Method for improving titanizing stability of sponge titanium and spraying device
By increasing the viscosity of water and the spraying device, the problems of uneven coating and safety hazards in the production of titanium sponges are solved, uniform mixing and efficient spraying of titanium powder are achieved, the success rate of titanium infiltration and process efficiency are improved, and the cost of titanium powder is reduced Dosage and safety risks.
Patent Information
- Application Number
- CN202410749583.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-06-12
- Publication Date
- 2024-10-01
AI Technical Summary
In the existing titanium sponge production process, the water-infiltrated titanium and oil-infiltrated titanium methods have problems such as uneven coating, high labor intensity, low efficiency, and safety hazards, resulting in reduced product quality and increased iron impurity content.
Use a thickening agent to increase the viscosity of water, prepare a glue-like solution and mix it with titanium powder, and spray it evenly to the inner wall of the reactor through a spraying device to improve the stability of titanium infiltration and reduce the dosage of titanium powder to avoid the safety risk of oil infiltration into titanium.
It achieves uniform mixing and efficient spraying of titanium powder, improves the success rate of titanium infiltration, reduces the amount of titanium powder, avoids safety hazards, and significantly improves process efficiency and product quality.
Smart Images

Figure CN118726897A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the field of nonferrous metal smelting equipment, and in particular to a method and a spraying device for improving the stability of titanium infiltration in titanium sponge. Background Art
[0002] The production of titanium sponge currently adopts the Klauer process. At high temperature, the reaction between titanium tetrachloride and liquid magnesium is a gas-gas reaction. At room temperature, liquid titanium tetrachloride is instantly vaporized after entering the reactor from the feed port, and the liquid magnesium inside the reactor also evaporates in large quantities into the gaseous space at high temperature. Because the reaction is a highly exothermic reaction, the temperature at the liquid surface exceeds 1000°C, while the temperature of the liquid magnesium below is only 800°C. Due to the temperature difference in the reactor, the liquid magnesium has eddy disturbances and continuously washes the position of the reactor wall. This causes the liquid magnesium to continuously wash on the reactor wall. The greater the temperature difference, the faster the washing speed, and the more obvious the erosion phenomenon. Because the inner wall of the reactor is made of carbon steel, iron continuously penetrates into the liquid magnesium due to the washing effect. The iron value in the liquid magnesium is continuously enriched, resulting in an increase in the iron value of the impurity element of the final product, the titanium sponge product, and product degradation.
[0003] At present, all companies use the titanium infiltration method to paint the inner wall of the reactor by water infiltration or oil infiltration (mixing titanium powder with water and oil), and then place the reactor in a high-temperature resistance furnace to heat it up so that the titanium powder forms a hard shell to isolate the iron in the reactor from entering the reactor.
[0004] The current process has the following two problems: ① After water and titanium powder are mixed, they are quickly separated and it is difficult to mix them evenly. The thickness of the titanium powder applied on the reactor is also uneven. The titanium layer is often too thin to protect or too thick to cause cracking, which often leads to unsuccessful titanium infiltration, affecting product quality. In addition, the labor intensity of manual titanium powder application is too high and the efficiency is too low. Because the titanium powder is not applied evenly, a large amount of titanium powder is used; ② The method of mixing oil with titanium powder, although the oil has a large viscosity and can disperse the titanium powder to a certain extent, has a great safety hazard during high-temperature sintering. Summary of the invention
[0005] In view of this, the present invention aims to propose a method and device for improving the stability of titanium sponge infiltration, so as to solve the problem that water infiltration and oil infiltration in the prior art are prone to infiltration failure and safety risks.
[0006] To achieve the above object, the technical solution of the present invention is achieved as follows:
[0007] A method for improving the titanium infiltration stability of titanium sponge comprises the following steps:
[0008] (1) using a thickener to increase the viscosity of water to prepare a glue-like solution;
[0009] (2) mixing titanium powder with a glue-like solution to prepare a titanium powder mixed solution;
[0010] (3) Using a spraying device, spray the titanium powder mixture in step (2) onto the inner wall of the reactor.
[0011] Furthermore, in step (1), the thickener is water starch, and the weight ratio of water to starch is 6:1 to 15:1.
[0012] Furthermore, the weight ratio of water to starch is 10:1.
[0013] Furthermore, in the step (2), when the titanium powder is mixed with the glue-like solution, the weight ratio of the two is 3:1 to 8:1.
[0014] Furthermore, the titanium powder and the solution are mixed in a weight ratio of 5:1.
[0015] The present invention also provides a spraying device for improving the stability of titanium infiltration in sponge titanium, comprising a storage tank, a material transport pipe, a booster pump, a telescopic rod and a nozzle, wherein the storage tank contains a titanium powder mixture, the material transport pipe comprises a first material transport pipe and a second material transport pipe, the storage tank is connected to the booster pump through the first material transport pipe, the booster pump is connected to the telescopic rod through the second material transport pipe, and a nozzle is provided at the end of the telescopic rod, and the titanium powder mixture in the storage tank is sprayed onto the inner wall of the reactor through the nozzle.
[0016] Furthermore, a stirrer is arranged in the storage tank, and a stirring paddle is arranged at the bottom of the stirrer, and the uniform state of the titanium powder mixed liquid is adjusted by the stirring operation of the stirrer and the stirring paddle.
[0017] Furthermore, the connection portion between the first material transport pipe and the material storage tank is arranged at the bottom of the material storage tank or near the bottom.
[0018] Furthermore, one end of the telescopic rod away from the booster pump is connected to the nozzle, and the telescopic rod is configured as a telescopic structure.
[0019] Furthermore, the nozzle is configured as a multi-hole rotating nozzle.
[0020] Compared with the prior art, the method for improving the stability of titanium sponge infiltration according to the present invention has the following advantages:
[0021] By increasing the viscosity of water, the problem of stratification of titanium powder and water can be solved. Titanium powder will no longer stratify within 10 hours of preparation. During the brushing reactor process, the entire process can be brushed by mixing evenly once, which improves the problem of frequent and multiple stirring in the past, increases the success rate of titanium infiltration, and simultaneously reduces the amount of titanium powder used. It eliminates the safety risks of oil titanium infiltration. This method is safe and environmentally friendly and has no safety hazards after review. The introduction of automatic spraying equipment has greatly improved the previous brushing efficiency and reduced the work intensity. The single titanium infiltration time has been reduced from 2h to 0.5h.
[0022] The present invention also provides a spraying device for use in the above-mentioned method for improving the stability of titanium sponge titanium infiltration. BRIEF DESCRIPTION OF THE DRAWINGS
[0023] Figure 1 This is a schematic diagram of the automatic spraying device described in an embodiment of the present invention.
[0024] Description of reference numerals:
[0025] 1- agitator, 2- stirring paddle, 3- storage tank, 4- material transport pipe, 41 first material transport pipe, 42- second material transport pipe, 5- booster pump, 6- telescopic rod, 7- nozzle DETAILED DESCRIPTION
[0026] In order to make the above-mentioned objects, features and advantages of the present invention more obvious and easy to understand, specific embodiments of the present invention are described in detail below with reference to the accompanying drawings.
[0027] A method for improving the titanium infiltration stability of titanium sponge comprises the following steps:
[0028] (1) using a thickener to increase the viscosity of water to prepare a glue-like solution;
[0029] (2) mixing titanium powder with a glue-like solution to prepare a titanium powder mixed solution;
[0030] (3) The titanium powder mixture in step (2) is sprayed onto the inner wall of the reactor using a spraying device, wherein the coating thickness is 1 mm and the spraying pressure is 0.3-0.5 MPa.
[0031] Specifically, the thickener is water starch, and the weight ratio of water to starch is 6:1 to 15:1, preferably 10:1. After water and starch are mixed in a weight ratio of 10:1 and stirred for 10 minutes, the viscosity of the solution increases and gradually becomes glue-like.
[0032] In step (2), when the titanium powder is mixed with the glue-like solution, the weight ratio of the two is 3:1 to 8:1, and preferably, the weight ratio of the two is 5:1. After the titanium powder and the solution are mixed in a weight ratio of 5:1, they are stirred until it can be seen visually that the titanium powder is evenly dispersed in the solution. Preferably, the stirring time is 1 to 10 minutes, and preferably, the stirring time is 2 minutes. According to the above method, the titanium powder can be evenly distributed for 10 hours without obvious stratification.
[0033] As part of the embodiment of the present invention, a spraying device is also provided. Figure 1 As shown, it includes a storage tank 3, a material transport pipe 4, a booster pump 5, a telescopic rod 6 and a nozzle 7, wherein the storage tank 3 contains a titanium powder mixture, the material transport pipe 4 includes a first material transport pipe 41 and a second material transport pipe 42, the storage tank 3 is connected to the booster pump 5 through the first material transport pipe 41, the booster pump 5 is connected to the telescopic rod 6 through the second material transport pipe 42, and a nozzle 7 is provided at the end of the telescopic rod 6, and the titanium powder mixture in the storage tank 3 is sprayed onto the inner wall of the reactor through the nozzle 7.
[0034] Specifically, a stirrer 1 is disposed in the storage tank 3, and a stirring paddle 2 is disposed at the bottom of the stirrer 1, and the uniform state of the titanium powder mixed liquid is adjusted by the stirring operation of the stirrer 1 and the stirring paddle.
[0035] Furthermore, the connection between the first material transport pipe 41 and the storage tank 3 is arranged at the bottom of the storage tank 3 or near the bottom, so as to facilitate the suction of all the mixed liquid inside the storage pipe 3.
[0036] One end of the telescopic rod 6 away from the booster pump 5 is connected to the nozzle 7. The telescopic rod is configured as a telescopic structure, which is convenient for adjusting the distance between the nozzle 7 and the other end of the telescopic rod 6 as needed, and is suitable for spraying the inner wall of reactors with different inner diameters.
[0037] Furthermore, the nozzle 7 is configured as a multi-hole rotary nozzle, which reduces the position movement of the spraying device, so that a large area of the reactor inner wall can be sprayed at the same position.
[0038] Example 1
[0039] (1) mixing water and starch in a weight ratio of 10:1 and stirring for 10 minutes to obtain a glue-like aqueous starch solution;
[0040] (2) mixing titanium powder and water starch solution in a weight ratio of 5:1, and stirring for about 2 minutes until the titanium powder is evenly dispersed in the solution;
[0041] (3) According to the set spraying parameters, spray the four reactors of different models shown in the table below.
[0042] The titanium infiltration time is recorded (wherein the titanium infiltration time is the time for spraying titanium powder). After the titanium infiltration is completed, the amount of titanium powder and the iron value in the titanium sponge prepared by the corresponding reactor are measured. The measured results are shown in Table 1. The four reactors II10-35, II10-40, II10-54, and II10-60 are all new reactors with the same size and shape, and are made of Q245R carbon steel.
[0043] Comparative Example
[0044] The titanium infiltration operation was carried out by conventional titanium infiltration method. After the titanium infiltration was completed, the amount of titanium powder and the iron value in the titanium sponge prepared by the corresponding reactor were measured. The measured results are shown in Table 1. The reactor used in the comparative example has the same specifications as the above reactor.
[0045] Table 1 Comparison between conventional titanium infiltration and titanium infiltration in Example 1
[0046]
[0047] From the above comparison, it can be seen that by adopting the titanium infiltration method described in Example 1, the titanium infiltration time is shortened by nearly 90 minutes, the amount of titanium powder used is reduced by an average of 7 kg, and the sponge titanium iron value is also effectively controlled.
[0048] Although the present invention is disclosed as above, the present invention is not limited thereto. Any person skilled in the art can make various changes and modifications without departing from the spirit and scope of the present invention. Therefore, the protection scope of the present invention shall be subject to the scope defined by the claims.
Claims
1. A method for improving the titaniumization stability of titanium sponge, characterized in that: The steps include: (1) using a thickener, starch in water, to increase the viscosity of water and prepare a glue-like solution; (2) mixing titanium powder with a glue-like solution to prepare a titanium powder mixed solution; (3) Using a spraying device, spray the titanium powder mixture in step (2) onto the inner wall of the reactor.
2. The method for improving the titaniumization stability of titanium sponge according to claim 1, characterized in that: In the step (1), the weight ratio of water to starch in the thickener is 6:1 to 15:
1.
3. The method for improving the titaniumization stability of titanium sponge according to claim 2, characterized in that: The weight ratio of water to starch is 10:
1.
4. The method for improving the titaniumization stability of titanium sponge according to claim 1, characterized in that: When the titanium powder and the glue-like solution are mixed in the step (2), the weight ratio of the two is 3:1 to 8:
1.
5. The method for improving the titaniumization stability of titanium sponge according to claim 4, characterized in that: The titanium powder and the solution are mixed in a weight ratio of 5:
1.
6. A spraying device for improving the stability of titanium sponge titanium infiltration, characterized in that: The invention comprises a storage tank (3), a material transport pipe (4), a booster pump (5), a telescopic rod (6) and a nozzle (7), wherein the storage tank (3) contains a titanium powder mixture, the material transport pipe (4) comprises a first material transport pipe (41) and a second material transport pipe (42), the storage tank (3) is connected to the booster pump (5) via the first material transport pipe (41), the booster pump (5) is connected to the telescopic rod (6) via the second material transport pipe (42), and a nozzle (7) is arranged at the end of the telescopic rod (6), and the titanium powder mixture in the storage tank (3) is sprayed onto the inner wall of the reactor via the nozzle (7).
7. The spraying device for improving the titaniumization stability of titanium sponge according to claim 6, characterized in that: A stirrer (1) is arranged in the storage tank (3), and a stirring paddle (2) is arranged at the bottom of the stirrer (1). The uniform state of the titanium powder mixed liquid is adjusted through the stirring operation of the stirrer (1) and the stirring paddle (2).
8. The spraying device for improving the titaniumization stability of titanium sponge according to claim 6, characterized in that: The connection portion between the first material transport pipe (41) and the material storage tank (3) is arranged at the bottom of the material storage tank (3) or at a position close to the bottom.
9. The spraying device for improving the titaniumization stability of titanium sponge according to claim 6, characterized in that: One end of the telescopic rod (6) away from the booster pump (5) is connected to a spray head (7), and the telescopic rod (6) is configured as a telescopic structure.
10. The spraying device for improving the titaniumization stability of titanium sponge according to claim 6, characterized in that: The nozzle (7) is configured as a multi-hole rotary nozzle.
Citation Information
Patent Citations
Titanium infiltrating method used for inner wall of sponge titanium stainless reactor and titanium infiltrating agent
CN111378921A
Paint spraying ware for construction