Oxygen absorbent and preparation method thereof
Through the preparation method of solid granular oxygen absorbers and the use of specific ingredients and catalyst combinations, the problem of loss caused by too fast oxygen absorption speed is solved, efficient oxygen absorption capacity and safe food or drug storage are achieved, and the generation of dust is avoided.
Patent Information
- Application Number
- CN202411012160.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-26
- Publication Date
- 2024-10-01
AI Technical Summary
Existing oxygen absorbers absorb oxygen too quickly during the compounding process, resulting in loss, reducing the oxygen absorbing capacity of the product, and easily generating dust, affecting the preservation safety of food or medicines.
The preparation method of solid granular oxygen absorbing agent is adopted, including reduced iron powder, vitamin C, sodium VC, ferrous sulfate, etc. as oxygen absorbing components, magnesium chloride, sodium chloride, etc. as catalysts, starch, sugar powder, etc. as fillers, Silica, diatomaceous earth, etc. are used as water-retaining agents, starch slurry, methyl cellulose, etc. are used as binders, and micro-powder silica gel, magnesium stearate, etc. are used as flow aids, and are pressed into a high-hardness solid oxygen absorbing agent through a tablet press. agent and sealed and packaged under nitrogen-filled conditions.
The prepared solid granular oxygen absorbing agent is small in size, dust-free, and has excellent oxygen absorbing capacity, which improves the storage safety of food or medicine and avoids the generation of dust.
Smart Images

Figure BDA0004964701340000011 
Figure BDA0004964701340000031 
Figure BDA0004964701340000032
Abstract
Description
Technical Field
[0001] The invention belongs to the technical field of oxygen absorbers, and in particular relates to a solid granular oxygen absorber and a preparation method thereof. Background Art
[0002] In the past, as oxygen absorbers for removing oxygen from packages, for example, oxygen absorbers with iron powder as the main component, oxygen absorbers with ascorbic acid or its salt as the main component, oxygen absorbers containing olefinic unsaturated compounds such as polybutadiene and transition metal catalysts such as cobalt, oxygen absorbers containing m-xylylenediphthalimide compounds or m-xylylenediphthalimide compounds and transition metal catalysts such as cobalt, and oxygen absorbers containing hexamethylenebisbenzamide compounds or m-xylylenediphthalimide compounds and transition metal catalysts such as cobalt.
[0003] The original oxygen absorber mainly used iron powder as the oxygen-absorbing basic material, and added a reactive group made of salts, the water content of which did not exceed 35%. The actual oxygen absorption level of the product made with this reactive group and iron powder as the oxygen-absorbing component was about 100-125 ml / g. The oxygen absorption rate was too fast, resulting in loss during the compounding process, reducing the oxygen absorption capacity of the product during use. Summary of the invention
[0004] The object of the present invention is to provide an oxygen absorbent and a preparation method thereof to solve the problems raised in the above background technology.
[0005] To achieve the above object, the present invention provides the following technical solution: an oxygen absorbent comprising, by mass percentage,
[0006]
[0007] Preferably, the oxygen absorber is in solid granular form.
[0008] Preferably, in any of the above schemes, the oxygen absorbing component includes one or more combinations of reduced iron powder, vitamin C, sodium VC, ferrous sulfate, polyether, and oxygen-absorbing hydrocarbons.
[0009] In any of the above schemes, it is preferred that the catalyst comprises a combination of one or more of magnesium chloride, sodium chloride and calcium chloride.
[0010] Preferably, in any of the above schemes, the filler comprises a combination of one or more of starch, powdered sugar, dextrin, lactose, compressible starch, microcrystalline cellulose, and calcium sulfate dihydrate.
[0011] In any of the above schemes, it is preferred that the water retaining agent comprises a combination of one or more of silicon dioxide, diatomaceous earth, artificial zeolite and water-absorbing resin.
[0012] In any of the above schemes, it is preferred that the adhesive comprises a combination of one or more of starch slurry, methyl cellulose, sodium carboxymethyl cellulose and hydroxypropyl cellulose.
[0013] Preferably, in any of the above schemes, the glidant comprises a combination of one or more of micro-powdered silica gel, magnesium stearate and talc.
[0014] A method for preparing an oxygen absorbent comprises the following steps:
[0015] S1: Prepare a solid granular oxygen absorber in proportion and mix the mixture evenly; at room temperature, first, fully stir the oxygen absorbing component and the catalyst for 3 minutes at a stirring rate of 36r / min, then add the filler, water retaining agent and adhesive and stir evenly for 5 minutes at a stirring rate of 45r / min, finally add the flow aid and stir at a rate of 45r / min for 3 minutes, then sieve and seal and package, and the whole process is carried out under nitrogen filling conditions;
[0016] S2: Use tablet press to press into solid oxygen absorbent with higher hardness: the turntable rotates clockwise driven by the power transmission device, and the granular raw materials fall from the feeding hopper into the middle mold framed by the feeding shoe by their own weight. After being scraped flat by the feeding shoe, the upper and lower punches are squeezed by the upper and lower pressure wheels to press the granular raw materials into sheets, and then the sheets are discharged through the sheet discharge device. The turntable undergoes filling, main pressing and sheet discharge once every rotation. Tablet press parameters: maximum working pressure 40KN, maximum tablet diameter 12mm, tablet output 10,000 tablets / hour, maximum filling depth 15mm, speed: 32 rpm.
[0017] S3: Put it into a solid plastic can and seal it inside;
[0018] S4: Put the product into a sealed container where oxygen is required for storage.
[0019] The technical effects and advantages of the present invention: The solid granular oxygen absorber prepared by the present invention is small in size, dust-free, and has excellent oxygen absorption capacity. It can be effectively used in the field of oxygen absorption and storage of food or medicines to prevent dust, thereby improving the safety of use. DETAILED DESCRIPTION
[0020] The following will be described clearly and completely in conjunction with the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0021] Example 1
[0022] A solid granular oxygen absorber, comprising by mass percentage
[0023]
[0024] The oxygen absorbing component is reduced iron powder.
[0025] The catalyst is magnesium chloride.
[0026] The filler is starch.
[0027] The water retaining agent is silicon dioxide.
[0028] The adhesive is starch paste.
[0029] The flow aid is micro powder silica gel.
[0030] Example 2
[0031] A solid granular oxygen absorber, comprising by mass percentage
[0032]
[0033]
[0034] The oxygen-absorbing ingredient is sodium VC.
[0035] The catalyst is sodium chloride.
[0036] The filler is powdered sugar.
[0037] Water-retaining agent: diatomaceous earth.
[0038] The binder is sodium carboxymethyl cellulose.
[0039] The glidant is magnesium stearate.
[0040] Example 3
[0041] An oxygen absorbent comprising, by mass percentage,
[0042]
[0043] The oxygen absorbing ingredient is a mixture of vitamin C and ferrous sulfate.
[0044] The catalyst is a mixture of sodium chloride and calcium chloride.
[0045] The filler is a mixture of dextrin and lactose.
[0046] The water retaining agent is a mixture of diatomaceous earth and artificial zeolite.
[0047] The binder is a mixture of methyl cellulose and sodium carboxymethyl cellulose.
[0048] The glidant is a mixture of magnesium stearate and talc.
[0049] Example 4
[0050] A method for preparing an oxygen absorbent comprises the following steps:
[0051] S1: Prepare a solid granular oxygen absorber in proportion and mix the mixture evenly; at room temperature, first, fully stir the oxygen absorbing component and the catalyst for 3 minutes at a stirring rate of 36r / min, then add the filler, water retaining agent and adhesive and stir evenly for 5 minutes at a stirring rate of 45r / min, finally add the flow aid and stir at a rate of 45r / min for 3 minutes, then sieve and seal and package, and the whole process is carried out under nitrogen filling conditions;
[0052] S2: Use tablet press to press into solid oxygen absorbent with higher hardness: the turntable rotates clockwise driven by the power transmission device, and the granular raw materials fall from the feeding hopper into the middle mold framed by the feeding shoe by their own weight. After being scraped flat by the feeding shoe, the upper and lower punches are squeezed by the upper and lower pressure wheels to press the granular raw materials into sheets, and then the sheets are discharged through the sheet discharge device. The turntable undergoes filling, main pressing and sheet discharge once every rotation. Tablet press parameters: maximum working pressure 40KN, maximum tablet diameter 12mm, tablet output 10,000 tablets / hour, maximum filling depth 15mm, speed: 32 rpm.
[0053] S3: Put it into a solid plastic can and seal it inside;
[0054] S4: Put the product into a sealed container where oxygen is required for storage.
[0055] Finally, it should be noted that the above is only a preferred embodiment of the present invention and is not intended to limit the present invention. Although the present invention has been described in detail with reference to the aforementioned embodiments, it is still possible for those skilled in the art to modify the technical solutions described in the aforementioned embodiments or to make equivalent substitutions for some of the technical features therein. Any modifications, equivalent substitutions, improvements, etc. made within the spirit and principles of the present invention should be included in the protection scope of the present invention.
Claims
1. An oxygen absorbent, characterized in that: In terms of mass percentage, 2. An oxygen absorbent according to claim 1, characterized in that: The oxygen absorbent is in solid granular form.
3. An oxygen absorbent according to claim 1, characterized in that: The oxygen absorbing component comprises one or more combinations of reduced iron powder, vitamin C, VC sodium, ferrous sulfate, p-aminophenol, sodium dithionite, ferrous oxide and ferrous carbonate.
4. An oxygen absorbent according to claim 1, characterized in that: The catalyst includes a combination of one or more of magnesium chloride, sodium chloride and calcium chloride.
5. An oxygen absorbent according to claim 1, characterized in that: The filler comprises one or more combinations of starch, powdered sugar, dextrin, lactose, compressible starch, microcrystalline cellulose, and calcium sulfate dihydrate.
6. An oxygen absorbent according to claim 1, characterized in that: The water retaining agent comprises one or more combinations of silicon dioxide, diatomaceous earth, artificial zeolite and water absorbing resin.
7. An oxygen absorbent according to claim 1, characterized in that: The adhesive comprises a combination of one or more of starch slurry, methyl cellulose, sodium carboxymethyl cellulose and hydroxypropyl cellulose.
8. An oxygen absorbent according to claim 1, characterized in that: The glidant includes one or more combinations of micro powder silica gel, magnesium stearate and talc.
9. A method for preparing an oxygen absorbent according to claim 2, characterized in that: The following steps are involved: S1: Prepare a solid granular oxygen absorber in proportion and mix the mixture evenly; at room temperature, first, fully stir the oxygen absorbing component and the catalyst for 3 minutes at a stirring rate of 36r / min, then add the filler, water retaining agent and adhesive and stir evenly for 5 minutes at a stirring rate of 45r / min, finally add the flow aid and stir at a rate of 45r / min for 3 minutes, then sieve and seal and package, and the whole process is carried out under nitrogen filling conditions; S2: Use tablet press to press into solid oxygen absorbent with high hardness: the turntable rotates clockwise under the drive of the power transmission device, and the granular raw materials fall from the feeding hopper to the middle mold framed by the feeding shoe by their own weight. After being scraped flat by the feeding shoe, the upper and lower punches are squeezed by the upper and lower pressure wheels to press the granular raw materials into sheets, and then the sheets are discharged through the sheet discharge device. Each rotation of the turntable goes through filling, main pressing, and sheet discharge. Tablet press parameters: maximum working pressure 40KN, maximum tablet diameter 12mm, tablet output 10,000 tablets / hour, maximum filling depth 15mm, speed: 32 rpm; S3: Put it into a solid plastic can and seal it inside; S4: Put the product into a sealed container where oxygen is required for storage.