Protective coating for supporting strip of laser cutting machine

By using a combined coating protective layer on the support bar of the laser cutting machine, the problems of slag adhesion and thermal deformation are solved, the life of the support bar is extended and the cost is reduced.

CN118725622APending Publication Date: 2024-10-01葛富堂
View PDF 2 Cites -1 Cited by

Patent Information

Application Number
CN202410738806.4
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-06-07
Publication Date
2024-10-01
Patent Text Reader

Abstract

The protective coating for the supporting strip of the laser cutting machine comprises a slag protective coating and a thermal deformation protective coating, the slag protective coating is prepared from quick-hardening sulphoaluminate cement, magnesium hydroxide, antimony trioxide, aluminum hydroxide, water, sodium stearate, polyethylene glycol, slag powder, titanate modified sodium bentonite, decabromodiphenyl ethane, steel slag powder, a water reducing agent, expanded perlite powder, alum, a flocculating agent, anhydrite, an expanding agent, hydroxypropyl methyl, polyvinyl alcohol and filler; the thermal deformation protective coating comprises water, a binder and 55 parts of sodium bicarbonate; according to the protective coating for the supporting strip of the laser cutting machine provided by the invention, a tight protective layer is formed on the surface of the supporting strip in a manner of combining the thermal deformation protective coating and the slag protective coating, so that slag generated during working of the laser cutting machine is effectively prevented from being adhered to the supporting strip below; and meanwhile, the problem of precision reduction caused by thermal deformation of the supporting strip is avoided.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the field of laser cutting, and in particular relates to a protective coating for a support strip of a laser cutting machine. Background Art

[0002] Laser cutting machine is a kind of equipment that uses high energy density laser beam to melt, gasify or ablate the material by irradiating the laser beam to the surface of the material, so as to achieve the purpose of cutting. Laser cutting is widely used in the processing of metal and non-metal materials, including but not limited to metal processing, automobile manufacturing, aerospace, electronics, medical, architectural decoration and other industries. The machine tool is one of the core components of the laser cutting machine. It provides the necessary mechanical structure and support for the laser cutting process. The support bar is an important component of the machine tool. Its main function is to support the material and ensure the stability and processing accuracy of the material during the laser cutting process. During the use of the laser cutting machine, due to the high temperature, a large amount of metal slag of thousands of degrees will be generated after cutting the workpiece, which will fall onto the support bar. After cooling, the slag will be firmly combined with the support bar and difficult to handle. With the accumulation of slag, the support bar will eventually become unusable and have to be replaced with a new one, which greatly increases the manpower and material costs of laser cutting. In addition, during the operation of the laser cutting machine, the high temperature generated by the laser will also cause the support bar of the cutting machine to produce thermal deformation, thereby affecting the accuracy of the cutting machine. Therefore, how to avoid the adverse effects of slag and high temperature on the support bar is a difficult problem that needs to be solved urgently in the field of laser cutting. Summary of the invention

[0003] In order to solve the above problems, the present invention provides a technical solution: a protective coating for a support bar of a laser cutting machine, characterized in that the protective coating includes a slag protective coating and a thermal deformation protective coating; the slag protective coating includes the following components by mass: 58 parts of fast-hardening sulphoaluminate cement, 17 parts of magnesium hydroxide, 4 parts of antimony trioxide, 7.5 parts of aluminum hydroxide, 12 parts of water, 9 parts of sodium stearate, 3 parts of polyethylene glycol, 20 parts of slag powder, 20 parts of titanate-modified sodium-based bentonite, 7.5 parts of decabromodiphenyl ethane, 10 parts of steel slag powder, 2 parts of water reducer, 27.5 parts of expanded perlite powder, 15 parts of alum, 15 parts of flocculant, 3.5 parts of anhydrous gypsum, 0.55 parts of expander, 1 part of hydroxypropyl methyl, 5 parts of polyvinyl alcohol, and 5 parts of filler; the coating configuration process includes the following steps: S1: Weigh each component according to the formula ratio, add magnesium hydroxide, sodium stearate and polyethylene glycol in turn and stir to mix evenly, then modify at 80°C for one hour to obtain a flame retardant mixture A; S2: Weigh each component according to the formula ratio, mix aluminum hydroxide, antimony trioxide, titanate-modified sodium bentonite, and decabromodiphenylethane, add water until the mixture becomes a paste, stir and mix evenly, and obtain a flame retardant mixture B; S3: After the flame retardant mixture A and the flame retardant mixture B are mixed and stirred evenly, each component is weighed according to the formula ratio, and slag powder, steel slag powder, water reducer, expanded perlite powder, alum, flocculant, anhydrous gypsum, water, fast-hardening sulphoaluminate cement and expansion agent are added, and the high temperature resistant fast-setting fireproof material is obtained after stirring evenly; S4: weigh each component according to the formula ratio, mix the high temperature resistant quick-curing fireproof material with hydroxypropyl methyl, polyvinyl alcohol and filler, dilute with water at a mass ratio of 1:1-1.5, stir evenly, and obtain a slag protective coating; The thermal deformation protective coating comprises the following components by mass: 30 parts of water, 15 parts of binder, and 55 parts of sodium bicarbonate. The preparation and use methods are as follows: weigh each component according to the formula ratio, stir and mix the water, binder and sodium bicarbonate into a mud-like state; when using, first evenly apply the thermal deformation protective coating, and spray the slag protective coating after drying and solidification.

[0004] The thermal deformation protection coating and the slag protection coating can be dried and solidified by standing for 4-12 hours.

[0005] Preferably, the filler is heavy calcium.

[0006] Preferably, the binder can be selected from one of polyvinyl alcohol, polyvinyl acetate and polyvinyl acetate.

[0007] Compared with the prior art, the present invention has the following benefit effects: the protective coating for the support bar of a laser cutting machine provided by the present invention forms a tight protective layer on the surface of the support bar by combining a thermal deformation protective coating with a slag protective coating, thereby effectively preventing the slag generated when the laser cutting machine is working from adhering to the support bar below, and at the same time avoiding the problem of decreased accuracy caused by thermal deformation of the support bar. The preparation process is simple and easy to use, which extends the service life of the support bar and greatly reduces the labor and material costs required for laser cutting. DETAILED DESCRIPTION

[0008] In order to make the purpose, technical solution and advantages of the present invention clearer, the technical solution of the present invention will be clearly and completely described below in conjunction with the specific embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without making creative work are within the scope of protection of the present invention.

[0009] The present invention provides the following technical solution: a protective coating for a support bar of a laser cutting machine, characterized in that the protective coating comprises a slag protective coating and a thermal deformation protective coating; the slag protective coating comprises the following components by mass: 58 parts of fast-hardening sulphoaluminate cement, 17 parts of magnesium hydroxide, 4 parts of antimony trioxide, 7.5 parts of aluminum hydroxide, 12 parts of water, 9 parts of sodium stearate, 3 parts of polyethylene glycol, 20 parts of slag powder, 20 parts of titanate-modified sodium-based bentonite, 7.5 parts of decabromodiphenylethane, 10 parts of steel slag powder, 2 parts of water reducer, 27.5 parts of expanded perlite powder, 15 parts of alum, 15 parts of flocculant, 3.5 parts of anhydrous gypsum, 0.55 parts of expander, 1 part of hydroxypropyl methyl, 5 parts of polyvinyl alcohol, and 5 parts of filler; the coating configuration process comprises the following steps: S1: Weigh each component according to the formula ratio, add magnesium hydroxide, sodium stearate and polyethylene glycol in turn and stir to mix evenly, then modify at 80°C for one hour to obtain a flame retardant mixture A; S2: Weigh each component according to the formula ratio, mix aluminum hydroxide, antimony trioxide, titanate-modified sodium bentonite, and decabromodiphenylethane, add water until the mixture becomes a paste, stir and mix evenly, and obtain a flame retardant mixture B; S3: After the flame retardant mixture A and the flame retardant mixture B are mixed and stirred evenly, each component is weighed according to the formula ratio, and slag powder, steel slag powder, water reducer, expanded perlite powder, alum, flocculant, anhydrous gypsum, water, fast-hardening sulphoaluminate cement and expansion agent are added, and the high temperature resistant fast-setting fireproof material is obtained after stirring evenly; S4: weigh each component according to the formula ratio, mix the high temperature resistant quick-curing fireproof material with hydroxypropyl methyl, polyvinyl alcohol and filler, dilute with water at a mass ratio of 1:1-1.5, stir evenly, and obtain a slag protective coating; The thermal deformation protective coating comprises the following components by mass: 30 parts of water, 15 parts of binder, and 55 parts of sodium bicarbonate. The preparation and use methods are as follows: weigh each component according to the formula ratio, stir and mix the water, binder and sodium bicarbonate into a mud-like state; when using, first evenly apply the thermal deformation protective coating, and spray the slag protective coating after drying and solidification. Example

[0010] 17 parts of magnesium hydroxide, 9 parts of sodium stearate, and 3 parts of polyethylene glycol were mixed and stirred uniformly according to the mass components, and modified at 80° C. for one hour to obtain a flame retardant mixture A.

[0011] According to the mass components, 7.5 parts of aluminum hydroxide, 4 parts of antimony trioxide, 20 parts of titanate-modified sodium bentonite, and 7.5 parts of decabromodiphenylethane were mixed, and water was added until a paste was formed. The mixture was stirred and mixed evenly to obtain a flame retardant mixture B.

[0012] Mix flame retardant mixture A and flame retardant mixture B, stir evenly, then add 20 parts of slag powder, 10 parts of steel slag powder, 2 parts of water reducer, 27.5 parts of expanded perlite powder, 15 parts of alum, 15 parts of flocculant, 3.5 parts of anhydrous gypsum, 12 parts of water, 58 parts of fast-hardening sulphoaluminate cement and 0.55 parts of expansion agent according to mass components, stir evenly to obtain a high temperature resistant and fast-curing fireproof material.

[0013] The high temperature resistant quick-curing fireproof material is mixed with 1 part of hydroxypropylmethyl, 5 parts of polyvinyl alcohol and 5 parts of filler, and then 1.5 times the mass portion of water is added and stirred evenly to obtain a slag protective coating.

[0014] 30 parts of water, 15 parts of polyvinyl alcohol, 15 parts of polyvinyl acetate, and 55 parts of sodium bicarbonate were stirred and mixed into a muddy state to obtain a heat deformation protective coating.

[0015] Apply the heat deformation protection coating evenly on the surface of the support bar. After it dries and solidifies, pour the slag protection coating into a high-pressure spray pot and spray it evenly on the surface of the laser cutting machine support bar. After spraying, wait for it to dry and solidify.

Claims

1. A protective coating for a laser cutting machine support strip, characterized in that: The protective coating includes slag protective coating and thermal deformation protective coating; the slag protective coating includes the following components by mass: 58 parts of fast-hardening sulphoaluminate cement, 17 parts of magnesium hydroxide, 4 parts of antimony trioxide, 7.5 parts of aluminum hydroxide, 12 parts of water, 9 parts of sodium stearate, 3 parts of polyethylene glycol, 20 parts of slag powder, 20 parts of titanate-modified sodium-based bentonite, 7.5 parts of decabromodiphenylethane, 10 parts of steel slag powder, 2 parts of water reducer, 27.5 parts of expanded perlite powder, 15 parts of alum, 15 parts of flocculant, 3.5 parts of anhydrous gypsum, 0.55 parts of expansion agent, 1 part of hydroxypropyl methyl, 5 parts of polyvinyl alcohol, and 5 parts of filler; The coating configuration process includes the following steps: S1: Weigh each component according to the formula ratio, add magnesium hydroxide, sodium stearate and polyethylene glycol in turn and stir to mix evenly, then modify at 80°C for one hour to obtain a flame retardant mixture A; S2: Weigh each component according to the formula ratio, mix aluminum hydroxide, antimony trioxide, titanate-modified sodium bentonite, and decabromodiphenylethane, add water until the mixture becomes a paste, stir and mix evenly, and obtain a flame retardant mixture B; S3: After the flame retardant mixture A and the flame retardant mixture B are mixed and stirred evenly, each component is weighed according to the formula ratio, and slag powder, steel slag powder, water reducer, expanded perlite powder, alum, flocculant, anhydrous gypsum, water, fast-hardening sulphoaluminate cement and expansion agent are added, and the high temperature resistant fast-setting fireproof material is obtained after stirring evenly; S4: weigh each component according to the formula ratio, mix the high temperature resistant quick-curing fireproof material with hydroxypropyl methyl, polyvinyl alcohol and filler, dilute with water at a mass ratio of 1:1-1.5, stir evenly, and obtain a slag protective coating; The thermal deformation protective coating comprises the following components by mass: 30 parts of water, 15 parts of binder, and 55 parts of sodium bicarbonate. The preparation and use methods are as follows: weigh each component according to the formula ratio, stir and mix the water, binder and sodium bicarbonate into a mud-like state; when using, first evenly apply the thermal deformation protective coating, and spray the slag protective coating after drying and solidification.

Citation Information

Patent Citations

  • Mining inorganic plugging fireproof grouting material and preparation method thereof

    CN115368102A

  • Inorganic high-temperature-resistant fireproof coating and preparation method

    WO2020244363A1