Anti-adhesion lining assembly, manufacturing method thereof and reaction kettle
By arranging a carbon fiber anti-adhesion layer in the reactor and a tight combination of the sleeve, the problem of adhesion between the silver lining and the reactor body under high temperature and pressure is solved, extending the service life of the reactor and promoting mass production.
Patent Information
- Application Number
- CN202410764488.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-06-13
- Publication Date
- 2024-10-01
AI Technical Summary
Under high temperature and high pressure conditions, the silver lining easily adheres to the reactor body, making it difficult to remove and causing damage to the reactor body, which limits the multiple uses of the reactor and the mass production of crystals.
An anti-adhesive layer is installed in the reactor body, including a wrapped carbon fiber material and a sleeve. The anti-adhesive layer is tightly combined with the lining body to resist expansion pressure and avoid serious adhesion with the kettle body. Heating and cooling processes are used to make it It's squeezed together.
It effectively avoids the adhesion between the lining and the kettle body, extends the service life of the reactor, facilitates the removal of the lining and the integrity of the kettle body, and promotes the mass production of gallium nitride crystals.
Smart Images

Figure CN118718933A_ABST
Abstract
Description
Technical Field
[0001] The present application relates to the technical field of structural design and processing and manufacturing of a reactor and its lining, and in particular to an anti-adhesion lining component and a manufacturing method thereof, and a reactor. Background Art
[0002] In applications such as the preparation of gallium nitride single crystals by the ammonothermal method, the maximum reaction temperature can reach 650°C or higher, and the maximum reaction pressure can reach 200MPa. Under these temperature and pressure conditions, it is usually necessary to use a nickel-based alloy material that can withstand high temperature and pressure to manufacture the reactor, and a precious metal lining (also called an inner cylinder) needs to be set inside the nickel-based alloy to resist corrosion from the ammonia fluid solution.
[0003] For example, the silver lining has both anti-corrosion effect and low cost. However, since the deformation of the silver lining under high temperature and high pressure is much greater than that of the nickel-based material of the kettle body, the silver lining is prone to adhesion to the kettle body after being subjected to high temperature and high pressure, causing the silver lining to still adhere to the kettle body after returning to normal temperature and pressure. This adhesion is very tight and the silver lining cannot be removed by normal means. The inventor found that it is inconvenient to remove the silver lining even with the use of lubricants.
[0004] After repeated use of the equipment, the silver lining will inevitably produce cracks and other defects. In order to ensure the sealing effect of the reactor under high temperature and high pressure, the silver lining must be replaced. Due to the above reasons, the silver lining can only be removed by destructive methods, which will inevitably cause damage to the reactor body and is not conducive to large-scale multi-batch production of crystals.
[0005] Therefore, there is still room for improvement in the reactor. Summary of the invention
[0006] In order to solve or alleviate at least one of the problems mentioned in the background technology, the present application provides an anti-adhesion lining component and a manufacturing method thereof, and a reactor.
[0007] The anti-sticking lining assembly provided in the embodiment of the present application is used to be arranged in the kettle body of the reactor. The lining assembly includes a lining body and an anti-sticking layer arranged on the outside of the lining body. The material of the lining body is different from that of the anti-sticking layer.
[0008] In at least one embodiment, the anti-sticking layer includes a first material wrapped around the outer side of the lining body.
[0009] In at least one embodiment, the first material is carbon fiber.
[0010] In at least one embodiment, the anti-sticking layer includes a single-layer sleeve or a multi-layer sleeve.
[0011] In at least one embodiment, the anti-sticking layer includes a first material wrapped around the outside of the lining body and a sleeve disposed on the outside of the first material.
[0012] In at least one embodiment, the thickness A of the anti-sticking layer satisfies 3mm≤A≤50mm, the straightness of the anti-sticking layer is less than or equal to 0.02mm, and the material of the sleeve is the same as that of the kettle body.
[0013] The manufacturing method of the anti-adhesion liner assembly provided in the embodiment of the present application is used to manufacture the anti-adhesion liner assembly as described above, wherein the anti-adhesion layer is a single-layer sleeve or a multi-layer sleeve, and the manufacturing method comprises:
[0014] heating the anti-sticking layer and / or cooling the lining body;
[0015] Assembling the lining body in the anti-sticking layer;
[0016] The room temperature is restored to allow the liner body and the anti-sticking layer to shrink together.
[0017] The manufacturing method of the anti-adhesion liner assembly provided in the embodiment of the present application is used to manufacture the anti-adhesion liner assembly as described above, and the manufacturing method comprises:
[0018] A first material is provided, and the first material is wrapped around the outer side of the lining body which is at room temperature or has been cooled.
[0019] In at least one embodiment, the manufacturing method comprises:
[0020] Heating sleeve;
[0021] placing the first material and the lining body in the sleeve;
[0022] The room temperature is restored to allow the liner body and the anti-sticking layer to shrink together.
[0023] The reactor provided in the embodiment of the present application comprises:
[0024] The anti-adhesion lining assembly as described above;
[0025] A kettle body, wherein the liner assembly is arranged in the kettle body.
[0026] It can be understood that the adhesion between the liner body and the kettle body in the prior art has become an obstacle to the repeated use of the kettle body. The present application sets an anti-adhesion layer between the liner body and the kettle body, which are prone to adhesion. The anti-adhesion layer can resist the expansion pressure of the liner body when it is heated and deformed, so that the liner body is at most adhered to the anti-adhesion layer, and the anti-adhesion layer does not adhere to the kettle body or the adhesion between the anti-adhesion layer and the kettle body is not serious, so that the liner body and the anti-adhesion layer can be easily removed, thereby ensuring the integrity of the kettle body, extending the service life of the reactor, and facilitating large-scale and multi-batch production of gallium nitride crystals, for example. BRIEF DESCRIPTION OF THE DRAWINGS
[0027] Figure 1 A schematic exploded view of an anti-sticking liner assembly according to an embodiment of the present application is shown.
[0028] Figure 2 A cross-sectional view of an anti-sticking liner assembly according to an embodiment of the present application is shown.
[0029] Figure 3 A schematic structural diagram of a reactor, an anti-sticking layer and an inner lining body according to an embodiment of the present application is shown.
[0030] Figure 4 A cross-sectional view of a reactor according to an embodiment of the present application is shown.
[0031] Description of Reference Numerals
[0032] 100 kettle body; 200 liner body; 300 anti-sticking layer; 310 first material; 320 sleeve; 400 sealing ring; 500 bottom gasket; 600 gland; 700 locking nut. DETAILED DESCRIPTION
[0033] The exemplary embodiments of the present application are described below with reference to the accompanying drawings. It should be understood that these specific descriptions are only used to teach those skilled in the art how to implement the present application, and are not intended to exhaust all possible methods of the present application, nor to limit the scope of the present application.
[0034] See also Figure 3 The present application provides an anti-adhesion liner assembly (hereinafter, sometimes simply referred to as a "liner assembly"), which is used to be arranged in a kettle body 100 of a reaction kettle.
[0035] See also Figures 1 to 4 The lining assembly may include a lining body 200 (also called an "inner cylinder") and an anti-sticking layer 300 disposed on the outside of the lining body 200, and the material of the lining body 200 is different from the material of the anti-sticking layer 300.
[0036] It can be understood that the adhesion phenomenon between the liner and the kettle body in the prior art has become an obstacle to the repeated use of the kettle body. The present application sets an anti-sticking layer 300 between the liner body 200 and the kettle body 100, which are prone to adhesion. The anti-sticking layer 300 can resist the expansion pressure of the liner body 200 when it is deformed by heat, so that the liner body 200 is at most adhered to the anti-sticking layer 300, and the anti-sticking layer 300 is not adhered to the kettle body 100 or the anti-sticking layer 300 is not seriously adhered to the kettle body 100, so that the liner body 200 and the anti-sticking layer 300 can be easily removed, ensuring the integrity of the kettle body 100, extending the service life of the reactor, and facilitating, for example, large-scale and multi-batch production of gallium nitride crystals. It can be understood that the reactor provided by the present application can be used for crystal manufacturing, for example, it can be used to produce nitride crystals or other crystals.
[0037] Exemplarily, the material of the lining body 200 may be silver.
[0038] In one embodiment of the present application, see Figure 1 The anti-adhesive layer 300 includes a first material 310 wrapped around the outer side of the lining body 200. The wrapping method can provide a compressive prestress for the lining body 200 to resist the expansion deformation of the lining body 200.
[0039] In one embodiment of the present application, the first material 310 may be a relatively soft material with relatively high tensile strength, such as carbon fiber.
[0040] In one embodiment of the present application, see Figure 1 The anti-sticking layer 300 may include a single-layer sleeve 320 or a multi-layer sleeve 320. It is understood that when a multi-layer sleeve 320 is provided, the deformation degree between the sleeves 320 may have a gradient difference, so that the outermost sleeve 320 may not be deformed as much as possible without damaging the kettle body 100, so as to facilitate the removal of the liner assembly from the kettle body 100.
[0041] In one embodiment of the present application, the material of the sleeve 320 and the material of the kettle body 100 can be the same, for example, both can be nickel-based alloys to prevent adhesion between the sleeve 320 and the kettle body 100. The sleeve 320 can be a nickel-based alloy seamless steel pipe.
[0042] In one embodiment of the present application, see Figure 1 and Figure 2 The anti-sticking layer 300 includes a first material 310 wrapped around the outside of the lining body 200 and a sleeve 320 arranged on the outside of the first material 310 .
[0043] The inventors have optimized the parameters of the anti-adhesive layer 300 through computer simulation and physical measurement in order to achieve the best use effect and economic benefit. Figure 3According to the inner diameter of the lining body 200 of different diameters, the thickness A (wall thickness) of the anti-sticking layer 300 can meet 3mm≤A≤50mm, and the straightness of the anti-sticking layer 300 can be less than or equal to 0.02mm. When the anti-sticking layer 300 only has the sleeve 320, the matching relationship between the anti-sticking layer 300 and the lining body 200 can be an interference fit, for example, the matching relationship between the anti-sticking layer 300 and the lining body 200 can be H7 / p6, H7 / r6, etc. The interference fit method can provide compressive prestress for the lining body 200 and reduce the deformation of the anti-sticking layer 300.
[0044] The present application provides a method for manufacturing an anti-adhesion liner assembly, which is used to manufacture the aforementioned anti-adhesion liner assembly.
[0045] In an example where the anti-sticking layer 300 is only a single-layer sleeve 320 or a multi-layer sleeve 320, the manufacturing method may include:
[0046] (S110) heating the anti-sticking layer 300 and / or cooling the lining body 200;
[0047] (S120) Assembling the lining body 200 in the anti-sticking layer 300;
[0048] (S130) Restoring the room temperature so that the lining body 200 and the anti-sticking layer 300 are compacted together.
[0049] Furthermore, when the anti-sticking layer 300 is in the form of a multi-layer sleeve 320, the multi-layer sleeve 320 can be assembled together by thermal expansion and contraction.
[0050] The sleeve 320 can be precisely machined and the sleeve fitting process can be carefully controlled to ensure the theoretical sleeve fitting stress. The implementation method has the following advantages: the geometric shape of the anti-sticking layer 300 is ensured to be relatively accurate; the designed interference is ensured; the anti-sticking layer 300 is closely fitted to the liner body 200, which is conducive to improving heat transfer and reducing the temperature of the liner body 200; the stress distribution of the liner body 200 is relatively uniform, ensuring the strength of the liner body 200; and the manufacturing errors and defects of the liner body 200 are effectively eliminated.
[0051] In an example where the anti-sticking layer 300 includes the first material 310 , the manufacturing method may include:
[0052] ( S210 ) Provide a first material 310 , and wrap the first material 310 around the outer side of the lining body 200 at room temperature or after cooling.
[0053] Furthermore, the manufacturing method may also include:
[0054] (S220) heating the outer sleeve 320;
[0055] (S230) placing the first material 310 and the lining body 200 in the outer sleeve 320;
[0056] ( S240 ) The outer sleeve 320 is cooled to shrink the liner body 200 and the anti-sticking layer 300 together.
[0057] The winding method has the following advantages: ensuring that the geometric shape of the anti-adhesive layer 300 is relatively accurate; the anti-adhesive layer 300 is closely attached to the lining body 200; making the stress distribution of the lining body 200 relatively uniform, and ensuring the strength of the lining body 200. When the first material 310 is carbon fiber, the strength is relatively high, and it can be applied to the scene where the diameter of the lining body 200 is relatively large.
[0058] Of course, the steps of the aforementioned manufacturing method are merely examples, and their content and sequence may be adjusted according to common sense.
[0059] See also Figure 3 The reactor provided in the present application may include the aforementioned anti-adhesion lining component and a reactor body 100, wherein the lining component is disposed in the reactor body 100. Figure 3 In the figure, for the purpose of clear expression, the liner assembly loaded into the kettle body 100 is shown, and the liner body 200 and the anti-sticking layer 300 are shown separated outside the kettle body 100.
[0060] Further, see Figure 3 , a sealing ring 400 can be arranged on the top of the liner assembly, for example, the sealing ring 400 can be welded to the top of the liner body 200 by welding. The material of the sealing ring 400 can be a nickel-based alloy that is the same as the material of the kettle body. In addition to the sealing function, the sealing ring 400 can also play a positioning role. The top of the anti-sticking layer 300 can be against the bottom of the sealing ring 400 to determine the axial position of the anti-sticking layer 300.
[0061] Exemplarily, the method for manufacturing the reactor may include:
[0062] The pure silver ingot is vacuum-melted into a pure silver tube and processed into a liner body 200, and the nickel-based alloy forging is processed into an annular part to form a sealing ring 400, and the two parts are cleaned;
[0063] The liner body 200 and the sealing ring 400 are positioned by a welding fixture and welded together;
[0064] The anti-sticking layer 300 and the liner body 200 are assembled together to form a liner assembly, and then the liner assembly is installed in the kettle body 100. Exemplarily, the liner assembly and the kettle body 100 may be interference-fitted.
[0065] The reactor may further include a bottom pad 500, a gland 600 and a locking nut 700. The bottom pad 500 may be disposed in the reactor body 100, at the lower portion of the liner assembly. The gland 600 is disposed at the upper portion of the liner assembly, and the locking nut 700 may lock and fix the gland 600 to the reactor body 100.
[0066] The above is a preferred embodiment of the present application. It should be pointed out that for those skilled in the art, several improvements and modifications can be made without departing from the principles of the present application. These improvements and modifications should also be regarded as the scope of protection of the present application.
Claims
1. An anti-adhesion lining assembly, characterized in that: Used to be arranged in a kettle body (100) of a reaction kettle, the lining component comprises a lining body (200) and an anti-sticking layer (300) arranged on the outside of the lining body (200), and the material of the lining body (200) is different from the material of the anti-sticking layer (300).
2. The anti-adhesion lining assembly according to claim 1, characterized in that: The anti-sticking layer (300) comprises a first material (310) wrapped around the outside of the lining body (200).
3. The anti-adhesion lining assembly according to claim 2, characterized in that: The first material (310) is carbon fiber.
4. The anti-adhesion lining assembly according to claim 1, characterized in that: The anti-sticking layer (300) includes a single-layer sleeve (320) or a multi-layer sleeve (320).
5. The anti-adhesion lining assembly according to claim 1, characterized in that: The anti-sticking layer (300) comprises a first material (310) wrapped around the outside of the lining body (200) and a sleeve (320) arranged on the outside of the first material (310).
6. The anti-adhesion lining assembly according to claim 4, characterized in that: The thickness A of the anti-sticking layer (300) satisfies 3mm≤A≤50mm, the straightness of the anti-sticking layer (300) is less than or equal to 0.02mm, and the material of the sleeve (320) is the same as that of the kettle body (100).
7. A method for manufacturing an anti-adhesion lining component, characterized in that: Used for manufacturing the anti-adhesion lining assembly according to any one of claims 1 to 6, the anti-adhesion layer (300) is a single-layer sleeve (320) or a multi-layer sleeve (320), and the manufacturing method comprises: heating the anti-sticking layer (300) and / or cooling the lining body (200); Assembling the lining body (200) in the anti-sticking layer (300); The room temperature is restored to allow the lining body (200) and the anti-sticking layer (300) to shrink together.
8. A method for manufacturing an anti-adhesion lining component, characterized in that: For manufacturing the anti-adhesion lining component according to any one of claims 1 to 6, the manufacturing method comprises: A first material (310) is provided, and the first material (310) is wrapped around the outer side of the lining body (200) which is at room temperature or has been cooled.
9. The method for manufacturing a liner assembly according to claim 8, characterized in that: The manufacturing method comprises: A heating sleeve (320); placing the first material (310) and the lining body (200) in the sleeve (320); The room temperature is restored to allow the lining body (200) and the anti-sticking layer (300) to shrink together.
10. A reaction kettle, characterized in that: include: The anti-adhesion lining assembly according to any one of claims 1 to 6; A kettle body (100), wherein the liner assembly is arranged in the kettle body (100).