pH to 5, continue the reaction for 2 hours, and after the reaction is completed, let it stand and precipitate, filter, wash with ethanol and water in turn, and dry in an oven to obtain modified chitosan; the ratio of the mixed solution of acetic acid and toluene, chitosan, intermediate 3, and piperidine is 150mL:10g:41.2g:10mL;
[0025] Under the action of the condensation agent, the aldehyde group on the intermediate 3 condenses with the amino group on the chitosan to form an imine group (C=N Schiff base structure) to obtain modified chitosan;
[0026] Chitosan is a natural antibacterial agent that is non-toxic, easily degradable, has strong antibacterial properties, and can also promote the rapid sedimentation of flocculants. By modifying it and connecting it with organic antibacterial agents through C=N, the hydrogen bonding effect of chitosan amino groups is weakened, and the biological activity and antibacterial properties of chitosan are improved. In addition, the Schiff base structure can interact with proteins and enzymes, hindering the synthesis of bacterial nucleotides and amino acids, further improving the antibacterial properties. In addition, the modified chitosan also contains imidazoline, quaternary ammonium salts and long carbon chain structures, among which imidazoline can enhance the flocculation effect of the matrix; the introduction of quaternary ammonium As an excellent antibacterial structure, salt can play a synergistic role with chitosan and Schiff base, significantly enhancing the antibacterial properties of the matrix. Quaternary ammonium salts, as cations, can also adsorb anionic pollutants and improve the matrix's adsorption performance for pollutants. Finally, the introduction of long carbon chains has strong hydrophobicity, which can promote the interaction between chitosan and bacterial cell walls, further enhancing the antibacterial properties of the matrix. It can also be interspersed in the cross-linked grid of polyacrylamide, which not only ensures the stability of the performance, but also increases the distance between molecular chains, allowing the matrix to fully contact with the pollutant solution to improve the adsorption capacity.
[0027] Beneficial effects of the present invention: 1. The present invention obtains hydrogel by grafting modified chitosan with acrylamide, and then mixes it with polymerized alumina to obtain a composite material, which gives the material significant adsorption and flocculation properties;
[0028] 2. Using the freeze polymerization method, the hydrogel obtained has a porous structure, which further improves the adsorption capacity of the composite material for pollutants;
[0029] 3. Modification of chitosan has better antibacterial properties than ordinary chitosan, and can further improve the adsorption capacity of the material with stable performance;
[0030] Therefore, the composite material prepared by the present invention has stable and efficient adsorption performance, flocculation performance and antibacterial performance, and has important application value in the field of sewage treatment technology. DETAILED DESCRIPTION
[0031] The following will be combined with the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0032] Example 1
[0033] S1. In a three-necked flask equipped with a stirring reflux device, 28.4 g of stearic acid, 11.2 g of diethylenetriamine and 100 mL of xylene were mixed, vigorously stirred at room temperature, and the temperature was raised to 150° C. After reflux reaction for 2 h, a water separator was connected, and the temperature was continued to be raised to 200° C. until no water was generated and the reaction was completed, and distilled under reduced pressure to obtain intermediate 1;
[0034] S2, in a three-necked flask equipped with a stirring device, 35.1g of intermediate 1, 11.4g of glutaraldehyde, 10mL of piperidine and 100mL of toluene were stirred and mixed uniformly, the reaction temperature was controlled to 50°C, and the reaction was kept warm for 6h. After the reaction was completed, it was naturally cooled, and part of the solvent was removed by rotary evaporation, and then purified by column chromatography (the eluent was a mixed solvent of petroleum ether / ethyl acetate, and the volume ratio of the two was 4:1), and the eluent was removed by rotary evaporation to obtain intermediate 2;
[0035] S3, in a three-necked flask equipped with a stirring device, 44.8 g of intermediate 2, 14.1 g of methyl iodide and 100 mL of toluene were mixed and stirred evenly, the reaction temperature was controlled at 80° C., the reaction was carried out for 6 h, and after the reaction was completed, intermediate 3 was obtained by rotary evaporation;
[0036] S4. Add 10 g of chitosan to a mixed solution of 150 mL of acetic acid and toluene (the mass fraction of acetic acid is 28%), stir until completely dissolved, then add 41.2 g of intermediate 3 and 10 mL of piperidine, stir and react at room temperature for 1 h, add dropwise sodium hydroxide solution to adjust the pH to 5, continue the reaction for 2 h, and after the reaction is completed, let it stand and precipitate, filter, wash with ethanol and water in turn, and dry in an oven to obtain modified chitosan.
[0037] Example 2
[0038] S1. In a three-necked flask equipped with a stirring reflux device, 56.8 g of stearic acid, 22.4 g of diethylenetriamine and 200 mL of xylene were mixed, vigorously stirred at room temperature, and the temperature was raised to 150° C. After reflux reaction for 2 h, a water separator was connected, and the temperature was continued to be raised to 200° C. until no water was generated and the reaction was completed, and distillation was performed under reduced pressure to obtain intermediate 1;
[0039] S2, in a three-necked flask equipped with a stirring device, 70.2g of intermediate 1, 22.8g of glutaraldehyde, 20mL of piperidine and 200mL of toluene were stirred and mixed uniformly, the reaction temperature was controlled to 50°C, and the reaction was kept warm for 6h. After the reaction was completed, it was naturally cooled, and part of the solvent was removed by rotary evaporation, and then purified by column chromatography (the eluent was a mixed solvent of petroleum ether / ethyl acetate, and the volume ratio of the two was 4:1), and the eluent was removed by rotary evaporation to obtain intermediate 2;
[0040] S3, in a three-necked flask equipped with a stirring device, 44.8g of intermediate 2, 14.1g of iodomethane and 100mL of toluene were mixed and stirred uniformly, the reaction temperature was controlled at 80°C, the reaction was carried out for 6h, and the reaction was completed, and intermediate 3 was obtained by rotary evaporation; the ratio of intermediate 2, iodomethane and toluene was 44.8g:14.1g:100mL;
[0041] S4. Add 10 g of chitosan to a mixed solution of 150 mL of acetic acid and toluene (the mass fraction of acetic acid is 28%), stir until completely dissolved, then add 41.2 g of intermediate 3 and 10 mL of piperidine, stir and react at room temperature for 1 h, add dropwise sodium hydroxide solution to adjust the pH to 5, continue the reaction for 2 h, and after the reaction is completed, let it stand and precipitate, filter, wash with ethanol and water in turn, and dry in an oven to obtain modified chitosan.
[0042] Example 3
[0043] A method for preparing a polyaluminium chloride composite material comprises the following steps:
[0044] A1. Add 5 g of the modified chitosan prepared in Example 1 to 100 mL of acetic acid aqueous solution (6% by mass), place in a 60° C. water bath and stir until the modified chitosan is completely dissolved, add 20 g of acrylamide and 1.5 g of 2-mercaptobenzoic acid, stir thoroughly until dissolved, place in an ice water bath to cool, then add 0.4 g of ammonium persulfate and 0.6 g of tetramethylethylenediamine in sequence, mix quickly and transfer to a -20° C. environment, continue to react for 48 h, and after polymerization is completed, add sodium hydroxide aqueous solution (5% by mass) to neutralize excess acetic acid, wash with deionized water, and freeze-dry to obtain a polyacrylamide / modified chitosan hydrogel;
[0045] A2. Add 80 g of polyaluminium chloride and 50 g of polyacrylamide / modified chitosan hydrogel into a three-dimensional motion mixer and mix well (the speed of the mixer is set to 15 rpm and the mixing time is 6 h) to obtain a polyaluminium chloride composite material.
[0046] Example 4
[0047] A method for preparing a polyaluminium chloride composite material comprises the following steps:
[0048] A1. Add 5 g of the modified chitosan prepared in Example 2 to 100 mL of acetic acid aqueous solution (6% by mass), place in a 60° C. water bath and stir until the modified chitosan is completely dissolved, add 20 g of acrylamide and 1.5 g of 2-mercaptobenzoic acid, stir thoroughly until dissolved, place in an ice water bath to cool, then add 0.4 g of ammonium persulfate and 0.6 g of tetramethylethylenediamine in sequence, mix quickly and transfer to a -20° C. environment, continue to react for 48 h, and after polymerization is completed, add sodium hydroxide aqueous solution (5% by mass) to neutralize excess acetic acid, wash with deionized water, and freeze-dry to obtain a polyacrylamide / modified chitosan hydrogel;
[0049] A2. Add 90 g of polyaluminium chloride and 55 g of polyacrylamide / modified chitosan hydrogel into a three-dimensional motion mixer and mix well (the speed of the mixer is set to 15 rpm and the mixing time is 6 h) to obtain a polyaluminium chloride composite material.
[0050] Example 5
[0051] A method for preparing a polyaluminium chloride composite material comprises the following steps:
[0052] A1. Add 5 g of the modified chitosan prepared in Example 2 to 100 mL of acetic acid aqueous solution (6% by mass), place in a 60° C. water bath and stir until the modified chitosan is completely dissolved, add 20 g of acrylamide and 1.5 g of 2-mercaptobenzoic acid, stir thoroughly until dissolved, place in an ice water bath to cool, then add 0.4 g of ammonium persulfate and 0.6 g of tetramethylethylenediamine in sequence, mix quickly and transfer to a -20° C. environment, continue to react for 48 h, and after polymerization is completed, add sodium hydroxide aqueous solution (5% by mass) to neutralize excess acetic acid, wash with deionized water, and freeze-dry to obtain a polyacrylamide / modified chitosan hydrogel;
[0053] A2. Add 100 g of polyaluminium chloride and 60 g of polyacrylamide / modified chitosan hydrogel into a three-dimensional motion mixer and mix well (the speed of the mixer is set to 15 rpm and the mixing time is 6 h) to obtain a polyaluminium chloride composite material.
[0054] Comparative Example 1
[0055] Ordinary chitosan of the same mass was used to replace the modified chitosan in Example 5, and the remaining steps were the same as in Example 5.
[0056] Comparative Example 2
[0057] A commercially available polyaluminium chloride water purifier produced by Jiangsu Zhonghao Yuanda Environmental Engineering Co., Ltd. was used.
[0058] The following performance tests were performed on Examples 3-5 and Comparative Examples 1-2:
[0059] Determine the removal rate of the sample for arsenic (concentration 0.1 mg / L) and lead (concentration 0.1 mg / L) in sewage;
[0060] Determine the removal rate of COD and BOD in sewage by the sample;
[0061] The bactericidal effect was tested by using the "Static Sterilization Test of Heterotrophic Bacteria" in the "Analysis and Test Methods for Cooling Water" compiled by the Production Department and Development Department of China Petrochemical Corporation;
[0062] The measured results are shown in the following table:
[0063]
[0064] It can be seen from the above table that the material prepared in the embodiment of the present invention has a high removal rate for various pollutants and good bactericidal properties, and has important application value in the field of sewage treatment technology.
[0065] In the description of the specification, the description with reference to the terms "one embodiment", "example", "specific example", etc. means that the specific features, structures, materials or characteristics described in conjunction with the embodiment or example are included in at least one embodiment or example of the present invention. In this specification, the schematic representation of the above terms does not necessarily refer to the same embodiment or example. Moreover, the specific features, structures, materials or characteristics described can be combined in any one or more embodiments or examples in a suitable manner.
[0066] The above contents are merely examples and explanations of the present invention. Those skilled in the art may make various modifications or additions to the specific embodiments described or replace them in a similar manner. As long as they do not deviate from the invention or exceed the scope defined by the claims, they shall all fall within the protection scope of the present invention.
Claims
1. A method for preparing a polyaluminium chloride composite material, characterized in that: The following steps are involved: A1. Add modified chitosan to an acetic acid aqueous solution, heat and stir until the modified chitosan is completely dissolved, add acrylamide and 2-mercaptobenzoic acid, stir thoroughly until dissolved, place in an ice water bath to cool, add ammonium persulfate and tetramethylethylenediamine, mix quickly, continue to react for 48 hours in a -20°C environment, add sodium hydroxide aqueous solution after polymerization is completed, wash, and freeze-dry to obtain a polyacrylamide / modified chitosan hydrogel; A2, mixing polyaluminium chloride and polyacrylamide / modified chitosan hydrogel to obtain a polyaluminium chloride composite material; Wherein, the modified chitosan is prepared by the following steps: S1. Stearic acid, diethylenetriamine and xylene were mixed, stirred vigorously at room temperature, refluxed at 150°C for 2h, and then heated to 200°C until no water was generated and the reaction was complete. The intermediate 1 was obtained by distillation under reduced pressure. S2, mixing the intermediate 1, glutaraldehyde, piperidine and toluene uniformly, keeping the mixture at 50°C for 6 hours, cooling naturally, rotary evaporating, purifying by column chromatography, and rotary evaporating to obtain the intermediate 2; S3, mixing and stirring the intermediate 2, methyl iodide and toluene, controlling the reaction temperature at 80°C, reacting for 6 hours, and after the reaction is completed, rotary evaporation is performed to obtain the intermediate 3; S4. Add chitosan to the mixed solution of acetic acid and toluene, stir until completely dissolved, then add intermediate 3 and piperidine, stir and react at room temperature for 1 hour, add sodium hydroxide solution dropwise to adjust the pH, continue the reaction for 2 hours, and after the reaction is completed, let stand and precipitate, filter, wash and dry to obtain modified chitosan.
2. The method for preparing a polyaluminium chloride composite material according to claim 1, wherein: In step S1, the ratio of stearic acid, diethylenetriamine and xylene is 28.4 g:11.2 g:100 mL.
3. The method for preparing a polyaluminium chloride composite material according to claim 1, wherein: In step S2, the ratio of the amount of intermediate 1, glutaraldehyde, piperidine and toluene is 35.1 g:11.4 g:10 mL:100 mL.
4. The method for preparing a polyaluminium chloride composite material according to claim 1, wherein: In step S3, the ratio of the amount of intermediate 2, methyl iodide and toluene used is 44.8 g:14.1 g:100 mL.
5. The method for preparing a polyaluminium chloride composite material according to claim 1, wherein: In step S4, the ratio of the mixed solution of acetic acid and toluene, chitosan, intermediate 3, and piperidine is 150 mL: 10 g: 41.2 g: 10 mL.
6. The method for preparing a polyaluminium chloride composite material according to claim 1, wherein: In step A1, the ratio of the amount of acetic acid aqueous solution, modified chitosan, acrylamide, 2-mercaptobenzoic acid, ammonium persulfate, and tetramethylethylenediamine is 100 mL: 5 g: 20 g: 1.5 g: 0.4 g: 0.6 g.
7. The method for preparing a polyaluminium chloride composite material according to claim 1, characterized in that: The raw materials in step A2 are calculated in parts by weight as follows: 80-100 parts of polyaluminium chloride, 50-60 parts of polyacrylamide / modified chitosan hydrogel.
8. Application of the polyaluminium chloride composite material obtained according to the preparation method according to any one of claims 1 to 7 in the field of sewage treatment.
Citation Information
Patent Citations
Method for treating acid uranium-bearing wastewater by utilizing modified chitosan adsorbents
CN102863045A
Flocculating agent applied to food processing wastewater
CN104129839A