An organic metal iridium complex and an organic electroluminescent device and an organic electroluminescent device containing the same
By using organic metal iridium complexes with specific structures as doping materials for the emitting layer in organic electroluminescent devices, the problems of reduced efficiency and short life of phosphorescent materials are solved, and the effects of low driving voltage and high luminous efficiency are achieved.
Patent Information
- Application Number
- CN202410956886.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-17
- Publication Date
- 2024-10-18
- Estimated Expiration
- 2044-07-17
AI Technical Summary
The efficiency of phosphorescent materials in existing organic electroluminescent devices decreases rapidly under high-brightness conditions. The synthesis process is complex and the lifespan is short, making it difficult to meet the high-performance needs of industrial applications.
An organic metal iridium complex with a specific structure is used as the doping material of the light-emitting layer. By changing the molecular spatial configuration, the triplet energy of the compound is increased, the driving voltage is reduced, and the luminous efficiency and lifetime are improved.
It significantly reduces the driving voltage of organic electroluminescent devices, improves luminous efficiency and service life, and meets the comprehensive characteristics requirements of high performance and low voltage.
Smart Images

Figure CN118496279B_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the field of organic electroluminescence, and in particular relates to an organic metal iridium complex and an organic electroluminescent device and an organic electroluminescent apparatus containing the same. Background Art
[0002] Organic electronic devices include, but are not limited to, organic light-emitting diodes (OLEDs), organic field-effect transistors (O-FETs), organic light-emitting transistors (OLETs), organic photovoltaic devices (OPVs), dye-sensitized solar cells (DSSCs), organic optical detectors, organic photoreceptors, organic field-effect devices (OFQDs), light-emitting electrochemical cells (LECs), organic laser diodes, and organic plasmonic light-emitting devices.
[0003] In 1987, Tang and Van Slyke of Eastman Kodak reported a double-layer organic electroluminescent device, which included an arylamine hole transport layer and a tris-8-hydroxyquinoline-aluminum layer as an electron transport layer and a light-emitting layer. Once a bias voltage was applied to the device, green light was emitted from the device. This invention laid the foundation for the development of modern organic light-emitting diodes (OLEDs). The most advanced OLEDs can include multiple layers, such as charge injection and transport layers, charge and exciton blocking layers, and one or more light-emitting layers between the cathode and the anode. Since OLEDs are self-luminous solid-state devices, they offer great potential for display and lighting applications. In addition, the inherent properties of organic materials, such as their flexibility, can make them very suitable for special applications, such as on flexible substrates.
[0004] The luminous color of OLED can be achieved by designing the structure of luminescent materials. OLED can include one luminescent layer or multiple luminescent layers to achieve the desired spectrum. At present, the efficiency of phosphorescent OLED decreases rapidly under high brightness conditions, which is still a problem. In addition, the synthesis process of phosphorescent materials is relatively complex, time-consuming, and has a short lifespan. In view of the current industrial application requirements of OLED devices and the requirements for the optoelectronic characteristics of OLED devices, it is necessary to select more suitable luminescent layer doping materials with high performance.
[0005] Therefore, how to develop a high-performance phosphorescent material that enables an organic electroluminescent device to have comprehensive characteristics such as high efficiency, long life and low voltage is a technical problem that people in this field need to solve urgently. Summary of the invention
[0006] In view of this, the present invention provides an organic metal iridium complex and an organic electroluminescent device and an organic electroluminescent apparatus containing the same. The organic metal iridium complex described in the present invention is applied to a specific light-emitting device, which has low driving voltage, high luminous efficiency and long service life.
[0007] In order to achieve the above object, the present invention adopts the following technical solution:
[0008] The first technical purpose of the present invention is to provide an organometallic iridium complex, wherein the organometallic iridium complex has a structure shown in general formula I:
[0009] ;
[0010] wherein n is selected from 0, 1 and 2;
[0011] R1, R2 and R3 are each independently selected from hydrogen, deuterium, fluorine, cyano, substituted or unsubstituted C1-C20 alkyl, substituted or unsubstituted C6-C30 aryl, substituted or unsubstituted 3-15 membered cycloalkyl, substituted or unsubstituted C1-C20 alkoxy and combinations thereof;
[0012] R4, R5, R6 and R7 are each independently selected from hydrogen, deuterium, fluorine, alkyl, aryl, cycloalkyl, alkoxy and combinations thereof, and at least one of R4, R5, R6 and R7 is selected from fluorine or phenyl;
[0013] R8 and R9 are each independently selected from hydrogen, deuterium, and methyl;
[0014] R 10 , R 11 , R 12 , R 13 , R 14 , R 15 , R 16 and R 17 Each is independently selected from hydrogen, deuterium, substituted or unsubstituted C1-C20 alkyl, substituted or unsubstituted C6-C30 aryl, and substituted or unsubstituted 3-6 membered cycloalkyl.
[0015] Furthermore, n is selected from 1, and the C1-C20 alkyl groups may be deuterated.
[0016] Furthermore, the L A The ligand is selected from any of the following structures: .
[0017] Furthermore, the L B The ligand is selected from any of the following structures:
[0018] .
[0019] The term "substituted" refers to substitution by one, two or more substituents selected from the following: deuterium, C1-C10 alkyl, C3-C10 cycloalkyl, 3-membered to 10-membered heterocycloalkyl, whose heteroatoms are selected from oxygen, nitrogen, and sulfur; C6-C20 aryl, 3-membered to 10-membered heteroaryl, whose heteroatoms are selected from oxygen, nitrogen, and sulfur.
[0020] Furthermore, the organometallic iridium complex is selected from any one of the following structures: .
[0021] Only some specific structural forms are listed above, but this series of organometallic iridium complexes are not limited to the above molecular structures. Other specific molecular structures can be obtained by simple changes of some simple groups and their substituted groups and substitution positions, which will not be described one by one here.
[0022] The organometallic iridium complex disclosed in the present invention can be prepared by synthetic methods known to those skilled in the art.
[0023] The second object of the present invention is to provide the use of the above-mentioned organometallic iridium complex in an organic electroluminescent device.
[0024] An electroluminescent device, comprising the organic metal iridium complex. The organic electroluminescent device comprises: a first electrode, a second electrode and an organic layer disposed between the two electrodes, wherein the organic layer comprises the organic metal iridium complex of the present invention; the organic metal iridium complex is in a single form or mixed with other substances and exists in the organic layer.
[0025] The organic layer at least includes one or more of a hole injection layer, a hole transport layer, a layer having both hole injection and hole transport skills, an electron blocking layer, a light-emitting layer, a hole blocking layer, an electron transport layer, an electron injection layer and a layer having both electron transport and electron injection skills.
[0026] The organic electroluminescent device comprises at least one functional layer, namely the organic metal iridium complex of the present invention.
[0027] The organic electroluminescent device comprises a light-emitting layer, and the light-emitting layer contains the organic metal iridium complex of the present invention.
[0028] The light-emitting layer of the organic electroluminescent device comprises a main material and a doping material, wherein the doping material is the organic metal iridium complex of the present invention, and the mixing ratio of the main material to the doping material is 90:10-99.5:0.5.
[0029] The device of the present invention can be used in organic light-emitting devices, organic solar cells, electronic paper, organic photoreceptors or organic thin film transistors.
[0030] It can be seen from the above technical solution that compared with the prior art, the present invention has the following beneficial effects:
[0031] The present invention provides an organic metal iridium complex, which has good spatial twisting ability and improves the triplet energy of the compound by changing the molecular spatial configuration, so that the organic electroluminescent device prepared by using the compound of the present invention as a doping material for a light-emitting layer has a significantly lower driving voltage, and the luminous efficiency and life are significantly improved compared with the organic electroluminescent device prepared in a comparative example. BRIEF DESCRIPTION OF THE DRAWINGS
[0032] In order to more clearly illustrate the embodiments of the present invention or the technical solutions in the prior art, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are only embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on the provided drawings without paying creative work.
[0033] Figure 1 This is the hydrogen nuclear magnetic resonance spectrum of compound G-15 in Example 1. DETAILED DESCRIPTION
[0034] The technical solutions in the embodiments of the present invention are described clearly and completely below. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of them. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0035] The embodiment of the present invention discloses a method for preparing an organic metal iridium complex.
[0036] In addition, it should be noted that the numerical values given in the following examples are as accurate as possible, but those skilled in the art understand that due to unavoidable measurement errors and experimental operation problems, each number should be understood as an approximate number rather than an absolutely accurate value.
[0037] Example 1 Preparation of G-15
[0038]
[0039] Step 1: First, add 4L trifluorotetramethylpyridine to the reactor, replace nitrogen twice, and under nitrogen protection, add 10L of the prepared mixed acid solution (concentrated sulfuric acid: concentrated nitric acid = 1.4:1) to the reaction system. When adding acid, the reaction temperature is controlled between 40℃~50℃. After the addition is completed, the temperature of the reaction system is controlled at 60℃~65℃ for one hour. After the reaction is completed, let it stand for 30 minutes and separate the liquids. The target product is washed twice with an equal volume of cold water, then washed several times with 10% sodium carbonate solution until the washing liquid is no longer acidic, and finally washed twice with deionized water, added with anhydrous calcium chloride and dried to obtain intermediate B-15 (1639g), with a yield of 26.99%.
[0040] Mass spectrometry test value 156.03.
[0041]
[0042] Step 2: Weigh A-15 (269.97 mmol), B-15 (283.46 mmol), and cesium carbonate (Cs2CO3) (404.95 mmol) in turn and add them to the reactor, replace nitrogen three times, and add 750 ml of dimethyl sulfoxide (DMSO) to the reactor under nitrogen protection, replace nitrogen three times, and react at room temperature for 72 hours. After the reaction, pour the reaction solution into 750 ml of ice water, stir at room temperature for 30 minutes, and filter to obtain a yellow solid. Take the solid and dissolve it in 750 ml of chloroform, wash it with water twice, and dry it with magnesium sulfate to obtain intermediate C-15 (85.5 g, yield: 98.87%).
[0043] Mass spectrometry test value 321.16;
[0044] HPLC: >99.2%;
[0045] 1 HNMR(400MHz,Chloroform-d)δ8.10(dd,1H),8.00(dd,1H),7.88(dd,1H),7.58–7.5 2(m,2H),7.43–7.35(m,2H),7.27(td,1H),7.22(td,1H),7.09(td,1H),2.36(d,3H).
[0046]
[0047] Step 3: Weigh C-15 (124.87 mmol), tin chloride dihydrate (399.58 mmol), and anhydrous ethanol (840 ml) and add them to the reactor, replace nitrogen three times, and react at an internal temperature of 70 ° C for 8 hours. After the reaction is completed, concentrate the reaction solution, wash it twice with a 1 mol / L sodium hydroxide solution, and filter it. Dissolve the filtered solid in 1.4 L of toluene, add 1 L of 1 mol / L sodium hydroxide solution, wash it twice, separate the liquids, and dry it with magnesium sulfate. Recrystallize it with isopropyl ether to obtain a yellow solid C-15-1 (21.43 g, yield: 59.11%).
[0048] Mass spectrometry test value 291.41.
[0049] 1 HNMR(400MHz,Chloroform-d)δ8.05–7.96(m,2H),7.53(dd,1H),7.32–7.23(m,2H),7.18(td,1 H),7.12–7.02(m,2H),7.02–6.96(m,1H),6.61(dd,1H),5.06(d,1H),4.76(d,1H),2.25(d,3H).
[0050] Step 4: Under a nitrogen atmosphere, first measure acetic acid (210ml) and concentrated sulfuric acid (21ml) and slowly add them into the reactor, then add C-15-1 (72.32mmol) into the reactor, and control the internal temperature at 10°C. Slowly drip a solution of sodium nitrite (72.32mmol) dissolved in distilled water (113.4ml). After the addition is complete, keep warm for 30 minutes. Heat to 130°C and stir for 20 minutes. After the reaction is completed, add distilled water (210ml) to the system, filter, and rinse with methanol (500ml) to obtain a brown solid. Purify by column chromatography, use petroleum ether and dichloromethane as the developing solvent, and recrystallize to obtain intermediate C-15-2 (14.48g, yield: 73.02%).
[0051] Mass spectrometry test value 274.62;
[0052] HPLC: >99.3%;
[0053] 1 HNMR(400MHz,Chloroform-d)δ8.49(d,1H),8.05(ddd,2H),7.91(dd,1H),7.49(t,1H),7.43(dd,1H),7.34(dq,1H),7.09(td,1H),2.47(d,3H).
[0054]
[0055] Step 5: Under nitrogen protection, weigh D-15 (88.63 mmol) and IrC13•3H2O (40.28 mmol) into the reaction system, add a mixed solution of 300 ml of ethylene glycol ethyl ether and 100 ml of pure water, reflux for 48 hours under nitrogen protection, then cool to room temperature, precipitate, filter the precipitate, rinse and dry with water, anhydrous ethanol, and petroleum ether in turn. The bridged ligand E-15 (20.38 g, yield 89.7%) was obtained.
[0056] Step 6: Weigh the bridging ligand E-15 (17.72 mmol), add silver trifluoromethanesulfonate (38.98 mmol), then add 400 ml of dichloromethane and 135 ml of methanol to the system, react at room temperature for 48 hours under nitrogen protection, pass through a funnel, and spin dry to obtain the bridging ligand F-15 (24.26 g, yield 92.48%).
[0057] Step 7: Weigh the bridged ligand F-15 (20.26 mmol), add the ligand C-15-2 (50.65 mmol), and then add 300 ml of anhydrous ethanol to the system. Under nitrogen protection, reflux for 48 hours, filter, wash with alcohol, and dry. Use petroleum ether and dichloromethane as developing solvents, column chromatography, concentrate the filtrate, and solid precipitate to obtain the organometallic iridium complex G-15 (6.25 g, yield 38.48%).
[0058] HPLC: >99.3%;
[0059] Mass spectrometry test value 802.14;
[0060] Elemental analysis: theoretical value C, 62.90%; H, 3.77%; F, 2.37%; N, 6.99%;
[0061] The measured values are C, 62.84%; H, 3.79%; F, 2.36%; N, 7.01%.
[0062] Example 2 Preparation of G-25
[0063]
[0064] Step 1: The same method as that for preparing B-15 was used to obtain intermediate B-25 (1634 g) with a yield of 26.91%.
[0065] Mass spectrometry test value: 156.13.
[0066]
[0067] Step 2: Weigh A-15 (269.97 mmol), B-25 (283.46 mmol), and cesium carbonate (Cs2CO3) (404.95 mmol) in sequence and add them to the reactor, replace nitrogen three times, and add 750 ml of dimethyl sulfoxide (DMSO) to the reactor under nitrogen protection, replace nitrogen three times, and react at room temperature for 72 hours. After the reaction, pour the reaction solution into 750 ml of ice water, stir at room temperature for 30 minutes, and filter to obtain a yellow solid. Take the solid and dissolve it in 750 ml of chloroform, wash it with water twice, and dry it with magnesium sulfate to obtain intermediate C-25 (84.3 g, yield: 97.18%).
[0068] Mass spectrometry test value 321.24;
[0069] HPLC: >99.2%;
[0070] 1 HNMR(400MHz,Chloroform-d)δ8.21(dd,1H),8.15(dd,1H),8.01(dd,1H),7.62–7.57( m,1H),7.47–7.43(m,1H),7.41(dd,1H),7.31–7.21(m,2H),7.09(td,1H),2.45(d,3H).
[0071]
[0072] Step 3: Weigh C-25 (124.87 mmol), tin chloride dihydrate (399.58 mmol), and anhydrous ethanol (840 ml) and add them to the reactor, replace nitrogen three times, and react at an internal temperature of 70°C for 8 hours. After the reaction is completed, concentrate the reaction solution, wash it twice with a 1 mol / L sodium hydroxide solution, and filter it. Dissolve the filtered solid in 1.4 L of toluene, add 1 L of 1 mol / L sodium hydroxide solution, wash it twice, separate the liquids, and dry it with magnesium sulfate. Recrystallize it with isopropyl ether to obtain a yellow solid C-25-1 (22.1 g, yield: 61.15%).
[0073] Mass spectrometry test value: 291.42.
[0074] 1HNMR(400MHz,Chloroform-d)δ8.07(dd,1H),8.01(dd,1H),7.89(dd,1H),7.62–7.58(m,1H),7.53(dd ,1H),7.34(dd,1H),7.27(td,1H),7.20(td,1H),7.09(td,1H),6.24(d,1H),6.01(d,1H),2.45(d,3H).
[0075] Step 4: Under a nitrogen atmosphere, first measure acetic acid (210ml) and concentrated sulfuric acid (21ml) and slowly add them into the reactor, then add C-25-1 (75.51mmol) into the reactor, and control the internal temperature at 10°C. Slowly drip a solution of sodium nitrite (75.51mmol) dissolved in distilled water (118.8ml). After the addition is complete, keep warm for 30 minutes. Heat to 130°C and stir for 20 minutes. After the reaction is completed, add distilled water (210ml) to the system, filter, and rinse with methanol (500ml) to obtain a brown solid. Purify by column chromatography, use petroleum ether and dichloromethane as the developing solvent, and recrystallize to obtain intermediate C-25-2 (14.3g, yield: 69%).
[0076] Mass spectrometry test value 274.55;
[0077]
[0078] Step 5: Under nitrogen protection, weigh D-25 (87.08 mmol) and IrC13•3H2O (39.58 mmol) into the reaction system, add a mixed solution of 300 ml of ethylene glycol ethyl ether and 100 ml of pure water, reflux for 48 hours under nitrogen protection, then cool to room temperature, precipitate, filter the precipitate, rinse and dry with water, anhydrous ethanol, and petroleum ether in turn. The bridged ligand E-25 (19.9 g, yield 88.52%) was obtained.
[0079] Step 6: Weigh the bridging ligand E-25 (17.45 mmol), add silver trifluoromethanesulfonate (38.39 mmol), then add 400 ml of dichloromethane and 135 ml of methanol to the system, react at room temperature for 48 hours under nitrogen protection, pass through a funnel, and spin dry to obtain the bridging ligand F-25 (24.2 g, yield 93%).
[0080] Step 7: Weigh the bridging ligand F-25 (20.11 mmol), add the ligand C-25-2 (50.27 mmol), and then add 300 ml of anhydrous ethanol to the system. Under nitrogen protection, reflux for 72 hours, filter, wash with alcohol, and dry. Use petroleum ether and dichloromethane as developing solvents, column chromatography, concentrate the filtrate, and solid precipitate to obtain the organometallic iridium complex G-25 (6.3 g, yield 38.79%).
[0081] HPLC: >99.3%;
[0082] Mass spectrometry test value 802.14;
[0083] 1 HNMR(400MHz,Chloroform-d)δ8.48(q,1H),8.33(d,2H),8.13–8.06(m,3H),7.68(dd,2H),7.64(d,2H ),7.52–7.44(m,4H),7.32–7.24(m,3H),7.23(dd,1H),7.12(td,2H),7.03(td,1H),2.46–2.42(m,2H).
[0084] Elemental analysis: Theoretical value C, 62.43%; H, 4.49%; F, 2.35%; N, 6.93%; Measured value C, 62.49%; H, 4.47%; F, 2.34%; N, 6.98%.
[0085] The synthesis methods of other organometallic iridium complexes G-9, G-12, G-33, G-36, G-44, G-60, G-96, G-144, G-216, G-276, G-288, G-300, G-336, G-384 and G-405 are the same as those in the above embodiments, and are not described in detail here. The molecular formulas or mass spectra of other synthesized organometallic iridium complexes are shown in Table 1 below:
[0086] Table 1 Molecular formula, mass spectrum and purity of iridium metal complexes
[0087]
[0088] In order to further describe the present invention, more specific embodiments are listed below:
[0089] Device Example 1: Fabrication of an organic electroluminescent device containing compound G-15
[0090] The ITO glass substrate with a coating thickness of 150nm was cleaned twice in distilled water and ultrasonically washed for 30 minutes, and then repeatedly cleaned twice with distilled water and ultrasonically washed for 10 minutes. After the distilled water cleaning, ultrasonically washed with isopropyl alcohol, acetone, methanol and other solvents in sequence, and then dried and transferred to a plasma cleaning machine. The above substrate was washed for 5 minutes and sent to a vapor deposition machine.
[0091] First, 60nm of 4,4',4''-tri[2-naphthylphenylamino]triphenylamine ("2-TNATA") was vacuum-deposited on the ITO (anode) as a hole injection layer; then 60nm of N,N'-diphenyl-N,N'-(1-naphthyl)-1,1'-biphenyl-4,4'-diamine (NPB) was vacuum-deposited on the hole injection layer as a hole transport layer; and the light-emitting layer was vacuum-deposited on the hole transport layer. Among them, the main material of the light-emitting layer 4,4'-N,N'-biphenyl dicarbazole (CBP) and the doping material compound G-15 are mixed and evaporated at a weight ratio of 90:10 to form a light-emitting layer; then 10nm thick BAlq is vacuum evaporated to form a hole blocking layer; then Alq3 with a thickness of 40nm is vacuum evaporated on the hole blocking layer as an electron transport layer; then LiF with a thickness of 0.2nm is vacuum evaporated on it as an electron injection layer; and 150nm thick Al is vacuum evaporated on the electron injection layer as a cathode. The electroluminescent device is prepared in this way. Under the condition of certain brightness, the performance and luminescence characteristics of the obtained electroluminescent device are tested to evaluate the driving voltage, maximum external quantum efficiency and phosphorescence lifetime.
[0092] Device Example 2-Device Example 17
[0093] An organic electroluminescent device was prepared in the same manner as in Device Example 1, except that the light-emitting layer doping material G-15 was replaced with G-9, G-12, G-25, G-33, G-36, G-44, G-60, G-96, G-144, G-216, G-276, G-288, G-300, G-336, G-384, and G-405, and the other operating steps remained unchanged.
[0094] Comparative Example 1, Comparative Example 2
[0095] An organic electroluminescent device was prepared in the same manner as in device example 1, except that the light-emitting layer doping material G-15 was replaced with that in comparative example 1 and comparative example 2. The specific structure is as follows:
[0096]
[0097] The prepared organic electroluminescent device was subjected to the same tests as those in device example 1. The results are shown in Table 2.
[0098] Table 2 Test results of organic electroluminescent devices
[0099]
[0100] It can be seen from Table 2 that the organic electroluminescent devices prepared by using the organometallic iridium complex provided by the present invention as the doping material for the light-emitting layer (such as Tables G-15 and G-25) are compared with the electroluminescent devices prepared by using Comparative Example 1 and Comparative Example 2 as the doping material for the light-emitting layer. When the current density is the same, the driving voltage of the organic electroluminescent devices prepared by using the present invention is significantly reduced and the life span is significantly improved.
[0101] The above description of the disclosed embodiments enables one skilled in the art to implement or use the present invention. Various modifications to these embodiments will be apparent to one skilled in the art, and the general principles defined herein may be implemented in other embodiments without departing from the spirit or scope of the present invention. Therefore, the present invention will not be limited to the embodiments shown herein, but rather to the widest scope consistent with the principles and novel features disclosed herein.
Claims
1. An organometallic iridium complex, characterized in that: It has the structure shown in general formula I: ; wherein n is selected from 1 and 2; L A The ligand is selected from any of the following structures: ; L B The ligand is selected from any of the following structures: 。 2. The organometallic iridium complex according to claim 1, characterized in that n is selected from 1.
3. The organometallic iridium complex according to claim 1, characterized in that The organometallic iridium complex is selected from any one of the compounds represented by the following structural formulas: 。 4. An organic electroluminescent device, characterized in that: The organic electroluminescent device comprises the organometallic iridium complex according to claim 1.
5. The organic electroluminescent device according to claim 4, characterized in that: The organic electroluminescent device comprises a first electrode, a second electrode, and an organic layer disposed between the first electrode and the second electrode; the organic layer comprises the organic metal iridium complex as claimed in claim 1.
6. The organic electroluminescent device according to claim 5, characterized in that: The organic layer at least includes one or more of a hole injection layer, a hole transport layer, a layer having both hole injection and hole transport skills, an electron blocking layer, a light-emitting layer, a hole blocking layer, an electron transport layer, an electron injection layer and a layer having both electron transport and electron injection skills.
7. The organic electroluminescent device according to claim 6, characterized in that: The light-emitting layer of the organic electroluminescent device comprises a main material and a doping material, the doping material is the organic metal iridium complex, and the mixing ratio of the main material to the doping material is 90:10-99.5:0.
5.
8. An organic electroluminescent device, characterized in that: The organic electroluminescent device comprises the organic electroluminescent device according to claim 4.
Citation Information
Patent Citations
Synthesis method of 3-trifluoromethylpyridine or 3-difluoromethylpyridine compound
CN117304094A