Laser annealing energy control method and laser annealing equipment

By gradually adjusting the laser power during the laser annealing process, the problems of difficult heat dissipation and energy peaks at the edge of the substrate are solved, the annealing uniformity and yield are improved, and substrate cracking is avoided.

CN118737816APending Publication Date: 2024-10-01AMIES TECHNOLOGY CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202310339587.8
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2023-03-31
Publication Date
2024-10-01

AI Technical Summary

Technical Problem

During the laser annealing process, the lack of a heat dissipation surface at the edge of the substrate makes it difficult to dissipate heat, increases the thermal budget, and is prone to substrate cracking or yield reduction after being stimulated by thermal stress.

Method used

By gradually adjusting the laser power during the laser annealing process, the first laser power is reduced to the second laser power, then raised to the third laser power at the second position, and the power is rapidly increased at the incised point of the edge of the substrate to preheat Optical path to avoid fragmentation problems caused by energy spikes and thermal stress.

Benefits of technology

It effectively reduces energy spikes and thermal stress at the edge of the substrate, avoids substrate fragmentation and yield reduction, and improves annealing uniformity and spot quality.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118737816A_ABST
    Figure CN118737816A_ABST
Patent Text Reader

Abstract

The invention provides a laser annealing energy control method and a laser annealing device.The laser annealing energy control method comprises the steps that a laser spot moves relative to a substrate at first laser power, and the laser power of the laser spot is reduced to second laser power at a first position relative to the substrate; moving the laser spot relative to the substrate to a second position relative to the substrate; moving the laser spot relative to the substrate from the second position relative to the substrate to a third position relative to the substrate, and increasing the laser power to third laser power; and the laser spot performs scanning annealing on the substrate at the third laser power. The laser spot moves to the edge of the substrate relative to the substrate, so that the laser power is reduced, and the substrate edge energy peak problem and the fragment problem caused by thermal stress are avoided.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the field of semiconductor technology, and in particular to a laser annealing energy control method and laser annealing equipment. Background Art

[0002] In recent years, as the process nodes of integrated circuits have developed towards smaller and smaller sizes (40nm and below), the junction depths of the source-drain region and the lightly doped drain (LDD) region have gradually decreased, and the corresponding shallow junction manufacturing has become an increasingly important process module. In order to solve the short channel effect caused by the reduction in gate length, the source and drain electrodes need to be shallowly ion implanted to form an ultra-shallow junction (USJ). The annealing process determines the junction depth and lateral dimensions of the source-drain PN junction and the lightly doped drain PN junction, so the annealing process is required to have a high annealing temperature and a low annealing thermal budget to meet the requirements of advanced manufacturing processes for low stress, low diffusion, high activation, and high uniformity.

[0003] Laser annealing is a commonly used annealing process in integrated circuit technology. Laser annealing uses a laser beam with a certain amount of energy to quickly scan the surface of the substrate, thereby achieving the effect of microsecond annealing of a certain differential area on the substrate. During laser scanning, the heat in the middle part of the substrate can be dissipated to the edge area of ​​the substrate, but the situation at the edge of the substrate is more complicated: on the one hand, the edge of the substrate lacks a heat dissipation surface, which makes heat dissipation difficult, and the annealing time is extended in disguise, increasing the thermal budget; on the other hand, there are some potential defects at the edge of the substrate, which are easily broken by the defects after being stimulated by thermal stress.

[0004] One solution to the above problem is to set a guard ring at the edge of the substrate. However, when annealing is performed from the edge of the substrate, there is a phenomenon of substrate edge fragmentation caused by high power entry, edge defects or thermal stress. This is because during the annealing process, due to heat diffusion in the middle area of ​​the substrate, edge defects and energy control switching at the edge of the substrate, energy spikes will appear, so it is easy to cause substrate fragmentation or yield reduction after being stimulated by thermal stress.

[0005] Another solution to the above problem is to perform constant power control through a software interface, and suppress the laser power output through a gate signal during the annealing process, that is, high-level light output and low-level light shut-off. However, this method has the problem of excessive power mutation after large energy switching, and energy spikes appear in the energy control at the edge of the substrate, resulting in uneven annealing surface temperature, prone to abnormal traces, thereby reducing the yield, or causing fragmentation problems. Summary of the invention

[0006] The object of the present invention is to provide a laser annealing energy control method and a laser annealing device to reduce or avoid the probability of substrate fragmentation or yield reduction during the laser annealing process.

[0007] In order to solve the above technical problems, the present invention provides a laser annealing energy control method, comprising:

[0008] A laser spot is moved relative to a substrate with a first laser power, and the laser power of the laser spot is reduced to a second laser power at a first position relative to the substrate; the laser spot is moved relative to the substrate to a second position relative to the substrate; the laser spot is moved relative to the substrate from the second position relative to the substrate to a third position relative to the substrate and the laser power is increased to a third laser power; the laser spot performs scanning annealing on the substrate with the third laser power.

[0009] Optionally, the laser spot is moved relative to the substrate from a first position relative to the substrate to a second position relative to the substrate with the second laser power.

[0010] Optionally, the laser spot is moved relative to the substrate from a second position relative to the substrate to a third position relative to the substrate, and the second laser power is first increased to a fourth laser power and then increased to the third laser power.

[0011] Optionally, a rate of increasing the laser power from the second laser power to the fourth laser power is greater than a rate of increasing the laser power from the fourth laser power to the third laser power.

[0012] Optionally, the fourth laser power is 50% to 150% of the first laser power.

[0013] Optionally, the first position relative to the substrate is at the tangent point of the substrate edge along the movement direction of the laser spot relative to the substrate or in front of the tangent point of the substrate edge; the second position relative to the substrate is at the intangent point of the substrate edge along the movement direction of the laser spot relative to the substrate or behind the intangent point of the substrate edge.

[0014] Optionally, the first laser power is one third to two thirds of the third laser power; and the second laser power is less than one third of the third laser power.

[0015] Based on the same inventive concept, the present invention also provides a laser annealing device for executing any of the above-mentioned laser annealing energy control methods.

[0016] In a laser annealing energy control method and laser annealing equipment provided by the present invention, a laser spot is moved relative to a substrate with a first laser power, and the laser power of the laser spot is reduced to a second laser power at a first position relative to the substrate; the laser spot is moved relative to the substrate to a second position relative to the substrate; the laser spot is moved relative to the substrate from the second position relative to the substrate to a third position relative to the substrate and the laser power is increased to a third laser power; the laser spot performs scanning annealing on the substrate with the third laser power. The laser spot is moved relative to the substrate to the first position of the substrate, and the first laser power is switched to the second laser power to reduce the laser power and avoid substrate fragments.

[0017] Furthermore, the laser spot is moved relative to the substrate to the second position of the substrate, and the second laser power is first increased to the fourth laser power. The rapid increase in power can preheat the lens in the light path, reduce the expansion effect, improve the uniformity of the spot, allow a higher spot quality to enter the scan, and improve the annealing uniformity. Then the fourth laser power is increased to the third laser power, avoiding the problem of energy peaks at the edge of the substrate and the problem of fragments caused by thermal stress. BRIEF DESCRIPTION OF THE DRAWINGS

[0018] Those skilled in the art will appreciate that the accompanying drawings are provided for a better understanding of the present invention and do not constitute any limitation on the scope of the present invention.

[0019] Figure 1 is a schematic flow chart of a laser annealing energy control method according to an embodiment of the present invention;

[0020] Figure 2 It is a schematic structural diagram of the process flow of substrate position and laser power variation in the laser annealing process of an embodiment of the present invention;

[0021] Figure 3 is a schematic diagram of a process curve of substrate position and laser power variation in a laser annealing process according to an embodiment of the present invention;

[0022] Figure 4 is a schematic structural diagram of a substrate scanning field in a laser annealing process according to an embodiment of the present invention;

[0023] In the attached figure:

[0024] 10 - substrate; 10a - first field scan; 10b - second field scan. DETAILED DESCRIPTION

[0025] In order to make the purpose, advantages and features of the present invention clearer, the present invention is further described in detail below in conjunction with the accompanying drawings and specific embodiments. It should be noted that the drawings are all in a very simplified form and are not drawn to scale, and are only used to conveniently and clearly assist in explaining the purpose of the embodiments of the present invention. In addition, the structure shown in the drawings is often a part of the actual structure. In particular, the emphasis of each drawing is different, and sometimes different scales are used.

[0026] As used in the present invention, the singular forms "a", "an" and "the" include plural objects, the term "or" is generally used in a sense including "and / or", the term "several" is generally used in a sense including "at least one", and the term "at least two" is generally used in a sense including "two or more". In addition, the terms "first", "second" and "third" are used for descriptive purposes only and cannot be understood as indicating or suggesting relative importance or implicitly indicating the number of the indicated technical features. Therefore, the features defined as "first", "second", and "third" may explicitly or implicitly include one or at least two of the features. The term "proximal end" is usually the end close to the operator, and the term "distal end" is usually the end close to the patient. "One end" and "the other end" as well as "proximal end" and "distal end" usually refer to two corresponding parts, which include not only the endpoints. The terms "installed", "connected", and "connected" should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral body; it can be a mechanical connection or an electrical connection; it can be directly connected or indirectly connected through an intermediate medium, and it can be the internal connection of the two elements or the interaction relationship between the two elements. In addition, as used in the present invention, an element is arranged on another element, which usually only means that there is a connection, coupling, matching or transmission relationship between the two elements, and the connection, coupling, matching or transmission between the two elements can be direct or indirect through an intermediate element, and it cannot be understood as indicating or implying the spatial position relationship between the two elements, that is, one element can be in any position such as inside, outside, above, below or on one side of another element, unless the content clearly indicates otherwise. For those skilled in the art, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.

[0027] Figure 1 FIG. 1 is a flow chart of a laser annealing energy control method according to an embodiment of the present invention. Figure 1 As shown, this embodiment provides a laser annealing energy control method, comprising:

[0028] Step S10, moving the laser spot relative to the substrate at a first laser power, and reducing the laser power of the laser spot to a second laser power at a first position relative to the substrate;

[0029] The first laser power may be reduced to the second laser power gradually or immediately.

[0030] Step S20, moving the laser spot relative to the substrate to a second position relative to the substrate; moving the laser spot relative to the substrate from the second position relative to the substrate to a third position relative to the substrate and increasing the laser power to a third laser power, the laser spot scanning annealing the substrate with the third laser power.

[0031] The laser spot can be moved relative to the substrate from a first position relative to the substrate to a second position relative to the substrate at the second laser power. During the movement, the power can also be increased or decreased.

[0032] Further, the laser spot moves relative to the substrate from a second position relative to the substrate to a third position relative to the substrate, and the second laser power is first increased to a fourth laser power, and then increased to the third laser power. The rate of increasing the laser power from the second laser power to the fourth laser power is greater than the rate of increasing the laser power from the fourth laser power to the third laser power.

[0033] Step S30, moving the laser spot relative to the substrate at a third laser power, and reducing the laser power of the laser spot to the second laser power at a fourth position relative to the substrate;

[0034] Step S40, moving the laser spot relative to the substrate with the second laser power, switching the laser power of the laser spot to the first laser power at a fifth position relative to the substrate, and ending the first field scan;

[0035] Step S50, looping the above field scanning process until the entire substrate completes the annealing process.

[0036] In this embodiment, the laser annealing process can use analog signals to control the increase or decrease of laser power. Laser modulation uses light as a carrier to load signals onto light, and realizes signal transmission according to application requirements. General modulation is divided into external modulation and internal modulation. External modulation refers to mechanical modulation or acousto-optic modulation performed outside the laser, and internal modulation refers to power drive modulation. Among them, internal modulation is further divided into TTL (Transister-Transister-Logic) modulation and analog modulation. TTL modulation in the prior art is to input a high or low level (0V or 5V) DC signal of a certain frequency to the laser through the outside world. The low level turns off the light, and the high level outputs full power, and the high level amplitude is not adjustable. The laser modulation of this embodiment chooses to use analog modulation, which can freely adjust the waveform and amplitude of the input signal, and the laser output power changes linearly with the input analog voltage signal.

[0037] like Figure 2 As shown, before the laser annealing process is performed on the substrate, the laser is located in a safe position, that is, there is no positive film under the laser, and a test film or a blocking device that will not be burned by the laser is set under the laser. The laser power is increased to the annealing power (Annealing Power), and the power stability is tested, and then set to the safe power (safePower). The laser power is reduced to the safe shutter power, and then switched to the travel power. Then, the laser spot is moved relative to the substrate to the first position relative to the substrate at the travel power (first laser power). The laser power is reduced from the travel power to the safe power. The laser spot is moved relative to the substrate to the second position relative to the substrate and immediately increased to the travel power. Then, it is increased to the annealing power by the ramp control function. That is, the laser power is the annealing power when the laser spot is moved relative to the substrate to the third position relative to the substrate. The laser spot is moved relative to the substrate to the fourth position relative to the substrate, and the annealing power is switched to the safe power. The laser spot is moved relative to the substrate to the fifth position relative to the substrate, and the first field scan is completed. The laser spot is switched to the travel power, and then the next field scan is performed. The laser spot is moved relative to the substrate to the second position relative to the substrate and immediately increased to the travel power means that the safe power is increased to the travel power within the fastest response time of the laser device.

[0038] Specifically, Figure 2As shown, a substrate 10 is provided, and a laser spot is moved relative to the substrate with a first laser power P1 to a first position A relative to the substrate, and the first laser power P1 is reduced to a second laser power P2, which can be reduced immediately or gradually; the first position A of the substrate 10 is located at the first tangent point outside the edge of the substrate 10 or before the first tangent point on the edge of the substrate along the movement direction of the laser spot relative to the substrate, and the distance between the first position A of the substrate and the first tangent point outside the edge of the substrate is, for example, 0-5mm. In this embodiment, the distance between the first position A of the substrate 10 and the first tangent point outside the edge of the substrate is, for example, 0.5mm, that is, before the laser spot is moved relative to the substrate to the edge of the substrate 10, the first laser power P1 has been reduced to the second laser power P2. The first laser power P1 is the inter-field switching power, and the first laser power P1 (Travel Power) can be configured as a machine constant according to the process requirements. The configuration parameter is used for the inter-field switching transition power during the scanning process. The first laser power P1 is, for example, 1000W-2000W. The first laser power P1 is one-third to two-thirds of the third laser power P3. The second laser power P2 is a safe power. The second laser power P2 (SafePower) can be configured as a machine constant according to process requirements. This configuration parameter is used for annealing protection power at the edge of the substrate. The second laser power P2 is, for example, 0-1000W. The second laser power P2 is less than one-third of the third laser power P3. At the edge of the substrate, the safe laser power is used to move the laser spot relative to the substrate to enter, and the internal power of the laser is ensured to be in a stable state to avoid a decrease in laser power stability caused by power switching.

[0039] like Figure 2 and Figure 3As shown, the laser spot is moved from the first position A of the substrate 10 relative to the substrate to the second position B of the substrate with the second laser power P2, and the second laser power P2 is immediately increased to the fourth laser power P4, and then the fourth laser power P4 is increased to the third laser power P3 within a predetermined time. In other words, the laser spot is moved from the second position B relative to the substrate to the third position C relative to the substrate, and the second laser power P2 is first increased to the fourth laser power P4, and then increased to the third laser power P3. The rate of increasing the laser power from the second laser power P2 to the fourth laser power P4 is greater than the rate of increasing the laser power from the fourth laser power P4 to the third laser power P3. The fourth laser power P4 is 50% to 150% of the first laser power P1. In this embodiment, the fourth laser power P4 is 100% of the first laser power P1, that is, the second laser power P2 is immediately increased to the first laser power P1. The second position B of the substrate 10 is located at the first inscribed point in the edge of the substrate or after the first inscribed point along the moving direction of the laser spot relative to the substrate. That is, after the laser spot moves relative to the substrate to the first inscribed point on the edge of the substrate, the laser power is immediately increased to the first laser power P1. The laser spot is moved relative to the substrate at a low power to the first inscribed point in the edge of the substrate so that the second laser power P2 is immediately increased to the first laser power P1. The rapid increase in power can preheat the lens in the light output path, reduce the expansion effect, improve the uniformity of the spot, and allow a higher spot quality to enter the scan, thereby improving the annealing uniformity. The laser power is increased to the third laser power P3, and the position of the substrate is just scanned to the annealing starting point, for example, 2 mm from the edge of the substrate. The substrate within the range of 2 mm from the edge of the substrate does not need to be annealed, and the third laser power P3 is the annealing power. The third laser power P3 is, for example, 2000W-3000W. The third laser power P3 can modify the process parameters according to the process requirements. This configuration parameter is used for the annealing process power, and this embodiment is not limited. The ramp power control function is used to increase the first laser power P1 to the third laser power P3. The time for immediately increasing the second laser power P2 to the first laser power P1 is less than the time for increasing the first laser power P1 to the third laser power P3. The predetermined time for increasing the first laser power P1 to the third laser power P3 within a predetermined time is, for example, less than 50ms. In this embodiment, the predetermined time for increasing the first laser power P1 to the third laser power P3 within a predetermined time is 0.01ms-10ms. The ramp power control time is within 50ms, which can effectively avoid the laser energy spike problem and the substrate fragmentation problem, and the power climbing rate is 500W / ms for the best. Start executing the scanning annealing process of the first field.The ramp power control can configure the machine constants according to the process requirements. This configuration parameter is used to control the power control during the switching process between scanning fields from the first laser power P1 to the third laser power P3. The power ramp time can be adjusted to preheat the scanning start position to avoid the problem of energy overshoot when switching with high power. By switching the states of the first laser power P1 and the third laser power P3, the abnormal trace or fragmentation phenomenon at the scanning start position of the substrate 10 caused by the excessive power of the first pulse in the high energy switching process can be reduced. The ramp power control function can be used to preheat the laser spot relative to the substrate to the starting position of the substrate 10, while reducing the energy overshoot phenomenon, avoiding the fragmentation problem, and improving the annealing uniformity. The ramp power control function can avoid the problem of energy spikes during energy switching, so that the laser beam energy can be smoothly transitioned and output smoothly, avoiding edge defects or thermal stress causing fragmentation problems.

[0040] Continue to refer Figure 2 and Figure 3 , the laser spot is moved from the third position C of the substrate 10 relative to the substrate to the fourth position D of the substrate 10 with the third laser power P3, and the third laser power P3 is switched to the second laser power P2; the fourth position D of the substrate 10 is located at the second inscribed point in the edge of the substrate along the moving direction of the laser spot relative to the substrate or before the second inscribed point, that is, the laser spot has not moved relative to the substrate to the second inscribed point in the edge of the substrate, and the laser power has been reduced to the second laser power. In this embodiment, the laser power is switched to the second laser power P2 at a position 0.5mm before the end of the first field scanning at the edge inscribed position of the substrate.

[0041] The laser spot is moved relative to the substrate with the second laser power P2 to the fifth position E of the substrate 10, and the second laser power P2 is switched to the first laser power P1, and the first field scan is ended; the fifth position E of the substrate 10 is located at the second circumscribed point outside the edge of the substrate along the movement direction of the laser spot relative to the substrate or after the second circumscribed point, and the distance between the fifth position E of the substrate and the second circumscribed point outside the edge of the substrate is 0-5mm. In other words, the second laser power P2 is switched to the first laser power P1 only after the laser spot moves relative to the substrate to the second circumscribed point outside the edge of the substrate. Specifically, after the scanning synchronization moves to the outside of the edge of the substrate, after the first field receives the scanning synchronization end signal, the laser power is controlled to be reduced to the first laser power P1 through the analog (Analog) signal. In order to solve the problem of damage caused by the same point of light being relatively still when the workpiece stage slows down and accelerates during field switching, there is a relative speed still section when the motion stage slows down at the end of scanning and starts to accelerate between scanning fields. Through laser power control, the laser power is reduced from the first laser power P1 to the second laser power P2 in the still section, reducing static annealing at the same position and the appearance of abnormal traces at the edge of the substrate annealing position. At the beginning of the workpiece stage acceleration stage, the laser is increased to the first laser power P1 to keep the laser power stable, maintain thermal deformation of the lens, and maintain a good spot shape.

[0042] The above field scanning process is repeated until the entire substrate completes the annealing process. Figure 1 and 4 As shown, there are multiple field scans in the substrate, for example, including the first field scan 10a and the second field scan 10b. After completing the first field scan 10a, the second field scan 10b continues. Specifically, the second field scan 10b switches the energy to the second laser power P2 (Safe Power) at the first position of the substrate, and moves the laser spot relative to the substrate at a low power to the inscribed position within the edge of the substrate so that the second laser power P2 (Safe Power) is immediately increased to the first laser power P1 (Travel Power). The laser output power is increased to the third laser power P3 through the ramp power control function, and the scanning annealing process of the second field is started, and the above scanning process is cycled to the last field.

[0043] exist Figure 4In the figure, the circumscribed point is where the laser spot contacts the outer edge of the substrate, and the inscribed point is where the laser spot contacts the inner edge of the substrate. In the present embodiment, the first position A of the substrate 10 is located at the first circumscribed point outside the edge of the substrate 10 along the movement direction of the laser spot relative to the substrate or before the first circumscribed point, and the distance between the first position A of the substrate and the first circumscribed point outside the edge of the substrate is, for example, 0-5 mm. The second position B of the substrate 10 is located at the first inscribed point inside the edge of the substrate along the movement direction of the laser spot relative to the substrate or after the first inscribed point. The third position C of the substrate 10 is switched to the third laser power relative to the movement direction of the laser spot of the substrate. The fourth position D of the substrate 10 is located at the second inscribed point inside the edge of the substrate along the movement direction of the laser spot relative to the substrate or before the second inscribed point. The fifth position E of the substrate 10 is located at or behind the second circumference point outside the edge of the substrate along the movement direction of the laser spot relative to the substrate, and the distance between the fifth position E of the substrate and the second circumference point outside the edge of the substrate is 0-5mm.

[0044] This embodiment also provides a laser annealing device for executing the above-mentioned laser annealing energy control method.

[0045] In summary, in a laser annealing energy control method and laser annealing equipment provided by an embodiment of the present invention, a laser spot is moved relative to a substrate with a first laser power, and the laser power of the laser spot is reduced to a second laser power at a first position relative to the substrate; the laser spot is moved relative to the substrate to a second position relative to the substrate; the laser spot is moved relative to the substrate from the second position relative to the substrate to a third position relative to the substrate and the laser power is increased to a third laser power; the laser spot performs scanning annealing on the substrate with the third laser power. The laser spot is moved relative to the substrate to the first position and the fourth position of the substrate, and the first laser power is switched to the second laser power to reduce the laser power and avoid substrate fragments; the laser spot is moved relative to the substrate to the second position of the substrate, and the second laser power is increased to the fourth laser power. The rapid increase in power can preheat the lens in the light path, reduce the expansion effect, improve the uniformity of the spot, and allow a higher spot quality to enter the scan, thereby improving the uniformity of the annealing. The laser power is increased to the third laser power by a ramp power control method, which avoids the problem of energy peaks at the edge of the substrate and the problem of fragments caused by thermal stress. There is a period of near-stationary state between the deceleration or acceleration of the workpiece stage during the switching process between scanning fields. By switching the laser power to a safe power, energy trace abnormalities or damage can be avoided at the stationary position.

[0046] It should be noted that the various embodiments in this specification are described in a progressive manner, and each embodiment focuses on the differences from other embodiments. The same or similar parts between the various embodiments can be referenced to each other. In addition, the different parts between the various embodiments can also be used in combination with each other, and the present invention is not limited to this.

[0047] In addition, it should be recognized that although the present invention has been disclosed as a preferred embodiment, the above embodiment is not intended to limit the present invention. For any technician familiar with the art, without departing from the scope of the technical solution of the present invention, the technical content disclosed above can be used to make many possible changes and modifications to the technical solution of the present invention, or modified into equivalent embodiments of equivalent changes. Therefore, any simple modification, equivalent change and modification made to the above embodiment according to the technical essence of the present invention without departing from the content of the technical solution of the present invention still belongs to the scope of protection of the technical solution of the present invention.

Claims

1. A laser annealing energy control method, characterized in that: include: Moving a laser spot relative to a substrate at a first laser power, and reducing the laser power of the laser spot to a second laser power at a first position relative to the substrate; The laser spot is moved relative to the substrate to a second position relative to the substrate; the laser spot is moved relative to the substrate from the second position relative to the substrate to a third position relative to the substrate and the laser power is increased to a third laser power; the laser spot performs scanning annealing on the substrate with the third laser power.

2. The laser annealing energy control method according to claim 1, characterized in that: The laser spot is moved relative to the substrate at the second laser power from a first position relative to the substrate to a second position relative to the substrate.

3. The laser annealing energy control method according to claim 1, characterized in that: The laser spot is moved relative to the substrate from a second position relative to the substrate to a third position relative to the substrate, and the second laser power is first increased to a fourth laser power and then increased to the third laser power.

4. The laser annealing energy control method according to claim 3, characterized in that: An increasing rate of increasing the laser power from the second laser power to the fourth laser power is greater than an increasing rate of increasing the laser power from the fourth laser power to the third laser power.

5. The laser annealing energy control method according to claim 3, characterized in that: The fourth laser power is 50% to 150% of the first laser power.

6. The laser annealing energy control method according to claim 1, characterized in that: The first position relative to the substrate is at the tangent point of the substrate edge or in front of the tangent point of the substrate edge along the movement direction of the laser spot relative to the substrate; the second position relative to the substrate is at the intangent point of the substrate edge or behind the intangent point of the substrate edge along the movement direction of the laser spot relative to the substrate.

7. The laser annealing energy control method according to claim 1, characterized in that: The first laser power is one third to two thirds of the third laser power; and the second laser power is less than one third of the third laser power.

8. A laser annealing device, characterized in that: Used to execute the laser annealing energy control method according to any one of claims 1 to 7.