Control method and system of multi-station electronic testing machine

By formulating tensile test control parameters and using standard specimens for correction, the problem of low consistency of experimental results at each station in the multi-station testing machine is solved, the accuracy and reliability of the test are improved, and support for material performance evaluation is provided. .

CN118565997BActive Publication Date: 2024-10-01深圳三思纵横科技股份有限公司
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411021739.0
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2024-07-29
Publication Date
2024-10-01
Estimated Expiration
2044-07-29

AI Technical Summary

Technical Problem

The consistency of experimental results between various stations in the multi-station testing machine is low, which affects the accuracy and reliability of the test results.

Method used

By obtaining the material parameters of the target sample, the tensile test control parameters are formulated, and the standard sample is used for correction, the deviation of each work station is identified, and the tensile test parameters are adjusted to reduce equipment errors and ensure the consistency of the test results.

Benefits of technology

It improves the accuracy and consistency of tensile testing, reduces the impact of equipment errors, provides reliable test data, and supports material performance evaluation and engineering design.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118565997B_ABST
    Figure CN118565997B_ABST
Patent Text Reader

Abstract

The present invention relates to the field of testing machine control technology, solves the problem of low consistency of experimental results between various stations in a multi-station testing machine in the prior art, and provides a control method and system for a multi-station electronic testing machine. The method comprises: obtaining tensile test control parameters according to the material parameters of the target sample, performing a tensile test on a standard sample according to the tensile test parameters, and obtaining a first tensile test result according to the deformation obtained by the displacement sensor and the load value obtained by the force sensor; obtaining the first test deviation of the corresponding station according to each of the first tensile test results; performing a tensile test on the target sample according to the tensile test parameters and the first test deviation to obtain a second tensile test result. The present invention can effectively reduce the differences between various stations in a multi-station testing machine, improve the accuracy and consistency of tensile test results, and ensure the reliability of material performance testing.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the technical field of testing machine control, and in particular to a control method and system for a multi-station electronic testing machine. Background Art

[0002] Tensile test is a basic and widely used material testing method. By applying tensile force to the material, its mechanical properties under different stress states, such as elastic modulus, yield strength and tensile strength, are measured. The results of tensile test are of great significance for engineering design, material selection and quality control.

[0003] The multi-station electronic testing machine is a highly efficient material testing equipment that can perform tensile tests on multiple specimens on the same device at the same time. It can test multiple specimens at the same time, which improves the test efficiency, saves time and cost, and because multiple specimens are tested under the same environment and conditions, it reduces the errors caused by environmental changes and improves the consistency of the test results.

[0004] Although multi-station testing machines have significant advantages in improving test efficiency and consistency, there are also some problems in actual use. Even on the same testing machine, there may be slight differences in the mechanical and electronic components of different stations. These differences will affect the loading process and sensor readings, and thus affect the test results. If the differences between these stations are not effectively controlled, they will affect the accuracy and reliability of the final test results. Therefore, how to accurately obtain the deviation of each station and correct and optimize the tensile test is an urgent problem to be solved. Summary of the invention

[0005] In view of this, an embodiment of the present invention provides a control method and system for a multi-station electronic testing machine, so as to solve the problem of low consistency of experimental results between various stations in the multi-station testing machine in the prior art.

[0006] In a first aspect, an embodiment of the present invention provides a control method for a multi-station electronic testing machine, the multi-station electronic testing machine comprising a base, a frame and a crossbeam, wherein the frame is fixedly connected to the upper surface of the base, the crossbeam is slidably connected to the frame, a preset number of stations are arranged between the crossbeam and the base, each of the stations comprises a sensor, a loading device and a fixture, the fixture comprises an upper fixture connected to the crossbeam and a lower fixture connected to the base, the loading device is connected to the upper fixture, and is used to drive the upper fixture to load the sample, the sensor comprises a displacement sensor for measuring the deformation amount of the sample during the loading process and a force sensor for measuring the load value applied to the sample, the method comprises:

[0007] According to the material parameters of the target sample, the tensile test control parameters are obtained, wherein the tensile test parameters include load increase rate, preload load and sampling frequency;

[0008] Performing a tensile test on a standard sample according to the tensile test parameters, wherein the material parameters of the standard sample are the same as the material parameters of the target sample;

[0009] Obtaining the preset number of first tensile test results according to the deformation value obtained by the displacement sensor and the load value obtained by the force sensor;

[0010] According to each of the first tensile test results, obtaining a first test deviation of the corresponding workstation;

[0011] A tensile test is performed on the target sample according to the tensile test parameters and the first test deviation to obtain a second tensile test result.

[0012] Preferably, obtaining the tensile test parameters according to the material parameters of the target sample includes:

[0013] Acquiring material parameters of the target sample, wherein the material parameters include: material type information and material size information;

[0014] Acquiring the expected strength parameter of the target sample according to the material type information and the material size information;

[0015] According to the material type, obtaining an elastic modulus range, an initial yield strength range, and an initial tensile strength range;

[0016] Calculating the minimum cross-sectional area of ​​the target sample in the stretching direction according to the material size information;

[0017] According to the minimum cross-sectional area, obtaining a yield strength adjustment factor and a tensile strength adjustment factor;

[0018] According to the yield strength adjustment coefficient and the tensile strength adjustment coefficient, the initial yield strength range and the initial tensile strength range are adjusted respectively to obtain a yield strength range and a tensile strength range;

[0019] Obtaining the expected strength parameter according to the respective minimum values ​​or intermediate values ​​of the elastic modulus range, the yield strength range, and the tensile strength range, wherein the expected strength parameter includes the expected elastic modulus, the expected yield strength, and the expected tensile strength;

[0020] The tensile test control parameters are determined according to the expected strength parameters.

[0021] Preferably, determining the tensile test control parameter according to the expected strength parameter comprises:

[0022] determining the preload load based on the material type, the expected strength parameter, and the minimum cross-sectional area;

[0023] According to the expected strength parameter and material type, the expected deformation stage of the target sample is obtained, wherein the expected deformation stage includes an elastic deformation stage, a yield stage, a plastic deformation stage, a necking stage and a fracture stage;

[0024] Determining the load increase rates of the elastic deformation stage, the yield stage, and the plastic deformation stage according to the expected strength parameter, wherein the load increase rates of the elastic deformation stage, the yield stage, and the plastic deformation stage decrease in sequence;

[0025] According to a preset necking rate and a preset fracture rate, setting the load increase rate in the necking stage and the fracture stage, wherein the preset necking rate is greater than the preset fracture rate;

[0026] Setting the sampling frequency of the elastic deformation stage and the plastic deformation stage to a first sampling frequency;

[0027] Setting the sampling frequency of the yield stage to a second sampling frequency;

[0028] Setting the sampling frequencies of the necking stage and the fracture stage to a third sampling frequency, wherein the first sampling frequency, the second sampling frequency, and the third sampling frequency are increased in sequence;

[0029] The tensile test parameters are determined according to the sampling frequency, load increase rate and the preload load of each expected deformation stage.

[0030] Preferably, controlling the loading device to perform a tensile test on the standard specimen according to the tensile test parameters comprises:

[0031] Fixing a preset number of standard specimens between the upper and lower clamps of each station respectively;

[0032] Controlling the loading device of each station to apply an initial load to the standard specimen according to the preload load;

[0033] Controlling the loading device of each station to gradually increase the applied load according to the load increase rate;

[0034] The force sensor and the displacement sensor are controlled to perform sampling according to the sampling frequency to obtain original load data and original displacement data.

[0035] Preferably, obtaining the preset number of first tensile test results according to the deformation amount obtained by the displacement sensor and the load value obtained by the force sensor includes:

[0036] Preprocessing the original load data and original displacement data of each workstation to obtain corresponding target load data and target displacement data;

[0037] According to the target load data and the target displacement data, a stress-strain curve of the standard sample of each station is drawn;

[0038] According to the stress-strain curve, the actual elastic modulus, actual yield strength, actual tensile strength and elongation at break of each of the standard samples are obtained;

[0039] The first tensile test result of each standard sample is obtained according to the actual elastic modulus, the actual yield strength and the actual tensile strength.

[0040] Preferably, obtaining the test deviation of the corresponding workstation according to each of the first tensile test results includes:

[0041] Calculating the standard deviation of the actual elastic modulus, the actual yield strength and the actual tensile strength according to the first tensile test results of each station;

[0042] If the standard deviation of the actual elastic modulus of a workstation is greater than the first preset standard deviation, and / or the standard deviation of the actual yield strength is greater than the second preset standard deviation, and / or the standard deviation of the actual tensile strength is greater than the third preset standard deviation, the workstation is marked as a first abnormal workstation and the workstations other than the first abnormal workstation are marked as non-abnormal workstations, wherein the first preset standard deviation is less than the second preset standard deviation, and the second preset standard deviation is less than or equal to the third preset standard deviation;

[0043] Performing data alignment and curve fusion on the stress-strain curves of each of the non-abnormal workstations to obtain a first stress-strain reference curve;

[0044] According to the first tensile test result of the first abnormal station, a first stress-strain abnormal curve is obtained;

[0045] According to the curve characteristics, the first stress-strain reference curve and the first stress-strain abnormal curve are divided to obtain a reference interval and a comparison interval, respectively, wherein the reference interval and the comparison interval both include an elastic deformation interval, a yield stage interval, a plastic deformation interval, a necking interval, and a fracture interval;

[0046] Determine a first abnormal interval in the comparison interval according to the similarity between the reference interval and the corresponding comparison interval, wherein the similarity between the first abnormal interval and the corresponding reference interval is less than a similarity threshold;

[0047] A first test deviation is obtained according to the first abnormal interval and the corresponding reference interval.

[0048] Preferably, performing a tensile test on the target sample according to the tensile test parameter and the first test deviation to obtain a second tensile test result includes:

[0049] According to the first test deviation, adjusting the load increase rate of the expected deformation stage corresponding to the abnormal interval in the tensile test parameter to obtain a first target tensile test parameter;

[0050] Fixing a preset number of target samples between the upper and lower clamps of each station respectively;

[0051] According to the tensile test parameters, controlling the non-abnormal station to perform a tensile test on the target sample;

[0052] According to the first target tensile test parameter, controlling the first abnormal station to perform a tensile test on the target sample;

[0053] The force sensor and the displacement sensor at each station are controlled to perform sampling according to the sampling frequency to obtain a second tensile test result.

[0054] Preferably, after performing a tensile test on the target sample according to the tensile test parameters and the first test deviation to obtain a second tensile test result, the method further includes:

[0055] According to the second tensile test results of each of the workstations, determining whether there is a second abnormal workstation with a test deviation;

[0056] If the second abnormal workstation exists and the second abnormal workstation is the first abnormal workstation, adjusting the load increase rate and sampling frequency of the first target tensile test parameter according to the first tensile test result and the second tensile test result to obtain a second target tensile test parameter;

[0057] If the second abnormal workstation exists and the second abnormal workstation is not the first abnormal workstation, obtaining a first test condition when performing a tensile test on the standard specimen and a second test condition when performing a tensile test on the target specimen, wherein the first test condition and the second test condition both include a test equipment state, a test environment condition, and a test operation condition;

[0058] If the first test condition and the second test condition are inconsistent, adjusting the second test condition according to the first test condition;

[0059] If the first test condition is consistent with the second test condition, record the number of abnormal occurrences of the second abnormal station;

[0060] If the number of abnormal occurrences is greater than a preset abnormal occurrence threshold, the tensile test parameters of the second abnormal workstation are adjusted according to the second tensile test results corresponding to the number of abnormal occurrences of each workstation.

[0061] Preferably, if the second abnormal workstation exists and the second abnormal workstation is the first abnormal workstation, the first target tensile test parameter is adjusted according to the first tensile test result and the second tensile test result to obtain the second target tensile test parameter:

[0062] According to the second tensile test results of the workstations other than the second abnormal workstation, obtaining a corresponding second stress-strain curve;

[0063] Performing data alignment and curve fusion on the second stress-strain curves to obtain a second stress-strain reference curve;

[0064] a second stress-strain abnormal curve according to the second tensile test result of the second abnormal station;

[0065] Obtaining a second abnormal interval having a second test deviation according to the second stress-strain abnormal curve and the second stress-strain reference curve;

[0066] Obtaining a parameter adjustment deviation of the first target tensile test parameter according to the first stress-strain anomaly curve and the second stress-strain anomaly curve;

[0067] According to the second test deviation and the parameter adjustment deviation, the load increase rate corresponding to the second abnormal interval in the first target tensile test parameter is adjusted, and according to the preset sampling frequency increment, the sampling frequency of the expected deformation stage corresponding to the second abnormal interval in the first target tensile test parameter is increased to obtain the second target tensile test parameter.

[0068] In the second aspect, an embodiment of the present invention provides a control system for a multi-station electronic testing machine, the control system comprising: a control module, a loading module, a sensor module and a power supply module, the loading module is used to apply a load to the test sample, the sensor module is used to monitor the load and displacement applied to the sample in real time, the power supply module is used to supply energy to the control system, and the control module is used to execute the control method of the multi-station electronic testing machine described in the first aspect.

[0069] In summary, the beneficial effects of the present invention are as follows:

[0070] The control method and system of the multi-station electronic testing machine provided by the embodiment of the present invention can ensure that the load applied to the material and the frequency of measurement during the test are adapted to the actual characteristics of the material by formulating control parameters according to specific material parameters. Using a standard sample with the same material parameters as the target sample can provide a consistent benchmark to ensure that there is a basis for subsequent correction of test deviations. Testing on standard samples can expose potential problems of equipment and systems, such as nonlinearity of the loading device, accuracy of the sensor, etc., which is convenient for adjustment and correction before formal testing of the target sample. According to the deformation obtained by the displacement sensor and the load value obtained by the force sensor, a preset number of first tensile test results are obtained. These first tensile test results provide basic data for subsequent calculation of test deviations to ensure the accuracy and comprehensiveness of the analysis. By comparing the test results of the standard sample, the deviations between the stations are identified, and the errors existing in the equipment and operation process are quantified. Finally, the target sample is subjected to a tensile test according to the tensile test parameters and the test deviation to obtain a second tensile test result. The adjusted tensile test parameters take into account the station deviation, so that the loading of the target sample is more accurate and the impact caused by the equipment error is reduced.

[0071] In summary, through the gradual implementation of the above steps, the accuracy and consistency of the tensile test can be effectively improved, ensuring that the multi-station testing machine can provide reliable test data while performing efficient testing, providing strong support for material performance evaluation and engineering design. BRIEF DESCRIPTION OF THE DRAWINGS

[0072] In order to more clearly illustrate the technical solution of the embodiment of the present invention, the drawings required for use in the embodiment of the present invention will be briefly introduced below. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying any creative work, and these are all within the protection scope of the present invention.

[0073] Figure 1 It is a structural schematic diagram of a multi-station electronic testing machine according to an embodiment of the present invention.

[0074] Figure 2 The present invention is a flowchart of a control method for a multi-station electronic testing machine according to an embodiment of the present invention.

[0075] Figure 3 The present invention is a flowchart of a control method for a multi-station electronic testing machine according to an embodiment of the present invention.

[0076] Figure 4 The present invention is a flowchart of a control method for a multi-station electronic testing machine according to an embodiment of the present invention.

[0077] Figure 5 It is a structural schematic diagram of a control system of a multi-station electronic testing machine according to an embodiment of the present invention.

[0078] Reference numerals:

[0079] 1. Base; 11. Frame; 12. Crossbeam; 2. Workstation; 21. Lower fixture; 22. Upper fixture; 23. Sensor; 24. Loading device. DETAILED DESCRIPTION

[0080] The features and exemplary embodiments of various aspects of the present invention will be described in detail below. In order to make the purpose, technical solutions and advantages of the present invention clearer, the present invention will be further described in detail below in conjunction with the accompanying drawings and Examples. It should be understood that the specific embodiments described herein are only configured to explain the present invention and are not configured to limit the present invention. For those skilled in the art, the present invention can be implemented without the need for some of these specific details. The following description of the embodiments is only to provide a better understanding of the present invention by illustrating examples of the present invention.

[0081] It should be noted that, in this article, relational terms such as first and second, etc. are only used to distinguish one entity or operation from another entity or operation, and do not necessarily require or imply any such actual relationship or order between these entities or operations. Moreover, the terms "include", "comprise" or any other variants thereof are intended to cover non-exclusive inclusion, so that a process, method, article or device including a series of elements includes not only those elements, but also other elements not explicitly listed, or also includes elements inherent to such process, method, article or device. In the absence of further restrictions, the elements defined by the statement "include..." do not exclude the presence of other identical elements in the process, method, article or device including the elements.

[0082] Example 1

[0083] See also Figure 1 An embodiment of the present invention provides a multi-station electronic testing machine, which includes a base 1, a frame 11 and a beam 12, wherein the frame is fixedly connected to the upper surface of the base, the beam is slidably connected to the frame, a preset number of stations 2 are arranged between the beam and the base, each of the stations includes a sensor 23, a loading device 24 and a fixture, the fixture includes an upper fixture 22 connected to the beam and a lower fixture 21 connected to the base, the loading device is connected to the upper fixture, and is used to drive the upper fixture to load the sample, the sensor includes a displacement sensor for measuring the deformation amount of the sample during the loading process and a force sensor for measuring the load value applied to the sample.

[0084] Specifically, in a multi-station electronic testing machine, the base is the main load-bearing part of the multi-station electronic testing machine, providing support and stability for the entire device. It is fixed to the ground in the laboratory or test site to ensure that the device does not move or tilt during the test. The frame is fixedly connected to the upper surface of the base, and is a structural frame that supports beams and other components. It is fixed to the base through a strong connection method (such as bolts or welding) to form a stable structure to support beams and multiple stations. The beam is slidably connected to the frame and can move vertically on the frame to adjust and align the positions of multiple stations to ensure accurate loading and measurement of each specimen.

[0085] A preset number of stations are arranged between the crossbeam and the base, each of which is an independent test unit. Each station includes a sensor, a loading device and a fixture for independently performing tensile testing of materials. The sensor includes a displacement sensor and a force sensor, wherein the displacement sensor is used to measure the deformation of the sample during the loading process, i.e., the displacement. When the sample is deformed by force, the displacement sensor records the length change of the sample in real time and provides accurate deformation data. The force sensor is used to measure the load value applied to the sample. When the loading device applies force to the sample, the force sensor records the magnitude of the force and provides accurate load data.

[0086] The fixture includes an upper fixture connected to the crossbeam, used to clamp the upper end of the sample and connected to the loading device, and can apply force to the sample under the drive of the loading device; and a lower fixture connected to the base, used to clamp the lower end of the sample, providing support and fixation for the sample.

[0087] The loading device is connected to the upper fixture and is used to drive the upper fixture to load the sample. The loading force is generated by a mechanical, electric or hydraulic system to push the upper fixture downward, thereby applying tension or pressure to the sample. The loading device accurately controls the rate and size of the applied load to ensure the accuracy of the test.

[0088] The multi-station electronic testing machine utilizes the coordinated work of the base, frame, beam and each station to achieve synchronous tensile testing of multiple groups of specimens.

[0089] In one embodiment, the upper clamp and the lower clamp are pneumatic clamps;

[0090] Based on the above multi-station electronic testing machine, please refer to Figure 2 This embodiment also provides a control method for a multi-station electronic testing machine, the method comprising:

[0091] S1. According to the material parameters of the target sample, obtain the tensile test control parameters, wherein the tensile test parameters include load increase rate, preload load and sampling frequency;

[0092] Specifically, material parameters include material type, size information, etc. Tensile test control parameters are the parameters required for tensile tests, including load increase rate, preload load and sampling frequency. The load increase rate is the rate at which the load of the specimen increases during the test. The preload load is the initial load applied before formal loading to ensure that the specimen does not loosen during stretching. The sampling frequency is the frequency of data collection, which determines the precision of the test data.

[0093] First, determine the material type of the target sample, such as metal, plastic, composite material, etc., obtain the length, width and thickness of the sample, and calculate the cross-sectional area of ​​the sample. Based on the material type, the expected elastic modulus, yield strength and tensile strength can be obtained from the material database or set according to empirical values, and the appropriate load increase rate can be set according to the strength of the material and the size of the sample. For high-strength materials, the rate can be lower; for low-strength materials, the rate can be higher. According to the material type and size, set an initial load value less than the yield strength, and according to the deformation characteristics of the material, set a high frequency of data acquisition to ensure that the deformation details are captured.

[0094] Preferably, see Figure 3 , obtaining tensile test parameters according to the material parameters of the target sample, including

[0095] S11, obtaining material parameters of the target sample, wherein the material parameters include: material type information and material size information;

[0096] Specifically, obtaining the material parameters of the target sample mainly includes two aspects of information: material type information and material size information. The material type information involves the type of material used for the target sample, such as metal, plastic, rubber, etc. The type of material will have a great impact on the results of the tensile test, because different materials have different properties, characteristics and mechanical behaviors; the material size information includes the size parameters of the target sample, such as length, width, thickness, etc. The size of the material will also affect the results of the tensile test, especially in the calculation of load, strain, etc.

[0097] S12, acquiring the expected strength parameter of the target sample according to the material type information and the material size information;

[0098] Specifically, the expected strength parameters are obtained according to the material type information and material size information of the target sample. The expected strength parameters refer to the material strength indicators expected to be achieved in the tensile test, usually including elastic modulus, yield strength and tensile strength;

[0099] The elastic modulus is an indicator of the stiffness of a material during stretching, and describes the material's ability to deform elastically after being subjected to force. The yield strength is an indicator of the material's strength when it undergoes plastic deformation during stretching, and indicates the maximum stress at which the material begins to produce observable plastic deformation. The tensile strength is an indicator of the material's maximum bearing capacity during stretching, and indicates the maximum tensile stress that the material can withstand before breaking under tension.

[0100] According to the material type and size information of the target specimen, the expected strength parameters such as the expected elastic modulus, yield strength and tensile strength are reasonably estimated. These expected strength parameters will provide an important reference for the determination of subsequent tensile test parameters to ensure the accuracy and reliability of the test.

[0101] Preferably, see Figure 4 , the obtaining of the expected strength parameter of the target sample according to the material type information and the material size information includes:

[0102] S121. Obtaining an elastic modulus range, an initial yield strength range, and an initial tensile strength range according to the material type;

[0103] According to the material type, you can consult material manuals, literature or use resources such as material databases to obtain the range of elastic modulus of this type of material. There are usually certain differences in the elastic modulus of different material types, so it is necessary to determine the range according to the specific material type. Similarly, according to the material type, you can look up corresponding material data, such as standard material specifications, experimental research data or literature, to obtain the range of yield strength and tensile strength of this type of material. These ranges can reflect the mechanical performance characteristics of this material type.

[0104] The elastic modulus is usually an inherent property of the material itself, and for a given material type, its elastic modulus has a relatively stable value range. Therefore, when determining the expected elastic modulus, this stable range can be used directly without additional adjustments.

[0105] However, yield strength and tensile strength may be affected by many factors, such as material preparation process, microstructure differences, specimen geometry, etc. Therefore, these strength parameters may be different for a specific specimen size or preparation process. In actual testing, in order to more accurately predict the test results, these parameters may need to be adjusted based on the specimen size information to take into account the specific characteristics of the specimen.

[0106] S122, calculating the minimum cross-sectional area of ​​the target sample in the stretching direction according to the material size information;

[0107] Specifically, based on the material size information provided, the minimum cross-sectional area of ​​the target specimen in the tensile direction is calculated. This usually involves the geometric shape (such as circular, rectangular, etc.) and dimensional parameters (such as diameter, width, thickness, etc.) of the specimen.

[0108] S123. Obtaining a yield strength adjustment coefficient and a tensile strength adjustment coefficient according to the minimum cross-sectional area;

[0109] Specifically, the yield strength adjustment factor and the tensile strength adjustment factor can be determined based on the minimum cross-sectional area. These factors take into account the effect of the sample size on the yield strength and tensile strength, and are usually used to correct or adjust the standard strength value to better reflect the actual performance of the target sample.

[0110] Therefore, the elastic modulus range can be used directly, while the yield strength and tensile strength may need to be adjusted based on the dimensional information of the specimen to better reflect the actual situation under the test conditions.

[0111] S124, adjusting the initial yield strength range and the initial tensile strength range respectively according to the yield strength adjustment coefficient and the tensile strength adjustment coefficient to obtain a yield strength range and a tensile strength range;

[0112] Specifically, according to the adjustment coefficient, the initial yield strength range and the initial tensile strength range are adjusted accordingly to obtain the yield strength range and the tensile strength range of the target sample.

[0113] S125. Obtain the expected strength parameters according to the respective minimum values ​​or intermediate values ​​of the elastic modulus range, the yield strength range, and the tensile strength range, wherein the expected strength parameters include the expected elastic modulus, the expected yield strength, and the expected tensile strength.

[0114] Finally, according to the minimum or middle value of the elastic modulus range, yield strength range and tensile strength range, the expected strength parameters of the target sample are determined, including the expected elastic modulus, expected yield strength and expected tensile strength. These expected strength parameters will provide important references for subsequent tensile test parameters to ensure that the test process can accurately reflect the performance characteristics of the target sample.

[0115] Using the minimum value of the range may be more conservative because it reflects the lowest strength level of the material. This ensures that the test parameters are set conservatively enough to ensure that the material properties do not exceed the range during the test. For critical applications, such as aerospace or medical devices, safety is of paramount importance. Therefore, choosing the minimum value may be more conducive to ensuring that the material properties meet the design and safety standards.

[0116] Using the middle value of the range can balance the different situations in the range and provide a more comprehensive consideration. It can avoid being too conservative and at the same time not being too optimistic because it takes into account the diversity in the range. For some applications, especially in material design or engineering design, the minimum value may be too conservative and the maximum value may be too optimistic. In this case, the middle value may be a more appropriate choice because it is more in line with the requirements of the actual application.

[0117] In summary, the choice of minimum or middle value depends on the requirements of the specific application and the emphasis on safety and feasibility. When making a decision, factors such as the material's use environment, expected application scenarios, and design standards need to be considered comprehensively.

[0118] S13. Determine the tensile test control parameters according to the expected strength parameters.

[0119] Determine the appropriate load increase rate based on the expected elastic modulus, yield strength and tensile strength, as well as the material parameters and dimensional information of the specimen. This rate should allow the load applied to the specimen to gradually increase to the expected value within a suitable time during the test. Generally, the smaller the load increase rate, the smoother the load change during the test, which is conducive to observing the various deformation stages of the specimen.

[0120] Determine an appropriate preload according to the purpose of the test and the characteristics of the specimen. The preload is the load applied to the specimen before the formal tensile test begins. The purpose is to make the specimen fully contact the loading device and keep the specimen in a suitable initial state to ensure the accuracy and repeatability of the test results.

[0121] Determine the appropriate sampling frequency based on the amount of data to be acquired during the test and the accuracy requirements of the data. The sampling frequency should be high enough to capture key data changes during the test, but not too high to cause excessive data volume and difficulty in data processing. Generally speaking, the higher the sampling frequency, the more refined the data obtained, but it will also increase the cost of data processing and storage.

[0122] In one embodiment, determining the tensile test control parameter according to the expected strength parameter includes:

[0123] S131, determining the preload load according to the material type, the expected strength parameter and the minimum cross-sectional area;

[0124] The purpose of the preload is to make the specimen fully contact the loading device and keep the specimen in a suitable initial state. The preload should be large enough to ensure good contact between the specimen and the loading device and maintain the stability of the specimen, but not too large to affect the deformation behavior of the specimen in advance.

[0125] According to the material properties of the specimen and the expected strength parameters, determine a ratio of the preload to the yield strength of the specimen or a ratio of the preload to the elastic modulus of the specimen material. This ratio can be adjusted according to the needs of the test, usually between 0.1 and 0.3;

[0126] In the formula, F preload is the preload; k is the proportionality coefficient between the preload and the yield strength of the specimen, which can be adjusted as needed; A is the minimum cross-sectional area of ​​the specimen; σ yield is the yield strength of the specimen.

[0127] According to the ratio and the minimum cross-sectional area, a preload can be obtained. The preload should be set large enough to ensure that the specimen is in full contact with the loading device while keeping the specimen in a suitable initial state to ensure the accuracy and repeatability of the test.

[0128] S132, acquiring the expected deformation stage of the target sample according to the expected strength parameter and material type, wherein the expected deformation stage includes an elastic deformation stage, a yield stage, a plastic deformation stage, a necking stage, and a fracture stage;

[0129] Specifically, in a tensile test, the deformation process of the specimen can usually be divided into several stages, including the elastic deformation stage, the yield stage, the plastic deformation stage, the necking stage, and the fracture stage;

[0130] At the beginning of the test, the specimen will deform elastically when loaded. The deformation of the specimen during this stage is reversible, that is, the specimen will return to its original shape after the external load is removed. Usually the stress-strain relationship at this stage is linear. The elastic deformation stage of the specimen can be determined based on the expected elastic modulus. If the specimen has a high elastic modulus, the elastic deformation stage may be relatively long.

[0131] As the external load continues to increase, the specimen will enter the yield stage. In this stage, the specimen begins to deform nonlinearly, that is, the deformation of the specimen is no longer proportional to the load. The yield point of the specimen refers to the point where the specimen begins to undergo continuous plastic deformation and does not return to its initial state. Based on the expected yield strength, the yield stage of the specimen can be determined. Usually, when the load on the specimen reaches the expected yield strength, it enters the yield stage.

[0132] After the yield point, the specimen enters the plastic deformation stage. During this stage, the specimen continues to be loaded and continues to deform plastically, and the shape and size of the specimen continue to change. This stage usually lasts until the specimen breaks. The duration of the plastic deformation stage depends on the material's properties such as strength and ductility. Based on the specimen geometry and the material's mechanical properties, a range of loads and strains can be expected for the specimen to enter the necking stage.

[0133] When the stress on the specimen reaches its maximum value, the specimen will shrink locally and form necking. The necking stage is one of the most prominent features of the specimen, which is manifested by the reduction of the specimen cross section and stress concentration.

[0134] Eventually, after the necking stage, the specimen will suddenly break. Fracture is the process by which a specimen loses its structural integrity under external loads, usually at the narrowest point of the specimen. The expected tensile strength can help determine when the specimen is likely to break. Generally, fracture occurs when the stress in the specimen reaches the expected tensile strength.

[0135] By combining expected strength parameters such as elastic modulus, yield strength, and tensile strength with factors such as material type and specimen geometry, reasonable inferences and predictions can be made about the expected deformation stages of the specimen in a tensile test.

[0136] Determining the expected deformation stages helps in designing and planning tensile tests. By understanding the expected behavior of the specimen at different stages, appropriate test parameters such as loading rate, load range, and sampling frequency can be better selected to ensure the accuracy and reliability of test results.

[0137] S133, determining the load increase rates of the elastic deformation stage, the yield stage, and the plastic deformation stage according to the expected strength parameter, wherein the load increase rates of the elastic deformation stage, the yield stage, and the plastic deformation stage decrease in sequence;

[0138] The elastic deformation stage is the linear deformation stage of the specimen during loading. At this time, the material exhibits completely elastic behavior, and the stress is proportional to the strain. A larger load increase rate can be selected to apply enough load in a shorter time to make the specimen produce linear elastic deformation. Usually, this load increase rate can be relatively high to improve test efficiency.

[0139] The yield stage is the stage where the specimen begins to produce plastic deformation. At this time, the material exhibits obvious nonlinear behavior, the stress begins to exceed the yield strength of the material, and the specimen begins to produce considerable plastic deformation. It is necessary to gradually reduce the load increase rate to ensure that the specimen produces typical yield behavior near the yield point, rather than over-stretching or damage at a premature stage.

[0140] After the specimen enters the plastic deformation stage, the material will continue to produce obvious plastic deformation, but the relationship between stress and strain is no longer linear. In order to fully observe and record the behavior of the specimen in the plastic deformation stage, it is necessary to further reduce the load increase rate so that the specimen has enough time to produce plastic deformation while maintaining the stability and controllability of the test.

[0141] By gradually reducing the load increase rate, the mechanical behavior of the material at different stages can be better simulated and the accuracy and reliability of the test results can be ensured. This gradual reduction strategy helps to effectively control the test process, avoid overloading or premature damage to the specimen, and thus improve the repeatability and comparability of the test.

[0142] S134, setting the load increase rate of the necking stage and the fracture stage according to a preset necking rate and a preset fracture rate, wherein the preset necking rate is greater than the preset fracture rate;

[0143] The load increase rate in the necking stage and the fracture stage needs to be set considering the actual behavior of the specimen and the purpose of the test. Generally speaking, the load increase rate in the necking stage can be set lower to observe and record the local necking process of the specimen, which helps to understand the local deformation behavior of the material. The load increase rate in the fracture stage can be set higher to accelerate the failure of the specimen, thereby obtaining a clear fracture surface and accurate failure data.

[0144] Specifically, when setting the load increase rate in the necking stage and the fracture stage, appropriate adjustments and settings can be made according to the preset necking rate and fracture rate, combined with the test requirements and the characteristics of the specimen. Usually, the load increase rate in the necking stage can be set to a lower value, such as a few Newtons per second, while the load increase rate in the fracture stage can be set to a higher value, such as tens of Newtons per second, to ensure that the test can proceed smoothly and obtain accurate test results.

[0145] S135, setting the sampling frequency of the elastic deformation stage and the plastic deformation stage to a first sampling frequency;

[0146] S136, setting the sampling frequency of the yield stage to a second sampling frequency;

[0147] S137, setting the sampling frequency of the necking stage and the fracture stage to a third sampling frequency, wherein the first sampling frequency, the second sampling frequency, and the third sampling frequency are increased in sequence;

[0148] Specifically, the elastic deformation stage and the plastic deformation stage are two important stages that occur after the specimen is subjected to force. In these two stages, the deformation of the specimen is small and the deformation rate is relatively low. Therefore, the sampling frequency can be relatively low and set to the first sampling frequency. This ensures that sufficient data points are obtained in these two stages to accurately describe the deformation behavior of the specimen.

[0149] The yield stage is the stage when the specimen begins to undergo plastic deformation, and it is also one of the key stages in the test. At this stage, the deformation rate of the specimen increases and the deformation begins to become significant. Therefore, in order to capture the exact location of the yield point and the plastic deformation behavior of the specimen, the sampling frequency should be set slightly higher, that is, the second sampling frequency.

[0150] The necking stage and the fracture stage are two key stages from the stress of the specimen to the final failure. In these two stages, the deformation rate of the specimen will increase sharply, and irreversible deformation and damage may occur. Therefore, in order to capture the accurate position of the necking point and the fracture point, and to record the deformation behavior of the specimen in these two stages, the sampling frequency should be further increased and set to the third sampling frequency to ensure that enough data points are obtained to describe the entire stage of the test process.

[0151] S138. Determine the tensile test parameters according to the sampling frequency, load increase rate and preload load of each expected deformation stage.

[0152] The final tensile test parameters are determined by comprehensively considering the preload, the load increase rate at each stage, and the sampling frequency. These parameters should be able to meet the purpose of the test, ensure that the data obtained during the test is accurate and reliable, and can effectively describe the mechanical properties and behavior of the specimen. Through the above steps, the appropriate tensile test parameters can be determined, thereby achieving accurate measurement and description of the mechanical properties of the specimen.

[0153] S2. performing a tensile test on a standard sample according to the tensile test parameters, wherein the material parameters of the standard sample are the same as the material parameters of the target sample;

[0154] Specifically, the standard specimen and the target specimen have the same material parameters, which are used to calibrate the test equipment and parameters. Under the conditions of the tensile test parameters, the testing machine is controlled to apply tensile force to the specimen, and the deformation and stress of the specimen are continuously measured during the process.

[0155] Preferably, controlling the loading device to perform a tensile test on the standard specimen according to the tensile test parameters comprises:

[0156] S21, fixing a preset number of standard samples between the upper clamps and the lower clamps of each station respectively;

[0157] A preset number of standard specimens are placed on the testing machine’s station, ensuring they are in the proper position and orientation. The specimens are clamped between two fixtures to ensure stability and safety during the test.

[0158] S22, controlling the loading device of each station to apply an initial load to the standard sample according to the preload load;

[0159] Before starting the tensile test, the loading device is controlled to apply an initial load to the specimen at each station according to the preload setting value. The purpose of the preload is to put the specimen in a suitable starting state so as to obtain accurate initial data at the beginning of the tensile test and ensure the repeatability of the test process.

[0160] S23, controlling the loading device of each station to gradually increase the applied load according to the load increase rate;

[0161] In this step, the loading device gradually increases the load applied to the specimen according to a preset load increase rate. This ensures that the rate at which the specimen is stressed is controllable and that the load can be gradually increased during the test to simulate the mechanical behavior in real applications.

[0162] S24. Control the force sensor and the displacement sensor to perform sampling according to the sampling frequency to obtain original load data and original displacement data.

[0163] In this step, according to the preset sampling frequency, the force sensor and displacement sensor are controlled to sample the load and displacement during the test. These sensors convert the collected data into raw load data and raw displacement data for subsequent data processing and analysis.

[0164] Through these steps, accurate control and measurement of specimen force and displacement during the test can be ensured, thereby obtaining reliable test data.

[0165] S3, obtaining the preset number of first tensile test results according to the deformation value obtained by the displacement sensor and the load value obtained by the force sensor;

[0166] Specifically, displacement sensors and force sensors are used to collect the deformation and load values ​​of the sample in real time during the stretching process. The collected raw data is preprocessed to remove noise and outliers to ensure the accuracy of the data. According to the stress formula (σ=F / A) and the strain formula (ε=ΔL / L0), the stress-strain data is calculated and the stress-strain curve is drawn to obtain the first tensile test results.

[0167] Preferably, obtaining the preset number of first tensile test results according to the deformation amount obtained by the displacement sensor and the load value obtained by the force sensor includes:

[0168] S31, preprocessing the original load data and original displacement data of each workstation to obtain corresponding target load data and target displacement data;

[0169] In this step, the raw data obtained from the force sensor and displacement sensor are preprocessed, which may include filtering, denoising or calibration operations to improve data quality and accuracy. The preprocessed data will be converted into target load data and target displacement data for subsequent analysis and processing.

[0170] S32, drawing a stress-strain curve of a standard sample of each station according to the target load data and the target displacement data;

[0171] Using the target load data and target displacement data, the stress-strain curves of the standard specimens at each station are calculated through the stress-strain relationship. These curves will show the mechanical behavior of the specimens during the tensile test, including the elastic stage, yield stage, plastic deformation stage, and fracture stage.

[0172] S33, obtaining the actual elastic modulus, actual yield strength, actual tensile strength and elongation at break of each of the standard samples according to the stress-strain curve;

[0173] By analyzing the characteristic points of the stress-strain curve, such as the slope change point and the curve shape, the actual elastic modulus, actual yield strength, actual tensile strength, elongation at break and other mechanical performance parameters of each standard specimen can be calculated. These parameters provide a comprehensive description and evaluation of the material's performance.

[0174] S34. Obtain a first tensile test result of each of the standard specimens according to the actual elastic modulus, the actual yield strength and the actual tensile strength.

[0175] Finally, the first tensile test results of each standard specimen were obtained based on the calculated actual elastic modulus, actual yield strength, actual tensile strength and other parameters. These results provide a detailed evaluation of the mechanical properties of the material and provide an important reference for subsequent research and application.

[0176] S4. Obtaining a first test deviation of the corresponding workstation according to each of the first tensile test results;

[0177] Specifically, the test results at each station are different due to differences in equipment and operations. For example, the parallelism and centering between the upper and lower fixtures. If the fixtures are not completely symmetrical, the specimen will be unevenly stressed during the stretching process, which will affect the test results. The loading devices at different stations may have manufacturing and assembly errors, resulting in different accuracy and consistency of applied loads. Over time, force sensors and displacement sensors may drift, affecting the accuracy of the measurement. When operators install specimens at different stations, there may be problems such as loose clamping of the specimens or asymmetric positions, resulting in uneven stress.

[0178] After the tensile test is performed on each station, the first tensile test results of each station are recorded, including the load value measured by the force sensor and the deformation measured by the displacement sensor. Data processing is performed on the first tensile test results of each station, including calculation of key parameters such as stress-strain curve, elastic modulus, yield strength, and tensile strength. Statistical analysis is performed on each key parameter, and statistical quantities such as the mean value and standard deviation of each station are calculated. Based on the results of the statistical analysis, the test deviation data of the station can be obtained.

[0179] Preferably, obtaining the test deviation of the corresponding workstation according to each of the first tensile test results includes:

[0180] S41, calculating the standard deviation of the actual elastic modulus, the actual yield strength and the actual tensile strength according to the first tensile test results of each station;

[0181] First, we need to analyze the data for each workstation and calculate the values ​​of the actual elastic modulus, actual yield strength, and actual tensile strength. Then, based on these values, we can calculate the standard deviation of the actual elastic modulus, actual yield strength, and actual tensile strength for each workstation. The standard deviation is a statistic that measures the degree of dispersion of data. It tells us how the data points in a data set are distributed relative to the mean. In this step, the calculation of the standard deviation can help us evaluate the stability and consistency of the data for each workstation, thereby determining the degree of difference between the workstations.

[0182] For the actual elastic modulus, actual yield strength, and actual tensile strength, first calculate the average value of each station, and for each data point of each station, calculate its deviation from the average value (i.e., the square of the difference), sum all the squares of the deviations, and then divide by the number of data points to get the variance, and finally take the square root of the variance as the standard deviation;

[0183] By calculating the standard deviation, we can understand the degree of deviation between the test data of each workstation and its average value, and thus determine whether the difference in test results between workstations is significant.

[0184] S42. If the standard deviation of the actual elastic modulus of a workstation is greater than the first preset standard deviation, and / or the standard deviation of the actual yield strength is greater than the second preset standard deviation, and / or the standard deviation of the actual tensile strength is greater than the third preset standard deviation, the workstation is marked as a first abnormal workstation and the workstations other than the first abnormal workstation are marked as non-abnormal workstations, wherein the first preset standard deviation is less than the second preset standard deviation, and the second preset standard deviation is less than or equal to the third preset standard deviation;

[0185] Specifically, an abnormality detection is performed on the test results of each workstation, and according to a preset standard deviation threshold, if the standard deviation of any indicator of a workstation exceeds the preset threshold, the workstation is marked as the first abnormal workstation. At the same time, other workstations are marked as non-abnormal workstations.

[0186] When setting the preset standard deviation threshold, the reliability of the test and the stability of the data are usually considered. The size of the preset standard deviation threshold can be adjusted according to the actual situation to ensure that the first abnormal station can be discovered in time, so as to conduct timely investigation and correction.

[0187] In this embodiment, the first preset standard deviation is less than the second preset standard deviation, and the second preset standard deviation is less than or equal to the third preset standard deviation;

[0188] This is done because the actual elastic modulus is usually used to evaluate the stiffness and elastic properties of a material, and the fluctuation requirements for the test data are relatively low. Therefore, the first preset standard deviation can be set relatively small to ensure that possible abnormalities are discovered in a timely manner.

[0189] The actual yield strength is an important parameter of the material in the tensile test, which represents the threshold value at which the material begins to undergo plastic deformation. Compared with the elastic modulus, the measurement of the yield strength may be more easily affected by some external factors, so the second preset standard deviation may be set slightly larger to ensure that abnormalities in the yield strength can be more accurately identified.

[0190] The actual tensile strength represents the maximum load-bearing capacity of the material in a tensile test, which is usually an extreme value. Therefore, the third preset standard deviation may be set relatively large to ensure that extreme abnormal situations can be discovered and handled in a timely manner.

[0191] Therefore, different preset standard deviations are set according to the characteristics and importance of different parameters, which helps to evaluate the test results more comprehensively and carefully, so as to better identify and deal with the first abnormal station.

[0192] S43. Obtain a test deviation of the first abnormal workstation according to the first tensile test results of the first abnormal workstation and the non-abnormal workstation.

[0193] Specifically, the average values ​​of the first tensile test results of the first abnormal station and the non-abnormal station are calculated, and then the test result of the first abnormal station is compared with the average value of the non-abnormal station to obtain the test deviation of the first abnormal station;

[0194] In one embodiment, the values ​​of the actual elastic modulus, the actual yield strength, and the actual tensile strength may be summed and divided by the number of samples to obtain the average values ​​of the first abnormal station and the non-abnormal station. For each parameter (actual elastic modulus, actual yield strength, actual tensile strength), the corresponding value of the first abnormal station is compared with the average value of the non-abnormal station, and the difference is calculated, i.e., the test deviation of the first abnormal station. The test deviation can be measured by calculating the difference between the value of the first abnormal station and the average value of the non-abnormal station, and can be expressed in the form of an absolute value or a percentage.

[0195] Preferably, obtaining the test deviation of the first abnormal workstation according to the first tensile test result of the first abnormal workstation and the first tensile test results of workstations other than the first abnormal workstation comprises:

[0196] S431, performing data alignment and curve fusion on the stress-strain curves of the non-abnormal workstations to obtain a first stress-strain reference curve;

[0197] Specifically, first, the stress-strain curves of each non-abnormal station need to be aligned to ensure that they have corresponding data values ​​at the same strain or stress point. This usually requires interpolation or extrapolation of the data to ensure that the number of data points and data range of each curve are consistent;

[0198] The aligned stress-strain curves of each non-abnormal workstation are fused to obtain a comprehensive stress-strain reference curve. The curve fusion method can be a simple average curve or a weighted average curve, where the weight can be set according to the actual situation, for example, according to the number of samples of each workstation or other relevant factors.

[0199] The stress-strain reference curve obtained after fusion can be used as a reference for subsequent comparative analysis. This reference curve represents the average level of multiple stations, can be used to evaluate the test deviation of the first abnormal station, and provide a basis for further analysis and processing.

[0200] S432, dividing the first stress-strain reference curve and the stress-strain curve of the first abnormal workstation according to curve characteristics to obtain a reference interval and a comparison interval, respectively, wherein the reference interval and the comparison interval both include an elastic deformation interval, a yield stage interval, a plastic deformation interval, a necking interval, and a fracture interval;

[0201] Specifically, the stress-strain reference curve and the stress-strain curve of the first abnormal station are divided according to the curve characteristics to obtain the reference interval and the comparison interval respectively. Both intervals include different deformation stages of the material, including elastic deformation interval, yield stage interval, plastic deformation interval, necking interval and fracture interval;

[0202] The elastic deformation interval corresponds to the elastic deformation stage of the material after the load is applied, that is, the linear segment of the stress-strain curve. In the reference interval and the comparison interval, the division of the elastic deformation interval is usually determined based on the linear segment of the curve, which can be identified by fitting a straight line or slope.

[0203] The yield stage is the stage where the material begins to undergo plastic deformation, and on the stress-strain curve it usually corresponds to a nonlinear segment with obvious stress and strain increases. In the reference and comparison intervals, the division of the yield stage interval is usually determined based on the nonlinear part of the curve, which can be identified by the stress change rate or strain change rate.

[0204] The plastic deformation interval corresponds to the stage when the material begins to enter the plastic deformation stage, the stress gradually increases but the strain does not increase significantly. On the stress-strain curve, the plastic deformation interval is usually shown as an approximately flat curve segment. In the reference interval and comparison interval, the division of the plastic deformation interval is usually determined based on the flat segment of the curve.

[0205] The necking interval corresponds to the stage where the material begins to neck, that is, the cross-sectional reduction phenomenon occurs in the tensile test. On the stress-strain curve, the necking interval is usually manifested as a section where the stress drops sharply but the strain is still increasing. In the reference interval and the comparison interval, the division of the necking interval is determined according to the section where the stress drops sharply on the curve.

[0206] The fracture interval corresponds to the stage where the material breaks, that is, the material loses its load capacity and breaks during the tensile test. On the stress-strain curve, the fracture interval is usually shown as a section where the stress drops sharply and the strain stops increasing. In the reference interval and comparison interval, the division of the fracture interval is determined based on the sharp drop in stress and the cessation of strain increase in the curve.

[0207] Through the above steps, the stress-strain reference curve and the stress-strain curve of the first abnormal station can be divided into different deformation stages, and the reference interval and comparison interval can be obtained for subsequent analysis and comparison.

[0208] S433, determining an abnormal interval in the comparison interval according to the similarity between the reference interval and the corresponding comparison interval, wherein the similarity between the abnormal interval and the corresponding reference interval is less than a similarity threshold;

[0209] For each reference interval, it is necessary to calculate the similarity between it and the corresponding comparison interval. The similarity can be calculated by some distance metrics or similarity metrics. Common methods include Euclidean distance, correlation coefficient, cosine similarity, etc. These metrics can be used to measure the similarity of the shape and change trend between two intervals. According to the calculated similarity, the abnormal interval in the comparison interval is determined. If the similarity between a comparison interval and its corresponding reference interval is less than the preset similarity threshold, the comparison interval is marked as an abnormal interval. The selection of the similarity threshold usually needs to be determined according to the specific situation and experimental requirements. In general, the similarity threshold can be set based on experience or previous research results. A higher similarity threshold means that the requirements for the comparison interval and the reference interval are more stringent, and fewer abnormal intervals may be screened out; while a lower similarity threshold means that more intervals may be marked as abnormal intervals.

[0210] S434. Obtain a first test deviation according to the abnormal interval and the corresponding reference interval.

[0211] Based on the comparison results of the abnormal interval and the reference interval, the test deviation can be calculated. The test deviation can be measured by different methods, such as mean absolute error, mean square error, etc. These methods can be used to quantify the degree of difference between the abnormal interval and the reference interval, thereby obtaining a specific value of the test deviation.

[0212] S5. Perform a tensile test on the target sample according to the tensile test parameters and the first test deviation to obtain a second tensile test result.

[0213] Specifically, after obtaining the test deviation, the corresponding workstation can be adjusted according to the test deviation or the tensile test parameters of the corresponding workstation can be adjusted, and the target sample can be tested according to the calibrated parameters and equipment to obtain the test results; through the calibrated parameters and equipment, the test results of the target sample can be ensured to be accurate and reliable, and the target sample tests of multiple workstations can be completed at one time, thereby improving the test efficiency.

[0214] Preferably, performing a tensile test on the target sample according to the tensile test parameter and the first test deviation to obtain a second tensile test result includes:

[0215] S51, adjusting the load increase rate of the expected deformation stage corresponding to the abnormal interval in the tensile test parameter according to the first test deviation, to obtain a first target tensile test parameter;

[0216] First, the experimental deviation obtained in step S43 is analyzed. The experimental deviation reflects the difference between the abnormal interval and the reference interval, which is specifically manifested as deviations in shape, slope, peak value, etc.

[0217] According to the test deviation of the abnormal interval, the load increase rate of the expected deformation stage corresponding to the interval is adjusted. By increasing or decreasing the load increase rate, the rate of change of the load applied to the specimen during the test can be adjusted to better adapt to the characteristics of the test sample and the performance of the abnormal interval.

[0218] The target tensile test parameters are set based on the adjusted load increase rate and other test parameters, including load increase rate, preload, sampling frequency, etc., in order to make the test process more accurate and controllable.

[0219] S52, fixing a preset number of target samples between the upper clamps and the lower clamps of each of the workstations respectively;

[0220] Place a preset number of target specimens between the upper and lower fixtures of each station. The distance between the upper and lower fixtures should be adjusted according to the size of the specimens and experimental requirements to ensure that the specimens can be subjected to uniform tensile force.

[0221] S53, controlling the non-abnormal station to perform a tensile test on the target sample according to the tensile test parameters;

[0222] For non-abnormal stations, according to the set tensile test parameters, the corresponding loading device is used to control the testing machine to apply tensile load to the target specimen. The tensile test parameters include load increase rate, preload load, etc. These parameters determine the load changes applied to the specimen during the test.

[0223] S54, controlling the first abnormal station to perform a tensile test on the target sample according to the first target tensile test parameter;

[0224] For the first abnormal station, the loading device is used to control the testing machine to apply a tensile load to the target sample according to the set first target tensile test parameters. By adjusting the tensile test parameters, the test deviation of the first abnormal station is reduced as much as possible to improve the accuracy and reliability of the test.

[0225] S55. Control the force sensor and the displacement sensor at each station to perform sampling according to the sampling frequency to obtain a second tensile test result.

[0226] During the tensile test, the force sensors and displacement sensors at each station are controlled by sampling frequency to collect data. These sensors will record the load and displacement values ​​during the test, thereby obtaining the second tensile test result, that is, the stress-strain curve of the sample during the tensile process. Through the above steps, the tensile test of the target sample is completed, and the second tensile test result is obtained. These results will be used for further analysis and evaluation to draw conclusions about the material properties.

[0227] In one embodiment, after step S5, the method further includes:

[0228] S6. judging whether there is a second abnormal workstation with test deviation according to the second tensile test results of each of the workstations;

[0229] Specifically, this step uses the second tensile test results of each station to determine whether there is still a test deviation when the tensile test parameters are adjusted according to the first test deviation and the tensile test is performed on the sample again according to the adjusted test parameters. The expected value of each test result can be determined according to the test results of the non-abnormal station in the first test, and the expected value is compared with the second tensile test result. If the deviation of a station exceeds a preset threshold, the station is marked as a second abnormal station.

[0230] By judging whether there are abnormal workstations through the results of the second test, it can be verified whether the first adjustment of the test parameters is effective. If there are still abnormal workstations, it means that the first adjustment may not completely solve the problem and further adjustment is needed. Various factors in the test may cause uncertainty and deviation. The analysis of the second test results can help dynamically adjust the test parameters to ensure the optimization of experimental conditions and the reliability of the results. By continuously monitoring the test results and making feedback adjustments, the test parameters can be gradually optimized so that the entire test system reaches the optimal state. Each abnormality detection and adjustment is part of refined optimization.

[0231] S7. If the second abnormal workstation exists and the second abnormal workstation is the first abnormal workstation, adjust the load increase rate and sampling frequency of the first target tensile test parameter according to the first tensile test result and the second tensile test result to obtain a second target tensile test parameter;

[0232] Specifically, when there is a second abnormal workstation, and the second abnormal workstation and the abnormal workstation when testing the standard specimen belong to the same abnormal workstation, it means that the first parameter adjustment is not in place. At this time, it is necessary to further adjust the parameters of the second abnormal workstation according to the results of the first and second tensile tests, and compare the stress-strain curves of the first and second tests to find out the specific deviation stage. According to the deviation found, finely adjust the load increase rate to make it closer to the ideal value, and increase the sampling frequency, especially in the stage with large deviations, to obtain more detailed data for analysis and adjustment.

[0233] In a preferred embodiment, the step S7 specifically includes:

[0234] S71, obtaining a corresponding second stress-strain curve according to a second tensile test result of a workstation other than the second abnormal workstation;

[0235] Specifically, the second tensile test data of all workstations except the second abnormal workstation are collected. These data include corresponding values ​​of stress and strain obtained by sensors. The collected raw data are preprocessed, such as removing noise, smoothing curves, etc. Then, the stress-strain curve of each workstation is extracted from the preprocessed data, and the integrity and accuracy of the curve are ensured;

[0236] The set of stress-strain curves of workstations other than the second abnormal workstation can be used as a reference for normal working conditions. By comparing the curves of each workstation, the overall stress-strain relationship can be identified, which helps to determine which data are normal.

[0237] S72, performing data alignment and curve fusion on the second stress-strain curves to obtain a second stress-strain reference curve;

[0238] Specifically, firstly, the stress-strain curves of the workstations other than the second abnormal workstation are aligned on the time axis or the strain axis to ensure that all curves are compared under the same strain; then, mathematical methods such as the average value or the weighted average method are used to fuse the aligned curves to generate a comprehensive second stress-strain reference curve. During the fusion process, possible outliers are identified and processed to ensure the smoothness and stability of the reference curve, thereby obtaining a smooth and representative stress-strain reference, reducing the influence of individual abnormal data. Through the reference curve, the abnormal interval of the second abnormal workstation can be more clearly identified.

[0239] S73, a second stress-strain abnormal curve according to the second tensile test result of the second abnormal station;

[0240] Specifically, similar to step S71, the second tensile test data of the second abnormal station is collected, and the collected raw data is preprocessed, such as removing noise, smoothing the curve, etc., and then the stress-strain curve of the second abnormal station is extracted from the preprocessed data to provide a specific basis for subsequent abnormal interval analysis and parameter adjustment;

[0241] S74, obtaining a second abnormal interval having a second test deviation according to the second stress-strain abnormal curve and the second stress-strain reference curve;

[0242] Specifically, the abnormal curve of the second abnormal workstation is compared with the second stress-strain reference curve to find out the difference between the two, identify the interval where the stress or strain obviously deviates from the reference curve, mark it as the second abnormal interval, and conduct a detailed analysis of the data in the abnormal interval to quantify the degree of deviation, thereby clarifying the location and range of the abnormal interval, making subsequent adjustments more targeted.

[0243] S75. Obtaining a parameter adjustment deviation of the first target tensile test parameter according to the first stress-strain anomaly curve and the second stress-strain anomaly curve;

[0244] Specifically, the first stress-strain anomaly curve is obtained based on the initial tensile test (test before adjustment), and the second stress-strain anomaly curve is obtained based on the adjusted first target tensile test parameters. The first stress-strain anomaly curve is compared with the second stress-strain anomaly curve. During the comparison process, the curve alignment method can be used to ensure that the two curves are compared within the same strain range. The focus of the comparison is to identify the similarities and differences between the two abnormal intervals, mainly including:

[0245] Location of abnormal interval: whether the second abnormal interval overlaps with the first abnormal interval;

[0246] Abnormal amplitude: whether the stress deviation degree of the second abnormal interval is smaller than that of the first;

[0247] Abnormal trend: whether the stress change trend in the second test is closer to the expected one;

[0248] Through the comparative analysis results of the above three aspects, the tensile test parameters that need to be further adjusted are determined. For example, if there is still deviation in the abnormal interval of the second test, but the amplitude is reduced, it can be judged that the first parameter adjustment is effective, but further optimization is needed to determine the specific parameter adjustment deviation, such as the load increase rate. These parameter adjustment deviations are based on the comparative results of the two tests and are determined by analyzing the specific deviation degree and trend of the abnormal interval.

[0249] By comparing the two abnormal curves, the specific needs for parameter adjustment can be accurately identified, the pertinence and effectiveness of the adjustment can be improved, and the location, amplitude and trend of the abnormal interval can be analyzed, which helps to fully understand the root cause of the abnormality and thus make parameter adjustments more scientifically. The obtained parameter adjustment deviation provides detailed guidance for subsequent experiments and improves the accuracy and repeatability of the experiments.

[0250] S76. According to the second test deviation and the parameter adjustment deviation, adjust the load increase rate corresponding to the second abnormal interval in the first target tensile test parameter, and according to the preset sampling frequency increment, increase the sampling frequency of the expected deformation stage corresponding to the second abnormal interval in the first target tensile test parameter to obtain the second target tensile test parameter.

[0251] Specifically, according to the analysis in step S75, the position and range of the second abnormal interval have been determined. The second abnormal interval refers to the area where the stress-strain curve deviates in both the first test and the second test after adjustment. The load increase rate in the second abnormal interval is determined based on the second test deviation and the parameter adjustment deviation. The adjustment goal of the load increase rate is to make the stress-strain curve closer to the ideal value in the abnormal interval, thereby eliminating or reducing the deviation. If the second test deviation shows that the stress value in the abnormal interval is low, the load increase rate can be increased; if the stress value is high, the load increase rate is reduced.

[0252] According to the preset sampling frequency increment, the sampling frequency is increased in the expected deformation stage corresponding to the second abnormal interval. The increase in sampling frequency helps to capture the changes in the stress-strain curve in the abnormal interval in more detail, thereby providing more accurate data for analysis and adjustment. The sampling frequency increment can be determined based on historical data and experience, such as increasing the sampling frequency from 1 time per second to 10 times per second in the stage of large deviation. The adjusted load increase rate and the parameters of increasing the sampling frequency are combined to form the new second target tensile test parameters;

[0253] By fine-tuning the load increase rate, the stress-strain curve is closer to the ideal state in the abnormal range, thereby improving the accuracy of the test results; by increasing the sampling frequency, more detailed data can be obtained, which helps to more accurately analyze the stress-strain relationship, identify potential problems and make adjustments. The dynamic adjustment of parameters can more flexibly respond to the test needs of different stages, especially special treatment in the abnormal range, to ensure the stability and reliability of the overall test process.

[0254] S8. If the second abnormal workstation exists and the second abnormal workstation is not the first abnormal workstation, obtain a first test condition when performing a tensile test on the standard sample and a second test condition when performing a tensile test on the target sample, wherein the first test condition and the second test condition both include a test equipment state, a test environment condition, and a test operation condition;

[0255] Specifically, if the second abnormal station exists and the second abnormal station is not the first abnormal station, it means that in the second test, a station that was not marked as abnormal before appeared as an abnormal station. The abnormal station in the first test may be caused by a specific equipment state, environmental conditions or operation mode. The new abnormal station that appeared in the second test may be a new problem caused by different reasons. The first adjustment may be effective under specific conditions, but it does not solve all potential problems.

[0256] The consistency of test conditions is the basis for ensuring the comparability of results. If the test conditions are different for two tests, the abnormal results may be caused by the difference in conditions, rather than problems with the sample or equipment itself.

[0257] Therefore, in this case, the test conditions of the two tensile tests are obtained, wherein the first test condition and the second test condition both include the test equipment status, test environment conditions and test operation conditions, the test equipment status includes the calibration status, usage time, maintenance records, etc. of the equipment; the test environment conditions include but are not limited to environmental factors such as temperature, humidity, vibration, etc. of the space where the test machine is located; the test operation conditions include operation steps, operators, etc.;

[0258] The calibration status of the test equipment affects the measurement precision and accuracy. Improperly calibrated equipment may cause deviations in test data. Equipment may wear out or change in performance after long-term use, affecting its stability and the consistency of measurement results.

[0259] Temperature changes can affect the strength and toughness of materials, thus affecting test results. High temperatures can cause materials to soften, while low temperatures can increase their brittleness. High humidity can cause materials to absorb moisture, changing their mechanical properties, especially for hygroscopic materials such as cellulose. Vibrations in the space where the test machine is located can interfere with the stability and measurement accuracy of the test equipment, especially for precision measurement equipment.

[0260] The skill level and experience of the operator will have an impact on the quality of the test execution. Experienced operators may be better able to control the variables in the test process and ensure the consistency and accuracy of the data.

[0261] S9. If the first test condition and the second test condition are inconsistent, adjusting the second test condition according to the first test condition;

[0262] Specifically, check whether the equipment is in the same state for the two tests, such as whether the same calibration has been performed. Check whether the environmental conditions such as temperature and humidity are consistent for the two tests, and check whether the operating steps and operators are consistent, so as to determine the specific differences in the two test conditions, such as different equipment calibrations, different environmental temperatures, etc., and adjust the conditions of the second test to the same conditions as the first test to ensure the consistency of the test, so as to eliminate the influence of the condition differences on the results.

[0263] S10. If the first test condition is consistent with the second test condition, record the number of abnormal occurrences of the second abnormal station;

[0264] Specifically, under the same test conditions, record the number of abnormalities at the second abnormal station. If the test conditions have not changed, but the second abnormal station still has abnormalities, this may indicate that there are problems with the material or the test procedure itself under the same operating environment and equipment status. Some abnormalities may be caused by random changes in the system or accidental factors in a specific test. In this case, the occurrence of different abnormal stations under the same conditions may be due to different test cycles or the occurrence of specific events. By recording the number of abnormalities, it can be ensured that it is not accidental or short-term fluctuations.

[0265] S101. If the number of abnormal occurrences is greater than a preset abnormal occurrence threshold, adjust the tensile test parameters of the second abnormal workstation according to the second tensile test results corresponding to the number of abnormal occurrences of each workstation.

[0266] Specifically, a preset threshold for abnormal occurrence is set. This threshold can be determined based on historical data, quality control standards or experience. Exceeding this threshold means that the test results of a certain station have shown instability or deviation from expectations, and are not caused by random changes in the system or accidental factors in a specific experiment. At this time, according to the second abnormal station and the second tensile test results of the stations other than the second abnormal station when each abnormality occurs, according to the stress-strain curve in the second tensile test result, the load increase rate is adjusted, specifically by comparing the curve of the abnormal station with the curve of the non-abnormal station. If the curve shows an abnormal or abnormal trend, the corresponding interval needs to reduce the load increase rate to stabilize the test process. According to the test stage that needs to be accurately monitored, adjust the frequency of data acquisition. Increasing the sampling frequency can capture more detailed changes in the test process, which helps to accurately analyze the test results. Through the above steps, the tensile test parameters of the abnormal station can be systematically processed and adjusted to ensure the accuracy and stability of the test data, while improving product quality and production efficiency.

[0267] Example 2

[0268] See also Figure 5 An embodiment of the present invention provides a control system for a multi-station electronic testing machine, the control system comprising: a control module, a loading module, a sensor module and a power module, the loading module is used to apply a load to a test sample, the sensor module is used to monitor the load and displacement applied to the sample in real time, the power module is used to supply energy to the control system, and the control module is used to execute the control method of the multi-station electronic testing machine described in the first aspect.

[0269] Specifically, the control module can realize intelligent control of the multi-station testing machine, with a high degree of automation, which improves the test efficiency and production efficiency. The sensor module can monitor the load and displacement applied to the specimen in real time to ensure the accuracy and reliability of the test data. The loading module can apply different loads to the test specimen according to the test requirements, meet the requirements of different materials and test standards, and has strong applicability and flexibility. Through intelligent control of the testing machine, the control system can realize full monitoring and safety assurance of the test process, reduce operational risks, and ensure the safety of operators. The power module can provide a stable power supply for the entire control system, ensure the continuity and stability of the test process, and improve the reliability and continuous operation capability of the system.

[0270] In summary, the control system can improve test efficiency, ensure the accuracy of test data, meet different test requirements, and ensure operational safety, and has high practical value and economic benefits.

[0271] It should be clear that the present invention is not limited to the specific configuration and processing described above and shown in the figures. For the sake of simplicity, a detailed description of the known method is omitted here. In the above embodiments, several specific steps are described and shown as examples. However, the method process of the present invention is not limited to the specific steps described and shown, and those skilled in the art can make various changes, modifications and additions, or change the order between the steps after understanding the spirit of the present invention.

[0272] The functional blocks shown in the structural block diagram described above can be implemented as hardware, software, firmware or a combination thereof. When implemented in hardware, it can be, for example, an electronic circuit, an application specific integrated circuit (ASIC), appropriate firmware, a plug-in, a function card, etc. When implemented in software, the elements of the present invention are programs or code segments used to perform the required tasks. The program or code segment can be stored in a machine-readable medium, or transmitted on a transmission medium or a communication link by a data signal carried in a carrier. "Machine-readable medium" may include any medium capable of storing or transmitting information. Examples of machine-readable media include electronic circuits, semiconductor memory devices, ROMs, flash memories, erasable ROMs (EROMs), floppy disks, CD-ROMs, optical disks, hard disks, optical fiber media, radio frequency (RF) links, etc. The code segment can be downloaded via a computer network such as the Internet, an intranet, etc.

[0273] It should also be noted that the exemplary embodiments mentioned in the present invention describe some methods or systems based on a series of steps or devices. However, the present invention is not limited to the order of the above steps, that is, the steps can be performed in the order mentioned in the embodiments, or in a different order from the embodiments, or several steps can be performed simultaneously.

[0274] The above is only a specific implementation of the present invention. Those skilled in the art can clearly understand that for the convenience and simplicity of description, the specific working process of the system, module and unit described above can refer to the corresponding process in the aforementioned method embodiment, and will not be repeated here. It should be understood that the protection scope of the present invention is not limited to this. Any technician familiar with the technical field can easily think of various equivalent modifications or replacements within the technical scope disclosed by the present invention, and these modifications or replacements should be covered within the protection scope of the present invention.

Claims

1. A control method for a multi-station electronic testing machine, characterized in that: The multi-station electronic testing machine comprises a base, a frame and a crossbeam, wherein the frame is fixedly connected to the upper surface of the base, the crossbeam is slidably connected to the frame, a preset number of stations are arranged between the crossbeam and the base, each of the stations comprises a sensor, a loading device and a fixture, the fixture comprises an upper fixture connected to the crossbeam and a lower fixture connected to the base, the loading device is connected to the upper fixture and is used to drive the upper fixture to load the sample, the sensor comprises a displacement sensor for measuring the deformation amount of the sample during the loading process and a force sensor for measuring the load value applied to the sample, and the method comprises: According to the material parameters of the target sample, obtaining tensile test parameters, wherein the tensile test parameters include load increase rate, preload load and sampling frequency; Performing a tensile test on a standard sample according to the tensile test parameters, wherein the material parameters of the standard sample are the same as the material parameters of the target sample; Obtaining the preset number of first tensile test results according to the deformation value obtained by the displacement sensor and the load value obtained by the force sensor; According to each of the first tensile test results, obtaining a first test deviation of the corresponding workstation; Performing a tensile test on the target sample according to the tensile test parameters and the first test deviation to obtain a second tensile test result; The step of obtaining tensile test parameters according to the material parameters of the target sample includes: Acquiring material parameters of the target sample, wherein the material parameters include: material type information and material size information; Acquiring the expected strength parameter of the target sample according to the material type information and the material size information; According to the material type, obtaining an elastic modulus range, an initial yield strength range, and an initial tensile strength range; Calculating the minimum cross-sectional area of ​​the target sample in the stretching direction according to the material size information; According to the minimum cross-sectional area, obtaining a yield strength adjustment factor and a tensile strength adjustment factor; According to the yield strength adjustment coefficient and the tensile strength adjustment coefficient, the initial yield strength range and the initial tensile strength range are adjusted respectively to obtain a yield strength range and a tensile strength range; Obtaining the expected strength parameter according to the respective minimum values ​​or intermediate values ​​of the elastic modulus range, the yield strength range, and the tensile strength range, wherein the expected strength parameter includes the expected elastic modulus, the expected yield strength, and the expected tensile strength; Determining the tensile test parameters according to the expected strength parameters; Determining the tensile test parameters according to the expected strength parameters includes: determining the preload load based on the material type, the expected strength parameter, and the minimum cross-sectional area; According to the expected strength parameter and material type, the expected deformation stage of the target sample is obtained, wherein the expected deformation stage includes an elastic deformation stage, a yield stage, a plastic deformation stage, a necking stage and a fracture stage; Determining the load increase rates of the elastic deformation stage, the yield stage, and the plastic deformation stage according to the expected strength parameter, wherein the load increase rates of the elastic deformation stage, the yield stage, and the plastic deformation stage decrease in sequence; According to a preset necking rate and a preset fracture rate, setting the load increase rate in the necking stage and the fracture stage, wherein the preset necking rate is greater than the preset fracture rate; Setting the sampling frequency of the elastic deformation stage and the plastic deformation stage to a first sampling frequency; Setting the sampling frequency of the yield stage to a second sampling frequency; Setting the sampling frequencies of the necking stage and the fracture stage to a third sampling frequency, wherein the first sampling frequency, the second sampling frequency, and the third sampling frequency are increased in sequence; Determining the tensile test parameters according to the sampling frequency, load increase rate and preload load of each expected deformation stage; The method of performing a tensile test on a standard specimen according to the tensile test parameters comprises: Fixing a preset number of standard specimens between the upper and lower clamps of each station respectively; Controlling the loading device of each station to apply an initial load to the standard specimen according to the preload load; Controlling the loading device of each station to gradually increase the applied load according to the load increase rate; Control the force sensor and the displacement sensor to perform sampling according to the sampling frequency to obtain original load data and original displacement data; The step of obtaining the preset number of first tensile test results according to the deformation value obtained by the displacement sensor and the load value obtained by the force sensor comprises: Preprocessing the original load data and original displacement data of each workstation to obtain corresponding target load data and target displacement data; According to the target load data and the target displacement data, a stress-strain curve of the standard sample of each station is drawn; According to the stress-strain curve, the actual elastic modulus, actual yield strength, actual tensile strength and elongation at break of each of the standard samples are obtained; Obtaining a first tensile test result of each of the standard specimens according to the actual elastic modulus, the actual yield strength and the actual tensile strength; The obtaining the test deviation of the corresponding workstation according to each of the first tensile test results includes: If the standard deviation of the actual elastic modulus of a workstation is greater than the first preset standard deviation, and / or the standard deviation of the actual yield strength is greater than the second preset standard deviation, and / or the standard deviation of the actual tensile strength is greater than the third preset standard deviation, the workstation is marked as a first abnormal workstation and the workstations other than the first abnormal workstation are marked as non-abnormal workstations, wherein the first preset standard deviation is less than the second preset standard deviation, and the second preset standard deviation is less than or equal to the third preset standard deviation; Performing data alignment and curve fusion on the stress-strain curves of each of the non-abnormal workstations to obtain a first stress-strain reference curve; According to the first tensile test result of the first abnormal station, a first stress-strain abnormal curve is obtained; According to the curve characteristics, the first stress-strain reference curve and the first stress-strain abnormal curve are divided to obtain a reference interval and a comparison interval, respectively, wherein the reference interval and the comparison interval both include an elastic deformation interval, a yield stage interval, a plastic deformation interval, a necking interval, and a fracture interval; Determine a first abnormal interval in the comparison interval according to the similarity between the reference interval and the corresponding comparison interval, wherein the similarity between the first abnormal interval and the corresponding reference interval is less than a similarity threshold; Obtaining a first test deviation according to the first abnormal interval and the corresponding reference interval; The step of performing a tensile test on the target sample according to the tensile test parameter and the first test deviation to obtain a second tensile test result includes: According to the first test deviation, adjusting the load increase rate of the expected deformation stage corresponding to the abnormal interval in the tensile test parameter to obtain a first target tensile test parameter; Fixing a preset number of target samples between the upper and lower clamps of each station respectively; According to the tensile test parameters, controlling the non-abnormal station to perform a tensile test on the target sample; According to the first target tensile test parameter, controlling the first abnormal station to perform a tensile test on the target sample; The force sensor and the displacement sensor at each station are controlled to perform sampling according to the sampling frequency to obtain a second tensile test result.

2. The control method of the multi-station electronic testing machine according to claim 1, characterized in that: After performing a tensile test on the target sample according to the tensile test parameters and the first test deviation to obtain a second tensile test result, the method further includes: According to the second tensile test results of each of the workstations, determining whether there is a second abnormal workstation with a test deviation; If the second abnormal workstation exists and the second abnormal workstation is the first abnormal workstation, adjusting the load increase rate and sampling frequency of the first target tensile test parameter according to the first tensile test result and the second tensile test result to obtain a second target tensile test parameter; If the second abnormal workstation exists and the second abnormal workstation is not the first abnormal workstation, obtaining a first test condition when performing a tensile test on the standard specimen and a second test condition when performing a tensile test on the target specimen, wherein the first test condition and the second test condition both include a test equipment state, a test environment condition, and a test operation condition; If the first test condition and the second test condition are inconsistent, adjusting the second test condition according to the first test condition; If the first test condition is consistent with the second test condition, record the number of abnormal occurrences of the second abnormal station; If the number of abnormal occurrences is greater than a preset abnormal occurrence threshold, the tensile test parameters of the second abnormal workstation are adjusted according to the second tensile test results corresponding to the number of abnormal occurrences of each workstation.

3. The control method of the multi-station electronic testing machine according to claim 2, characterized in that: If the second abnormal workstation exists and the second abnormal workstation is the first abnormal workstation, adjusting the load increase rate and the sampling frequency of the first target tensile test parameter according to the first tensile test result and the second tensile test result to obtain the second target tensile test parameter, comprises: According to the second tensile test results of the workstations other than the second abnormal workstation, obtaining a corresponding second stress-strain curve; Performing data alignment and curve fusion on the second stress-strain curves to obtain a second stress-strain reference curve; a second stress-strain abnormal curve according to the second tensile test result of the second abnormal station; Obtaining a second abnormal interval having a second test deviation according to the second stress-strain abnormal curve and the second stress-strain reference curve; Obtaining a parameter adjustment deviation of the first target tensile test parameter according to the first stress-strain anomaly curve and the second stress-strain anomaly curve; According to the second test deviation and the parameter adjustment deviation, the load increase rate corresponding to the second abnormal interval in the first target tensile test parameter is adjusted, and according to the preset sampling frequency increment, the sampling frequency of the expected deformation stage corresponding to the second abnormal interval in the first target tensile test parameter is increased to obtain the second target tensile test parameter.

4. A control system for a multi-station electronic testing machine, characterized in that: The control system includes: a control module, a loading module, a sensor module and a power module. The loading module is used to apply a load to the test sample, the sensor module is used to monitor the load and displacement applied to the sample in real time, the power module is used to supply energy to the control system, and the control module is used to execute the control method of the multi-station electronic testing machine described in any one of claims 1 to 3.