A quality inspection method and device for gel packaging
Through ultrasonic microscopy technology and image fitting analysis, combined with thermal shock and vibration shock testing equipment, it solves the problems of traditional testing being difficult to detect internal defects in packages and cumbersome data management, improving the accuracy and efficiency of packaging quality testing and reducing costs.
Patent Information
- Application Number
- CN202411021132.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-29
- Publication Date
- 2024-10-29
- Estimated Expiration
- 2044-07-29
AI Technical Summary
Traditional packaging inspection methods are difficult to detect small-scale defects inside electronic packages, and test data management is cumbersome, affecting efficiency.
Ultrasonic microscopy technology is used for appearance, function and reliability testing. Micro defect data is obtained through ultrasonic ranging and microscopic imaging. Combined with image fitting and logical judgment analysis, quality testing equipment for thermal shock and vibration shock is designed to simplify Data management.
It improves detection accuracy and efficiency, reduces detection costs, and can effectively evaluate the heat resistance and shock resistance of packaging materials.
Smart Images

Figure CN118548937B_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of packaging quality detection, in particular to a quality detection method and device for gel packaging. Background Art
[0002] Electronic devices such as chips, transistors, resistors, capacitors, etc. need to be packaged through specific processes and materials. This process is to fix and protect electronic devices, ensure that electronic components are not damaged by environmental factors such as moisture, dust, temperature, etc., and ensure that the electrical connection between components is stable and reliable. Gel packaging technology mainly utilizes the excellent properties of materials such as aerogel and silicone gel to package sensitive components or circuits through a specific process to improve the reliability, stability and safety of products. With the development of related technologies and processes, packaging technology has put forward a series of new requirements for material properties, including: the packaging glue material must have a sufficiently high insulation strength; the packaging material should not have too many by-products and impurities; the packaging material should have certain heat resistance, waterproof, mechanical resistance, impact resistance, shock absorption and other protective properties.
[0003] Packaging testing is a crucial part of the electronic device manufacturing process, which ensures that the packaged electronic devices can meet the design requirements and performance standards. It aims to timely discover and eliminate defective electronic devices after packaging through strict packaging testing, ensure that product quality meets standards, and improve product reliability and durability by evaluating the stability and reliability of electronic devices and packaging materials under different environmental conditions.
[0004] However, packaging inspection technology still has some shortcomings in the electronic manufacturing process. Due to the small size of internal defects in electronic packaging and pin welding, it is difficult to detect them with traditional inspection methods. At the same time, the testing process involves the management of a large amount of test data, including data collection, storage, analysis and reporting. These cumbersome management processes may consume a lot of time and energy, affecting the test efficiency. Summary of the invention
[0005] In order to overcome the problems and shortcomings in the background technology, the embodiments of the present invention provide a quality detection method and device for gel packaging.
[0006] The purpose of the present invention can be achieved by the following technical scheme: a quality inspection method for gel packaging, including step 1, appearance inspection; step 2, function inspection; step 3, reliability inspection; step 4, data analysis; step 5, feedback display, specifically:
[0007] Step 1: Appearance inspection;
[0008] After gel encapsulation, the electronic devices will change in size, hereinafter referred to as the package. The length la0, width lb0 and average thickness T0 of the package to be tested are obtained by the ultrasonic rangefinder, and the size evaluation parameter e1 is calculated by the formula e1=k1*(la0-la0´)+k2*(lb0-lb0´)+k3*(T0-T0´), where k1, k2 and k3 are preset influencing factors; la0´ is the preset standard length; lb0´ is the preset standard width; T0´ is the preset standard thickness.
[0009] As a preferred embodiment of the present invention, an ultrasonic microscope obtains the thickness T0 of the surface of the package body through ultrasonic ranging, sends and collects high-frequency ultrasonic waves in a preset frequency range at every preset detection thickness dt, obtains an ultrasonic image at the thickness, extracts the tiny defect area S therein, records the number of tiny defects corresponding to each thickness to form a group of data points (t, S), generates a two-dimensional rectangular coordinate system with thickness t as the horizontal axis and tiny defect area s as the vertical axis, fills all data points (t, S) into the coordinate system to generate a two-dimensional image of the tiny defect area s changing with thickness t, and obtains the corresponding functional relationship S=f1(t) through image fitting.
[0010] When the packaged electronic device is bent and twisted as a whole, the farther the tiny defects are from the neutral axis of the package, the greater the stress generated, and the faster the tiny defects expand. The subsequent expansion speed of tiny defects at each thickness is preset to be v=k4*(T0-t)^2, where k4 is the preset influencing factor, and the formula is Calculate the micro-defect evaluation parameter e2.
[0011] Step 2: Functional testing;
[0012] As a preferred embodiment of the present invention, an ultrasonic microscope is used to detect the surface, sub-surface and internal deep structure of the electronic device of the package to be detected in a preset frequency range 2 and perform microscopic imaging, and the characteristics of lead offset, lead deformation, chip offset, chip warping and wafer cracking generated on the surface of the electronic device are captured based on image processing technology. The displacement of lead offset and lead deformation δ1i is obtained, where i is the total number of offset and deformed leads, i=1, 2, ..., m1. The displacement of chip offset and warping δ2j is obtained, where j is the total number of chips that are offset and warped, j=1, 2, ..., m2. The number of wafer cracks k1 is obtained, and the formula The electrical connection evaluation parameter e3 is obtained, wherein λ1, λ2 and λ3 are preset weight factors.
[0013] The package to be tested is placed in an external electric field, and the strength of the external electric field is gradually increased until the packaging material is broken down. The electric field strength at this time is recorded as the dielectric strength EQ, which is recorded as the insulation evaluation parameter e4.
[0014] Step 3: Reliability testing;
[0015] The package to be tested is placed in a high temperature environment, and thermally shocked at a preset number N1 and a preset temperature T.
[0016] The ultrasonic microscope obtains the thickness T1 of the surface of the package after thermal shock through ultrasonic ranging, sends and collects high-frequency ultrasonic waves in a preset frequency range at every preset detection thickness dt, obtains the ultrasonic image at the thickness, extracts the tiny defect area S, records the number of tiny defects corresponding to each thickness to form a group of data points (t, S), generates a two-dimensional rectangular coordinate system with thickness t as the horizontal axis and tiny defect area s as the vertical axis, fills all data points (t, S) into the coordinate system to generate a two-dimensional image of the tiny defect area s changing with thickness t, and obtains the corresponding functional relationship S=f2(t) through image fitting.
[0017] The subsequent expansion speed of small defects at each thickness is preset to be v=k4*(T1-t)^2, where k4 is the preset influencing factor. Calculate the thermal shock parameter e5.
[0018] The package to be tested is placed in a vibration environment, and is subjected to vibration shock at a preset amplitude A1 and a preset frequency f1.
[0019] The ultrasonic microscope obtains the thickness T2 of the surface of the package after vibration impact through ultrasonic ranging, sends and collects high-frequency ultrasonic waves in a preset frequency range at every preset detection thickness dt, obtains the ultrasonic image at the thickness, extracts the tiny defect area S, records the number of tiny defects corresponding to each thickness to form a group of data points (t, S), generates a two-dimensional rectangular coordinate system with thickness t as the horizontal axis and tiny defect area s as the vertical axis, fills all data points (t, S) into the coordinate system to generate a two-dimensional image of the tiny defect area s changing with thickness t, and obtains the corresponding functional relationship S=f3(t) through image fitting.
[0020] The subsequent expansion speed of small defects at each thickness is preset to be v=k4*(T2-t)^2, where k4 is the preset influencing factor. Calculate the vibration shock parameter e6.
[0021] The heat resistance index E1 is calculated by the formula E1=c1*(e5-e2) / e2, where C1 is the preset influencing factor; the seismic resistance index E2 is calculated by the formula E2=c2*(e6-e2) / e2, where C2 is the preset influencing factor.
[0022] Step 4: Data analysis;
[0023] As a preferred embodiment of the present invention, logical judgment is carried out based on the numerical values of the size evaluation parameter e1, micro-defect evaluation parameter e2, electrical connection evaluation parameter e3, insulation evaluation parameter e4, thermal shock parameter e5, vibration shock parameter e6, heat resistance index E1 and seismic resistance index E2. When the values of the size evaluation parameter e1, micro-defect evaluation parameter e2, electrical connection evaluation parameter e3, insulation evaluation parameter e4, thermal shock parameter e5 and vibration shock parameter e6 do not exceed their respective thresholds, and the heat resistance index E1 and seismic resistance index E2 do not exceed their respective thresholds, the test is determined to be qualified; when at least one of the values of the size evaluation parameter e1, micro-defect evaluation parameter e2, electrical connection evaluation parameter e3, insulation evaluation parameter e4, thermal shock parameter e5 and vibration shock parameter e6 exceeds the threshold but the exceeding part is less than the criterion δ, and the heat resistance index E1 and seismic resistance index E2 do not exceed their respective thresholds, the test is determined to be qualified; otherwise, the test is determined to be unqualified.
[0024] Step 5: Feedback display;
[0025] Generate a calculation sheet for the specific operation process of each parameter, display the determined test results on the display screen, and highlight the specific parameters that exceed the threshold when the test results are unqualified.
[0026] As a preferred embodiment of the present invention, a quality inspection device for gel packaging is used for thermal shock and vibration shock tests, and includes an equipment table on which a vibrator and a heater are installed.
[0027] The vibrator includes a base, a motor shaft, a servo motor, a vibration platform shaft, a transmission belt, a vibration platform, an eccentric cam support shaft, a spring 1 and a spring 2. The motor shaft and the servo motor are mounted on the base, and the vibration platform shaft is mounted on the base. The transmission belt is mounted on the motor shaft and the vibration platform shaft, and the transmission belt and the motor shaft are meshed for transmission, and the transmission belt and the vibration platform shaft are meshed for transmission. The servo motor drives the motor shaft to rotate, and the transmission belt transmits the rotational angular momentum of the drive motor shaft to the vibration platform shaft. The vibration platform shaft contacts and meshes with the eccentric cam support shaft, and transmits the angular momentum of the vibration platform shaft to the eccentric cam support shaft. The eccentric cam support shaft is mounted on the vibration platform, and the eccentric cam support shaft drives the vibration platform to vibrate periodically through periodic eccentric rotation. Spring 1 connects the base and the vibration platform, and spring 2 connects the base and the vibration platform. Spring 1 and spring 2 jointly limit the displacement amplitude of the vibration platform.
[0028] Compared with the prior art, the present invention has the following beneficial effects:
[0029] 1. The present invention uses focused high-frequency ultrasound to perform detection through ultrasonic microscopy technology, which can perform microscopic imaging of the surface, sub-surface and fine structures within a certain depth of the sample, thus overcoming the problem that traditional detection methods are difficult to detect tiny scale defects inside electronic packaging, and improving the accuracy of packaging quality detection methods;
[0030] 2. The present invention processes the data collected from appearance testing, function testing and reliability testing and obtains the test results through logical judgment and analysis of all data, thereby improving the efficiency of data collection, storage, analysis and reporting, reducing a lot of time and energy costs in the cumbersome data management process, and improving the test efficiency;
[0031] 3. The present invention proposes a quality inspection device for thermal shock and vibration shock tests, which realizes the simulation of thermal environment and vibration environment in the packaging inspection process through a simple structure; and reduces the total cost of the test through low-cost replaceable parts. BRIEF DESCRIPTION OF THE DRAWINGS
[0032] In order to facilitate understanding by those skilled in the art, the present invention is further described below with reference to the accompanying drawings:
[0033] Figure 1 is a flow chart of the method of the present invention;
[0034] Figure 2 It is a schematic diagram of the principle of the focused high-frequency ultrasonic microscopic imaging technology of the present invention;
[0035] Figure 3 It is a two-dimensional image of the variation of the area of the micro defect with the thickness of the present invention;
[0036] Figure 4 It is a schematic diagram of the microscopic imaging of the sub-surface and internal deep structure of the present invention;
[0037] Figure 5 It is a schematic diagram of the data analysis logic judgment process of the present invention;
[0038] Figure 6 It is a structural schematic diagram of the quality inspection equipment for thermal shock and vibration shock tests of the present invention;
[0039] Figure 7 It is an exploded diagram of the vibrator structure of the present invention.
[0040] Figure numerals: 1. Equipment table; 2. Vibrator; 3. Heater; 201. Base; 202. Motor shaft; 203. Servo motor; 204. Vibration platform shaft; 205. Transmission belt; 206. Vibration platform; 207. Eccentric cam support shaft; 208. Spring one; 209. Spring two. DETAILED DESCRIPTION
[0041] The technical solution of the present invention will be clearly and completely described below in conjunction with the embodiments. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0042] See also Figure 1 As shown, a quality inspection method for gel encapsulation comprises the following steps:
[0043] Step 1: Appearance inspection;
[0044] After gel encapsulation, the electronic devices will change in size, hereinafter referred to as the package. The length la0, width lb0 and average thickness T0 of the package to be tested are obtained by the ultrasonic rangefinder, and the size evaluation parameter e1 is calculated by the formula e1=k1*(la0-la0´)+k2*(lb0-lb0´)+k3*(T0-T0´), where k1, k2 and k3 are preset influencing factors; la0´ is the preset standard length; lb0´ is the preset standard width; T0´ is the preset standard thickness.
[0045] During the packaging process of electronic devices, micro defects may occur due to uncontrollable factors such as materials and processes, including delamination, pores, micro cracks, voids, burrs, foreign particle contamination, etc. These micro defects will cause stress concentration and affect the packaging effect, reducing the performance and reliability of semiconductor devices.
[0046] See also Figure 2 As shown in the figure, the principle diagram of the focused high-frequency ultrasonic microscopic imaging technology of the ultrasonic microscope is that the high-frequency focused sound beam generated by the ultrasonic microscope is focused on a point inside the package to be detected. When the surface of the package to be detected is placed in the defocused area of the high-frequency focused sound beam, Rayleigh waves will be excited within the thickness of one sound wave wavelength on the surface and near the surface of the package to be detected. Rayleigh waves are very sensitive to the inhomogeneity of the surface medium and can be used to detect tiny defects on the surface of the object. The water near the package to be detected acts as a sound propagation medium to transmit ultrasonic waves to the surface of the package to be detected, and then the high-frequency ultrasonic waves reflected by the surface of the package to be detected return along the same path, generate digital information after analog-to-digital conversion, and then generate a two-dimensional ultrasonic image containing tiny defect information at a certain depth plane of the package to be detected.
[0047] See also Figure 3As shown, the ultrasonic microscope obtains the thickness T0 of the surface of the package body through ultrasonic ranging, sends and collects high-frequency ultrasonic waves in a preset frequency range at every preset detection thickness dt, obtains the ultrasonic image at the thickness, extracts the tiny defect area S, records the number of tiny defects corresponding to each thickness to form a group of data points (t, S), generates a two-dimensional rectangular coordinate system with thickness t as the horizontal axis and tiny defect area s as the vertical axis, fills all data points (t, S) into the coordinate system to generate a two-dimensional image of the tiny defect area s changing with thickness t, and obtains the corresponding function relationship S=f1(t) through image fitting.
[0048] When the packaged electronic device is bent and twisted as a whole, the farther the tiny defects are from the neutral axis of the package, the greater the stress generated, and the faster the tiny defects expand. The subsequent expansion speed of tiny defects at each thickness is preset to be v=k4*(T0-t)^2, where k4 is the preset influencing factor, and the formula is Calculate the micro-defect evaluation parameter e2.
[0049] Step 2: Functional testing;
[0050] During the packaging process of electronic devices, the flow of gel in the package may cause deformation or displacement of the leads of the electronic devices, offset and warping of the chip base in the electronic devices, wafer cracking and other adverse factors, affecting the use function of the electronic devices. At the same time, the electrical insulation performance of the gel package also needs to be tested to ensure that it meets the transportation and use requirements.
[0051] See also Figure 4 As shown, an ultrasonic microscope is used to detect the surface, sub-surface and internal deep structure of the electronic device of the package to be inspected in a preset frequency range 2 and perform microscopic imaging. The characteristics of lead offset, lead deformation, chip offset, chip warping and wafer cracking generated on the surface of the electronic device are captured based on image processing technology. The displacement of lead offset and lead deformation δ1i is obtained, where i is the total number of offset and deformed leads, i=1, 2, ..., m1. The displacement of chip offset and warping δ2j is obtained, where j is the total number of chips that are offset and warped, j=1, 2, ..., m2. The number of wafer cracks k1 is obtained, and the formula The electrical connection evaluation parameter e3 is obtained, wherein λ1, λ2 and λ3 are preset weight factors.
[0052] The package to be tested is placed in an external electric field, and the strength of the external electric field is gradually increased until the packaging material is broken down. The electric field strength at this time is recorded as the dielectric strength EQ, which is recorded as the insulation evaluation parameter e4.
[0053] Step 3: Reliability testing;
[0054] During the use of electronic devices, with the changes in ambient temperature and humidity, and the influence of the thermal and electromagnetic effects and stress fields of the electronic products themselves, the tiny defects of the package itself will further expand and cause new tiny defects to continue to appear.
[0055] The package to be tested is placed in a high temperature environment, and thermally shocked at a preset number N1 and a preset temperature T.
[0056] The ultrasonic microscope obtains the thickness T1 of the surface of the package after thermal shock through ultrasonic ranging, sends and collects high-frequency ultrasonic waves in a preset frequency range at every preset detection thickness dt, obtains the ultrasonic image at the thickness, extracts the tiny defect area S, records the number of tiny defects corresponding to each thickness to form a group of data points (t, S), generates a two-dimensional rectangular coordinate system with thickness t as the horizontal axis and tiny defect area s as the vertical axis, fills all data points (t, S) into the coordinate system to generate a two-dimensional image of the tiny defect area s changing with thickness t, and obtains the corresponding functional relationship S=f2(t) through image fitting.
[0057] The subsequent expansion speed of small defects at each thickness is preset to be v=k4*(T1-t)^2, where k4 is the preset influencing factor. Calculate the thermal shock parameter e5.
[0058] The package to be tested is placed in a vibration environment, and is subjected to vibration shock at a preset amplitude A1 and a preset frequency f1.
[0059] The ultrasonic microscope obtains the thickness T2 of the surface of the package after vibration impact through ultrasonic ranging, sends and collects high-frequency ultrasonic waves in a preset frequency range at every preset detection thickness dt, obtains the ultrasonic image at the thickness, extracts the tiny defect area S, records the number of tiny defects corresponding to each thickness to form a group of data points (t, S), generates a two-dimensional rectangular coordinate system with thickness t as the horizontal axis and tiny defect area s as the vertical axis, fills all data points (t, S) into the coordinate system to generate a two-dimensional image of the tiny defect area s changing with thickness t, and obtains the corresponding functional relationship S=f3(t) through image fitting.
[0060] The subsequent expansion speed of small defects at each thickness is preset to be v=k4*(T2-t)^2, where k4 is the preset influencing factor. Calculate the vibration shock parameter e6.
[0061] The heat resistance index E1 is calculated by the formula E1=c1*(e5-e2) / e2, where C1 is the preset influencing factor; the seismic resistance index E2 is calculated by the formula E2=c2*(e6-e2) / e2, where C2 is the preset influencing factor.
[0062] Step 4: Data analysis;
[0063] See also Figure 5 As shown in the figure, the logical judgment flow diagram of data analysis is used to carry out logical judgment based on the numerical values of size evaluation parameter e1, micro defect evaluation parameter e2, electrical connection evaluation parameter e3, insulation evaluation parameter e4, thermal shock parameter e5, vibration shock parameter e6, heat resistance index E1 and seismic resistance index E2. When the values of size evaluation parameter e1, micro defect evaluation parameter e2, electrical connection evaluation parameter e3, insulation evaluation parameter e4, thermal shock parameter e5 and vibration shock parameter e6 do not exceed their respective thresholds, and the heat resistance index E1 and seismic resistance index E2 do not exceed their respective thresholds, the test is judged to be qualified; when at least one of the values of size evaluation parameter e1, micro defect evaluation parameter e2, electrical connection evaluation parameter e3, insulation evaluation parameter e4, thermal shock parameter e5 and vibration shock parameter e6 exceeds the threshold but the exceeding part is less than the judgment criterion δ, and the heat resistance index E1 and seismic resistance index E2 do not exceed their respective thresholds, the test is judged to be qualified; in other cases, the test is judged to be unqualified.
[0064] Step 5: Feedback display;
[0065] Generate a calculation sheet for the specific operation process of each parameter, display the determined test results on the display screen, and highlight the specific parameters that exceed the threshold when the test results are unqualified.
[0066] See also Figure 6 As shown, a quality inspection device for gel packaging is used for thermal shock and vibration shock tests, including an equipment table 1, on which a vibrator 2 and a heater 3 are installed.
[0067] See also Figure 7As shown, the vibrator 2 includes a base 201, a motor shaft 202, a servo motor 203, a vibration platform shaft 204, a transmission belt 205, a vibration platform 206, an eccentric cam support shaft 207, a spring 1 208 and a spring 2 209. The motor shaft 202 and the servo motor 203 are mounted on the base 201, and the vibration platform shaft 204 is mounted on the base 201. The transmission belt 205 is mounted on the motor shaft 202 and the vibration platform shaft 204, and the transmission belt 205 and the motor shaft 202 are meshed for transmission, and the transmission belt 205 and the vibration platform shaft 204 are meshed for transmission. The servo motor 203 drives the motor shaft 202 to rotate, and the transmission belt 205 transmits the rotational angular momentum of the driving motor shaft 202 to the vibration platform shaft 204. The vibration platform shaft 204 contacts and meshes with the eccentric cam support shaft 207 for transmission, and transmits the angular momentum of the vibration platform shaft 204 to the eccentric cam support shaft 207. The eccentric cam support shaft 207 is installed on the vibration platform 206. The eccentric cam support shaft 207 drives the vibration platform 206 to vibrate periodically through periodic eccentric rotation. The spring 1 208 connects the base 201 and the vibration platform 206, and the spring 2 209 connects the base 201 and the vibration platform 206. The spring 1 208 and the spring 2 209 jointly limit the displacement amplitude of the vibration platform 206.
[0068] It should be understood that the terms "include" and "comprising" used in the specification and claims of the present disclosure indicate the presence of described features, integers, steps, operations, elements and / or components, but do not exclude the presence or addition of one or more other features, integers, steps, operations, elements, components and / or collections thereof.
[0069] It should also be understood that the terms used in this disclosure are only for the purpose of describing specific embodiments and are not intended to limit the disclosure. As used in this disclosure and claims, the singular forms "a", "an", and "the" are intended to include plural forms unless the context clearly indicates otherwise. It should also be further understood that the term "and / or" used in this disclosure and claims refers to any combination of one or more of the associated listed items and all possible combinations, and includes these combinations;
[0070] The preferred embodiments of the present invention disclosed above are only used to help explain the present invention. The preferred embodiments do not describe all the details in detail, nor do they limit the invention to only specific implementation methods. Obviously, many modifications and changes can be made according to the content of this specification. This specification selects and specifically describes these embodiments in order to better explain the principles and practical applications of the present invention, so that those skilled in the art can understand and use the present invention well. The present invention is limited only by the claims and their full scope and equivalents.
Claims
1. A quality inspection method for gel encapsulation, Features: include: Step 1: Appearance inspection: Use an ultrasonic rangefinder to obtain the length, width and average thickness of the package to be inspected, and calculate the size evaluation parameters through formula calculation; Use an ultrasonic microscope to obtain the thickness of the surface of the package through ultrasonic ranging, send and collect high-frequency ultrasonic waves at a preset frequency range at every preset detection thickness, obtain an ultrasonic image at the thickness, extract the area of tiny defects therein, record the number of tiny defects corresponding to each thickness to form a set of data points to generate a two-dimensional image of the variation of the area of tiny defects with thickness, preset a formula for the subsequent expansion speed of tiny defects at each thickness, and obtain micro-defect evaluation parameters through calculation; Step 2: Functional testing: Use an ultrasonic microscope to detect the surface, sub-surface and internal deep structure of the electronic device of the package to be tested in a preset frequency range 2 and perform microscopic imaging, and capture the characteristics of lead offset, lead deformation, chip offset, chip warping and wafer cracking generated on the surface of the electronic device based on image processing technology; Obtain the displacement of lead offset and lead deformation, the displacement of chip offset and warpage, and the number of wafer cracks, and obtain electrical connection evaluation parameters through calculation. Place the package to be tested in an external electric field, and gradually increase the strength of the external electric field until the packaging material is broken down. The electric field strength at this time is recorded as the dielectric strength, which is recorded as the insulation evaluation parameter. Step 3, reliability testing; obtaining thermal shock parameters and vibration shock parameters through thermal shock tests and vibration shock tests, obtaining a heat resistance index through calculation of micro-defect evaluation parameters and thermal shock parameters, and obtaining a seismic resistance index through calculation of micro-defect evaluation parameters and vibration shock parameters; The specific process of obtaining thermal shock parameters and vibration shock parameters through thermal shock test and vibration shock test is as follows: The package to be tested is placed in a high-temperature environment to conduct a thermal shock test; the thickness of the surface of the package after the thermal shock test is obtained by ultrasonic ranging using an ultrasonic microscope, and high-frequency ultrasonic waves are sent and collected at a preset frequency range at every preset test thickness to obtain an ultrasonic image at the thickness, and the area of tiny defects therein is extracted, and the number of tiny defects corresponding to each thickness is recorded to form a set of data points to generate a two-dimensional image of the variation of the area of tiny defects with thickness, and a formula for the subsequent expansion speed of tiny defects at each thickness is preset, and thermal shock parameters are obtained through calculation; The package to be tested is placed in a vibration environment and subjected to a vibration impact test; the ultrasonic microscope obtains the thickness of the surface of the package after the vibration impact test through ultrasonic ranging, sends and collects high-frequency ultrasonic waves at a preset frequency range at every preset test thickness, obtains an ultrasonic image at the thickness, extracts the area of tiny defects therein, records the number of tiny defects corresponding to each thickness to form a set of data points to generate a two-dimensional image of the variation of the area of tiny defects with thickness, presets a formula for the subsequent expansion speed of tiny defects at each thickness, and obtains vibration impact parameters through calculation; The specific process of obtaining thermal shock parameters and vibration shock parameters through calculation is: The ultrasonic microscope obtains the thickness T1 of the surface of the package after thermal shock through ultrasonic ranging, sends and collects high-frequency ultrasonic waves in a preset frequency range at every preset detection thickness dt, obtains the ultrasonic image at the thickness, extracts the tiny defect area S, records the number of tiny defects corresponding to each thickness to form a group of data points (t, S), generates a two-dimensional rectangular coordinate system with thickness t as the horizontal axis and tiny defect area s as the vertical axis, fills all data points (t, S) into the coordinate system to generate a two-dimensional image of the tiny defect area s changing with thickness t, and obtains the corresponding function relationship S=f2(t) through image fitting; the subsequent expansion speed of tiny defects at each thickness is preset to be v=k4*(T1-t)^2, where k4 is the preset influencing factor, and the formula Calculate the thermal shock parameter e5; The package to be tested is placed in a vibration environment, and is subjected to a vibration shock with a preset amplitude A1 and a preset frequency f1. The ultrasonic microscope obtains the thickness T2 of the surface of the package after the vibration shock through ultrasonic ranging, and sends and collects high-frequency ultrasonic waves in a preset frequency range every preset detection thickness dt, obtains an ultrasonic image at the thickness, extracts the tiny defect area S therein, records the number of tiny defects corresponding to each thickness to form a group of data points (t, S), generates a two-dimensional rectangular coordinate system with thickness t as the horizontal axis and tiny defect area s as the vertical axis, fills all data points (t, S) into the coordinate system to generate a two-dimensional image of the tiny defect area s changing with thickness t, and obtains the corresponding function relationship S=f3(t) through image fitting; the subsequent expansion speed of tiny defects at each thickness is preset to be v=k4*(T2-t)^2, where k4 is a preset influencing factor, and the formula Calculate the vibration shock parameter e6; Step 4, data analysis: based on the numerical values of size evaluation parameters, micro-defect evaluation parameters, electrical connection evaluation parameters, insulation evaluation parameters, thermal shock parameters, vibration shock parameters, heat resistance index and seismic resistance index, logical judgment is carried out. When the values of size evaluation parameters, micro-defect evaluation parameters, electrical connection evaluation parameters, insulation evaluation parameters, thermal shock parameters and vibration shock parameters do not exceed their respective thresholds, and the heat resistance index and seismic resistance index do not exceed their respective thresholds, the test is judged to be qualified; when at least one of the values of size evaluation parameters, micro-defect evaluation parameters, electrical connection evaluation parameters, insulation evaluation parameters, thermal shock parameters and vibration shock parameters exceeds the threshold but the exceeding part is less than the value of the criterion, and the heat resistance index and seismic resistance index do not exceed their respective thresholds, the test is judged to be qualified; in other cases, the test is judged to be unqualified; Step 5: Feedback display: Generate a calculation sheet for the specific operation process of each parameter, display the determined test results on the display screen, and highlight the specific parameters that exceed the threshold when the test results are unqualified.
2. A gel encapsulation quality inspection method according to claim 1, It is characterized in that The specific process of obtaining micro-defect evaluation parameters and micro-defect evaluation parameters through calculation is as follows: The length la0, width lb0 and average thickness T0 of the package to be inspected are obtained by an ultrasonic rangefinder, and the size evaluation parameter e1 is calculated by the formula e1=k1*(la0-la0´)+k2*(lb0-lb0´)+k3*(T0-T0´), where k1, k2 and k3 are preset influencing factors; la0´ is the preset standard length; lb0´ is the preset standard width; T0´ is the preset standard thickness; The subsequent expansion speed of small defects at each thickness is preset to be v=k4*(T0-t)^2, where k4 is the preset influencing factor. Calculate the micro-defect evaluation parameter e2, where f1(t) is the corresponding function relationship S=f1(t) obtained by image fitting in the two-dimensional image of the micro-defect area s changing with the thickness t, and T0 is the average thickness.
3. A gel encapsulation quality inspection method according to claim 1, It is characterized in that The specific process of obtaining the electrical connection evaluation parameters through calculation is as follows: Get the displacement of lead offset and lead deformation δ1i, where i is the total number of offset and deformed leads, i=1,2,…,m1; get the displacement of chip offset and warpage δ2j, where j is the total number of chips that have offset and warpage, j=1,2,…,m2; get the number of wafer cracks k1, through the formula The electrical connection evaluation parameter e3 is obtained, wherein λ1, λ2 and λ3 are preset weight factors.
4. A quality inspection device for gel packaging, It is characterized in that A gel encapsulation quality inspection method for implementing any one of claims 1 to 3, comprising: The reliability detection module performs thermal shock and vibration shock tests on the package body to obtain thermal shock parameters and vibration shock parameters, obtains a heat resistance index by calculating the micro-defect evaluation parameters and thermal shock parameters, and obtains a seismic resistance index by calculating the micro-defect evaluation parameters and vibration shock parameters; Thermal shock test module: placing the package to be tested in a high temperature environment, and subjecting the package to be tested to thermal shock at a preset number of times N1 and a preset temperature T, to implement a thermal shock test; Vibration shock test module: Place the package to be tested in a vibration environment, and perform vibration shock on the package to be tested with a preset amplitude A1 and a preset frequency f1 to implement a vibration shock experiment.
5. A gel packaging quality inspection device according to claim 4, It is characterized in that Also includes: A device table (1) is provided, wherein a vibrator (2) and a heater (3) are installed on the device table (1); the vibrator (2) comprises a base (201), a motor shaft (202), a servo motor (203), a vibration platform shaft (204), a transmission belt (205), a vibration platform (206), an eccentric cam support shaft (207), a spring 1 (208) and a spring 2 (209); the motor shaft (202) and the servo motor (203) are installed on the base (201), and the vibration platform shaft (204) is installed on the base (201); the transmission belt (205) is installed on the motor shaft (202) and the vibration platform shaft (204), the transmission belt (205) and the motor shaft (202) are meshed for transmission, and the transmission belt (205) and the vibration platform shaft (204) are meshed for transmission; the servo motor (203) drives The driving motor shaft (202) rotates, and the transmission belt (205) transmits the rotational angular momentum of the driving motor shaft (202) to the vibration platform shaft (204); the vibration platform shaft (204) contacts and meshes with the eccentric cam support shaft (207) to transmit the angular momentum of the vibration platform shaft (204) to the eccentric cam support shaft (207); the eccentric cam support shaft (207) is installed on the vibration platform (206), and the eccentric cam support shaft (207) drives the vibration platform (206) to vibrate periodically through periodic eccentric rotation; the first spring (208) connects the base (201) and the vibration platform (206), the second spring (209) connects the base (201) and the vibration platform (206), and the first spring (208) and the second spring (209) jointly limit the displacement amplitude of the vibration platform (206).
Citation Information
Patent Citations
Eccentric shock-excitation vibration table
CN203688187U