Annealing device for high-strength alloy steel shaft forgings and use method thereof

By using adjustable positioning components and displacement mechanisms in the annealing device, combined with heat-absorbing layers and sealing grooves, the problems of unstable clamping and uneven heating of forgings with complex shapes in traditional annealing devices are solved, achieving uniform annealing and high efficiency of forgings. Heating improves the consistency of material properties and product quality.

CN118600191BActive Publication Date: 2024-10-01SHANXI TIANBAO GRP CO LTD
View PDF 10 Cites 0 Cited by

Patent Information

Application Number
CN202411082042.4
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2024-08-08
Publication Date
2024-10-01
Estimated Expiration
2044-08-08

AI Technical Summary

Technical Problem

When traditional annealing equipment handles shaft forgings with complex shapes and variable sizes, problems are prone to unstable clamping and uneven heating. In particular, it is difficult to adaptively heat the thicker steel shaft parts, which affects the consistency of material properties. .

Method used

An annealing device including a first annealing furnace and a sliding second annealing furnace is designed. Through adjustable positioning components and displacement mechanisms, it can automatically adapt to forgings of different diameters, ensuring stable clamping and achieving uniform annealing. The positioning component consists of an annular hollow disk, a threaded rod and an arc-shaped clamping plate, combined with a heat-absorbing layer and a sealing groove, to achieve high-temperature heating of the thicker part of the forging.

Benefits of technology

Through the cooperation of precise positioning components and displacement mechanisms, uniform annealing of forgings is achieved, improving the consistency of material properties, energy saving and high efficiency, and reducing heat loss through sealing grooves and heat-absorbing layers, ensuring the temperature uniformity of the annealing process and product quality.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118600191B_ABST
    Figure CN118600191B_ABST
Patent Text Reader

Abstract

The invention discloses an annealing device for high-strength alloy steel shaft forgings and a use method thereof, and relates to the technical field of forging annealing, comprising a first annealing furnace and a second annealing furnace slidably installed at the rear side of the first annealing furnace, a bracket for supporting is provided below the first annealing furnace, a connecting ring is provided at the connection between the first annealing furnace and the second annealing furnace, a side of the second annealing furnace away from the first annealing furnace is connected to the first annealing furnace through a displacement mechanism, the displacement mechanism comprises an external ring located at a side of the second annealing furnace away from the first annealing furnace, a plurality of slide rails are distributed circumferentially on the first annealing furnace, each slide rail is provided with an electric slider, each electric slider is provided with a connecting frame for connecting with the external ring on the second annealing furnace, a group of positioning components are provided in the first annealing furnace and the second annealing furnace, and the invention can automatically adapt to forgings of different diameters through an adjustable positioning component, ensure stable clamping, and achieve uniform annealing.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of forging annealing, and in particular to an annealing device for high-strength alloy steel shaft forgings and a use method thereof. Background Art

[0002] Annealing is an important part of metal processing, which aims to eliminate the internal stress of the material and improve its mechanical properties. In traditional processes, for shaft forgings with complex shapes and variable sizes, annealing equipment often faces problems such as poor adaptability, uneven heating, and insufficient sealing, which affect the quality of the final product and production efficiency.

[0003] However, existing annealing devices are prone to problems such as unstable clamping and uneven annealing when used for steel shaft forgings of different diameters. In particular, it is difficult to adaptively identify and heat the thicker parts of the steel shaft, which affects the consistency of material properties. Summary of the invention

[0004] In order to solve the above technical problems, the present invention provides an annealing device for high-strength alloy steel shaft forgings and a method of using the same. Through an adjustable positioning component, the device can automatically adapt to forgings of different diameters, ensure stable clamping, and achieve uniform annealing.

[0005] To achieve the above object, the present invention provides the following technical solution: an annealing device for high-strength alloy steel shaft forgings, comprising a first annealing furnace and a second annealing furnace slidably installed at the rear side of the first annealing furnace, wherein a support for supporting is provided below the first annealing furnace;

[0006] A connecting ring is provided at the connection between the first annealing furnace and the second annealing furnace;

[0007] The side of the second annealing furnace away from the first annealing furnace is connected to the first annealing furnace through a displacement mechanism;

[0008] The displacement mechanism comprises an external ring located at a side of the second annealing furnace away from the first annealing furnace, a plurality of slide rails are distributed on the circumference of the first annealing furnace, each of the slide rails is provided with an electric slider, and each of the electric sliders is provided with a connecting frame for connecting with the external ring on the second annealing furnace;

[0009] The outer diameter of the second annealing furnace is smaller than the inner diameter of the first annealing furnace, and the first annealing furnace and the second annealing furnace are arranged in a concentric structure, and the second annealing furnace can be moved to the inside of the first annealing furnace by a displacement mechanism;

[0010] A group of positioning components are provided in each of the first annealing furnace and the second annealing furnace.

[0011] Preferably, the positioning assembly includes an annular hollow disk, and the hollow disk and the first annealing furnace and the second annealing furnace are all concentric structures. The outer wall of the hollow disk is provided with a plurality of fixing columns connected to the inner wall of the annealing furnace, and the surface of the hollow disk facing the outside of the first annealing furnace is provided with a plurality of groups of circumferentially distributed engaging grooves, and rotatable threaded sleeves are provided on both sides of the engaging grooves, and each of the threaded sleeves is provided with a threaded rod threadedly matched therewith, and the bottoms of the two adjacent threaded rods are connected to the same arc-shaped clamping plate located directly below them.

[0012] Preferably, the arc-shaped clamping plates are provided in four groups, and the four groups of arc-shaped clamping plates are moved closer to or farther away from each other under the action of the threaded rod to match steel shaft forgings of different diameters, thereby increasing the adaptability of the device during clamping.

[0013] Preferably, the positioning assembly located inside the first annealing furnace has a circumferential surface facing the second annealing furnace provided with a positioning block corresponding to the position of the interlocking groove on the positioning assembly located inside the second annealing furnace, and each of the positioning blocks is provided with a straight rod corresponding to the interlocking groove on the positioning assembly provided in the second annealing furnace. When the second annealing furnace moves toward the direction of the positioning assembly located in the first annealing furnace under the action of the displacement mechanism, the straight rod on the positioning assembly located in the first annealing furnace can be inserted into the interlocking groove on the positioning assembly located in the second annealing furnace. During the insertion process, the straight rod drives the threaded sleeve to rotate, so that the threaded rod on the positioning assembly located in the second annealing furnace can continuously approach the center of the hollow disk under the action of the threaded sleeve, thereby making the arc-shaped clamping plates connected thereto approach each other to clamp the steel shaft forging located in the second annealing furnace.

[0014] Preferably, the inner diameter of the hollow disk in the positioning assembly located in the first annealing furnace is smaller than the inner diameter of the hollow disk in the positioning assembly located in the second annealing furnace. When the forging enters the second annealing furnace from the first annealing furnace, the thicker part of the forging can be clamped by the positioning assembly on the second annealing furnace, and the inner diameter of the second annealing furnace is smaller than that of the first annealing furnace. Therefore, the thicker part of the forging located in the second annealing furnace can be better heated at a relatively high temperature, thereby ensuring that different parts of the forging are annealed to different degrees, so as to achieve uniformity of the overall annealing of the forging.

[0015] Preferably, a plurality of circumferentially distributed sealing grooves are provided at the port of the first annealing furnace away from the second annealing furnace, and a closing cover hinged on the first annealing furnace and capable of closing the first annealing furnace is provided near the sealing grooves. The closing cover is provided with a plurality of sealing rings matched with the sealing grooves. When the closing cover covers the port of the first annealing furnace, the sealing rings can be embedded in the sealing grooves to increase the sealing performance of the port of the first annealing furnace.

[0016] Preferably, a plurality of groups of bosses corresponding to the positions of the interlocking grooves in the positioning assembly in the first annealing furnace are installed on the surface of the closing cover facing the first annealing furnace. When the closing cover closes the first annealing furnace, the bosses can be inserted into the interlocking grooves on the positioning assembly in the first annealing furnace, driving the threaded sleeve to rotate, so that the threaded rod pushes the arc-shaped clamping plate to fix and clamp the steel shaft forging in the first annealing furnace.

[0017] Preferably, the first annealing furnace and the second annealing furnace both include an outer wall and an inner wall, an insulating layer is provided between the outer wall and the inner wall in the first annealing furnace, and a heat absorption layer is provided between the outer wall and the inner wall in the second annealing furnace, so that when the second annealing furnace is in the first annealing furnace, it absorbs the heat of the first annealing furnace plus the heat of the second annealing furnace so that the temperature in the second annealing furnace is higher than the internal temperature of the first annealing furnace without increasing external heating. At the same time, the inner diameter of the second annealing furnace is smaller than that of the first annealing furnace, so that the heat source can be more concentrated, thereby more evenly heating the thicker part of the steel shaft forging in the second annealing furnace.

[0018] A method for using an annealing device for high-strength alloy steel shaft forgings comprises the following steps:

[0019] S1. Place the high-strength alloy steel shaft forging to be annealed on the positioning assembly in the first annealing furnace, close the closing cover on the port of the first annealing furnace through the hinge mechanism, and ensure that the sealing ring is completely embedded in the sealing groove to increase the sealing performance of the first annealing furnace. At this time, the convex column on the closing cover will be inserted into the fitting groove of the positioning assembly in the first annealing furnace to achieve preliminary clamping of the steel shaft forging;

[0020] S2. After the initial clamping, the electric slider on the displacement mechanism moves on the slide rail to slide the second annealing furnace into the first annealing furnace. The interlocking groove in the positioning assembly in the second annealing furnace cooperates with the straight rod in the first annealing furnace. The straight rod in the first annealing furnace will be inserted into the interlocking groove of the positioning assembly in the second annealing furnace, and drive the threaded sleeve to rotate, so that the threaded rod in the second annealing furnace approaches the center of the hollow disk, and then the arc-shaped clamping plates are close to each other. When the forging is placed, the thicker end of the forging is located in the second annealing furnace, clamping the thicker part of the steel shaft forging in the second annealing furnace. At the same time, the second annealing furnace moves closer to the port of the first annealing furnace, and the clamping diameter is smaller. Therefore, the external displacement mechanism can be controlled to position and clamp the thicker part of the steel shaft forging required for annealing;

[0021] S3. After the position is fixed, start the first annealing furnace and the second annealing furnace, and perform annealing according to the predetermined annealing temperature and time. The heat absorption layer in the second annealing furnace will absorb the heat of the first annealing furnace, and work together with its own heating system to perform relatively high-temperature annealing on the thicker part of the steel shaft forging. Since the inner diameter of the second annealing furnace is smaller, the heat source is more concentrated, and the thicker part of the forging can be heated more evenly;

[0022] S4. After annealing is completed, the second annealing furnace moves away from the port of the first annealing furnace to loosen the arc clamping plate, and then the closing cover of the first annealing furnace is opened to take out the annealed steel shaft forging.

[0023] Compared with the prior art, the present invention has the following beneficial effects:

[0024] 1. The present invention includes a positioning assembly, which can not only adapt to steel shaft forgings of different diameters by adjusting the threaded rod and the arc-shaped clamping plate to achieve a stable clamping of the forgings, but also realize the precise sliding docking of the second annealing furnace to the first annealing furnace through the displacement mechanism, thereby enhancing the processing capacity of the same steel shaft forgings with a gradually changing diameter and ensuring the uniformity of the annealing process. The most important thing is the cooperation between the positioning assembly and the displacement mechanism. The engaging groove in the positioning assembly in the second annealing furnace cooperates with the straight rod in the first annealing furnace. The closer the second annealing furnace is to the port of the first annealing furnace, the smaller the diameter of the steel shaft clamped by the positioning assembly in the second annealing furnace. Therefore, by controlling the external displacement mechanism, the part of the steel shaft that needs to be precisely heated can be precisely controlled, which is particularly suitable for the thicker part of the steel shaft forging, thereby improving the accuracy of annealing of the forging.

[0025] 2. In the present invention, the inner diameter of the second annealing furnace is smaller than that of the first annealing furnace, and a heat absorption layer is provided inside, so that it can absorb more heat when in the first annealing furnace, and achieve a heating effect with a temperature higher than that of the first annealing furnace. Such a design does not require additional external heating, which is both energy-saving and efficient. At the same time, the small inner diameter helps to concentrate the heat source, and the thicker part of the forging can be heated more concentratedly and evenly.

[0026] 3. The sealing groove provided at the port of the first annealing furnace in the present invention is combined with the sealing ring on the closing cover, which effectively enhances the sealing of the furnace body, reduces heat loss, and ensures the stability of the temperature in the furnace, which is very important for controlling the temperature uniformity and product quality during the annealing process. BRIEF DESCRIPTION OF THE DRAWINGS

[0027] In order to make the contents of the present invention more clearly understood, the present invention is further described in detail below based on specific embodiments in conjunction with the accompanying drawings.

[0028] Figure 1 It is a schematic diagram of the overall structure of the present invention;

[0029] Figure 2 It is a rear view of the present invention;

[0030] Figure 3 A cross-sectional view of a first annealing furnace and a second annealing furnace in the present invention;

[0031] Figure 4 It is a structural schematic diagram of the positioning component in the present invention;

[0032] Figure 5 It is a schematic diagram of the structural installation of the interlocking groove of the positioning component in the present invention.

[0033] In the figure: 1. first annealing furnace; 101. bracket; 2. second annealing furnace; 3. connecting ring; 4. displacement mechanism; 401. external ring; 402. slide rail; 403. electric slider; 404. connecting frame; 5. positioning assembly; 501. hollow disk; 502. fixing column; 503. fitting groove; 504. threaded sleeve; 5041. threaded rod; 505. arc clamping plate; 6. positioning block; 7. straight rod; 8. sealing groove; 9. closing cover; 901. sealing ring; 10. convex column; 11. heat insulation layer; 12. heat absorption layer. DETAILED DESCRIPTION

[0034] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0035] See also Figures 1 to 3 , an annealing device for high-strength alloy steel shaft forgings, comprising a first annealing furnace 1 and a second annealing furnace 2 slidably mounted on the rear side of the first annealing furnace 1, wherein a support bracket 101 is provided below the first annealing furnace 1;

[0036] A connecting ring 3 is provided at the connection between the first annealing furnace 1 and the second annealing furnace 2;

[0037] The side of the second annealing furnace 2 away from the first annealing furnace 1 is connected to the first annealing furnace 1 through a displacement mechanism 4;

[0038] The displacement mechanism 4 comprises an external ring 401 located on the side of the second annealing furnace 2 away from the first annealing furnace 1, a plurality of slide rails 402 are distributed circumferentially on the first annealing furnace 1, each of the slide rails 402 is provided with an electric slider 403, and each of the electric sliders 403 is provided with a connecting frame 404 for connecting with the external ring 401 on the second annealing furnace 2;

[0039] The outer diameter of the second annealing furnace is smaller than the inner diameter of the first annealing furnace 1, and the first annealing furnace 1 and the second annealing furnace 2 are arranged in a concentric structure, and the second annealing furnace 2 can be moved to the inside of the first annealing furnace 1 by the displacement mechanism 4;

[0040] A set of positioning components 5 is disposed in each of the first annealing furnace 1 and the second annealing furnace 2 .

[0041] See also Figure 3 and Figure 4 Preferably, the positioning assembly 5 includes a ring-shaped hollow disk 501, and the hollow disk 501 is arranged in a concentric structure with the first annealing furnace 1 and the second annealing furnace 2. The outer wall of the hollow disk 501 is provided with a plurality of fixing columns 502 connected to the inner wall of the annealing furnace. The surface of the hollow disk 501 facing the outside of the first annealing furnace 1 is provided with a plurality of groups of circumferentially distributed engaging grooves 503, and rotatable threaded sleeves 504 are provided on both sides of the engaging grooves 503. Each of the threaded sleeves 504 is provided with a threaded rod 5041 threadably matched therewith, and the bottoms of the two adjacent threaded rods 5041 are connected to the same arc-shaped clamping plate 505 located directly below them.

[0042] See also Figure 4 Preferably, the arc-shaped clamping plates 505 are provided with four groups and the four groups of arc-shaped clamping plates 505 are moved closer to or farther away from each other under the action of the threaded rod 5041 to match steel shaft forgings of different diameters, thereby increasing the adaptability of the device during clamping.

[0043] See also Figure 3 , Figure 4 and Figure 5 Preferably, the positioning assembly 5 located inside the first annealing furnace 1 has a circumferential surface facing the second annealing furnace 2 provided with a positioning block 6 corresponding to the position of the fitting groove 503 on the positioning assembly 5 located inside the second annealing furnace 2, and each of the positioning blocks 6 is provided with a straight rod 7 corresponding to the fitting groove 503 on the positioning assembly 5 provided in the second annealing furnace 2.

[0044] It should be noted that when the second annealing furnace 2 moves toward the positioning assembly 5 located in the first annealing furnace 1 under the action of the displacement mechanism 4, the straight rod 7 on the positioning assembly 5 located in the first annealing furnace 1 can be inserted into the fitting groove 503 on the positioning assembly 5 located in the second annealing furnace 2. Figure 5As shown, during the insertion process, the outer surface of the straight rod 7 contacts the outer surface of the threaded sleeve 504. Due to the friction force, the straight rod 7 drives the threaded sleeve 504 to rotate during the movement, so that the threaded rod 5041 on the positioning assembly 5 located in the second annealing furnace 2 can be continuously moved closer to the center of the hollow disk 501 under the action of the threaded sleeve 504, so that the arc-shaped clamping plates 505 connected thereto are moved closer to each other to clamp the steel shaft forging located in the second annealing furnace 2.

[0045] See also Figure 3 Preferably, the inner diameter of the hollow disk 501 in the positioning assembly 5 located in the first annealing furnace 1 is smaller than the inner diameter of the hollow disk 501 in the positioning assembly 5 located in the second annealing furnace 2 .

[0046] It should be noted that when the forging enters the second annealing furnace 2 from the first annealing furnace 1, the thicker part of the forging can be clamped by the positioning assembly 5 on the second annealing furnace 2, and the inner diameter of the second annealing furnace 2 is smaller than the inner diameter of the first annealing furnace 1, so the thicker part of the forging located in the second annealing furnace 2 can be better heated at a relatively high temperature, thereby ensuring that different parts of the forging are annealed to different degrees, so as to achieve uniformity of the overall annealing of the forging.

[0047] See also Figure 1 Preferably, a plurality of circumferentially distributed sealing grooves 8 are provided at the port of the first annealing furnace 1 away from the second annealing furnace 2, and a closing cover 9 hinged on the first annealing furnace 1 and capable of closing the first annealing furnace 1 is provided near the sealing groove 8. The closing cover 9 is provided with a plurality of sealing rings 901 adapted to the sealing groove 8. When the closing cover 9 covers the port of the first annealing furnace 1, the sealing ring 901 can be embedded in the sealing groove 8 to increase the sealing performance of the port of the first annealing furnace 1.

[0048] See also Figure 1 and Figure 5 Preferably, a plurality of groups of bosses 10 corresponding to the positions of the fitting grooves 503 in the positioning assembly 5 in the first annealing furnace 1 are installed on the surface of the closing cover 9 facing the first annealing furnace 1. When the closing cover 9 closes the first annealing furnace 1, the bosses 10 can be inserted into the fitting grooves 503 on the positioning assembly 5 in the first annealing furnace 1, driving the threaded sleeve 504 to rotate, so that the threaded rod 5041 pushes the arc-shaped clamping plate 505 to fix and clamp the steel shaft forging in the first annealing furnace 1.

[0049] See also Figure 3Preferably, the first annealing furnace 1 and the second annealing furnace 2 both include an outer wall and an inner wall, a heat insulating layer 11 is provided between the outer wall and the inner wall in the first annealing furnace 1, and a heat absorbing layer 12 is provided between the outer wall and the inner wall in the second annealing furnace 2, so that when the second annealing furnace 2 is in the first annealing furnace 1, it absorbs the heat of the first annealing furnace 1 and the heat of the second annealing furnace 2, so that the temperature in the second annealing furnace 2 is higher than the internal temperature of the first annealing furnace 1 without increasing external heating. At the same time, the inner diameter of the second annealing furnace 2 is smaller than that of the first annealing furnace 1, so that the heat source can be more concentrated, thereby more evenly heating the thicker part of the steel shaft forging in the second annealing furnace 2.

[0050] A method for using an annealing device for high-strength alloy steel shaft forgings comprises the following steps:

[0051] S1. Place the high-strength alloy steel shaft forging to be annealed on the positioning assembly 5 in the first annealing furnace 1, close the port of the first annealing furnace 1 with the closing cover 9 through the hinge mechanism, and ensure that the sealing ring 901 is completely embedded in the sealing groove 8 to increase the sealing performance of the first annealing furnace 1. At this time, the protruding column 10 on the closing cover 9 will be inserted into the fitting groove 503 of the positioning assembly 5 in the first annealing furnace 1 to achieve preliminary clamping of the steel shaft forging;

[0052] S2. After the initial clamping, the electric slider 403 on the displacement mechanism 4 moves on the slide rail 402 to slide the second annealing furnace 2 into the first annealing furnace 1. The engaging groove 503 in the positioning assembly 5 in the second annealing furnace 2 cooperates with the straight rod 7 in the first annealing furnace 1. The straight rod 7 in the first annealing furnace 1 will be inserted into the engaging groove 503 of the positioning assembly 5 in the second annealing furnace 2, and drive the threaded sleeve 504 to rotate, so that the threaded rod 5041 in the second annealing furnace 2 approaches the center of the hollow disk 501, and then the arc-shaped clamping plates 505 are close to each other to clamp the thicker part of the steel shaft forging in the second annealing furnace 2. At the same time, the second annealing furnace 2 moves closer to the port of the first annealing furnace 1, and the clamping diameter is smaller. Therefore, the external displacement mechanism 4 can be controlled to position and clamp the thicker part of the steel shaft forging to be annealed;

[0053] S3. After the position is fixed, start the first annealing furnace 1 and the second annealing furnace 2, and perform annealing according to the predetermined annealing temperature and time. The heat absorption layer 12 in the second annealing furnace 2 will absorb the heat of the first annealing furnace 1, and work together with its own heating system to perform relatively high-temperature annealing on the thicker part of the steel shaft forging. Since the second annealing furnace 2 has a smaller inner diameter, the heat source is more concentrated, and the thicker part of the forging can be heated more evenly;

[0054] S4. After annealing is completed, the second annealing furnace 2 moves away from the port of the first annealing furnace 1 to loosen the arc-shaped clamping plate 505, and then the closing cover 9 of the first annealing furnace 1 is opened to take out the annealed steel shaft forging.

[0055] The above description is only a preferred embodiment of the present invention and is not intended to be a further limitation of the present invention. All equivalent changes made using the contents of the present specification and drawings are within the protection scope of the present invention.

Claims

1. An annealing device for high-strength alloy steel shaft forgings, characterized in that: It comprises a first annealing furnace (1) and a second annealing furnace (2) slidably mounted on the rear side of the first annealing furnace (1), wherein a support bracket (101) is provided below the first annealing furnace (1); A connecting ring (3) is provided at the connection between the first annealing furnace (1) and the second annealing furnace (2); The side of the second annealing furnace (2) away from the first annealing furnace (1) is connected to the first annealing furnace (1) via a displacement mechanism (4); The displacement mechanism (4) comprises an external ring (401) located on a side of the second annealing furnace (2) away from the first annealing furnace (1); a plurality of slide rails (402) are distributed circumferentially on the first annealing furnace (1); each of the slide rails (402) is provided with an electric slider (403); each of the electric sliders (403) is provided with a connecting frame (404) for connecting to the external ring (401) on the second annealing furnace (2); The outer diameter of the second annealing furnace is smaller than the inner diameter of the first annealing furnace (1), and the first annealing furnace (1) and the second annealing furnace (2) are arranged in a concentric structure, and the second annealing furnace (2) can be moved to the inside of the first annealing furnace (1) by a displacement mechanism (4); A set of positioning components (5) is provided in each of the first annealing furnace (1) and the second annealing furnace (2); The positioning assembly (5) comprises an annular hollow disk (501), the hollow disk (501) and the first annealing furnace (1) and the second annealing furnace (2) are all arranged in a concentric structure, the outer wall of the hollow disk (501) is provided with a plurality of fixing columns (502) connected to the inner wall of the annealing furnace, the surface of the hollow disk (501) facing the outside of the first annealing furnace (1) is provided with a plurality of groups of circumferentially distributed interlocking grooves (503), both sides of the interlocking grooves (503) are provided with rotatable threaded sleeves (504), each of the threaded sleeves (504) is provided with a threaded rod (5041) threadedly matched therewith, and the bottoms of two adjacent threaded rods (5041) are connected to the same arc-shaped clamping plate (505) located directly below them.

2. The annealing device for high-strength alloy steel shaft forgings according to claim 1, characterized in that: The arc-shaped clamping plates (505) are provided in four groups, and the four groups of arc-shaped clamping plates (505) are moved closer to or farther away from each other under the action of the threaded rod (5041) to match steel shaft forgings of different diameters.

3. The annealing device for high-strength alloy steel shaft forgings according to claim 2, characterized in that: The positioning assembly (5) located inside the first annealing furnace (1) has a circumferential surface facing the second annealing furnace (2) provided with a positioning block (6) corresponding to the position of the engaging groove (503) on the positioning assembly (5) located inside the second annealing furnace (2), and each of the positioning blocks (6) is provided with a straight rod (7) corresponding to the engaging groove (503) on the positioning assembly (5) provided in the second annealing furnace (2).

4. The annealing device for high-strength alloy steel shaft forgings according to claim 3, characterized in that: The inner diameter of the hollow disk (501) in the positioning assembly (5) located in the first annealing furnace (1) is smaller than the inner diameter of the hollow disk (501) in the positioning assembly (5) located in the second annealing furnace (2).

5. The annealing device for high-strength alloy steel shaft forgings according to claim 4, characterized in that: A plurality of circumferentially distributed sealing grooves (8) are provided at a port of the first annealing furnace (1) away from the second annealing furnace (2), and a closing cover (9) hinged on the first annealing furnace (1) and capable of closing the first annealing furnace (1) is provided near the sealing grooves (8). The closing cover (9) is provided with a plurality of sealing rings (901) adapted to the sealing grooves (8).

6. The annealing device for high-strength alloy steel shaft forgings according to claim 5, characterized in that: A plurality of groups of bosses (10) corresponding to the positions of the engaging grooves (503) in the positioning assembly (5) in the first annealing furnace (1) are installed on the surface of the closing cover (9) facing the first annealing furnace (1).

7. The method for using the annealing device for high-strength alloy steel shaft forgings according to claim 6, characterized in that: The first annealing furnace (1) and the second annealing furnace (2) both comprise an outer wall and an inner wall, a heat insulating layer (11) is provided between the outer wall and the inner wall in the first annealing furnace (1), and a heat absorbing layer (12) is provided between the outer wall and the inner wall in the second annealing furnace (2).

8. The method for using the annealing device for high-strength alloy steel shaft forgings according to claim 7, characterized in that: The following steps are included: S1. Place the high-strength alloy steel shaft forging to be annealed on the positioning assembly (5) in the first annealing furnace (1), close the port of the first annealing furnace (1) with the closing cover (9) through the hinge mechanism, ensure that the sealing ring (901) is completely embedded in the sealing groove (8), and increase the sealing performance of the first annealing furnace (1). At this time, the protruding column (10) on the closing cover (9) will be inserted into the fitting groove (503) of the positioning assembly (5) in the first annealing furnace (1), so as to achieve preliminary clamping of the steel shaft forging; S2. After the initial clamping, the electric slider (403) on the displacement mechanism (4) moves on the slide rail (402) to slide the second annealing furnace (2) into the first annealing furnace (1). The fitting groove (503) in the positioning component (5) in the second annealing furnace (2) cooperates with the straight rod (7) in the first annealing furnace (1). The straight rod (7) in the first annealing furnace (1) is inserted into the fitting groove (503) of the positioning component (5) in the second annealing furnace (2) and drives the threaded sleeve (504) to rotate. The second annealing furnace (2) is moved so that the threaded rod (5041) in the second annealing furnace (2) approaches the center of the hollow disk (501), thereby causing the arc-shaped clamping plates (505) to approach each other. When the forging is placed, the thicker end of the forging is located in the second annealing furnace, clamping the thicker part of the steel shaft forging in the second annealing furnace (2). At the same time, the second annealing furnace (2) moves closer to the end of the first annealing furnace (1), and the clamping diameter becomes smaller. Therefore, the external displacement mechanism (4) can be controlled to position and clamp the thicker part of the steel shaft forging to be annealed. S3. After the position is fixed, the first annealing furnace (1) and the second annealing furnace (2) are started, and annealing treatment is performed according to the predetermined annealing temperature and time. The heat absorption layer (12) in the second annealing furnace (2) absorbs the heat of the first annealing furnace (1) and works together with its own heating system to perform a relatively high-temperature annealing treatment on the thicker part of the steel shaft forging. Since the inner diameter of the second annealing furnace (2) is smaller, the heat source is more concentrated, and the thicker part of the forging can be heated more evenly. S4. After annealing is completed, the second annealing furnace (2) moves away from the port of the first annealing furnace (1) to loosen the arc-shaped clamping plate (505), and then the closing cover (9) of the first annealing furnace (1) is opened to take out the annealed steel shaft forging.

Citation Information

Patent Citations

  • Annealing furnace with high annealing efficiency for brake disc production

    CN112779405A

  • Heat treatment furnace and heat treatment method for alloy resistance material

    CN116445706A

  • Lead device suitable for heating cover of annealing furnace

    CN203360498U

  • Stepped shaft induction heating device

    CN210117404U

  • Efficient circulating annealing furnace

    CN214694287U