A method and device for determining the crystallization interface of crystals grown by guided mode method
By using the parallel calculation of the main thread and sub-thread to adjust the crystallization interface during the growth of gallium oxide crystal by the guided mode method, the problem of difficulty in obtaining the crystallization interface is solved, and the crystal quality and the control accuracy of the growth process are improved.
Patent Information
- Application Number
- CN202411074055.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-07
- Publication Date
- 2024-10-18
- Estimated Expiration
- 2044-08-07
AI Technical Summary
In the process of growing gallium oxide crystals by the guided mode method, it is difficult to obtain the crystalline interface, making it difficult to control the crystal growth process, resulting in vacancies and dislocation defects often appearing inside the crystal.
By performing steady-state calculations in the target calculation domain, determine whether the temperature of the three-dimensional non-axisymmetric crystallization interface meets the preset conditions, and use the main thread and sub-threads to perform parallel calculations, adjust the target grid nodes to achieve temperature balance, and determine and optimize crystallization interface.
It achieves accurate crystallization interface determination of gallium oxide crystals, improves the control accuracy of crystal quality and growth process, and reduces the generation of vacancies and dislocation defects.
Smart Images

Figure CN118581565B_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of crystal growth, and in particular to a method and device for determining a crystal interface of a crystal grown by a guided mode method. Background Art
[0002] Gallium oxide (Ga2O3) crystals have a high bandgap (4.9eV) and good conductivity, luminescence, electronics, optics and thermal properties. They are widely used in laser devices, accelerators and radar systems, sensors, visual image sensors, deformable mirrors, video lens controllers and high-performance imaging systems.
[0003] Since the melting point of gallium oxide crystals is relatively high (1800°C), the growth of plate-shaped Ga2O3 crystals is currently mainly carried out by the guided mold method in a crystal growth furnace above 2000°C. Specifically, the gallium oxide melt is placed in a crucible fixed with a mold, and a capillary slit is provided in the middle of the mold. The gallium oxide melt can rise to the top of the mold by capillary action, forming a thin film and diffusing around, and crystallizing into Ga2O3 crystals induced by the seed crystal.
[0004] However, during the growth process of Ga2O3 crystals, defects such as vacancies and dislocations often appear inside the crystals, seriously affecting the quality of the crystals. Most of these defects are caused by the concave crystal interface caused by unreasonable heat and mass transfer conditions in the crystal growth furnace. Since the furnace temperature for growing Ga2O3 crystals is relatively high, it is usually difficult to directly obtain the specific conditions of the crystal interface during the crystal growth process through actual measurement methods such as experiments, and thus it is impossible to control the growth process of Ga2O3 crystals based on the crystal interface. Summary of the invention
[0005] The embodiments of the present invention provide a method and device for determining the crystallization interface of crystals grown by the guided mold method, which can solve the problem in the related art that it is difficult to control the growth process of the crystal due to the difficulty in obtaining the crystallization interface during the process of growing crystals by the guided mold method.
[0006] In a first aspect, an embodiment of the present invention provides a method for determining a crystallization interface of a crystal grown by a guided mode method, which is applied to an electronic device, wherein the electronic device includes a main thread and at least two sub-threads controlled by the main thread; the method includes:
[0007] In the case of temperature imbalance in the target computational domain, a steady-state calculation is performed on the target computational domain to obtain a temperature field of the target computational domain; the target computational domain is a computational domain obtained by meshing a target geometric model, the target geometric model comprising a three-dimensional non-axisymmetric crystallization interface between a target crystal grown by a guided mode method and a melt corresponding to the target crystal; the target computational domain comprises at least two target mesh surfaces constituting the three-dimensional non-axisymmetric crystallization interface, and each of the subthreads corresponds to at least one of the target mesh surfaces;
[0008] According to the temperature field, determining whether the temperature of the three-dimensional non-axisymmetric crystallization interface meets a preset condition, and when the temperature of the three-dimensional non-axisymmetric crystallization interface does not meet the preset condition, using the main thread to obtain the calculation parameters of the three-dimensional non-axisymmetric crystallization interface; the preset condition is that the temperature of the three-dimensional non-axisymmetric crystallization interface is uniform and reaches the crystal solidification temperature of the target crystal;
[0009] The main thread is used to send the calculation parameters to each of the sub-threads, and the sub-threads are used to calculate the movement parameters of the target grid nodes in the target grid surface corresponding to the sub-threads according to the calculation parameters; the target grid nodes in the target grid surface corresponding to each of the sub-threads are different from each other;
[0010] According to the movement parameters of each of the target grid nodes, the target grid nodes are controlled to move to obtain an adjusted three-dimensional non-axisymmetric crystallization interface;
[0011] When the temperature of the target calculation domain is balanced and the temperature of the three-dimensional non-axisymmetric crystallization interface meets the preset condition, the three-dimensional non-axisymmetric crystallization interface is determined as the target crystallization interface.
[0012] In a second aspect, an embodiment of the present invention provides a device for determining a crystallization interface of a crystal grown by a guided mode method, which is applied to an electronic device, wherein the electronic device comprises a main thread and at least two sub-threads controlled by the main thread; the device comprises:
[0013] A first calculation module is used to perform steady-state calculation on the target calculation domain to obtain the temperature field of the target calculation domain when the temperature of the target calculation domain is unbalanced; the target calculation domain is a calculation domain obtained after meshing the target geometric model, and the target geometric model includes a three-dimensional non-axisymmetric crystallization interface between a target crystal grown by a guided mode method and a melt corresponding to the target crystal; the target calculation domain includes at least two target mesh surfaces constituting the three-dimensional non-axisymmetric crystallization interface, and each of the sub-threads corresponds to at least one of the target mesh surfaces;
[0014] A first determination module is used to determine whether the temperature of the three-dimensional non-axisymmetric crystallization interface meets a preset condition according to the temperature field, and to obtain calculation parameters of the three-dimensional non-axisymmetric crystallization interface using the main thread when the temperature of the three-dimensional non-axisymmetric crystallization interface does not meet the preset condition; the preset condition is that the temperature of the three-dimensional non-axisymmetric crystallization interface is uniform and reaches the crystal solidification temperature of the target crystal;
[0015] A second calculation module is used to send the calculation parameters to each of the sub-threads by using the main thread, and calculate the movement parameters of the target grid nodes in the target grid surface corresponding to the sub-thread according to the calculation parameters by using the sub-thread; the target grid nodes in the target grid surface corresponding to each of the sub-threads are different from each other;
[0016] A control module, used for controlling the target grid nodes to move according to the movement parameters of each target grid node, so as to obtain an adjusted three-dimensional non-axisymmetric crystallization interface;
[0017] The second determination module is used to determine the three-dimensional non-axisymmetric crystallization interface as a target crystallization interface when the temperature of the target calculation domain is balanced and the temperature of the three-dimensional non-axisymmetric crystallization interface meets the preset condition.
[0018] In a third aspect, an embodiment of the present invention provides an electronic device, comprising: a memory and a processor, wherein the memory is used to store a computer program, and the processor is used to implement the method for determining the crystallization interface of a crystal grown by a guided mode method as described in any one of the above items when executing the computer program.
[0019] In a fourth aspect, an embodiment of the present invention provides a readable storage medium, wherein the readable storage medium stores a computer program, and when the computer program is executed by a processor, the method for determining the crystallization interface of a crystal grown by a guided mode method as described in any one of the above items is implemented.
[0020] According to the method for determining the crystallization interface of crystals grown by the guided mode method provided in an embodiment of the present invention, when the temperature of a target calculation domain is unbalanced, the electronic device first performs steady-state calculation on the target calculation domain to obtain the temperature field of the target calculation domain, and then determines whether the temperature of the three-dimensional non-axisymmetric crystallization interface meets a preset condition according to the temperature field of the target calculation domain; when the temperature of the three-dimensional non-axisymmetric crystallization interface is uneven and / or does not reach the crystal solidification temperature of the target crystal, indicating that the currently determined three-dimensional non-axisymmetric crystallization interface is not the actual three-dimensional non-axisymmetric crystallization interface between the target crystal and the melt corresponding to the target crystal, the main thread is used to obtain the calculation parameters of the currently determined three-dimensional non-axisymmetric crystallization interface, and the calculation parameters are sent to each sub-thread, and the sub-thread is used to parallelly calculate the movement parameters of the target grid nodes in the target grid surface corresponding to the sub-thread according to the calculation parameters; finally, according to the movement parameters of each target grid node, The target grid nodes are controlled to move to obtain an adjusted three-dimensional non-axisymmetric crystallization interface until the temperature of the target calculation domain is balanced and the temperature of the three-dimensional non-axisymmetric crystallization interface meets the preset conditions, indicating that the currently determined three-dimensional non-axisymmetric crystallization interface is the actual three-dimensional non-axisymmetric crystallization interface between the target crystal and the melt corresponding to the target crystal, and the three-dimensional non-axisymmetric crystallization interface can be determined as the target crystallization interface; the embodiment of the present invention not only realizes the determination of the target crystallization interface, that is, the actual three-dimensional non-axisymmetric crystallization interface between the target crystal and the melt corresponding to the target crystal, but also utilizes the main thread in the electronic device and at least two sub-threads controlled by the main thread to obtain the target calculation parameters and parallelly calculate the movement parameters, thereby improving the efficiency of determining the target crystallization interface, improving the accuracy of controlling the growth process of the target crystal based on the target crystallization interface and the crystal quality of the target crystal grown by the guided mode method. BRIEF DESCRIPTION OF THE DRAWINGS
[0021] In order to more clearly illustrate the technical solutions of the embodiments of the present invention, the accompanying drawings required for use in the description of the embodiments of the present invention will be briefly introduced below. Obviously, the accompanying drawings in the following description are only some embodiments of the present invention. For ordinary technicians in this field, other accompanying drawings can be obtained based on these accompanying drawings without paying creative labor.
[0022] Figure 1 It is a flow chart of the steps of a method for determining a crystallization interface of a crystal grown by a guided mode method provided by an embodiment of the present invention;
[0023] Figure 2 is a schematic structural diagram of a target geometric model provided by an embodiment of the present invention;
[0024] Figure 3 is a schematic structural diagram of a liquid bridge provided by an embodiment of the present invention;
[0025] Figure 4 is a schematic structural diagram of a three-dimensional non-axisymmetric crystallization interface provided by an embodiment of the present invention;
[0026] Figure 5 is a schematic diagram of allocation of a target grid surface provided by an embodiment of the present invention;
[0027] Figure 6 is a schematic diagram of the structure of an electronic device provided by an embodiment of the present invention;
[0028] Figure 7 is a schematic structural diagram of another electronic device provided by an embodiment of the present invention;
[0029] Figure 8 It is a flowchart of the steps of another method for determining the crystallization interface of a crystal grown by a guided mode method provided by an embodiment of the present invention;
[0030] Fig. 9 It is a logic block diagram of a crystallization interface determination device for crystals grown by a guided mode method provided by an embodiment of the present invention;
[0031] Reference numerals:
[0032] 10-crystal growth furnace; 101-crucible; 102-induction coil; 103-mold; 1031-capillary slit; 20-target crystal; 30-liquid bridge; 40-melt. DETAILED DESCRIPTION
[0033] In order to make the above-mentioned purposes, features and advantages of the present invention more obvious and easy to understand, the technical solutions in the embodiments of the present invention will be clearly and completely described below in conjunction with the drawings in the embodiments of the present invention. Obviously, the described embodiments are part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0034] Method Embodiment
[0035] Reference Figure 1 , shows a flow chart of the steps of a method for determining a crystallization interface of a crystal grown by a guided mode method of the present invention, wherein the method may specifically include the following steps S101 to S105:
[0036] The method for determining the crystallization interface of a crystal grown by a guided mode method provided in an embodiment of the present invention can be applied to an electronic device, which includes a main thread and at least two sub-threads controlled by the main thread, and a communication connection is established between the main thread and the sub-threads.
[0037] Among them, the main thread is used to obtain the calculation parameters of the three-dimensional non-axisymmetric crystallization interface through the following step S102, and control each sub-thread based on the communication connection between each sub-thread; the sub-thread is used to receive the calculation parameters sent by the main thread, and calculate the movement parameters of each target grid node in the target grid surface corresponding to the sub-thread according to the calculation parameters.
[0038] Step S101 : When the temperature of a target calculation domain is unbalanced, a steady-state calculation is performed on the target calculation domain to obtain a temperature field of the target calculation domain.
[0039] Among them, the target computational domain is the computational domain obtained after meshing the target geometric model, and the target geometric model includes a three-dimensional non-axisymmetric crystallization interface between a target crystal grown by the guided mode method and a melt corresponding to the target crystal; the target computational domain includes at least two target mesh surfaces constituting the three-dimensional non-axisymmetric crystallization interface, and each sub-thread corresponds to at least one target mesh surface.
[0040] The crystallization interface of the crystal grown by the guided mode method in the embodiment of the present invention is the solid-liquid interface between the melt corresponding to the target crystal and the target crystal in the crystal growth furnace, that is, the three-dimensional non-axisymmetric crystallization interface. The target geometric model is a three-dimensional geometric model including the three-dimensional non-axisymmetric crystallization interface.
[0041] Reference Figure 2 , shows a schematic structural diagram of a target geometric model of the present invention; the target geometric model includes a crystal growth furnace 10, a target crystal 20 grown by the crystal growth furnace 10, and a melt 40 corresponding to the target crystal 20; wherein the crystal growth furnace 10 includes a crucible 101, a mold 103, and an induction coil 102. The induction coil 102 is a spiral induction coil, which is arranged on the outer wall of the crucible 101. When current is passed into the induction coil 102, the induction coil 102 induction heats the crucible 101, and the power of the induction coil 102 induction heating the crucible 101 can be controlled by controlling the magnitude of the current passed into the induction coil 102; the melt 40 corresponding to the target crystal 20 is contained in the crucible 101, and a capillary slit 1031 is provided in the mold 103, so that the melt 40 corresponding to the target crystal 20 in the crucible 101 can rise to the top of the mold 103 by capillary action, and form a thin film on the top and diffuse to the surroundings, thereby forming a liquid bridge 30 between the crystal growth furnace 10 and the target crystal 20, as shown in FIG. Figure 3 As shown, the upper surface of the liquid bridge 30 is the solid-liquid interface between the target crystal 20 and the melt 40 corresponding to the target crystal 20, and the solid-liquid interface is a three-dimensional non-axisymmetric crystallization interface.
[0042] Among them, the crystal growth furnace is a growth furnace that can realize the guided mold method to grow the target crystal, and the target crystal is a plate-like crystal grown by the guided mold method using the crystal growth furnace; the target crystal may include but is not limited to gallium oxide crystal, sapphire, synthetic ruby, yttrium aluminum garnet, etc.
[0043] It should be noted that, since it is difficult to obtain the specific shape of the three-dimensional non-axisymmetric crystallization interface during the growth of the target crystal 20, when the target geometric model is first established, it can be assumed that the three-dimensional non-axisymmetric crystallization interface in the target geometric model is as follows: Figure 2 The horizontal plane shown in the figure is adjusted continuously through the operations corresponding to steps S101 to S104, until the temperature of the target calculation domain is balanced and the temperature of the three-dimensional non-axisymmetric crystallization interface meets the preset conditions, and the three-dimensional non-axisymmetric crystallization interface is determined as the target crystallization interface.
[0044] It can be understood that the target crystallization interface is a crystallization interface that is identical to or similar to the actual three-dimensional non-axisymmetric crystallization interface between the target crystal and the melt corresponding to the target crystal, as determined by the crystallization interface determination method for crystals grown by the guided mold method provided in an embodiment of the present invention; in the process of growing the target crystal by the guided mold method, the growth process of the target crystal can be controlled according to the shape of the target crystal interface, thereby reducing or avoiding the generation of defects such as vacancies and dislocations, ensuring the stability of the target crystal growth process, and thereby improving the crystal quality of the target crystal grown by the guided mold method.
[0045] In the process of determining the target geometric model in the embodiment of the present invention, the electronic device can first obtain the positional relationship and size information between each component in the crystal growth furnace, the target crystal, and the melt corresponding to the target crystal; then establish a three-dimensional geometric model based on the positional relationship and size information to obtain the target geometric model.
[0046] After determining the target geometric model, the electronic device can mesh the target geometric model to obtain a target computational domain corresponding to the target geometric model; the target computational domain includes computational grids obtained after meshing the target geometric model; wherein the number of computational grids in the target computational domain is at least 2.
[0047] Reference Figure 4 , showing a schematic structural diagram of a three-dimensional non-axisymmetric crystallization interface of the present invention, such as Figure 4As shown, since the target geometric model includes a three-dimensional non-axisymmetric crystallization interface, the computational mesh in the target computational domain includes a target computational mesh where the three-dimensional non-axisymmetric crystallization interface is located, and the mesh surface where the three-dimensional non-axisymmetric crystallization interface is located in the target computational mesh is the target mesh surface, and the mesh nodes constituting the target mesh surface are the target mesh nodes. Among them, the number of target computational meshes is at least 2, and the number of target mesh surfaces constituting the three-dimensional non-axisymmetric crystallization interface is also at least 2.
[0048] Considering that each target mesh node in the target mesh surface needs to be moved in step S104, in order to accurately control the shape of the three-dimensional non-axisymmetric crystallization interface and ensure the deformation quality of the three-dimensional non-axisymmetric crystallization interface, in an embodiment of the present invention, in the process of meshing the target geometric model, the target computational mesh where the three-dimensional non-axisymmetric crystallization interface is located in the target geometric model can be divided into a hexahedral mesh, and the computational mesh outside the target computational mesh in the target geometric model can be divided into a tetrahedral mesh, and the interface between the hexahedral mesh and the tetrahedral mesh is a non-common node mesh interface (INTERFACE surface), and data between the computational grids is transferred through numerical difference technology.
[0049] In an embodiment of the present invention, considering that in actual application scenarios, the number of target grid surfaces is tens of thousands, the amount of calculation required to calculate the movement parameters of the target grid nodes in each target grid surface is too large, and the efficiency of the electronic device calculating the movement parameters of the target grid nodes in each target grid surface in sequence is extremely low; therefore, the target grid surfaces constituting the three-dimensional non-axisymmetric crystallization interface can be allocated to sub-threads in the electronic device, so that each sub-thread corresponds to at least one target grid surface, and the movement parameters of the target grid nodes in the target grid surfaces are calculated in parallel by using each sub-thread, which can improve the efficiency of calculating the movement parameters, thereby improving the efficiency of determining the target crystallization interface.
[0050] Reference Figure 5 , showing a schematic diagram of the allocation of a target grid surface of the present invention; the electronic device includes a sub-thread 1 and a sub-thread 2. In the process of allocating the target grid surface to the sub-thread, the electronic device can allocate the target grid surface according to the running status of the sub-thread 1 and the sub-thread 2. The corresponding relationship between the allocated target grid surface and the sub-thread is as follows: Figure 5 As shown; wherein, the running status of sub-thread 1 and sub-thread 2 may include but is not limited to the current idle state of the sub-thread, the computing power of the sub-thread, etc.
[0051] It can be understood that adjacent target grid surfaces include common target grid nodes. In the process of allocating target grid surfaces to sub-threads, when the adjacent target grid surfaces are divided into different sub-threads, the electronic device can divide the common target grid nodes in the adjacent target grid surfaces into a certain sub-thread according to the preset target grid node division rule, so that the target grid nodes in the target grid surfaces corresponding to each sub-thread are different from each other.
[0052] Exemplarily, the target grid node division rules may include but are not limited to: when the positional relationship between adjacent target grid surfaces is an up-and-down relationship, the common target grid nodes are divided into the sub-thread where the target grid surface located above the adjacent target grid surfaces is located; when the positional relationship between adjacent target grid surfaces is a left-and-right relationship, the common target grid nodes are divided into the sub-thread where the target grid surface located on the left of the adjacent target grid surfaces is located.
[0053] In an embodiment of the present invention, after determining the target computational domain and dividing the target grid surface in the target computational domain into various sub-threads in the electronic device, when the temperature of the target computational domain is unbalanced, the electronic device performs steady-state calculation on the target computational domain to obtain the temperature field of the target computational domain.
[0054] The temperature imbalance of the target calculation domain refers to the temperature of each region in the current temperature field of the target calculation domain not reaching a balanced state; in the case of temperature imbalance of the target calculation domain, it is necessary to recalculate the target calculation domain in a steady state to obtain a temperature field in which the temperature of each region reaches a balanced state. It can be understood that step S101 obtains that the temperature of each region in the temperature field of the target calculation domain reaches a balanced state.
[0055] It should be noted that scenarios that lead to temperature imbalance in the target computational domain may include but are not limited to: changes in the number of computational grids in the target computational domain, changes in the size of computational grids in the target computational domain, movement of grid nodes in the target computational domain (for example, controlling the movement of target grid nodes in step S104 to obtain an adjusted three-dimensional non-axisymmetric crystallization interface), changes in temperature in the target computational domain (for example, changes in the furnace temperature of a crystal growth furnace), etc.
[0056] Specifically, in this step, when the temperature of the target computing domain is unbalanced, the electronic device can first obtain the steady-state calculation parameters required for steady-state calculation of the target computing domain, and then perform steady-state calculation on the target computing domain based on the steady-state calculation parameters, thereby obtaining the temperature field of the target computing domain.
[0057] Among them, the steady-state calculation parameters may include but are not limited to the thermophysical characteristic parameters of each component in the target geometric model, the control equations corresponding to each calculation grid in the target calculation domain, and the boundary conditions and source terms of the target calculation domain. The control equation is a physical model determined according to the physical process involved in the crystal growth furnace and used to describe the physical process involved in the crystal growth furnace. The control equation may include but is not limited to: energy conservation equation, momentum conservation equation, radiation transfer equation, electromagnetic induction control equation, mass conservation equation and Young's equation (Young-Laplace equation).
[0058] It is understandable that, in the case of temperature balance in the target calculation domain, it indicates that the temperatures of various regions in the current temperature field of the target calculation domain are in a balanced state, and there is no need to perform step S101 for steady-state calculation. The electronic device can directly perform operations corresponding to steps S102 to S105 based on the temperature field in which the temperatures of various regions are in a balanced state.
[0059] Step S102: determine whether the temperature of the three-dimensional non-axisymmetric crystallization interface meets the preset conditions according to the temperature field, and when the temperature of the three-dimensional non-axisymmetric crystallization interface does not meet the preset conditions, use the main thread to obtain the calculation parameters of the three-dimensional non-axisymmetric crystallization interface.
[0060] The preset condition is that the temperature of the three-dimensional non-axisymmetric crystallization interface is uniform and reaches the crystal solidification temperature of the target crystal. For example, when the target crystal is a gallium oxide crystal, the crystal solidification temperature is 2080K (thermodynamic temperature scale, Kelvin).
[0061] Specifically, in the process of determining whether the temperature of the three-dimensional non-axisymmetric crystallization interface meets the preset conditions according to the temperature field, the electronic device first determines the area where the three-dimensional non-axisymmetric crystallization interface is located from the temperature field; then, obtains the temperature of the three-dimensional non-axisymmetric crystallization interface from the area where the three-dimensional non-axisymmetric crystallization interface is located in the temperature field; then, matches the temperature of the three-dimensional non-axisymmetric crystallization interface with the preset conditions; when the temperature of the three-dimensional non-axisymmetric crystallization interface reaches the crystal solidification temperature of the target crystal and the temperature is uniform, it indicates that the three-dimensional non-axisymmetric crystallization interface at this time is the actual three-dimensional between the target crystal and the melt corresponding to the target crystal. For a non-axisymmetric crystallization interface, step S105 can be executed to determine the three-dimensional non-axisymmetric crystallization interface as the target crystallization interface; when the temperature of the three-dimensional non-axisymmetric crystallization interface does not reach the crystal solidification temperature of the target crystal and / or the temperature of the three-dimensional non-axisymmetric crystallization interface is uneven, it indicates that the three-dimensional non-axisymmetric crystallization interface at this time is not the actual three-dimensional non-axisymmetric crystallization interface between the target crystal and the melt corresponding to the target crystal, then step S102 needs to be executed to use the main thread to obtain the calculation parameters of the three-dimensional non-axisymmetric crystallization interface, and steps S103 to S104 need to be executed to adjust the current three-dimensional non-axisymmetric crystallization interface.
[0062] In an embodiment of the present invention, when the temperature of the three-dimensional non-axisymmetric crystallization interface does not meet the preset conditions, the electronic device uses the main thread to obtain the calculation parameters of the three-dimensional non-axisymmetric crystallization interface as follows: first, the main thread is used to send calculation parameter acquisition instructions to each sub-thread, so that the sub-thread obtains the mesh surface parameters of each target mesh surface corresponding to the sub-thread based on the calculation parameter acquisition instruction, and sends the mesh surface parameters of each target mesh surface to the main thread; the main thread is used to receive the mesh surface parameters sent by each sub-thread, and then the mesh surface parameters of each mesh surface are summarized, and the summarized mesh surface parameters are determined as the calculation parameters of the three-dimensional non-axisymmetric crystallization interface.
[0063] The mesh surface parameters may include the temperature and coordinates of the target mesh nodes in the target mesh surface.
[0064] Step S103: using the main thread to send the calculation parameters to each sub-thread, and using the sub-thread to calculate the movement parameters of the target grid node in the target grid surface corresponding to the sub-thread according to the calculation parameters.
[0065] Among them, the target grid nodes in the target grid surface corresponding to each sub-thread are different from each other.
[0066] Step S104: Control the target mesh nodes to move according to the movement parameters of the target mesh nodes to obtain an adjusted three-dimensional non-axisymmetric crystallization interface.
[0067] It can be understood that each time the electronic device executes the operations corresponding to step S103 to step S104 to adjust the three-dimensional non-axisymmetric crystallization interface, each target grid node is moved only once; in order to avoid repeated calculation of the movement parameters of the same target grid node in step S103, resulting in a waste of sub-thread computing resources, and to avoid the problem of repeated movement of the same target grid node in step S104 resulting in excessive movement distance, in an embodiment of the present invention, the target grid nodes in the target grid surface corresponding to each sub-thread are different.
[0068] Wherein, the moving parameters include the moving direction and the moving distance in the moving direction; wherein, the moving direction includes upward and downward. It should be noted that the temperature of the actual three-dimensional non-axisymmetric crystallization interface is uniform and equal to the crystal solidification temperature; in the target geometric model, the target crystal is above the actual three-dimensional non-axisymmetric crystallization interface, and the melt corresponding to the target crystal is below the actual three-dimensional non-axisymmetric crystallization interface. When the temperature of the three-dimensional non-axisymmetric crystallization interface in step S102 is lower than the crystal solidification temperature, it indicates that the position of the three-dimensional non-axisymmetric crystallization interface in step S102 in the target geometric model is higher than the actual three-dimensional non-axisymmetric crystallization interface, and the three-dimensional non-axisymmetric crystallization interface in step S102 needs to be moved downward; similarly, when the temperature of the three-dimensional non-axisymmetric crystallization interface in step S102 is higher than the crystal solidification temperature, it indicates that the position of the three-dimensional non-axisymmetric crystallization interface in step S102 in the target geometric model is lower than the actual three-dimensional non-axisymmetric crystallization interface, and the three-dimensional non-axisymmetric crystallization interface in step S102 needs to be moved upward.
[0069] In the embodiment of the present invention, the corresponding relationship between the target grid node moving distance and the temperature can be predetermined. For example, the unit moving distance of the target moving node can be predetermined when the temperature of the target grid node differs from the crystal solidification temperature by 1K.
[0070] Specifically, in the process of using a sub-thread to calculate the movement parameters of a target grid node in a target grid surface corresponding to the sub-thread according to calculation parameters, the electronic device first uses the sub-thread to calculate the temperature difference between the target grid node corresponding to the sub-thread and the crystal solidification temperature, and calculates the product between the temperature difference and the unit movement distance, and determines the product as the movement parameter.
[0071] It can be understood that, when the temperature of the target grid node is greater than the crystal solidification temperature, the temperature difference is a positive value. When the temperature difference is a positive value, in step S104, the electronic device moves the target grid node upward by a distance indicated by the absolute value of the temperature difference; when the temperature of the target grid node is less than the crystal solidification temperature, the temperature difference is a negative value. When the temperature difference is a negative value, in step S104, the electronic device moves the target grid node downward by a distance indicated by the absolute value of the temperature difference.
[0072] The number of target grid nodes in the target grid surface corresponding to each sub-thread is at least 1; when the number of target grid nodes in the target grid surface corresponding to the sub-thread is greater than 1, the sub-thread can repeatedly execute step S103 to calculate the movement parameters of each target grid node in the target grid surface corresponding to the sub-thread according to the calculation parameters.
[0073] It should be noted that after controlling the movement of the target grid nodes according to the movement parameters of each target grid node to obtain the adjusted three-dimensional non-axisymmetric crystallization interface, the temperature of the target calculation domain is unbalanced due to the movement of the grid nodes in the target calculation domain, and it is necessary to repeat step S101 to perform steady-state calculation on the target calculation domain, obtain the temperature field of the target calculation domain and execute step S102 to determine whether the temperature of the three-dimensional non-axisymmetric crystallization interface meets the preset conditions according to the temperature field. When the temperature of the three-dimensional non-axisymmetric crystallization interface meets the preset conditions, step S105 is executed; when the temperature of the three-dimensional non-axisymmetric crystallization interface does not meet the preset conditions, step S102 is continued to obtain the calculation parameters and steps S103 and S104 are continued to adjust the three-dimensional non-axisymmetric crystallization interface until the temperature of the target calculation domain is balanced and the temperature of the three-dimensional non-axisymmetric crystallization interface meets the preset conditions, and the corresponding operation of step S105 is executed.
[0074] Step S105: When the temperature of the target calculation domain is balanced and the temperature of the three-dimensional non-axisymmetric crystallization interface meets a preset condition, the three-dimensional non-axisymmetric crystallization interface is determined as the target crystallization interface.
[0075] It can be understood that when the temperature of the target calculation domain is balanced and the temperature of the three-dimensional non-axisymmetric crystallization interface meets the preset conditions, it indicates that the three-dimensional non-axisymmetric crystallization interface is the same as or close to the actual three-dimensional non-axisymmetric crystallization interface between the target crystal and the melt corresponding to the target crystal. At this time, the three-dimensional non-axisymmetric crystallization interface can be determined as the target crystallization interface. Among them, the target interface is the crystallization interface closest to the actual three-dimensional non-axisymmetric crystallization interface determined by the embodiment of the present invention.
[0076] In the embodiment of the present invention, after determining the target crystallization interface, the growth process of the target crystal can be controlled according to the shape of the target crystallization interface. For example, when the shape of the target crystallization interface is as follows: Figure 4 In the case of the concave target crystal shown in the figure, the growth process of the target crystal can be controlled by improving the structure of the crystal growth furnace body and enhancing the thermal insulation effect of the crystal growth furnace (for example, thickening the thermal insulation layer of the crystal growth furnace, adding a thermal insulation cover to the crucible in the crystal growth furnace, etc.), thereby reducing or avoiding defects such as vacancies and dislocations caused by the crystallization interface of the concave crystal, and improving the quality of the gallium oxide crystal.
[0077] In the process of growing gallium oxide crystals by the guided mold method, it is difficult to observe and control the shape of the non-axisymmetric crystallization interface during the growth of gallium oxide crystals due to the difficulty in obtaining the crystallization interface, and there is a problem of difficulty in controlling the growth process of gallium oxide crystals. The method for determining the crystallization interface of crystals grown by the guided mold method provided in the embodiment of the present invention not only realizes the determination of the target crystallization interface, that is, the actual three-dimensional non-axisymmetric crystallization interface between the target crystal and the melt corresponding to the target crystal, but also uses the main thread in the electronic device and at least two sub-threads controlled by the main thread to obtain the target calculation parameters and parallel calculation of the movement parameters, thereby improving the efficiency of determining the target crystallization interface, improving the accuracy of controlling the growth process of the target crystal based on the target crystallization interface, and improving the crystal quality of the target crystal grown by the guided mold method.
[0078] In an optional embodiment, the three-dimensional non-axisymmetric crystallization interface includes a vertex and a center point of the target mesh surface; step S102 determines whether the temperature of the three-dimensional non-axisymmetric crystallization interface meets a preset condition according to the temperature field, including steps S1021 to S1024:
[0079] Step S1021: Determine the first temperature of the vertex according to the temperature field.
[0080] Step S1022: When the first temperature is equal to the crystal solidification temperature, obtain a second temperature of the center point according to the temperature field.
[0081] Step S1023: When the temperature difference between the second temperature and the first temperature is less than or equal to a first preset threshold, determine that the temperature of the three-dimensional non-axisymmetric crystallization interface meets a preset condition.
[0082] Step S1024: when the temperature difference between the second temperature and the first temperature is greater than the first preset threshold, determine that the temperature of the three-dimensional non-axisymmetric crystallization interface does not meet the preset condition.
[0083] In the embodiment of the present invention, the three-dimensional non-axisymmetric crystallization interface includes vertices and center points of the target mesh surface. Specifically, when the three-dimensional non-axisymmetric crystallization interface is a rectangle, the number of vertices is 4; the center point is the center point of the target mesh surface constituting the three-dimensional non-axisymmetric crystallization interface, and in the three-dimensional non-axisymmetric crystallization interface, the number of center points is the same as the number of target mesh surfaces.
[0084] It can be understood that the temperature field obtained in step S101 includes temperature data of the three-dimensional non-axisymmetric crystallization interface, and the temperature data of the three-dimensional non-axisymmetric crystallization interface includes a first temperature at the vertex and a second temperature at the center.
[0085] When the electronic device determines the target geometric model, it can also establish the following equations with the center point of the bottom of the crucible in the crystal growth furnace in the target geometric model as the origin (O), the growth direction of the target crystal as the z-axis, the thickness direction of the target crystal as the x-axis, and the width direction of the target crystal as the y-axis: Figure 2 The three-dimensional rectangular coordinate system shown.
[0086] According to the three-dimensional rectangular coordinate system, the electronic device can determine the coordinates of each position in the temperature field, thereby determining the first coordinates of each vertex and the second coordinates of each center point; according to the first coordinate, the electronic device can obtain the first temperature of the vertex from the temperature field, and according to the second coordinate, the electronic device can obtain the second temperature of the center point from the first temperature field.
[0087] In an embodiment of the present invention, the electronic device determines whether the temperature of the three-dimensional non-axisymmetric crystallization interface meets a preset condition based on the temperature field, specifically:
[0088] First, according to the temperature field and the first coordinate of the vertex, the first temperature of the vertex is obtained from the temperature field.
[0089] Then, the first temperature is compared with the crystal solidification temperature of the target crystal.
[0090] Then, when the first temperature is equal to the crystal solidification temperature, it indicates that the temperature at the vertex position of the three-dimensional non-axisymmetric crystallization interface is equal to the crystal solidification temperature of the target crystal, that is, the vertex of the three-dimensional non-axisymmetric crystallization interface is located in the actual three-dimensional non-axisymmetric crystallization interface. At this time, the electronic device can continue to execute the operation corresponding to step S1022.
[0091] In the case where the first temperature is not equal to the crystal solidification temperature, it indicates that the temperature at the vertex position of the three-dimensional non-axisymmetric crystallization interface is not equal to the crystal solidification temperature of the target crystal, that is, the vertex is not located in the actual three-dimensional non-axisymmetric crystallization interface; specifically, in the case where the first temperature is less than the crystal solidification temperature, it indicates that the temperature at the vertex position of the three-dimensional non-axisymmetric crystallization interface is too low, which easily causes the target crystal to separate from the liquid bridge; in the case where the first temperature is greater than the crystal solidification temperature, it indicates that the temperature at the vertex position of the three-dimensional non-axisymmetric crystallization interface is too high, which easily causes the target crystal to adhere to the mold in the crystal growth furnace. In an embodiment of the present invention, in the case where the first temperature is not equal to the crystal solidification, the heating power on the crucible can be controlled by adjusting the magnitude of the current in the induction coil. It can be understood that adjusting the magnitude of the current in the induction coil will cause the furnace temperature of the crystal growth furnace to change, so that the temperature in the target calculation domain changes, and then the temperature of the target calculation domain is unbalanced, and it is necessary to repeat the operation corresponding to step S101 to obtain the temperature field of the target calculation domain, and after obtaining the temperature field of the target calculation domain, continue to perform the operations corresponding to steps S1021 to S1024.
[0092] Then, when the second temperature is obtained through step S1022, the temperature difference between each second temperature and the first temperature is calculated, and when the temperature difference is less than or equal to the first preset threshold, it is determined that the temperature of the three-dimensional non-axisymmetric crystallization interface meets the preset condition; it can be understood that step S1023 is performed when the first temperature is equal to the crystal solidification temperature in step S1022, and when the temperature difference between the second temperature and the first temperature in step S1023 is less than or equal to the first preset threshold, it can be determined that the temperature of the three-dimensional non-axisymmetric crystallization interface is uniform and meets the preset condition.
[0093] In a case where the temperature difference between the second temperature and the first temperature is greater than the first preset threshold, it is determined that the temperature of the three-dimensional non-axisymmetric crystallization interface does not satisfy the preset condition.
[0094] Among them, the first preset threshold is the acceptable temperature fluctuation range in the three-dimensional non-axisymmetric crystallization interface in the actual application scenario. For example, the first preset threshold can be 0.5°C, that is, when the temperature difference between the second temperature and the first temperature is less than or equal to 0.5°C, it can be determined that the temperature of the three-dimensional non-axisymmetric crystallization interface is uniform.
[0095] The method for determining the crystallization interface of crystals grown by the guided mode method provided in an embodiment of the present invention determines whether the temperature of the three-dimensional non-axisymmetric crystallization interface in step S102 meets a preset condition based on the temperatures (first temperature and second temperature) of representative points (vertices and center points of the target mesh surface) in the three-dimensional non-axisymmetric crystallization interface. There is no need to confirm all temperature data of the three-dimensional non-axisymmetric crystallization interface, which simplifies the comparison process for determining whether the temperature of the three-dimensional non-axisymmetric crystallization interface meets the preset conditions and improves the efficiency of determining whether the temperature of the three-dimensional non-axisymmetric crystallization interface meets the preset conditions.
[0096] In an optional embodiment, the target geometric model includes a crystal growth furnace, and the crystal growth furnace is used to grow the target crystal by a guided mode method; the method further includes step S1025:
[0097] Step S1025: When the first temperature is not equal to the crystal solidification temperature, adjust the furnace temperature of the crystal growth furnace according to the first temperature.
[0098] Specifically, when the first temperature is greater than the crystal solidification temperature, the electronic device can reduce the heating power on the crucible by reducing the current in the induction coil, thereby reducing the furnace temperature of the crystal growth furnace; when the first temperature is lower than the crystal solidification temperature, the electronic device can increase the heating power on the crucible by increasing the current in the induction coil, thereby increasing the furnace temperature of the crystal growth furnace.
[0099] It should be noted that after the electronic device adjusts the furnace temperature of the crystal growth furnace through step S1025, it will cause temperature imbalance in the target calculation domain; after step S1025, the electronic device first needs to execute step S101 to obtain the temperature field of the target calculation domain, and then execute step S1021 to obtain the first temperature of the vertex, and compare the first temperature with the crystal solidification temperature of the target crystal until the first temperature is equal to the crystal solidification temperature, and continue to execute the corresponding operation of step S1022.
[0100] The method for determining the crystallization interface of a crystal grown by a guided mold method provided in an embodiment of the present invention, when the first temperature of the vertex of the three-dimensional non-axisymmetric crystallization interface is not equal to the crystal solidification temperature, adjusts the furnace temperature of the crystal growth furnace according to the first temperature until the first temperature is equal to the crystal solidification temperature, and then continues to determine whether the temperature of the three-dimensional non-axisymmetric crystallization interface is uniform based on the temperature difference between the second temperature of the center point of the target grid surface and the first temperature, thereby increasing the probability that the three-dimensional non-axisymmetric crystallization interface meets the preset conditions in step S102 and shortening the process of determining the target crystallization interface.
[0101] In an optional embodiment, when the temperature of the three-dimensional non-axisymmetric crystallization interface does not meet the preset conditions in step S102, the calculation parameters of the three-dimensional non-axisymmetric crystallization interface are obtained by using the main thread, including steps S1026 to S1028:
[0102] Step S1026: When the temperature of the three-dimensional non-axisymmetric crystallization interface does not meet the preset conditions, the main thread is used to obtain the first coordinates of the target grid nodes in the target grid surface corresponding to each sub-thread, as well as the second coordinates and the second temperature of the center point of the target grid surface corresponding to the sub-thread.
[0103] Step S1027: using the main thread, determine the first coordinate, the second coordinate and the second temperature corresponding to each target grid surface as the target data group corresponding to the target grid surface.
[0104] Step S1028, obtaining the grid surface identifier of the target grid surface, and sorting the target data group according to the grid surface identifier to obtain the calculation parameters of the three-dimensional non-axisymmetric crystallization interface.
[0105] The calculation parameters include target data groups corresponding to each target grid surface.
[0106] In the embodiment of the present invention, the calculation parameters include the first coordinates of the target grid nodes in each target grid surface, and the second coordinates and the second temperature of the center point of the target grid surface.
[0107] Reference Figure 6 , shows a schematic diagram of the structure of an electronic device of the present invention. Figure 6As shown, the electronic device includes a main thread and a group of sub-threads controlled by the main thread, wherein the number of main threads is 1, the number of sub-threads is m, the sub-threads are marked in the order of 0 to m, and m is an integer greater than 1. Specifically, in the process of using the main thread to obtain the calculation parameters of the three-dimensional non-axisymmetric crystallization interface, the main thread can first send a calculation parameter acquisition instruction to each sub-thread, so that the sub-thread can obtain the second coordinates and the second temperature of the center point of each target grid surface corresponding to the sub-thread and the first coordinate of the target grid node in the target grid surface based on the calculation parameter acquisition instruction, and send the second coordinates and the second temperature of the center point of the target grid surface and the first coordinate of the target grid node in the target grid surface to the main thread; after receiving the first coordinates, the second coordinates and the second temperature sent by each sub-thread, the main thread determines the first coordinates, the second coordinates and the second temperature corresponding to the target grid surface as a target data group corresponding to the target grid surface one by one according to the corresponding relationship between the target grid surface and the first coordinates, the second coordinates and the second temperature; finally, the target data group is sorted according to the grid surface identifiers of each target grid surface to obtain the calculation parameters of the three-dimensional non-axisymmetric crystallization interface.
[0108] Among them, the grid surface identifier is an identifier that corresponds one-to-one to the target grid surface. According to the grid surface identifier, the target grid surface corresponding to the grid identifier can be uniquely determined; illustratively, each target grid surface in the three-dimensional non-axisymmetric crystallization interface can be numbered in the order of 1, 2, 3,... as the grid surface identifier of the target grid surface.
[0109] In an optional implementation, the electronic device may organize the target data group according to the grid surface identifiers of each target grid surface by establishing a one-to-one correspondence between the target grid surface and the target data group, thereby obtaining the calculation parameters of the three-dimensional non-axisymmetric crystallization interface.
[0110] In another optional implementation, the electronic device may organize the target data group according to the grid surface identifiers of each target grid surface by: first, establishing a one-to-one correspondence between the grid surface identifier and the target array according to the one-to-one correspondence between the target grid surface and the target data group; then, sorting the grid surface identifiers and the target array corresponding one-to-one to the grid surface identifiers according to the order between the grid surface identifiers to obtain the calculation parameters of the three-dimensional non-axisymmetric crystallization interface.
[0111] In an embodiment of the present invention, when the electronic device uses a sub-thread to calculate the movement parameters of the target grid node in the target grid surface corresponding to the sub-thread according to the calculation parameters, the sub-thread can search for the target data group corresponding to the grid surface identifier from the calculation parameters according to the grid surface identifier of the target grid surface, and then obtain the first coordinates of the target grid node in the target grid surface and the second coordinates and the second temperature of the center point of the target grid surface from the target data group; finally, according to the first coordinates of the target grid node in the target grid surface and the second coordinates and the second temperature of the center point of the target grid surface, calculate the movement parameters of the target grid node in the target grid surface corresponding to the sub-thread.
[0112] In an alternative embodiment, referring to Figure 7 , shows a structural schematic diagram of another electronic device of the present invention. The electronic device includes a main thread and a group of sub-threads controlled by the main thread, wherein the number of main threads is 1, the number of sub-threads is n, the sub-threads are marked in the order of 0 to n-1, and n is an integer greater than 2; the main thread can accept a calculation parameter acquisition instruction or a movement parameter calculation instruction from the electronic device, and pass the calculation parameter acquisition instruction or the movement parameter calculation instruction to sub-thread 0, and then sub-thread 0 forwards the calculation parameter acquisition instruction or the movement parameter calculation instruction to other sub-threads, and other sub-threads except sub-thread 0 receive the calculation parameter acquisition instruction or the movement parameter calculation instruction sent by the main thread through sub-thread 0.
[0113] Specifically, in the process of the electronic device using the main thread to obtain the calculation parameters of the three-dimensional non-axisymmetric crystallization interface, the main thread can first send a calculation parameter acquisition instruction to the sub-thread 0; then, the sub-thread 0 forwards the calculation parameter acquisition instruction sent by the main thread to the sub-threads 1 to the sub-threads n-1; the sub-threads 1 to the sub-threads n-1 obtain the second coordinates and the second temperature of the center point of each target grid surface corresponding to the sub-thread and the first coordinates of the target grid node in the target grid surface based on the calculation parameter acquisition instruction, and send the second coordinates and the second temperature of the center point of the target grid surface and the first coordinates of the target grid node in the target grid surface to the sub-thread 0; the sub-thread 0 receives the target grid surface sent by the sub-threads 1 to the sub-threads n-1. After obtaining the second coordinate and the second temperature of the center point of the grid surface and the first coordinate of the target grid node in the target grid surface, the first coordinate, the second coordinate and the second temperature corresponding to each target grid surface are sorted according to the grid surface identifier of the target grid surface to obtain the sorted summary data, and the sorted summary data is forwarded to the main thread; after receiving the sorted summary data forwarded by the child thread 0, the main thread determines the first coordinate, the second coordinate and the second temperature corresponding to the target grid surface as a target data group corresponding to the target grid surface one by one according to the correspondence between the grid surface identifier and the first coordinate, the second coordinate and the second temperature in the summary data, and obtains the calculation parameters of the target data group corresponding to each target grid surface.
[0114] It should be noted that after the electronic device uses the main thread to obtain the calculation parameters of the three-dimensional non-axisymmetric crystallization interface, it can use the main thread to send the calculation parameters to each of the sub-threads, so that each sub-thread can continue to perform the operation corresponding to step S103 based on the calculation parameters.
[0115] According to the method for determining the crystallization interface of crystals grown by the guided mode method provided by the embodiment of the present invention, in the process of using the main thread to obtain the calculation parameters of the three-dimensional non-axisymmetric crystallization interface, the electronic device uses the control relationship between the main thread and the sub-thread to parallelly obtain the first coordinates of the target grid node in the target grid surface corresponding to each sub-thread, and the second coordinates and the second temperature of the center point of the target grid surface corresponding to the sub-thread, and uses the main thread to determine the first coordinates, the second coordinates and the second temperature corresponding to each target grid surface as the target data group corresponding to the target grid surface, and sorts the target data group according to the grid surface identifier of the target grid surface to obtain the calculation parameters of the three-dimensional non-axisymmetric crystallization interface. While improving the efficiency of obtaining the calculation parameters, the obtained calculation parameters also include the corresponding relationship between the target grid surface and the first coordinates, the second coordinates and the second temperature, which is beneficial for the sub-thread to quickly find the required target data group in the process of calculating the movement parameters of the target grid node according to the calculation parameters, thereby improving the calculation efficiency and the accuracy of the calculated movement parameters.
[0116] In an optional embodiment, the step S103 of using the child thread to calculate the movement parameters of the target mesh node in the target mesh surface corresponding to the child thread according to the calculation parameters includes step S1031:
[0117] Step S1031, using the sub-thread, according to the first coordinates of the target grid nodes in each target grid surface and the second coordinates and the second temperature of the center point of the target grid surface, the movement parameters of the target grid nodes in the target grid surface corresponding to the sub-thread are calculated as follows:
[0118] (1)
[0119] in, represents the movement parameters of the target grid node; A mesh face identifier representing a target mesh face around a target mesh node; Indicates the total number of target mesh faces around the target mesh node; Indicates The second temperature of the center point of the target grid surface; Indicates The distance between the second coordinate of the center point of the target mesh surface and the first coordinate of the target mesh node; Indicates the crystal solidification temperature of the target crystal; Represents the movement coefficient, which is used to adjust the moving distance of the target grid node.
[0120] In an embodiment of the present invention, when the calculation parameters include the first coordinates of the target grid nodes in each target grid surface, and the second coordinates and the second temperature of the center point of the target grid surface, the sub-thread can calculate the movement parameters of each target grid node respectively through Formula 1.
[0121] It should be noted that in order to ensure that the target mesh nodes are moved according to the movement parameters of each target mesh node in step S104 to obtain the mesh quality of the adjusted three-dimensional non-axisymmetric crystallization interface, it is necessary to control the distance of the target mesh node to be moved once to be smaller than the size of the calculation mesh near the target mesh node. Some calculations result in temperature difference values, which do not meet the requirements of the target grid node moving distance. In order to ensure that the distance of a single movement of the target grid node is less than the size of the calculation grid near the target grid node, the movement coefficient can be determined in advance based on the size of the calculation grid near the three-dimensional non-axisymmetric crystallization interface. .
[0122] In the embodiment of the present invention, the electronic device may be a parallel solver.
[0123] In an optional embodiment, the target computational domain includes a computational grid obtained by meshing the target geometric model, and the computational grid includes a target grid surface; the moving distance indicated by the moving parameter is smaller than the side length of the computational grid adjacent to the target grid node in the moving direction indicated by the moving parameter.
[0124] The method for determining the crystallization interface of crystals grown by the guided mold method provided in an embodiment of the present invention realizes the adjustment of the three-dimensional non-axisymmetric crystallization interface so that the three-dimensional non-axisymmetric crystallization interface continuously approaches the actual three-dimensional non-axisymmetric crystallization interface between the target crystal and the melt corresponding to the target crystal. At the same time, in the process of adjusting the three-dimensional non-axisymmetric crystallization interface, the moving distance of each target grid node is less than the side length of the calculation grid adjacent to the target grid node in the moving direction indicated by the moving parameter, so that the shape of the three-dimensional non-axisymmetric crystallization interface can be accurately controlled and the deformation quality of the three-dimensional non-axisymmetric crystallization interface can be guaranteed.
[0125] In an optional embodiment, the target computational domain includes a computational grid obtained by meshing the target geometric model, and the computational grid includes a target computational grid where the target grid surface is located; step S101 performs steady-state calculation on the target computational domain in the case of temperature imbalance in the target computational domain to obtain a temperature field of the target computational domain, including steps S1011 to S1012:
[0126] Step S1011, when the temperature of the target computational domain is unbalanced, obtain grid parameters corresponding to the target computational grid and computational domain parameters corresponding to the target computational domain; the grid parameters include parameters for characterizing dielectric radiation inside the target crystal.
[0127] Step S1012: Based on the grid parameters and the calculation domain parameters, a steady-state calculation is performed on the target calculation domain to obtain the temperature field of the target calculation domain.
[0128] In an embodiment of the present invention, the grid parameters are parameters related to the target computational grid in the target computational domain, and the grid parameters are used to characterize the dielectric radiation inside the target crystal. Specifically, the grid parameters may include a control equation corresponding to the target computational grid; wherein the control equation is a physical model determined according to the physical process involved in the crystal growth furnace and used to describe the physical process involved in the crystal growth furnace.
[0129] In the case where the grid parameters include control equations, in step S1012, the control equations may be solved according to the calculation domain parameters to perform steady-state calculations on the target calculation domain to obtain a temperature field corresponding to the target calculation domain.
[0130] The computational domain parameters are parameters related to the target computational domain as a whole, and the computational domain parameters may include but are not limited to: thermophysical property parameters of each component in the target geometric model, boundary conditions of the target computational domain, and source items corresponding to the target computational domain.
[0131] Among them, the thermophysical property parameters of each component in the target geometric model may include but are not limited to the thermophysical property parameters of the crucible, the thermophysical property parameters of the mold, the thermophysical property parameters of the induction coil, the thermophysical property parameters of the target crystal, and the thermophysical property parameters of the melt corresponding to the target crystal. The thermophysical property parameters may include but are not limited to anisotropic thermal conductivity tensor, absorption coefficient, thermal expansion coefficient, specific heat capacity, density, etc. In the embodiment of the present invention, the thermophysical property parameters of each component part in the target geometric model may be experimental data obtained by experiment. The experimental data may be published by previous research or obtained by self-experimental testing, and the embodiment of the present invention is not limited by comparison.
[0132] The boundary conditions of the target computational domain include the temperature and surface emissivity of the contact interface in the target geometric model, and the contact interfaces in the target geometric model are all coupled, non-slip walls. The temperature of the contact interface includes the temperature of the furnace wall of the crystal growth furnace, and the surface emissivity of the contact interface in the target geometric model may include but is not limited to: the surface emissivity of the target crystal, the surface emissivity of the crucible, the surface emissivity of the melt corresponding to the target crystal, the surface emissivity of the furnace wall of the crystal growth furnace, etc.
[0133] The source term corresponding to the target computational domain reflects the influence of other factors in the target computational domain other than the basic part in the target computational domain on the three-dimensional non-axisymmetric crystallization interface. In an embodiment of the present invention, the source term may include a first source term in a first region corresponding to the crucible and a second source term in a second region corresponding to the three-dimensional non-axisymmetric crystallization interface.
[0134] Among them, the first source term is the induction heating power on the crucible; specifically, the induction heating power is calculated by Formula 2 to Formula 5 according to the current loaded on the induction coil, the heating frequency, and the relative position of the induction coil and the crucible:
[0135] (2)
[0136] (3)
[0137] (4)
[0138] (5)
[0139] in, represents the Laplace operator, represents the magnetic vector potential, represents the magnetic induction intensity, represents the magnetic permeability, represents the current frequency, represents the conductivity, represents the applied current density in the induction coil, is the induced current density, express The complex conjugate / complex conjugate of Indicates the induction heating power.
[0140] The second source term is the additional heat generated by the phase change of the three-dimensional non-axisymmetric crystallization interface. Specifically, the additional heat generated by the phase change of the three-dimensional non-axisymmetric crystallization interface can be calculated according to the growth rate of the target crystal, the latent heat of crystal solidification, and the crystal density by the following formula 6:
[0141] (6)
[0142] in, represents the additional heat generated by the phase change at the three-dimensional non-axisymmetric crystal interface, represents the density of the target crystal, Indicates the growth rate of the target crystal, Represents the latent heat of solidification of the target crystal.
[0143] In an embodiment of the present invention, when the grid parameters corresponding to the target computational grid and the computational domain parameters corresponding to the target computational domain are obtained through step S1011, a steady-state calculation can be performed on the target computational domain based on the grid parameters and the computational domain parameters to obtain a temperature field corresponding to the target computational domain.
[0144] Specifically, in the process of executing step S1012, the electronic device can first initialize the target computational domain, and then iteratively calculate the target computational domain according to the target geometric model, mesh parameters, and computational domain parameters until the mass, energy, and momentum in the entire target computational domain are conserved or stable, and the temperature field corresponding to the target computational domain is obtained.
[0145] Specifically, initializing the target computational domain includes: inputting the grid parameters and computational domain parameters obtained in step S1011 into the target computational domain. Specifically, iteratively calculating the target computational domain according to the target geometric model, grid parameters, and computational domain parameters includes: solving the control equations in the grid parameters according to the target geometric model and computational domain parameters.
[0146] In an optional embodiment, the step S1011 of obtaining the grid parameters corresponding to the target computing grid includes steps A11 to A13:
[0147] Step A11, according to the dielectric radiation and anisotropic thermal conductivity characteristics inside the target crystal, when there is no momentum change and mass change in the target crystal region in the target calculation domain, determine the energy conservation equation corresponding to the target calculation grid.
[0148] Step A12: Determine the radiation transfer equation corresponding to the target calculation grid according to the absorption characteristics of free carriers in the target crystal.
[0149] Step A13: determine the energy conservation equation and the radiation transfer equation as grid parameters corresponding to the target calculation grid.
[0150] In an embodiment of the present invention, taking into account the influence of dielectric radiation inside the target crystal on the three-dimensional non-axisymmetric crystallization interface, control equations for describing the physical processes related to dielectric radiation inside the target crystal are determined according to the physical processes related to dielectric radiation inside the target crystal involved in the crystal growth furnace, including the energy conservation equation and the radiation transfer equation corresponding to the target calculation grid, so that the temperature data at the three-dimensional non-axisymmetric crystallization interface in the temperature field obtained by steady-state calculation of the target calculation domain according to the control equation in the grid parameters and the calculation domain parameters is close to the temperature data in the actual scene, thereby making the target crystallization interface determined according to the temperature field closer to the actual three-dimensional non-axisymmetric crystallization interface, thereby improving the reliability of the target crystallization interface determined in the embodiment of the present invention, while realizing the control of the growth process of the target crystal according to the target crystallization interface, it also improves the accuracy of controlling the growth process of the target crystal, thereby improving the stability of the growth process of the target crystal and the crystal quality of the target crystal.
[0151] Specifically, according to the dielectric radiation inside the target crystal, when there is no momentum change and mass change in the target crystal region in the target calculation domain, the energy conservation equation corresponding to the target calculation grid can be expressed by the following formula 7:
[0152] (7)
[0153] in, represents the heat flow in the target crystal, Represents the radiative heat flow within the target crystal.
[0154] According to the anisotropic thermal conductivity of the target crystal, the thermal conduction heat flow in the target crystal is expanded into Formula 8 to Formula 9:
[0155] (8)
[0156] (9)
[0157] In addition, according to the absorption characteristics of free carriers in the target crystal, the radiation transfer equation corresponding to the target calculation grid determined by the discrete coordinate method is shown in formula 10:
[0158] (10)
[0159] in, Indicates spatial location In the direction The radiation intensity, represents the radiation absorption coefficient in the target crystal, is the refractive index of the target crystal, Indicates boldface.
[0160] For any spatial position, the spatial angle of 4π is divided into finite discrete angles, and the discrete coordinate method is used to discretize the radiation transfer equation into a series of partial differential equations in space, such as formula 11:
[0161] (11)
[0162] in, represents the integral set weight, Indicates the discrete direction m in azimuth The radiation intensity under .
[0163] In an optional embodiment, the target computational domain includes a computational grid obtained by meshing the target geometric model, the computational grid includes a target grid surface, and the size of the computational grid is a first size; before determining in step S102 whether the temperature of the three-dimensional non-axisymmetric crystallization interface meets a preset condition according to the temperature field, the method further includes steps A21 to A23:
[0164] Step A21, obtaining first monitoring data of the temperature field.
[0165] Step A22: Compare the first monitoring data with the target monitoring data.
[0166] Among them, the target monitoring data is the monitoring data of the target temperature field, the target temperature field is the temperature field corresponding to the target calculation domain determined according to the calculation grid of the second size, and the second size is larger than the first size; the second size is the size of the calculation grid obtained by meshing the target geometric model again before obtaining the calculation grid of the first size after meshing the target geometric model.
[0167] Step A23: When the first monitoring data is different from the target monitoring data, the target geometric model is re-grid according to the third size to obtain a target calculation domain corresponding to the target geometric model.
[0168] The third size is smaller than the first size; the third size is the size of a computational grid obtained by meshing the target geometric model again after meshing the target geometric model to obtain a computational grid of the first size.
[0169] Step A24: when the first monitoring data is the same as the target monitoring data, an operation is performed to determine whether the temperature of the three-dimensional non-axisymmetric crystallization interface meets a preset condition according to the temperature field.
[0170] In an embodiment of the present invention, after obtaining the temperature field corresponding to the target computational domain in step S101 and before executing step S102, the electronic device may also perform mesh independence verification on the computational grid in the target computational domain. If the computational grid in the target computational domain passes the mesh independence verification, the operation corresponding to step S102 is continued. If the computational grid in the target computational domain fails to pass the mesh independence verification, the computational grid in the target computational domain is first meshed (the computational grid size is reduced and the number of computational grids is increased), and then mesh independence verification is performed on the computational grid in the target computational domain after meshing, until the computational grid in the target computational domain passes the mesh independence verification. It can be understood that the computational grid of the first size obtained after meshing the target geometric model is a process of encrypting the computational grid of the second size, and the computational grid of the third size obtained after meshing the target geometric model is a process of encrypting the computational grid of the first size.
[0171] Among them, the computational grid in the target computational domain passes the grid independence verification, which means that the steady-state calculation result obtained after the steady-state calculation based on the computational grid in the target computational domain does not change with the reduction of the computational grid size or the increase of the number of grids. In an embodiment of the present invention, the steady-state calculation result can be the temperature of any area in the target computational domain or the temperature field corresponding to the target computational domain; when the temperature field corresponding to the target computational domain or the temperature of any area in the temperature field corresponding to the target computational domain does not change with the reduction of the computational grid size or the increase of the number of grids, it is determined that the computational grid in the target computational domain passes the grid independence verification.
[0172] In the case where the computational grid in the target computational domain passes the grid independence verification, the target computational domain corresponding to the maximum value of the computational grid size or the minimum value of the computational grid number in the target computational domain that passes the grid independence verification can be selected to perform the operation corresponding to step S102. It can be understood that in the case where the computational grid in the target computational domain passes the grid independence verification, it indicates that the size or number of the computational grid has little effect on the calculation result of the steady-state calculation. In theory, the grid independence verification can be satisfied by increasing the number of computational grids or reducing the size of the computational grids. However, the more the number of computational grids, the greater the workload of numerical calculation. In order to save numerical calculation resources, the target computational domain with the least number of grids or the largest size of computational grids in the target computational domain that passes the grid independence verification can be selected for subsequent calculations.
[0173] As an optional implementation, when the computational mesh in the target computational domain fails to pass the mesh independence verification, only the hexahedral mesh in the target computational domain (that is, the target computational mesh where the three-dimensional non-axisymmetric crystallization interface is located) can be mesh encrypted, and then the computational mesh in the target computational domain after the mesh encryption can be mesh-independent verified until the computational mesh in the target computational domain passes the mesh independence verification. This can ensure the mesh quality while further reducing the workload of numerical calculations in the process of determining the target crystallization interface based on the temperature field.
[0174] Specifically, when the first monitoring data obtained in step A21 is different from the target monitoring data, it indicates that the computational grid in the target computational domain has not passed the grid independence verification, and the size of the computational grid in the target computational domain is encrypted from the first size to the third size through step A22, and then the computational grid in the target computational domain after the mesh encryption is subjected to grid independence verification until the computational grid in the target computational domain passes the grid independence verification.
[0175] In an embodiment of the present invention, when the first monitoring data is different from the target monitoring data, only the hexahedral mesh in the target computing domain may be encrypted to the third size, and then the computational mesh in the target computing domain after the mesh encryption may be subjected to mesh independence verification until the computational mesh in the target computing domain passes the mesh independence verification.
[0176] When the first monitoring data is identical to the target monitoring data, it indicates that the computing grid in the target computing domain passes the grid independence verification, and the operation corresponding to step S102 may continue to be performed.
[0177] Reference Figure 8 , shows a flow chart of steps of another method for determining a crystallization interface of a crystal grown by a guided mode method of the present invention, the method comprising the following steps S201 to S214:
[0178] Step S201: The electronic device obtains a target geometric model.
[0179] Specifically, the target geometric model includes a crystal growth furnace, a target crystal grown by the crystal growth furnace and a melt corresponding to the target crystal, and a three-dimensional non-axisymmetric crystallization interface between the target crystal and the melt corresponding to the target crystal; wherein the crystal growth furnace includes a crucible, a mold, and an induction coil. The induction coil is a spiral induction coil, which is arranged on the outer wall of the crucible. When current is passed into the induction coil, the induction coil induction heats the crucible, and the power of the induction coil induction heating the crucible can be controlled by controlling the magnitude of the current passed into the induction coil; the melt corresponding to the target crystal is contained in the crucible, and a capillary slit is arranged in the mold, so that the melt corresponding to the target crystal in the crucible can rise to the top of the mold by capillary action, and form a thin film on the top and diffuse to the surroundings, thereby forming a liquid bridge between the crystal growth furnace and the target crystal, and the upper surface of the liquid bridge is the solid-liquid interface between the target crystal and the melt corresponding to the target crystal, and the solid-liquid interface is the three-dimensional non-axisymmetric crystallization interface.
[0180] In the embodiment of the present invention, the target crystal is a plate-shaped gallium oxide single crystal, and the melt corresponding to the target crystal is a gallium oxide melt.
[0181] In the crystal growth furnace, the current input into the induction coil is alternating current (AC), and the induction coil is a spiral induction coil. The induction coil can generate induction heating power in the crucible and the post-heater. The crucible in the crystal growth furnace is an iridium crucible, which contains a gallium oxide melt. An iridium mold is fixed in the gallium oxide melt, and a capillary slit is provided in the iridium mold. The gallium oxide melt rises to the top of the mold through the capillary slit in the mold under the capillary action to form a liquid bridge. The liquid bridge forms a plate-shaped gallium oxide crystal under the induction of the seed crystal.
[0182] The atmosphere in the crystal growth furnace is argon, the isodiametric growth rate of the gallium oxide crystal is 10 millimeters per hour (mm / h), the growth direction (z-axis) of the gallium oxide crystal is the
[010] crystal direction, and the width direction (y-axis) of the gallium oxide crystal is the
[001] crystal direction.
[0183] Step S202: The electronic device meshes the target geometric model to obtain a target calculation domain corresponding to the target geometric model.
[0184] Specifically, the electronic device meshes the target geometric model according to the first size target to obtain the target computational domain corresponding to the target geometric model. The computational domain includes hexahedral computational grids and tetrahedral computational grids. Among them, the mold-liquid bridge and the surrounding crystal area are hexahedral grids, and other areas are tetrahedral grids. The size of the hexahedral grid of the liquid bridge part is 0.15mm, and the size of the minimum hexahedral grid of the crystal and mold area is 1mm; the minimum size of the tetrahedral grid in other areas is 1mm and the maximum size is 18mm. The number of computational grids in the entire target computational domain is about 6.7 million.
[0185] It should be noted that the first size includes a first sub-size of a tetrahedral mesh and a second sub-size of a hexahedral mesh in the target computational domain; the first sub-size and the second sub-size may be the same or different.
[0186] In an embodiment of the present invention, the region where the three-dimensional non-axisymmetric crystallization interface is located in the target geometric model can be divided into hexahedral meshes according to the first size, and other regions outside the region where the three-dimensional non-axisymmetric crystallization interface is located in the target geometric model can be divided into tetrahedral meshes, thereby obtaining a target computational domain including tetrahedral meshes and hexahedral meshes. The target computational domain is the computational domain corresponding to the entire target geometric model, and the computational domain may include but is not limited to: the first region corresponding to the crucible, the second region corresponding to the crystallization interface, etc.
[0187] Step S203: The electronic device obtains grid parameters corresponding to the target computing grid and computing domain parameters corresponding to the target computing domain.
[0188] The grid parameters corresponding to the target computational grid include control equations corresponding to the target computational grid; and the control equations include energy conservation equations and radiation transfer equations corresponding to the target computational grid.
[0189] Specifically, in the case of temperature imbalance in the target calculation domain, the electronic device first determines the energy conservation equation corresponding to the target calculation grid according to the dielectric radiation and anisotropic thermal conductivity characteristics inside the gallium oxide crystal, when there is no momentum change and mass change in the gallium oxide crystal region in the target calculation domain, determines the radiation transfer equation corresponding to the target calculation grid according to the absorption characteristics of free carriers in the target crystal, and determines the energy conservation equation and the radiation transfer equation as grid parameters corresponding to the target calculation grid.
[0190] In an embodiment of the present invention, the computational domain parameters corresponding to the target computational domain include thermophysical characteristic parameters corresponding to the target computational domain and boundary conditions and source items corresponding to the target computational domain.
[0191] The thermophysical characteristic parameters corresponding to the target calculation domain include the thermophysical characteristic parameters of the crucible, the thermophysical characteristic parameters of the mold, the thermophysical characteristic parameters of the induction coil, and the thermophysical characteristic parameters of the gallium oxide melt. The thermophysical characteristic parameters include anisotropic thermal conductivity tensor, absorption coefficient, thermal expansion coefficient, specific heat capacity, density, etc.
[0192] In an embodiment of the present invention, the thermophysical characteristic parameters corresponding to the target calculation domain may adopt experimental data obtained by experiments. The experimental data may be published by previous studies or obtained by self-experimental testing, and the embodiment of the present invention is not limited thereto.
[0193] The boundary conditions corresponding to the target computational domain include the temperature and surface emissivity of the contact interface in the target geometric model, and the contact interfaces in the target geometric model are all coupled, no-slip walls. The temperature of the crystal growth furnace wall is set to room temperature 300 K, the surface emissivity of the insulation material and gallium oxide crystal is 0.4, the surface emissivity of the crucible is 0.5, the surface emissivity of the gallium oxide melt is 0.3, and the surface emissivity of the stainless steel furnace wall is 0.21.
[0194] The source terms corresponding to the target computational domain include the induction heating power on the crucible and the additional heat generated by the phase change at the three-dimensional non-axisymmetric crystal interface.
[0195] Step S204: The electronic device performs steady-state calculation on the target calculation domain based on the grid parameters and the calculation domain parameters to obtain the temperature field of the target calculation domain.
[0196] Specifically, the electronic device first inputs the control equation corresponding to the target computational grid obtained in step S203, as well as the thermal physical characteristic parameters, boundary conditions and source terms corresponding to the target computational domain into the target computational domain obtained in step S202; then solves the control equation according to the target geometric model, thermal physical characteristic parameters, boundary conditions and source terms to obtain the temperature field of the target computational domain.
[0197] Step S205: The electronic device determines whether the computational grid in the target computational domain passes the grid independence verification.
[0198] Specifically, the electronic device first obtains the first monitoring data of the temperature field; then compares the first monitoring data with the target monitoring data, wherein the target monitoring data is the monitoring data of the target temperature field, the target temperature field is the temperature field corresponding to the target computing domain determined according to the computing grid of the second size, and the second size is larger than the first size; then, if the first monitoring data is different from the target monitoring data, it indicates that the computing grid in the target computing domain has not passed the grid independence verification, then according to the third size, the corresponding operations of step S202 to step S205 are repeatedly performed until the computing grid in the target computing domain passes the grid independence verification; if the first monitoring data is the same as the target monitoring data, it indicates that the computing grid in the target computing domain passes the grid independence verification, then the corresponding operations of step S206 are continued to be performed. Wherein, the third size is smaller than the first size.
[0199] Step S206: The electronic device obtains a first temperature of a vertex of the three-dimensional non-axisymmetric crystallization interface according to the temperature field, and determines whether the first temperature is equal to a crystal solidification temperature of the gallium oxide crystal.
[0200] Among them, the crystal solidification temperature of gallium oxide crystal is 2080K.
[0201] When the computational grid in the target computational domain passes the grid independence verification and the first temperature is equal to the crystal solidification temperature, it indicates that the temperature at the vertex position of the three-dimensional non-axisymmetric crystallization interface is equal to the crystal solidification temperature of the gallium oxide crystal, that is, the vertex is located in the actual three-dimensional non-axisymmetric crystallization interface, and step S208 can be executed; when the computational grid in the target computational domain passes the grid independence verification and the first temperature is not equal to the crystal solidification temperature, it indicates that the temperature at the vertex position of the three-dimensional non-axisymmetric crystallization interface is not equal to the crystal solidification temperature of the gallium oxide crystal, that is, the vertex is not located in the actual three-dimensional non-axisymmetric crystallization interface, and step S207 is executed.
[0202] Step S207: The electronic device adjusts the furnace temperature of the crystal growth furnace according to the first temperature.
[0203] Specifically, when the first temperature is not equal to the crystal solidification temperature, the electronic device controls the heating power on the crucible by adjusting the current in the induction coil, and repeats the operations corresponding to steps S203 to S206 until the first temperature is equal to the crystal solidification temperature, and continues to execute step S208.
[0204] Among them, when the first temperature is lower than the crystal solidification temperature, it indicates that the temperature at the vertex of the three-dimensional non-axisymmetric crystallization interface is too low, which may easily cause the gallium oxide crystal to separate from the liquid bridge. The current in the induction coil may be increased to increase the furnace temperature of the crystal growth furnace. When the first temperature is higher than the crystal solidification temperature, it indicates that the temperature at the vertex of the three-dimensional non-axisymmetric crystallization interface is too high, which may easily cause the gallium oxide crystal to stick to the mold in the crystal growth furnace. The current in the induction coil may be decreased to reduce the furnace temperature of the crystal growth furnace.
[0205] Step S208: The electronic device determines whether the temperature distribution of the three-dimensional non-axisymmetric crystallization interface is uniform.
[0206] Wherein, when the first temperature of the vertex is equal to the crystal solidification temperature, the electronic device can continue to determine whether the temperature distribution of the three-dimensional non-axisymmetric crystallization interface is uniform.
[0207] Specifically, first, the second temperature of the center point of the target grid surface is obtained according to the temperature field.
[0208] Then, when it is determined that the temperature difference between the second temperature and the first temperature is greater than the first preset threshold, it indicates that the middle temperature of the entire three-dimensional non-axisymmetric crystallization interface is greatly different from the surrounding temperatures, the temperature distribution is uneven, and the temperature of the three-dimensional non-axisymmetric crystallization interface does not meet the preset conditions, then it is necessary to execute steps S209 to S213 to adjust the three-dimensional non-axisymmetric crystallization interface, and repeat the operations corresponding to steps S204 to S208 until the temperature difference between the second temperature and the first temperature is less than or equal to the first preset threshold, that is, when the temperature distribution of the adjusted three-dimensional non-axisymmetric crystallization interface is uniform, it indicates that the temperature of the three-dimensional non-axisymmetric crystallization interface meets the preset conditions, and the operation corresponding to step S214 is executed.
[0209] Step S209: The electronic device uses the main thread to obtain the first coordinates of the target grid nodes in the target grid surface corresponding to each sub-thread, and the second coordinates and the second temperature of the center point of the target grid surface corresponding to the sub-thread.
[0210] Step S210: The electronic device uses the main thread to determine the first coordinate, the second coordinate, and the second temperature corresponding to each target grid surface as a target data group corresponding to the target grid surface.
[0211] Step S211: The electronic device obtains a grid surface identifier of a target grid surface, and sorts the target data group according to the grid surface identifier to obtain calculation parameters of a three-dimensional non-axisymmetric crystallization interface.
[0212] The calculation parameters include target data groups corresponding to each target grid surface.
[0213] Step S212: The electronic device uses the main thread to send the calculation parameters to each sub-thread, and uses the sub-thread to calculate the movement parameters of the target grid node in the target grid surface corresponding to the sub-thread according to the calculation parameters.
[0214] Step S213: The electronic device controls the target grid nodes to move according to the movement parameters of each target grid node to obtain an adjusted three-dimensional non-axisymmetric crystallization interface.
[0215] Specifically, when the temperature of the three-dimensional non-axisymmetric crystallization interface does not meet the preset conditions, the electronic device first obtains the calculation parameters of the three-dimensional non-axisymmetric crystallization interface through steps S209 to S211; then uses the main thread to send the calculation parameters to each sub-thread through step S212, and uses the sub-thread to calculate the movement parameters of the target grid nodes in the target grid surface corresponding to the sub-thread according to the calculation parameters; finally, through step S213, the target grid nodes are controlled to move according to the movement parameters of each target grid node to obtain an adjusted three-dimensional non-axisymmetric crystallization interface.
[0216] Step S214: When the temperature of the electronic device in the target calculation domain is balanced and the temperature of the three-dimensional non-axisymmetric crystallization interface meets a preset condition, the three-dimensional non-axisymmetric crystallization interface is determined as the target crystallization interface.
[0217] Specifically, the target interface is a crystallization interface that is closest to the actual three-dimensional non-axisymmetric crystallization interface between the gallium oxide crystal and the gallium oxide melt determined by the embodiment of the present invention. After determining the target crystallization interface, the growth process of the gallium oxide crystal can be controlled according to the shape of the target crystallization interface. For example, when the shape of the target crystallization interface is as follows: Figure 4 In the case of the concave gallium oxide crystal shown in the figure, the growth process of the gallium oxide crystal can be controlled by improving the structure of the crystal growth furnace body and enhancing the thermal insulation effect of the crystal growth furnace (for example, thickening the thermal insulation layer of the crystal growth furnace, adding a thermal insulation cover to the crucible in the crystal growth furnace, etc.), thereby reducing or avoiding defects such as vacancies and dislocations caused by the crystallization interface of the concave crystal, and improving the quality of the gallium oxide crystal.
[0218] In summary, the method for determining the crystallization interface of crystals grown by the guided mold method provided in the embodiment of the present invention realizes the determination of the three-dimensional non-axisymmetric crystallization interface between the target crystal and the melt corresponding to the target crystal, so that the growth process of the target crystal can be controlled according to the target crystal interface, thereby improving the accuracy of controlling the growth process of the target crystal, and further improving the crystal quality of the target crystal.
[0219] Device Embodiment
[0220] The embodiment of the present invention further provides a device for determining a crystal interface of a crystal grown by a guided mode method, which is applied to an electronic device, wherein the electronic device comprises a main thread and at least two sub-threads controlled by the main thread; Fig. 9 A logic block diagram of a device for determining a crystal interface of a crystal grown by a guided mode method according to the present invention is shown, and the device may include:
[0221] The first calculation module 901 is used to perform steady-state calculation on the target calculation domain to obtain the temperature field of the target calculation domain when the temperature of the target calculation domain is unbalanced; the target calculation domain is a calculation domain obtained by meshing the target geometric model, and the target geometric model includes a three-dimensional non-axisymmetric crystallization interface between a target crystal grown by a guided mode method and a melt corresponding to the target crystal; the target calculation domain includes at least two target mesh surfaces constituting the three-dimensional non-axisymmetric crystallization interface, and each of the sub-threads corresponds to at least one of the target mesh surfaces;
[0222] The first determination module 902 is used to determine whether the temperature of the three-dimensional non-axisymmetric crystallization interface meets a preset condition according to the temperature field, and to obtain the calculation parameters of the three-dimensional non-axisymmetric crystallization interface using the main thread when the temperature of the three-dimensional non-axisymmetric crystallization interface does not meet the preset condition; the preset condition is that the temperature of the three-dimensional non-axisymmetric crystallization interface is uniform and reaches the crystal solidification temperature of the target crystal;
[0223] The second calculation module 903 is used to send the calculation parameters to each of the sub-threads by using the main thread, and calculate the movement parameters of the target grid nodes in the target grid surface corresponding to the sub-thread according to the calculation parameters by using the sub-thread; the target grid nodes in the target grid surface corresponding to each of the sub-threads are different from each other;
[0224] A control module 904 is used to control the target grid nodes to move according to the movement parameters of each target grid node to obtain an adjusted three-dimensional non-axisymmetric crystallization interface;
[0225] The second determination module 905 is used to determine the three-dimensional non-axisymmetric crystallization interface as a target crystallization interface when the temperature of the target calculation domain is balanced and the temperature of the three-dimensional non-axisymmetric crystallization interface meets the preset condition.
[0226] Optionally, the three-dimensional non-axisymmetric crystallization interface includes a vertex and a center point of the target mesh surface; and the first determination module includes:
[0227] A first determination submodule, used for determining a first temperature of the vertex according to the temperature field;
[0228] A first acquisition submodule, configured to acquire a second temperature of the center point according to the temperature field when the first temperature is equal to the crystal solidification temperature;
[0229] A second determination submodule, configured to determine that the temperature of the three-dimensional non-axisymmetric crystallization interface meets a preset condition when the temperature difference between the second temperature and the first temperature is less than or equal to a first preset threshold;
[0230] The third determination submodule is used to determine that the temperature of the three-dimensional non-axisymmetric crystallization interface does not meet the preset condition when the temperature difference between the second temperature and the first temperature is greater than the first preset threshold.
[0231] Optionally, the target geometric model includes a crystal growth furnace, and the crystal growth furnace is used to grow the target crystal by a guided mode method; the first determination module also includes:
[0232] The adjusting submodule is used to adjust the furnace temperature of the crystal growth furnace according to the first temperature when the first temperature is not equal to the crystal solidification temperature.
[0233] Optionally, the first determining module includes:
[0234] A second acquisition submodule is used for, when the temperature of the three-dimensional non-axisymmetric crystallization interface does not meet the preset condition, using the main thread to acquire the first coordinates of the target grid nodes in the target grid surface corresponding to each of the sub-threads, and the second coordinates and the second temperature of the center point of the target grid surface corresponding to the sub-thread;
[0235] A fourth determination submodule is used to use the main thread to determine the first coordinate, the second coordinate and the second temperature corresponding to each of the target grid surfaces as a target data group corresponding to the target grid surface;
[0236] The third acquisition submodule is used to obtain the grid surface identifier of the target grid surface, and sort the target data group according to the grid surface identifier to obtain the calculation parameters of the three-dimensional non-axisymmetric crystallization interface; the calculation parameters include the target data group corresponding to each of the target grid surfaces.
[0237] Optionally, the calculation parameters include first coordinates of target grid nodes in each of the target grid surfaces, and second coordinates and second temperatures of the center points of the target grid surfaces; the second calculation module includes:
[0238] The first calculation submodule is used to calculate the movement parameters of the target grid nodes in the target grid surface corresponding to the subthread according to the first coordinates of the target grid nodes in each of the target grid surfaces and the second coordinates and the second temperature of the center point of the target grid surface by using the subthread:
[0239] ;
[0240] in, represents the movement parameters of the target grid node; A mesh face identifier representing a target mesh face around a target mesh node; Indicates the total number of target mesh faces around the target mesh node; Indicates The second temperature of the center point of the target grid surface; Indicates The distance between the second coordinate of the center point of the target mesh surface and the first coordinate of the target mesh node; Indicates the crystal solidification temperature of the target crystal; Represents the movement coefficient, which is used to adjust the moving distance of the target grid node.
[0241] Optionally, the target computational domain includes a computational grid obtained by meshing the target geometric model, and the computational grid includes the target grid surface; the moving distance indicated by the movement parameter is smaller than the side length of the computational grid adjacent to the target grid node in the moving direction indicated by the movement parameter.
[0242] Optionally, the target computational domain includes a computational grid obtained by meshing the target geometric model, and the computational grid includes a target computational grid where the target grid surface is located; the first computational module includes:
[0243] A fourth acquisition submodule is used to acquire, when the temperature of the target computational domain is unbalanced, grid parameters corresponding to the target computational grid and computational domain parameters corresponding to the target computational domain; the grid parameters include parameters for characterizing dielectric radiation inside the target crystal;
[0244] The second calculation submodule is used to perform steady-state calculation on the target calculation domain based on the grid parameters and the calculation domain parameters to obtain the temperature field of the target calculation domain.
[0245] Optionally, the fourth acquisition submodule includes:
[0246] A first determination unit is used to determine the energy conservation equation corresponding to the target calculation grid according to the medium radiation and anisotropic thermal conductivity characteristics inside the target crystal, when there is no momentum change and mass change in the target crystal region in the target calculation domain;
[0247] A second determining unit is used to determine the radiation transfer equation corresponding to the target calculation grid according to the absorption characteristics of free carriers in the target crystal;
[0248] The third determining unit is used to determine the energy conservation equation and the radiation transfer equation as grid parameters corresponding to the target calculation grid.
[0249] Optionally, the target computational domain includes a computational grid obtained by meshing the target geometric model, the computational grid includes the target grid surface, and the size of the computational grid is a first size; the device further includes:
[0250] An acquisition module, used for acquiring first monitoring data of the temperature field;
[0251] a comparison module, configured to compare the first monitoring data with target monitoring data; the target monitoring data is monitoring data of a target temperature field, the target temperature field is a temperature field corresponding to a target calculation domain determined according to a calculation grid of a second size, the second size being larger than the first size; the second size is a size of a calculation grid obtained by meshing the target geometric model again before obtaining a calculation grid of the first size after meshing the target geometric model;
[0252] A meshing module, for re-meshing the target geometric model according to a third size to obtain a target computational domain corresponding to the target geometric model when the first monitoring data is different from the target monitoring data; the third size is smaller than the first size; the third size is the size of a computational grid obtained by meshing the target geometric model again after meshing the target geometric model to obtain a computational grid of the first size;
[0253] An execution module is used to execute an operation of determining whether the temperature of the three-dimensional non-axisymmetric crystallization interface meets a preset condition according to the temperature field when the first monitoring data is the same as the target monitoring data.
[0254] As for the device embodiment, since it is basically similar to the method embodiment, the description is relatively simple, and the relevant parts can be referred to the partial description of the method embodiment.
[0255] The various embodiments in this specification are described in a progressive manner, and each embodiment focuses on the differences from other embodiments. The same or similar parts between the various embodiments can be referenced to each other.
[0256] An embodiment of the present invention further provides an electronic device, comprising a memory and a processor, wherein the memory is used to store a computer program, and the processor is used to implement the method for determining the crystallization interface of a crystal grown by a guided mode method as described above when executing the computer program.
[0257] An embodiment of the present invention further provides a readable storage medium, wherein the readable storage medium stores a computer program, and when the computer program is executed by a processor, the method for determining a crystallization interface of a crystal grown by a guided mode method as described above is implemented.
[0258] The various embodiments in this specification are described in a progressive manner, and each embodiment focuses on the differences from other embodiments. The same or similar parts between the various embodiments can be referenced to each other.
[0259] It will be appreciated by those skilled in the art that the embodiments of the present invention may be provided as methods, devices, or computer program products. Therefore, the embodiments of the present invention may take the form of a complete hardware embodiment, a complete software embodiment, or an embodiment combining software and hardware. Moreover, the embodiments of the present invention may take the form of a computer program product implemented on one or more computer-usable storage media (including but not limited to disk storage, CD-ROM, optical storage, etc.) containing computer-usable program codes.
[0260] The embodiments of the present invention are described with reference to the flowcharts and / or block diagrams of the methods, terminal devices (systems), and computer program products according to the embodiments of the present invention. It should be understood that each process and / or block in the flowchart and / or block diagram, as well as the combination of the processes and / or blocks in the flowchart and / or block diagram, can be implemented by computer program instructions. These computer program instructions can be provided to a processor of a general-purpose computer, a special-purpose computer, an embedded processor, or other programmable data processing terminal device to generate a machine, so that the instructions executed by the processor of the computer or other programmable data processing terminal device generate instructions for implementing the processes in the flowchart and / or block diagram. Figure 1 A process or multiple processes and / or boxes Figure 1 A device that provides the functions specified in a block or multiple blocks.
[0261] These computer program instructions may also be stored in a computer readable memory capable of directing a computer or other programmable data processing terminal device to operate in a predictable manner, so that the instructions stored in the computer readable memory produce a manufactured product including an instruction device, which implements the process Figure 1A process or multiple processes and / or boxes Figure 1 A function specified in one or more boxes.
[0262] These computer program instructions can also be loaded onto a computer or other programmable data processing terminal device so that a series of operating steps are executed on the computer or other programmable terminal device to produce a computer-implemented process, thereby providing instructions for executing on the computer or other programmable terminal device to implement the process. Figure 1 A process or multiple processes and / or boxes Figure 1 The steps for the functions specified in one or more boxes.
[0263] Although the preferred embodiments of the present invention have been described, those skilled in the art may make additional changes and modifications to these embodiments once they have learned the basic creative concept. Therefore, the appended claims are intended to be interpreted as including the preferred embodiments and all changes and modifications that fall within the scope of the embodiments of the present invention.
[0264] Finally, it should be noted that, in this article, relational terms such as first and second, etc. are only used to distinguish one entity or operation from another entity or operation, and do not necessarily require or imply any such actual relationship or order between these entities or operations. Moreover, the terms "include", "comprise" or any other variants thereof are intended to cover non-exclusive inclusion, so that a process, method, article or terminal device including a series of elements includes not only those elements, but also other elements not explicitly listed, or also includes elements inherent to such process, method, article or terminal device. In the absence of further restrictions, the elements defined by the sentence "comprise a ..." do not exclude the existence of other identical elements in the process, method, article or terminal device including the elements.
[0265] The above is a detailed introduction to the method and device for determining the crystallization interface of a crystal grown by a guided mode method provided by the present invention. Specific examples are used herein to illustrate the principles and implementation methods of the present invention. The description of the above embodiments is only used to help understand the method of the present invention and its core idea. At the same time, for a person skilled in the art, according to the idea of the present invention, there will be changes in the specific implementation method and application scope. In summary, the content of this specification should not be understood as a limitation on the present invention.
Claims
1. A method for determining the crystallization interface of a crystal grown by a guided mode method, characterized in that: Applied to an electronic device, the electronic device comprises a main thread and at least two sub-threads controlled by the main thread; the method comprises: In the case of temperature imbalance in the target computational domain, a steady-state calculation is performed on the target computational domain to obtain a temperature field of the target computational domain; the target computational domain is a computational domain obtained by meshing a target geometric model, the target geometric model comprising a three-dimensional non-axisymmetric crystallization interface between a target crystal grown by a guided mode method and a melt corresponding to the target crystal; the target computational domain comprises at least two target mesh surfaces constituting the three-dimensional non-axisymmetric crystallization interface, and each of the subthreads corresponds to at least one of the target mesh surfaces; According to the temperature field, determining whether the temperature of the three-dimensional non-axisymmetric crystallization interface meets a preset condition, and when the temperature of the three-dimensional non-axisymmetric crystallization interface does not meet the preset condition, using the main thread to obtain the calculation parameters of the three-dimensional non-axisymmetric crystallization interface; the preset condition is that the temperature of the three-dimensional non-axisymmetric crystallization interface is uniform and reaches the crystal solidification temperature of the target crystal; The main thread is used to send the calculation parameters to each of the sub-threads, and the sub-threads are used to calculate the movement parameters of the target grid nodes in the target grid surface corresponding to the sub-threads according to the calculation parameters; the target grid nodes in the target grid surface corresponding to each of the sub-threads are different from each other; According to the movement parameters of each of the target grid nodes, the target grid nodes are controlled to move to obtain an adjusted three-dimensional non-axisymmetric crystallization interface; When the temperature of the target calculation domain is balanced and the temperature of the three-dimensional non-axisymmetric crystallization interface meets the preset condition, the three-dimensional non-axisymmetric crystallization interface is determined as the target crystallization interface.
2. The method according to claim 1, characterized in that The three-dimensional non-axisymmetric crystallization interface includes a vertex and a center point of the target mesh surface; and determining whether the temperature of the three-dimensional non-axisymmetric crystallization interface meets a preset condition according to the temperature field includes: Determining a first temperature of the vertex according to the temperature field; When the first temperature is equal to the solidification temperature of the crystal, obtaining a second temperature of the center point according to the temperature field; When the temperature difference between the second temperature and the first temperature is less than or equal to a first preset threshold, determining that the temperature of the three-dimensional non-axisymmetric crystallization interface meets a preset condition; In a case where the temperature difference between the second temperature and the first temperature is greater than the first preset threshold, it is determined that the temperature of the three-dimensional non-axisymmetric crystallization interface does not satisfy the preset condition.
3. The method according to claim 2, characterized in that The target geometric model includes a crystal growth furnace, and the crystal growth furnace is used to grow the target crystal by a guided mode method; the method also includes: When the first temperature is not equal to the crystal solidification temperature, the furnace temperature of the crystal growth furnace is adjusted according to the first temperature.
4. The method according to claim 1, characterized in that: When the temperature of the three-dimensional non-axisymmetric crystallization interface does not meet the preset condition, using the main thread to obtain the calculation parameters of the three-dimensional non-axisymmetric crystallization interface includes: When the temperature of the three-dimensional non-axisymmetric crystallization interface does not meet the preset condition, using the main thread to obtain the first coordinates of the target grid nodes in the target grid surface corresponding to each of the sub-threads, and the second coordinates and the second temperature of the center point of the target grid surface corresponding to the sub-thread; Using the main thread, determining the first coordinate, the second coordinate and the second temperature corresponding to each of the target grid surfaces as a target data group corresponding to the target grid surface; The grid surface identifier of the target grid surface is obtained, and the target data group is sorted according to the grid surface identifier to obtain the calculation parameters of the three-dimensional non-axisymmetric crystallization interface; the calculation parameters include the target data group corresponding to each of the target grid surfaces.
5. The method according to claim 1, characterized in that The calculation parameters include first coordinates of target grid nodes in each of the target grid surfaces, and second coordinates and second temperatures of the center points of the target grid surfaces; The using the sub-thread to calculate the movement parameters of the target mesh node in the target mesh surface corresponding to the sub-thread according to the calculation parameters includes: Using the subthread, according to the first coordinates of the target grid nodes in each of the target grid surfaces and the second coordinates and the second temperature of the center point of the target grid surface, the movement parameters of the target grid nodes in the target grid surface corresponding to the subthread are calculated as follows: ; in, represents the movement parameters of the target grid node; A mesh face identifier representing a target mesh face around a target mesh node; Indicates the total number of target mesh faces around the target mesh node; Indicates The second temperature of the center point of the target grid surface; Indicates The distance between the second coordinate of the center point of the target mesh surface and the first coordinate of the target mesh node; Indicates the crystal solidification temperature of the target crystal; Represents the movement coefficient, which is used to adjust the moving distance of the target grid node.
6. The method according to claim 1, characterized in that The target computational domain includes a computational grid obtained by meshing the target geometric model, and the computational grid includes the target grid surface; the moving distance indicated by the movement parameter is smaller than the side length of the computational grid adjacent to the target grid node in the moving direction indicated by the movement parameter.
7. The method according to claim 1, characterized in that The target computational domain includes a computational grid obtained by meshing the target geometric model, and the computational grid includes a target computational grid where the target grid surface is located; In the case where the temperature of the target computing domain is unbalanced, performing steady-state calculation on the target computing domain to obtain the temperature field of the target computing domain includes: In the case where the temperature of the target computational domain is unbalanced, obtaining grid parameters corresponding to the target computational grid and computational domain parameters corresponding to the target computational domain; the grid parameters include parameters for characterizing dielectric radiation inside the target crystal; Based on the grid parameters and the computational domain parameters, a steady-state calculation is performed on the target computational domain to obtain a temperature field of the target computational domain.
8. The method according to claim 7, characterized in that The obtaining of the grid parameters corresponding to the target computing grid includes: According to the dielectric radiation and anisotropic thermal conductivity characteristics inside the target crystal, in the case where there is no momentum change and mass change in the target crystal region in the target calculation domain, determining the energy conservation equation corresponding to the target calculation grid; Determining a radiation transfer equation corresponding to the target computational grid according to the absorption characteristics of free carriers in the target crystal; The energy conservation equation and the radiation transfer equation are determined as grid parameters corresponding to the target calculation grid.
9. The method according to claim 1, characterized in that: The target computational domain includes a computational grid obtained by meshing the target geometric model, the computational grid includes the target grid surface, and the size of the computational grid is a first size; Before determining whether the temperature of the three-dimensional non-axisymmetric crystallization interface meets a preset condition according to the temperature field, the method further includes: Acquiring first monitoring data of the temperature field; Compare the first monitoring data with target monitoring data; the target monitoring data is monitoring data of a target temperature field, the target temperature field is a temperature field corresponding to a target calculation domain determined according to a calculation grid of a second size, the second size being larger than the first size; the second size is the size of a calculation grid obtained by meshing the target geometric model again before obtaining a calculation grid of the first size after meshing the target geometric model; In the case where the first monitoring data is different from the target monitoring data, the target geometric model is re-meshed according to a third size to obtain a target computational domain corresponding to the target geometric model; the third size is smaller than the first size; the third size is the size of a computational grid obtained by meshing the target geometric model again after the computational grid of the first size is obtained by meshing the target geometric model; In a case where the first monitoring data is the same as the target monitoring data, an operation of determining whether the temperature of the three-dimensional non-axisymmetric crystallization interface meets a preset condition is performed according to the temperature field.
10. A device for determining a crystal interface of a crystal grown by a guided mode method, characterized in that: Applied to an electronic device, the electronic device comprises a main thread and at least two sub-threads controlled by the main thread; the device comprises: A first calculation module is used to perform steady-state calculation on the target calculation domain to obtain the temperature field of the target calculation domain when the temperature of the target calculation domain is unbalanced; the target calculation domain is a calculation domain obtained after meshing the target geometric model, and the target geometric model includes a three-dimensional non-axisymmetric crystallization interface between a target crystal grown by a guided mode method and a melt corresponding to the target crystal; the target calculation domain includes at least two target mesh surfaces constituting the three-dimensional non-axisymmetric crystallization interface, and each of the sub-threads corresponds to at least one of the target mesh surfaces; A first determination module is used to determine whether the temperature of the three-dimensional non-axisymmetric crystallization interface meets a preset condition according to the temperature field, and to obtain calculation parameters of the three-dimensional non-axisymmetric crystallization interface using the main thread when the temperature of the three-dimensional non-axisymmetric crystallization interface does not meet the preset condition; the preset condition is that the temperature of the three-dimensional non-axisymmetric crystallization interface is uniform and reaches the crystal solidification temperature of the target crystal; A second calculation module is used to send the calculation parameters to each of the sub-threads by using the main thread, and calculate the movement parameters of the target grid nodes in the target grid surface corresponding to the sub-thread according to the calculation parameters by using the sub-thread; the target grid nodes in the target grid surface corresponding to each of the sub-threads are different from each other; A control module, used for controlling the target grid nodes to move according to the movement parameters of each target grid node, so as to obtain an adjusted three-dimensional non-axisymmetric crystallization interface; The second determination module is used to determine the three-dimensional non-axisymmetric crystallization interface as a target crystallization interface when the temperature of the target calculation domain is balanced and the temperature of the three-dimensional non-axisymmetric crystallization interface meets the preset condition.
Citation Information
Patent Citations
Solid-liquid interface control method for growing gallium oxide crystal by utilization of pulling method
CN106048723A
Method for quickly growing rare earth crystal optical fiber by utilizing micro-pulling-down method
CN109326333A
Forward modeling method, device and equipment for three-dimensional steady-state heat conduction ground temperature field and medium
CN114036805A
Heating power matching method, device and equipment for gallium oxide single crystal growth
CN118147750A
Method and System for Controlling Temperature during Crystal Growth