Marine equipment multi-zone low-temperature stress corrosion test device and test method
By designing a multi-zone low-temperature stress corrosion test device for marine equipment, the problem of inaccuracy of test conditions in a marine multi-zone low-temperature stress corrosion environment has been solved, a true assessment of the low-temperature stress corrosion performance of marine equipment materials has been achieved, and the test has been improved. accuracy and efficiency of results.
Patent Information
- Application Number
- CN202411049045.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-01
- Publication Date
- 2024-10-01
AI Technical Summary
In the multi-zone low-temperature stress corrosion environment of the ocean, it is difficult for the existing technology to accurately simulate the low-temperature corrosion environment and ensure the sealing and anti-corrosion performance of the test device, resulting in inaccuracy and low efficiency of the test results.
A multi-zone low-temperature stress corrosion testing device for marine equipment is designed, including a tensile testing machine, a low-temperature corrosion environment chamber, a refrigeration device and a corrosion solution circulation device. The sealing structure and circulation system enable dynamic monitoring of the specimen in different environments. and adjustments to ensure the authenticity and consistency of test conditions.
It achieves a true assessment of the low-temperature stress corrosion performance of marine equipment materials, improves the accuracy and efficiency of test results, can dynamically adjust test parameters according to different service environments, and enhances the reliability and application breadth of the test device.
Smart Images

Figure CN118730754A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of stress corrosion testing, in particular to a multi-zone low-temperature stress corrosion testing device and a testing method for marine equipment. Background Art
[0002] Marine equipment such as offshore platforms, icebreakers, and scientific research platforms are subjected to large seasonal temperature changes, corrosion environments in different ocean zones, atmospheric zones, tidal zones, and full immersion zones, and stress coupling during service. Long-term high and low temperature stress corrosion will inevitably produce cumulative damage, seriously threatening the structural safety of polar equipment. Conducting low-temperature stress corrosion tests in polar marine environments is an important means to study the stress corrosion cracking mechanism of polar equipment materials / structures and accurately evaluate the stress corrosion life. Among them, accurate simulation of the corrosion environment in different marine zones and real-time coupling of the corrosion environment and stress are one of the key technologies for obtaining stress corrosion test data for equipment materials.
[0003] Different from the tensile test in air environment, the technical difficulties of low-temperature stress corrosion test in marine multi-zone corrosion environment are mainly reflected in the following aspects.
[0004] 1 Accurate simulation of low temperature corrosion environment in different zones of the ocean,
[0005] 2. Precise connection and sealing of specimens, measuring devices and test devices in corrosive environments
[0006] 3. It is difficult to ensure the uniformity of the corrosion environment during the entire test cycle
[0007] 4. Anti-corrosion measures for key components of the test device and reliable sealing of volatile corrosive media.
[0008] Therefore, in the complex environment of combined low-temperature corrosion and stress in multiple zones of the ocean, how to achieve accurate simulation of the low-temperature corrosion environment and improve the reliable connection, sealing and corrosion resistance of the device is an important issue that needs to be solved in the actual application of low-temperature stress corrosion testing in marine environments.
[0009] To this end, we proposed a multi-zone low-temperature stress corrosion test device and test method for marine equipment. Summary of the invention
[0010] In view of the shortcomings in the above-mentioned existing production technologies, the applicant provides a multi-zone low-temperature stress corrosion test device and test method for marine equipment, so as to assess the low-temperature stress corrosion performance of marine equipment material specimens through a real test environment, and freely configure environmental test parameters according to different service environments of marine equipment, dynamically monitor and adjust the temperature, liquid level height and stress level of the corrosion environment in which the specimen is located.
[0011] The technical solution adopted by the present invention is as follows:
[0012] A multi-zone low-temperature stress corrosion test device for marine equipment, comprising:
[0013] Tensile testing machine;
[0014] Low temperature corrosion environment box, set in the tensile testing machine;
[0015] The test piece has a test section in a low-temperature corrosion environment box, and a transition section sealedly connected to the low-temperature corrosion environment box;
[0016] A refrigeration device is connected to the low-temperature corrosion environment box through pipelines;
[0017] A corrosion solution circulation device is connected to the low-temperature corrosion environment box through pipelines;
[0018] Among them, the low-temperature corrosion solution circulation is realized by a refrigeration device and a corrosion solution circulation device, and the low-temperature stress corrosion test is carried out by a tensile testing machine.
[0019] It is further characterized by:
[0020] The low-temperature corrosion environment box includes a box body, a refrigeration cycle module, a corrosion solution circulation module, a corrosion gas balance module, a gas sealing structure, and a liquid sealing structure. The refrigeration cycle module, the corrosion solution circulation module, and the corrosion gas balance module are arranged in the box body, and the test piece and the box body are sealed by the gas sealing structure and the liquid sealing structure.
[0021] The box body is divided into a cooling solution pool and a corrosion solution pool by partition one, and the corrosion solution pool is divided into a buffer pool and a test pool by partition two. The height of partition two is lower than that of partition one. The inner wall of partition one and the outer wall of partition two both have irregularly distributed convex buffer structures, and the inner wall of partition one and the outer wall of partition two both have irregularly distributed convex buffer structures.
[0022] The refrigeration cycle module includes a refrigerant filling pipe, a refrigeration coil and a refrigerant return pipe. The refrigeration coil is arranged in a cooling solution pool. The refrigerant filling pipe passes through a through hole 1 on the outer plate of the box body to enter the interior of the box body, and is connected to the filling end of the refrigeration coil through a bend pipe 1, a straight pipe 1, and a bend pipe 2. The refrigerant return pipe is connected to the refrigeration coil's refrigeration end through a bend pipe 3, a straight pipe 2, a bend pipe 4, and a bend pipe 5. The refrigerant return pipe passes through a through hole 2 on the outer plate of the box body and extends out of the box body. The refrigeration coil's refrigeration end is lower than the filling end of the refrigeration coil.
[0023] The corrosion solution circulation module includes a corrosion solution adding pipe, a corrosion solution cooling coil, a buffer tank adding pipe, a test tank extraction pipe and a corrosion solution reflux pipe. The corrosion solution adding pipe passes through a through hole three on the outer plate of the box body to enter the interior of the box body, and is connected to the liquid inlet end of the corrosion solution cooling coil through a bend pipe six, a straight pipe three, a bend pipe seven and a bend pipe eight. The corrosion solution cooling coil is arranged in the cooling solution pool. The liquid inlet end of the buffer tank adding pipe is connected to the liquid outlet end of the corrosion solution cooling coil through a bend pipe nine, a straight pipe four and a bend pipe ten. The straight pipe four passes through a through hole four on a partition plate one. The buffer tank adding pipe is arranged in the buffer tank. The liquid outlet end of the buffer tank adding pipe extends into the bottom of the buffer tank. The test tank extraction pipe is arranged in the test tank. The test tank extraction pipe is connected to the corrosion solution reflux pipe through a bend pipe eleven. The corrosion solution reflux pipe passes through a through hole five on the partition plate one and a through hole six on the outer plate of the box body and extends out of the box body. The liquid outlet end of the corrosion solution cooling coil is higher than its liquid inlet end.
[0024] The corrosion gas balance module includes a corrosion gas reflux pipe, a corrosion gas cooling coil, and a corrosion gas exhaust pipe. The corrosion gas cooling coil is arranged in a cooling solution pool. The corrosion gas reflux pipe extends out of the corrosion solution pool through a through hole seven on a partition plate one. A section of the corrosion gas reflux pipe located in the corrosion solution pool is an air inlet end, and an end thereof located in the cooling solution pool is an exhaust end. The exhaust end of the corrosion gas reflux pipe is connected to the air inlet end of the corrosion gas cooling coil through a bend pipe twelve, and the exhaust end of the corrosion gas cooling coil is connected to the corrosion gas exhaust pipe through a bend pipe thirteen. The corrosion gas exhaust pipe extends out of the box body through a through hole eight on the outer panel of the box body, and the air inlet end of the corrosion gas cooling coil is higher than its exhaust end.
[0025] The gas sealing structure is arranged between the test piece and the cover plate of the corrosion solution pool. The gas sealing nut of the gas sealing structure is connected to the gas sealing stud by threads. A through hole is opened in the middle of the gas sealing stud. The through hole of the gas sealing stud is aligned with the through hole nine on the cover plate of the corrosion solution pool and welded as a whole. The upper end of the gas sealing nut is provided with a step inside. Rubber sealing gasket one, metal gasket one, rubber sealing gasket two, metal gasket two, rubber sealing gasket three, and metal gasket three are installed between the internal step of the gas sealing nut and the external thread end face of the gas sealing stud. The upper surface of the rubber sealing gasket one is a plane, the lower surface of the rubber sealing gasket one is a plane, the upper surface of the metal gasket one is a plane, the lower surface of the metal gasket one is an inner cone surface, the upper surface of the rubber sealing gasket one is in direct contact with the internal step surface of the gas sealing nut through the plane, and the lower surface of the rubber sealing gasket one is in direct contact with the upper surface of the metal gasket one through the plane contact, the upper surface of rubber sealing gasket 2 is an outer conical surface, the lower surface of rubber sealing gasket 2 is a plane, the lower surface of metal gasket 1 and the upper surface of rubber sealing gasket 2 are in contact with each other through conical surfaces with the same slope, the upper surface of metal gasket 2 is a plane, the lower surface of metal gasket 2 is an inner conical surface, the upper surface of rubber sealing gasket 3 is an outer conical surface, the lower surface of rubber sealing gasket 3 is a plane, the lower surface of rubber sealing gasket 2 and the upper surface of metal gasket 2 are in direct contact with each other through a plane, the lower surface of metal gasket 2 and the upper surface of rubber sealing gasket 3 are in contact with each other through conical surfaces with the same slope, the upper surface of metal gasket 3 is a plane, the lower surface of metal gasket 3 is a plane, the lower surface of rubber sealing gasket 3 and the upper surface of metal gasket 3 are in direct contact with each other through a plane, and the lower surface of metal gasket 3 is in direct contact with the external threaded end face of gas sealing stud through a plane; the test piece passes through the middle of the gas sealing structure.
[0026] The liquid sealing structure is arranged between the test piece and the bottom plate of the box body. The watertight elastic screw of the liquid sealing structure is a hollow structure with a boss 1 at one end. The major diameter of the thread of the screw rod 1 of the watertight elastic screw is smaller than the through hole on the bottom plate of the test pool. The screw rod 1 of the watertight elastic screw passes through the through hole on the bottom plate of the test pool from the inside to the outside. An inner watertight rubber gasket is installed between the boss 1 of the watertight elastic screw and the inner surface of the bottom plate of the test pool. The watertight nut has a boss 2 at one end. The internal thread of the watertight nut is a conical internal thread. The convex part of the watertight nut is a conical internal thread. The two ends of the platform face the bottom plate of the test pool and are screwed together with the watertight elastic screw through threads. An outer watertight rubber gasket is installed between the boss 2 of the watertight nut and the outer surface of the bottom plate of the test pool. The test piece passes through the through hole of the watertight elastic screw of the liquid sealing structure. There is a gap between the inner surface of the through hole of the watertight elastic screw and the outer surface of the test piece. A cylindrical watertight rubber gasket is installed between the inner surface of the through hole of the watertight elastic screw and the outer surface of the test piece. A guide angle is opened at one end of the screw of the watertight elastic screw, and four elastic grooves are opened at the matching section of the screw and the watertight nut.
[0027] The low temperature corrosion environment box also includes a temperature sensor and a liquid level sensor. The temperature sensor is fixed to the temperature sensor support on the inner wall of the second partition plate through a temperature sensor clamp and a fastening screw group 1. The liquid level sensor is fixed to the liquid level sensor support on the bottom plate of the box body of the low temperature corrosion environment box through a liquid level sensor clamp and a fastening screw group 4.
[0028] The low-temperature corrosion environment box also includes a platinum electrode and a reference electrode. The platinum electrode is installed on a platinum electrode spring clamp on the inner wall of the second partition. The platinum electrode spring clamp is fixed to the platinum electrode support through a group of fastening screws group two. The reference electrode is installed on the reference electrode spring clamp. The reference electrode spring clamp is fixed to the reference electrode support on the inner wall of the second partition through a group of fastening screws group three. The temperature sensor, liquid level sensor, platinum electrode and reference electrode are arranged in the test pool.
[0029] The corrosion solution circulation device comprises a corrosion solution adding pump, a corrosion solution adding flowmeter, a corrosion solution reflux pump and a corrosion solution reflux flowmeter, wherein the corrosion solution adding flowmeter is installed between the corrosion solution adding pump and the corrosion solution adding pipe; one end of the corrosion solution adding pump is connected to the corrosion solution storage tank through pipeline one, and the other end thereof is connected to the corrosion solution adding pipe through pipeline two, the corrosion solution adding flowmeter and pipeline three; a corrosion solution reflux flowmeter is installed between the corrosion solution reflux pump and the corrosion solution reflux pipe; one end of the corrosion solution reflux pump is connected to the corrosion solution storage tank through pipeline four, and the other end thereof is connected to the corrosion solution reflux pipe through pipeline five, the corrosion solution reflux flowmeter and pipeline six.
[0030] It also includes a supporting tooling, which is fixed to the column of the tensile testing machine through an elastic clamp, the elastic clamp is hingedly connected to the swing arm through a second screw and a nut, and the tray is welded and fixed to the swing arm; when the second screw and the nut are loosened, the swing arm and the tray can rotate around the second screw, and when the second screw and the nut are tightened, the rotation of the swing arm and the tray is restricted; the supporting tooling is divided into two parts, which are respectively fixed on the two columns of the tensile testing machine, and the two parts of the supporting tooling are rotated toward the middle and closed through the swing arm, and the two trays jointly support the low-temperature corrosion solution box.
[0031] The chassis of the tensile testing machine is installed on the horizontal ground through feet, two columns are fixed on the chassis, a crossbeam is installed on the columns, a limit baffle and a lifting ring are provided at the end of the crossbeam, and the crossbeam can slide under the guidance of the two columns; a loading device is installed on the crossbeam, the loading device includes an electric cylinder base, an electric cylinder body, and an electric cylinder piston rod, the electric cylinder base is installed on the electric cylinder fixing flange of the crossbeam through a bolt group 1, the electric cylinder body and the crossbeam through-hole are matched through a shaft sleeve, an integrated control box is provided on the side of the electric cylinder base, and the integrated control box is fixed to the electric cylinder base through a bolt group 2; a workbench is fixedly installed on the chassis, and a fixed support is installed on the workbench A movable support is installed on the fixed support, and a transfer nut is installed on the movable support; one end of the upper pull rod of the connecting tooling is an external thread, which is fixed to the piston rod of the electric cylinder through a threaded connection; the other end of the upper pull rod is an internal thread, which is fixed to the upper double fork ear through a threaded connection, and the upper double fork ear is connected to the upper single fork ear through a pin shaft 1; one end of the lower pull rod is an external thread, which is fixed to the transfer nut through a threaded connection; the other end of the lower pull rod is an internal thread, which is fixed to the lower double fork ear through a threaded connection, and the lower double fork ear is connected to the lower single fork ear through a pin shaft 2, and the upper single fork ear and the lower single fork ear are fixed to the external threads at both ends of the specimen through internal threads.
[0032] The corrosion solution circulation device is connected to the corrosion solution tank and the control computer through pipelines and lines respectively. The temperature probe of the temperature sensor, the metal platinum sheet of the platinum sheet electrode, and the liquid junction of the reference electrode are all installed at the same height as the test section of the specimen. The temperature monitoring data of the temperature sensor, the liquid level monitoring data of the liquid level sensor, and the flow monitoring data of the corrosion solution addition flowmeter and the corrosion solution reflux flowmeter are all integrated and transmitted to the control computer through signal lines.
[0033] The test piece in the test cell serves as a working electrode, forms a three-electrode test system with a platinum electrode and a reference electrode, and the test piece is isolated from the tensile testing machine and the low-temperature corrosion environment box by insulating materials to ensure that the test piece is in an electrochemical insulation state.
[0034] The present invention also discloses a multi-zone low-temperature stress corrosion test method for marine equipment, comprising the following steps:
[0035] Step 1: Adjust the support fixture to a suitable height, tighten the locking screws and locking nuts, and fix the position of the support fixture;
[0036] Step 2: Install the low-temperature corrosion environment box, place the low-temperature corrosion environment box on the supporting tooling, and connect the pipelines between the low-temperature corrosion environment box and the refrigeration device, the corrosion solution circulation device, and the corrosion solution box;
[0037] Step 3: Install the test piece, retract the electric cylinder piston rod, firmly connect the upper end of the test piece with the upper single fork ear through threads, extend the electric cylinder piston rod, make the test piece pass through the low-temperature corrosion environment box, firmly connect the lower single fork ear with the lower end of the test piece through threads, adjust the extension amount of the electric cylinder piston rod, and connect the lower single fork ear with the lower double fork ear through pin 2;
[0038] Step 4: Add cooling solution into the cooling solution pool and cover the cooling solution pool with a cover plate;
[0039] Step 5: Seal the low temperature corrosion environment box, tighten the watertight nut to make the low temperature corrosion environment box liquid-tight, tighten the gas sealing nut to make the low temperature corrosion environment box gas-tight;
[0040] Step 6: Start the refrigeration device and circulation device through the control computer to start the circulation of low-temperature corrosion solution;
[0041] Step 7: Start the tensile testing machine to perform stress cycle and start the low-temperature stress corrosion test.
[0042] The beneficial effects of the present invention are as follows:
[0043] The present invention has a compact and reasonable structure and is easy to operate. It can assess the low-temperature stress corrosion performance of marine equipment material specimens through a real test environment, and can freely configure environmental test parameters according to different service environments of marine equipment, dynamically monitor and adjust the temperature, liquid level height and stress level of the corrosive environment in which the specimen is located, and has important practical significance for exploring the safety and reliability of marine equipment materials used in different low-temperature corrosive environments. The present invention solves the problems of uneven composition and uneven temperature of the corrosive environment medium during the test process that cannot be solved by existing devices. The entire invention device is easy to install and operate, and is automatically controlled, which can greatly improve the test efficiency and the accuracy of the test results. At the same time, the present invention can also be promoted and applied to the low-temperature stress corrosion performance assessment of non-metallic materials of marine equipment and metal and non-metallic materials in the construction and oil and gas industries.
[0044] At the same time, the present invention also has the following advantages:
[0045] 1. The refrigeration device cools the refrigerant to a low temperature and then adds it to the refrigeration coil through the refrigerant adding pipe. The low-temperature refrigerant exchanges heat with the cooling solution in the cooling solution pool through the refrigeration coil, takes away the heat and flows back to the refrigeration device through the refrigerant return pipe. The refrigerant circulates in the refrigeration device and the refrigeration cycle module to cool the cooling solution.
[0046] 2. The corrosion solution storage tank has sufficient storage space and stores a sufficient amount of corrosion solution. The corrosion solution circulation device transports the corrosion solution in the corrosion solution tank to the corrosion solution adding pipe. The corrosion solution enters the corrosion solution cooling coil through the corrosion solution adding pipe. The corrosion solution exchanges heat with the cooling solution through the corrosion solution cooling coil. The low-temperature corrosion solution after the temperature is reduced enters the buffer tank of the low-temperature corrosion solution through the corrosion solution buffer tank adding pipe. After the low-temperature corrosion solution enters the buffer tank, the flow speed gradually slows down and the liquid level gradually increases. When the liquid level of the low-temperature corrosion solution is higher than the second partition, the low-temperature corrosion solution overflows from the buffer tank to the test tank; the corrosion solution circulation device extracts the low-temperature corrosion solution in the test tank through the test tank extraction pipe and the corrosion solution reflux pipe and transports it back to the corrosion solution tank to realize the circulation of the corrosion solution.
[0047] 3. The specimen in the test pool of the low-temperature corrosion environment box is used as the working electrode to form a three-electrode test system with the platinum electrode and the reference electrode. The specimen is isolated from the tensile testing machine and the low-temperature corrosion environment box by insulating materials to ensure that the specimen is in an electrochemical insulation state.
[0048] 4. A guide angle is provided at one end of the screw of the watertight elastic screw, and four elastic grooves are provided at the matching section between the screw and the watertight nut. The external thread of the watertight elastic screw in the natural state is a cylindrical external thread, and the basic middle diameter is slightly larger than the average middle diameter of the conical internal thread of the watertight nut. When the watertight elastic screw and the watertight nut are tightened, the screw of the watertight elastic screw produces elastic deformation toward the center, and the external thread of the watertight elastic screw becomes a conical external thread that matches the conical internal thread of the watertight elastic screw. BRIEF DESCRIPTION OF THE DRAWINGS
[0049] Figure 1 It is a structural schematic diagram of the present invention.
[0050] Figure 2 for Figure 1 Cross-sectional view of the low temperature corrosion environment chamber installed in.
[0051] Figure 3 for Figure 2 Cross-sectional view of the medium and low temperature corrosion environment chamber.
[0052] Figure 4 for Figure 2 A three-dimensional diagram of the refrigeration cycle module.
[0053] Figure 5 for Figure 2 A three-dimensional view of the corrosion solution circulation module.
[0054] Figure 6 for Figure 2 A three-dimensional diagram of the corrosion gas balance module.
[0055] Figure 7for Figure 2 Magnified view of the gas seal device.
[0056] Figure 8 for Figure 2 Magnified view of the liquid sealing device.
[0057] Fig. 9 for Figure 8 A magnified stereoscopic view of the watertight elastic screw.
[0058] Fig.10 for Figure 1 Schematic diagram of the structure of the medium circulation device.
[0059] Fig.11 for Figure 1 Magnified view of the support fixture installed in.
[0060] Fig.12 for Figure 1 Schematic diagram of the structure of the tensile testing machine.
[0061] Among them: 1. Tensile testing machine; 2. Loading device; 3. Connecting tooling; 4. Support tooling; 5. Low-temperature corrosion environment box; 6. Refrigeration device; 7. Corrosive solution circulation device; 8. Corrosive solution box; 9. Control computer; A. Box body; B. Refrigeration circulation module; C. Corrosive solution circulation module; D. Corrosive gas balance module; E. Gas sealing structure; F. Liquid sealing structure;
[0062] A01, bottom plate; A02, outer plate; A03, partition one; A04, partition two; A05, cooling solution pool cover; A06, corrosion solution pool cover; A07, through hole one; A08, through hole two; A09, through hole three; A10, through hole four; A11, through hole five; A12, through hole six; A13, through hole seven; A14, through hole eight; A15, raised buffer structure; A16, through hole nine; A17, test pool bottom plate through hole; A18, cooling solution pool; A19, corrosion solution pool; A20, buffer pool; A21, test pool;
[0063] B01, refrigerant liquid adding pipe; B02, elbow pipe 1; B03, straight pipe 1; B04, elbow pipe 2; B05, refrigeration coil; B06, elbow pipe 5; B07, elbow pipe 4; B08, straight pipe 2; B09, elbow pipe 3; B10, refrigerant return pipe;
[0064] C01, corrosive solution adding pipe; C02, elbow pipe six; C03, straight pipe three; C04, elbow pipe seven; C05, elbow pipe eight; C06, corrosive solution cooling coil; C07, elbow pipe ten; C08, straight pipe four; C09, elbow pipe nine; C10, buffer tank adding pipe; C11, buffer elbow pipe one; C12, buffer elbow pipe two; C13, test tank extraction pipe; C14, elbow pipe eleven; C15, corrosive solution reflux pipe;
[0065] D01, corrosive gas reflux pipe; D02, elbow pipe 12; D03, corrosive gas cooling coil; D04, elbow pipe 13; D05, corrosive gas exhaust pipe;
[0066] E01, gas sealing nut; E02, gas sealing stud; E03, rubber sealing gasket 1; E04, metal gasket 1; E05, rubber sealing gasket 2; E06, metal gasket 2; E07, rubber sealing gasket 3; E08, metal gasket 3;
[0067] F01, watertight elastic screw; F02, inner watertight rubber gasket; F03 outer watertight rubber gasket; F04, watertight nut; F05, cylindrical watertight rubber gasket; F011, boss 1; F012, screw 1; F013, chamfer; F014, elastic groove; F015, external thread;
[0068] 101, foot; 102, chassis; 103, workbench; 104, column; 105, beam; 106, limit baffle; 107, lifting ring; 108, fixed support; 109, movable support; 110, adapter nut;
[0069] 201, electric cylinder base; 202, electric cylinder fixing flange; 203, bolt group 1; 204, integrated control box; 205, bolt group 2; 206, shaft sleeve; 207, electric cylinder body; 208, electric cylinder piston rod;
[0070] 301, upper tie rod; 302, upper double fork ear; 303, pin one; 304, upper single fork ear; 305, lower tie rod; 306, lower double fork ear; 307, pin two; 308, lower single fork ear;
[0071] 401, elastic clamp; 402, swing arm; 403, tray; 404, screw rod 2; 405, nut; 406, locking screw; 407, locking nut;
[0072] 501, test piece; 502, temperature sensor; 503, temperature sensor clamp; 504, fastening screw group 1; 505, temperature sensor support; 506, platinum electrode; 507, platinum electrode spring clamp; 508, fastening screw group 2; 509, platinum electrode support; 510, reference electrode; 511, reference electrode spring clamp; 512, fastening screw group 3; 513, reference electrode support; 514, liquid level sensor; 515, liquid level sensor clamp; 516, fastening screw group 4; 517, liquid level sensor support;
[0073] 701. Corrosive solution adding pump; 702. Corrosive solution adding flowmeter; 703. Corrosive solution reflux pump; 704. Corrosive solution reflux flowmeter; 705. Pipeline 1; 706. Pipeline 2; 707. Pipeline 3; 708. Pipeline 4; 709. Pipeline 5; 710. Pipeline 6. DETAILED DESCRIPTION
[0074] The specific implementation of the present invention will be described below in conjunction with the accompanying drawings.
[0075] like Figure 1-Figure 12 As shown, a multi-zone low-temperature stress corrosion test device for marine equipment includes a tensile testing machine 1, a loading device 2, a connecting tool 3, a supporting tool 4, a low-temperature corrosion environment box 5, a refrigeration device 6, a corrosion solution circulation device 7, a corrosion solution box 8, a control computer 9, a box body A, a refrigeration circulation module B, a corrosion solution circulation module C, a corrosion gas balance module D, a gas sealing structure E, and a liquid sealing structure F. The tensile testing machine 1 is provided with a tensile testing machine column 104, on which a supporting tool 4 is provided, and the low-temperature corrosion environment box 5 is placed on the supporting tool 4. The test section of the test piece 501 is completely in the low-temperature corrosion environment box 5, and the transition section of the test piece 501 is sealed and connected to the low-temperature corrosion environment box 5. Both ends of the test piece 501 are connected to the tensile testing machine 1 through the connecting tool 3, and the low-temperature corrosion environment box 5 is respectively connected to the refrigeration device 6 and the corrosion solution circulation device 7 through pipelines, and the corrosion solution circulation device 7 is respectively connected to the corrosion solution box 8 and the control computer 9 through pipelines and lines.
[0076] like Figure 2-Figure 3As shown, the low-temperature corrosion environment box 5 includes a box body A, which is divided into a cooling solution pool A18 and a corrosion solution pool A19 by a partition A03. The cooling solution pool A18 is equipped with a refrigeration coil B05, a corrosion solution coil C06 and a corrosion gas cooling coil D03; the corrosion solution pool A19 is divided into a buffer pool A20 and a test pool A21 by a partition A04. The height of the partition A04 is lower than that of the partition A03. The buffer pool A20 is equipped with a corrosion solution adding pipe C10. The inner wall of the partition A03 and the outer wall of the partition A04 are both provided with irregularly distributed protruding buffer structures A15. The test pool A21 is equipped with a corrosion solution extraction pipe C13, a temperature sensor 502, a platinum electrode 506, a reference electrode 510 and a liquid level sensor 514; the cooling solution pool A18 is sealed with a cooling solution pool cover A05, and the corrosion solution pool A19 is sealed with a corrosion solution pool cover A06.
[0077] The low-temperature corrosion environment box 5 includes a refrigeration cycle module B, which includes a refrigerant liquid adding pipe B01, a refrigeration coil B05 and a refrigerant return pipe B10. The refrigerant liquid adding pipe B01 passes through a through hole A07 on the outer plate A02 of the box body A to enter the interior of the box body A, and is connected to the liquid adding end of the refrigeration coil B05 through a bend pipe B02, a straight pipe B03, and a bend pipe B04. The straight pipe B03 is fixed to the inner wall of the outer plate A02 of the box body A by a clamp and screws. The refrigerant return pipe B10 is connected to the return end of the refrigeration coil B05 through a bend pipe B09, a straight pipe B08, a bend pipe B07, and a bend pipe B06. , straight pipe No. 2 B08 is fixed to the inner wall of the outer plate A02 of the box A by clamps and screws, the refrigeration coil B05 is fixed to the bottom plate A01 of the cooling solution pool A18 by clamps and screws, the refrigerant return pipe B10 passes through the through hole No. 2 A08 on the outer plate A02 of the box A and extends out of the box A, the return end of the refrigeration coil B05 is lower than the liquid adding end of the refrigeration coil B05 in spatial position, the pipe joints of the refrigeration cycle module B are all sealed and connected by pipe threads, and the refrigerant liquid adding pipe B01 and the refrigerant return pipe B10 are sealed and connected to the through hole No. 1 A07 and the through hole No. 2 A08 on the outer plate A02 of the box A by sealing sleeves and glue. After the refrigeration device 6 cools the refrigerant to a low temperature, it is added to the refrigeration coil B05 through the refrigerant adding pipe B01. The low-temperature refrigerant exchanges heat with the cooling solution in the cooling solution pool A18 through the refrigeration coil B05, takes away the heat and then flows back to the refrigeration device 6 through the refrigerant return pipe B10. The refrigerant circulates in the refrigeration device 6 and the refrigeration cycle module B to cool the cooling solution.
[0078] The low temperature corrosion environment box 5 also includes a corrosion solution circulation module C, which includes a corrosion solution adding pipe C01, a corrosion solution cooling coil C06, a buffer tank adding pipe C10, a test tank extraction pipe C13, and a corrosion solution reflux pipe C15. The corrosion solution adding pipe C01 passes through a through hole three A09 on the outer plate A02 of the box body A to enter the interior of the box body A, and passes through a bend pipe six C02, a straight pipe three C03, a bend pipe seven C04, and a bend pipe eight C05 to connect with the The liquid inlet end of the corrosion solution cooling coil C06 is connected, the straight pipe three C03 is fixed to the inner wall of the outer plate A02 of the box body A by a clamp and screws, the elbow eight C05 is fixed to the bottom plate A01 of the cooling solution pool A18 by a clamp and screws, the corrosion solution cooling coil C06 is fixed to the outer wall of the partition A03 by a clamp and screws, the buffer tank liquid adding pipe C10 is fixed to the inner wall of the partition A03 by a clamp and screws, and the liquid inlet end of the buffer tank liquid adding pipe C10 passes through the elbow nine C09 , straight pipe C08, curved pipe C07 are connected to the liquid outlet of the corrosion solution cooling coil C06, straight pipe C08 passes through the through hole A10 on the partition A03, the liquid outlet of the buffer tank adding pipe C10 extends into the bottom of the buffer tank A20, the test tank extraction pipe C13 is fixedly installed on the inner wall of the partition A04 by a clamp and screws, and is connected to the corrosion solution return pipe C15 through the curved pipe C14, and the corrosion solution return pipe C15 passes through the through hole A10 on the partition A03. Hole five A11 and through hole six A12 on the outer plate A02 of box body A extend out of box body A, the liquid outlet end of the corrosion solution cooling coil C06 is higher than the liquid inlet end in spatial position, the pipe joints of the corrosion solution circulation module C are all sealed and connected by pipe threads, and the corrosion solution circulation module C and through hole three A09, through hole six A12 on the outer plate A02 of box body A, through hole four A10 and through hole five A11 on partition one A03 are all sealed and connected by sealing sleeves and glue.
[0079] The corrosion solution storage tank 8 has sufficient storage space and stores a sufficient amount of corrosion solution. The corrosion solution circulation device 7 transports the corrosion solution in the corrosion solution tank 8 to the corrosion solution adding pipe C01. The corrosion solution enters the corrosion solution cooling coil C06 through the corrosion solution adding pipe C01. The corrosion solution exchanges heat with the cooling solution through the corrosion solution cooling coil C06. The low-temperature corrosion solution after the temperature is reduced enters the low-temperature corrosion solution buffer tank A20 through the corrosion solution buffer tank adding pipe C10. After the low-temperature corrosion solution enters the buffer tank A20, the flow speed gradually slows down and the liquid level gradually increases. When the liquid level of the low-temperature corrosion solution is higher than the partition A04, the low-temperature corrosion solution overflows from the buffer tank A20 to the test tank A21; the corrosion solution circulation device 7 extracts the low-temperature corrosion solution in the test tank A21 through the test tank extraction pipe C13 and the corrosion solution reflux pipe C15 and transports it back to the corrosion solution tank 8 to realize the circulation of the corrosion solution.
[0080] The low temperature corrosion environment box 5 also includes a temperature sensor 502 and a liquid level sensor 514. The temperature sensor 502 is fixed to the temperature sensor support 505 on the inner wall of the partition plate A04 through the temperature sensor clamp 503 and the fastening screw group 1 504. The liquid level sensor 514 is fixed to the liquid level sensor support 517 of the bottom plate A01 of the box body A of the low temperature corrosion environment box 5 through the liquid level sensor clamp 515 and the fastening screw group 4 516. The temperature probe of the temperature sensor 502, the metal platinum sheet of the platinum sheet electrode 506, and the liquid junction of the reference electrode 510 in the low temperature corrosion environment box 5 are all installed at the same height as the test section of the test piece 501. The test pool temperature monitoring data of the temperature sensor 502, the test pool liquid level monitoring data of the liquid level sensor 514, and the flow monitoring data of the corrosion solution addition flow meter 703 and the corrosion solution reflux flow meter 704 are all integrated and transmitted to the control computer 9 through the signal line. The corrosion solution circulation device 7 is connected to the control computer 9 through a signal line. The control computer 9 adjusts the addition rate of the corrosion solution addition pump 701 and the reflux rate of the corrosion solution reflux pump 702 in real time according to the temperature and liquid level data of the test pool A21, so that the temperature and liquid level of the corrosion solution in the test pool reach and stabilize at the target value.
[0081] The low temperature corrosion environment box 5 also includes a platinum electrode 506 and a reference electrode 510. The platinum electrode 506 is mounted on a platinum electrode spring clamp 507 on the inner wall of the second partition A04. The platinum electrode spring clamp 507 is fixed to the platinum electrode support 509 through a set of fastening screws 508. The reference electrode 510 is mounted on a reference electrode spring clamp 511. The reference electrode spring clamp 511 is fixed to the reference electrode support 513 on the inner wall of the second partition A04 through a set of fastening screws 512. The test piece 501 in the test pool A21 of the low temperature corrosion environment box 5 is used as a working electrode to form a three-electrode test system with the platinum electrode 506 and the reference electrode 510. The test piece 501 is isolated from the tensile testing machine 1 and the low temperature corrosion environment box 5 by insulating materials to ensure that the test piece 501 is in an electrochemical insulation state.
[0082] The low-temperature corrosion environment box 5 includes a corrosion gas balance module D, which includes a corrosion gas return pipe D01, a corrosion gas cooling coil D03, and a corrosion gas exhaust pipe D05. The corrosion gas return pipe D01 extends through the through hole A13 on the partition A03 to the corrosion solution pool A19. The section of the corrosion gas return pipe D01 located in the corrosion solution pool A19 is the air inlet end, and the end located in the cooling solution pool A18 is the exhaust end. The exhaust end of the corrosion gas return pipe D01 is connected to the air inlet end of the corrosion gas cooling coil D03 through the elbow D02. The corrosion gas cooling coil D03 It is fixed on the outer wall of the partition A03 by clamps and screws, the exhaust end of the corrosion gas cooling coil D03 is connected to the corrosion gas exhaust pipe D05 through the elbow thirteen D04, the corrosion gas exhaust pipe D05 passes through the through hole eight A14 on the outer plate A02 of the box body A and extends out of the box body A, the air inlet end of the corrosion gas cooling coil D03 is higher than the exhaust end in spatial position, the pipe joints of the corrosion gas balance module D are all sealed and connected by pipe threads, and the corrosion gas balance module D and the through hole seven A13 of the partition A03 and the through hole eight A14 on the outer plate A02 of the box body A are all sealed and connected by sealing sleeves and glue.
[0083] like Figure 7As shown, the low-temperature corrosion environment box 5 also includes a gas sealing structure E, which is arranged between the test piece 501 and the corrosion solution pool cover A06, and the gas sealing nut E01 is connected to the gas sealing stud E02 through a thread, and a through hole is opened in the middle of the gas sealing stud E02, and the through hole of the gas sealing stud E02 is aligned with the through hole A16 on the corrosion solution pool cover A06 and welded as a whole, and the inner part of the upper end of the gas sealing nut E01 has a step, and a rubber sealing gasket E03, a metal gasket E04, and a rubber sealing gasket E05 are installed between the inner step of the gas sealing nut E01 and the external thread end face of the gas sealing stud E02. , metal gasket E06, rubber sealing gasket E07, metal gasket E08, the upper surface of rubber sealing gasket E03 is a plane, the lower surface of rubber sealing gasket E03 is a plane, the upper surface of metal gasket E04 is a plane, the lower surface of metal gasket E04 is an inner cone, the upper surface of rubber sealing gasket E03 is in direct contact with the inner step surface of gas sealing nut E01 through a plane, the lower surface of rubber sealing gasket E03 is in direct contact with the upper surface of metal gasket E04 through a plane, the upper surface of rubber sealing gasket E05 is an outer cone, the lower surface of rubber sealing gasket E05 is a plane, metal gasket E0 The lower surface of 4 and the upper surface of the rubber sealing gasket E05 are in contact with each other through a conical surface with the same slope. The upper surface of the metal gasket E06 is a plane, and the lower surface of the metal gasket E06 is an inner cone. The upper surface of the rubber sealing gasket E07 is an outer cone, and the lower surface of the rubber sealing gasket E07 is a plane. The lower surface of the rubber sealing gasket E05 and the upper surface of the metal gasket E06 are in direct contact through a plane. The lower surface of the metal gasket E06 and the upper surface of the rubber sealing gasket E07 are in contact with each other through a conical surface with the same slope. The upper surface of the metal gasket E08 is a plane, and the lower surface of the metal gasket E08 is The specimen 501 is a plane, the lower surface of the rubber sealing gasket E07 is in direct contact with the upper surface of the metal gasket E08 through the plane, and the lower surface of the metal gasket E08 is in direct contact with the external thread end face of the gas sealing stud E02 through the plane; the specimen 501 passes through the middle of the gas sealing structure E, and there is a certain distance between the surface of the specimen 501 and the inner wall of the through hole of the gas sealing nut E01 and the inner wall of the through hole of the gas sealing stud E02, and there is a smaller distance between the surface of the specimen 501 and the inner wall of the through hole of the metal gasket E04, the metal gasket E06, and the metal gasket E08, and it is in direct contact with the inner wall of the through hole of the rubber sealing gasket E03, the rubber sealing gasket E05, and the rubber sealing gasket E07. When the gas sealing nut E01 and the gas sealing stud E02 are tightened through threads, the rubber sealing gasket 1 E03, the rubber sealing gasket 2 E05 and the rubber sealing gasket 3 E07 are deformed toward the center under the extrusion force until they fit the outer surface of the specimen 501, thereby forming a gas sealing structure E between the specimen 501 and the corrosion solution pool cover A06.
[0084] like Figure 8 As shown, the low-temperature corrosion environment box 5 also includes a liquid sealing structure F, which is arranged between the test piece 501 and the bottom plate A01 of the box body A. The watertight elastic screw F01 is a hollow structure with a boss F011 at one end. The major diameter of the thread of the screw rod F012 of the watertight elastic screw F01 is slightly smaller than the through hole A17 on the bottom plate A01 of the test pool A21. The screw rod F012 of the watertight elastic screw F01 passes through the through hole A17 on the bottom plate A01 of the test pool A21 from the inside to the outside. An inner watertight rubber gasket F02 is installed between the boss F011 of the watertight elastic screw F01 and the inner surface of the bottom plate A01 of the test pool A21. The watertight nut F04 has a boss 2 at one end, and the watertight nut The internal thread of F04 is a conical internal thread. The two ends of the boss of the watertight nut F04 face the bottom plate A01 of the test pool A21 and are screwed with the watertight elastic screw F01 through threads. An outer watertight rubber gasket F03 is installed between the boss 2 of the watertight nut F04 and the outer surface of the bottom plate A01 of the test pool A21. The test piece 501 passes through the through hole of the watertight elastic screw F01 of the liquid sealing structure F. There is a certain distance between the inner surface of the through hole of the watertight elastic screw F01 and the outer surface of the test piece 501. A cylindrical watertight rubber gasket F05 is installed between the inner surface of the through hole of the watertight elastic screw F01 and the outer surface of the test piece 501. There is a small distance between the inner surface of the cylindrical watertight rubber gasket F05 and the outer surface of the test piece 501.
[0085] When the watertight nut F04 and the watertight elastic screw F01 are tightened, the inner watertight rubber gasket F02 and the outer watertight rubber gasket F03 are subjected to extrusion pressure, forming a seal between the watertight elastic screw F01 and the bottom plate A01 of the box body A of the low-temperature corrosion environment box 5. At the same time, the watertight elastic screw F01 is elastically deformed toward the center when the watertight nut F04 is tightened, exerting an extrusion pressure on the cylindrical watertight rubber gasket F05, forming a seal between the watertight elastic screw F01 and the outer surface of the test piece 501.
[0086] like Fig. 9 As shown, the watertight elastic screw F01 has the following structure: the end of the screw rod F012 of the watertight elastic screw F01 is provided with a chamfer, and the matching section of the screw rod F012 and the watertight nut F04 is provided with four elastic grooves F014. The external thread of the watertight elastic screw F01 in the natural state is a cylindrical external thread, and the basic middle diameter is slightly larger than the average middle diameter of the conical internal thread of the watertight nut F04. When the watertight elastic screw F01 and the watertight nut F04 are tightened, the screw rod F012 of the watertight elastic screw F01 is elastically deformed toward the center, and the external thread of the watertight elastic screw F01 becomes a conical external thread that matches the conical internal thread of the watertight elastic screw F01.
[0087] like Fig.10As shown, the corrosion solution circulation device 7 includes a corrosion solution adding pump 701, a corrosion solution adding flowmeter 702, a corrosion solution reflux pump 703, and a corrosion solution reflux flowmeter 704. The corrosion solution adding flowmeter 702 is installed between the corrosion solution adding pump 701 and the corrosion solution adding pipe C01. One end of the corrosion solution adding pump 701 is connected to the corrosion solution storage tank 8 through a pipeline 1 705, and the other end is connected to the corrosion solution adding pipe C01 through a pipeline 2 706, the corrosion solution adding flowmeter 702, and a pipeline 3 707; the corrosion solution reflux flowmeter 704 is installed between the corrosion solution reflux pump 703 and the corrosion solution reflux pipe C15. One end of the corrosion solution reflux pump 703 is connected to the corrosion solution storage tank 8 through a pipeline 4 708, and the other end is connected to the corrosion solution reflux pipe C15 through a pipeline 5 709, the corrosion solution reflux flowmeter 704, and a pipeline 6 710.
[0088] like Fig.11 As shown, the support fixture 4 is fixed to the column 104 through an elastic clamp 401, the elastic clamp 401 is hingedly connected to the swing arm 402 through a screw rod 404 and a nut 405, and the tray 403 is welded and fixed to the swing arm 402; when the screw rod 404 and the nut 405 are loosened, the swing arm 402 and the tray 403 can rotate around the screw rod 404, and when the screw rod 404 and the nut 405 are tightened, the rotation of the swing arm 402 and the tray 403 is restricted; the support fixture 4 is divided into two parts, which are fixed to the tensile testing machine 1 On the two columns 104, the two parts of the supporting tooling 4 are rotated and closed toward the middle through the swing arm 402, and the two trays 403 jointly support the low-temperature corrosion solution box 5. By loosening the locking screws 406 and the locking nuts 407, the height of the tray 403 of the supporting tooling 4 and the low-temperature corrosion solution box 5 can be freely adjusted so that the test section of the specimen 501 is in a suitable position in the low-temperature corrosion solution box 5. By tightening the locking screws 406 and the locking nuts 407, the height of the supporting tooling tray 403 and the low-temperature corrosion solution box 5 can be fixed.
[0089] like Fig.12As shown, the chassis 102 of the tensile testing machine 1 is installed on the horizontal ground through the foot 101, two columns 104 are fixed on the chassis 102, and a beam 105 is installed on the column 104. The end of the beam 105 is provided with a limit baffle 106 and a lifting ring 107, and the beam 105 can slide upward or downward under the guidance of the two columns 104; a loading device 2 is installed on the beam 105, and the loading device 2 includes an electric cylinder base 201, an electric cylinder cylinder body 207, an electric cylinder piston rod 208, etc. The electric cylinder base 201 is installed on the electric cylinder fixing flange 202 of the beam 105 through a bolt group 203, and the electric cylinder cylinder body 207 and the through hole of the beam 105 are matched through a shaft sleeve 206. An integrated control box 204 is provided on the side of the electric cylinder base 201, and the integrated control box 204 is fixed to the electric cylinder base 201 through a bolt group 205; a workbench 1 is fixedly installed on the chassis 102 of the tensile testing machine 1 03, a fixed support 108 is installed on the workbench 103, a movable support 109 is installed on the fixed support 108, and a transfer nut 110 is installed on the movable support 109; one end of the upper pull rod 301 connecting the tooling 3 is an external thread, which is fixed to the electric cylinder piston rod 208 through a threaded connection; the other end of the upper pull rod 301 connecting the tooling 3 is an internal thread, which is fixed to the upper double fork ear 302 through a threaded connection, and the upper double fork ear 302 is connected to the upper single fork The ears 304 are connected by a pin 1 303, one end of the lower pull rod 305 is an external thread, and is fixed to the adapter nut 110 by a threaded connection; the other end of the lower pull rod 305 is an internal thread, and is fixed to the lower double fork ear 306 by a threaded connection, the lower double fork ear 306 is connected to the lower single fork ear 308 by a pin 2 307, and the upper single fork ear 304 and the lower single fork ear 308 are fixed to the external threads at both ends of the specimen 501 by the internal threads.
[0090] The low-temperature stress corrosion performance of marine equipment material specimens is assessed through a real test environment, and the environmental test parameters can be freely configured according to the different service environments of the marine equipment, and the temperature, liquid level height and stress level of the corrosive environment in which the specimen 501 is located are dynamically monitored and adjusted, which has important practical significance for the safety and reliability of marine equipment materials used in different low-temperature corrosion environments. The present invention solves the problems of uneven composition and uneven temperature of the corrosive environment medium during the test process that cannot be solved by existing devices. The entire invention device is easy to install and operate, and is automatically controlled, which can greatly improve the test efficiency and the accuracy of the test results. At the same time, the present invention can also be promoted and applied to the low-temperature stress corrosion performance assessment of non-metallic materials of marine equipment and metal and non-metallic materials in the construction and oil and gas industries.
[0091] The present invention also discloses a multi-zone low-temperature stress corrosion test method for marine equipment, comprising the following steps:
[0092] Step 1: Adjust the support fixture 4 to a suitable height, tighten the locking screw 406 and the locking nut 407 to fix the position of the support fixture 4;
[0093] Step 2: Install the low-temperature corrosion environment box 5, place the low-temperature corrosion environment box 5 on the supporting tooling 4, and connect the pipelines between the low-temperature corrosion environment box 5 and the refrigeration device 6, the corrosion solution circulation device 7, and the corrosion solution tank 8;
[0094] Step 3: Install the test piece 501, retract the electric cylinder piston rod 208, firmly connect the upper end of the test piece 501 with the upper single fork ear 304 through threads, extend the electric cylinder piston rod 208, make the test piece pass through the low-temperature corrosion environment box 5, firmly connect the lower single fork ear 308 with the lower end of the test piece 501 through threads, adjust the extension amount of the electric cylinder piston rod 208, and connect the lower single fork ear 308 with the lower double fork ear 306 through the pin 2 307;
[0095] Step 4: Add cooling solution into the cooling solution pool A18 and cover the cooling solution pool cover A05;
[0096] Step 5: Seal the low-temperature corrosion environment box 5, tighten the watertight nut F04, perform liquid sealing on the low-temperature corrosion environment box 5, tighten the gas sealing nut E01, perform gas sealing on the low-temperature corrosion environment box 5;
[0097] Step 6: Start the refrigeration device 6 and the circulation device 7 by controlling the computer 9 to start the circulation of the low-temperature corrosion solution;
[0098] Step 7: Start the tensile testing machine 1 to perform stress cycle and start the low temperature stress corrosion test.
[0099] The above description is an explanation of the present invention, not a limitation of the present invention. The scope of the present invention is defined in the claims. Any form of modification may be made within the scope of protection of the present invention.
Claims
1. A multi-zone low-temperature stress corrosion test device for marine equipment, characterized in that: include: Tensile testing machine (1); A low temperature corrosion environment box (5) is arranged in the tensile testing machine (1); A test piece (501), wherein a test section thereof is in a low temperature corrosion environment box (5), and a transition section thereof is sealedly connected to the low temperature corrosion environment box (5); A refrigeration device (6) is connected to the low-temperature corrosion environment box (5) through a pipeline; A corrosive solution circulation device (7) connected to the low-temperature corrosive environment box (5) via a pipeline; The low-temperature corrosion solution circulation is achieved through the refrigeration device (6) and the corrosion solution circulation device (7), and the low-temperature stress corrosion test is carried out through the tensile testing machine (1).
2. A multi-zone low temperature stress corrosion test device for marine equipment according to claim 1, characterized in that: The low-temperature corrosion environment box (5) comprises a box body (A), a refrigeration circulation module (B), a corrosion solution circulation module (C), a corrosion gas balance module (D), a gas sealing structure (E), and a liquid sealing structure (F); the refrigeration circulation module (B), the corrosion solution circulation module (C), and the corrosion gas balance module (D) are arranged in the box body (A); and the test piece (501) and the box body (A) are sealed by the gas sealing structure (E) and the liquid sealing structure (F).
3. A multi-zone low temperature stress corrosion test device for marine equipment according to claim 2, characterized in that: The box body (A) is divided into a cooling solution pool (A18) and a corrosion solution pool (A19) by a partition plate 1 (A03); the corrosion solution pool (A19) is divided into a buffer pool (A20) and a test pool (A21) by a partition plate 2 (A04); the height of the partition plate 2 (A04) is lower than the height of the partition plate 1 (A03); the inner wall of the partition plate 1 (A03) and the outer wall of the partition plate 2 (A04) both have irregularly distributed protruding buffer structures (A15); the inner wall of the partition plate 1 (A03) and the outer wall of the partition plate 2 (A04) both have irregularly distributed protruding buffer structures (A15).
4. A multi-zone low temperature stress corrosion test device for marine equipment as claimed in claim 3, characterized in that: The refrigeration cycle module (B) comprises a refrigerant liquid adding pipe (B01), a refrigeration coil (B05) and a refrigerant return pipe (B10); the refrigeration coil (B05) is arranged in a cooling solution pool (A18); the refrigerant liquid adding pipe (B01) passes through a through hole 1 (A07) on an outer plate (A02) of the box body (A) to enter the interior of the box body (A), and is connected to the refrigeration coil through a bend pipe 1 (B02), a straight pipe 1 (B03), and a bend pipe 2 (B04). The liquid filling end of the refrigeration coil (B05) is connected, the refrigerant return pipe (B10) is connected to the return end of the refrigeration coil (B05) through the bend pipe three (B09), the straight pipe two (B08), the bend pipe four (B07), and the bend pipe five (B06), the refrigerant return pipe (B10) passes through the through hole two (A08) on the outer plate (A02) of the box body (A) and extends out of the box body (A), and the return end of the refrigeration coil (B05) is lower than the liquid filling end of the refrigeration coil (B05).
5. A multi-zone low temperature stress corrosion test device for marine equipment according to claim 4, characterized in that: The corrosion solution circulation module (C) comprises a corrosion solution adding pipe (C01), a corrosion solution cooling coil (C06), a buffer tank adding pipe (C10), a test tank extraction pipe (C13) and a corrosion solution reflux pipe (C15). The corrosion solution adding pipe (C01) passes through a third through hole (A09) on an outer plate (A02) of the box body (A) to enter the interior of the box body (A), and is connected to a liquid inlet end of the corrosion solution cooling coil (C06) through a sixth bend (C02), a third straight pipe (C03), a seventh bend (C04) and an eighth bend (C05). The corrosion solution cooling coil (C06) is arranged in a cooling solution pool (A18). The liquid inlet end of the buffer tank adding pipe (C10) is connected to a liquid inlet end of the corrosion solution cooling coil (C06) through a ninth bend (C09), a fourth straight pipe (C08) and a tenth bend (C05). 7) is connected to the liquid outlet of the corrosion solution cooling coil (C06), the straight pipe four (C08) passes through the through hole four (A10) on the partition one (A03), the buffer tank liquid adding pipe (C10) is arranged in the buffer tank (A20), the liquid outlet of the buffer tank liquid adding pipe (C10) extends into the bottom of the buffer tank (A20), the test tank liquid extraction pipe (C13) is arranged in the test tank (A21), the test tank liquid extraction pipe (C13) is connected to the corrosion solution return pipe (C15) through the bent pipe eleven (C14), the corrosion solution return pipe (C15) passes through the through hole five (A11) on the partition one (A03) and the through hole six (A12) on the outer plate (A02) of the box body (A) and extends out of the box body (A), and the liquid outlet of the corrosion solution cooling coil (C06) is higher than its liquid inlet.
6. A multi-zone low temperature stress corrosion test device for marine equipment according to claim 5, characterized in that: The corrosion gas balance module (D) comprises a corrosion gas reflux pipe (D01), a corrosion gas cooling coil (D03), and a corrosion gas exhaust pipe (D05). The corrosion gas cooling coil (D03) is arranged in a cooling solution pool (A18). The corrosion gas reflux pipe (D01) passes through a through hole seven (A13) on a partition plate one (A03) and extends out of the corrosion solution pool (A19). A section of the corrosion gas reflux pipe (D01) located in the corrosion solution pool (A19) is an air inlet end. The section of the corrosion gas reflux pipe (D01) located in the cooling solution pool (A18) is an air inlet end. 8) is an exhaust end, the exhaust end of the corrosion gas return pipe (D01) is connected to the air inlet end of the corrosion gas cooling coil (D03) through an elbow 12 (D02), the exhaust end of the corrosion gas cooling coil (D03) is connected to the corrosion gas exhaust pipe (D05) through an elbow 13 (D04), the corrosion gas exhaust pipe (D05) passes through a through hole 8 (A14) on the outer plate (A02) of the box body (A) and extends out of the box body (A), and the air inlet end of the corrosion gas cooling coil (D03) is higher than its exhaust end.
7. A multi-zone low temperature stress corrosion test device for marine equipment according to claim 6, characterized in that: The gas sealing structure (E) is arranged between the test piece (501) and the corrosion solution pool cover plate (A06); the gas sealing nut (E01) of the gas sealing structure (E) is connected to the gas sealing stud (E02) by threads; a through hole is opened in the middle of the gas sealing stud (E02); the through hole of the gas sealing stud (E02) is aligned with the through hole nine (A16) on the corrosion solution pool cover plate (A06) and welded as a whole; the inner part of the upper end of the gas sealing nut (E01) is provided with a step; a rubber sealing gasket is installed between the inner step of the gas sealing nut (E01) and the outer thread end face of the gas sealing stud (E02) One (E03), metal gasket one (E04), rubber sealing gasket two (E05), metal gasket two (E06), rubber sealing gasket three (E07), metal gasket three (E08), the upper surface of rubber sealing gasket one (E03) is a plane, the lower surface of rubber sealing gasket one (E03) is a plane, the upper surface of metal gasket one (E04) is a plane, the lower surface of metal gasket one (E04) is an inner cone surface, the upper surface of rubber sealing gasket one (E03) is in direct contact with the inner step surface of gas sealing nut (E01) through a plane, and the lower surface of rubber sealing gasket one (E03) is in direct contact with the metal gasket The upper surface of the first (E04) is in direct contact with the rubber sealing gasket through a plane, the upper surface of the second (E05) rubber sealing gasket is an outer cone, the lower surface of the second (E05) rubber sealing gasket is a plane, the lower surface of the first (E04) metal gasket and the upper surface of the second (E05) rubber sealing gasket are in contact with each other through cone surfaces with the same slope, the upper surface of the second (E06) metal gasket is a plane, the lower surface of the second (E06) metal gasket is an inner cone, the upper surface of the third (E07) rubber sealing gasket is an outer cone, the lower surface of the third (E07) rubber sealing gasket is a plane, the lower surface of the second (E05) rubber sealing gasket and the metal gasket are in direct ... The upper surface of the second piece (E06) is in direct contact with the surface through a plane, the lower surface of the metal gasket second (E06) and the upper surface of the rubber sealing gasket three (E07) are in contact with each other through conical surfaces with the same slope, the upper surface of the metal gasket three (E08) is a plane, the lower surface of the metal gasket three (E08) is a plane, the lower surface of the rubber sealing gasket three (E07) and the upper surface of the metal gasket three (E08) are in direct contact with the surface through a plane, and the lower surface of the metal gasket three (E08) and the external threaded end face of the gas sealing stud (E02) are in direct contact with the surface through a plane; the test piece (501) passes through the middle of the gas sealing structure (E).
8. A multi-zone low temperature stress corrosion test device for marine equipment according to claim 7, characterized in that: The liquid sealing structure (F) is arranged between the test piece (501) and the bottom plate (A01) of the box body (A); the watertight elastic screw (F01) of the liquid sealing structure (F) is a hollow structure with a boss (F011) at one end; the major diameter of the thread of the screw (F012) of the watertight elastic screw (F01) is smaller than the through hole (A17) on the bottom plate (A01) of the test tank (A21); the watertight elastic screw (F01) is a hollow structure with a boss (F011) at one end; the major diameter of the thread of the screw (F012) of the watertight elastic screw (F01) is smaller than the through hole (A17) on the bottom plate (A01) of the test tank (A21); The screw rod 1 (F012) of the test tank (A21) passes through the through hole (A17) on the bottom plate (A01) of the test tank (A21) and goes out from the inside to the outside. The inner watertight rubber gasket (F02) is installed between the boss 1 (F011) of the watertight elastic screw (F01) and the inner surface of the bottom plate (A01) of the test tank (A21). The watertight nut (F04) has a boss 2 at one end. The internal thread of the watertight nut (F04) is a conical internal thread. The two ends of the boss of the watertight nut (F04) face the bottom plate (A01) of the test pool (A21) and are screwed together with the watertight elastic screw (F01) through threads. An outer watertight rubber gasket (F03) is installed between the boss 2 of the watertight nut (F04) and the outer surface of the bottom plate (A01) of the test pool (A21). The test piece (501) passes through the through hole of the watertight elastic screw (F01) of the liquid sealing structure (F). There is a gap between the inner surface of the through hole of the watertight elastic screw (F01) and the outer surface of the test piece (501). A cylindrical watertight rubber gasket (F05) is installed between the inner surface of the through hole of the watertight elastic screw (F01) and the outer surface of the test piece (501). The end of the screw rod 1 (F012) of the watertight elastic screw (F01) is provided with a chamfer, and the matching section between the screw rod 1 (F012) and the watertight nut (F04) is provided with four elastic grooves (F014).
9. A multi-zone low temperature stress corrosion test device for marine equipment according to claim 8, characterized in that: The low-temperature corrosion environment box (5) further comprises a temperature sensor (502) and a liquid level sensor (514); the temperature sensor (502) is fixed to a temperature sensor support (505) on the inner wall of the second partition (A04) via a temperature sensor clamp (503) and a fastening screw group (504); and the liquid level sensor (514) is fixed to a liquid level sensor support (517) on the bottom plate (A01) of the box body (A) of the low-temperature corrosion environment box (5) via a liquid level sensor clamp (515) and a fastening screw group (516); The low-temperature corrosion environment box (5) also includes a platinum electrode (506) and a reference electrode (510). The platinum electrode (506) is mounted on a platinum electrode spring clamp (507) on the inner wall of the second partition (A04). The platinum electrode spring clamp (507) is fixed to a platinum electrode support (509) by a set of fastening screws (set 2) (508). The reference electrode (510) is mounted on a reference electrode spring clamp (511). The reference electrode spring clamp (511) is fixed to a reference electrode support (513) on the inner wall of the second partition (A04) by a set of fastening screws (set 3) (512). The temperature sensor (502), the liquid level sensor (514), the platinum electrode (506) and the reference electrode (510) are arranged in a test pool (A21).
10. A multi-zone low temperature stress corrosion test device for marine equipment according to claim 9, characterized in that: The corrosive solution circulation device (7) comprises a corrosive solution adding pump (701), a corrosive solution adding flowmeter (702), a corrosive solution reflux pump (703) and a corrosive solution reflux flowmeter (704). The corrosive solution adding flowmeter (702) is installed between the corrosive solution adding pump (701) and the corrosive solution adding pipe (C01). One end of the corrosive solution adding pump (701) is connected to the corrosive solution storage tank (8) via a pipe 1 (705), and the other end of the corrosive solution adding pump (701) is connected to the corrosive solution storage tank (8) via a pipe 2 (706), a corrosive solution reflux pump (703) and a corrosive solution reflux flowmeter (704). The liquid addition flowmeter (702) and pipeline three (707) are connected to the corrosion solution addition pipe (C01); a corrosion solution reflux flowmeter (704) is installed between the corrosion solution reflux pump (703) and the corrosion solution reflux pipe (C15); one end of the corrosion solution reflux pump (703) is connected to the corrosion solution storage tank (8) through pipeline four (708), and the other end is connected to the corrosion solution reflux pipe (C15) through pipeline five (709), the corrosion solution reflux flowmeter (704), and pipeline six (710).
11. A multi-zone low temperature stress corrosion test device for marine equipment according to claim 10, characterized in that: The invention also comprises a supporting tool (4), wherein the supporting tool (4) is fixed to a column (104) of a tensile testing machine (1) via an elastic clamp (401), the elastic clamp (401) is hingedly connected to a swing arm (402) via a second screw rod (404) and a nut (405), and a tray (403) is welded and fixed to the swing arm (402); when the second screw rod (404) and the nut (405) are loosened, the swing arm (402) and the tray (403) are The support fixture (4) can rotate around the second screw rod (404). When the second screw rod (404) and the nut (405) are tightened, the rotation of the swing arm (402) and the tray (403) is restricted. The support fixture (4) is divided into two parts, which are respectively fixed on two columns (104) of the tensile testing machine (1). The two parts of the support fixture (4) are rotated toward the middle and closed through the swing arm (402). The two trays (403) jointly support the low-temperature corrosion solution box (5).
12. A multi-zone low temperature stress corrosion test device for marine equipment according to claim 11, characterized in that: The case (102) of the tensile testing machine (1) is installed on a horizontal ground via feet (101); two upright posts (104) are fixed to the case (102); a crossbeam (105) is installed on the upright posts (104); a limit baffle (106) and a lifting ring (107) are provided at the ends of the crossbeam (105); the crossbeam (105) can slide under the guidance of the two upright posts (104); a loading device (2) is installed on the crossbeam (105); the loading device (2) comprises an electric cylinder base (201), The electric cylinder body (207), the electric cylinder piston rod (208), and the electric cylinder base (201) are mounted on the electric cylinder fixing flange (202) of the crossbeam (105) through a bolt group 1 (203); the electric cylinder body (207) and the through hole of the crossbeam (105) are matched through a shaft sleeve (206); the side of the electric cylinder base (201) is provided with an integrated control box (204), and the integrated control box (204) is fixed to the electric cylinder base (201) through a bolt group 2 (205); a working The workbench (103) is provided with a fixed support (108), a movable support (109) is provided on the fixed support (108), and a transfer nut (110) is provided on the movable support (109); one end of an upper pull rod (301) of the connecting tool (3) is externally threaded and fixed to the electric cylinder piston rod (208) through a threaded connection; the other end of the upper pull rod (301) is internally threaded and fixed to the upper double fork ear (302) through a threaded connection, and the upper double fork ear (302) and the upper single fork ear (304) are connected by a pin one (303), one end of the lower pull rod (305) is an external thread and is fixed to the adapter nut (110) by a threaded connection; the other end of the lower pull rod (305) is an internal thread and is fixed to the lower double fork ear (306) by a threaded connection, the lower double fork ear (306) and the lower single fork ear (308) are connected by a pin two (307), and the upper single fork ear (304) and the lower single fork ear (308) are fixed by the internal thread and the external thread at both ends of the specimen (501).
13. A multi-zone low temperature stress corrosion test device for marine equipment according to claim 12, characterized in that: The corrosion solution circulation device (7) is connected to the corrosion solution tank (8) and the control computer (9) through pipelines and lines respectively. The temperature probe of the temperature sensor (502), the metal platinum sheet of the platinum sheet electrode (506), and the liquid junction of the reference electrode (510) are all installed at the same height as the test section of the test piece (501). The temperature monitoring data of the temperature sensor (502), the liquid level monitoring data of the liquid level sensor (514), and the flow monitoring data of the corrosion solution addition flow meter (703) and the corrosion solution reflux flow meter (704) are all integrated and transmitted to the control computer (9) through signal lines.
14. A multi-zone low temperature stress corrosion test device for marine equipment according to claim 13, characterized in that: The test piece (501) in the test cell (A21) serves as a working electrode, and forms a three-electrode test system with a platinum electrode (506) and a reference electrode (510). The test piece (501) is isolated from the tensile testing machine (1) and the low-temperature corrosion environment box (5) by insulating materials to ensure that the test piece (501) is in an electrochemically insulating state.
15. A method for testing multi-zone low-temperature stress corrosion of marine equipment, using a multi-zone low-temperature stress corrosion testing device for marine equipment as claimed in claim 1, characterized in that: The steps include: Step 1: Adjust the support fixture (4) to a suitable height, tighten the locking screw (406) and the locking nut (407) to fix the position of the support fixture (4); Step 2: Install the low-temperature corrosion environment box (5), place the low-temperature corrosion environment box (5) on the supporting tooling (4), and connect the pipelines between the low-temperature corrosion environment box (5) and the refrigeration device (6), the corrosion solution circulation device (7), and the corrosion solution box (8); Step 3: Install the test piece (501), retract the electric cylinder piston rod (208), firmly connect the upper end of the test piece (501) with the upper single fork ear (304) through threads, extend the electric cylinder piston rod (208), allow the test piece to pass through the low-temperature corrosion environment box (5), firmly connect the lower single fork ear (308) with the lower end of the test piece (501) through threads, adjust the extension amount of the electric cylinder piston rod (208), and connect the lower single fork ear (308) with the lower double fork ear (306) through the second pin (307); Step 4: Add cooling solution into the cooling solution pool (A18) and cover the cooling solution pool with a cover plate (A05); Step 5: Seal the low temperature corrosion environment box (5), tighten the watertight nut (F04), perform liquid sealing on the low temperature corrosion environment box (5), tighten the gas sealing nut (E01), perform gas sealing on the low temperature corrosion environment box (5); Step 6: By controlling the computer (9), the refrigeration device (6) and the circulation device (7) are started to start the circulation of the low-temperature corrosion solution; Step 7: Start the tensile testing machine (1) to perform stress cycling and start the low temperature stress corrosion test.
Citation Information
Cited By
High and low temperature composite environment sensitive fracture test system
CN119827316A
A high-low temperature combined environment sensitive fracture test system
CN119827316B