Optimized control system for cooling process of aluminum castings
Through array temperature monitoring and dynamic cooling control, the problems of unevenness and low efficiency of aluminum castings are solved, efficient and uniform cooling of aluminum castings are achieved, and production efficiency and product quality are improved.
Patent Information
- Application Number
- CN202411126073.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-16
- Publication Date
- 2024-11-29
- Estimated Expiration
- 2044-08-16
AI Technical Summary
The traditional aluminum casting cooling control method has problems such as cooling inhomogeneity, low efficiency, insufficient monitoring and a single cooling strategy, which cannot meet the cooling needs of different types and specifications of aluminum castings.
The key monitoring areas are determined by array temperature monitoring method, and through temperature sensor monitoring and analysis, combined with dynamic cooling control strategies and uniform cooling mechanism, the temperature and flow of the cooling medium are adjusted in real time to achieve accurate monitoring and optimization of the cooling process of aluminum castings.
It improves the cooling uniformity of aluminum castings, reduces stress concentration and deformation, shortens production cycle, reduces energy consumption and production costs, and ensures the cooling quality of aluminum castings.
Smart Images

Figure CN118663872B_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of cooling aluminum castings, in particular to an optimization control system used in the cooling process of aluminum castings. Background Art
[0002] Aluminum castings are widely used in the fields of automobile, aerospace, machinery manufacturing, etc. due to their light weight, high strength, good thermal conductivity and recyclability. In the manufacturing process of aluminum castings, cooling is a crucial step, which directly affects the microstructure, mechanical properties and subsequent processing and application of the castings. Traditional aluminum casting cooling control methods have some shortcomings, which are mainly manifested in the following aspects:
[0003] Cooling uniformity problem: During the cooling process of aluminum castings, due to differences in the geometry, wall thickness, distribution of cooling medium and other factors in different areas of the casting, the cooling speed is inconsistent, which is prone to uneven cooling, which may cause stress concentration and deformation inside the casting, affecting the quality and performance of the casting;
[0004] Cooling efficiency problem: Traditional cooling methods may have low cooling efficiency due to inaccurate temperature control of the cooling medium and unreasonable layout of the cooling equipment, which will extend the production cycle and increase energy consumption and production costs;
[0005] Insufficient monitoring of the cooling process: In some existing cooling control systems, the monitoring of the cooling process of castings is not comprehensive and accurate enough, and there is a lack of effective temperature monitoring and data analysis methods, making it difficult to promptly detect and handle abnormal conditions in the cooling process;
[0006] Single cooling strategy: Existing cooling control systems often adopt fixed cooling strategies and lack the ability to dynamically adjust according to the specific characteristics of the castings and production conditions, and cannot meet the cooling needs of aluminum castings of different types and specifications;
[0007] In order to solve the above defects, a technical solution is now provided. Summary of the invention
[0008] The purpose of the present invention is to solve the problem that the traditional cooling control is relatively single and cannot meet the cooling requirements of different aluminum castings, and to propose an optimized control system for the cooling process of aluminum castings.
[0009] The purpose of the present invention can be achieved through the following technical solutions:
[0010] Optimized control system for cooling process of aluminum castings, including:
[0011] The temperature monitoring unit is used to monitor the surface and internal temperature distribution of the casting using an array temperature monitoring method. The specific steps are as follows:
[0012] Firstly, the key monitoring area of the casting is determined, and the casting is divided into different areas according to logic. The importance of different areas is judged. The wall thickness, thermal gradient, cold time value, thermal node value, stress value, missing value and shape evaluation value of the key monitoring area are obtained by collecting the re-evaluation parameters of different areas of the casting for comprehensive analysis. After normalization, the product of wall thickness and thermal gradient plus cold time value is used as the bottom circle radius to establish the bottom circle, and the sum of thermal node value, stress value and missing value is used as the height to establish the cone model. The vertex of the cone model is selected as the center of the sphere, and the shape evaluation value multiplied by the weight factor is used as the diameter to establish the spherical model.
[0013] Then calculate the surface area of the irregular body formed by the cone and the sphere, and record it as the re-judgment value, and use this re-judgment value as the criterion for measuring the importance of the area;
[0014] The re-judgment values obtained from all the segmented areas of the casting are sorted by size, and the areas with the re-judgment values in the first half are selected as the key monitoring areas for temperature monitoring;
[0015] Arrange temperature sensors in key monitoring areas. After completing the arrangement of temperature sensors, analyze the areas where there are blind spots larger than the preset blind spots, and arrange additional temperature sensors in the areas to achieve an array layout for the entire casting.
[0016] Configure the data acquisition function to collect sensor data and set the sampling frequency to ensure that the temperature changes in the key areas of the casting are captured during the cooling process of the casting;
[0017] Temperature analysis unit, used to monitor the temperature of key areas of castings and determine cooling abnormalities;
[0018] The cooling control unit is used to perform corresponding cooling control according to cooling abnormalities.
[0019] Furthermore, the analysis process of the wall thickness, thermal gradient, cold time value, thermal node value, stress value, absence value and shape evaluation value of the key monitoring area in the temperature monitoring unit is as follows:
[0020] Thick wall is the average wall thickness of the casting in this area. When the average wall thickness is larger, the area needs a longer cooling time and its importance is higher.
[0021] The thermal gradient is the temperature difference between the inside and the surface or different parts of the casting in this area. When the thermal gradient is larger, the cooling importance is higher;
[0022] The cooling rate requirement is measured by the time required for cooling the area. When different parts of the area require different cooling times, the average cooling time of all parts of the area is calculated and recorded as the cooling time value. The smaller the cooling time value, the higher the cooling importance of the area.
[0023] The local hot spot and stress concentration area is the total area of the local hot spot or hot spot and stress concentration area in the casting in this area, which is recorded as the hot spot value and stress value respectively. When there is no local hot spot or hot spot and stress concentration area in this area, the hot spot value and stress value of this area are 0. The larger the hot spot value or stress value, the higher the cooling demand and the corresponding cooling importance.
[0024] The historical defect record is the number of cooling defects that occurred in the area, which is recorded as the absence value, and this absence value is used as a standard to measure the importance of the historical defect record in the area;
[0025] The regional geometry is to assign a complexity score of 1-100 to the geometry of the region of the casting, and record it as the shape evaluation value. This shape evaluation value is used as a standard to measure the geometry of the region. The larger the shape evaluation value, the greater the complexity of the geometry of the region, and the higher the corresponding cooling importance.
[0026] Furthermore, the specific operation steps of the temperature analysis unit analysis are as follows:
[0027] The temperatures monitored in different key areas are recorded as , after normalization, enter the following formula: Get the mean temperature , where The temperature monitored for each critical area;
[0028] Then the temperature average Substitute the following formula: To obtain the variance of temperature in different key areas , and then the obtained variance Compare with the preset threshold, when the variance When it is greater than a preset threshold, it is judged that there is uneven cooling during the cooling operation of the casting, and a cooling signal is generated;
[0029] Then, a temperature curve is established for the temperatures monitored in different key areas, with the horizontal axis being time and the vertical axis being temperature value;
[0030] The temperature drop standard curve of different regions of the casting when cooling is obtained by analyzing the historical records of the cooling of the same type of castings, and the temperature drop standard curve is bidirectionally expanded according to the preset standard to form a standard range of the temperature drop curve;
[0031] Then, the temperature curve established for the temperature monitored in different key areas is compared with the standard interval of the temperature drop curve obtained by analysis to determine whether there is a situation where the temperature curve trends outside the standard interval of the temperature drop curve. When the temperature curve trends outside the standard interval of the temperature drop curve, the time it takes for the temperature curve to trend outside the standard interval of the temperature drop curve is recorded. When the time exceeds the preset time threshold, it is determined that the cooling temperature drop of the casting in this area is abnormal, and an abnormal signal is generated.
[0032] Furthermore, the specific operation steps of the cooling control unit are as follows:
[0033] After receiving the cooling average signaling, the temperatures monitored in all key areas are obtained and the difference between the temperatures monitored in the key areas and the temperature average is calculated, and the obtained temperature difference is compared with the preset difference threshold. When the temperature difference is greater than the preset difference threshold, the corresponding key area is marked; then, through the comparison results of the received abnormal signaling and the temperature drop curve of the corresponding key area with the standard interval of the temperature drop curve, it is judged that the marked key area belongs to the area that cools too fast or the area that cools too slowly;
[0034] The specific cooling control steps for areas that cool too slowly are as follows:
[0035] First, obtain the specific location of the slow cooling area in the casting, and use the cooling attachment for the slow cooling area;
[0036] Then, the temperature of the cooling medium in the area is lowered gradually, and the flow rate of the cooling medium is increased to improve the cooling speed;
[0037] Then, the device holding the casting is controlled to rotate or move so that the area where the casting cools too slowly is closer to the cooling water channel. At the same time, the cross-sectional area of the cooling water channel is increased. In combination with accelerated cooling technology, the insulation material in the area where the casting cools too slowly is reduced or unnecessary insulation layers are removed.
[0038] The specific cooling control steps for areas that cool too quickly are as follows:
[0039] First, the specific location of the area where the cooling is too slow in the casting is obtained, and the temperature of the cooling medium or air is increased for the area where the cooling is too fast, the cooling speed is slowed down, and the flow rate of the cooling medium is adjusted to reduce the flow rate of the cooling medium and reduce the cooling intensity;
[0040] At the same time, add insulation materials around the area where cooling is too fast to slow down heat transfer, and then use local heating equipment, including heating belts or heating pads, to balance the cooling rate in the area where cooling is too fast, extending the cooling time of the entire casting to compensate for the rapid cooling of the local area.
[0041] Furthermore, the cooling control unit implements a dynamic cooling control strategy during the cooling control process, monitors in real time whether the temperature drop curve of the regional casting returns to the standard range of the temperature drop curve, and determines whether it is necessary to suspend cooling control or reduce control intensity.
[0042] Furthermore, the specific operation steps of the cooling control unit to implement the uniform cooling mechanism are as follows:
[0043] First, count the total number of areas that cool too fast or too slow, and calculate the ratio to all key areas, which is recorded as the abnormal ratio;
[0044] The obtained abnormal proportion is compared with the preset proportion threshold. When the abnormal proportion is greater than the preset proportion threshold, it is judged that the temperature of the cooling medium around the cooling of the casting is not uniform enough, and the immersion cooling method is enabled, specifically, by immersing the entire casting in the cooling medium, and stirring and neutralizing the cooling medium with a stirring or swirl device, thereby neutralizing the temperature of the cooling medium, so that the cooling of different areas of the casting by the cooling medium is more uniform;
[0045] Then, temperature sensors are evenly arranged at different positions in the cooling medium loading container to monitor the real-time temperature of the cooling medium in the loading container in real time;
[0046] Then, according to the degree of discreteness of the temperature values of the temperature sensors at different parts, it is determined whether it is necessary to start the stirring or swirling device to neutralize the cooling medium. When it is necessary to start the stirring or swirling device, the starting power of the stirring or swirling device is adjusted according to the degree of discreteness of the temperature at different parts in the loading container, so that the greater the temperature difference at different parts of the cooling medium in the loading container, the higher the power of the stirring or swirling device, so as to quickly neutralize the temperature of the cooling medium at different parts and quickly improve the cooling uniformity of the casting.
[0047] Compared with the prior art, the present invention has the following beneficial effects:
[0048] The present invention can effectively monitor the temperature distribution of aluminum castings during cooling through an array temperature monitoring method and determination of key monitoring areas, timely discover and handle uneven cooling, thereby improving the overall cooling uniformity of the castings, reducing stress concentration and deformation, and improving the quality of the castings.
[0049] The present invention adopts a dynamic cooling control strategy and a uniform cooling mechanism, which can adjust the temperature and flow rate of the cooling medium in real time according to the actual temperature changes during the cooling process of the casting, optimize the layout and use of the cooling equipment, improve the cooling efficiency, shorten the production cycle, and reduce energy consumption and production costs;
[0050] The present invention realizes comprehensive intelligent monitoring of the cooling process by establishing a standard interval of the temperature drop curve and real-time monitoring of the temperature drop curve of the casting, and neutralizing the cooling medium with a stirring or swirl device. This not only improves the controllability and stability of the cooling process, but also effectively prevents and promptly responds to abnormal situations that may occur in the cooling process, thereby ensuring the cooling quality of the aluminum casting. BRIEF DESCRIPTION OF THE DRAWINGS
[0051] In order to facilitate understanding by those skilled in the art, the present invention is further described below in conjunction with the accompanying drawings;
[0052] Figure 1 This is the overall system block diagram of the present invention. DETAILED DESCRIPTION
[0053] The technical solution of the present invention will be clearly and completely described below in conjunction with the embodiments. Obviously, the described embodiments are only part of the embodiments of the present invention, rather than all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0054] It should be understood that the terms "include" and "comprising" used in the specification and claims of the present disclosure indicate the presence of described features, integers, steps, operations, elements and / or components, but do not exclude the presence or addition of one or more other features, integers, steps, operations, elements, components and / or collections thereof.
[0055] It should also be understood that the terms used in this disclosure are only for the purpose of describing specific embodiments and are not intended to limit the disclosure. As used in this disclosure and claims, the singular forms of "a", "an", and "the" are intended to include the plural forms unless the context clearly indicates otherwise. It should also be further understood that the term "and / or" used in this disclosure and claims refers to any combination of one or more of the associated listed items and all possible combinations, and includes these combinations.
[0056] like Figure 1 As shown, the optimization control system used in the cooling process of aluminum castings includes a temperature monitoring unit, a temperature analysis unit and a cooling control unit;
[0057] The temperature monitoring unit is used to monitor the surface and internal temperature distribution of castings using an array temperature monitoring method. The specific process is as follows:
[0058] First, determine the key monitoring areas of the casting, divide the casting into different areas according to logic, judge the importance of different areas, and conduct a comprehensive analysis by collecting re-evaluation parameters of different areas of the casting. The re-evaluation parameters include: wall thickness, thermal gradient, cooling rate requirement, local thermal node, stress concentration area, historical defect record and regional geometry; thick wall is the average wall thickness of the casting in this area. When the average wall thickness is larger, the area requires a longer cooling time and its importance is higher; thermal gradient is the temperature difference between the inside and the surface or different parts of the casting in this area. When the thermal gradient is larger, the cooling importance is higher; cooling rate requirement is measured by the time required for cooling in this area. When the cooling time required for different parts of the area is different, calculate the average cooling time of all parts of the area and record it as the cold time value. The smaller the cold time value, the area The higher the cooling importance; the local hot spot and stress concentration area is the total area of the local hot spot or hot spot and stress concentration area in the casting in this area, which is recorded as the hot spot value and stress value respectively. When there is no local hot spot or hot spot and stress concentration area in this area, the hot spot value and stress value of this area are 0. The larger the hot spot value or stress value, the higher the cooling demand and the corresponding cooling importance; the historical defect record is the number of cooling defects in this area, which is recorded as the absence value, and this absence value is used as the standard for measuring the importance of the historical defect record in this area; the regional geometry is to assign a complexity score of 1-100 to the geometry of the casting in this area, and it is recorded as the shape evaluation value. This shape evaluation value is used as the standard for measuring the geometry of the area. When the shape evaluation value is larger, the geometry of the area is more complex, and the corresponding cooling importance is higher;
[0059] After normalizing the wall thickness, thermal gradient, cold time value, thermal node value, stress value, missing value and shape evaluation value of the casting area, the product of the wall thickness and the thermal gradient plus the cold time value is used as the bottom circle radius to establish the bottom circle, the sum of the thermal node value, the stress value and the missing value is used as the height to establish a cone model, the vertex of the cone model is selected as the center of the sphere, and the shape evaluation value multiplied by the weight factor is used as the diameter to establish a spherical model, wherein the weight factor is set between 0.1 and 0.18, and then the surface area of the irregular body formed by the cone and the sphere is calculated and recorded as the re-judgment value, and the re-judgment value is used as the judgment standard for measuring the importance of the area;
[0060] The re-judgment values obtained for all segmented areas of the casting are sorted by size, and the area with the re-judgment value in the first half is selected as the key monitoring area for temperature monitoring; temperature sensors are arranged in the key monitoring area, and after the arrangement of the temperature sensors is completed, the area with a blind area larger than the preset blind area is analyzed, and additional temperature sensors are arranged in the area to realize an array layout of the entire casting; the data acquisition function is configured to collect sensor data, and the sampling frequency is set to ensure that the temperature changes in the key areas of the casting are captured during the cooling process of the casting.
[0061] The temperature analysis unit is used to analyze the temperature of key areas of the monitored casting and determine cooling abnormalities;
[0062] The temperatures monitored in different key areas are recorded as , after normalization, enter the following formula: Get the mean temperature , where The temperature monitored for each key area, and then the average temperature Substitute the following formula: To obtain the variance of temperature in different key areas , and then the obtained variance Compare with the preset threshold, when the variance When it is greater than a preset threshold, it is judged that there is uneven cooling during the cooling operation of the casting, and a cooling signal is generated;
[0063] Then, a temperature curve is established for the temperatures monitored in different key areas, with the horizontal axis being time and the vertical axis being temperature value. Then, through the historical records of cooling of the same type of castings, a standard temperature drop curve when cooling different areas of the casting is obtained, and the temperature drop standard curve is bidirectionally expanded according to the preset standard to form a standard range of the temperature drop curve; the temperature curve established by the temperatures monitored in different key areas is compared with the standard range of the temperature drop curve obtained by analysis to determine whether there is a situation where the temperature curve trends outside the standard range of the temperature drop curve. When the temperature curve trends outside the standard range of the temperature drop curve, the time it takes for the temperature curve to trend outside the standard range of the temperature drop curve is recorded. When the time exceeds the preset time threshold, it is determined that the cooling temperature drop of the casting in this area is abnormal, and an abnormal signal is generated.
[0064] The cooling control unit is used to perform corresponding cooling control according to cooling abnormalities;
[0065] After receiving the cooling average signaling, the temperatures monitored in all key areas are obtained and the difference between the temperatures monitored in the key areas and the temperature average is calculated, and the obtained temperature difference is compared with the preset difference threshold. When the temperature difference is greater than the preset difference threshold, the corresponding key area is marked; then, through the comparison results of the received abnormal signaling and the temperature drop curve of the corresponding key area with the standard interval of the temperature drop curve, it is judged that the marked key area belongs to the area that cools too fast or the area that cools too slowly;
[0066] The specific cooling control steps for areas that cool too slowly are as follows:
[0067] First, the specific location of the area where the cooling is too slow in the casting is obtained, and cooling accessories are used for the location of the area where the cooling is too slow. The cooling accessories include cooling rods or cooling fixtures. Then, the temperature of the cooling medium at the location of the area is reduced. The temperature is reduced in a step-by-step manner, and the flow rate of the cooling medium is increased to increase the cooling speed. The distance between the area where the cooling is too slow and the cooling water channel is made closer by controlling the device that clamps the casting to rotate or move. At the same time, the cross-sectional area of the cooling water channel is increased, and accelerated cooling technology is used, including spray cooling or adding cooling fans to improve cooling efficiency, and the insulation material in the area where the cooling is too slow is reduced or unnecessary insulation layers are removed;
[0068] The specific cooling control steps for areas that cool too quickly are as follows:
[0069] First, the specific location of the area where the cooling is too slow in the casting is obtained, and the temperature of the cooling medium or air is increased for the area where the cooling is too fast, the cooling speed is slowed down, and the flow rate of the cooling medium is adjusted to reduce the flow rate of the cooling medium and reduce the cooling intensity. At the same time, heat insulation materials are added around the area where the cooling is too fast to slow down the heat transfer. Local heating equipment, including heating belts or heating pads, is used for the area where the cooling is too fast to balance the cooling speed and extend the cooling time of the entire casting to compensate for the rapid cooling of the local area.
[0070] In the process of executing cooling control, a dynamic cooling control strategy is implemented to monitor in real time whether the temperature drop curve of the regional casting returns to the standard range of the temperature drop curve, and determine whether it is necessary to suspend cooling control or reduce the control intensity;
[0071] The cooling control unit is also used to implement a uniform cooling mechanism, the specific steps are as follows:
[0072] The total number of areas where cooling is too fast or too slow is counted, and the proportion of all key areas is calculated and recorded as the abnormal proportion. The obtained abnormal proportion is compared with the preset proportion threshold. When the abnormal proportion is greater than the preset proportion threshold, it is judged that the temperature of the cooling medium around the cooling of the casting is not uniform enough, and the immersion cooling method is enabled. The casting is immersed in the cooling medium as a whole, and the cooling medium is stirred and neutralized with a stirring or swirl device, so as to neutralize the temperature of the cooling medium, so that the cooling of different areas of the casting by the cooling medium is more uniform, and temperature sensors are evenly arranged at different parts of the cooling medium loading container, and the real-time temperature of the cooling medium in the loading container is monitored in real time. According to the discrete degree of the temperature values of the temperature sensors at different parts, it is determined whether it is necessary to start the stirring or swirl device to neutralize the cooling medium. When it is necessary to start the stirring or swirl device, the starting power of the stirring or swirl device is adjusted according to the discrete degree of the temperature at different parts in the loading container, so that the greater the temperature difference at different parts of the cooling medium in the loading container, the higher the power of the stirring or swirl device, so as to quickly neutralize the temperature of the cooling medium at different parts, and quickly improve the cooling uniformity of the casting.
[0073] The preferred embodiments of the present invention disclosed above are only used to help explain the present invention. The preferred embodiments do not describe all the details in detail, nor do they limit the invention to only specific implementation methods. Obviously, many modifications and changes can be made according to the content of this specification. This specification selects and specifically describes these embodiments in order to better explain the principles and practical applications of the present invention, so that those skilled in the art can understand and use the present invention well. The present invention is limited only by the claims and their full scope and equivalents.
Claims
1. Used for optimization control system in the cooling process of aluminum castings, It is characterized in that include: The temperature monitoring unit is used to monitor the surface and internal temperature distribution of the casting using an array temperature monitoring method. The specific steps are as follows: Firstly, the key monitoring area of the casting is determined, and the casting is divided into different areas according to logic. The importance of different areas is judged. The wall thickness, thermal gradient, cold time value, thermal node value, stress value, missing value and shape evaluation value of the key monitoring area are obtained by collecting the re-evaluation parameters of different areas of the casting for comprehensive analysis. After normalization, the product of wall thickness and thermal gradient plus cold time value is used as the bottom circle radius to establish the bottom circle, and the sum of thermal node value, stress value and missing value is used as the height to establish the cone model. The vertex of the cone model is selected as the center of the sphere, and the shape evaluation value multiplied by the weight factor is used as the diameter to establish the spherical model. Then calculate the surface area of the irregular body formed by the cone and the sphere, and record it as the re-judgment value, and use this re-judgment value as the criterion for measuring the importance of the area; The re-judgment values obtained from all the segmented areas of the casting are sorted by size, and the areas with the re-judgment values in the first half are selected as the key monitoring areas for temperature monitoring; Arrange temperature sensors in key monitoring areas. After completing the arrangement of temperature sensors, analyze the areas where there are blind spots larger than the preset blind spots, and arrange additional temperature sensors in the areas to achieve an array layout for the entire casting. Configure the data acquisition function to collect sensor data and set the sampling frequency to ensure that the temperature changes in the key areas of the casting are captured during the cooling process of the casting; The analysis process of wall thickness, thermal gradient, cold time value, thermal node value, stress value, absence value and shape evaluation value in the key monitoring area is as follows: Thick wall is the average wall thickness of the casting in this area. When the average wall thickness is larger, the area needs a longer cooling time and its importance is higher. The thermal gradient is the temperature difference between the inside and the surface or different parts of the casting in this area. When the thermal gradient is larger, the cooling importance is higher; The cooling rate requirement is measured by the time required for cooling the area. When different parts of the area require different cooling times, the average cooling time of all parts of the area is calculated and recorded as the cooling time value. The smaller the cooling time value, the higher the cooling importance of the area. The local hot spot and stress concentration area is the total area of the local hot spot or hot spot and stress concentration area in the casting in this area, which is recorded as the hot spot value and stress value respectively. When there is no local hot spot or hot spot and stress concentration area in this area, the hot spot value and stress value of this area are 0. The larger the hot spot value or stress value, the higher the cooling demand and the corresponding cooling importance. The historical defect record is the number of cooling defects that occurred in the area, which is recorded as the absence value, and this absence value is used as a standard to measure the importance of the historical defect record in the area; The regional geometry is to assign a complexity score of 1-100 to the geometry of the region of the casting and record it as the shape evaluation value. This shape evaluation value is used as a standard to measure the geometry of the region. The larger the shape evaluation value, the greater the complexity of the geometry of the region, and the higher the corresponding cooling importance. The temperature analysis unit is used to monitor the temperature of the key areas of the casting and determine cooling abnormalities; the specific steps are as follows: The temperatures monitored in different key areas are recorded as , after normalization, enter the following formula: Get the mean temperature , where The temperature monitored for each critical area; Then the temperature average Substitute the following formula: To obtain the variance of temperature in different key areas , and then the obtained variance Compare with the preset threshold, when the variance When it is greater than a preset threshold, it is judged that there is uneven cooling during the cooling operation of the casting, and a cooling signal is generated; Then, a temperature curve is established for the temperatures monitored in different key areas, with the horizontal axis being time and the vertical axis being temperature value; The temperature drop standard curve of different regions of the casting when cooling is obtained by analyzing the historical records of the cooling of the same type of castings, and the temperature drop standard curve is bidirectionally expanded according to the preset standard to form a standard range of the temperature drop curve; Then, the temperature curve established by the temperature monitored in different key areas is compared with the standard interval of the temperature drop curve obtained by analysis to determine whether there is a situation where the temperature curve trends outside the standard interval of the temperature drop curve. When the temperature curve trends outside the standard interval of the temperature drop curve, the time when the temperature curve trends outside the standard interval of the temperature drop curve is recorded. When the time exceeds the preset time threshold, it is determined that the cooling temperature drop of the casting in this area is abnormal, and an abnormal signal is generated; The cooling control unit is used to perform corresponding cooling control according to cooling abnormalities. The specific operation steps are as follows: After receiving the cold average signaling, the temperature monitored in all key areas is obtained and the difference between the temperature monitored in the key areas and the temperature average is calculated, and the obtained temperature difference is compared with the preset difference threshold. When the temperature difference is greater than the preset difference threshold, the corresponding key area is marked; Then, by comparing the received abnormal signaling and the temperature drop curve of the corresponding key area with the standard range of the temperature drop curve, it is determined whether the marked key area is an area that cools too fast or an area that cools too slowly; The specific cooling control steps for areas that cool too slowly are as follows: First, obtain the specific location of the slow cooling area in the casting, and use the cooling attachment for the slow cooling area; Then, the temperature of the cooling medium in the area is lowered gradually, and the flow rate of the cooling medium is increased to improve the cooling speed; Then, the device holding the casting is controlled to rotate or move so that the area where the casting cools too slowly is closer to the cooling water channel. At the same time, the cross-sectional area of the cooling water channel is increased. In combination with accelerated cooling technology, the insulation material in the area where the casting cools too slowly is reduced or unnecessary insulation layers are removed. The specific cooling control steps for areas that cool too quickly are as follows: First, the specific location of the area where the cooling is too slow in the casting is obtained, and the temperature of the cooling medium or air is increased for the area where the cooling is too fast, the cooling speed is slowed down, and the flow rate of the cooling medium is adjusted to reduce the flow rate of the cooling medium and reduce the cooling intensity; At the same time, add insulation materials around the area where cooling is too fast to slow down heat transfer, and then use local heating equipment, including heating belts or heating pads, to balance the cooling rate in the area where cooling is too fast, extending the cooling time of the entire casting to compensate for the rapid cooling of the local area.
2. The optimized control system for cooling aluminum castings according to claim 1, It is characterized in that The cooling control unit implements a dynamic cooling control strategy during the cooling control process, monitors in real time whether the temperature drop curve of the regional casting returns to the standard range of the temperature drop curve, and determines whether it is necessary to suspend cooling control or reduce control intensity.
3. The optimized control system for cooling of aluminum castings according to claim 1, It is characterized in that The specific operation steps of the cooling control unit to implement the uniform cooling mechanism are as follows: First, count the total number of areas that cool too fast or too slow, and calculate the ratio to all key areas, which is recorded as the abnormal ratio; The obtained abnormal proportion is compared with the preset proportion threshold. When the abnormal proportion is greater than the preset proportion threshold, it is judged that the temperature of the cooling medium around the cooling of the casting is not uniform enough, and the immersion cooling method is enabled, specifically, by immersing the entire casting in the cooling medium, and stirring and neutralizing the cooling medium with a stirring or swirl device, thereby neutralizing the temperature of the cooling medium, so that the cooling of different areas of the casting by the cooling medium is more uniform; Then, temperature sensors are evenly arranged at different positions in the cooling medium loading container to monitor the real-time temperature of the cooling medium in the loading container in real time; Then, according to the degree of discreteness of the temperature values of the temperature sensors at different parts, it is determined whether it is necessary to start the stirring or swirling device to neutralize the cooling medium. When it is necessary to start the stirring or swirling device, the starting power of the stirring or swirling device is adjusted according to the degree of discreteness of the temperature at different parts in the loading container, so that the greater the temperature difference at different parts of the cooling medium in the loading container, the higher the power of the stirring or swirling device, so as to quickly neutralize the temperature of the cooling medium at different parts and quickly improve the cooling uniformity of the casting.
Citation Information
Patent Citations
Internal temperature monitoring device and monitoring method for heavy casting in cooling process
CN108380855A
Temperature control system applied to probiotic fermentation
CN118460362A