A layered structure coating method for solid-state batteries
Through the layered structure coating method, preset cooling curves and real-time monitoring technology are used to ensure the uniformity of the solid-state battery electrolyte coating layer, solve the problem of low thermal stability of solid-state batteries, and improve the overall performance and safety of the battery.
Patent Information
- Application Number
- CN202411096721.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-12
- Publication Date
- 2024-10-22
- Estimated Expiration
- 2044-08-12
AI Technical Summary
The thickness of the solid-state electrolyte coating layer of existing solid-state batteries is uneven, resulting in reduced thermal stability and affecting battery performance.
Using a layered structure coating method, the cooling of the coating liquid is controlled through a preset cooling curve, the particle size growth rate and temperature attenuation uniformity of the inner powder material are monitored in real time, and the cooling curve is adjusted to ensure the uniformity and accuracy of the coating layer properties, combined with ball mill surface grinding treatment, to achieve nanoscale coating.
It improves the thermal stability and overall performance of the solid-state battery electrolyte, ensures the thickness uniformity and compactness of the coating layer, and enhances the safety and cycle life of the solid-state battery.
Smart Images

Figure CN118645679B_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the technical field of solid-state batteries, and in particular to a layered structure coating method for solid-state batteries. Background Art
[0002] A solid-state battery is a battery whose electrolyte is a solid material. Compared with traditional liquid electrolyte batteries, it has many advantages such as higher safety, longer cycle life, and higher energy density. It is regarded as the light of hope for future battery technology. However, since the solid electrolyte and the electrode material can only make direct point-to-point contact, the ionic conductivity of the solid electrolyte is significantly lower than that of liquid electrolytes or semi-solid electrolytes.
[0003] Chinese patent publication number: CN116936914A, discloses a solid-state lithium-ion battery; its technical point is that through a composite layered solid electrolyte structure, combined with the different doping effects of pentavalent elements and divalent elements, a multilayer structure with a pentavalent doped halide solid electrolyte as an inner layer and a divalent element doped halide solid electrolyte as an outer coating layer is formed to improve the ionic conductivity of the halide solid electrolyte layer; it can be seen that since the current polymer solid electrolyte, sulfide crystalline solid electrolyte and oxide solid electrolyte all have defects to varying degrees, the layered structure solid electrolyte is one of the important means to achieve mass production of solid-state batteries. However, the solid electrolyte coating uniformity used in the current technology is poor, which makes the coating layer thickness of the solid electrolyte uneven, seriously affecting the ionic conductivity of the solid electrolyte, and easily causing the solid-state battery to overheat, resulting in reduced thermal stability of the solid-state battery. Summary of the invention
[0004] To this end, the present invention provides a layered structure coating method for solid-state batteries, which is used to overcome the problem of uneven coating layer thickness of layered structure solid electrolytes in the prior art, resulting in reduced thermal stability of solid-state batteries.
[0005] To achieve the above object, the present invention provides a layered structure coating method for a solid-state battery, comprising:
[0006] Step S1, adding the selected outer layer material into a dissolving solution, heating and stirring the dissolving solution to dissolve the outer layer material, and preparing a coating solution;
[0007] Step S2, putting the pre-cooled inner layer powder material to be coated with the electrolyte into the coating liquid while stirring, controlling the cooling of the coating liquid according to a preset cooling curve, obtaining the real-time powder particle size of the inner layer powder material through an image acquisition device and calculating the real-time particle size growth rate, determining whether to adjust the real-time cooling rate of the preset cooling curve to correct the preset cooling curve, so that the outer layer material is precipitated from the coating liquid and coated on the surface of the inner layer powder material to form a layered coating material;
[0008] Step S3, separating the layered coating material from the coating liquid, spreading the separated layered coating material evenly, drying and heating it, collecting a thermal imaging image of the heated layered coating material in real time by a thermal imaging device, and determining a number of powder particles as samples of the layered coating material by temperature boundaries in the thermal imaging image, determining a single product coating uniformity according to the temperature attenuation uniformity of each sample in the thermal imaging image, and correcting the total cooling time of the preset cooling curve according to the single product coating uniformity, and adjusting the preset cooling curve according to the corrected total cooling time;
[0009] Step S4, adding the layered coating material into a ball mill for surface grinding treatment, screening to remove grinding dust, and drying again after rinsing, so as to complete the layered structure coating of the inner layer powder material.
[0010] Furthermore, in the step S2, a standard coated powder particle size range is set, the total cooling time of the preset cooling curve and the initial powder particle size of the inner layer powder material are obtained, the growth particle size range is calculated according to the standard coated powder particle size range and the initial powder particle size, and the standard particle size growth rate range is calculated according to the growth particle size range and the total cooling time;
[0011] When using a numerical range for calculation, the minimum and maximum values of the numerical range are used for calculation to obtain the corresponding range.
[0012] Furthermore, in step S2, a real-time image of the inner layer powder material is obtained by the image acquisition device, and several powder particle sizes of the inner layer powder material are selected in the real-time image, and an average value of the powder particle sizes of the selected inner layer powder materials is calculated as the real-time powder particle size of the inner layer powder material at the current acquisition moment;
[0013] The difference between the real-time powder particle size of the inner layer powder material at the current acquisition moment and the real-time powder particle size of the inner layer powder material at the previous acquisition moment is calculated, and the interval time between the current acquisition moment and the previous acquisition moment is divided by the difference to obtain the real-time particle size growth rate.
[0014] Furthermore, in step S2, a standard cooling rate is set. If the real-time particle size growth rate is lower than the minimum value of the standard particle size growth rate range, the slope of the curve at the corresponding position on the preset cooling curve is obtained as the real-time cooling rate, and the real-time cooling rate is determined.
[0015] If the real-time cooling rate is zero, the corresponding position of the preset cooling curve will be corrected with the standard cooling rate;
[0016] If the real-time cooling rate is less than zero, the real-time cooling rate will be adjusted to decrease according to the minimum value of the real-time particle size growth rate and the standard particle size growth rate range, and the corresponding position of the preset cooling curve will be corrected with the reduced and adjusted real-time cooling rate;
[0017] Among them, K'=K×(Vs / Vb), K' is the real-time cooling rate after reduction adjustment, K is the real-time cooling rate of the corresponding position, Vs is the real-time particle size growth rate, and Vb is the minimum value of the standard particle size growth rate range;
[0018] The corresponding position of the preset cooling curve is the curve portion corresponding to the interval between the current acquisition moment and the next acquisition moment of the image acquisition device.
[0019] Furthermore, in step S2, if the real-time particle size growth rate is higher than the maximum value of the standard particle size growth rate range, the real-time cooling rate of the preset cooling curve is adjusted to zero, and the corresponding position of the preset cooling curve is corrected.
[0020] Furthermore, in the step S2, if the real-time particle size growth rate is within the standard particle size growth rate range, the preset cooling curve is not adjusted or corrected.
[0021] Furthermore, in step S3, the thermal imaging device is used to collect a thermal imaging image of the heated layered coating material in real time, and a number of powder particles are determined as samples of the layered coating material through temperature boundaries in the thermal imaging image, and the temperature attenuation uniformity of each sample is calculated respectively, and the average value of the temperature attenuation uniformity of each sample is used as the coating uniformity of the single product.
[0022] Furthermore, in step S3, a standard cooling time and a corresponding standard grayscale difference are set, and the process of calculating the temperature attenuation uniformity of any sample includes:
[0023] During the cooling process of the layered coating material, an initial thermal imaging image and a thermal imaging image at the moment when the cooling time reaches a standard cooling time are acquired;
[0024] Performing grayscale conversion on the two thermal imaging images respectively and determining the image position of the sample to be calculated in the two thermal imaging images;
[0025] Calculate the grayscale differences of two corresponding pixel points in the image positions of the samples in the two thermal imaging images respectively to obtain a number of pixel grayscale differences;
[0026] Calculate the average value of grayscale differences of several pixels;
[0027] Subtract the grayscale difference of any pixel from the average value to obtain the real-time grayscale difference;
[0028] If the real-time grayscale difference is less than or equal to the standard grayscale difference, the corresponding pixel point will be marked;
[0029] Determine the number of marked pixels;
[0030] Determine the total number of pixels within the image location of the sample;
[0031] The ratio of the number of marks to the total number of pixels is calculated as the temperature attenuation uniformity of the sample.
[0032] Furthermore, in the step S3, a standard coating uniformity is set, and the calculated single product coating uniformity is judged according to the standard coating uniformity. If the single product coating uniformity is greater than or equal to the standard coating uniformity, the total cooling time of the preset cooling curve is not corrected.
[0033] Furthermore, in step S3, if the single product coating uniformity is less than the standard coating uniformity, the total cooling time of the preset cooling curve is corrected and increased, and the preset cooling curve is proportionally stretched according to the corrected total cooling time, so as to complete the correction of the preset cooling curve;
[0034] Among them, Tj'=Tj ×[1+(Ab-Ao) / Ab], where Tj' is the total cooling time after correction, Tj is the total cooling time before correction, Ab is the standard coating uniformity, and Ao is the single product coating uniformity.
[0035] Compared with the prior art, the beneficial effect of the present invention lies in that, by dissolving the selected outer layer material and then coating it on the surface of the inner layer powder material in a precipitated manner, nano-scale coating of the powder material can be achieved, and at the same time, the coating liquid is cooled by a preset cooling curve, so that the accuracy of the precipitated crystal coating can be accurately controlled, and the coating accuracy can be improved. The preset cooling curve is adjusted in real time and with post-feedback based on the real-time particle size growth rate of the inner layer powder material and the uniformity of temperature attenuation after the coating is completed, which further improves the accuracy of the coating controlled by the preset cooling curve, so that the coating layer thickness of the layered solid electrolyte is uniform and controllable, thereby improving the thermal stability of the solid-state battery electrolyte.
[0036] Furthermore, by monitoring the real-time particle size growth rate of the inner layer powder material, not only can the overall coating size be determined, but also the coating uniformity of any powder particle itself can be improved. At the same time, the dense texture of the coating layer can be ensured, and the problem of the outer layer material's instability due to solubility precipitation affecting the coating layer generation can be reduced, thereby making the coating layer thickness of the layered solid electrolyte uniform and controllable, thereby improving the overall performance of the solid electrolyte. BRIEF DESCRIPTION OF THE DRAWINGS
[0037] Figure 1 This is a flow chart of the layered structure coating method for solid-state batteries in this embodiment;
[0038] Figure 2 This is a logic diagram for determining the real-time particle size growth rate in this embodiment;
[0039] Figure 3 A flow chart for calculating the temperature decay uniformity of any sample in this embodiment;
[0040] Figure 4 This is a logic diagram for determining the coating uniformity of a single product in this embodiment. DETAILED DESCRIPTION
[0041] In order to make the objects and advantages of the present invention more clearly understood, the present invention is further described below in conjunction with embodiments; it should be understood that the specific embodiments described herein are only used to explain the present invention and are not used to limit the present invention.
[0042] The preferred embodiments of the present invention are described below with reference to the accompanying drawings. It should be understood by those skilled in the art that these embodiments are only used to explain the technical principles of the present invention and are not intended to limit the protection scope of the present invention.
[0043] It should be noted that, in the description of the present invention, terms such as "up", "down", "left", "right", "inside" and "outside" indicating directions or positional relationships are based on the directions or positional relationships shown in the drawings. This is merely for the convenience of description and does not indicate or imply that the device or element must have a specific orientation, be constructed and operated in a specific orientation. Therefore, it cannot be understood as a limitation on the present invention.
[0044] In addition, it should be noted that in the description of the present invention, unless otherwise clearly specified and limited, the terms "installed", "connected", and "connected" should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection, or it can be indirectly connected through an intermediate medium, or it can be the internal communication of two components. For those skilled in the art, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.
[0045] See also Figure 1 As shown, it is a flow chart of the layered structure coating method for solid-state batteries in this embodiment. This embodiment provides a layered structure coating method for solid-state batteries, including:
[0046] Step S1, adding the selected outer layer material into a dissolving solution, heating and stirring the dissolving solution to dissolve the outer layer material, and preparing a coating solution;
[0047] Step S2, putting the pre-cooled inner layer powder material to be coated with the electrolyte into the coating liquid while stirring, controlling the cooling of the coating liquid according to a preset cooling curve, obtaining the real-time powder particle size of the inner layer powder material through an image acquisition device and calculating the real-time particle size growth rate, determining whether to adjust the real-time cooling rate of the preset cooling curve to correct the preset cooling curve, so that the outer layer material is precipitated from the coating liquid and coated on the surface of the inner layer powder material to form a layered coating material;
[0048] Step S3, separating the layered coating material from the coating liquid, spreading the separated layered coating material evenly, drying and heating it, collecting a thermal imaging image of the heated layered coating material in real time by a thermal imaging device, and determining a number of powder particles as samples of the layered coating material by temperature boundaries in the thermal imaging image, determining a single product coating uniformity according to the temperature attenuation uniformity of each sample in the thermal imaging image, and correcting the total cooling time of the preset cooling curve according to the single product coating uniformity, and adjusting the preset cooling curve according to the corrected total cooling time;
[0049] Step S4, adding the layered coating material into a ball mill for surface grinding treatment, screening to remove grinding dust, and drying again after rinsing, so as to complete the layered structure coating of the inner layer powder material.
[0050] By dissolving the selected outer layer material and then coating it on the surface of the inner layer powder material in the form of precipitation, nano-scale coating of the powder material can be achieved. At the same time, the cooling of the coating liquid is controlled by a preset cooling curve, which can accurately control the accuracy of the precipitated crystal coating and improve the coating accuracy. The preset cooling curve is adjusted in real time and with post-feedback based on the real-time particle size growth rate of the inner layer powder material and the uniformity of temperature attenuation after the coating is completed, which further improves the accuracy of the coating controlled by the preset cooling curve, so that the coating layer thickness of the layered solid electrolyte is uniform and controllable, thereby improving the thermal stability of the solid-state battery electrolyte.
[0051] Specifically, in step S2, a standard coated powder particle size range is set, the total cooling time of the preset cooling curve and the initial powder particle size of the inner layer powder material are obtained, the growth particle size range is calculated according to the standard coated powder particle size range and the initial powder particle size, and the standard particle size growth rate range is calculated according to the growth particle size range and the total cooling time;
[0052] When using the numerical range for calculation, the minimum and maximum values of the numerical range are used for calculation to obtain the corresponding range, which is set to 650 μm to 800 μm in this embodiment.
[0053] In this embodiment, the standard coating powder particle size range needs to be determined according to the type of material used for coating and the required powder particle process size.
[0054] Specifically, in step S2, a real-time image of the inner layer powder material is obtained by the image acquisition device, and several powder particle sizes of the inner layer powder material are selected in the real-time image, and the average value of the powder particle sizes of the selected inner layer powder materials is calculated as the real-time powder particle size of the inner layer powder material at the current acquisition moment;
[0055] The difference between the real-time powder particle size of the inner layer powder material at the current acquisition moment and the real-time powder particle size of the inner layer powder material at the previous acquisition moment is calculated, and the interval time between the current acquisition moment and the previous acquisition moment is divided by the difference to obtain the real-time particle size growth rate.
[0056] Please continue reading Figure 2 As shown, it is a logic diagram for determining the real-time particle size growth rate in this embodiment;
[0057] Specifically, in step S2, a standard cooling rate is set. If the real-time particle size growth rate is lower than the minimum value of the standard particle size growth rate range, the slope of the curve at the corresponding position on the preset cooling curve is obtained as the real-time cooling rate, and the real-time cooling rate is determined.
[0058] If the real-time cooling rate is zero, the corresponding position of the preset cooling curve will be corrected with the standard cooling rate;
[0059] If the real-time cooling rate is less than zero, the real-time cooling rate will be adjusted to decrease according to the minimum value of the real-time particle size growth rate and the standard particle size growth rate range, and the corresponding position of the preset cooling curve will be corrected with the reduced and adjusted real-time cooling rate;
[0060] Among them, K'=K×(Vs / Vb), K' is the real-time cooling rate after reduction adjustment, K is the real-time cooling rate of the corresponding position, Vs is the real-time particle size growth rate, and Vb is the minimum value of the standard particle size growth rate range;
[0061] The corresponding position of the preset cooling curve is the curve portion corresponding to the interval between the current acquisition moment and the next acquisition moment of the image acquisition device.
[0062] In this embodiment, the standard cooling rate is set as a slope value, which should be determined according to the actual material properties used and its corresponding precipitation temperature. In this embodiment, it is set to -0.7.
[0063] By monitoring the real-time particle size growth rate of the inner layer powder material, not only can the overall coating size be determined, but also the coating uniformity of any powder particle itself can be improved. At the same time, the dense texture of the coating layer can be ensured, and the problem of the outer layer material's instability due to solubility precipitation affecting the coating layer generation can be reduced. This makes the coating layer thickness of the layered solid electrolyte uniform and controllable, thereby improving the overall performance of the solid electrolyte.
[0064] Specifically, in step S2, if the real-time particle size growth rate is higher than the maximum value of the standard particle size growth rate range, the real-time cooling rate of the preset cooling curve is adjusted to zero, and the corresponding position of the preset cooling curve is corrected.
[0065] Specifically, in step S2, if the real-time particle size growth rate is within the standard particle size growth rate range, the preset cooling curve is not adjusted or corrected.
[0066] Specifically, in step S3, the thermal imaging device is used to collect a thermal imaging image of the heated layered coating material in real time, and a number of powder particles are determined as samples of the layered coating material through temperature boundaries in the thermal imaging image, and the temperature attenuation uniformity of each sample is calculated respectively, and the average value of the temperature attenuation uniformity of each sample is used as the coating uniformity of a single product.
[0067] Specifically, in step S3, a standard cooling time and a corresponding standard grayscale difference are set. In this embodiment, the standard cooling time is set to 2 minutes, and the corresponding standard grayscale difference is set to 0.32%;
[0068] Please continue reading Figure 3 As shown, it is a flow chart of calculating the temperature attenuation uniformity of any sample in this embodiment; the process of calculating the temperature attenuation uniformity of any sample includes:
[0069] During the cooling process of the layered coating material, an initial thermal imaging image and a thermal imaging image at the moment when the cooling time reaches a standard cooling time are acquired;
[0070] Performing grayscale conversion on the two thermal imaging images respectively and determining the image position of the sample to be calculated in the two thermal imaging images;
[0071] Calculate the grayscale differences of two corresponding pixel points in the image positions of the samples in the two thermal imaging images respectively to obtain a number of pixel grayscale differences;
[0072] Calculate the average value of grayscale differences of several pixels;
[0073] Subtract the grayscale difference of any pixel from the average value to obtain the real-time grayscale difference;
[0074] If the real-time grayscale difference is less than or equal to the standard grayscale difference, the corresponding pixel point will be marked;
[0075] Determine the number of marked pixels;
[0076] Determine the total number of pixels within the image location of the sample;
[0077] The ratio of the number of marks to the total number of pixels is calculated as the temperature attenuation uniformity of the sample.
[0078] Please continue reading Figure 4 As shown, it is a logic diagram for determining the coating uniformity of a single product in this embodiment;
[0079] Specifically, in step S3, a standard coating uniformity of 0.98 is set, and the calculated single product coating uniformity is judged according to the standard coating uniformity. If the single product coating uniformity is greater than or equal to the standard coating uniformity, the total cooling time of the preset cooling curve is not corrected.
[0080] Specifically, in step S3, if the single product coating uniformity is less than the standard coating uniformity, the total cooling time of the preset cooling curve is corrected and increased, and the preset cooling curve is proportionally stretched according to the corrected total cooling time to complete the correction of the preset cooling curve;
[0081] Among them, Tj'=Tj ×[1+(Ab-Ao) / Ab], where Tj' is the total cooling time after correction, Tj is the total cooling time before correction, Ab is the standard coating uniformity, and Ao is the single product coating uniformity.
[0082] So far, the technical solutions of the present invention have been described in conjunction with the preferred embodiments shown in the accompanying drawings. However, it is easy for those skilled in the art to understand that the protection scope of the present invention is obviously not limited to these specific embodiments. Without departing from the principle of the present invention, those skilled in the art can make equivalent changes or substitutions to the relevant technical features, and the technical solutions after these changes or substitutions will fall within the protection scope of the present invention.
[0083] The above description is only a preferred embodiment of the present invention and is not intended to limit the present invention. For those skilled in the art, the present invention may have various modifications and variations. Any modification, equivalent replacement, improvement, etc. made within the spirit and principle of the present invention shall be included in the protection scope of the present invention.
Claims
1. A layered structure coating method for solid-state batteries, It is characterized in that include, Step S1, adding the selected outer layer material into a dissolving solution, heating and stirring the dissolving solution to dissolve the outer layer material, and preparing a coating solution; Step S2, putting the pre-cooled inner layer powder material to be coated with the electrolyte into the coating liquid while stirring, controlling the cooling of the coating liquid according to a preset cooling curve, obtaining the real-time powder particle size of the inner layer powder material through an image acquisition device and calculating the real-time particle size growth rate, determining whether to adjust the real-time cooling rate of the preset cooling curve to correct the preset cooling curve, so that the outer layer material is precipitated from the coating liquid and coated on the surface of the inner layer powder material to form a layered coating material; Step S3, separating the layered coating material from the coating liquid, spreading the separated layered coating material evenly, drying and heating it, collecting a thermal imaging image of the heated layered coating material in real time by a thermal imaging device, and determining a number of powder particles as samples of the layered coating material by temperature boundaries in the thermal imaging image, determining a single product coating uniformity according to the temperature attenuation uniformity of each sample in the thermal imaging image, and correcting the total cooling time of the preset cooling curve according to the single product coating uniformity, and adjusting the preset cooling curve according to the corrected total cooling time; Step S4, adding the layered coating material into a ball mill for surface grinding treatment, screening to remove grinding dust, and drying again after rinsing, thereby completing the layered structure coating of the inner layer powder material; In the step S3, the thermal imaging device collects a thermal imaging image of the heated layered coating material in real time, and determines a number of powder particles as samples of the layered coating material through the temperature boundary in the thermal imaging image, calculates the temperature attenuation uniformity of each sample, and takes the average value of the temperature attenuation uniformity of each sample as the single product coating uniformity; In step S3, a standard cooling time and a corresponding standard grayscale difference are set, and the process of calculating the temperature attenuation uniformity of any sample includes: During the cooling process of the layered coating material, an initial thermal imaging image and a thermal imaging image at the moment when the cooling time reaches a standard cooling time are acquired; Performing grayscale conversion on the two thermal imaging images respectively and determining the image position of the sample to be calculated in the two thermal imaging images; Calculate the grayscale differences of two corresponding pixel points in the image positions of the samples in the two thermal imaging images respectively to obtain a number of pixel grayscale differences; Calculate the average value of grayscale differences of several pixels; Subtract the grayscale difference of any pixel from the average value to obtain the real-time grayscale difference; If the real-time grayscale difference is less than or equal to the standard grayscale difference, the corresponding pixel point will be marked; Determine the number of marked pixels; Determine the total number of pixels within the image location of the sample; The ratio of the number of marks to the total number of pixels is calculated as the temperature attenuation uniformity of the sample.
2. The layered structure coating method for solid-state batteries according to claim 1, It is characterized in that In the step S2, a standard coated powder particle size range is set, the total cooling time of the preset cooling curve and the initial powder particle size of the inner layer powder material are obtained, the growth particle size range is calculated according to the standard coated powder particle size range and the initial powder particle size, and the standard particle size growth rate range is calculated according to the growth particle size range and the total cooling time; When using a numerical range for calculation, the minimum and maximum values of the numerical range are used for calculation to obtain the corresponding range.
3. The layered structure coating method for solid-state batteries according to claim 2, It is characterized in that In step S2, a real-time image of the inner layer powder material is obtained by the image acquisition device, and several powder particle sizes of the inner layer powder material are selected in the real-time image, and an average value of the powder particle sizes of the selected inner layer powder materials is calculated as the real-time powder particle size of the inner layer powder material at the current acquisition moment; The difference between the real-time powder particle size of the inner layer powder material at the current acquisition moment and the real-time powder particle size of the inner layer powder material at the previous acquisition moment is calculated, and the interval time between the current acquisition moment and the previous acquisition moment is divided by the difference to obtain the real-time particle size growth rate.
4. The layered structure coating method for solid-state batteries according to claim 3, It is characterized in that In step S2, a standard cooling rate is set. If the real-time particle size growth rate is lower than the minimum value of the standard particle size growth rate range, the slope of the curve at the corresponding position on the preset cooling curve is obtained as the real-time cooling rate, and the real-time cooling rate is determined. If the real-time cooling rate is zero, the corresponding position of the preset cooling curve will be corrected with the standard cooling rate; If the real-time cooling rate is less than zero, the real-time cooling rate will be adjusted to decrease according to the minimum value of the real-time particle size growth rate and the standard particle size growth rate range, and the corresponding position of the preset cooling curve will be corrected with the reduced and adjusted real-time cooling rate; Among them, K'=K×(Vs / Vb), K' is the real-time cooling rate after reduction adjustment, K is the real-time cooling rate of the corresponding position, Vs is the real-time particle size growth rate, and Vb is the minimum value of the standard particle size growth rate range; The corresponding position of the preset cooling curve is the curve portion corresponding to the interval between the current acquisition moment and the next acquisition moment of the image acquisition device.
5. The layered structure coating method for solid-state batteries according to claim 4, It is characterized in that In step S2, if the real-time particle size growth rate is higher than the maximum value of the standard particle size growth rate range, the real-time cooling rate of the preset cooling curve is adjusted to zero, and the corresponding position of the preset cooling curve is corrected.
6. The layered structure coating method for solid-state batteries according to claim 5, It is characterized in that In the step S2, if the real-time particle size growth rate is within the standard particle size growth rate range, the preset cooling curve is not adjusted or corrected.
7. The layered structure coating method for solid-state batteries according to claim 1, It is characterized in that In the step S3, a standard coating uniformity is set, and the calculated single product coating uniformity is judged according to the standard coating uniformity. If the single product coating uniformity is greater than or equal to the standard coating uniformity, the total cooling time of the preset cooling curve is not corrected.
8. The layered structure coating method for solid-state batteries according to claim 7, It is characterized in that In step S3, if the single product coating uniformity is less than the standard coating uniformity, the total cooling time of the preset cooling curve is corrected and increased, and the preset cooling curve is proportionally stretched according to the corrected total cooling time to complete the correction of the preset cooling curve; Among them, Tj'=Tj ×[1+(Ab-Ao) / Ab], where Tj' is the total cooling time after correction, Tj is the total cooling time before correction, Ab is the standard coating uniformity, and Ao is the single product coating uniformity.