Wafer level testing after laser dicing
Through invisible laser cutting and back grinding technology, the problem of low-level defects in testing and separation after laser cutting is solved, high-quality electrical testing and die separation are achieved, and the efficiency and product quality of semiconductor manufacturing are improved.
Patent Information
- Application Number
- CN202410363576.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Priority Date
- 2023-03-31
- Filing Date
- 2024-03-28
- Publication Date
- 2024-10-01
AI Technical Summary
In the semiconductor manufacturing process, testing and separating dies after laser cutting suffers from low-level laser scattering or spatter defects, and existing technology makes it difficult to effectively perform high-quality electrical testing and die separation.
Stealth laser cutting technology is used to direct a laser beam along the scribe lane on the first side of the semiconductor substrate to create modified areas and induce cracks, followed by electrical testing and back grinding to separate the dies and use dicing tape to space the dies for pickup.
High-quality electrical testing after laser cutting is achieved to ensure the robustness of the die, and through the use of back grinding and cutting tape, the die is effectively separated and picked up, improving manufacturing efficiency and product quality.
Smart Images

Figure CN118737865A_ABST
Abstract
Description
Technical Field
[0001] The present description relates to systems and methods for performing wafer-level testing after laser dicing. Background Art
[0002] Die preparation is part of the semiconductor device manufacturing process, where the wafer is prepared for integrated circuit (IC) packaging and testing. The die preparation process usually includes wafer cutting (dicing). Before wafer cutting, the wafer is mounted on a tape (e.g., a dicing tape). The wafer cutting process is used to separate individual dies from the semiconductor wafer when mounted on the dicing tape. The cutting process can involve scribing and breaking, mechanical sawing, or laser cutting. After the wafer cutting is completed, the die will remain on the dicing tape until it is extracted by the die handling equipment (such as a die bonding machine or a die sorter) in the packaging process later. Summary of the invention
[0003] In one example described, a method includes thinning a first side of a semiconductor substrate, wherein a plurality of dies are formed on a second side of the substrate opposite the first side and separated from each other by scribe lanes of the substrate. The method also includes directing a laser beam along the scribe lanes thereof at an entry point at the first side, wherein the laser beam is focused within the substrate to form at least one modified region within the substrate at a location spaced apart from the first side, and at least one crack propagates from the modified region toward the first side. The method also includes electrically testing the dies on the substrate, wherein the tested dies are located between the modified regions of the corresponding scribe lanes of the substrate.
[0004] In another described example, a method includes directing a laser beam at a first surface of a semiconductor substrate along a scribe line thereof with an entry point, wherein the laser beam is focused within the substrate to form at least one modified region within a corresponding layer of the substrate at a location spaced apart from the first surface, and at least one crack propagates from the modified region toward the first surface. The method also includes removing a tape from a second surface of the substrate opposite the first surface, and electrically testing a plurality of dies on the substrate, wherein the tested dies are located between the modified regions of the corresponding scribe line of the substrate.
[0005] In another described example, a semiconductor device includes a semiconductor die, wherein the semiconductor die includes an integrated circuit in a semiconductor substrate. The semiconductor die has a sidewall extending between a first surface and a second surface, a first surface region of the sidewall extending from the first surface to an intermediate position has a first texture, and a second surface region extending from the intermediate position to the second surface has a second texture that is smoother than the first texture. BRIEF DESCRIPTION OF THE DRAWINGS
[0006] Figure 1is a flow chart describing an example die separation method that may be used to form a semiconductor device.
[0007] Figure 2A , Figure 2B , Figure 3 , Figure 4 , Figure 5 , Figure 6 , Fig. 7A , Figure 7B , Figure 7C , Figure 8 and Fig. 9 is based on Figure 1 A cross-sectional view of a semiconductor device processed by the method.
[0008] Fig.10 is a side view of a semiconductor die showing an example of texture along a sidewall of the die. DETAILED DESCRIPTION
[0009] The present specification relates to a semiconductor manufacturing method including wafer-level testing implemented after laser cutting, and a semiconductor device produced by this method. For example, the method includes performing stealth laser cutting, such as by guiding a laser beam along its scribe line with an entry point on a first side of a semiconductor substrate (e.g., a wafer). One or more integrated circuits are located on a second side (e.g., top or front) of the substrate opposite to the first side to which the laser beam is directed. The laser beam can be focused inside the substrate to form at least one modified region in the substrate at a position spaced apart from the first side. At least one crack propagates from the modified region to the first side of the substrate in the substrate. The crack can also propagate from the modified region to the second side of the substrate. After laser cutting, the die on the substrate is electrically tested, such as by testing equipment having an arrangement of probes or needles configured to contact pads on each die. Therefore, each die tested is located between the modified region and the associated crack of the corresponding scribe line of the substrate.
[0010] The method may further include separating the dies from each other along the cracks and through the corresponding modified areas that have been formed in the corresponding scribe lanes. For example, a tape (e.g., a back grinding tape) is applied to the second side of the substrate, and the first side is thinned, such as by back grinding the substrate using a surface grinder or a grinding wheel. The back grinding can remove a sufficient amount from the first side of the substrate to separate the dies. In an example, the back grinding is performed to remove a portion of the substrate so that it is sufficient to remove the cracks in the substrate between the first side and the modified area. Therefore, the sidewall surfaces of the corresponding dies each have a modified texture along a first sidewall surface area extending from the first surface to the middle position. The modified texture is provided in response to separating adjacent dies by the modified area. The sidewall surfaces of the corresponding dies also have different textures along a second sidewall surface area extending from the middle position to the second surface. For example, the different textures are in response to separating adjacent dies by the cracks.
[0011] A dicing tape may be applied to the thinned second side, and the back grinding tape may be removed from the first side so that the separated die is located on the dicing tape. The dicing tape may be expanded to space the respective die from each other, such as to provide a desired die-to-die gap to facilitate picking up the die for further manufacturing. Further manufacturing may include die attach operations and wire bonding relative to a lead frame or other packaging structure. The resulting IC chip may be encapsulated in a molding material, such as plastic or ceramic.
[0012] As used herein, the term semiconductor device (and its variants) refers to any structure or device including a semiconductor substrate. For example, a semiconductor substrate (e.g., a wafer) on which a plurality of integrated circuit (IC) dies are formed is a semiconductor device. Individual dies or groups of dies that may be on or separated from a wafer are another example of a semiconductor device. In addition, one or more dies encapsulated in a molding material are yet another example of a semiconductor device. Thus, a semiconductor device may be present at any stage of the semiconductor manufacturing workflow, including the resulting packaged IC chip or system on chip (SoC).
[0013] Figure 1 2-1 is a flowchart describing an example method 100 that can be implemented in an overall semiconductor manufacturing workflow to perform die preparation. Fig.10 The cross-sectional view of FIG2- Fig.10 The cross-sectional views of illustrate example processing progressions for wafer preparation that may be used in a semiconductor manufacturing workflow to form a semiconductor device.
[0014] At 102, a back grinding tape is applied to one side (eg, the front or top side) of a semiconductor substrate (eg, a wafer). For example, Figure 2A and Figure 2BAn example of a semiconductor wafer 200 is shown, which includes first and second opposing side surfaces 202 and 204 and a sidewall 210 extending between the side surfaces. The first surface 202 is the bottom side (also referred to as the backside) of the wafer 200, and the second surface 204 is the top side (also referred to as the front side) of the wafer. The wafer 200 includes a plurality of semiconductor dies 206 distributed across the second surface 204. Each die 206 includes a circuit system formed therein at or near a surface of the second surface 204. Each die 206 is spaced apart from each other by a corresponding scribe lane (as shown at 208) extending longitudinally across the wafer 200. Therefore, the corresponding scribe lane 208 is located between adjacent dies 206.
[0015] exist Figure 2B In the example of , a tape 212 is shown applied to the second side (e.g., front side) surface 204 of the wafer 200. The tape 212 can be an ultraviolet (UV) curable grinding tape, which includes one or more layers of material having an adhesive layer (e.g., an ultraviolet (UV) curable adhesive) to temporarily bond to the front side surface 204 of the wafer 200 during subsequent grinding at 104. The tape 212 may include one or more adhesive layers that can be cured to increase adhesion to the surface 204, such as by applying energy (e.g., ultraviolet light and / or heat). While the tape 212 is attached to the surface 204, the grinding at 104 can be performed to thin the back side of the substrate.
[0016] For example, in Figure 2B After the tape 212 has been applied, as shown Figure 3 As shown, the wafer 200 is mounted on a stage 300. The stage 300 is movable (e.g., providing at least two degrees of freedom of motion) in at least two orthogonal directions parallel to the surface of the wafer 200. For example, the stage 300 is movable in five degrees of freedom, such as along three orthogonal axes and pitch and roll directions. Figure 3 Also shown is a surface grinder 302 having a grinding wheel 304, which is supported above the stage and is configured to thin the substrate by grinding and / or polishing. In an example, the grinding at 104 can be performed to remove less than 10% of the thickness of the substrate from the first side of the substrate, such as removing a surface oxide layer from the backside surface 202. Thus, the grinder removes a layer of the substrate from the first side surface to provide a thinned first surface, as shown at 202'.
[0017] At 106, the method includes performing laser cutting on the substrate. Figure 4 As shown, laser cutting (at 106 ) may be performed on wafer 200 by a laser system 400 that includes a laser module 402 configured to generate an infrared (IR) laser beam 404 to perform stealth laser cutting. Figure 4The example of FIG. 4 shows a wafer 200 in an enlarged cross-sectional view, wherein each die 206 includes a circuit system 409 formed therein at or near the surface 204. Each of the dies 206 including the circuit system 409 is separated from each other by a corresponding scribe line 208. The laser system 400 also includes an arrangement of optical devices, such as including one or more focusing lenses, as shown at 406. The laser module 402 includes a laser source configured to perform pulsed oscillation of laser light along an optical axis 408, while the lens 406 is adjusted (e.g., by a control system) to focus the light beam at a focal point located within the wafer 200 along the corresponding scribe line 208 (e.g., between multiple groups of adjacent dies 206).
[0018] During laser dicing at 106, wafer 200 can be supported by stage 410. The distance between lens 406 and the focal point within wafer 200 defines the focal length. For example, during each pass of a multi-pass stealth dicing process, the focal length can be set (via a control system) to a different distance. As used herein, a pass refers to a movement of the laser beam across wafer 200 along a beam scanning direction 412 within a corresponding scribe line 208, such as by linearly moving stage 410 under a pulsed laser beam while set to a given focal length. For example, the laser beam scanning direction is shown as 412 (e.g., with Figure 4 orthogonal to the page it is on).
[0019] As a further example, during each pass of the laser across the wafer 200, the focused beam 404 is provided with sufficient energy to induce a thermal shock at a localized damage zone at a focal point within the wafer 200. The damage zone can be a volume of substrate material (e.g., silicon), referred to herein as a modified region (also referred to as a silicon damage region). As the pulsed beam 404 scans across the wafer 200, a plurality of adjacent modified regions are formed at a given depth (e.g., depending on the focal length and pulse rate of the beam scan) to provide a corresponding modified layer (e.g., a stealth cut layer) within the wafer along the length of the scribe line 208. Figure 4 In the example of , two separate modified regions 414 and 416 are shown, each of which can be considered as representative of a corresponding modified layer embedded within the wafer 200 during a given pass of the laser beam focused at a different depth along the scribe line 208. That is, each of the modified regions 414 and 416 is formed by generating a beam during a corresponding pass in which the focus of the laser beam is located at or near the center of each region. For example, the modified region 414 is spaced a greater distance from the surface 202' than the modified region 416. Although the modified regions 414 and 416 are schematically shown as having a circular or elliptical shape, the modified regions typically have more unstructured shapes depending on the crystal structure and the interaction between the beam 404 and the substrate material.
[0020] A modified region 414 further from the surface 202' is produced by a first pass of the laser beam 404 and is embedded within a thickness of the wafer 200 to form an embedded crack line 418 extending from the modified region 414 to the second side surface 204. Another modified region 416 can be formed during the first pass (e.g., by changing the focal length) or during a second pass of the laser beam 404, wherein the focus of the laser beam is offset from the first pass focus in a direction orthogonal to the modified region 414 toward the surface 202'. The energy of the laser during each pass can be set according to, for example, the type and configuration of the laser and the thickness of the wafer. The second pass of the laser produces a second crack line 420, which, for example, extends vertically and connects the modified regions 414 and 416 and is shallower (e.g., closer to the surface 202') than the embedded crack line 418. The second crack line 420 can be formed as an extension of the crack portion formed in response to forming the modified region 414. A third crack line 422 can also extend from the modified region 416 toward the surface 202' and intersect the surface 202' in some examples.
[0021] Reference Figure 1 After laser dicing at 106, the method proceeds to 108 where the back grinding tape (applied at 102) is removed. For example, the tape may be stripped from surface 204, such as manually or by an automated stripping process. At 110, the die on the substrate are tested. For example, Figure 5Schematically shown, the laser cut wafer (e.g., without the presence of a tape) is transferred to a wafer test system 500. The wafer test system 500 may include a chuck 502 configured to support a wafer 200 (e.g., a device under test) during testing, and the wafer test system 500 may also include automatic test equipment (e.g., a tester) 504 and one or more probe cards 506. The wafer test system 500 may also include a motion system (not shown), such as a combination of any of a mechanical actuator, a robotic arm, or the like, configured to control the relative position of the chuck 502 and / or the probe card 506 in two or three-dimensional space. For example, each probe card 506 includes one or more probe heads having an arrangement of needles (e.g., also referred to as pins) 508 extending outwardly from the probe head toward the surface 204 of the wafer 200. The probe card 506 may be coupled to the test equipment 504, which is configured to control the testing of the wafer 200 supported by the chuck 502. The needles 508 may be configured to test one or more dies simultaneously. For example, the needles can be arranged in a two-dimensional array and configured to contact corresponding conductive pads (e.g., copper, aluminum, or other conductive material) exposed along the surface 204 of the wafer 200 at the test location of each of the corresponding tube cores. The conductive pads can be coupled to (e.g., via electrical connections through the metallization structure of the wafer 200) the test circuit system on the die. In some examples, because the probe card and associated needles 508 can be "fanned out" across multiple tube cores, multiple tube cores can be tested in a single touch event. Because the electrical testing of the IC devices in the wafer is performed after laser cutting and through the full thickness of the wafer (e.g., a small amount of material is removed by pre-grinding at 104), the testing can help ensure high-quality robustness and prevent low-level laser scatter or spatter defects that may result from laser cutting at 106.
[0022] After the testing has been completed, the method proceeds to 112 where a back grinding tape is applied to the front side surface of the substrate. Figure 6 As shown, a UV curable back grinding tape 600 is applied to the front side surface 204. At 114, the method includes thinning (e.g., back grinding) the back side of the substrate to separate the dies. Figure 6 After the tape 600 has been applied to the front surface 204, as shown Fig. 7A As shown, the wafer 200 is mounted on a stage 700. The stage 700 may be movable in two or more orthogonal directions parallel to the surface of the wafer 200 (eg, providing five degrees of freedom of movement). Fig. 7AAlso shown is a surface grinder 702 having a rotating grinding wheel 704, which is supported above the stage 700 and is configured to thin the substrate by grinding and / or polishing. The grinder 702 can be the same or a different grinder than the grinder 302 used for pre-grinding at 104. Thus, at 114, the grinder 702 is configured to remove a portion of the substrate by grinding the first side surface 202' to a depth sufficient to separate the dies from each other along the corresponding scribe lanes. For example, the grinding platform is configured to control grinding into a modified region 416 (e.g., a silicon damage (SD) layer) deeper into the substrate (e.g., silicon) than prior methods. The grinding height and other grinding parameters can also be controlled to form an additional layer 706 on the back side of each die of the wafer (e.g., see Fig.10 Layer 1016 of the die in the die. Layer 706 may provide a standoff gap between surface 202" and corresponding modified region 416. Due to the thinning at 114, wafer 220 is provided with a further thinned first surface. Figure 7B and Figure 7C Shown as 202". Figure 7C The semiconductor wafer is shown after back grinding has been performed at 114. In an example, the grinding at 104 performed at 114 removes at least 50% (e.g., up to approximately 90%) of the thickness of the substrate from the back side of the wafer 200 (e.g., the back side 202' previously thinned at 104). For example, the grinder 702 is configured to perform back grinding so that the resulting surface 202" extends through the modified region 416, such as Figure 7B Reference Figure 4 and Figure 7B For example, back grinding removes a portion of the semiconductor substrate including a crack 422 in the semiconductor substrate extending between the back side 202' and the modified region 416. Back grinding can also partially thin down to the modified region 416 to provide a further thinned surface 202", such as Figure 7B and Figure 7C shown.
[0023] Reference Figure 1 At 116, the method includes applying a dicing tape to the back side of the substrate thinned at 114. For example, Figure 8 As shown, dicing tape 800 is applied to backside 202" opposite back grinding tape 600. For example, dicing tape 800 is an integrated tape structure having a backing layer (such as can be made of polyvinyl chloride (PVC), polyolefin or polyethylene backing material) and an adhesive to hold the wafer 200 in place during unwinding. After the dicing tape is applied, the back grinding tape can be removed from the front side surface 204 at 118, and the dicing tape will hold the singulated dies in place, such as Fig. 9At 120, the substrate is expanded so that the dies are further spaced apart from each other by a distance (eg, a known distance). Fig. 9 Schematically shown, as substrate 200 is uniformly spread in orthogonal directions (e.g., including as shown by arrow 900 and another direction orthogonal to arrow 900 and the surface of the drawing page, which is not shown), dicing tape 800 holds the separated dies in place. Thus, the direction of spreading is parallel to the backside surface and orthogonal to the direction of the corresponding scribe lanes, such as to space the corresponding dies along the scribe lanes by a desired die-to-die spacing. Spreading is facilitated at 120 because the dies have been separated from each other along the corresponding scribe lanes by back grinding at 114. The separated dies can remain on the dicing tape and be picked up (e.g., by a pick and place device) for further processing.
[0024] In an example, further processing may include picking up a corresponding die that may be picked up from the dicing tape 800 and physically attaching the die to the lead frame using a die attach material (e.g., epoxy attach, eutectic solder attach, or glass frit attach). In some examples, wire bonding may be used to connect the leads on the surface of the die to the corresponding terminals of the lead frame. The resulting die assembly may be packaged (e.g., encapsulated) in a molding material. The molding material may be any suitable IC chip packaging material, such as a plastic material or a ceramic material, thereby providing a packaged semiconductor device. Figure 1 The method can be used to produce devices according to almost any packaging technology, including wafer chip scale packaging, chip scale packaging or other packaging types.
[0025] Fig.10 is a side view showing the sidewalls of singulated die 1000, such as by Figure 1 The singulated tube die 1000 produced by the method. Fig.10 As shown, the sidewalls of the die have different surface textures, which is a result of using back grinding to separate the die as described herein. Fig.10 , the die has a front side surface layer 1002 that extends from the front side surface 1004 to a depth into the die 1000. Layer 1002 may contain some or all of the IC formed on the die. The next layer 1006 shows a surface in which a crack has been formed, extending from layer 1002 to a silicon damage (SD) layer 1008, toward surface 1004. SD layer 1008 exhibits a rough texture, such as in the form of ribs or other features extending longitudinally in a direction between adjacent layers 1006 and 1008. The texture shown in layer 1008 represents the roughness of the surface during laser cutting (e.g., Figure 1During invisible laser cutting at 106 in FIG. 1 , a laser beam is focused within the scribe lane to form SD layer 1008. For example, a corresponding ribbed texture can be formed by corresponding pulses of the laser beam, which are generated as the beam moves in a direction parallel to the longitudinal direction of the scribe lane of the wafer (as shown in 1010). Layer 1012 represents a portion of the die sidewall surface, where another crack is formed in the scribe lane extending from SD layer 1008 to another SD layer 1014. Fig.10 In the example of , SD layer 1014 exhibits a rough ribbed texture like layer 1008, however, layer 1014 is wider than layer 1008 (e.g., in a direction orthogonal to surfaces 1004 and 1018 of die 1000), such as due to providing a laser beam having a greater power focused within the region of layer 1014 than the laser beam used to form layer 1008. Backside layer 1016 (e.g., Figure 7B and Figure 7C 1000) extends between the SD layer 1014 and the backside surface 1018 of the die 1000. Thus, the backside layer 1016 provides a gap (e.g., a silicon-standoff gap) between the SD layer 1014 and the surface 1018. For example, during grinding (e.g., back grinding at 114), the backside layer 1016 is separated as the grinding force extends cracks from the SD layer 1014. For example, during back grinding at 114, the grinding height can be controlled to form the layer 1016 on the backside of the die 1000.
[0026] In this specification, the term "coupled" may encompass connections, communications, or signal paths that can achieve a functional relationship consistent with this specification. For example, if device A generates a signal to control device B to perform an action, then: (a) in the first example, device A is coupled to device B through a direct connection; or (b) in the second example, if the intervening component C does not change the functional relationship between device A and device B, device A is coupled to device B via the intervening component C, so that device B is controlled by device A via the control signal generated by device A.
[0027] The recitation "based on" means "based at least in part on." Thus, if X is based on Y, then X may be a function of Y and any other factors.
[0028] Modifications to the described embodiments are possible, and other embodiments are possible, within the scope of the claims.
Claims
1. A method comprising: Thinning a first side of a semiconductor substrate, wherein a plurality of dies are formed on a second side of the substrate opposite the first side and separated from each other by scribe lanes of the substrate; directing a laser beam along a scribe street thereof at an entry point at the first side, wherein the laser beam is focused inside the substrate to form at least one modified region within the substrate at a location spaced apart from the first side, and at least one crack propagates from the modified region toward the first side; as well as The die on the substrate is electrically tested, wherein the die under test is located between modified regions of corresponding scribe lines of the substrate. 2 . The method of claim 1 , wherein the substrate has a thickness, and the thinning comprises back grinding to remove less than 10% of the thickness of the substrate from the first side of the substrate. 3 . The method of claim 1 , further comprising removing tape from the second side of the substrate after directing the laser beam and before testing the die.
4. The method of claim 1 , wherein the substrate has a thickness, the thinning is a first thinning prior to directing the laser beam, and the method further comprises: A second thinning is performed on the first side of the substrate to reduce the thickness of the substrate and separate the dies along the modified regions in the scribe lanes. The method of claim 4 , wherein the second thinning comprises back grinding to remove at least 50% of the thickness of the substrate.
6. The method of claim 5, wherein the back grinding removes a portion of the substrate sufficient to remove a crack in the substrate between the first side and the modified region.
7. The method according to claim 4, further comprising: applying a first tape to the second side of the substrate prior to the second thinning; as well as A second tape is applied to the first side of the substrate after the second thinning.
8. The method according to claim 7, further comprising: removing the first tape from the second side of the substrate; as well as The substrate is unrolled using the second tape so that the separated dies are spaced a distance from each other.
9. A semiconductor device comprising a die produced by the method according to claim 1, wherein: The tube core has a first surface on the first side, a second surface on the second side, and a corresponding sidewall surface extending between the first surface and the second surface, and a first surface area of the sidewall extending from the first surface to an intermediate position has a modified texture responsive to separation of adjacent tube cores by the modified area, and a second surface area extending from the intermediate position to the second surface has a different texture responsive to separation of adjacent tube cores by a crack.
10. A method comprising: directing a laser beam at an entry point at a first surface of a semiconductor substrate along a scribe street thereof, wherein the laser beam is focused inside the substrate to form at least one modified region in a corresponding layer of the substrate at a location spaced apart from the first surface, and at least one crack propagates from the modified region toward the first surface; removing the tape from a second surface of the substrate opposite the first surface, and A plurality of dies on the substrate are electrically tested, wherein the dies being tested are located between modified regions of corresponding scribe lines of the substrate.
11. The method of claim 10, further comprising thinning the substrate from the first surface to reduce a thickness of the substrate and separating the dies along the modified regions in the scribe lanes and providing a thinned first surface.
12. The method of claim 11, wherein the thinning comprises back grinding to remove at least 50% of the thickness of the substrate from the first surface.
13. The method of claim 12, wherein the backside grinding thins the substrate an amount sufficient to provide the thinned first surface in the modified region.
14. The method according to claim 11, further comprising: applying a first tape to said second surface of said substrate prior to said thinning; as well as A second tape is applied to the first surface of the substrate after the thinning.
15. The method according to claim 14, further comprising: removing the first tape from the second side of the substrate; as well as The substrate is unrolled using the second tape so that the separated dies are spaced a distance from each other.
16. A semiconductor device comprising a die produced by the method according to claim 11, wherein: The die has a first die surface on the first side, a second die surface on the second side, and respective sidewall surfaces extending between the first die surface and the second die surface, and A surface region of the sidewall extending from the first die surface has a modified texture responsive to separation of adjacent dies by the modified region.
17. The method of claim 10, wherein prior to directing the laser beam, the method comprises thinning the first side of the substrate.
18. The method of claim 17, wherein the substrate has a thickness, and the thinning comprises back grinding to remove less than 10% of the thickness of the substrate from the first side of the substrate.
19. A semiconductor device comprising: A semiconductor die comprising an integrated circuit in a semiconductor substrate, wherein the semiconductor die has a sidewall extending between a first surface and a second surface, a first surface region of the sidewall extending from the first surface to an intermediate position having a first texture, and a second surface region extending from the intermediate position to the second surface having a second texture smoother than the first texture.
20. The semiconductor device of claim 19, wherein the first texture is responsive to separation of the semiconductor die by a modified portion of the substrate, and the second texture is responsive to separation of the semiconductor die from an adjacent die by a crack.