Hybrid channel SiC MOSFET and method of manufacturing the same
By designing a hybrid channel structure and integrated Schottky diode in SiC MOSFET, the problems of threshold voltage instability and conduction loss in planar SiC MOSFET devices in high power and high temperature fields are solved, significantly improving the current density and the third Quadrant performance and achieves reduction of cell size.
Patent Information
- Application Number
- CN202411141209.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-20
- Publication Date
- 2024-11-01
- Estimated Expiration
- 2044-08-20
AI Technical Summary
In the high power and high temperature fields, existing planar SiC MOSFET devices have problems such as unstable threshold voltage, large conduction loss, and poor reverse recovery characteristics, and cell size is difficult to shrink.
Using a hybrid channel SiC MOSFET design, the Schottky diode is integrated to improve the gate structure and narrow the cell size by forming transverse and longitudinal conductive channels in the semiconductor body.
It significantly improves current density, reduces switching losses, improves the third quadrant performance, and achieves the reduction of cell size.
Smart Images

Figure CN118658886B_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the field of semiconductor technology, and in particular to a hybrid channel SiC MOSFET and a manufacturing method thereof. Background Art
[0002] The development of power electronic systems has put forward higher requirements on the performance of power semiconductor devices. At present, silicon-based power semiconductor devices occupy the main market share of power devices. However, due to the limitations of silicon material properties, the performance of silicon-based power devices has reached its theoretical limit.
[0003] As a representative of the third generation of semiconductor materials, silicon carbide (SiC) has advantages such as a larger bandgap, a higher critical breakdown electric field, and a higher thermal conductivity. Therefore, SiC power devices have obvious advantages in high power and high temperature fields. SiC MOSFET power devices with a planar gate structure have been commercialized, and their market share is also expanding.
[0004] The schematic diagram of the current mainstream planar SiC MOSFET cell is as follows: Figure 3 As shown, the cell structure is provided with a second type of well region 4, a first type of source region 5, and a second type of contact region 13. A transverse conductive channel is formed between the well region 4 and the source region 5 on the surface of the epitaxial layer 3. C1 and C2 are conductive channel regions located below the gate. Since the conductive channel is located on the surface of the epitaxial layer, the cell size of the device is inevitably limited by the gate-source spacing and the channel length, and it is difficult to achieve 3μm and below. The channel located on the surface of the epitaxial layer is also easily affected by subsequent processes, causing the problem of unstable threshold voltage. In addition, under the third quadrant working conditions, Figure 3 The SiC MOSFET shown uses body diode freewheeling, which can cause problems such as excessive conduction loss and poor reverse recovery characteristics. Summary of the invention
[0005] Technical purpose: In view of the shortcomings of the above-mentioned planar SiC MOSFET devices, the present invention provides a hybrid channel SiC MOSFET and a manufacturing method thereof. The purpose of the present invention is to provide an optimized design structure of SiC MOSFET, which can significantly improve the device current density, more easily narrow the cell size, and integrate Schottky diodes in the cell, greatly improving the third quadrant characteristics.
[0006] Technical solution: In order to achieve the above technical objectives, the present invention adopts the following technical solution.
[0007] A hybrid channel SiC MOSFET, comprising:
[0008] Drain;
[0009] a substrate located above the drain;
[0010] an epitaxial layer disposed on a substrate;
[0011] A well region located in the epitaxial layer; the spacing between the top surface of the well region and the top surface of the epitaxial layer ranges from 0.1µm to 1.0µm;
[0012] A source region is located in the well region; the spacing between the boundary of the source region and the boundary of the well region ranges from 0.1µm to 0.5µm;
[0013] A gate trench is located in the epitaxial layer, the left and right bottom corners of the gate trench are both located in the adjacent source region, there are left and right adjacent well regions below the gate trench, and the spacing between the adjacent well regions below the gate trench ranges from 0.2µm to 1.0µm;
[0014] A gate dielectric disposed on the sidewalls and bottom of the gate trench;
[0015] A gate located in the gate trench, the gate being surrounded on three sides by a gate dielectric;
[0016] An isolation dielectric located on the epitaxial layer, the isolation dielectric completely covering the gate;
[0017] A Schottky electrode located on the surface of the epitaxial layer between adjacent isolation dielectrics;
[0018] A source is located on both sides and above the isolation dielectric.
[0019] A method for manufacturing a hybrid channel SiC MOSFET, used to manufacture the hybrid channel SiC MOSFET described above, comprises the following steps:
[0020] Step 1, forming a first epitaxial layer on a substrate;
[0021] Step 2, forming a well region in the first epitaxial layer;
[0022] Step 3, forming a source region in the well region;
[0023] Step 4, forming a second epitaxial layer on the first epitaxial layer, the well region, and the source region, wherein the first epitaxial layer and the second epitaxial layer constitute an epitaxial layer;
[0024] Step 5: forming a gate trench penetrating part of the epitaxial layer, the well region, and the source region by an etching process;
[0025] Step 6: forming a gate dielectric on the sidewall and bottom of the gate trench, and forming a gate in the gate trench;
[0026] Step 7: forming an isolation dielectric covering the gate and the gate dielectric, forming a source electrode on both sides and on the isolation dielectric, and forming a Schottky electrode at the contact surface between the source electrode and the epitaxial layer; and forming a drain electrode at the bottom of the substrate.
[0027] A hybrid channel SiC MOSFET, comprising:
[0028] Drain;
[0029] a substrate located above the drain;
[0030] an epitaxial layer disposed on a substrate;
[0031] a current spreading layer located above the epitaxial layer;
[0032] A well region located in the current spreading layer; the spacing between the top surface of the well region and the top surface of the current spreading layer is in the range of 0.1µm to 1.0µm;
[0033] A source region is located in the well region; the spacing between the boundary of the source region and the boundary of the well region ranges from 0.1µm to 0.5µm;
[0034] A gate trench located in the current spreading layer, wherein the left and right bottom corners of the gate trench are both located in the adjacent source region, and there are left and right adjacent well regions below the gate trench, and the spacing between the adjacent well regions below the gate trench ranges from 0.2µm to 1.0µm;
[0035] A gate dielectric disposed on the sidewalls and bottom of the gate trench;
[0036] A gate located in the gate trench, the gate being surrounded on three sides by a gate dielectric;
[0037] an isolation dielectric located above the current spreading layer, the isolation dielectric completely covering the gate;
[0038] A Schottky electrode located on a surface of a current spreading layer between adjacent isolation dielectrics;
[0039] A source is located on both sides and above the isolation dielectric.
[0040] A method for manufacturing a hybrid channel SiC MOSFET, used to manufacture the hybrid channel SiC MOSFET described above, comprises the following steps:
[0041] Step 1, forming an epitaxial layer on a substrate;
[0042] Step 2, forming a first current spreading layer on the epitaxial layer, and forming a well region in the first current spreading layer;
[0043] Step 3, forming a source region in the well region;
[0044] Step 4, forming a second current spreading layer on the first current spreading layer, the well region, and the source region, wherein the first current spreading layer and the second current spreading layer constitute a current spreading layer;
[0045] Step 5: forming a gate trench penetrating part of the current spreading layer, the well region, and the source region by an etching process;
[0046] Step 6: forming a gate dielectric on the sidewall and bottom of the gate trench, and forming a gate in the gate trench;
[0047] Step 7: forming an isolation dielectric covering the gate and the gate dielectric, forming a source electrode on both sides and on the isolation dielectric, and forming a Schottky electrode at the contact surface between the source electrode and the epitaxial layer; and forming a drain electrode at the bottom of the substrate.
[0048] Beneficial effects:
[0049] (1) The hybrid channel SiC MOSFET proposed in the present invention forms lateral conductive channels C1 and C2 and longitudinal conductive channels C3 and C4 in the semiconductor body through the structural design of the gate trench, well region and source region, which significantly improves the current density compared with the traditional planar SiC MOSFET. The structural design of the gate trench, well region and source region can also set the gate structure in the semiconductor body, thereby changing the gate-source isolation from lateral to longitudinal, leaving a larger margin for narrowing the cell size of the device, making it easier to reduce the cell size of the device to 3µm or less, significantly increasing the channel density and further improving the current density.
[0050] (2) The hybrid channel SiC MOSFET proposed in the present invention integrates a Schottky diode in the cell. When the device operates in the third quadrant, the bipolar degradation effect is eliminated, the switching loss is reduced, and the third quadrant performance of the device is greatly improved. BRIEF DESCRIPTION OF THE DRAWINGS
[0051] Figure 1 Schematic diagram of a hybrid channel SiC MOSFET of Example 1;
[0052] Figure 2 Schematic diagram of a hybrid channel SiC MOSFET of Example 2;
[0053] Figure 3 Schematic diagram of a planar SiC MOSFET cell in the prior art;
[0054] Figure 4~Figure 9 Schematic diagram of the preparation process of the hybrid channel SiC MOSFET of Example 1;
[0055] Explanation of the accompanying drawings: 1. drain; 2. substrate; 3. epitaxial layer; 4. well region; 5. source region; 6. gate trench; 7. gate dielectric; 8. gate; 9. isolation dielectric; 10. source; 11. Schottky electrode; 12. current spreading layer; 13. contact region. DETAILED DESCRIPTION
[0056] The present invention is further explained and illustrated below in conjunction with the accompanying drawings and embodiments.
[0057] The embodiments are only used to illustrate the present invention and do not limit the scope of the claims. Other alternative means that can be thought of by those skilled in the art are all within the scope of the claims of the present invention.
[0058] In addition, in the description of the present invention, it should be noted that the terms "central", "center", "up", "down", "left", "right", "vertical", "horizontal", "inside", "outside" and the like indicate positions or positional relationships based on the positions or positional relationships shown in the accompanying drawings, and are only for the convenience of describing the present invention and simplifying the description, rather than indicating or implying that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore cannot be understood as limiting the invention. In addition, the terms "first", "second", and "third" are used for descriptive purposes only and cannot be understood as indicating or implying relative importance.
[0059] Example 1
[0060] As attached Figure 1 As shown, a hybrid channel SiC MOSFET of this embodiment includes:
[0061] A drain electrode 1; a substrate 2 located on the drain electrode 1, wherein the substrate 2 is a 4H-SiC substrate;
[0062] An epitaxial layer 3 located on the substrate 2, wherein the epitaxial layer 3 is a 4H-SiC epitaxial layer;
[0063] The well region 4 is located in the epitaxial layer 3. The depth of the well region 4 ranges from 0.7µm to 3.0µm, and the doping concentration is 5e16cm -3 ~ 3e18cm -3 ;
[0064] The source region 5 is located in the well region 4, the distance between the boundary of the source region 5 and the boundary of the well region 4 is in the range of 0.1µm~0.5µm, and the doping concentration of the source region 5 is 1e19cm -3 ~ 3e20cm -3 ;
[0065] A gate trench 6 is located in the epitaxial layer 3, the left and right bottom corners of the gate trench 6 are both located in the adjacent source region 5, there are left and right adjacent well regions 4 below the gate trench 6, the spacing between adjacent well regions at the bottom of the gate trench 6 ranges from 0.2µm to 1.0µm, the depth of the gate trench 6 ranges from 0.5µm to 4.0µm, the width ranges from 0.8µm to 4.0µm, and the sidewall angle of the gate trench 6 is not less than 80 degrees;
[0066] The gate dielectric 7 is located on the sidewall and bottom of the gate trench 6, and the thickness of the gate dielectric 7 is in the range of 30nm to 100nm; the gate 8 is located in the gate trench 6, and the gate 8 is surrounded by the gate dielectric 7 on three sides;
[0067] An isolation dielectric 9 located on the epitaxial layer 3, wherein the isolation dielectric 9 completely covers the gate 8;
[0068] A Schottky electrode 11 is located on the surface of the epitaxial layer 3 between adjacent isolation dielectrics 9; the spacing between adjacent well regions 4 below the Schottky electrode ranges from 0.4µm to 4.0µm;
[0069] The source 10 is located on both sides and on the isolation dielectric 9 .
[0070] The hybrid channel SiC MOSFET proposed in the present invention forms lateral conductive channels C1 and C2 between the well region and the source region at the bottom of the gate trench, and forms longitudinal conductive channels C3 and C4 between the well region and the source region on both sides of the gate trench, through the structural design of the gate trench, the well region and the source region, that is, the present invention forms lateral conductive channels C1, C2 and longitudinal conductive channels C3, C4 in the semiconductor body, which significantly improves the current density compared with the traditional planar SiC MOSFET. The structural design of the gate trench, the well region and the source region can also set the gate structure in the semiconductor body, thereby changing the gate-source isolation from lateral to longitudinal, leaving a larger margin for narrowing the cell size of the device, making it easier to make the device cell size 3µm and below, significantly increasing the channel density, and further improving the current density.
[0071] A hybrid channel SiC MOSFET in the present invention shows a cell structure, and the layout of the cell can be a strip, square, hexagon, dodecagon or atomic lattice. The doping type of the substrate, epitaxial layer and source region is a first type, and the doping type of the well region is a second type. The first type can be N-type or P-type, and correspondingly, the second conductivity type can be P-type or N-type.
[0072] As attached Figure 4 To Attachment Fig. 9 As shown, a method for manufacturing a hybrid channel SiC MOSFET of the present invention comprises the following steps:
[0073] Step 1: forming a first epitaxial layer on a substrate 2; Figure 4 As shown, a first epitaxial layer is formed on a substrate 2 by epitaxial growth, the depth of the substrate 2 ranges from 80µm to 300µm, and the doping concentration of the substrate 2 is 1e19cm -3 ~ 1e20cm -3 ; The doping concentration of the first epitaxial layer is 5e15cm -3 ~ 1e17cm -3 .
[0074] Step 2: forming a well region 4 in the first epitaxial layer; Figure 5 As shown, a well region 4 is formed in the first epitaxial layer by an ion implantation process. The depth of the well region 4 ranges from 0.7µm to 3.0µm, and the doping concentration is 5e16cm -3 ~ 3e18cm -3 ;
[0075] Step 3: forming a source region 5 in the well region 4; Figure 6 As shown, a source region 5 is formed in the well region 4 by an ion implantation process, the distance between the boundary of the source region 5 and the boundary of the well region 4 is in the range of 0.1µm to 0.5µm, and the doping concentration of the source region 5 is 1e19cm -3 ~ 3e20cm -3 .
[0076] Step 4, forming a second epitaxial layer on the first epitaxial layer, the well region 4, and the source region 5, the first epitaxial layer and the second epitaxial layer constitute an epitaxial layer 3; forming a second epitaxial layer by epitaxial growth on the first epitaxial layer, the well region 4, and the source region 5, the doping concentration of the second epitaxial layer is the same as the doping concentration of the first epitaxial layer; the spacing between the top surface of the well region 4 and the top surface of the epitaxial layer 3 ranges from 0.1µm to 1.0µm; the depth of the epitaxial layer 3 ranges from 5µm to 50µm; the semiconductor material used for the substrate 2 and the epitaxial layer 3 can be 3C-SiC, 4H-SiC, 6H-SiC or 15R-SiC.
[0077] Step 5, forming a gate trench 6 penetrating part of the epitaxial layer, the well region, and the source region, wherein the left and right bottom corners of the gate trench 6 are both located in the adjacent source region 5, and there are left and right adjacent well regions 4 below the gate trench 6; Figure 7 As shown, a gate trench 6 is formed in the first epitaxial layer 3 by an etching process, and the left and right bottom corners of the gate trench 6 are both located in the adjacent source region 5. There are left and right adjacent well regions 4 below the gate trench 6. The spacing between adjacent well regions at the bottom of the gate trench 6 ranges from 0.2µm to 1.0µm. The depth of the gate trench 6 ranges from 0.5µm to 4.0µm, and the width ranges from 0.8µm to 4.0µm. The sidewall angle of the gate trench 6 is not less than 80 degrees. The gate trench is in the depth direction of the device, that is, perpendicular to Figure 1 The distribution in the paper direction may be continuous or discontinuous. Step 5 may adopt a reactive ion etching process or an inductively coupled plasma etching process, and the etching gas may be one or more combinations of SF6, HBr, Cl2, O2, Ar and the like.
[0078] Step 6: forming a gate dielectric 7 on the sidewalls and bottom of the gate trench 6, and forming a gate 8 in the gate trench 6; Figure 8As shown, a gate dielectric 7 is formed on the sidewall and bottom of the gate trench 6 by the LPCVD (Low Pressure Chemical Vapor Deposition) process. The material of the gate dielectric 7 is silicon oxide, silicon nitride, borophosphosilicate glass, aluminum oxide, sapphire or hafnium oxide. The thickness of the gate dielectric 7 ranges from 30nm to 100nm. The gate dielectric 7 is subjected to high temperature annealing treatment. Then, a gate 8 is formed in the gate trench 6 by the LPCVD process. The material of the gate 8 is metal or doped polysilicon. The gate 8 is implanted and activated by annealing. After the gate is formed, the device surface can be flattened by the CMP (Chemical-Mechanical Polishing) process.
[0079] Step 7, forming an isolation dielectric 9 covering the gate 8, the gate dielectric 7 and a portion of the epitaxial layer 3, forming a source 10 on both sides and on the isolation dielectric 9, forming a drain 1 at the bottom of the substrate 2, and forming a Schottky electrode 11 at the contact surface between the source 10 and the epitaxial layer 3; Fig. 9 As shown, an isolation dielectric 9 is formed on the epitaxial layer 3 by the LPCVD process. The material of the isolation dielectric 9 is SiO2, and the isolation dielectric 9 completely covers the gate 8. A source metal is grown on both sides and on the isolation dielectric 9 to form a source ohmic contact and a Schottky contact. A drain metal is deposited on the bottom layer of the substrate 2 to form a drain ohmic contact. A source 10 is formed on the surface of the source ohmic contact, a drain 1 is formed on the surface of the drain ohmic contact, and a Schottky electrode 11 is formed on the surface of the Schottky contact. The spacing between adjacent well regions 4 below the Schottky electrode ranges from 0.4µm to 4.0µm.
[0080] The well region and the source region are in full contact with the source electrode in the depth direction of the device to form an ohmic contact.
[0081] In this embodiment, the electrode materials of the source, drain, and Schottky electrode are one or more combinations of metals such as Ti, Al, Ni, and Pt; the isolation medium can be silicon dioxide, or nitride, or a composite of silicon dioxide and nitride.
[0082] The SiC MOSFET cell structure of the present invention can be laid out in a strip, square, hexagon, dodecagon or atomic lattice shape.
[0083] Example 2
[0084] As attached Figure 2As shown, a hybrid channel SiC MOSFET of this embodiment is different from that of embodiment 1 in that a current spreading layer 12 is formed above the well region 4, between adjacent well regions 4, and below the well region 4. At this time, Schottky electrodes 11 are still formed on both sides of the isolation dielectric 9 and above the current spreading layer 12. The depth of the current spreading layer 12 ranges from 1.0µm to 3.5µm, and the doping concentration is 1e16m -3 ~ 3e17cm -3 The introduction of the current spreading layer 12 can further reduce the on-resistance of the device.
[0085] The manufacturing method of a hybrid channel SiC MOSFET of this embodiment is different from that of Embodiment 1 in that:
[0086] Step 1: forming an epitaxial layer 3 on a substrate 2; forming an epitaxial layer 3 on the substrate 2 by epitaxial growth, the depth range and doping concentration of the substrate 2 are the same as those in Example 1; the doping concentration of the epitaxial layer is 5e15cm -3 ~ 1e17cm -3 The thickness of the epitaxial layer 3 ranges from 4.0µm to 45µm;
[0087] Step 2, forming a first current spreading layer on the epitaxial layer 3 by epitaxial growth, and forming a well region 4 in the first epitaxial layer by an ion implantation process in the first current spreading layer, wherein the depth range and doping concentration of the well region 4 are the same as those in Example 1;
[0088] Step 3, forming a source region 5 in the well region 4; Step 3 is the same as that in Embodiment 1.
[0089] Step 4: Form a second current spreading layer by epitaxial growth on the first current spreading layer, the well region 4, and the source region 5. The first current spreading layer and the second current spreading layer constitute a current spreading layer 12. The doping concentration of the second current spreading layer is the same as that of the first current spreading layer. The depth of the current spreading layer 12 ranges from 1.0µm to 3.5µm, and the doping concentration is 1e16m -3 ~ 3e17cm -3 .
[0090] Step 5: forming a gate trench 6 penetrating part of the current spreading layer 12, the well region, and the source region. The rest of the contents are the same as those in the first embodiment.
[0091] The above is only a preferred embodiment of the present invention. It should be pointed out that for ordinary technicians in this technical field, several improvements and modifications can be made without departing from the principle of the present invention. These improvements and modifications should also be regarded as the scope of protection of the present invention.
Claims
1. A hybrid channel SiC MOSFET, characterized in that: include: Drain; a substrate located above the drain; an epitaxial layer disposed on a substrate; a well region located in the epitaxial layer; The distance between the top surface of the well region and the top surface of the epitaxial layer ranges from 0.1µm to 1.0µm; A source region is located in the well region; the spacing between the boundary of the source region and the boundary of the well region ranges from 0.1µm to 0.5µm; A gate trench is located in the epitaxial layer, the left and right bottom corners of the gate trench are both located in the adjacent source region, there are left and right adjacent well regions below the gate trench, and the spacing between the adjacent well regions below the gate trench ranges from 0.2µm to 1.0µm; A gate dielectric disposed on the sidewalls and bottom of the gate trench; A gate located in the gate trench, the gate being surrounded on three sides by a gate dielectric; An isolation dielectric located on the epitaxial layer, the isolation dielectric completely covering the gate; A Schottky electrode located on the surface of the epitaxial layer between adjacent isolation dielectrics; A source is located on both sides and above the isolation dielectric.
2. A hybrid channel SiC MOSFET according to claim 1, characterized in that: The depth of the well region ranges from 0.7µm to 3.0µm, and the spacing between adjacent well regions below the Schottky electrode ranges from 0.4µm to 4.0µm.
3. A hybrid channel SiC MOSFET according to claim 1, characterized in that: The doping concentration of the well region is 5e16cm -3 ~ 3e18cm -3 , the doping concentration of the source region is 1e19cm -3 ~ 3e20cm -3 .
4. A hybrid channel SiC MOSFET according to claim 1, characterized in that: The gate trench has a depth ranging from 0.5µm to 4.0µm, a width ranging from 0.8µm to 4.0µm, and a sidewall angle of the gate trench is not less than 80 degrees.
5. A hybrid channel SiC MOSFET, characterized in that: include: Drain; a substrate located above the drain; an epitaxial layer disposed on a substrate; a current spreading layer located above the epitaxial layer; A well region located in the current spreading layer; the spacing between the top surface of the well region and the top surface of the current spreading layer is in the range of 0.1µm to 1.0µm; A source region is located in the well region; the spacing between the boundary of the source region and the boundary of the well region ranges from 0.1µm to 0.5µm; A gate trench located in the current spreading layer, wherein the left and right bottom corners of the gate trench are both located in the adjacent source region, and there are left and right adjacent well regions below the gate trench, and the spacing between the adjacent well regions below the gate trench ranges from 0.2µm to 1.0µm; A gate dielectric disposed on the sidewalls and bottom of the gate trench; A gate located in the gate trench, the gate being surrounded on three sides by a gate dielectric; an isolation dielectric located above the current spreading layer, the isolation dielectric completely covering the gate; A Schottky electrode located on a surface of a current spreading layer between adjacent isolation dielectrics; A source is located on both sides and above the isolation dielectric.
6. A hybrid channel SiC MOSFET according to claim 5, characterized in that: The depth of the current spreading layer ranges from 1.0µm to 3.5µm, and the doping concentration is 1e16m -3 ~ 3e17cm -3 .
7. A method for manufacturing a hybrid channel SiC MOSFET, used to manufacture a hybrid channel SiC MOSFET as claimed in any one of claims 1 to 4, characterized in that: The following steps are involved: Step 1, forming a first epitaxial layer on a substrate; Step 2, forming a well region in the first epitaxial layer; Step 3, forming a source region in the well region; Step 4, forming a second epitaxial layer on the first epitaxial layer, the well region, and the source region, wherein the first epitaxial layer and the second epitaxial layer constitute an epitaxial layer; Step 5: forming a gate trench penetrating part of the epitaxial layer, the well region, and the source region by an etching process; Step 6: forming a gate dielectric on the sidewall and bottom of the gate trench, and forming a gate in the gate trench; Step 7: forming an isolation dielectric covering the gate and the gate dielectric, forming a source electrode on both sides and on the isolation dielectric, and forming a Schottky electrode at the contact surface between the source electrode and the epitaxial layer; and forming a drain electrode at the bottom of the substrate.
8. The method for manufacturing a hybrid channel SiC MOSFET according to claim 7, characterized in that: In step 5, a reactive ion etching process or an inductively coupled ion etching process is adopted, and the etching gas is one or more combinations of SF6, HBr, Cl2, O2, and Ar gases.
9. The method for manufacturing a hybrid channel SiC MOSFET according to claim 7, characterized in that: After the gate is formed in step 6, the device surface is flattened using a CMP process.
10. A method for manufacturing a hybrid channel SiC MOSFET, used to manufacture a hybrid channel SiC MOSFET as claimed in claim 5 or 6, characterized in that: The following steps are involved: Step 1, forming an epitaxial layer on a substrate; Step 2, forming a first current spreading layer on the epitaxial layer, and forming a well region in the first current spreading layer; Step 3, forming a source region in the well region; Step 4, forming a second current spreading layer on the first current spreading layer, the well region, and the source region, wherein the first current spreading layer and the second current spreading layer constitute a current spreading layer; Step 5: forming a gate trench penetrating part of the current spreading layer, the well region, and the source region by an etching process; Step 6: forming a gate dielectric on the sidewall and bottom of the gate trench, and forming a gate in the gate trench; Step 7: forming an isolation dielectric covering the gate and the gate dielectric, forming a source electrode on both sides and on the isolation dielectric, and forming a Schottky electrode on the contact surface between the source electrode and the epitaxial layer; A drain is formed at the bottom of the substrate.
Citation Information
Patent Citations
Vertical semiconductor structure and method of fabrication
EP1930952A1
Power semiconductor device
JP2012033731A
MESFETs integrated with MOSFETs on common substrate and methods of forming the same
US20050184343A1
Silicon carbide switch device and manufacturing method therefor
WO2019019395A1
KR20220030587A