Screw extruder and resin composition manufacturing method
By designing multiple reaction sections and homogenization zones in the screw extruder, and using spiral edges, sleeves and kneading elements to extend the residence time of the resin, the problems of short reaction time and insufficient reaction in the existing technology are solved. The manufacture of highly efficient modified resin compositions was achieved.
Patent Information
- Application Number
- CN202410373730.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Priority Date
- 2023-03-30
- Filing Date
- 2024-03-29
- Publication Date
- 2024-10-01
AI Technical Summary
When the existing screw extruder is used to manufacture resin compositions, the reaction time is short and the reactant needs to be injected excessively, resulting in a waste of resources and difficulty in processing.
A screw extruder is designed, which includes a preheating area, a mixing area and multiple sealed reaction sections. Helical elements, sleeve elements and kneading elements are used to increase the residence time of the resin through the sleeve elements and promote the reaction. , and stir in the homogenization area to improve reaction efficiency.
It achieves efficient modification of raw resin without using excessive reactants, increases the manufacturing volume of the resin composition, and improves the adequacy of the reaction and product quality.
Smart Images

Figure CN118721670A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to a screw extruder and a method for producing a resin composition. Background Art
[0002] It is known that a method for manufacturing a resin composition containing a resin having different properties from the raw resin by continuously modifying the raw resin using a screw extruder. The screw of the screw extruder is composed of, for example, screw flight elements for moving the material, kneading elements for kneading, sealing rings for blocking the material, etc., mounted on the shaft. In the screw extruder, a reactant is mixed with the molten raw resin, and kneading is performed in a region having a kneading element, thereby reacting the raw resin and the reactant (for example, see Patent Document 1).
[0003] Prior art literature
[0004] Patent Literature
[0005] Patent Document 1: Japanese Patent Application Publication No. 2021-62552 Summary of the invention
[0006] Problem that the invention aims to solve
[0007] In order to increase the manufacturing volume, it is necessary to increase the flow velocity of the resin inside the screw extruder, so that the passing time in the area of mixing is shortened, so that the reaction is likely to become insufficient. In the case of manufacturing a resin combination to the raw resin mixed reactant, if the injection amount of the reactant is increased, the reaction time can be shortened. However, sometimes it is necessary to separate the reactant injected in excess, and the reactant separated is processed by methods such as burning, so it is desirable that the raw resin is modified without using excessive reactants. Therefore, the subject of the present invention is to provide a screw extruder and a method for manufacturing a resin combination that can efficiently modify the raw resin.
[0008] Solutions for solving problems
[0009] A technical solution of the present invention provides a screw extruder that modifies a raw material resin, wherein the screw extruder comprises: a preheating area in which the raw material resin is melted; a mixing area in which a reactant is mixed with the raw material resin; and a reaction area in which the raw material resin and the reactant are reacted, wherein the reaction area is divided into a plurality of reaction sections by a sealing ring.
[0010] In the above screw extruder, the reaction section may include screw flight elements, sleeve elements and kneading elements.
[0011] In the above screw extruder, the reaction zone may include the screw flight element, the sleeve element, and the kneading element in this order from the mixing region side.
[0012] In the above screw extruder, the sleeve element may be provided only in the reaction section.
[0013] The screw extruder may further include at least one of a homogenizing region for stirring and homogenizing the resin and a feeding region for feeding the resin, on the downstream side of the reaction region.
[0014] The screw extruder may further include, on the downstream side of the reaction zone, a homogenizing zone for stirring the resin to make it homogenous and a delivery zone for delivering the resin in this order.
[0015] Another aspect of the present invention provides a method for producing a resin composition, wherein a reactant is mixed with a raw resin by using the screw extruder to allow the mixture to react.
[0016] In the above method for producing a resin composition, the raw material resin may be an acrylic resin, and the reactant may be an imidizing agent.
[0017] Effects of the Invention
[0018] According to the screw extruder and the method for producing a resin composition of the present invention, a raw material resin can be efficiently modified. BRIEF DESCRIPTION OF THE DRAWINGS
[0019] Figure 1 It is a schematic diagram which shows the structure of the screw extruder which concerns on one Embodiment of this invention.
[0020] Description of Reference Numerals
[0021] 1. Screw extruder; 10. Cylinder; 11. Main feed port; 12. Side feed port; 13. Spout port; 20. Screw; 21. Shaft; 22. Screw wing element; 23. Kneading element; 24. Sleeve element; 25. Sealing ring; 31. Metering feeder; 32. Supply pipeline; B. Reaction section; Z1. Preheating area; Z2. Mixing area; Z3. Reaction area; Z4. Homogenizing area; Z5. Delivery area. DETAILED DESCRIPTION
[0022] Hereinafter, embodiments of the present invention will be described with reference to the accompanying drawings. In addition, for the sake of convenience, the sizes of various components in the accompanying drawings are adjusted so that they are easy to see. Figure 1 It is a schematic diagram which shows the structure of the screw extruder 1 which concerns on one Embodiment of this invention.
[0023] The screw extruder 1 is used to modify the raw material resin. The screw extruder 1 may be a multi-screw extruder, and typically, it is assumed to be a twin-screw extruder. The screw extruder 1 includes a barrel 10 and a screw 20 inserted into the barrel.
[0024] The barrel 10 has a main feed port 11 to which pellets of raw material resin are supplied, a side feed port 12 to which a reactant for modifying the raw material resin is supplied, and a discharge port 13 to discharge a resin composition obtained after the raw material resin is modified. A metering feeder 31 for supplying pellets of raw material resin is connected to the main feed port 11. A supply line 32 for supplying a liquid or gaseous reactant is connected to the side feed port 12. A pipe or the like for delivering the resin composition obtained after modification to the next process can be connected to the discharge port 13. In addition, a well-known component such as a porous plate can also be configured at the discharge port 13.
[0025] The screw 20 has a shaft 21, a screw element 22 mounted on the shaft 21, a kneading element 23, a sleeve element 24, and a seal ring 25. The screw element 22 moves the resin to the downstream side. The kneading element 23 kneads the resin. The sleeve element 24 allows the resin to pass without applying force to the resin as much as possible. The seal ring 25 blocks the resin and applies resistance to passing.
[0026] The screw extruder 1 divides the flow path of the resin by using a barrel 10 and a screw 20. The flow path of the screw extruder 1 is provided as a plurality of flow path sections through which the resin passes in sequence: a preheating zone Z1 in which the raw material resin is melted; a mixing zone Z2 in which the reactant is mixed (dispersed and dissolved) with the raw material resin; a reaction zone Z3 in which the raw material resin and the reactant are reacted; a homogenization zone Z4; and a delivery zone Z5.
[0027] The preheating zone Z1 can be configured to include a main feed port 11 and a plurality of screw flight elements 22. In the preheating zone Z1, the raw material resin pellets are heated and melted by the conveying pressure of the screw flight elements 22 and the radiation heat of the cylinder of the extruder.
[0028] The mixing zone Z2 can be configured to have a side feed port 12 and include a plurality of kneading elements 23. The mixing zone Z2 is preferably configured to include a screw element 22 in the center. By providing the screw element 22 between the kneading elements 23, the temperature of the resin composition can be prevented from rising excessively.
[0029] The reaction zone Z3 is divided into a plurality of, preferably more than three, reaction sections B by the sealing ring 25. That is, each reaction section B is a section sandwiched between two sealing rings 25. The reaction section B preferably includes at least one kneading element 23 and includes a screw element 22 and a sleeve element 24, respectively. More specifically, the reaction section B preferably includes more than one screw element 22, more than one sleeve element 24, and more than one kneading element 23 in the order of the screw element 22, the sleeve element 24, and the kneading element 23. In addition, in the reaction section B, similarly to the mixing zone Z2, when a plurality of kneading elements 23 are provided, it is preferred that the sleeve element 24 be provided between the kneading elements 23. That is, the reaction section B may also include a screw element 22 and repeated sleeve elements 24 and kneading elements 23.
[0030] The sleeve element 24 does not have a projection acting on the resin composition, so a flow path with a relatively large volume is formed. Therefore, by arranging the sleeve element 24 in the reaction zone Z3, the residence time of the resin can be increased, so the reaction of the resin composition can be promoted. In addition, by arranging the sleeve element 24 between the kneading elements 23, the temperature of the resin composition can be prevented from excessively rising. In other words, by arranging the sleeve element 24 in the reaction zone Z3, the number of the kneading elements 23 can be increased and the modification reaction can be more effectively promoted, and the discoloration of the resin composition can be suppressed.
[0031] The homogenization zone Z4 includes kneading elements 23, and stirs the resin composition obtained after the reaction to make it homogenized. In order to maintain the pressure and improve the stirring efficiency, the homogenization zone Z4 is also preferably sandwiched by seal rings 25.
[0032] The delivery area Z5 has a screw element 22, which delivers the resin composition to the next process. The number of screw elements 22 in the delivery area Z5 is selected according to the pressure required for supplying to the next process. As the next process, further modification such as esterification, mixing of additives such as lubricants, ultraviolet absorbers, antioxidants, etc., mixing with other resins, etc. can be considered.
[0033] In the screw 20, the sleeve element 24 is provided in the reaction zone B in order to ensure the reaction time. On the other hand, even if the sleeve element 24 is provided in the preheating zone Z1, the mixing zone Z2, the homogenizing zone Z4 and the delivery zone Z5, no advantageous effect can be obtained, and the length of the shaft 21 is only occupied unnecessarily. Therefore, the sleeve element 24 is preferably provided only in the reaction zone B.
[0034] The screw extruder 1 having the above structure has a reaction area Z3, which has multiple reaction sections B with increased residence time due to the sleeve element 24, thereby effectively promoting the modification reaction and efficiently modifying the raw material resin, thereby increasing the production volume without supplying excessive reactants.
[0035] As can be seen from the above description, one embodiment of the method for producing a resin composition of the present invention utilizes the screw extruder 1 to mix a reactant with a raw resin to react it. More specifically, the method for producing a resin composition of one embodiment of the present invention comprises a step of melting the raw resin (melting step), a step of mixing a reactant with the raw resin (mixing step), and a step of promoting a modification reaction of the raw resin (reaction promotion step).
[0036] (Melting process)
[0037] In the melting process, the pelletized raw material resin is melted in the preheating zone Z1 of the screw extruder 1. The raw material resin is supplied to the main feed port 11 of the screw extruder 1 by the metering feeder 31. The raw material resin is not particularly limited, and for example, maleimide resin, acrylic resin, etc. can be used. As the acrylic resin used as the raw material, for example, a homopolymer of methyl (meth)acrylate, a (meth)acrylate-aromatic vinyl copolymer, etc. are preferably used.
[0038] (Mixing process)
[0039] In the mixing step, the reactant is supplied to the side feed port 12 of the screw extruder 1 through the supply line 32, and the reactant is mixed with the melted raw material resin by stirring with the kneading element 23 in the mixing zone Z2 of the screw extruder 1. As the reactant, for example, an imidizing agent, alcohol, etc. can be used.
[0040] As a reactant, an imidizing agent that imparts positive birefringence to an acrylic resin is typically used. As an imidizing agent, for example, amines containing aliphatic hydrocarbon groups such as ammonia, monomethylamine, ethylamine, n-propylamine, isopropylamine, n-butylamine, isobutylamine, tert-butylamine, and n-hexylamine; amines containing aromatic hydrocarbon groups such as aniline, benzylamine, toluidine, and trichloroaniline; amines containing alicyclic hydrocarbon groups such as cyclohexylamine. In addition, urea compounds that produce the amines exemplified previously by heating, such as urea, 1,3-dimethylurea, 1,3-diethylurea, and 1,3-dipropylurea, can also be used. Among these imidizing agents, monomethylamine, ammonia, and cyclohexylamine are preferably used from the perspective of cost and physical properties, and monomethylamine is particularly preferably used. In addition, monomethylamine, which is gaseous at room temperature, can be used in a state dissolved in alcohols such as methanol. In addition, in the mixing process, in addition to the reactant, a catalyst such as a ring closure promoter can also be added as needed.
[0041] (Reaction promotion step)
[0042] In the reaction promotion step, the following operations are repeated in the reaction zone Z3 of the screw extruder 1: ensuring the reaction time by holding by the sleeve element 24 and promoting the modification reaction by kneading by the kneading element 23 .
[0043] The resin temperature in the reaction zone Z3 of the screw extruder 1 can be appropriately set according to the type and molecular weight of the resin used. When the glass transition temperature (Tg) of the resin is set, it is preferably Tg+50°C or more, and more preferably Tg+60°C or more. On the other hand, as the upper limit of the resin temperature in the reaction zone Z3, it is preferably Tg+160°C or less, and more preferably Tg+150°C or less. By setting it to this range, the reaction of the resin can be effectively promoted. As the lower limit of the resin temperature, for example, it is preferably 180°C, and more preferably 200°C. On the other hand, as the upper limit of the resin temperature in the reaction zone Z3, it is preferably 280°C, and more preferably 260°C. By making the resin temperature in the reaction zone Z3 above the lower limit, when using acrylic resin as the resin, the imidization reaction can be effectively promoted. In addition, by making the resin temperature in the reaction zone Z3 below the upper limit, the decomposition of the resin can be suppressed and the strength of the resin composition finally obtained can be prevented from being damaged.
[0044] As the lower limit of the residence time of the resin in reaction zone Z3, it is preferably 10 seconds, more preferably 30 seconds. On the other hand, as the upper limit of the residence time of the resin in reaction zone Z3, it is preferably 180 seconds, more preferably 60 seconds. By making the residence time of the resin in reaction zone Z3 above the lower limit, the reactant can be fully reacted with the raw resin. In addition, by making the residence time of the resin in reaction zone Z3 below the upper limit, the flow rate of the resin can be increased and the manufacturing amount of the resin combination can be increased.
[0045] As the lower limit of the resin pressure (relative pressure) in the reaction zone Z3, it is preferably 0.5MPa, and more preferably 1.0MPa. On the other hand, as the upper limit of the resin pressure in the reaction zone Z3, it is preferably 50MPa, and more preferably 10MPa. By making the resin pressure in the reaction zone Z3 above the lower limit, the dissolution of the reactant can be promoted and the reaction rate can be increased. In addition, by making the resin pressure in the reaction zone Z3 below the upper limit, it is possible to prevent the unnecessary increase of equipment cost for the pressure resistance of the screw extruder 1.
[0046] In the resin production method of the present embodiment using the screw extruder 1 capable of efficiently modifying the raw material resin, the production volume can be increased without supplying an excessive amount of reactants, and thus a high-quality resin composition can be efficiently produced.
[0047] Although the embodiments of the present invention have been described above, the present invention is not limited to the above embodiments, and various changes and modifications are possible. As an example, in the screw extruder of the present invention, the homogenization region and the delivery region are not essential.
Claims
1. A screw extruder that modifies raw resin. in, The screw extruder has: a preheating zone in which the raw material resin is melted; a mixing region in which reactants are mixed with the raw resin; and a reaction zone in which the raw material resin and the reactant are reacted, The reaction area is divided into a plurality of reaction sections by sealing rings.
2. The screw extruder according to claim 1, in, The reaction sections each have a screw element, a sleeve element and a kneading element.
3. The screw extruder according to claim 2, in, The reaction section comprises the screw flight element, the sleeve element and the kneading element in order from the mixing zone side.
4. The screw extruder according to claim 2 or 3, in, The sleeve element is only arranged in the reaction section.
5. The screw extruder according to any one of claims 1 to 4, in, The screw extruder further includes, on the downstream side of the reaction zone, at least one of a homogenizing zone for stirring the resin to make it homogenous and a feeding zone for feeding the resin.
6. The screw extruder according to any one of claims 1 to 4, in, The screw extruder further includes a homogenizing zone for stirring and homogenizing the resin and a delivery zone for delivering the resin in this order, on the downstream side of the reaction zone.
7. A method for producing a resin composition, in, A reactant is mixed with a raw material resin and reacted by using the screw extruder according to any one of claims 1 to 6.
8. The method for producing a resin composition according to claim 7, in, The raw material resin is an acrylic resin, and the reactant is an imidizing agent.