Preparation method of dental polymer-based temporary filling material
By mixing specific chemicals at a temperature of 50°C to prepare dental polymer-based temporary filling materials, the problem of adverse patient reactions caused by heat release when dental bonding restoration materials are cured is solved, and the material's high elasticity, compressive strength and easy removal are achieved. properties, enhanced antibacterial and antioxidant properties.
Patent Information
- Application Number
- CN202410675387.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-05-29
- Publication Date
- 2024-10-01
AI Technical Summary
Existing dental bonding restoration materials release a large amount of heat when curing, causing patients' tooth sensitivity, pain, oral mucosal burns, and may even cause pulpitis, and are difficult to completely remove.
A method for preparing dental polymer-based temporary filling materials is adopted, by mixing methacrylate monomers, acrylates, fluoride, photoinitiators, flavors, polymerization inhibitors and fillers at a temperature of 50°C. Stir and vacuum to ensure the material has high elasticity and compressive strength and is easy to remove.
This method improves the fluidity and mechanical properties of the material, increases the antibacterial and antioxidant effects, ensures the accessibility and integrity of the material after tooth filling, and reduces adverse patient reactions.
Smart Images

Figure CN118717536A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the field of dental medical technology, and in particular to a method for preparing a polymer-based temporary filling material for dentistry. Background Art
[0002] For a long time, the monomers in the production raw materials of intraoral curing materials for dental bonding and restoration, such as light-curing composite resins, light-curing fluid resins, light-curing pit and fissure sealants, light-curing / chemically curing temporary crown and bridge materials, light-curing temporary filling materials, orthodontic resin bonding materials, light-curing / chemically curing post and core materials, light-curing / chemically curing resin cement materials, light-curing adhesives, etc., are mostly acrylic monomers, which are cured by polymerization when used. The polymerization reaction is an exothermic reaction, so this type of material releases a lot of heat and high temperature when curing. When curing is completed in the mouth, patients often have many adverse reactions, such as allergic and painful teeth, burns to the oral mucosa and tongue, and some patients may develop pulpitis, and then take anti-inflammatory drugs and anti-inflammatory injections. Summary of the invention
[0003] In view of this, the present invention proposes a method for preparing a dental polymer-based temporary filling material, which has high elasticity after polymerization, and at the same time has high compressive strength, and is very easy to remove after the tooth filling operation, and can be removed completely.
[0004] The present invention adopts the following technical solutions to achieve the above technical effects:
[0005] A method for preparing a polymer-based temporary filling material for dentistry comprises the following steps:
[0006] Step 1: Turn on the mold temperature controller and set the temperature to 50°C. Turn on the mold temperature controller circulation pump. After the temperature of the mold temperature controller stabilizes to 50°C, add 70%-80% of methacrylate monomer into the kneader.
[0007] Step 2, after the solvent temperature reaches 50°C, add 2%-5% acrylate and 0.5%-0.8% fluoride;
[0008] Step 3, turn on the kneader and adjust the speed to 30-70r / min, stir until uniform, add 0.1%-0.2% of photoinitiator, add 0.5%-0.8% of flavor, add 0.1%-0.2% of inhibitor, and stir evenly;
[0009] Step 4, after the mixture is uniform, add 20%-30% of filler in 3-4 batches;
[0010] Step 5, after stirring evenly, perform vacuum treatment, and after the vacuum treatment is completed, take out the produced product.
[0011] Furthermore, the acrylate substance in step 2 includes, but is not limited to, one or more of polyamino acrylate, polyalkyl acrylate, sodium polyacrylate, and potassium polyacrylate.
[0012] Furthermore, the fluoride in step 2 includes but is not limited to one or more of sodium fluoride, sodium monofluorophosphate, magnesium fluoride, and strontium fluoride.
[0013] Furthermore, the methacrylate monomer in step 1 includes, but is not limited to, one or more of methyl methacrylate, hydroxyethyl methacrylate, glycidyl methacrylate, tetraethylene glycol dimethacrylate, and ethoxylated bisphenol A diester of methacrylate.
[0014] Furthermore, the flavor in step 3 is menthone.
[0015] Furthermore, the types of the filler include but are not limited to one or more of silicon dioxide, aluminum oxide, zirconium oxide, glass powder, and nano glass fiber.
[0016] Furthermore, the polymerization inhibitor includes, but is not limited to, one or more of γ-terpinene, 2,6-di-tert-butyl-p-cresol, and p-hydroxyanisole.
[0017] Compared with the prior art, the present invention has the following beneficial effects:
[0018] During the manufacturing process of the product of the present invention, the temperature is stabilized at 50°C, which can increase the fluidity of the product and make it easier to mix evenly. As the temperature increases, the activity range of the polymer chain will increase, which is manifested in increased fluidity. However, if the temperature is too high, the molecular chain will decompose, which is particularly obvious for the added polymer active monomers, so the processing temperature is set at 50°C.
[0019] The flavor used in the product is menthone, which not only acts as a flavor, but also has antibacterial effects. γ-terpinene is an inhibitor, but also has antibacterial effects. The two raw materials have a synergistic effect in antibacterial aspects. The addition of fluoride not only has an antibacterial effect, but also has a function of preventing regenerative caries. The two raw materials, γ-terpinene and 2,6-di-tert-butyl-p-cresol, not only act as inhibitors, but also have antioxidant effects, and also act as antioxidants.
[0020] Due to the addition of acrylate substances, the product has high elasticity after polymerization. While being elastic, it also has high compressive strength. After the tooth filling operation, it is very easy to remove and can be removed completely.
[0021] The silica filler used in the product is a silanized filler. Silica is an inorganic non-metallic material, and the resin matrix is an organic material. If silanization is not performed, there will only be physical force between the two phases, and the mechanical properties of the resin will be greatly reduced. The use of silanized silica filler can form silicon-oxygen bonds on the silica material, which will form chemical bonds when combined with the resin. There are both physical forces and chemical bonds in the process, which improves the mechanical properties of the material. BRIEF DESCRIPTION OF THE DRAWINGS
[0022] Figure 1 Schematic diagram for comparison of various embodiments of the present invention. DETAILED DESCRIPTION
[0023] Below, the present invention is further described in conjunction with the accompanying drawings.
[0024] First, turn on the mold temperature controller and set the temperature to 50°C, turn on the mold temperature controller circulation pump, and after the temperature of the mold temperature controller stabilizes to 50°C, add 70%-80% of methacrylate monomers, including but not limited to one or more of methyl methacrylate, hydroxyethyl methacrylate, glycidyl methacrylate, tetraethylene glycol dimethacrylate, and ethoxylated bisphenol A diester, add 2%-5% of acrylate substances, including but not limited to one or more of polyamino acrylate, polyalkyl acrylate, sodium polyacrylate, and potassium polyacrylate, add 0.5%-0.8% of fluoride, including but not limited to one or more of sodium fluoride, sodium monofluorophosphate, magnesium fluoride, and strontium fluoride, and turn on the kneading machine. The speed of the machine is adjusted to 30-70r / min, and the mixture is stirred until uniform. After stirring, 0.1%-0.2% of a photoinitiator is added, including one or two of camphor and TPO, 0.5%-0.8% of a flavor (menthone), and 0.1%-0.2% of a polymerization inhibitor is added, including but not limited to one or more of γ-terpinene, 2,6-di-tert-butyl-p-cresol, and MEHQ, and the mixture is stirred until uniform. After the mixture is uniform, 20%-30% of a filler is added in 3-4 batches, and the types of the filler include but are not limited to one or more of silicon dioxide, aluminum oxide, zirconium oxide, glass powder, and nano-glass fiber. After stirring, a vacuum treatment is performed, and the product produced is taken out after the vacuum treatment is completed.
[0025] The vacuum treatment is performed at a vacuum degree of 0.1 MPa, the kneader speed is adjusted to 4 r / min, and the vacuum is maintained for 30 minutes (more observations are made during this period to prevent high vacuum pressure from causing phase separation of the product).
[0026] The following are further explained through more detailed examples and their resulting performance effects:
[0027] Embodiment 1:
[0028]
[0029] A cylinder with a height of 3 mm and a diameter of 4 mm was made and subjected to a compression test. The compressive strength was measured to be 52.55 MP and the maximum force was 659.97 N.
[0030] Embodiment 2:
[0031]
[0032] A cylinder with a height of 3 mm and a diameter of 4 mm was made and subjected to a compression test. The compressive strength was measured to be 57.27 MP and the maximum force was 719.27 N.
[0033] Further, refer to Figure 1 Comparison of performance characteristics of other embodiments.
[0034] It should be understood that the above description of the specific implementation methods of this patent is only an exemplary description listed to facilitate ordinary technicians in the field to understand the patent scheme, and does not imply that the scope of protection of this patent is limited to these individual examples. Ordinary technicians in this field can fully understand the technical scheme of this patent and, without any creative work, obtain more specific implementation methods by combining technical features, replacing some technical features, adding more technical features, etc. to the examples listed in this patent. All these specific implementation methods are within the scope of the claims of this patent. Therefore, these new specific implementation methods should also be within the scope of protection of this patent.
[0035] In addition, for the purpose of simplifying the description, this patent may not list some common specific implementation schemes, which are naturally conceivable to ordinary technicians in this field after understanding the technical solution of this patent. Obviously, these solutions should also be included in the scope of protection of this patent.
Claims
1. A method for preparing a dental polymer-based temporary filling material, characterized in that: The following steps are involved: Step 1: Turn on the mold temperature controller and set the temperature to 50°C. Turn on the mold temperature controller circulation pump. After the temperature of the mold temperature controller stabilizes to 50°C, add 70%-80% of methacrylate monomer into the kneader. Step 2, after the solvent temperature reaches 50°C, add 2%-5% acrylate and 0.5%-0.8% fluoride; Step 3, turn on the kneader and adjust the speed to 30-70r / min, stir until uniform, add 0.1%-0.2% of photoinitiator, add 0.5%-0.8% of flavor, add 0.1%-0.2% of inhibitor, and stir evenly; Step 4, after the mixture is uniform, add 20%-30% of filler in 3-4 batches; Step 5, after stirring evenly, perform vacuum treatment, and after the vacuum treatment is completed, take out the produced product.
2. The method for preparing a dental polymer-based temporary filling material according to claim 1, characterized in that: The acrylate substance in step 2 includes, but is not limited to, one or more of polyamino acrylate, polyalkyl acrylate, sodium polyacrylate, and potassium polyacrylate.
3. The method for preparing a dental polymer-based temporary filling material according to claim 1, characterized in that: The fluoride in step 2 includes but is not limited to one or more of sodium fluoride, sodium monofluorophosphate, magnesium fluoride, and strontium fluoride.
4. The method for preparing a dental polymer-based temporary filling material according to claim 1, characterized in that: The methacrylate monomers in step 1 include, but are not limited to, one or more of methyl methacrylate, hydroxyethyl methacrylate, glycidyl methacrylate, tetraethylene glycol dimethacrylate, and ethoxylated bisphenol A diester of methacrylate.
5. The method for preparing a dental polymer-based temporary filling material according to claim 1, characterized in that: The flavor of step 3 is menthone.
6. The method for preparing a dental polymer-based temporary filling material according to claim 1, characterized in that: The types of the filler include, but are not limited to, one or more of silicon dioxide, aluminum oxide, zirconium oxide, glass powder, and nano glass fiber.
7. The method for preparing a dental polymer-based temporary filling material according to claim 1, characterized in that: The polymerization inhibitor includes, but is not limited to, one or more of γ-terpinene, 2,6-di-tert-butyl-p-cresol, and p-hydroxyanisole.
8. The method for preparing a dental polymer-based temporary filling material according to claim 1, characterized in that: The vacuum treatment was performed with a vacuum degree of 0.1 MPa, a kneading machine speed of 4 r / min, and a vacuum of 30 min.
9. The method for preparing a dental polymer-based temporary filling material according to claim 1, characterized in that: The photoinitiator includes one or two of camphor, TPO.