Preparation method of cobalt internal standard reagent for ore detection

The cobalt internal standard reagent is prepared by a method of melting, grinding and sieving in one step, which solves the problems of complex preparation and difficulty in controlling the accuracy of the cobalt internal standard reagent in the traditional method, realizes efficient and simple preparation of cobalt internal standard reagent, and improves the X-ray Detection efficiency of fluorescence spectroscopy.

CN118731076APending Publication Date: 2024-10-01PANGANG GRP XICHANG STEEL & VANADIUM CO LTD
View PDF 1 Cites 0 Cited by

Patent Information

Application Number
CN202410983359.9
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-22
Publication Date
2024-10-01

AI Technical Summary

Technical Problem

The preparation process of cobalt internal standard reagents used for iron ore detection using traditional methods is complicated and the accuracy is difficult to control. In particular, matrix interference and changes in ignition loss make it difficult to guarantee accuracy when measuring total iron content using glass flake fluorescence.

Method used

The cobalt internal standard reagent is prepared by a method of one-time melting, grinding and sieving, by mixing cobalt trioxide, lithium carbonate and lithium tetraborate in a ratio of 10:15:90, adding a release agent, melting at high temperature, and grinding and sieving after cooling. points to obtain internal standard reagents for XRF analysis.

Benefits of technology

The cobalt internal standard reagent can be prepared quickly and easily, and the weighing consistency accuracy is no more than 0.5mg, which shortens the preparation time, reduces the power consumption, and improves the detection efficiency.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure BDA0004956704680000031
    Figure BDA0004956704680000031
  • Figure BDA0004956704680000041
    Figure BDA0004956704680000041
  • Figure BDA0004956704680000051
    Figure BDA0004956704680000051
Patent Text Reader

Abstract

The invention relates to the technical field of preparation of internal standard reagents, in particular to a preparation method of a cobalt internal standard reagent for ore detection. The method comprises the following steps: (1) weighing cobalt sesquioxide, lithium carbonate and lithium tetraborate, and uniformly mixing; (2) putting the mixture obtained in the step (1) into a crucible, adding a release agent, and uniformly mixing; (3) melting the crucible filled with the mixture in the step (2) in a high-temperature muffle furnace, taking out, and cooling to room temperature to obtain a glass sheet; and (4) grinding the glass sheet obtained in the step (3) in a grinding machine, and screening to obtain the cobalt internal standard reagent for ore detection. According to the invention, the internal standard reagent can be rapidly prepared through one-time melting, grinding and sieving, and the weighing consistency precision is not more than 0.5 mg; the preparation time is short, the electric energy consumption is low, the operation is simple, convenient and rapid, and the detection efficiency of the X-ray fluorescence spectrometry is improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of internal standard reagent preparation, and in particular to a method for preparing an internal standard reagent for ore detection of cobalt. Background Art

[0002] The traditional chemical method for analyzing the main and secondary components of iron ore is inefficient and complicated to operate. The use of molten sample X-ray fluorescence spectrometry (XRF) is one of the important means to analyze the main and secondary components of iron ore. However, the composition of iron ore is relatively complex, and problems such as matrix interference and changes in loss on ignition make it difficult to control the accuracy of the total iron content when using the glass melt fluorescence method. The use of the internal standard method is one of the important measures to overcome problems such as matrix interference and changes in loss on ignition. At present, the industry uses the patented CN 108982562A method to prepare the internal standard reagent or directly weighs cobalt trioxide as the internal standard according to the GB / T6730.87-2023 method. The former requires multiple melting processes in the preparation process, and the operation is cumbersome; the latter does not require the weighing fluctuation to be greater than 0.2 mg, and the weighing consistency accuracy is required to be high. Summary of the invention

[0003] In order to solve the above technical problems, the present invention provides a method for preparing a cobalt internal standard reagent for ore detection, which can quickly prepare the internal standard reagent for XRF analysis through one-time melting, grinding and screening.

[0004] In order to achieve the above object, the technical solution of the present invention is as follows:

[0005] A method for preparing a cobalt internal standard reagent for ore detection, the method comprising the following steps:

[0006] (1) Weigh cobalt trioxide, lithium carbonate and lithium tetraborate and mix them evenly;

[0007] (2) placing the mixture obtained in step (1) in a crucible, adding a release agent, and mixing;

[0008] (3) placing the crucible containing the mixture in step (2) in a high-temperature muffle furnace for melting, taking it out and cooling it to room temperature to obtain a glass sheet;

[0009] (4) placing the glass sheet obtained in step (3) in a grinder, grinding, and sieving to obtain a cobalt internal standard reagent for ore detection.

[0010] In the above technical solution, further, in step (1), the mass ratio of cobalt trioxide, lithium carbonate and lithium tetraborate is 10:15:90.

[0011] In the above technical solution, further, in step (2), the release agent is lithium iodide.

[0012] In the above technical solution, further, in step (3), the melting temperature is 1120°C ± 10°C, and the melting time is ≥ 15 min.

[0013] In the above technical solution, further, in step (4), grinding is carried out in three stages, the rotation speed of the grinder is 1400 r / min, the time for the first grinding stage is 15±1 s, the time for the second grinding stage is 10±1 s, and the time for the third grinding stage is 5±1 s.

[0014] In the above technical solution, further, in step (4), screening uses a standard sieve with a pore size of 0.15 mm.

[0015] In the above technical solution, further, the crucible is a platinum-gold crucible.

[0016] The beneficial effects of the present invention are:

[0017] The invention can quickly prepare the internal standard reagent by melting, grinding and screening once, and the weighing consistency accuracy is no more than 0.5 mg.

[0018] The method of the present invention has short preparation time, low power consumption, simple and quick operation, and is more conducive to improving the detection efficiency of X-ray fluorescence spectroscopy. DETAILED DESCRIPTION

[0019] The following examples may enable those skilled in the art to more fully understand the present invention, but are not intended to limit the present invention in any way.

[0020] Unless otherwise specified, the materials used in the embodiments of the present invention can be obtained through commercial channels or prepared according to conventional methods well known to those skilled in the art.

[0021] The present invention provides a method for preparing a cobalt internal standard reagent for ore detection, comprising the following steps:

[0022] (1) Weigh 10.0000 g of cobalt trioxide, 15.0000 g of lithium carbonate, and 90.0000 g of lithium tetraborate respectively into a glass beaker and mix well;

[0023] (2) the mixture obtained in step (1) was divided into 6 platinum-gold crucibles, 10 drops (about 0.05 ml) of 500 g / L lithium iodide solution was added to each crucible, and mixed;

[0024] (3) placing the crucible containing the mixture in step (2) in a high-temperature muffle furnace at 1120° C.±10° C. and melting for 15 min, taking out and quickly shaking, and cooling to room temperature to obtain a glass sheet;

[0025] (4) The glass sheet obtained in step (3) is placed in a grinder and ground in three stages. The rotation speed of the grinder is 1400 r / min. The time for the first stage of grinding is 15±1 s, the time for the second stage of grinding is 10±1 s, and the time for the third stage of grinding is 5±1 s. The glass sheet is completely passed through a 0.15 mm standard sieve and is set aside.

[0026] GB / T6730.87-2023 “Determination of total iron and other multi-element content in iron ore-Wavelength dispersive X-ray fluorescence spectrometry (cobalt internal standard method)” was used to determine the standard sample. The cobalt internal standard prepared by the above preparation method is suitable for the composition detection of ore samples such as vanadium-titanium concentrate, general ore, vanadium-titanium iron concentrate, etc. The accuracy test results are shown in Tables 1 and 2.

[0027] Table 1 Results of the accuracy test of the components determined in the standard samples of vanadium-titanium ore and vanadium sintering (w / %)

[0028]

[0029]

[0030]

[0031] Table 2 Results of the accuracy test of the components determined in the standard samples of common ore (w / %)

[0032]

[0033]

[0034] The above embodiments are only preferred embodiments of the present invention and are not intended to limit the implementation methods. The protection scope of the present invention shall be subject to the scope defined in the claims. Other different forms of changes or modifications may be made based on the above description. Obvious changes or modifications derived therefrom are still within the protection scope of the present invention.

Claims

1. A method for preparing a cobalt internal standard reagent for ore detection, It is characterized in that The method comprises the following steps: (1) Weigh cobalt trioxide, lithium carbonate and lithium tetraborate and mix them evenly; (2) placing the mixture obtained in step (1) in a crucible, adding a release agent, and mixing; (3) placing the crucible containing the mixture in step (2) in a high-temperature muffle furnace for melting, taking it out and cooling it to room temperature to obtain a glass sheet; (4) placing the glass sheet obtained in step (3) in a grinder, grinding, and sieving to obtain a cobalt internal standard reagent for ore detection.

2. The method for preparing a cobalt internal standard reagent for ore detection according to claim 1, It is characterized in that In step (1), the mass ratio of cobalt trioxide, lithium carbonate and lithium tetraborate is 10:15:

90.

3. The method for preparing a cobalt internal standard reagent for ore detection according to claim 1, It is characterized in that In step (2), the release agent is lithium iodide.

4. The method for preparing a cobalt internal standard reagent for ore detection according to claim 1, It is characterized in that In step (3), the melting temperature is 1120°C ± 10°C, and the melting time is ≥ 15 min.

5. The method for preparing a cobalt internal standard reagent for ore detection according to claim 1, It is characterized in that In step (4), the grinding is carried out in three stages. The rotation speed of the grinding machine is 1400 r / min. The time for the first grinding stage is 15±1 s, the time for the second grinding stage is 10±1 s, and the time for the third grinding stage is 5±1 s.

6. The method for preparing a cobalt internal standard reagent for ore detection according to claim 1, It is characterized in that In step (4), a standard sieve with a pore size of 0.15 mm is used for screening.

7. The method for preparing a cobalt internal standard reagent for ore detection according to claim 1, It is characterized in that The crucible is a platinum-gold crucible.

Citation Information

Patent Citations

  • Method for preparing glass piece for cobalt internal standard XRF analysis based on demould aid