Processing method of ceiling metal skylight reinforcement frame
By dividing the metal skylight reinforcement frame into four independent secondary molded parts and riveted and fixed, the problem of material waste in traditional processing methods is solved, and cost reduction and strength guarantee are achieved.
Patent Information
- Application Number
- CN202411172181.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-26
- Publication Date
- 2024-11-22
- Estimated Expiration
- 2044-08-26
AI Technical Summary
The processing method of traditional metal skylight reinforced frames leads to waste of raw materials and increases production costs.
By dividing the metal skylight reinforcement frame into four independent secondary molded parts for split processing and fixing through riveting, the dependence on the entire board is reduced, material utilization is improved, and no additional riveting material is achieved through riveting holes fixed.
It effectively reduces manufacturing costs, improves product strength and material utilization, and reduces the demand for large-area sheets.
Smart Images

Figure CN118682000B_ABST
Abstract
Description
Technical Field
[0001] The present application relates to the field of ceiling metal skylight reinforcement frame processing equipment, and in particular to a ceiling metal skylight reinforcement frame processing method. Background Art
[0002] In some higher-configuration cars, a skylight will be installed on the top of the car. Although the setting of the car sunroof can increase the lighting and ventilation functions inside the vehicle, in the design of the car, not only the lighting and ventilation of the vehicle should be considered, but also the compressive strength of the skylight, etc. Therefore, many manufacturers will install a metal skylight reinforcement frame with a frame-type structure at the car sunroof to increase the strength here.
[0003] The current traditional processing method of metal skylight reinforcement frames is: placing the entire plate into a larger stamping and stretching die for stamping and stretching to form a primary molded part, which includes a frame-shaped structure and the middle plate. The primary molded part is then placed into a stamping and trimming die to stamp out all the plates except the frame structure, thereby forming a metal skylight reinforcement frame with a frame structure.
[0004] However, the inventor believes that although this traditional processing method can ensure the integrity and strength of the metal skylight reinforcement frame, the material consumption is too serious. It can be seen from the above processing method that most of the material will be cut off during the process of processing the entire plate into a metal skylight reinforcement frame, which undoubtedly causes a large amount of raw materials. Waste, greatly increases the procurement cost of manufacturers, and the manufacturing cost also increases accordingly. Summary of the invention
[0005] In order to minimize the manufacturing cost of the product and improve the utilization rate of raw materials without reducing the product strength as much as possible.
[0006] The present application provides a method for processing a ceiling metal skylight reinforcement frame, which adopts the following technical solution:
[0007] A method for processing a ceiling metal skylight reinforcement frame, characterized in that it comprises the following steps:
[0008] Step 1: Place the plate to be processed into a stamping and stretching die, and perform stamping and stretching to form an O-shaped primary molded part;
[0009] Step 2: Place the primary molded part into a stamping and trimming die, and perform stamping and trimming processing on the middle parts of the two opposite ends of the primary molded part at the same time, so that each primary molded part forms two independent secondary molded parts;
[0010] Step 3: Punching at opposite ends of the secondary molded part to form at least two spaced rivet holes with flanges;
[0011] Step 4: four secondary molded parts with flanged rivet holes are placed into a forming stamping die to form a frame structure, and adjacent ends of adjacent secondary molded parts are overlapped with each other so that the rivet holes of adjacent ends of adjacent secondary molded parts are all in one-to-one correspondence;
[0012] Step 5: The forming stamping die is closed to make the flange of the rivet hole be stamped again in a direction away from the center of the rivet hole, so that the adjacent ends of the adjacent secondary molded parts are riveted from the rivet hole;
[0013] Among them, step 2 and step 3 can be carried out simultaneously in the stamping and trimming die, or the processing order of step 2 and step 3 can be swapped.
[0014] In some embodiments, the stamping and stretching die includes a first upper die and a first lower die, the first upper die includes at least one group of first upper die cavities, each group of first upper die cavities includes two first upper die cavities, and the adjacent ends of the two first upper die cavities are connected by an upper connecting cavity; the first lower die includes at least one group of first lower die cavities, the position and number of the first lower die cavities correspond to the first upper die cavities, each group of first lower die cavities includes two first lower die cavities, and the adjacent ends of the first lower die cavities are connected by a lower connecting cavity, and after the first upper die and the first lower die are closed, each group of first upper die cavities and the corresponding first lower die cavities form an O-shaped first molding cavity.
[0015] In some embodiments, at least two first grooves spaced apart are respectively provided at the opposite ends of each of the first upper cavities, and stamping protrusions corresponding in position and number to the first grooves are respectively provided at the opposite ends of each of the first lower cavities, and a gap is left between the stamping protrusions and the first grooves after the mold is closed.
[0016] In some embodiments, the stamping and trimming mold includes a second upper mold and a second lower mold, the second upper mold includes at least one group of second upper mold cavities, each group of second upper mold cavities includes two independent second upper mold cavities; the second lower mold includes at least one group of second lower mold cavities, the position and number of the second lower mold cavities correspond to the second upper mold cavities, each group of second lower mold cavities includes two independent second lower mold cavities, and after the second upper mold and the second lower mold are combined, each second upper cavity and the corresponding second lower cavity form an independent second molding cavity.
[0017] In some embodiments, the adjacent ends of the two second upper mold cavities in each group of the second upper mold cavities are separated by a trimming boss; a partition area is provided between the adjacent ends of the two second lower mold cavities in each group of the second lower mold cavities, and the trimming boss cooperates with the partition area at the corresponding position for trimming.
[0018] In some embodiments, at least two second grooves are arranged at intervals at the opposite ends of each of the second upper cavities, the second upper mold is provided with a first punch hole connected to the middle part of the bottom of each second groove, and the second upper mold is provided with a first punch needle which can be axially displaced relative to the corresponding first punch hole in each first punch hole; punch holes corresponding to the positions and numbers of the second grooves are arranged at the opposite ends of each of the second lower cavities, and an annular positioning stop edge is arranged at the mouth of each punch hole in the second lower cavity, and a gap is left between the positioning stop edge and the second groove after the mold is closed.
[0019] In some embodiments, the forming stamping die includes a third upper die and a third lower die, the third upper die includes at least one third upper die cavity, each third upper die cavity includes four third upper cavities, and the four third upper cavities are connected end to end in sequence to form a third upper die cavity with a frame structure; the third lower die includes at least one third lower die cavity, the position and number of the third lower die cavities correspond to the third upper die cavity, each third lower die cavity includes four third lower cavities, and the four third lower cavities are connected end to end in sequence to form a third lower die cavity with a frame structure, and after the third upper die and the third lower die are closed, each third upper die cavity and the corresponding third lower die cavity form a third molding cavity with a frame structure.
[0020] In some embodiments, each of the third upper die cavities is respectively provided with four groups of punching holes, each group of punching holes includes a plurality of second punching holes arranged at intervals, and the third upper die is provided with a second punch needle that can be axially displaced relative to the corresponding second punching hole in each second punching hole, and each group of punching holes is correspondingly arranged at each corner of the third upper die cavity or at a position close to the corresponding corner; each third lower die cavity is respectively provided with four support seats, and the support seats correspond one-to-one to each group of punching holes in the corresponding third upper die cavity.
[0021] In some embodiments, a positioning shaft is provided in the middle of the end surface of the second punch needle facing the third lower die, and each support seat is provided with third grooves whose number and position are matched with the second punch holes of the corresponding group of punching holes, and a positioning hole matched with the positioning shaft is provided in the middle of the bottom of the third groove.
[0022] In some embodiments, an annular groove is provided around the positioning shaft on the end surface of the second punch facing the third lower die, and the bottom of the annular groove is arranged in an arc shape. An expansion portion with an outer diameter gradually increasing is provided toward the annular groove at one end of the positioning shaft close to the annular groove, and the expansion portion is connected to the annular groove; a guide end is provided at the end of the positioning shaft away from the annular groove, and the outer diameter of the guide end gradually decreases in the direction away from the annular groove.
[0023] In summary, the present application includes at least one of the following beneficial technical effects: by dividing the metal skylight reinforcement frame into four parts for separate processing and forming, and by riveting and fixing the four separately processed secondary molded parts, the utilization rate of raw materials is effectively improved in the entire processing process. There is no need to use a large-area whole plate, but a smaller area plate can be used for processing, so that the procurement cost is greatly reduced and the manufacturing cost is also minimized. At the same time, through the design of the structure of the secondary molded part itself, the rivet holes can be used to achieve riveting fixation in the final molding process, without the need for additional riveting materials, thereby improving the utilization rate of the product itself, and the secondary molded parts at the riveted joints are fixed by double overlapping, so that the strength of the connection can be maximized. BRIEF DESCRIPTION OF THE DRAWINGS
[0024] Figure 1 It is a structural schematic diagram of the first upper mold in a method for processing a ceiling metal skylight reinforcement frame in an embodiment of the present application.
[0025] Figure 2 yes Figure 1 Schematic diagram of the local enlarged structure of part A.
[0026] Figure 3 yes Figure 1 Schematic diagram of the local enlarged structure of part B.
[0027] Figure 4 It is a structural schematic diagram of the first lower mold in a method for processing a ceiling metal skylight reinforcement frame in an embodiment of the present application.
[0028] Figure 5 yes Figure 4 Schematic diagram of the local enlarged structure of part C in the middle.
[0029] Figure 6 yes Figure 4 Schematic diagram of the local enlarged structure of part D in the middle.
[0030] Figure 7 It is a structural schematic diagram of a second upper mold in a method for processing a ceiling metal skylight reinforcement frame in an embodiment of the present application.
[0031] Figure 8 yes Figure 7 Schematic diagram of the local enlarged structure of part E in the middle.
[0032] Fig. 9 yes Figure 7 Schematic diagram of the local enlarged structure of part F in the middle.
[0033] Fig.10 It is a structural schematic diagram of the second lower mold in a method for processing a ceiling metal skylight reinforcement frame in an embodiment of the present application.
[0034] Fig.11 yes Fig.10 Schematic diagram of the local enlarged structure of part G in the middle.
[0035] Fig.12 yes Fig.10 Schematic diagram of the local enlarged structure of part H in the middle.
[0036] Fig.13 It is a structural schematic diagram of a third upper mold in a method for processing a ceiling metal skylight reinforcement frame in an embodiment of the present application.
[0037] Fig.14 yes Fig.13 Schematic diagram of the local enlarged structure of part I.
[0038] Fig.15 It is a schematic diagram of the partial cross-sectional structure of a second punch pin in a method for processing a ceiling metal skylight reinforcement frame in an embodiment of the present application.
[0039] Fig.16 It is a structural schematic diagram of a third lower mold in a method for processing a ceiling metal skylight reinforcement frame in an embodiment of the present application.
[0040] Fig.17 yes Fig.16 Schematic diagram of the local enlarged structure of part J in the middle.
[0041] Explanation of the accompanying drawings: 1. first upper cavity; 2. upper connecting cavity; 3. first lower cavity; 4. lower connecting cavity; 5. first groove; 6. stamping protrusion; 7. second upper cavity; 8. second lower cavity; 9. trimming boss; 10. partition area; 11. second groove; 12. first punch needle; 13. punching hole; 14. positioning stop edge; 15. third upper cavity; 16. third lower cavity; 17. second punch needle; 18. support seat; 19. positioning shaft; 20. third groove; 21. positioning hole; 22. annular groove; 23. expansion portion; 24. guide end. DETAILED DESCRIPTION
[0042] The following is combined with Figures 1 to 17 This application is described in further detail.
[0043] The present application embodiment discloses a method for processing a ceiling metal skylight reinforcement frame, comprising the following steps:
[0044] Step 1: Place the plate to be processed into a stamping and stretching die, and perform stamping and stretching to form an O-shaped primary molded part;
[0045] Step 2: Place the primary molded part into a stamping and trimming die, and perform stamping and trimming processing on the middle parts of the two opposite ends of the primary molded part at the same time, so that each primary molded part forms two independent secondary molded parts;
[0046] Step 3: Punching at opposite ends of the secondary molded part to form at least two spaced rivet holes with flanges;
[0047] Step 4: four secondary molded parts with flanged rivet holes are placed into a forming stamping die to form a frame structure, and adjacent ends of adjacent secondary molded parts are overlapped with each other so that the rivet holes of adjacent ends of adjacent secondary molded parts are all in one-to-one correspondence;
[0048] Step 5: The forming stamping die is closed to make the flange of the rivet hole be stamped again in a direction away from the center of the rivet hole, so that the adjacent ends of the adjacent secondary molded parts are riveted from the rivet hole;
[0049] Among them, step two and step three can be carried out simultaneously in the stamping trimming mold, or the processing order of step two and step three can be swapped, that is, if step two and step three do not need to be carried out simultaneously, step two can be carried out first and then step three, or step three can be carried out first and then step two. If step two and step three are carried out simultaneously, on the one hand, processing time can be saved and processing efficiency can be improved, and on the other hand, the use of molds can be reduced, which can effectively control manufacturing costs.
[0050] Reference Figures 1 to 6 In this embodiment, the stamping and stretching die used in step one includes a first upper die and a first lower die, the first upper die includes at least one group of first upper die cavities, each group of first upper die cavities includes two first upper die cavities 1, and the adjacent ends of the two first upper die cavities 1 are connected through an upper connecting cavity 2; the first lower die includes at least one group of first lower die cavities, the position and number of the first lower die cavities correspond to those of the first upper die cavities, each group of first lower die cavities includes two first lower die cavities 3, and the adjacent ends of the first lower die cavities 3 are connected through a lower connecting cavity 4, after the first upper die and the first lower die are closed, each group of first upper die cavities and the first lower die cavities corresponding to the position form an O-shaped first molding cavity; in this embodiment, the first upper die cavities are divided into two groups and the first lower die cavities are divided into two groups for explanation, the two groups of first upper die cavities and the two groups of first lower die cavities can form two O-shaped first molding cavities, and the two first molding cavities can simultaneously form two O-shaped primary molded parts.
[0051] In order to enable the product to form a riveted structure using its own structure in subsequent processing, the initial shape of the riveted structure can be formed in the process of forming the initial molded part, that is, at least two first grooves 5 spaced apart can be provided at the opposite ends of each first upper cavity 1, and stamping protrusions 6 corresponding in position and number to the first grooves 5 can be provided at the opposite ends of each first lower cavity 3. After the mold is closed, a gap is left between the stamping protrusion 6 and the first groove 5, that is, after the mold is closed, a protrusion structure will be formed on the plate to be processed between the stamping protrusion 6 and the first groove 5.
[0052] Reference Figures 7 to 12 In this embodiment, the stamping and trimming mold in step two and step three includes a second upper mold and a second lower mold, the second upper mold includes at least one group of second upper mold cavities, each group of second upper mold cavities includes two independent second upper mold cavities 7; the second lower mold includes at least one group of second lower mold cavities, the position and number of the second lower mold cavities correspond to the second upper mold cavities, each group of second lower mold cavities includes two independent second lower mold cavities 8, after the second upper mold and the second lower mold are combined, each second upper mold cavity 7 and the second lower mold cavity 8 corresponding to the position form an independent second molding cavity; in this embodiment, the second upper mold cavity is divided into two groups and the second lower mold cavity is divided into two groups for explanation, and the two groups of second upper mold cavities and the two groups of second lower mold cavities can form four independent second molding cavities.
[0053] Among them, the adjacent ends of the two second upper cavities 7 in each group of second upper cavities are separated by a trimming boss 9; a partition area 10 is arranged between the adjacent ends of the two second lower cavities 8 in each group of second lower cavities, and the trimming boss 9 cooperates with the partition area 10 at the corresponding position for trimming, that is, after the mold is closed, except for the part where the primary molded part is adapted to the two independent second molding cavities in the corresponding group, part of the primary molded part at the corresponding position of the trimming boss 9 and the partition area 10 will be cut off, that is, it can be understood that in the stamping and stretching die, the primary molded part itself is composed of two parts that can be divided into two independent parts, but because a complete plate is used during the initial stamping and stretching, there will be an intermediate connecting part between the adjacent ends of the two independent parts, and after stamping and trimming in the stamping and trimming die, the intermediate connecting part is cut off, so that each primary molded part forms two independent secondary molded parts, and the four second molding cavities can form four independent secondary molded parts, that is to say, processing in two groups can effectively improve the processing efficiency of the product.
[0054] In this embodiment, at least two second grooves 11 are arranged at intervals at the opposite ends of each second upper cavity 7 in the stamping trimming die, the second upper die is provided with a first punching hole connected to the middle part of the groove bottom of each second groove 11, and the second upper die is installed with a first punching needle 12 in each first punching hole that can be axially displaced relative to the corresponding first punching hole; at the opposite ends of each second lower cavity 8, punching holes 13 corresponding in position and number to the second grooves 11 are arranged, and an annular positioning stop edge 1 is arranged at the opening of each punching hole 13 in the second lower cavity 8. 4. After the mold is closed, a gap is left between the positioning stop 14 and the second groove 11. When punching the riveting hole after the mold is closed, the driving component in the second upper mold drives the first punch needle 12 to punch along the axial direction of the first punch hole toward the second lower mold. During the punching process, the positioning stop 14 and the corresponding second groove 11 are formed to ensure that the raised structure of the secondary molded part here will not produce a large deformation, and the raised structure of the secondary molded part corresponding to the first punch needle 12 will be broken by the first punch needle 12, and as the first punch needle 12 continues to punch, a flange is formed toward the second lower mold.
[0055] In order to enable the first punch needle 12 to achieve rapid breakthrough, the first punch needle 12 can be tilted toward the end face of the second lower mold, or the first punch needle 12 can be provided with a conical tip toward the end face of the second lower mold. In this way, when the first punch needle 12 contacts the corresponding raised structure of the secondary molded part, the force bearing area is reduced and the pressure point is more concentrated, so that the effect of rapid breakthrough can be achieved. At the same time, in order to ensure that the first punch needle 12 can smoothly achieve the effect of driving the flanging, the diameter of the first punch needle 12 can be designed to be smaller than the diameter of the corresponding punching hole 13.
[0056] Reference Figures 13 to 17 The forming stamping die in step four and step five includes a third upper die and a third lower die, the third upper die includes at least one third upper die cavity, each third upper die cavity includes four third upper cavities 15, and the four third upper cavities 15 are connected end to end in sequence to form a third upper die cavity with a frame-type structure; the third lower die includes at least one third lower die cavity, the position and number of the third lower die cavities correspond to those of the third upper die cavity, each third lower die cavity includes four third lower cavities 16, and the four third lower cavities 16 are connected end to end in sequence to form a third lower die cavity with a frame-type structure, and after the third upper die and the third lower die are closed, each third upper die cavity forms a third molding cavity with a frame-type structure with the corresponding third lower die cavity.
[0057] During processing, the four independent secondary molded parts mentioned above can be placed in the third molding cavity to form a frame-type structure, and the adjacent ends of adjacent secondary molded parts overlap each other. After overlapping each other, the rivet holes at the adjacent ends of adjacent secondary molded parts can correspond one to one. In order to enable the secondary molded parts that form the frame-type structure to be riveted using their own structures, each third upper mold cavity is respectively provided with four groups of punching holes, each group of punching holes includes a plurality of second punching holes arranged at intervals, and the third upper mold is installed with a second punching needle 17 axially displaceable relative to the corresponding second punching hole in each second punching hole, wherein each group of punching holes is correspondingly arranged at each corner of the third upper mold cavity or at a position close to the corresponding corner, and the second punching needle 17 forms a one-to-one correspondence with the rivet holes of the secondary molded parts at the corresponding positions.
[0058] At the same time, each third lower die cavity is respectively provided with four support seats 18, and the support seats 18 correspond one-to-one to each group of punching holes in the corresponding third upper die cavity. In addition, a positioning shaft 19 is provided in the middle of the end surface of the second punch needle 17 facing the third lower die, and each support seat 18 is provided with a third groove 20 whose number and position are matched with the second punching holes of the corresponding group of punching holes, and a positioning hole 21 matched with the positioning shaft 19 is provided in the middle of the groove bottom of the third groove 20. In order to enable the flange at each riveting hole to form a riveted fixed relationship after flanging again, an annular groove 22 is provided around the positioning shaft 19 on the end surface of the second punch needle 17 facing the third lower die, and the groove bottom of the annular groove 22 is arranged in an arc shape, so that the flange can be bent along the groove bottom of the annular groove 22 toward the third lower die. At the same time, in order to ensure that the flange at the riveting hole can In order to smoothly enter the annular groove 22, an expansion portion 23 with a gradually increasing outer diameter can be provided at one end of the positioning shaft 19 close to the annular groove 22 and facing the annular groove 22, and the expansion portion 23 is connected to the annular groove 22, so that during the stamping process, the flange at the riveted joint is firstly gradually flanged along the expansion portion 23 in the direction away from the center of the riveting hole, and when reaching the annular groove 22, it can be bent and flanged again, so that the riveted structure of the flange at the riveted joint can be ensured to be more stable and reliable, and the end of the flange will not be exposed, so that it can be ensured to remain flush with the final molded product; in addition, in order to enable it to pass through the riveting hole more quickly and accurately into the guide hole, a guide end head 24 can be provided at the end of the positioning shaft 19 away from the annular groove 22, and the outer diameter of the guide end head 24 gradually decreases in the direction away from the annular groove 22.
[0059] In the present embodiment, it should be noted that the first punch pin 12 and the second punch pin 17 are driven by the driving mechanism in their corresponding molds for axial displacement, and the driving mechanism can be a cylinder, a hydraulic cylinder, etc., and these driving mechanisms and driving methods are conventional designs in traditional mold manufacturing, so no additional explanation is given in the present embodiment.
[0060] The above are all preferred embodiments of the present application, and the protection scope of the present application is not limited thereto. Therefore, any equivalent changes made according to the structure, shape, and principle of the present application should be included in the protection scope of the present application.
Claims
1. A method for processing a ceiling metal skylight reinforcement frame, characterized in that: The steps include: Step 1: Place the plate to be processed into a stamping and stretching die, and perform stamping and stretching to form an O-shaped primary molded part; Step 2: Place the primary molded part into a stamping and trimming die, and perform stamping and trimming processing on the middle parts of the two opposite ends of the primary molded part at the same time, so that each primary molded part forms two independent secondary molded parts; Step 3: Punching two opposite ends of the secondary molded part to form at least two spaced rivet holes with flanges; Step 4: four secondary molded parts with flanged rivet holes are placed into a forming stamping die to form a frame structure, and adjacent ends of adjacent secondary molded parts are overlapped with each other so that the rivet holes of adjacent ends of adjacent secondary molded parts are all in one-to-one correspondence; Step 5: The forming stamping die is closed to make the flange of the rivet hole be stamped again in a direction away from the center of the rivet hole, so that the adjacent ends of the adjacent secondary molded parts are riveted from the rivet hole; Wherein, step 2 and step 3 can be performed simultaneously in the stamping and trimming die, or the processing order of step 2 and step 3 can be reversed; The stamping and stretching die comprises a first upper die and a first lower die, the first upper die comprises at least one group of first upper die cavities, each group of first upper die cavities comprises two first upper die cavities (1), and the adjacent ends of the two first upper die cavities (1) are connected via an upper connecting cavity (2); the first lower die comprises at least one group of first lower die cavities, the positions and number of the first lower die cavities correspond to those of the first upper die cavities, each group of first lower die cavities comprises two first lower die cavities (3), and the adjacent ends of the first lower die cavities (3) are connected via a lower connecting cavity (4), and after the first upper die and the first lower die are closed, each group of first upper die cavities and the first lower die cavities corresponding in position form an O-shaped first molding cavity; At least two first grooves (5) are arranged at intervals at the opposite ends of each first upper cavity (1), and at least two first grooves (5) are arranged at the opposite ends of each first lower cavity (3), and the positions and numbers of stamping protrusions (6) corresponding to the first grooves (5) are arranged at the opposite ends of each first lower cavity (3), and a gap is left between the stamping protrusions (6) and the first grooves (5) after the mold is closed.
2. The method for processing a ceiling metal skylight reinforcement frame according to claim 1, characterized in that: The stamping trimming die comprises a second upper die and a second lower die, the second upper die comprises at least one group of second upper die cavities, each group of second upper die cavities comprises two independent second upper cavities (7); the second lower die comprises at least one group of second lower die cavities, the positions and number of the second lower die cavities correspond to those of the second upper die cavities, each group of second lower die cavities comprises two independent second lower cavities (8), and after the second upper die and the second lower die are closed, each second upper cavity (7) forms an independent second molding cavity with the second lower cavity (8) corresponding to the position.
3. The method for processing a ceiling metal skylight reinforcement frame according to claim 2, characterized in that: The adjacent ends of the two second upper cavities (7) in each group of the second upper cavities are separated by a trimming boss (9); a partition area (10) is provided between the adjacent ends of the two second lower cavities (8) in each group of the second lower cavities, and the trimming boss (9) cooperates with the partition area (10) at the corresponding position for trimming.
4. The method for processing a ceiling metal skylight reinforcement frame according to claim 2, characterized in that: At the opposite ends of each second upper cavity (7), at least two second grooves (11) are arranged at intervals, the second upper die is provided with a first punching hole connected to the middle part of the groove bottom of each second groove (11), and the second upper die is provided with a first punching needle (12) which can be axially displaced relative to the corresponding first punching hole in each first punching hole; at the opposite ends of each second lower cavity (8), punching holes (13) whose positions and numbers correspond to the second grooves (11) are arranged, and an annular positioning stop edge (14) is arranged at the opening of each punching hole (13) in the second lower cavity (8), and a gap is left between the positioning stop edge (14) and the second groove (11) after the mold is closed.
5. The method for processing a ceiling metal skylight reinforcement frame according to claim 1, characterized in that: The forming stamping die comprises a third upper die and a third lower die, the third upper die comprises at least one third upper die cavity, each of the third upper die cavities comprises four third upper die cavities (15), the four third upper die cavities (15) are connected end to end in sequence to form a third upper die cavity of a frame-type structure; the third lower die comprises at least one third lower die cavity, the position and number of the third lower die cavities correspond to those of the third upper die cavity, each of the third lower die cavities comprises four third lower die cavities (16), the four third lower die cavities (16) are connected end to end in sequence to form a third lower die cavity of a frame-type structure, and after the third upper die and the third lower die are closed, each third upper die cavity and the third lower die cavity corresponding in position form a third forming cavity of a frame-type structure.
6. The method for processing a ceiling metal skylight reinforcement frame according to claim 5, characterized in that: Each of the third upper die cavities is respectively provided with four groups of punching holes, each group of punching holes includes a plurality of second punching holes arranged at intervals, and the third upper die is provided with a second punching needle (17) which can be axially displaced relative to the corresponding second punching hole in each second punching hole, and each group of punching holes is correspondingly arranged at each corner of the third upper die cavity or at a position close to the corresponding corner; each of the third lower die cavities is respectively provided with four support seats (18), and the support seats (18) correspond one-to-one to each group of punching holes in the corresponding third upper die cavity.
7. The method for processing a ceiling metal skylight reinforcement frame according to claim 6, characterized in that: A positioning shaft (19) is arranged in the middle of the end surface of the second punching needle (17) facing the third lower die, and each support seat (18) is provided with a third groove (20) whose number and position are matched with the second punching holes of the corresponding group of punching holes, and a positioning hole (21) matched with the positioning shaft (19) is arranged in the middle of the groove bottom of the third groove (20).
8. The method for processing a ceiling metal skylight reinforcement frame according to claim 7, characterized in that: The end surface of the second punch needle (17) facing the third lower die is provided with an annular groove (22) around the positioning shaft (19), the bottom of the annular groove (22) is arranged in an arc shape, and the positioning shaft (19) is provided with an expanding portion (23) with an outer diameter gradually increasing towards the annular groove (22) at one end close to the annular groove (22), and the expanding portion (23) is connected to the annular groove (22); the end of the positioning shaft (19) away from the annular groove (22) is provided with a guide end head (24), and the outer diameter of the guide end head (24) gradually decreases in the direction away from the annular groove (22).