A modeling method and system for finite element model of steel structure weld

By identifying and classifying weld shapes, calculating welding evaluation index and quality index, and evaluating welding defects, the problem of unstable welding quality in the existing technology is solved, and the efficiency, safety and reliability of the welding process are achieved.

CN118569047BActive Publication Date: 2024-11-08ZHEJIANG JUNRUN MACHINERY MANUFACTURING CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411036290.5
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2024-07-31
Publication Date
2024-11-08
Estimated Expiration
2044-07-31

AI Technical Summary

Technical Problem

The existing finite element modeling method for welds in the welds fail to effectively consider the impact of weld shape, bevel angle and depth on welding quality, resulting in unstable welding quality and increasing the risk of welding defects, such as weld cracks, Fusing and pores affect the safety of steel structures.

Method used

Using a modeling system of a steel structure weld finite element model, a three-dimensional model is established through visual detection technology, and the weld shape is identified and classified, the weld pool volume, bevel angle, depth and geometric feature index are collected, and the welding evaluation is calculated. Index and quality index, evaluate welding defects and adjust welding plans to ensure welding quality.

Benefits of technology

It improves welding quality and efficiency, promptly detects welding abnormalities, prevents weld cracks, unfusion and pores, enhances the reliability and safety of the welding process, and provides a basis for targeted adjustment of welding solutions.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118569047B_ABST
    Figure CN118569047B_ABST
Patent Text Reader

Abstract

The invention discloses a modeling method and system of a finite element model of a steel structure weld, and relates to the technical field of steel structures. The system obtains weld characteristic parameters with high precision through a three-dimensional laser scanner and a digital image processing system, comprehensively evaluates parameters and quality in a welding process through calculation of a welding evaluation index Hc and a welding quality index Hz, timely discovers welding quality problems, prevents weld cracks, unfusion and pores, and takes corresponding measures to correct them; through comprehensive evaluation of a weld molten pool index Rz, a welding evaluation index Hc and a welding quality index Hz, the system comprehensively evaluates the quality and structural characteristics of the weld, and then calculates a weld defect index QX, discovers potential defects in welding and takes corresponding measures to correct them in time, and then compares the weld molten pool index Rz, the welding evaluation index Hc and the welding quality index Hz, so as to solve welding quality problems in a targeted manner and improve welding quality and structural safety.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of steel structures, and in particular to a modeling method and system for a finite element model of a steel structure weld. Background Art

[0002] The origin of the modeling system of the finite element model of the weld of a ship steel structure can be traced back to the increasing demand for ship structure design and welding process optimization. In the patent with application number CN202010904901.9, the patent discloses a method for modeling a finite element model of a welded steel structure weld, which belongs to the field of welding technology. The modeling method includes: establishing a three-dimensional model of a welded steel structure including a weld, obtaining the position coordinates and feature information of the weld and generating a weld information data file, wherein the feature information includes the weld type, weld leg size and weld length; and creating a weld finite element model according to the weld information data file. The method for modeling a finite element model of a welded steel structure provided in the present disclosure improves the simulation height of the weld and further improves the accuracy of the weld simulation calculation results.

[0003] However, in the application number CN202010904901.9, the influence of weld shape, groove angle and depth was not carefully considered. The features were extracted only by the length of the size, ignoring the potential influence of the molten pool formed by different weld shapes, grooves and depths on the welding quality. In the actual welding process, welds can be roughly divided into different shapes such as I, V, and U. Traditional methods mostly use fixed welding evaluation indexes and universal groove designs, ignoring the potential influence of different weld shapes on welding quality, resulting in unstable welding quality or increased risk of welding defects. These defects include weld cracks, lack of fusion and pores, which not only affect the welding strength, but also lead to safety hazards of steel structures in use. Summary of the invention

[0004] Technical issues solved

[0005] In view of the deficiencies in the prior art, the present invention provides a modeling method and system for a finite element model of a steel structure weld, which solves the problems in the background technology.

[0006] Technical Solution

[0007] To achieve the above objectives, the present invention is implemented through the following technical solutions: a modeling system for a finite element model of a steel structure weld, comprising a model building module, an identification and extraction module, a welding mid-term monitoring module, a welding quality monitoring module, and an evaluation generation module;

[0008] The model building module is used to collect ship weld information using visual inspection technology, draw the geometric shape and connection parts of the ship weld through CAD, build a three-dimensional ship steel structure weld model, and generate a grid in the three-dimensional ship steel structure weld model to analyze the weld area;

[0009] The identification and extraction module is used to identify the weld shape and classify the welds with the same shape to obtain an I-shaped weld area, a V-shaped weld area and a U-shaped weld area, and perform a first classification mark in the three-dimensional ship steel structure weld model;

[0010] The molten pool volume Tj, groove angle Pjd, groove depth Pkj and geometric characteristic index Jtz of each weld in the I-shaped weld area, the V-shaped weld area and the U-shaped weld area are collected to construct a molten pool data set for the weld to be welded, and the molten pool index Rz of the weld to be welded is obtained by calculation, and then the value of the molten pool index Rz of the weld to be welded is marked as the second classification in the three-dimensional ship steel structure weld model;

[0011] The welding mid-term monitoring module is used to collect various parameters of the I-shaped weld area, the V-shaped weld area and the U-shaped weld area during the welding process, and to construct a welding data set, and to calculate the welding evaluation index Hc using the welding data set;

[0012] The welding quality monitoring module is used to collect quality data of the I-shaped weld area, the V-shaped weld area and the U-shaped weld area after welding, establish a quality data set, and extract the welding quality index Hz in the quality data set to obtain the weld construction defect index QX;

[0013] The evaluation generation module is used to evaluate the defect index QX. The evaluation defect index QX is evaluated by using the preset threshold value X of the evaluation unit, and the loading conditions of the steel structure welding area are set. The analysis results and the visual charts are then integrated into the analysis report, which is presented to the user through the generation unit to help the user understand the analysis results and make corresponding decisions.

[0014] Preferably, the model building module includes a visual inspection unit, a drawing unit, a material setting unit and a grid generation unit. The ship steel structure is scanned by the visual inspection unit to obtain the geometric shape and connection part information of the weld; then, the data obtained by the visual inspection unit is accurately drawn into a geometric model using the CAD software in the drawing unit; finally, the material setting unit is used to set the material parameters; and the grid generation unit is used to automatically grid the welding connection parts.

[0015] Preferably, the I-shaped weld area, the V-shaped weld area and the U-shaped weld area correspond to different welding processes and structural requirements, respectively, and the weld areas of different shapes are distinguished by the first classification mark;

[0016] The second classification mark shows the quality and structural characteristics of each weld area, and the weld pool volume Tj is the volume of the molten pool formed by the molten metal during the welding process;

[0017] The groove angle Pkj refers to the angle formed on both sides of the weld joint after notching;

[0018] The groove depth Pks is the distance from the workpiece surface to the bottom of the groove before welding;

[0019] The geometric characteristic index Jtz includes: weld length Hfc, weld width Hfk, weld depth Hfs and weld cross area Hfj.

[0020] The weld pool volume Tj and groove depth PkJ are measured by a three-dimensional laser scanner to perform high-precision three-dimensional scanning on the weld surface, thereby obtaining the weld volume and groove depth;

[0021] During welding, the weld is filled with molten metal, so the volume of the weld is equal to the weld pool volume Tj as the volume of the molten metal pool;

[0022] The weld length Hfc, weld width Hfk and weld depth Hfs are measured by taking a digital image of the weld surface through a digital image processing system and then combining image processing technology;

[0023] The weld intersection area Hfj is obtained by scanning and measuring the cross section of the weld using a cross section scanner to obtain the intersection area of ​​the weld cross section and the substrate.

[0024] Preferably, the geometric characteristic index Jtz is obtained by extracting the weld length Hfc, weld width Hfk, weld depth Hfs and weld cross area Hfj of each weld, performing dimensionless processing, and calculating the geometric characteristic index Jtz by the following formula:

[0025]

[0026] Where n is the number of welds; Hfc i is the length of the ith weld; Hfk i is the width of the ith weld; Hfs i is the depth of the ith weld; Hfj i is the cross-sectional area of ​​the ith weld; w i is the weight of the ith weld feature, and A is represented as the first correction constant;

[0027] The weld pool index Rz is obtained by the following calculation formula:

[0028]

[0029] Wherein, q1, q2, q3 and q4 represent the weight values ​​of the weld pool volume Tj, groove depth Pks, groove angle Pkj and geometric characteristic index Jtz, respectively, and the weld pool volume Tj, groove depth Pks, groove angle Pkj and geometric characteristic index Jtz are all dimensionless, and B is the second correction constant.

[0030] Preferably, the welding evaluation index Hc includes: welding current Hdl, welding voltage Hdy, welding speed Hsd, shielding gas flow rate Bql and welding temperature Hwd;

[0031] The welding current Hdl and the welding voltage Hdy are measured by a voltmeter of an arc welding device;

[0032] The welding speed Hsd is measured by the encoder;

[0033] The shielding gas flow rate Bql is monitored by a gas flow meter;

[0034] The welding temperature Hwd is monitored by an infrared thermal imager;

[0035] After dimensionless processing of welding current Hdl, welding voltage Hdy, welding speed Hsd, shielding gas flow rate Bql and welding temperature Hwd, the welding evaluation index Hc is calculated by the following formula:

[0036] ;

[0037] Wherein, Bz represents the preset flow rate threshold for the I-shaped weld area, the V-shaped weld area and the U-shaped weld area, and Bz has different preset flow rate thresholds according to the I-shaped weld area, the V-shaped weld area and the U-shaped weld area, and can be adjusted by the user. is a sigmoid function with a value range of [0,1]. w1, w2, w3, w4 and w5 represent the weight values ​​of welding current Hdl, welding voltage Hdy, welding speed Hsd, shielding gas flow rate Bql and welding temperature Hwd respectively. C represents the third correction constant.

[0038] Preferably, the welding quality index Hz includes heat influence index Ryx, welding penetration Hrs and residual stress Cyl;

[0039] The heat impact index Ryx is obtained by monitoring with a thermal simulation instrument;

[0040] The welding penetration gap density value Hrs is obtained by analyzing and evaluating the weld through X-ray diffraction analysis. The density value of the welding penetration gap indicates the degree of fusion between the material in the weld and the inner surface of the weld structure. The greater the degree of fusion, the greater the gap density value, which reduces the sealing performance of the weld. The smaller the degree of fusion, the smaller the gap density value, which is in direct and inverse proportion.

[0041] The residual stress Cyl is obtained by measuring with an electron diffractometer;

[0042] After the heat influence index Ryx, welding penetration Hrs and residual stress Cyl are dimensionless The welding quality index Hz is calculated by the following formula:

[0043]

[0044] Wherein, e1, e2 and e3 represent the weight values ​​of heat influence index Ryx, welding penetration Hrs and residual stress Cyl respectively, 3 represents the total number of parameters, and D represents the fourth correction constant.

[0045] Preferably, the weld pool index Rz, welding evaluation index Hc, and welding quality index Hz are dimensionlessly processed and the defect index QX is calculated by the following formula:

[0046]

[0047] In the formula, w i represents the weight coefficient and 3 represents the total number of parameters.

[0048] Preferably, the evaluation unit performs evaluation by using a preset threshold value X and a defect index QX to obtain the following solution:

[0049] If the preset threshold value X>defect index QX, it means that the current ship steel structure welding is qualified, there are no weld cracks, lack of fusion, and pores, and there is no need to adjust the welding plan;

[0050] If the preset threshold value X is less than the defect index QX, it means that the welding of the current ship steel structure is unqualified, and problems such as weld cracks, lack of fusion, and pores occur, and the welding plan should be adjusted;

[0051] When the welding of the ship steel structure is unqualified, the weld pool index Rz, welding evaluation index Hc and welding quality index Hz are compared to obtain the defect points of the ship steel structure and make targeted adjustments to the welding plan.

[0052] Preferably, the evaluation generation module uses a condition setting unit to set loading conditions for the welding area of ​​the steel structure, and sets the loading conditions according to the weld pool data set, welding data set and quality data set; the generation unit presents the analysis report to the user through an interactive interface.

[0053] Preferably, a modeling method for a steel structure weld finite element model comprises the following steps:

[0054] Step 1, the model building module collects ship weld information by using visual inspection technology, draws the geometric shape and connection parts of the ship weld by CAD, builds a three-dimensional ship steel structure weld model, and generates a grid in the three-dimensional ship steel structure weld model to analyze the weld area;

[0055] Step 2: an identification and extraction module identifies the weld shape and classifies the welds with the same shape to obtain an I-shaped weld area, a V-shaped weld area, and a U-shaped weld area, and performs a first classification mark in the three-dimensional ship steel structure weld model;

[0056] The molten pool volume Tj, groove angle Pjd, groove depth Pkj and geometric characteristic index Jtz of each weld in the I-shaped weld area, the V-shaped weld area and the U-shaped weld area are collected to construct a molten pool data set (201) for the weld to be welded, and the molten pool index Rz of the weld to be welded is obtained by calculation, and the value of the molten pool index Rz of the weld to be welded is marked as a second classification in the three-dimensional ship steel structure weld model;

[0057] Step 3, the welding mid-term monitoring module collects various parameters of the I-shaped weld area, the V-shaped weld area and the U-shaped weld area during the welding process, and constructs a welding data set, and uses the welding data set to calculate the welding evaluation index Hc;

[0058] Step 4, the welding quality monitoring module establishes a quality data set by collecting quality data of the I-shaped weld area, the V-shaped weld area and the U-shaped weld area after welding, and extracts the welding quality index Hz in the quality data set to obtain the weld construction defect index QX;

[0059] Step 5: Evaluation generation module evaluates the defect index QX, sets the loading conditions of the steel structure welding area, calculates the indicators of the overall welding area using the solution unit, and integrates the analysis results and visualization charts into the analysis report. It is presented to the user through the generation unit to help the user understand the analysis results and make corresponding decisions.

[0060] Beneficial Effects

[0061] The present invention provides a modeling method and system for a finite element model of a steel structure weld, which has the following beneficial effects:

[0062] (1) A modeling method and system for a finite element model of a steel structure weld. The identification and extraction module automatically identifies welds of different shapes and classifies them to facilitate subsequent data processing and analysis; a weld pool data set 201 is constructed, and the weld pool index Rz is calculated to detect potential welding quality problems in advance; a welding evaluation index Hc is calculated to detect abnormal conditions in the welding process in time and improve welding quality and efficiency; a welding quality monitoring module collects quality data after welding is completed and extracts the welding quality index Hz and the weld defect index QX; a comprehensive understanding of welding quality and existing defects is provided to provide a basis for subsequent repair and improvement; and an evaluation generation module helps users understand the analysis results and make corresponding decisions.

[0063] (2) A modeling method and system for a finite element model of a steel structure weld seam, through a three-dimensional laser scanner and a digital image processing system, obtains weld seam characteristic parameters with high precision, thereby improving the accuracy and reliability of data; through the calculation of the welding evaluation index Hc and the welding quality index Hz, comprehensively evaluates the parameters and quality in the welding process, timely discovers welding quality problems, prevents weld cracks, lack of fusion and pores, and takes corresponding measures to correct them; through the comprehensive evaluation of the weld molten pool index Rz, the welding evaluation index Hc and the welding quality index Hz, systematically and comprehensively evaluates the quality and structural characteristics of the weld seam, and then calculates the weld seam defect index QX, discovers potential defects in welding and takes corresponding measures to correct them in time.

[0064] (3) A modeling method and system for a finite element model of a steel structure weld. The evaluation generation module helps users quickly understand whether the current welding quality meets the standard by comparing the preset threshold value X and the defect index QX; quickly identify welding failures and take timely measures to adjust the welding plan to avoid further quality problems; based on the weld pool index Rz, the welding evaluation index Hc and the welding quality index Hz, solve welding quality problems in a targeted manner to improve welding quality and structural safety; by utilizing the weld pool data set, the welding data set and the quality data set; the generation unit presents the analysis report to the user through an interactive interface, improving the user experience while promoting effective communication and exchange between the user and the system. BRIEF DESCRIPTION OF THE DRAWINGS

[0065] Figure 1 A schematic diagram of the framework flow of a modeling system for a finite element model of a steel structure weld according to the present invention;

[0066] Figure 2 The present invention is a schematic diagram of a method for modeling a finite element model of a steel structure weld.

[0067] In the figure: 1. Model building module; 101. Visual inspection unit; 102. Drawing unit; 103. Material setting unit; 104. Mesh generation unit; 2. Identification and extraction module; 201. Molten pool data set for welding seam; 3. Mid-term welding monitoring module; 301. Welding data set; 4. Welding quality monitoring module; 401. Quality data set; 5. Evaluation and generation module; 501. Evaluation unit; 502. Condition setting unit; 503. Solution unit; 504. Generation unit. DETAILED DESCRIPTION

[0068] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0069] Example 1

[0070] See also Figure 1 The present invention provides a modeling system for a finite element model of a steel structure weld, comprising a model building module 1, an identification and extraction module 2, a welding mid-term monitoring module 3, a welding quality monitoring module 4, and an evaluation generation module 5;

[0071] The model building module 1 is used to collect ship weld information using visual inspection technology, and draw the geometric shape and connection parts of the ship weld through CAD, establish a three-dimensional ship steel structure weld model, and generate a grid in the three-dimensional ship steel structure weld model to analyze the weld area;

[0072] The identification and extraction module 2 is used to identify the weld shape and classify the welds with the same shape to obtain an I-shaped weld area, a V-shaped weld area and a U-shaped weld area, and perform a first classification mark in the three-dimensional ship steel structure weld model;

[0073] Collect the weld pool volume Tj, groove angle Pjd, groove depth Pkj and geometric characteristic index Jtz of each weld pool in the I-shaped weld area, the V-shaped weld area and the U-shaped weld area, construct a weld pool data set 201, and obtain the weld pool index Rz by calculation, and then perform a second classification mark on the value of the weld pool index Rz in the three-dimensional ship steel structure weld model;

[0074] The welding mid-term monitoring module 3 is used to collect various parameters of the I-shaped weld area, the V-shaped weld area and the U-shaped weld area during the welding process, and to construct a welding data set 301, and to calculate the welding evaluation index Hc using the welding data set 301;

[0075] The welding quality monitoring module 4 is used to collect quality data of the I-shaped weld area, the V-shaped weld area and the U-shaped weld area after welding, establish a quality data set 401, and extract the welding quality index Hz in the quality data set 401 to obtain the weld construction defect index QX;

[0076] The evaluation generation module 5 is used to evaluate the defect index QX. The evaluation unit 501 presets a threshold value X to evaluate the evaluation defect index QX, and sets the loading conditions of the steel structure welding area. The solution unit 503 is used to calculate the index of the entire welding area, and the analysis results and visualization charts are integrated into the analysis report, which is presented to the user through the generation unit 504 to help the user understand the analysis results and make corresponding decisions.

[0077] In this embodiment, the ship weld information is collected based on the visual inspection technology, and the geometric shape and connection parts of the ship weld are drawn using CAD, and then a three-dimensional ship steel structure weld model is established, and the three-dimensional model is gridded at the same time, so as to facilitate the subsequent analysis of the weld area; by identifying the weld shape, the weld is classified, marked and analyzed; in the weld areas of different shapes, the four parameters of the weld pool volume Tj, groove angle Pjd, groove depth Pkj and geometric characteristic index Jtz of each weld are collected to construct the weld pool data set 201 to serve as a basis for the subsequent welding quality evaluation; in the welding process, the welding data is collected and constructed Data set 301 is collected, and the welding evaluation index Hc is calculated. The welding quality is monitored in real time through the welding evaluation index Hc, the welding quality is quantified, and problems are found and measures are taken in time. After welding is completed, the quality data of the welding area is collected, the quality data set 401 is established, and the welding quality index Hz is extracted to evaluate the construction quality and defects of the weld. According to the evaluation defect index QX, the loading conditions of the welding area are set, and the indicators of the overall welding area are calculated using the solution unit. Finally, the analysis results and visual charts are integrated into the analysis report and presented to the user through the generation unit to help the user understand the analysis results and make corresponding decisions.

[0078] Example 2

[0079] See also Figure 1 The model building module 1 includes a visual inspection unit 101, a drawing unit 102, a material setting unit 103 and a grid generation unit 104. The visual inspection unit 101 is used to scan the ship steel structure to obtain the geometric shape and connection part information of the weld; then, the CAD software in the drawing unit 102 is used to accurately draw the data obtained by the visual inspection unit 101 into a geometric model; finally, the material setting unit 103 is used to set the material parameters; and the grid generation unit 104 is used to automatically grid the welding connection part.

[0080] The I-shaped weld area, the V-shaped weld area and the U-shaped weld area correspond to different welding processes and structural requirements, respectively, and the weld areas of different shapes are distinguished by the first classification mark;

[0081] The second classification mark shows the quality and structural characteristics of each weld area, and the weld pool volume Tj is the volume of the molten pool formed by the molten metal during the welding process;

[0082] The groove angle Pkj refers to the angle formed on both sides of the weld joint after notching;

[0083] The groove depth Pks is the distance from the workpiece surface to the bottom of the groove before welding;

[0084] The geometric characteristic index Jtz includes: weld length Hfc, weld width Hfk, weld depth Hfs and weld cross area Hfj.

[0085] The weld pool volume Tj and groove depth PkJ are measured by a three-dimensional laser scanner to perform high-precision three-dimensional scanning on the weld surface, thereby obtaining the weld volume and groove depth;

[0086] During welding, the weld is filled with molten metal, so the volume of the weld is equal to the weld pool volume Tj as the volume of the molten metal pool;

[0087] The weld length Hfc, weld width Hfk and weld depth Hfs are measured by taking a digital image of the weld surface through a digital image processing system and then combining image processing technology;

[0088] The weld intersection area Hfj is obtained by scanning and measuring the cross section of the weld using a cross section scanner to obtain the intersection area of ​​the weld cross section and the substrate.

[0089] In this embodiment, the model building module 1 uses visual inspection technology to scan the ship steel structure to obtain the geometric shape and connection information of the weld, providing high-precision data while providing accurate basic information for subsequent modeling. The drawing unit 102 draws a geometric model based on the data obtained by the visual inspection unit 101 to ensure the accuracy and consistency of the shape of the weld and the connection during the modeling process; when building the model, it is necessary to consider the characteristics of the material used, so the material setting unit 103 is used to set the parameters of the material, because the properties of the material will directly affect the thermodynamic behavior during the welding process; the welding connection needs to be meshed for finite element analysis, and the mesh generation unit 104 is responsible for automatically meshing the welding connection to ensure that the details and complexity of the model are accurately reflected in the finite element analysis; the purpose of extracting the characteristic index is to evaluate the welding quality and detect potential defects.

[0090] Example 3

[0091] The geometric characteristic index Jtz is obtained by extracting the weld length Hfc, weld width Hfk, weld depth Hfs and weld cross area Hfj of each weld, performing dimensionless processing, and calculating the geometric characteristic index Jtz by the following formula:

[0092]

[0093] Where n is the number of welds; Hfc i is the length of the ith weld; Hfk i is the width of the ith weld; Hfs i is the depth of the ith weld; Hfj i is the cross-sectional area of ​​the ith weld; w i is the weight of the ith weld feature, and A is represented as the first correction constant;

[0094] The weld pool index Rz is obtained by the following calculation formula:

[0095]

[0096] Wherein, q1, q2, q3 and q4 represent the weight values ​​of the weld pool volume Tj, groove depth Pks, groove angle Pkj and geometric characteristic index Jtz, respectively, and the weld pool volume Tj, groove depth Pks, groove angle Pkj and geometric characteristic index Jtz are all dimensionless, and B is the second correction constant.

[0097] The welding evaluation index Hc includes: welding current Hdl, welding voltage Hdy, welding speed Hsd, shielding gas flow rate Bql and welding temperature Hwd;

[0098] The welding current Hdl and the welding voltage Hdy are measured by a voltmeter of an arc welding device;

[0099] The welding speed Hsd is measured by the encoder;

[0100] The shielding gas flow rate Bql is monitored by a gas flow meter;

[0101] The welding temperature Hwd is monitored by an infrared thermal imager;

[0102] After dimensionless processing of welding current Hdl, welding voltage Hdy, welding speed Hsd, shielding gas flow rate Bql and welding temperature Hwd, the welding evaluation index Hc is calculated by the following formula:

[0103] ;

[0104] Wherein, Bz represents the preset flow rate threshold for the I-shaped weld area, the V-shaped weld area and the U-shaped weld area, and Bz has different preset flow rate thresholds according to the I-shaped weld area, the V-shaped weld area and the U-shaped weld area, and can be adjusted by the user. is a sigmoid function with a value range of [0,1]. w1, w2, w3, w4 and w5 represent the weight values ​​of welding current Hdl, welding voltage Hdy, welding speed Hsd, shielding gas flow rate Bql and welding temperature Hwd respectively. C represents the third correction constant.

[0105] The welding quality index Hz includes heat influence index Ryx, welding penetration Hrs and residual stress Cyl;

[0106] The heat impact index Ryx is obtained by monitoring with a thermal simulation instrument;

[0107] The welding penetration gap density value Hrs is obtained by analyzing and evaluating the weld through X-ray diffraction analysis. The density value of the welding penetration gap indicates the degree of fusion between the material in the weld and the inner surface of the weld structure. The greater the degree of fusion, the greater the gap density value, which reduces the sealing performance of the weld. The smaller the degree of fusion, the smaller the gap density value, which improves the sealing performance of the weld, showing a positive and negative proportional relationship.

[0108] The residual stress Cyl is obtained by measuring with an electron diffractometer;

[0109] After the heat influence index Ryx, welding penetration Hrs and residual stress Cyl are dimensionless The welding quality index Hz is calculated by the following formula:

[0110]

[0111] Wherein, e1, e2 and e3 represent the weight values ​​of heat influence index Ryx, welding penetration Hrs and residual stress Cyl respectively, 3 represents the total number of parameters, and D represents the fourth correction constant.

[0112] After the weld pool index Rz, welding evaluation index Hc, and welding quality index Hz are dimensionlessly processed, the defect index QX is calculated using the following formula:

[0113]

[0114] In the formula, wi represents the weight coefficient and 3 represents the total number of parameters.

[0115] In this embodiment, the welding current Hdl is measured by the ammeter of the welding equipment. The welding current Hdl refers to the current transmitted through the welding rod, welding wire and electrode during the arc welding process, and the magnitude of the welding current affects the penetration and fusion of the weld, and directly affects the quality of the weld; the welding voltage Hdy is measured by the voltmeter of the welding equipment. The welding voltage indicates the magnitude of the voltage during the arc welding process, and together with the welding current determines the electric power during the welding process, and directly affects the heat input and molten pool formation during the welding process; the welding speed Hsd refers to the speed at which the welding arc moves along the weld during the welding process. The speed of the welding speed affects the cooling speed of the welding molten pool and the formation of the weld. The welding speed is measured by the encoder on the welding equipment; the shielding gas flow rate Bql refers to the flow rate of the shielding gas used in the welding process. The shielding gas is used to protect the welding area from the influence of oxygen and other impurities in the atmosphere. The shielding gas flow rate is measured by the gas flow meter on the welding equipment; the welding temperature Hwd refers to the temperature of the welding area during the welding process, which reflects the heat input and heat distribution of the welding area during the welding process. The welding temperature is measured by an infrared thermal imager. The defect index QX comprehensively considers the influence of the weld pool index Rz, the welding evaluation index Hc, and the welding quality index Hz, and is used to finally evaluate the defects of steel structure welding.

[0116] Example 4

[0117] The evaluation unit 501 performs evaluation by using the preset threshold value X and the defect index QX to obtain the following solution:

[0118] If the preset threshold value X>defect index QX, it means that the current ship steel structure welding is qualified, there are no weld cracks, lack of fusion, and pores, and there is no need to adjust the welding plan;

[0119] If the preset threshold value X is less than the defect index QX, it means that the welding of the current ship steel structure is unqualified, and problems such as weld cracks, lack of fusion, and pores occur, and the welding plan should be adjusted;

[0120] When the welding of the ship steel structure is unqualified, the weld pool index Rz, welding evaluation index Hc and welding quality index Hz are compared to obtain the defect points of the ship steel structure and make targeted adjustments to the welding plan.

[0121] The evaluation generation module 5 uses the condition setting unit 502 to set loading conditions for the welding area of ​​the steel structure, and sets the loading conditions according to the weld pool data set 201, the welding data set 301 and the quality data set 401; the generation unit 504 presents the analysis report to the user through an interactive interface.

[0122] In this embodiment, when the welding of the ship steel structure is unqualified, the evaluation generation module 5 will further analyze the weld pool index Rz, the welding evaluation index Hc and the welding quality index Hz, and quickly determine the specific defects of the ship steel structure by comparing these indices, such as poor quality of the weld pool and incorrect welding parameters. According to the defects, the evaluation generation module puts forward targeted welding scheme adjustment suggestions to solve the problems arising in the welding process and improve the welding quality. The evaluation generation module 5 is based on the weld pool data set 201, the welding data set 301 and the quality data set 401. The generation unit presents the analysis report to the user through an interactive interface, so that the user can clearly understand the evaluation results and the recommended welding scheme adjustments.

[0123] Example 5

[0124] A modeling method for finite element model of steel structure welds, see Figure 2 , including the following steps:

[0125] Step 1, the model building module 1 collects ship weld information by using visual inspection technology, draws the geometric shape and connection parts of the ship weld by CAD, builds a three-dimensional ship steel structure weld model, and generates a grid in the three-dimensional ship steel structure weld model to analyze the weld area;

[0126] Step 2, identification and extraction module 2, by identifying the weld shape and classifying the welds with the same shape, obtains I-shaped weld area, V-shaped weld area and U-shaped weld area, and performs the first classification mark in the three-dimensional ship steel structure weld model;

[0127] Collect the weld pool volume Tj, groove angle Pjd, groove depth Pkj and geometric characteristic index Jtz of each weld pool in the I-shaped weld area, the V-shaped weld area and the U-shaped weld area, construct a weld pool data set 201, and obtain the weld pool index Rz by calculation, and then perform a second classification mark on the value of the weld pool index Rz in the three-dimensional ship steel structure weld model;

[0128] Step 3, the welding mid-term monitoring module 3 collects various parameters of the I-shaped weld area, the V-shaped weld area and the U-shaped weld area during the welding process, and constructs a welding data set 301, and calculates the welding evaluation index Hc using the welding data set 301;

[0129] Step 4, the welding quality monitoring module 4, by collecting the quality data of the I-shaped weld area, the V-shaped weld area and the U-shaped weld area after welding, establishes a quality data set 401, and extracts the welding quality index Hz in the quality data set 401 to obtain the weld construction defect index QX;

[0130] Step 5, the evaluation generation module 5 evaluates the evaluation defect index QX, sets the loading conditions of the steel structure welding area, and then uses the solution unit 503 to calculate the indicators of the overall welding area. The analysis results and visualization charts are then integrated into the analysis report, which is presented to the user through the generation unit 504 to help the user understand the analysis results and make corresponding decisions.

[0131] In this embodiment, the information of the ship's welds is collected through step one, the welds are scanned and photographed using a digital camera, the collected data is processed and drawn using CAD software, a three-dimensional ship steel structure weld model is established, and a grid is generated in the three-dimensional model to analyze the weld area.

[0132] Through steps 2 to 4, welds of different shapes are identified and classified and marked, and relevant parameters of each shape of weld area are collected to construct a weld pool dataset 201, a welding dataset 301 and a quality dataset 401, which are used to calculate and evaluate the quality of welds and provide data support for the subsequent identification of defects in ship steel structure welds.

[0133] Through step five, the defect index QX of the weld is evaluated, and the loading conditions are set. The analysis results and visual charts are integrated into the analysis report and presented to the user through an interactive interface to help the user understand the analysis results and make corresponding decisions.

[0134] Although embodiments of the present invention have been shown and described, it will be appreciated by those skilled in the art that various changes, modifications, substitutions and variations may be made to the embodiments without departing from the principles and spirit of the present invention, and that the scope of the present invention is defined by the appended claims and their equivalents.

Claims

1. A modeling system for a finite element model of a steel structure weld, characterized by: It includes a model building module (1), an identification and extraction module (2), a welding mid-term monitoring module (3), a welding quality monitoring module (4), and an evaluation generation module (5); The model building module (1) is used to collect ship weld information using visual inspection technology, and draw the geometric shape and connection position of the ship weld through CAD, establish a three-dimensional ship steel structure weld model, and generate a grid in the three-dimensional ship steel structure weld model to analyze the weld area; The identification and extraction module (2) is used to identify the weld shape and classify welds with the same shape to obtain an I-shaped weld area, a V-shaped weld area and a U-shaped weld area, and to perform a first classification mark in the three-dimensional ship steel structure weld model; The molten pool volume Tj, groove angle Pjd, groove depth Pks and geometric characteristic index Jtz of each weld in the I-shaped weld area, the V-shaped weld area and the U-shaped weld area are collected to construct a molten pool data set (201) for the weld to be welded, and the molten pool index Rz of the weld to be welded is obtained by calculation, and then the value of the molten pool index Rz of the weld to be welded is marked as a second classification in the three-dimensional ship steel structure weld model; The welding mid-term monitoring module (3) is used to collect various parameters of the I-shaped weld area, the V-shaped weld area and the U-shaped weld area during the welding process, and to construct a welding data set (301), and to calculate a welding evaluation index Hc using the welding data set (301); The welding quality monitoring module (4) is used to collect quality data of an I-shaped weld area, a V-shaped weld area and a U-shaped weld area after welding is completed, establish a quality data set (401), calculate a welding quality index Hz using the quality data set (401), and obtain a weld construction defect index QX; The evaluation generation module (5) is used to evaluate the defect index QX, using the evaluation unit (501) to preset a threshold value X to evaluate the evaluation defect index QX, and setting the loading conditions of the steel structure welding area, and then using the solution unit (503) to calculate the index of the entire welding area, and then integrating the analysis results and the visual chart into the analysis report, and presenting it to the user through the generation unit (504) to help the user understand the analysis results and make corresponding decisions; The I-shaped weld area, the V-shaped weld area and the U-shaped weld area correspond to different welding processes and structural requirements, respectively, and the weld areas of different shapes are distinguished by the first classification mark; The second classification mark shows the quality and structural characteristics of each weld area, and the weld pool volume Tj is the volume of the molten pool formed by the molten metal during the welding process; The groove angle Pkj refers to the angle formed on both sides of the weld joint after notching; The groove depth Pks is the distance from the workpiece surface to the bottom of the groove before welding; The geometric characteristic index Jtz includes: weld length Hfc, weld width Hfk, weld depth Hfs and weld cross area Hfj; The weld pool volume Tj and groove depth Pks are measured by a three-dimensional laser scanner to perform high-precision three-dimensional scanning on the weld surface, thereby obtaining the weld volume and groove depth; During welding, the weld is filled with molten metal, so the volume of the weld is equal to the weld pool volume Tj as the volume of the molten metal pool; The weld length Hfc, weld width Hfk and weld depth Hfs are measured by taking a digital image of the weld surface through a digital image processing system and then combining image processing technology; The weld cross section area Hfj is scanned and measured by a cross section scanner to obtain the cross section area of ​​the weld and the substrate; The geometric characteristic index Jtz is obtained by extracting the weld length Hfc, weld width Hfk, weld depth Hfs and weld cross area Hfj of each weld, performing dimensionless processing, and calculating the geometric characteristic index Jtz by the following formula: Where n is the number of welds; Hfc i is the length of the ith weld; Hfk i is the width of the ith weld; Hfs i is the depth of the ith weld; Hfj i is the cross-sectional area of ​​the ith weld; w i is the weight of the ith weld feature, and A is represented as the first correction constant; The weld pool index Rz is obtained by the following calculation formula: Wherein, q1, q2, q3 and q4 represent the weight values ​​of weld pool volume Tj, groove depth Pks, groove angle Pkj and geometric characteristic index Jtz, respectively, and weld pool volume Tj, groove depth Pks, groove angle Pkj and geometric characteristic index Jtz are all dimensionless, and B is the second correction constant; The welding evaluation index Hc includes: welding current Hdl, welding voltage Hdy, welding speed Hsd, shielding gas flow rate Bql and welding temperature Hwd; The welding current Hdl and the welding voltage Hdy are measured by a voltmeter of an arc welding device; The welding speed Hsd is measured by the encoder; The shielding gas flow rate Bql is monitored by a gas flow meter; The welding temperature Hwd is monitored by an infrared thermal imager; After dimensionless processing of welding current Hdl, welding voltage Hdy, welding speed Hsd, shielding gas flow rate Bql and welding temperature Hwd, the welding evaluation index Hc is calculated by the following formula: ; Wherein, Bz represents the preset flow rate threshold for the I-shaped weld area, the V-shaped weld area and the U-shaped weld area, and Bz has different preset flow rate thresholds according to the I-shaped weld area, the V-shaped weld area and the U-shaped weld area, and can be adjusted by the user. is a sigmoid function with a value range of [0,1]. w1, w2, w3, w4 and w5 represent the weight values ​​of welding current Hdl, welding voltage Hdy, welding speed Hsd, shielding gas flow rate Bql and welding temperature Hwd respectively. C represents the third correction constant. The welding penetration gap density value Hrs is obtained by analyzing and evaluating the weld through X-ray diffraction analysis. The density value of the welding penetration gap indicates the degree of fusion between the material in the weld and the inner surface of the weld structure. The greater the degree of fusion, the greater the gap density value, which reduces the sealing performance of the weld. The smaller the degree of fusion, the smaller the gap density value, which is in direct and inverse proportion. The residual stress Cyl is obtained by measuring with an electron diffractometer; After dimensionless processing of the heat influence index Ryx, the welding penetration gap density value Hrs and the residual stress Cyl, the welding quality index Hz is calculated by the following formula: Wherein, e1, e2 and e3 represent the weight values ​​of heat influence index Ryx, welding penetration gap density value Hrs and residual stress Cyl respectively, 3 represents the total number of parameters, and D represents the fourth correction constant; the heat influence index Ryx is obtained by monitoring through a thermal simulation instrument; After the weld pool index Rz, welding evaluation index Hc, and welding quality index Hz are dimensionlessly processed, the defect index QX is calculated using the following formula: In the formula, w i represents the weight coefficient and 3 represents the total number of parameters.

2. The modeling system of a steel structure weld finite element model according to claim 1, characterized in that: The model building module (1) comprises a visual inspection unit (101), a drawing unit (102), a material setting unit (103) and a mesh generation unit (104). The visual inspection unit (101) is used to scan the ship steel structure to obtain the geometric shape of the weld and the connection part information; then, the CAD software in the drawing unit (102) is used to accurately draw the data obtained by the visual inspection unit (101) into a geometric model; finally, the material setting unit (103) is used to set the material parameters; and the mesh generation unit (104) is used to automatically mesh the weld connection part.

3. The modeling system of a steel structure weld finite element model according to claim 2, characterized in that: The evaluation unit (501) performs evaluation by using a preset threshold value X and a defect index QX to obtain the following solution: If the preset threshold value X>defect index QX, it means that the current ship steel structure welding is qualified, there are no weld cracks, lack of fusion, and pores, and there is no need to adjust the welding plan; If the preset threshold value X is less than the defect index QX, it means that the welding of the current ship steel structure is unqualified, and problems such as weld cracks, lack of fusion, and pores occur, and the welding plan should be adjusted; When the welding of the ship steel structure is unqualified, the weld pool index Rz, welding evaluation index Hc and welding quality index Hz are compared to obtain the defect points of the ship steel structure and make targeted adjustments to the welding plan.

4. The modeling system of a steel structure weld finite element model according to claim 3, characterized in that: The evaluation generation module (5) uses a condition setting unit (502) to set loading conditions for the welding area of ​​the steel structure, and sets the loading conditions according to the weld pool data set (201), the welding data set (301) and the quality data set (401); the generation unit (504) presents the analysis report to the user through an interactive interface.

5. A modeling method of a modeling system for a steel structure weld finite element model according to any one of claims 1 to 4, characterized in that: The following steps are involved: Step 1, the model building module (1) collects ship weld information by using visual inspection technology, draws the geometric shape and connection parts of the ship weld by CAD, builds a three-dimensional ship steel structure weld model, and generates a grid in the three-dimensional ship steel structure weld model to analyze the weld area; Step 2, an identification and extraction module (2), which identifies the weld shape and classifies welds with the same shape to obtain an I-shaped weld area, a V-shaped weld area, and a U-shaped weld area, and performs a first classification mark in the three-dimensional ship steel structure weld model; The molten pool volume Tj, groove angle Pjd, groove depth Pks and geometric characteristic index Jtz of each weld in the I-shaped weld area, the V-shaped weld area and the U-shaped weld area are collected to construct a molten pool data set (201) for the weld to be welded, and the molten pool index Rz of the weld to be welded is obtained by calculation, and then the value of the molten pool index Rz of the weld to be welded is marked as a second classification in the three-dimensional ship steel structure weld model; Step 3, a welding mid-term monitoring module (3), which collects various parameters of the I-shaped weld area, the V-shaped weld area, and the U-shaped weld area during the welding process, and constructs a welding data set (301), and calculates a welding evaluation index Hc using the welding data set (301); Step 4, a welding quality monitoring module (4), by collecting quality data of an I-shaped weld area, a V-shaped weld area, and a U-shaped weld area after welding, establishes a quality data set (401), calculates a welding quality index Hz using the quality data set (401), and obtains a weld construction defect index QX; Step 5, the evaluation generation module (5) evaluates the evaluation defect index QX and sets the loading conditions of the steel structure welding area, and then uses the solution unit (503) to calculate the indicators of the entire welding area, and then integrates the analysis results and visualization charts into the analysis report, which is presented to the user through the generation unit (504) to help the user understand the analysis results and make corresponding decisions.