Acoustic element and acoustic element integrated circuit

By arranging lateral convex portions with an inclined angle on the electrode base of the capacitive acoustic element, the voltage vibration between the electrodes is used to generate a capacitor, which solves the problem of limited output power in the existing technology and achieves higher output power of the acoustic element.

CN118743249APending Publication Date: 2024-10-01矽系半导体科技有限公司
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202380019812.8
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Priority Date
2022-02-04
Filing Date
2023-02-03
Publication Date
2024-10-01

AI Technical Summary

Technical Problem

The power output of existing capacitive acoustic components is limited when transmitting signals, and it is difficult to increase the output power without applying a large voltage.

Method used

A flat-shaped first electrode base and a second electrode base are used, and side protrusions with specific inclination angles are provided on them respectively. The electrode bases are vibrated by applying a voltage to generate a capacitor that depends on the electric force line between the side walls and increase the static electricity. able.

Benefits of technology

The transmission output power can be increased without applying large voltages, enhancing the performance of the acoustic components.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118743249A_ABST
    Figure CN118743249A_ABST
Patent Text Reader

Abstract

A second electrode base (11) facing the first electrode base, first electrode-side protrusions (12aq-1, 12aq, 12aq + 1,...) provided on the first electrode base and having a first stepped side wall inclined at 45 DEG or less with respect to the vibration direction, and second electrode-side protrusions (11ap-1, 11app, 11ap1 + 1,...) provided on the second electrode base and having a second stepped side wall inclined at 45 DEG or less with respect to the vibration direction and having a second stepped side wall inclined at 45 DEG or less with respect to the vibration direction, the first electrode-side protrusions (12aq-1, 12aq, 12aq + 1,...) being provided on the second electrode base and having a second stepped side wall inclined at 45 DEG or less with respect to the vibration direction. And a second stepped side wall that faces the first electrode-side convex part so as to at least partially intersect the first electrode-side convex part, and that is inclined at the same inclination angle as the first stepped side wall. A voltage applied between the first and second electrode bases causes the first or second electrode bases to vibrate in a vibration direction. At least a portion generates a capacitor by means of a power line between the first and second stepped sidewalls, and electrostatic energy in a vibration cavity between the first and second electrode bases increases.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to a capacitive acoustic element and an acoustic element integrated circuit composed of a plurality of such acoustic element arrays, and in particular to a structure of a transmitting acoustic element. Background Art

[0002] Recently, a capacitive acoustic element with a vibration cavity has been developed using micro-electromechanical system (MEMS) technology. This capacitive acoustic element is called a "capacitive micro-mechanical ultrasonic transducer" (cMUT). It has characteristics close to the acoustic impedance of the human body and is expected to be used in medical applications. The cMUT has a vibrating membrane that can vibrate through a vibration cavity that is decompressed to a near vacuum. When transmitting signals, a high voltage is required to vibrate the vibrating membrane. Currently, the high power output of the cMUT is limited.

[0003] In view of this situation, one of the inventors proposed a structure in which a plurality of protrusions protruding toward the vibration cavity are provided on the bottom surface of the vibration membrane provided below the upper electrode (vibration electrode), and further, holes are provided on the lower electrode (counter electrode) below the protrusions according to the arrangement of the protrusion pattern so that a large voltage can be applied (see FIGS. 14 and 15 of Patent Document 1). According to the invention described in Patent Document 1, even when the voltage applied to the upper and lower electrodes reaches a level where the lower surface of the vibration membrane contacts the lower insulating film covering the upper surface of the counter electrode, the protrusions can function as pillars to prevent the entire lower surface of the vibration membrane from contacting the lower insulating film covering the lower electrode, making it possible to apply a large voltage.

[0004] However, the invention described in Patent Document 1 aims to provide a structure and a manufacturing method for preventing contact between an upper electrode (vibration electrode) and a lower electrode (counter electrode) and making it difficult for charges to be injected into an insulating film without causing it to collapse even when the lower surface of the film contacts the lower electrode, thereby transmitting the charge. A technique for increasing the output power of an acoustic element without causing collapse is not considered.

[0005] Prior art documents

[0006] Patent Literature

[0007] Patent document 1: Patent publication number 2007-74263. Summary of the invention

[0008] Problems to be solved by the present invention

[0009] In view of the above problems, an object of the present invention is to provide an acoustic element capable of improving transmission output power without applying a large voltage, and an acoustic element integrated circuit composed of a plurality of such acoustic element arrays.

[0010] Solutions to the problem

[0011] In order to achieve the above-mentioned purpose, in a first aspect of the present invention, an acoustic element comprises: (a) a flat-plate-shaped first electrode base; (b) a flat-plate-shaped second electrode base parallel to and opposite to the first electrode base; (c) a first electrode side protrusion disposed on the first electrode base, wherein the first step side wall thereof is composed of a plane inclined at an angle of less than 45° to the vibration direction; and (d) a second electrode side protrusion disposed on the second electrode base, which is opposite to the first electrode side protrusion in a manner that at least a portion thereof crosses the first electrode side protrusion, and has a second step side wall composed of a plane inclined at the same inclination angle as the first step side wall. In the acoustic element according to the first aspect, by applying a voltage between the first electrode base and the second electrode base, the first electrode base or the second electrode base vibrates in the vibration direction, generating a capacitor that at least a portion of which depends on the electric field lines between the first step difference side wall and the second step difference side wall, and the electrostatic energy in the vibration cavity sandwiched by the first electrode base and the second electrode base increases.

[0012] The second aspect of the present invention relates to an acoustic element integrated circuit, including a plurality of units, each of which is distributed with a specific number of capacitive acoustic element units, arranged in a two-dimensional manner on the same curved surface. According to the acoustic element integrated circuit of the second aspect, each of the plurality of units distributed according to the specific number of units includes: (a) a first flat electrode base; (b) a second flat electrode base parallel to and opposite to the first electrode base; (c) a first electrode side protrusion arranged on the first electrode base, whose first step side wall is composed of a plane with an inclination angle within 45° to the vibration direction; (d) a second electrode side protrusion arranged on the second electrode base, which is opposite to the first electrode side protrusion in a manner that at least a portion crosses the first electrode side protrusion, and has a second step side wall composed of a plane inclined at the same inclination angle as the first step side wall. In each transmitting unit, the voltage applied between the first and second electrode bases causes the first or second electrode base to vibrate along the vibration direction. In the acoustic element integrated circuit of the second aspect of the present invention, in each transmitting unit, a capacitor is generated that at least partially depends on the electric line between the first differential side wall and the second differential side wall, and the electrostatic energy in the vibration cavity clamped by the first electrode base and the second electrode base is increased.

[0013] Effects of the Invention

[0014] According to the present invention, it is possible to provide an acoustic element capable of improving transmission output power without applying a large voltage, and an acoustic element integrated circuit composed of an array of a plurality of such acoustic elements. BRIEF DESCRIPTION OF THE DRAWINGS

[0015] Figure 1 : A plan view showing a schematic diagram of an acoustic element integrated circuit according to a first embodiment of the present invention.

[0016] Figure 2A :Indicates that Figure 1 A plan view of a schematic plan pattern of a basic unit consisting of an element array.

[0017] Figure 2B :express Figure 2A Schematic diagram of the cross-sectional structure viewed in the IIB-IIB direction.

[0018] Figure 2C : A cross-sectional schematic diagram showing the deflection shape of a stepped vibrating electrode in the vibration direction.

[0019] Figure 2D :express Figure 2C Schematic diagram of the cross-sectional topological structure of the crossed (nested) stepped vibration electrodes and stepped counter electrodes near the center.

[0020] Figure 2E : A schematic cross-sectional view illustrating the structure of the outer periphery of the vibration cavity of the acoustic element of the first embodiment.

[0021] Figure 3 : A diagram showing the transient response simulation results of the transmitted sound pressure when the same step voltage is applied to the acoustic element representing the basic concept compared with the acoustic element of the prior art.

[0022] Figure 4 : A diagram showing the simulation results of the amount of charge accumulation between the electrode base and the vibration electrode base when the same step applied voltage is input when comparing the acoustic element of the basic concept of the present invention with the acoustic element of the prior art.

[0023] Figure 5 :Indicates that the basic concept of acoustic elements is compared with the acoustic elements of the prior art, according to Figure 3 and Figure 4 As a result, the relationship between stored electrical energy and transmitted acoustic energy is obtained.

[0024] Fig. 6A : A cross-sectional view illustrating an example process of the acoustic element manufacturing method according to the first embodiment (Part 1).

[0025] Figure 6B : The method for manufacturing the acoustic element of the first embodiment is exemplarily described. Fig. 6A The process after the cross-sectional structure shown in , focuses on the cross-sectional structure of the periphery of the vibration cavity to be formed (Part 2) process cross-sectional diagram.

[0026] Figure 6C : A plan view illustrating the second embedding groove portion embedded in the opposing protrusion, as well as three corrosion medium channels (pipes), etc.

[0027] Fig.6D: The acoustic element manufacturing method according to the first embodiment is exemplarily described, and Figure 6B The cross-sectional structure corresponds to that of the process cross-sectional diagram, with the focus being on the cross-sectional structure of the periphery of the vibration cavity (Part 3).

[0028] Fig. 6E : A method for manufacturing an acoustic element according to a first embodiment (Part 4) is exemplarily described, and Fig.6D The process cross-sectional diagram corresponding to the cross-sectional structure.

[0029] Fig. 6F : A method for manufacturing an acoustic element according to a first embodiment is exemplarily described, and Fig. 6E The cross-sectional structure of (Part 5) corresponds to the process cross-sectional diagram.

[0030] Figure 6G : A plan view illustrating the process of mask matching the hole pattern used to form the cavity with the pipe end pattern.

[0031] Figure 6H : A method for manufacturing an acoustic element according to a first embodiment (Part 6) is exemplarily described, and Fig. 6F The process cross-sectional diagram corresponding to the cross-sectional structure.

[0032] Fig. 7A : Shows the first variant of the first embodiment, focusing on the plan view of the stepped counter electrode of the acoustic element.

[0033] Figure 7B : A plan view showing a schematic diagram of an acoustic element integrated circuit according to a first variation of the first embodiment.

[0034] Fig. 8A : Shows the second variant of the first embodiment, focusing on the plan view of the stepped counter electrode of the acoustic element.

[0035] Figure 8B : A schematic plan view of an acoustic element integrated circuit showing a second variation of the first embodiment.

[0036] Fig.9A : A plan view showing a third variation of the first embodiment focusing on a lattice-shaped stepped vibration electrode of an acoustic element.

[0037] Fig. 9B : A third variation of the first embodiment is shown with focus on a plan view of a stepped counter electrode of an acoustic element.

[0038] Fig.10 : A schematic plan view showing an acoustic element according to a second embodiment of the present invention.

[0039] Fig.11: A plan view of the stepped electrodes of the acoustic element of the second embodiment illustrating the three first, second and third pairs of electrode bases, with emphasis on the stepped electrodes.

[0040] Fig.12 :from Fig.11 Cross-sectional view taken along the XII-XII direction.

[0041] Fig.13 : A schematic diagram illustrating the acoustic element of the second embodiment, with emphasis on a schematic cross-sectional diagram of the structure on the outer periphery of the vibration chamber.

[0042] Fig.14A : A cross-sectional view illustrating an example process of the acoustic element manufacturing method according to the second embodiment (Part 1).

[0043] Fig. 14B According to the method of the acoustic element of the second embodiment, the method of Fig.14A Process flow manufacturing process cross-sectional diagram of the cross-sectional structure shown in .

[0044] Fig. 14C According to the method of the acoustic element of the second embodiment, the method of Fig. 14B Process flow manufacturing process cross-sectional diagram of the cross-sectional structure shown in .

[0045] Fig.14D According to the method of the acoustic element of the second embodiment, the method of Fig. 14C Process flow manufacturing process cross-sectional diagram of the cross-sectional structure shown in .

[0046] Fig.14E According to the second embodiment, a method for manufacturing an acoustic element is exemplarily described. Fig.14D Post-process cross-sectional view of the cross-sectional structure shown.

[0047] Fig.14F According to the method of the acoustic element of the second embodiment, the method of Fig.14E Process flow manufacturing process cross-sectional diagram of the cross-sectional structure shown in .

[0048] Figure 14G According to the method of the acoustic element of the second embodiment, the method of Fig.14F Process flow manufacturing process cross-sectional diagram of the cross-sectional structure shown in .

[0049] Fig.14H According to the method of the acoustic element of the second embodiment, the method of Figure 14G Cross-sectional diagram of the process flow manufacturing process of the cross-sectional structure shown.

[0050] Fig.14IAccording to the method of the acoustic element of the second embodiment, the method of Fig.14H Cross-sectional diagram of the process flow manufacturing process of the cross-sectional structure shown.

[0051] Fig.15A : A cross-sectional view illustrating an example process of a method for manufacturing an acoustic element according to a variant of the second embodiment (Part 1).

[0052] Fig. 15B : A method for manufacturing an acoustic element according to a variation of the second embodiment, exemplarily illustrating Fig.15A A post-process cross-sectional diagram of the cross-sectional structure shown in FIG.

[0053] Fig. 15C : A method for manufacturing an acoustic element according to a variation of the second embodiment, exemplarily illustrating Fig. 15B Post-process cross-sectional view of the cross-sectional structure shown.

[0054] Fig.15D : A method for manufacturing an acoustic element according to a variation of the second embodiment, exemplarily illustrating Fig. 15C Post-process cross-sectional view of the cross-sectional structure shown.

[0055] Fig.15E : A method for manufacturing an acoustic element according to a variation of the second embodiment, exemplarily illustrating Fig.15D Post-process cross-sectional view of the cross-sectional structure shown.

[0056] Fig.15F : A method for manufacturing an acoustic element according to a variation of the second embodiment exemplarily illustrates the method according to Fig.15E Process cross-sectional diagram of the cross-sectional structure shown in .

[0057] Figure 15G : A method for manufacturing an acoustic element according to a variation of the second embodiment, exemplarily illustrating Fig.15F Post-process cross-sectional view of the cross-sectional structure shown.

[0058] Fig.15H : A method of an acoustic element according to a variation of the second embodiment, exemplarily illustrating the method according to Figure 15G Process flow manufacturing process cross-sectional diagram of the cross-sectional structure shown in .

[0059] Fig.15I : The method of the acoustic element according to the variation of the second embodiment exemplarily illustrates the method according to Fig.15H Cross-sectional diagram of the process flow manufacturing process of the cross-sectional structure shown.

[0060] Fig.15J : A method of an acoustic element according to a variation of the second embodiment, exemplarily illustrating the method according to Fig.15I Process flow manufacturing process cross-sectional diagram of the cross-sectional structure shown in .

[0061] Fig.16 : A schematic cross-sectional view of the acoustic element of the third embodiment of the present invention, with emphasis on the structure on the outer periphery of the vibration cavity.

[0062] Fig.17A : A plan view of the bases of three first, second and third vibration electrodes, focusing on the stepped vibration electrodes of the acoustic element of the third embodiment.

[0063] Fig. 17B :from Fig.17A Cross-sectional view taken along the XVIIB-XVIIB direction.

[0064] Fig.18A : A cross-sectional view illustrating an example process of a method for manufacturing an acoustic element according to the third embodiment (Part 1).

[0065] Fig.18B According to the third embodiment of the acoustic element method, the method of Fig.18A Process flow manufacturing process cross-sectional diagram of the cross-sectional structure shown in .

[0066] Fig. 18C : The method of the acoustic element according to the third embodiment exemplarily illustrates the method according to Fig.18B Cross-sectional diagram of the process flow manufacturing process of the cross-sectional structure shown.

[0067] Fig.18D According to the third embodiment, a method for manufacturing an acoustic element is exemplarily described. Fig. 18C Post-process cross-sectional view of the cross-sectional structure shown.

[0068] Fig.18E According to the third embodiment of the acoustic element method, the method of Fig.18D Cross-sectional diagram of the process flow manufacturing process of the cross-sectional structure shown.

[0069] Fig.18F According to the third embodiment of the acoustic element method, the method of Fig.18E Cross-sectional diagram of the process flow manufacturing process of the cross-sectional structure shown.

[0070] Figure 18G According to the third embodiment of the acoustic element method, the method of Fig.18F Cross-sectional diagram of the process flow manufacturing process of the cross-sectional structure shown.

[0071] Fig.19 : Schematic cross-sectional views of the acoustic elements of the fourth and fifth embodiments, with emphasis on the structure on the outer peripheral side of the vibration cavity.

[0072] Fig. 20 : Illustrate the rigidity reinforcement effect of the acoustic element in other embodiments.

[0073] Fig.21 : A plan view illustrating a six-segment vibrating electrode base of an acoustic element in other embodiments.

[0074] Fig. 22 : Characteristic schematic cross-sectional view of an acoustic element illustrating the basic concepts of the present invention.

[0075] Fig.23 : As a comparative example of the basic concept acoustic element description, a schematic cross-sectional diagram illustrating the direction of electric field lines and electric field flux when a small dielectric constant insulator is used as a protrusion.

[0076] Fig.24A : A conceptual cross-sectional diagram showing the direction of the electric field lines and electric field flux when the conductor is a convex part to illustrate the basic concept of an acoustic element.

[0077] Fig. 24B : A cross-sectional schematic diagram showing the direction of current flow when an insulator with a large dielectric constant is used as a convex part in an acoustic element of the basic concept as a conceptual diagram.

[0078] Fig.25 : A diagram showing the result of a simulation of the relationship between the distance d between electrodes and the transmitted peak sound pressure when a voltage V=180V is applied between the electrode and the vibration electrode.

[0079] Fig.26 : A diagram showing the result of simulating the relationship between the transmission peak sound pressure and the relative dielectric constant of the intersecting grooves when the applied voltage V=180V is applied between the electrode and the vibration electrode and the horizontal inter-electrode distance d is changed. DETAILED DESCRIPTION

[0080] Basic concept of invention

[0081] The first to sixth embodiments of the present invention will be described below, but before that, the basic concept of the present invention will be explained through approximate calculation simulation. When explaining the basic concept, we first consider Fig. 22 (a) shows a structure in which a stepped counter electrode 1a having vertical side walls faces a stepped vibration electrode 2a having vertical side walls and an inclination angle θ = 0°. Fig. 22 When the capacitance of the structure shown in (a) can be approximated as a constant with respect to the applied voltage V, the small signal model is considered. Fig. 22In the structure shown in (a), the conductor protrusion protruding upward from the stepped counter electrode 1a is defined as the "opposite side protrusion (second electrode side protrusion)", and the conductor protrusion protruding downward from the stepped vibration electrode 2a and nested (nested) and intersecting with the opposite side protrusion is defined as the "vibration side protrusion (first electrode side protrusion)".

[0082] exist Fig. 22 In (a), the horizontal direction (lateral direction) is the x-axis, and the width of the opposite-side convex portion of the stepped counter electrode 1a and the width of the vibration-side convex portion of the stepped vibration electrode 2a are x0. Fig. 22 In (a), the vertical (perpendicular) direction is the y-axis, and the width of the opposite side convex portion and the height of the vibration side convex portion are y o . And, if Fig. 22 As shown in (a), the vertical gap of the nested interlocking of the step-type counter electrode 1a and the step-type vibration electrode 2a is y0-y, and the horizontal (lateral) gap of the nested interlocking is d. In addition, it is assumed that the width of the counter-side convex portion and the vibration convex portion extends in the direction perpendicular to the paper surface (z direction), and the total length is L. Fig. 22 In (a), the dielectric constant of the medium (air) between the opposite convex portion and the vibrating convex portion is ε. The capacitance per unit length (C / εL) normalized by the dielectric constant ε of the opposite convex portion as a conductor and the pair of vibrating convex portions as a conductor can be approximately expressed by formula (1) if the disorder of the electric lines at the end of the convex portion is ignored.

[0083] [Number 1]

[0084]

[0085] Here, the electric energy E of static electricity in the state where the step-type counter electrode 1 a and the step-type vibrating electrode 2 a are nested is considered. Fig. 22 The longitudinal gap shown in (a) is y0-y. The value depends on the voltage V applied between the step-type counter electrode 1a and the step-type vibration electrode 2a, so the capacitance C will also change. However, if the capacitance C between the step-type counter electrode 1a and the step-type vibration electrode 2a can be approximated to be constant when the voltage V is applied between the step-type counter electrode 1a and the step-type vibration electrode 2a, the electrostatic electric energy E can be approximated by integrating the voltage V while making the capacitance C constant. If the capacitance C is linearly proportional to the voltage V, from the formula (2a), the form of the electric energy E depends on V. 3 On the other hand, if equation (1) is considered, under the condition that equation (2a) is approximately true, the electrostatic energy E stored in the opposite side convex portion of the step counter electrode 1a and the vibrating convex portion of the step vibrating electrode 2a is approximately given by equation (2b).

[0086] [Number 2]

[0087]

[0088] That is, in Fig. 22 In the structure shown in A, a voltage V is applied between the step-type counter electrode 1a and the step-type vibration electrode 2a, and the electrostatic electric energy E accumulated between the width of the counter-side convex portion and the pair of vibration-side convex portions of the step-type vibration electrode 2a is approximately expressed by equation (2b). When the electric energy E is accumulated, the force F acting between the counter-side convex portion and the pair of vibration-side convex portions can be approximately expressed by equation (3) by differentiating equation (2b) with the longitudinal displacement y.

[0089] [Number 3]

[0090]

[0091] Therefore, the pressure P per unit area defined by the width (x0+d) between a pair of opposing vibration convexities can be approximately calculated by formula (4).

[0092] [Number 4]

[0093]

[0094] Under the condition that it can be assumed that when a voltage V is applied between the step-type counter electrode 1a and the step-type vibration electrode 2a, the capacitance C between them does not change (independent variable), when the voltage V changes by ΔV, if the pressure P at the convex point per unit area defined by the width (x0+d) between the counter-side convex portion and the vibration-side convex portion changes by ΔP, then equation (4) can be expressed as equation (5), and thus the pressure change ΔP is approximated by equation (6).

[0095] [Number 5]

[0096]

[0097] It should be noted that formulas (5) and (6) are approximate values ​​and are valid only when the value of y0-y is independent of the voltage V applied between the step-type counter electrode 1a and the step-type vibration electrode 2a. In the signal model, formula (6) shows that the transmission sensitivity ξ(d, y0-y) is a function of the longitudinal gap y0-y and the transverse gap d between the step-type counter electrode 1a and the step-type vibration electrode 2a. Therefore, the transmission sensitivity ξ(d, y0-y) is a function that increases almost monotonically as the longitudinal gap y0-y decreases. In addition, formula (6) shows that the transmission sensitivity ξ(d, y0-y) is a function that also increases approximately monotonically with respect to the decrease in the transverse gap d. For example, when a voltage V=100V is applied between the step-type counter electrode 1a and the step-type vibration electrode 2a, the vibration side protrusion width x0=50nm, and the longitudinal gap y0-y=100nm between the step-type counter electrode 1a and the step-type vibration electrode 2a, when the lateral gap d=50nm, the transmission sensitivity ξ(d,y0-y)=221(kPa / V), and when the lateral gap d=20nm, the transmission sensitivity ξ(d,y0-y)=695(kPa / V).

[0098] Likewise, consider Fig. 22 (b) shows a case where the inclination angle θ≠0°, that is, a structure in which a stepped counter electrode 1b having a trapezoidal counter side protrusion with a specific inclination angle θ and a non-vertical side wall and a stepped vibration electrode 2b having a trapezoidal vibration side protrusion with an inclination angle θ face each other. Fig. 22 In the structure shown in (b), the conductor trapezoidal protrusion protruding upward from the stepped counter electrode 1b is defined as the "opposite side protrusion", and the conductor trapezoidal protrusion protruding downward from the stepped vibration electrode 2b and intersecting with the opposite side protrusion is defined as the "vibration side protrusion". Fig. 22 In (b), the dielectric constant of the dielectric (air) between the trapezoidal opposite side protrusion and the trapezoidal vibration side protrusion is ε. Fig. 22 In the model diagram shown in (b), an approximate study of the small signal model is also conducted, that is, the capacitance between the step-type counter electrode 1b and the step-type vibration electrode 2b can be approximated as a constant of the voltage V applied between the step-type counter electrode 1b and the step-type vibration electrode 2b. Fig. 22 The horizontal direction in (b) is the x-axis, and the width of the counter-side convex portion of the step-type counter electrode 1 b and the width of the vibration-side convex portion of the step-type vibration electrode 2 b are x0, respectively.

[0099] like Fig. 22 (a) Fig. 22 The longitudinal direction (vertical direction) of (b) is the y-axis, and the longitudinal gap between the step-type counter electrode 1b and the step-type vibration electrode 2b is y. Fig. 22As shown in (a), it is assumed that the width of the opposing convex portion and the vibration side convex portion extends in the direction perpendicular to the paper surface (z direction), and the total length is L. In this case, with a pair of trapezoidal opposing convex portions and a pair of trapezoidal vibration side convex portions as the center, the capacitance per unit length (C / εL) is normalized to the dielectric constant ε of the pair of opposing convex portions, which is approximated by formula (7).

[0100] [Number 6]

[0101]

[0102] The value of the longitudinal gap y between the step-type counter electrode 1b and the step-type vibration electrode 2b depends on the voltage V applied between the step-type counter electrode 1b and the step-type vibration electrode 2b. However, if the capacitance C between the step-type counter electrode 1b and the step-type vibration electrode 2b can be approximated as a constant when the voltage V is applied between the step-type counter electrode 1b and the step-type vibration electrode 2b, then the equation (8a) can be established by integrating the voltage V when the capacitance C remains unchanged. Therefore, under the condition that the equation (8a) can be approximately expressed, the electrostatic electric energy E stored in the opposite side convex portion of the step-type counter electrode 1b and the vibration side convex portion of the step-type vibration electrode 2b can be approximately expressed by the equation (8b).

[0103] [Number 7]

[0104]

[0105] When a voltage V is applied between the step-type counter electrode 1b and the step-type vibration electrode 2b, the width of the counter-side convex portion and the pair of vibration side convex portions of the step-type vibration electrode 2b are approximately expressed by formula (8b). When the electric energy E is stored, the force F acting between the counter-side convex portion and the pair of vibration side convex portions can be approximately expressed by formula (9) by differentiating formula (8b) through the longitudinal displacement y.

[0106] [Number 8]

[0107]

[0108] therefore, Fig. 22 The pressure P per unit area defined by the width (x0+x1) between the opposite-side convex portion and the vibration-side convex portion shown in (b) can be approximately expressed by formula (10).

[0109] [Number 9]

[0110]

[0111] If the voltage V applied between the stepped opposite side electrode 1b and the stepped vibration electrode 2b changes by ΔV, the pressure P within the unit area defined by the width (x0+x1) between the opposite side protrusion and the vibration side protrusion changes by ΔP, then formula (10) can be expressed as formula (11), and therefore the pressure change ΔP can be approximately expressed by formula (12).

[0112] [Number 10]

[0113]

[0114] It should be noted that formulas (11), (12a) and (12b) are approximate values ​​and are valid only when the value of the longitudinal gap y between the step-type counter electrode 1b and the step-type vibration electrode 2b is an independent variable of the voltage V applied between the step-type counter electrode 1b and the step-type vibration electrode 2b. In the small signal model, the value of y is independent of the voltage V. Formulas (12a) and (12b) show that the transmission sensitivity η(θ, y) is a function of the tilt angle θ and the longitudinal gap y between the step-type counter electrode 1b and the step-type vibration electrode 2b. Therefore, as the longitudinal gap y increases, η(θ, y) is a monotonically decreasing function. For example, if x0<<x 01 , and the tilt angle θ = π / 6, the transmission sensitivity η(θ, y) can be increased four times.

[0115] The second term in the numerator on the right side of formula (12a) is x / sin 2 The value of θ, where h is the height of the trapezoidal protrusion on the opposite side of the step electrode 1b, can be expressed as:

[0116] x1 / sin 2 θ=h / sinθcosθ=2h / sin2θ……(13)

[0117] Therefore, it can be seen that the smaller the inclination angle θ of the first and second step sidewalls, the larger the transmission sensitivity η(θ, y) in formula (12b), which is preferred. However, it can be seen from formula (7) that θ = 0° corresponds to Fig. 22 In the case of x1=0 in (b), and the step-type counter electrode 1b and the step-type vibration electrode 2b are in contact, the transmission sensitivity η(θ, y) in formulas (12a) and (12b) is not within the approximate formula range. When θ=0°, the approximate formula shown in the transmission sensitivity ξ(d, y0-y) of formula (6) can be used. sin2θ=1, that is, θ=45°, and the value in formula (13) is the minimum value.

[0118] Figure 2E The acoustic element of the first embodiment of the present invention is shown in FIG. Fig. 22The structure corresponding to the case (a) is that both the opposite side convex portion of the step type counter electrode 1a and the vibration side convex portion of the step type vibration electrode 2a are conductive. That is, a longitudinal capacitor C is formed between the concave portion of the step type counter electrode 1a and the first vibration side convex portion 12a1 of the conductive body. udv1 , the concave portion of the step-type vibration electrode 2a and the step side wall 11a0 of the conductor and the concave portion of the step-type vibration electrode 2a and the first pair of side convex portions 11a of the conductor 11 The longitudinal capacitors C udv1 In addition, a lateral capacitor C is formed in the horizontal direction between the first vibration side convex portion 12a1 of the conductor and the first vibration side convex portion 12a1 of the conductor. udh , between the first vibration side convex portion 12a1 of the conductor and the first pair of side convex portions 11a of the conductor 11 The horizontal direction forms a lateral capacitor C udh . The lateral capacitor C udh This means that the electric force lines extend in the horizontal direction.

[0119] Relative to Figure 2E , Fig.23 The vibration side convex portion 12c is formed of a solid dielectric having a relative dielectric constant ε1 (≒ε2). ij Here, relative to the vibration side convex portion 12c ij The relative dielectric constant ε1 will exist between the step electrode 1a and the vibration side convex portion 12c ij The relative dielectric constant of the vacuum or gas dielectric in the intersection space is set to ε2. That is, Fig.23 The vibration side convex part 12c of the dielectric material with a relative dielectric constant ε2=1 and a small relative dielectric constant ε1 is inserted into the concave part (intersecting groove) of the step-type opposite side electrode 1a of the conductor. ij The structure of the comparative example ( Fig.26 Indicated in the relative dielectric constant ε r = 1). Fig.23 In the comparative example shown, Fig. 22 The step-type vibration electrode 2a of (a) is composed of a vibration electrode base 12 of a conductor and a vibration side convex portion 12c of a dielectric material mounted on the vibration electrode base 12. ij In the case of a composite structure replacement, the dashed line indicates the electric flux D = ε when a voltage is applied between the vibrating electrode base 12 and the stepped counter electrode 1a. E . Fig.23 The step-type counter-side electrode 1a shown on the lower side of the comparative example is Fig. 22 A is also made of a conductor. ijThe relative dielectric constant ε1 will exist between the step-type opposite electrode 1a and the vibration side convex portion 12c ij The relative dielectric constant of the vacuum or gas dielectric in the intersection space is set to ε2, and the electric flux when ε1≒ε2 is schematically represented. That is, Fig.23 The vibrating side convex part 12c of the dielectric with a relatively small dielectric constant ε1 is inserted into the concave part (intersecting groove) of the step-type opposite side electrode 1a of the conductor. ij If the intersecting groove with a relative dielectric constant ε2 and the vibration side convex portion 12c with a relative dielectric constant ε1 ij The normal direction of the boundary surface is set to θ2, and the angle formed by the electric flux on the cross groove side is set to θ2, and the vibration side convex part 12c ij The angle formed by the electric flux on the side is set to θ1, then according to the law of refraction (Snell's law), the relationship tanθ1 / tanθ2=ε1 / ε2 holds. The law of refraction is derived from the continuous condition, in which the component in the normal direction of the interface of the electric flux D is continuous, and the component in the direction parallel to the interface of the electric field E is continuous. Therefore, if Fig. 24B As shown in FIG. 1 , when ε2<ε1, the vibration side convex portion 12c ij The angle θ1 formed by the electric flux inside the side gradually increases and moves away from the normal direction.

[0120] and Fig. 22 The situation shown in (a) is different. Fig. 22 The convex portion including the intersecting groove in (a) is formed of a conductive material, while Fig.23 In the comparative example shown in FIG. , the vibration side convex portion 12c ij The convex portion is formed of a solid dielectric, which allows the electric flux to pass from the convex side wall of the step-type counter electrode 1a through the vibration side convex portion 12c ij The vibration side convex part 12c ij The internal electric flux will cause the vibrating side convex part 12c ij A force is generated inside, but no force is generated between the vibrating electrode base 12 and the stepped counter electrode 1a. The force between the vibrating electrode base 12 and the stepped counter electrode 1a is guided by the electric flux in the gap, which is composed of a gas or vacuum dielectric having a relative dielectric constant ε2. Fig.23 The figure shows a comparative example of electric flux when ε1 ≒ ε2. The longitudinal capacitance C between the conductor vibration electrode base 12 and the top of the protrusion of the step counter electrode 1a is shown. udv1 The concave portion of the step counter electrode 1a and the conductor vibration electrode base 12 are connected by the vibration side convex portion 12c. ij The longitudinal capacitance C udv2 constitute the main capacitor.

[0121] However, even in Fig.23In the comparative example where ε1 ≒ ε2, it can also be observed that the electric flux flows from the side wall of the convex portion of the step counter electrode 1a through the vibration side convex portion 12c. ij Reaching the base 12 of the vibration electrode. Compared with the comparative example, in the case of ε2<<ε1 as the object of the present invention, the vibration side convex portion 12c ij The electric field in the vibrating side convex part 12c is only weakened by ε1 / ε2. ij The equipotential lines in the vertical direction are elongated and sparse. ij When the equipotential lines in the inner part become sparse, the distribution profile of the equipotential lines will be deformed, and the convex part side wall of the step counter electrode 1a will pass through the vibration side convex part 12c. ij The electric flux reaching the vibrating electrode base 12 increases. In addition, under the conditions that the normal direction of the electric flux D is continuous and the parallel direction of the electric field E is continuous, the electric flux D passes through the vibrating side protrusion 12c from the side wall of the protrusion of the step-type counter electrode 1a. ij The slope of the electric flux between the gaps of the dielectric constant ε2 of the electric flux reaching the vibrating electrode base 12 becomes close to horizontal, and is almost equal to the slope when the convex portion is formed of a conductive material.

[0122] and Fig.23 Compared with the comparative example shown, Fig.24A This is a conceptual representation of the distribution of electric lines when a conductor is used as a convex portion. Since the electric lines are in the normal direction of the conductor surface, Fig.24A In the figure, it can be seen that the vibration side convex portion 12c ij The vertical side surface and the opposite side convex portion 11c ij On the other hand, the vertical sides of the Fig. 24B and Fig.23 Compared with the comparative example, the vibration side convex portion 12c is schematically shown. ij The electric flux distribution when the relative dielectric constant ε1 is set to a large dielectric with ε2<<ε1. Fig. 24B In addition to the vibration side convex portion 12c ij In addition, the electric flux distribution when the convex part of the stepped counter electrode 1a is set as a dielectric with a large relative dielectric constant ε1 of ε2<<ε1 and the convex parts of the solid dielectric provided on the two electrodes intersect is schematically shown. Since ε2<<ε1, it can be known from the law of refraction that Fig.23 Compared with the case shown in FIG. 1 , the angle θ1 formed by the electric flux inside the vibration side convex portion is tilted more. Fig. 24B As shown, the electrode side protrusion 11c ij (and Fig. 22 The definition is the same as that of the opposite side convex portion 11c, hereinafter referred to as "the opposite side conv ij ”) as a relay point, through the opposite side convex portion 11c ijThe internal electric flux passes through the opposite side convex part 11c ij The side surface near the intersection passes through the vibration side convex portion 12c ij The vibration side convex part 12c is ij The side wall near the front end side is used as a relay point, through the vibration side convex part 12c ij The internal electric flux passes through the vibration side convex part 12c ij The side surface near the intersection passes through the opposite side convex portion 11c ij The inside of the counter electrode base 12 (hereinafter, the counter electrode side convex portion 11c is provided) ij The plate electrode of the vibrating electrode base 12 is referred to as the "counter electrode base 11"). Therefore, the charges induced on the surfaces of the vibrating electrode base 12 and the counter electrode base 11 attract each other by Coulomb force. ij The internal electric flux guides the internal force to the vibration side convex part 12c ij The inside of the vibrating electrode base 12 does not guide the force between the vibrating electrode base 12 and the counter electrode base 11. Similarly, the counter convex portion 11c ij The internal electric flux flows to the opposite convex part 11c ij The internal force is guided inside, but the force between the vibration electrode base 12 and the counter electrode base 11 is not guided.

[0123] As can be seen from formula (3) and the like, the force F between the vibrating electrode base 12 and the counter electrode base 11 is obtained by differentiating the displacement y between the vibrating electrode base 12 and the counter electrode base 11 with respect to the electrostatic energy E accumulated by the electric flux existing in the gap with the relative dielectric constant ε2. The reason for the force F in formula (3) is that Fig. 24B The charges induced on the surfaces of the vibration electrode base 12 and the counter electrode base 11 are subjected to a force from the electric field between the vibration electrode base 12 and the counter electrode base 11. Fig.23 As in the comparative example of the case of ε1≒ε2, between the vibrating electrode base 12 of the conductor and the counter electrode base 11 of the conductor, the longitudinal capacitor C udv1 When a dielectric having a large relative permittivity ε1 where ε2<<ε1 is used, the vibration side convex portion 12c as the dielectric ij and the opposite convex portion 11c ij Inside, the absolute value of the electric field vector is only weakened by ε1 / ε2, and according to the law of refraction, the electric flux is inclined to the longitudinal direction. As a result, the vibration side convex part 12c ij and the opposite convex portion 11c ij The equipotential lines inside are stretched in the longitudinal direction and become sparse. ijThe internal equipotential lines pass through the gap formed by the dielectric of vacuum or gas with relative dielectric constant ε2 and the opposite side convex part 11c. ij The internal equipotential lines are continuous, and the distribution curve of the equipotential lines is deformed. Fig.25 It shows that as the horizontal distance d between electrodes decreases, the transmitted peak sound pressure increases approximately monotonically. Fig. 24B Although the equipotential lines are not shown, in the case where ε2<<ε1 and the vibration side convex portion 12c ij The vertical side surface and the opposite convex portion 11c ij When the horizontal gap d between the vertical sides is narrow, the inclination of the equipotential lines in the horizontal gap with the relative dielectric constant ε2 becomes a steep slope close to the vertical direction. Since the electric flux is in the normal direction of the equipotential lines, Fig. 24B As shown, at the vibration side convex portion 12c ij The vertical side surface and the opposite side convex portion 11c ij The vertical side surfaces of the vibrating side convex portion 12c generate nearly horizontal electric flux and electric lines of force. ij The opposite side convex portion 11c ij When the horizontal gap d between the vibration side protrusions 12c is narrow, ij The opposite side convex portion 11c ij A capacitor is formed between the two electrodes, which at least partly depends on the bending of the electric field lines. Fig. 24B The contour of the electric flux D = εE shown shows that even a perfect insulator becomes Fig.24A The contour of the electric flux is the same as that of the convex portion of the conductor shown.

[0124] Equations (3) and (9) illustrate the essence of electrical-mechanical energy conversion (electrical-mechanical coupling). Changes in the electrical system variable V are guided by changes in the electrical capacitance C, which is in response to changes in the distance of the mechanical system variable y. In other words, for the basic concept, the capacitance C is configured to change with changes in the distance y, which is the essence of the acoustic element. Fig. 22 (a) and 22(b) show examples of structures of acoustic elements related to the basic concept, in which the cross slots are formed by a conductor, but even if an insulator, a high dielectric, a ferroelectric, a semiconductor, or a semimetal is used to construct the cross slots, the capacitance C can change with the change of the distance y. Even if these high dielectrics, ferroelectrics, semiconductors, semimetals, etc. are insulators, their resistivity ρ can be approximated to be infinite, but if the dielectric constant ε is greater than 1, even if a similar Fig. 22 For the cross slots in (a) and (b), the capacitance C can also vary with the distance y. Fig.25The results of simulating the relationship between the horizontal inter-electrode distance d and the transmitted peak sound pressure when the applied voltage V=180V between the step-type opposite-side electrode 1a and the step-type vibration electrode 2a are shown. The simulation used the "Piezoelectric Fluctuation Analysis Software PZFlex" developed by Weidlinger Associates of the United States. In the simulation, a vibration electrode top protective film 56 composed of a silicon oxide film with a thickness of 5μm is arranged on the vibration electrode 2a, and the structure of the vibration side protrusions and the opposite-side protrusions arranged at a pitch of 400nm in a cavity with a width of 120μm measured in the horizontal direction is taken as the object. It is assumed that the vibration side protrusions and the opposite-side protrusions are composed of polysilicon with a relative dielectric constant εr=11.9. As Fig.25 As shown, it can be seen that the same tendency as that of equation (6) is shown, that is, when the horizontal inter-electrode distance d decreases, the transmission peak sound pressure increases approximately monotonically.

[0125] exist Fig.26 In the figure, the relationship between the peak sound pressure and the relative dielectric constant εr of the cross grooves is simulated by using the piezoelectric wave analysis soft cone PZFlex when the applied voltage V=180V is between the step-type counter electrode 1a and the step-type vibration electrode 2a. Fig.26 In the simulation, Fig.25 The same protective film 56 on the vibrating electrode, the same cavity width, and the same spacing structure are used as the object, but the horizontal distance between electrodes is changed as a parameter to d = 20nm, 30nm, and 40nm. Fig.23 In the case of relative dielectric constant εr=1 (comparative example), there is no effect, but Fig.26It means that when the relative dielectric constant εr increases, the peak sound pressure increases. Therefore, it can be seen that as a dielectric constituting the cross slot, a high dielectric constant material (hereinafter referred to as "high dielectric body") with a large relative dielectric constant εr is preferred for increasing the peak sound pressure. Relative dielectric constant εr = 3.8 to 4 for silicon oxide film (SiO2 film), relative dielectric constant εr = 7 for silicon nitride (Si3N4) film. The relative dielectric constant εr = 5 to 5.5 obtained by the three-layer stacked film of silicon oxide film / silicon nitride film (Si3N4 film) / silicon oxide film, i.e., ONO film, is about the same. In addition, as a dielectric having a large relative dielectric constant εr, for example, a strontium oxide (SrO) film having εr=6, an aluminum oxide (Al2O3) film having εr=8-9, a magnesium oxide (MgO) film having εr=10, an yttrium oxide (Y2O3) film having εr=16-17, a lanthanum oxide (La2O3) film having a relative dielectric constant εr=21 or so, a hafnium oxide (HfO2) film having εr=22-26, a zirconium oxide (ZrO2) film having εr=22-25, a tantalum oxide (Ta2O5) film having εr=25-27, a bismuth oxide (Bi2O3) film having εr=40, any single layer film or a composite film formed by stacking a plurality of these. However, according to Fig.26 When the horizontal distance between electrodes is d=30nm, the relative dielectric constant εr=16.2 indicates a separation in which the peak sound pressure is reduced, so it is necessary to pay attention to the use of Y2O3 film.

[0126] Alternatively, a dielectric may be a ternary compound such as a hafnium aluminate (HfAlOx) film having a relative dielectric constant εr of about 11 or a hafnium silicate (HfSixOy) having a relative dielectric constant εr of about 11. In other words, an oxide containing at least one of strontium (Sr), aluminum (Al), magnesium (Mg), yttrium (Y), hafnium (Hf), zirconium (Zr), tantalum (Ta), and bismuth (Bi) or silicon nitride containing these elements may be used as a "dielectric" constituting the cross-groove.

[0127] As the "ferroelectric" that constitutes the cross slot, strontium titanate (SrTiO3), magnesium titanate (MgTiO3), calcium titanate (CaTiO3), bismuth titanate (Bi4Ti3O 12 ), lead titanate (PbTiO3), lead zirconate (PbZrO3), barium strontium titanate (BaSrTiO3), strontium bismuth tantalate (SrBi2Ta2O9) and other perovskite oxides, lead titanate zirconate (PbZr x Ti 1-x Mixed crystals such as MgTiO3) can also be used. The relative dielectric constants εr of MgTiO3 and CaTiO3 are about 150 to 300, and the larger ones are "paraelectric dielectrics". Therefore, the dielectric constituting the cross groove can also be a paraelectric with a large relative dielectric constant εr.

[0128] Relative dielectric constant ε of silicon (Si) r = 11.2 to 11.9. In addition, the relative dielectric constant ε of germanium (Ge) r = about 16.2, the relative dielectric constant ε of gallium arsenide (GaAs) r = 12.9. Therefore, even if these semiconductors have semi-insulating properties with a resistivity ρ of 1 kΩ·cm or more, their relative dielectric constant ε r is also very large, so in the composition and Fig. 22 In the case of the same cross grooves as (a) and (b), the capacitance C can be changed with the change of distance y. In addition, if the resistivity ρ of these semiconductors is low, such as 1Ω·cm or less, it is also possible to construct a similar Fig. 22 (a) and 22(b) are used as conductors to achieve the change of capacitance C with distance y. Similarly, conductive dielectrics such as tin oxide (SnO2), tin oxide containing indium (In) (ITO), tin oxide containing zinc (Zn) (ZTO), tin oxide containing gallium (Ca) (GTO), and tin oxide containing aluminum (Al) (ATO) have similar Fig. 22 In the case of the intersecting grooves in (a) and (b), the capacitance C can be varied with the distance y. For example, it is reported that the dielectric constant ε of ITO at low frequencies is r = about 9, depending on the composition and manufacturing method. The "dielectric film" used in the following description refers to a film made of these high dielectrics, ferrodielectrics, normal dielectrics, semiconductors, etc.

[0129] (Sending capability simulation)

[0130] When the convex portion is formed of a solid dielectric that is almost a perfect insulator, the approximate analysis shown in formulas (1)-(13) is more difficult than when the convex portion is formed of a conductor. Therefore, quantitative research is required through numerical simulation. The simulation results of improving the transmission capability using the piezoelectric wave analysis software PZFlex are as follows: Figure 3-Figure 5 shown. Figure 3-Figure 5 The comparative object "acoustic element of the prior art" of the simulation shown has only Figure 2B The planar counter electrode base 11 and the vibrating electrode base 12 of the structure shown do not have the counter electrode protrusion 11a. p-1 , 11a p , 11a p+1 , ... and the vibration electrode protrusion 12a q-1 , 12a q , 12a q+1 , ... The structure of the convex part. Figure 3(a) Figure 3 (b) and Figure 4 For the acoustic element in the prior art shown by the middle dotted line, the distance between the electrode base 11 and the vibration electrode base 12, that is, the height of the vibration cavity 18 measured in the vertical direction (cavity height) in the initial state is 360nm, and the width of the vibration cavity measured in the horizontal direction (cavity width) is 120μm.

[0131] In addition, as the basic concept of the present invention, two acoustic elements with different initial crossover values ​​were prepared, whose convex parts of solid dielectrics are almost perfect insulators (ρ≈∞). Figure 2B As shown, Figure 3 (a) Figure 3 (b) and Figure 4 The acoustic element with mutually intersecting dielectric protrusions indicated by the dotted line in the figure has a vibration electrode base 12 which is flat when not vibrating and has a vibration side protrusion 12a in the vibration direction. q-1 , 12a q , 12a q+1 , ..., as a structure in which a solid dielectric protrusion is added having a first step side wall formed by a plane parallel to the vibration direction. On the other hand, in the plane parallel to the vibration electrode base 12, the side convex portion 11a p-1 , 11a p , 11a p+1 , ... are added as solid dielectric protrusions having second step side walls formed of planes parallel to the vibration direction. As described above, the vibration side convex portion 12a q-1 , 12a q , 12a q+1 , ... and the opposite side convex portion 11a p-1 , 11a p , 11a p+1 , ... is also composed of a solid dielectric that is almost a complete insulator (ρ≈∞), assuming that the vibration side convex portion 12a q-1 , 12a q , 12a q+1 , ... and the opposite side convex portion 11a p-1 , 11a p , 11a p+1 , ... are high resistivity polycrystalline silicon (polysilicon), and the relative dielectric constant of silicon is εr. The vibration cavity height (cavity height) measured in the vertical direction is set to 900nm, Figure 2B The width of the middle vibration cavity in the left-right direction is set to 120 μm, which is the same as the acoustic element in the prior art. Figure 3 (a) Figure 3 (b) and Figure 4 The dotted lines in the figure represent the opposite side convex portions 11a with a pitch of 400 nm in a cavity width of 120 μm.p-1 , 11a p , 11a p+1 , ... and the vibration side convex portion 12a q-1 , 12a q , 12a q+1 , ...Simulation results for a structure in which the structure is alternately arranged in a nested manner with a gap of 20 nm.

[0132] exist Figure 3 (a) Figure 3 (b) and Figure 4 In the acoustic element in which the dielectric protrusions indicated by the middle dotted line intersect each other, the perpendicular intersection (initial intersection) between the counter electrode base 11 and the vibration electrode base 12 is 50% in the initial state before the driving voltage is applied. Figure 5 The 50% initial intersection has the same meaning. However, we assume an ideal state in which the vibration electrode base 12 is uniformly displaced as a parallel plate. The 50% initial intersection means that in the cross-sectional structure showing the intersection state, the upper end of the counter electrode base 11 and the lower end of the vibration electrode base 12 intersect with each other as an initial setting with a protrusion amount of half of the protrusion part. In an acoustic element having an intersecting dielectric protrusion, the face-to-face area determined between the mutually meshing vibration side protrusion and the step side protrusion varies with the voltage applied between the vibration electrode base 12 and the counter electrode base 11.

[0133] Figure 3 (a) Figure 3 (b) and Figure 4 The acoustic element shown by the solid line in the middle is a case where the horizontal plane on the cross section of the upper end of the opposite-side convex portion is the same as the horizontal plane on the cross section of the lower end of the vibration-side convex portion. Figure 3 (a) Figure 3 (b) and Figure 4 The result of the target structure shown by the solid line in FIG. 1 is also an ideal case assuming that the vibrating electrode base 12 is uniformly displaced as a parallel plate. Figure 3-Figure 5 In the embodiment, the case where the electrode base 11 has the same horizontal plane in the cross section of the upper end of the opposite convex portion and the lower end of the vibration convex portion is defined as "no initial intersection". The cavity height in the case of 50% initial intersection shown by the dotted line is 900nm, while Figure 3 (a) Figure 3 (b) and Figure 4 The cavity height of the acoustic element without initial crossover shown by the solid line is 700nm. The cavity width is 120μm, the same as the acoustic element of the prior art and the acoustic element with an initial crossover rate of 50%. In addition, in the cavity width of 120μm, the spacing is 400nm, and the opposite side convex parts and the vibration side convex parts are alternately arranged in a nested manner with a gap of 20nm, which is the same as the case of 50% initial crossover.

[0134] like Figure 3(a) and Figure 3 As shown in the transient response waveform in (b), for the transient response characteristics of the transmitted sound pressure generated by the step input of the same applied voltage of 180V, namely the attenuated vibration (underbraking), it is shown that the acoustic element with mutually intersecting dielectric protrusions can obtain better results than the acoustic element of the prior art. Figure 3 The horizontal axis of (a) shows the time variation of the transient response. Figure 3 The left vertical axis of (a) shows the applied voltage of the step input. Figure 3 The right vertical axis of (a) shows the transmitted sound pressure generated by the step input. Figure 3 The dashed line in (a) shows the transient response waveform within 5μs of the applied voltage inputted in a step between the electrode base and the vibrating electrode base 12. The applied voltage rises at a predetermined time constant from 0μs, and at 2μs, the constant voltage is 180V. When the applied voltage of the step input drops to 0V at 5μs, as shown by the solid line, dotted line and dashed line, the three types of capacitive acoustic elements ring after the overshoot occurs at the vibrating electrode base 12, respectively, and produce attenuated vibration (insufficient braking). Similar to the RLC series resonant circuit in the known circuit, the "attenuated vibration" of these three acoustic elements is the exponential attenuation vibration of the envelope of the peak value (amplitude) of the sinusoidal vibration.

[0135] In a differentiable way, such as Figure 3 As shown by the single-dot line in (a), the falling waveform of the applied voltage is set to quickly change to 0 V with a time constant of 1 / 4 sine wave. Figure 3 (a) shows that even when an almost perfect insulator (ρ≈∞) is used as the dielectric, by creating a structure in which protrusions of the dielectric material intersect each other, the input applied voltage suddenly becomes 0 V, the vibration electrode base 12 attenuates the vibration, and the transient response waveform of the transmitted sound pressure generated after time 5 μs shows a different transmitted sound pressure according to the acoustic element of the prior art. Figure 3 (b) shows Figure 3 (a) is the enlarged time axis of the transient response waveform after 5μs. Figure 3 The left vertical axis in (b) shows the change in the transmitted sound pressure generated by the acoustic element.

[0136] It is well known from the transient response theory in the circuit that the natural angular frequency (ω0=2πf) of the sine wave showing the decaying oscillation in the RLC series resonant circuit depends on the capacitance C. In the capacitive acoustic element, the natural angular frequency of the sine wave showing the decaying oscillation also depends to some extent on the capacitance between the electrode base 11 and the vibrating electrode base 12. However, since the electromechanical coupling is very small, the effect of the capacitance on the natural angular frequency can be ignored. Therefore, in Figure 3 (a) and Figure 3In (b), the simulation was performed assuming that the frequency f of the conventional acoustic element shown by the dotted line and the acoustic element having two types of intersecting dielectric protrusions shown by the dotted line and the solid line are both f = 3 MHz (constant). Figure 3 (b) It can be seen that the attenuation vibration peak value of the sound pressure transmitted by the acoustic element without initial crossing shown by the solid line is greater than the attenuation vibration peak value of the sound pressure transmitted by the acoustic element with an initial crossing rate of 50% shown by the dotted line. This is because in actual operation, the change in the amount of crossing (crossing area) when there is no initial crossing is greater than the change when there is an initial crossing of 50%. In actual operation, the simulation condition is that the vibrating side convex part crosses at a depth of 2 / 3 of the opposite side convex part. Compared with the prior art acoustic element shown by the dotted line, the attenuation oscillation peak value of the propagation sound pressure of the acoustic element without initial crossing shown by the solid line means that even if an almost perfect insulator (ρ≈∞) is used as the dielectric, it is possible to simulate a situation where the transmitted sound pressure can be increased by nearly two times.

[0137] In addition, if Figure 4 As shown, in terms of the amount of charge accumulated between the counter electrode base and the vibration electrode base 12, for the same applied voltage of 180V, the acoustic element with the dielectric protrusion in two different cross modes has better simulation results than the acoustic element in the prior art. Figure 4 The horizontal axis represents the time variation of transient response. Figure 4 The left vertical axis represents the applied voltage of the step input, Figure 4 The right vertical axis of represents the amount of charge accumulated between the counter electrode base and the vibrating electrode base 12 by the step input. That is, similar to the simulation results of the transmitted sound pressure, the amount of charge accumulated in the dielectric protrusion acoustic element with no initial intersection is greater than the amount of charge accumulated in the dielectric protrusion acoustic element with an initial intersection of 50%. Compared with the dielectric protrusion acoustic element with no initial intersection shown by the solid line, the dielectric protrusion acoustic element with no initial intersection shown by the dotted line is more than 2.5 times larger than the acoustic element of the prior art, even when a nearly perfect insulator (ρ≈∞) is used as the medium. In addition, the amount of charge accumulated in the acoustic element with a dielectric protrusion of 50% of the initial intersection shown by the dotted line is more than twice that of the acoustic element of the prior art.

[0138] also, Figure 5 The horizontal axis represents the electric energy stored between the counter electrode base 11 and the vibrating electrode base 12. Figure 5 The vertical axis represents the transmitted sound energy. Figure 5 As shown, regarding the sending of sound wave energy, Figure 5 The acoustic wave element ratio with an initial crossover ratio of 50% shown on the right side of the middle row Figure 5 The prior art acoustic wave element shown at the bottom left stores more electrical energy, so the transmitted acoustic wave energy is greater even when using an almost perfect insulator (ρ≈∞) as the dielectric. Figure 5The acoustic element shown above right with no initial crossover Figure 5 Compared with the acoustic element with an initial crossover rate of 50% shown on the right side of the middle row, the relative area change between the side wall of the vibration side convex part and the side wall of the opposite side convex part is greater, resulting in greater stored electrical energy. Therefore, it can be confirmed through simulation that the acoustic element with no initial crossover rate also has greater transmitted sound energy than the acoustic element with an initial crossover rate of 50%.

[0139] Based on the above description of the basic concept of the present invention and the accompanying simulation diagrams, the present invention will now be exemplified by describing the 1st to 6th embodiments of the present invention. The 1st to 4th embodiments of the present invention will be mainly described when the opposite side protrusions and the vibration side protrusions are conductors. On the other hand, the 5th embodiment of the present invention is to illustrate the case where the opposite side protrusions and the vibration protrusions are almost perfect insulators (resistivity ρ≈∞), while the 6th embodiment mainly illustrates the case where the opposite side protrusions or the vibration protrusions are almost perfect insulators or equivalent to perfect insulators. However, it should be noted that, as explained in the basic concept of the present invention, the opposite side protrusions and the vibration protrusions can be conductors with low resistivity ρ, almost perfect insulators (ρ≈∞) or equivalent to perfect insulators.

[0140] In the following drawings, the same or similar parts are marked with the same or similar symbols. However, it should be noted that the drawings are schematic diagrams, and the relationship between thickness and plane dimensions, the size ratio of each component, etc. may be different from the actual situation. Therefore, the specific thickness, size, size, etc. should be combined with the purpose of the technical concept that can be understood from the following description to make a more diverse judgment. In addition, of course, there may be different size relationships and ratios between the drawings.

[0141] The first to sixth embodiments shown below are examples of the technical concept method of the present invention and the device used in the method, etc. The technical concept of the present invention does not make the following provisions on the materials, shapes, structures, arrangements, etc. of the constituent parts and the procedures of the method, etc. The technical concept of the present invention is not limited to the contents described in the first to sixth embodiments, and various changes can be made within the technical scope defined by the specific matters of the invention in the claims.

[0142] (First embodiment)

[0143] like Figure 1 As shown, in the acoustic element integrated circuit of the first embodiment of the present invention, in the element array portion, the regular hexagonal unit cell X (i-1),(j+1) , X i,(j+1) , X (i+1),(j+1) , …, X (i-1),j , X i,j , X (i+1),j , …, X (i-1),(j-1) , X i,(j-1) , X(i+1),(j-1) , ..., etc., are arranged on the same plane (same surface) to form a two-dimensional matrix. Figure 1 As shown, the unit array constituting the two-dimensional matrix defined on the same plane is distributed as a group of acoustic elements, each acoustic element has a unit number n (n is a positive integer greater than 1), and these acoustic elements with unit number n can be collectively driven by the driving circuits provided for each group of acoustic elements. That is, in the acoustic element integrated circuit of the first embodiment, a unit is composed of n acoustic elements, and a driving circuit is provided for each group of acoustic elements, and the n acoustic elements composed of a group of unit numbers can be uniformly driven by their respective driving circuits. However, for simplicity, the following description will take the case where the unit number n=1 as an example. In addition, as Figure 2A and Figure 2B As shown, in most cases described below, the unit cell X i,j It is centered on the image and represents multiple unit cells arranged in a two-dimensional matrix for comprehensive expression. Figure 2A and 2B The unit cell X shown in i,j It is a capacitive acoustic element having a new structure vibration cavity introduced in this specification, and its new structure is introduced here. Unit cell X i,j It is an acoustic element that transmits ultrasonic signals. Figure 2A and Figure 2B The multiple transmitting acoustic elements shown in the above are arranged in a Figure 1 In the matrix shown, a high power acoustic element integrated circuit is formed.

[0144] like Figure 2A As shown, the acoustic element of the first embodiment includes a plurality of vibration side protrusions (first electrode side protrusions) 12a. q-1 , 12a q , 12a q+1 , ..., these convex parts are composed of multiple wall-like conductors, forming a group of multiple concentric hexagonal rings in the cavity. The plane figure of the cavity is a regular hexagon with equidistant hexagonal rings on it. The convex parts have equally spaced gaps and are arranged at a certain distance. Figure 2B As shown, a plurality of vibration side convex portions 12a q-1 , 12a q , 12a q+1 Each of , ... has a first stepped side wall (vertical side wall) including a plane parallel to the vibration direction. Figure 2C and Figure 2D As shown, the "vibration direction" is a plurality of vibration side convex portions 12a. q-1 , 12a q , 12a q+1, ..., each side convexity in the convex portion 12a determines the direction of the maximum amplitude when it is bent like a bulge, thereby forming a downward convex surface. q-1 , 12a q , 12a q+1 , ..., in a manner sandwiched by the gaps between them, a wall-shaped opposing side protrusion (second electrode side protrusion) 11a composed of a plurality of conductors constituting another set of a plurality of concentric hexagonal rings p-1 , 11a p , 11a p+1 , ... have equally spaced gaps and are arranged at a certain pitch. Figure 2C and 2D As shown, a plurality of vibration side convex portions 12a q-1 , 12a q , 12a q+1 , ... and a plurality of wall-shaped opposite side protrusions 11a p-1 , 11a p , 11a p+1 , ...are constructed as a cross structure capable of cross-sectional structure.

[0145] like Figure 2B As shown in the cross-sectional view, a plurality of opposite side protrusions 11a p-1 , 11a p , 11a p+1 Each of the side protrusions in , ... also has a second step side wall (vertical side wall) composed of a plane parallel to the first step side wall. Figure 2C and Figure 2D In the cross-sectional structure shown, the first step sidewall and the second step sidewall face each other, forming a parallel plate capacitor, and positive and negative charges as true charges can be induced on their respective surfaces according to Gauss's law. However, Figure 2A This is a simplified schematic structure. For the convenience of explanation, the number of concentric hexagonal rings is reduced. As an actual structure, for example, Figure 2A In the regular hexagon whose opposite sides are 120 μm measured along the cross section IIB-IIB direction, for example, concentric hexagonal rings with a pitch of 400 nm and a width of about 180 nm can be used, with opposite side convex portions 11a p-1 , 11a p , 11a p+1 A structure with about 150 configurations of , ... is possible, but it cannot be seen if we draw about 150 concentric hexagonal rings in Figure 2a, so a sparse representation is used.

[0146] In the actual structure, for example, assuming that there are 151 opposite side protrusions 11a p-1 , 11a p , 11a p+1, ..., 150 concentric hexagonal rings with a width of 180 nm form the vibration side convex portion 12a q-1 , 12a q , 12a q+1 , ..., alternately arranged at a gap of 20nm, so that 150 concave-convex pairs can be formed. That is, the side convex portions can use the outermost pair of step side walls 11a0 as the side wall structure, and from the side wall structure to the inside, a plurality of first pair of side convex portions 11a1, second pair of side convex portions 11a2, ..., 149th pair of side convex portions 11a1 with a width of 180nm and a pitch of 400nm are arranged. 149 In this case, the 150th pair of convex portions 11a 150 As a hexagonal column located in a regular hexagonal unit cell X i,j The center of the vibration cavity. However, it is not always necessary to construct a plurality of concentric hexagonal rings with the same gap and spacing. By making the gap and spacing of the plurality of concentric hexagonal rings uneven, the frequency band of the acoustic element integrated circuit of the first embodiment can be widened. Therefore, when the frequency bandwidth is to be widened, the gap or spacing of the plurality of concentric hexagonal rings can be changed.

[0147] The first pair of side protrusions 11a1, the second pair of side protrusions 11a2, ..., the 150th pair of side protrusions 11a 150 Correspondingly, the vibration side convex parts with a width of 180 nm are headed by the outermost first vibration side convex part 12a1, the second vibration side convex part 12a2, the third vibration side convex part 12a3, ..., the 150th vibration side convex part 12a 150 The concentric hexagonal rings face each other in a manner that forms 150 concave and convex pairs. The 150th vibration side convex portion 12a 150 The 150th facing side protrusion 11a surrounds the hexagonal column disposed at the center of the vibration chamber from the outside. 150 Alternatively, the 150th pair of side protrusions 11a located at the center may be 150 The hexagonal column at the position is expanded to increase the diameter to the 150th vibration side convex part 12a 150 In this case, the 150th vibration side convex portion 12a relative to the electrode side convex portion 12a is 150 It is not a hexagonal ring, but a hexagonal column as an insulator vibrating electrode side protrusion, and the top of the opposite electrode side protrusion and the top of the vibrating electrode side protrusion can be configured to collide with each other, and at least one of the opposite electrode side protrusions or the vibrating electrode side protrusions should be made of insulating material. In other words, the top of the opposite electrode side protrusion and the top of the vibrating electrode side protrusion collide with each other to prevent the other first pair of electrode side protrusions 11a1 to the 149th pair of electrode side protrusions 11a 149and the other first vibration side convex portions 12a1 to the 149th vibration side convex portions 12a corresponding thereto respectively 149 The role of contact between.

[0148] In order to play the role of a baffle, the top height of the electrode side protrusion and the height of the vibration electrode side protrusion should be adjusted so that the first electrode side protrusion 11a1 to the 149th electrode side protrusion 11a 149 and the first vibration electrode side protrusion 12a1 to the 149th vibration electrode side protrusion 12a 149 The electrodes are nested to a depth sufficient to cross each other, so as to maximize the area facing each other. When the central electrode side protrusion and the vibration electrode side protrusion act as baffles, the first electrode side protrusion 11a1 to the 149th electrode side protrusion 11a 149 and the corresponding first vibration electrode side protrusion 12a1 to the 149th vibration electrode side protrusion 12a 149 149 concave-convex pairs composed of concentric hexagonal rings act as electrodes. If it is a pair, the gap between the first vibration side convex portion 12a1 surrounding the first pair of electrode side convex portions 11a1 as viewed from the outside, the gap between the second vibration side convex portion 12a2 surrounding the second pair of electrode side convex portions 11a2 as viewed from the outside, ... and the gap between the second vibration side convex portion 12a2 surrounding the 150th pair of electrode side convex portions 11a as viewed from the outside 150 The 150th vibration side convex portion 12a 150 Each gap is configured to be 20nm, with the vertical side walls facing each other alternately. The 150th vibration side convex part 12a 150 It can be configured as a hexagonal column, located in the center of the vibration cavity, with the innermost 150th electrode side protrusion 11a 150 Surrounding the 150th vibration-side convex portion 12a from the outside 150 , forming 150 concave-convex pairs.

[0149] exist Figure 1 , Figure 2A and Figure 6C etc., it is explained that the unit cell X x,j The plane pattern is a regular hexagon, but the unit cell X x,j The plane pattern is not limited to a regular hexagon. For example, various plane patterns including a regular octagon as shown in FIG7a, a regular dodecagon as shown in FIG8a, and a square and a regular pentagon in which the plane pattern is omitted can be used. However, since the harmonics of ultrasonic vibrations become more obvious, regular polygons with fewer angles than regular pentagons are not desirable except for modes that actively use harmonics.

[0150] Figure 2A The plurality of vibration side convex portions 12a shown in q-1 , 12a q , 12aq+1 , ... are respectively formed on a plate-shaped vibrating electrode base (first electrode base) 12 having a main surface that is flat when not vibrating (in Figure 2B The lower surface side of the vibration electrode base 12 in the representation is arranged in a suspended manner with a rectangular convex portion in cross section. q-1 , 12a q , 12a q+1 The cross-sectional shape of , ... is not limited to a rectangle, but may also be Fig. 22 (b) The angle between the hypotenuse of the trapezoid and the vibration direction should preferably be within 45°. When the inclination angle θ = 45°, sin2θ = 1 in equation (13) is the minimum value. That is, each vibration side convex portion 12a q-1 , 12a q , 12a q+1 , ..., the first step side wall presented is composed of a plane with an inclination angle θ within 45° relative to the vibration direction. This can be understood from formulas (12a), (12b) and (13), etc. The smaller the inclination angle θ, the better, preferably within 10°. Figure 2A As shown, it can be seen from equation (12a) etc. that a topological structure in which the tilt angle θ relative to the vibration direction is 0° is preferred. The vibration electrode base 12 is made of a conductive material such as metal.

[0151] Regarding the vibration side convex portion 12a q-1 , 12a q , 12a q+1 According to the first embodiment, any conductive material having a resistivity of about ρ = 3Ω·cm or less, whether dielectric or non-dielectric, can be used as the structure of the acoustic element. However, more generally, the vibration side convex portion can be a dielectric having a resistivity of ρ≈∞. The vibration side convex portion 12a q-1 , 12a q , 12a q+1 , ..., for example, metal, semimetal, semiconductor to which impurities as a conductor are added, oxide to which impurities as a conductor are added, etc., are used as one of the materials for the structure of the acoustic element according to the first embodiment. Fig.13 In the examples of the case where a semiconductor with low resistivity ρ is used and impurities are added, a material that is polarized when voltage is applied is called a "dielectric", so a semiconductor without impurities is a dielectric, and a semiconductor with impurities is also a dielectric. A perfect conductor can also be regarded as a dielectric, and its relative dielectric constant is ε r =∞. Therefore, by adding impurities to various semiconductor materials (dielectrics) and oxides, they can be made into conductors with low resistivity ρ, which can be used to vibrate the side convex portion 12a. q-1 , 12a q , 12a q+1, ... a polycrystalline semiconductor containing impurities, such as polycrystalline silicon, that is, doped polycrystalline silicon (DOPOS), can also be used for the vibration side protrusion 12a q-1 , 12a q , 12a q+1 , .... Usually, the metal part is called "electrode". In the present invention, for two opposite regions with different potentials constituting a capacitor, the part that induces positive charge and negative charge on the surface of the opposite regions, respectively, is also called "electrode" even if it is the surface of a dielectric, etc. Therefore, the component that forms the same potential convex region electrically connected to the vibration electrode base 12 and induces true charge (free charge) on its surface according to Gauss's law is also called "vibration side convex part" even if it is the surface of a dielectric, etc., and can be defined as a part of the "electrode".

[0152] Multiple vibration side convex parts 12a q-1 , 12a q , 12a q+1 , ...are the opposite side convex parts 11a p-1 , 11a p , 11a p+1 , ... The convex parts are arranged so as to be inserted into the inner space of the defined concave part. The vibration electrode base 12 and the vibration side convex part 12a suspended from the bottom of the vibration electrode base 12 q-1 , 12a q , 12a q+1 The overall structure of the vibrating electrode 12 is referred to as a "stepped vibrating electrode" herein. "Flat-shaped" means that the first main surface (upper surface) and the second main surface (lower surface) of the vibrating electrode base 12 are both flat and parallel to each other in a non-vibrating state. Figure 2C and 2D As shown in FIG. 1 , when vibrating (when voltage biased), the vibrating electrode base 12 bends like a bulge, thus forming a curved surface. Figure 2A The structure of multiple concentric hexagonal rings shown in Figure 2B The cross-sectional view of FIG. 1 is schematically shown as an array of multiple rectangles (rectangles). Figure 2B middle, Figure 2A The plurality of opposite side protrusions 11a shown in p-1 , 11a p , 11a p+1,..., each convex portion is arranged on the counter electrode base (second electrode base) 11, and the convex portion has a rectangular cross-section. In the acoustic element of the first embodiment, the vibrating electrode base 12 is referred to as the "first electrode base 12", and the counter electrode base 11 is referred to as the "second electrode base 11". In addition, the corresponding vibrating side convex portion is referred to as the "first electrode side convex portion", and the counter side convex portion is referred to as the "second electrode side convex portion", but this is just a name chosen for the convenience of explanation. It is also possible to choose to call the vibrating electrode base defined in the acoustic element of the first embodiment the "second electrode base", the counter electrode base the "first electrode base", the corresponding vibrating side convex portion the "second electrode side convex portion", and the counter side convex portion the "first electrode side convex portion".

[0153] In addition, if the vibration side convex portion 12a q-1 , 12a q , 12a q+1 , ..., the cross-sectional shape is a trapezoid, then the convex portion 11a on the opposite side p-1 , 11a p , 11a p+1 The cross-sectional shape of , ... can also be a trapezoid, similar to Fig. 22 (b) shows the structure. That is, the opposite side convex part 11a p-1 , 11a p , 11a p+1 The second step side wall of the first step is formed by an inclined plane with the same inclination angle θ as the first step side wall. Therefore, as shown in formulas (12a), (12b) and (13), the side convex portion 11a p-1 , 11a p , 11a p+1 ,... The angle between the trapezoidal hypotenuse and the vibration direction should also be within 45°, but the inclination angle θ should be smaller. If the inclination angle θ of the first step sidewall and the vibration direction are within 10°, the inclination angle θ of the second step sidewall should also be within 10°. If the inclination angles of the first step sidewall and the second step sidewall to the vibration direction are greater than 45°, the nested cross-density between the step-type vibration electrode and the step-type counter electrode will be reduced, resulting in reduced area efficiency and weakened capacity increase effect. However, if the reduction in area efficiency is not a problem, a tilt angle θ exceeding 45° is acceptable. If Figure 2A As shown, when the tilt angle θ is 0° with the vibration direction, the area efficiency is the highest and the capacity expansion effect is the best.

[0154] The counter electrode base 11 has a flat main surface and a plurality of counter convex portions 11a. p-1 , 11a p , 11a p+1, ..., this overall structure is referred to as a "stepped counter electrode" in this article. For the counter electrode base 11, "flat plate" also refers to a structure in which the first main surface (upper surface) and the second main surface (lower surface) of the counter electrode base 11 are flat and parallel to each other, which is the same as the vibration electrode base 12. The counter electrode base 11 is made of a conductive material such as metal. The side convex portion 11a p-1 , 11a p , 11a p+1 , ... are also low resistivity conductors, whether dielectric or non-dielectric, with a resistivity of about ρ = 3Ω·cm or less, and can be used as the structure of the acoustic element in the first embodiment. More generally, the opposite side protrusions can be dielectrics with a resistivity of ρ≈∞. For example, as follows Fig.16 As shown in the figure, the convex part 11a on the opposite side p-1 , 11a p , 11a p+1 , ... can be made of a semiconductor material with a low resistivity ρ as a dielectric. As described above, in the present invention, a component that induces positive charge and negative charge respectively on the surface of the opposite region at different potentials to form a capacitor is defined as an "electrode". Therefore, in the case where a true charge is induced in the region where a convex portion of the same potential electrically connected to the counter electrode base 11 is formed, that is, on the surface of the region where the convex portion is formed, even if it is the surface of a dielectric, the "opposite convex portion" as the convex portion can be defined as a component that is a part of the electrode.

[0155] Although its deflection does not Figure 2C and Figure 2D The counter electrode base 11 is as large as the vibrating electrode base 12 shown in the figure, but the counter electrode base 11 is also deflected toward the vibrating electrode base 12, and the deflection direction is opposite to that of the vibrating electrode base 12. Therefore, strictly speaking, the counter electrode base 11 is also flat when not vibrating. Figure 2B In the cross section, the plurality of opposite side protrusions 11a constituting the stepped opposite side electrode p-1 , 11a p , 11a p+1 , ... and a plurality of vibration side convex portions 12a constituting a stepped vibration electrode q-1 , 12a q , 12a q+1 , ...are opposed in a manner that allows them to form interdigitated structures (nested structures), and the respective first step side walls and the corresponding respective second step side walls constitute a plurality of parallel plate capacitors to increase the capacitance.

[0156] like Figure 2BAs shown, the counter electrode base 11 is located on the top of the counter electrode support layer 25, wherein at least the top layer is an insulator. On the other hand, a vibration electrode top protective film 56 composed of an insulator is disposed on the vibration electrode base 12 to cover the vibration electrode base 12. The cavity side wall 23 is configured to surround the space sandwiched between the vibration electrode base 12 and the counter electrode base 11, thereby forming a vibration cavity. In other words, the vibration cavity is a sealed space surrounded by the counter electrode base 11, the vibration electrode base 12 and the cavity side wall 23. The acoustic element in the first embodiment is a capacitive acoustic element. Figure 2B An electric signal is applied between the counter electrode base 11 and the vibration electrode base 12 in the vibration cavity shown. That is, by applying an electric signal between the counter electrode base 11 and the vibration electrode base 12 and bending the vibration electrode base 12 in the vibration cavity, an ultrasonic signal can be transmitted.

[0157] As mentioned above, Figure 2A and Figure 2B This is a schematic diagram. The purpose is to make the structure easier to understand. Therefore, 13 rectangles are used to represent the opposite side convex part 11a in the cross-sectional view. p-1 , 11a p , 11a p+1 , ... and 12 rectangles represent the vibration side convex portion 12a q-1 , 12a q , 12a q+1 , ... are represented as simplified structures with reduced numbers. Figure 2A As can be seen from the plan view in the figure, the 13 opposite convex portions 11a in the cross-sectional view p-1 , 11a p , 11a p+1 The central opposite side convex parts of ... are hexagonal. Figure 2A It can be seen that the remaining 12 rectangles on the cross-sectional view represent the opposite side protrusions 11a. p-1 , 11a p , 11a p+1 , ... are six wall-shaped opposite side protrusions 11a forming a plurality of concentric hexagonal rings surrounding the central opposite side protrusion p-1 , 11a p , 11a p+1 ,…….Right now, Figure 2B The opposite side convex part 11a represented by 13 rectangles p-1 , 11a p , 11a p+1 ,…is the cross section of six concentric hexagonal rings connected on the back of the paper and a hexagonal column in the middle.

[0158] On the other hand, the vibration side convex portion 12a is represented by 12 rectangles in the cross-sectional view. q-1 , 12a q , 12aq+1 ,……,exist Figure 2A The plan view in FIG. 1 shows the contralateral convex portion 11a. p-1 , 11a p , 11a p+1 , ... between the convex points. It can be seen that the multiple concentric hexagonal rings form six wall shapes with vertical side walls, and the thickness thereof can be inserted into the concave part between the convex parts. Vibration side convex part 12a q-1 , 12a q , 12a q+1 , ...are respectively inserted into the opposite side protrusions 11a p-1 , 11a p , 11a p+1 , ..., a nested structure is formed. In fact, the convex part 11a on the side p-1 , 11a p , 11a p+1 , ... and the vibration side convex portion 12a q-1 , 12a q , 12a q+1 , ...are far more than Figure 2A and Figure 2B The number shown is, as described above, 151 pairs of convex portions 11a p-1 , 11a p , 11a p+1 , ... and 150 vibration side protrusions 12a q-1 , 12a q , 12a q+1 The concave and convex pairs of ,... can be arranged alternately with a gap of 20nm.

[0159] like Figure 2B As shown, the acoustic element according to the first embodiment transmits an ultrasonic signal by applying an electric signal between the opposing electrode base 11 and the vibration electrode base 12 and bending the vibration electrode base 12. The vibration electrode base 12 and the vibration side convex portion 12a made of a conductive material on the surface of the vibration electrode base 12 are q-1 , 12a q , 12a q+1 , ...The schematic diagram of deflection during vibration is as follows Figure 2C As shown in Figure 1, the concave and convex pairs are alternately nested with a gap of 20 nm, forming about 150 concave and convex pairs. Figure 2C In the figure, the actual structure is thinned to about 1 / 10 to show 15 concave-convex pairs, the vibration electrode base 12 and the vibration side convex portion 12a. q-1 , 12a q , 12a q+1 , ...The deflection during vibration is represented by a simplified schematic diagram. Figure 2C The displacement units shown on the vertical axis are nm, and Figure 2CThe position coordinate unit shown on the horizontal axis is μm. Therefore, it should be noted that Figure 2C The aspect ratio in the image is about 100 times different, and the displacement on the longitudinal axis is exaggerated compared to the actual ratio. For example, when the aspect ratio is 1:1, the convex surface of the vibrating side of the periphery is tilted outward by about 7-8°, but Figure 2C At the aspect ratio shown, no outward tilt is visible.

[0160] Depend on Figure 2C It can be seen that the displacement of the vibrating electrode base 12 during vibration is larger in the central part of the vibration cavity and smaller in the peripheral part. Figure 2C In the middle, the opposite side convex part 11a p-1 , 11a p , 11a p+1 , ... and the vibration side convex portion 12a q-1 , 12a q , 12a q+1 , ...intersect in the central part of the vibration cavity but do not intersect in the outer part. Figure 2C The example structure is to place the opposite side convex portion 11a p-1 , 11a p , 11a p+1 , ... and the vibration side convex portion 12a q-1 , 12a q , 12a q+1 , ...is set to 150nm, so that the outer portions do not intersect. However, if the opposite side protrusion 11a p-1 , 11a p , 11a p+1 , ... and the vibration side convex portion 12a q-1 , 12a q , 12a q+1 ,...are respectively increased to 300nm or higher, the outer parts may intersect. Figure 2D express Figure 2C A magnified view of a portion of the IID in the crossover region circled in . Figure 2D In the middle, the opposite side convex part 11a p-1 , 11a p , ... and the vibration side convex portion 12a q-1 , 12a q , 12a q+1 , ... intersect, and between the respective first step sidewalls and the opposite second step sidewalls, a capacitor capacitance C is configured udh Increased lateral capacitor C udh . The lateral capacitor C udh Indicates that the electric lines extend in the horizontal direction. In addition, Figure 2D It is shown that at the vibration side convex part 12a u-1 The top and the opposite side convex portion 11ad-1 The side walls of the capacitor C uds , on the vibration side convex portion 12a u+1 The top and the opposite side convex portion 11a d The side walls of the capacitor C uds In addition, the schematic diagram also shows that the contralateral convex portion 11a d-1 The top and the vibration side convex part 12a u Between the side walls and the opposite convex portion 11a d The top and the vibration side convex part 12a u A diagonal capacitor C is also formed between the side walls uds , capacitor capacity C uds Increase. The oblique capacitance C uds It means that the electric force lines extend in the inclined direction.

[0161] Figure 2E The cross-sectional structure of the acoustic element of the first embodiment is shown, with the focus on the peripheral structure of the vibration chamber. That is, the outermost first vibration side convex portion 12a1 is inserted between the groove formed by the outermost pair of stepped side wall portions 11a0 and the first pair of side convex portions 11a1, and the second vibration side convex portion 12a2 is inserted into the inner groove of the first pair of side convex portions 11a1, and the longitudinal capacitor C udv1 , C udv2 and the lateral capacitor C udh That is, on the surface of the opposite step side wall portion 11a0 and the surface of the first pair of side convex portions 11a1, and on the surface of the first vibration side convex portion 12a1 and the surface of the second vibration side convex portion 12a2, true charges that become the starting point and the end point of the electric lines of force of the vibration cavity 18 are induced according to Gauss's law, forming a longitudinal capacitor C udv1 , C udv2 and the lateral capacitor C udh . The longitudinal capacitor C udv1 , C udv2 The electromotive force lines extend along the normal direction of the main surfaces of the first electrode base (vibration electrode base) 12 and the second electrode base (opposing electrode base) 11. Here, the longitudinal capacitor C udv1 , C udv2 It is called "normal direction capacitor". On the other hand, the lateral capacitor C udh It means that the direction in which the electric force lines extend is perpendicular to the electric force lines in the normal direction of the main surfaces of the first and second electrode bases. In this specification, a capacitor that at least partially relies on electric force lines that are inclined to the normal direction of the main surfaces of the first electrode base (vibration electrode base) 12 and the second electrode base (counter electrode base) 11 is hereinafter referred to as a "non-normal direction capacitor". This situation is different from Figure 2CThe situation of the outer periphery of the structure shown is different, but in the manufacturing process stage, the interval and intersection of the step side wall portion 11a0 and the first pair of side protrusions 11a1 and the first vibration side protrusion 12a1 are set as the initial setting conditions. Figure 2C In the structure shown, the stepped vibration electrode and the stepped counter electrode do not intersect in a nested manner at the periphery. Figure 2E It is shown that if each of the step-type vibration electrode and the step-type counter electrode has a step structure, even if they do not intersect in a nested manner, they contribute to the normal direction capacitor capacity C udv1 , C udv2 And the non-linear direction capacitor capacity C udh That is, in the acoustic element of the first embodiment, it is not necessary for all of the step-type vibration electrodes and the step-type counter electrodes to intersect in a nested manner, but only necessary for at least some of them to intersect in a nested manner.

[0162] Figure 2B The counter electrode support layer 25 shown in the figure is composed of a component substrate 51 (such as a silicon substrate), a base insulating film 52 (such as a silicon oxide film (SiO film) on the original substrate 51) and a counter electrode bottom protective film 53 (such as a silicon nitride film (SiN film) on the base insulating film 52) in a stacked structure. The counter electrode base 11 is located on the counter electrode bottom protective film 53. When the vibration electrode base 12 is set to the ground potential V ss = 0 V, and a driving potential V is applied to the electrode base 11 dr When the step vibration electrode (12; 12a q-1 , 12a q , 12a q+1 , ...) and a first step side wall and a step counter electrode (11; 11a p-1 , 11a p , 11a p+1 , ...) the relative area defined between the two vertical side walls of the second step side wall changes with the driving potential V dr For example, the driving potential V dr Can be V dr =30V or more. The electrode base 11 can be made of a conductive material, such as tungsten (W). The opposite side stepped side wall portion 11a0 and the first opposite side convex portion 11a1 are arranged above the electrode base 11 to form a structure protruding upward from the electrode base 11, and can also be made of metal (such as W).

[0163] like Figure 2EAs shown, the side surface of the vibration cavity 18 of the opposite side stepped side wall portion 11a0 and the surface of the first pair of side convex portions 11a1, as well as the upper surface of the opposite side electrode base portion 11 where the opposite side stepped side wall portion 11a0 and the first pair of side convex portions 11a1 are not configured, are covered with an opposite side dielectric layer 54 composed of a dielectric film such as a silicon nitride film. Similarly, the surface of the first vibration side convex portion 12a1 and the second vibration side convex portion 12a2 and the bottom surface of the vibration electrode base portion 12 where the first vibration side convex portion 12a1 and the second vibration side convex portion 12a2 are not configured are covered with a vibration side dielectric layer 55 composed of a dielectric film such as a silicon nitride film. The opposite side dielectric layer 54 and the vibration side dielectric layer 55 can be made of various high dielectric, ferroelectric, normal dielectric and other films, as described in the latter part of the basic concept explanation at the beginning of this section. A vibration electrode top protective film 56, such as a silicon oxide film, is provided on the vibration electrode base portion 12. As described above, the vibration side convex portion 12a q-1 , 12a q , 12a q+1 , ... and the opposite side convex portion 11a p-1 , 11a p , 11a p+1 , ...can be made of conductive materials such as metal or dielectric with low resistivity ρ.

[0164] In particular, when the vibration side convex portion 12a q-1 , 12a q , 12a q+1 , ... and the opposite side convex portion 11a p-1 , 11a p , 11a p+1 , ... When made of metal, the vibration side convex portion 12a q-1 , 12a q , 12a q+1 The surface of the convex portion 11a is covered with a vibration-side dielectric layer 55. p-1 , 11a p , 11a p+1 The surfaces of the vibration side convex portion 12a and the vibration side convex portion 12a are covered with the opposite side dielectric layer 54. This is because, if the vibration side dielectric layer 55 or the opposite side dielectric layer 54 is not applied, the metal vibration side convex portion 12a in the bare state q-1 , 12a q , 12a q+1 , ... and metal opposite side protrusions 11a p-1 , 11a p , 11a p+1 ,... come into contact with each other, an electrical short circuit will occur between the metals.

[0165] In addition, the opposite side dielectric layer 54 and the vibration side dielectric layer 55 also have the function of increasing the capacitance. Therefore, the thickness of the portion located on the side wall of the opposite side dielectric layer 54 and the vibration side dielectric layer 55 is greater than that of the vibration side convex portion 12a. q-1 , 12a q , 12a q+1 , ... and the opposite side convex portion 11a p-1 , 11a p , 11a p+1 , the width of... (such as Fig. 22 The convex width x0) defined in (a) is relatively thick. Figure 2B The cavity sidewall portion 23 shown in FIG. 1 is composed of a composite structure of a sidewall insulating film bottom layer 21 (such as a silicon oxide film) and a sidewall insulating film 22 (such as a silicon oxide film deposited on the sidewall insulating film bottom layer 21). Figure 2E The sidewall insulating film bottom layer 21 is deposited on the upper surface of the bottom insulating film 52 in such a manner as to embed the counter electrode base 11 , and the sidewall insulating film 22 is deposited on the sidewall insulating film bottom layer 21 including the upper surface of the edge of the counter electrode base 11 .

[0166] First Embodiment Method for Manufacturing Acoustic Element

[0167] The following will refer to Figure 6A-6H The manufacturing method of the acoustic element according to the first embodiment of the present invention is described. Fig. 6A As shown, a film forming method such as chemical vapor deposition (CVD) is used to form, for example, a bottom insulating film 52 (such as a silicon oxide film) on an element substrate 51 (such as a single crystal silicon substrate) with a thickness of about 100 nm on the entire surface. Next, a counter electrode bottom protective film 53 such as a silicon nitride film is formed on the bottom insulating film 52 with a thickness of about 50 nm using a CVD method or the like. In addition, a side wall insulating film bottom layer 21 such as a silicon oxide film is formed on the entire surface of the counter electrode bottom protective film 53 using a CVD method or the like with a thickness of about 100 nm.

[0168] Then, a first photoresist film is spin-coated on the entire surface of the sidewall insulating film bottom layer 21, and the first photoresist film is exposed and developed using a photolithography technique to open a pattern of a first embedding groove portion embedded in the counter electrode substrate 11. Using the pattern of the first photoresist film as an etching mask, the sidewall insulating film bottom layer 21 is selectively etched by using a dry etching technique (such as reactive ion etching (RIE)) until the upper surface of the counter electrode bottom protection film 53 is exposed, thereby forming a first embedding groove portion. If the counter electrode bottom protection film 53 is a silicon nitride film and the sidewall insulating film bottom layer 21 is a silicon oxide film, the counter electrode bottom protection film 53 can be used as an etching stop layer.

[0169] Then, after forming a first conductive film such as W by a film forming method such as a CVD method so as to fill the first damascene groove, a film polishing method such as a chemical mechanical polishing (CMP) method is used to expose the upper surface of the flattened sidewall insulating film base layer 21, thereby burying the first conductive film in the first damascene groove. The first conductive film embedded in the first damascene groove portion becomes a flat plate-shaped counter electrode base 11 having a flat main surface.

[0170] Next, a side wall insulating film 22 such as a silicon oxide film is formed with a thickness of 250 to 900 nm on the entire surface of the side wall insulating film base 21 and the counter electrode base 11 by using a CVD method or the like. Then, a second photoresist film is spin-coated on the entire surface of the side wall insulating film 22, and the second photoresist film is exposed and developed by using a photolithography technique to form a pattern to open the second inlay groove portion, which is embedded in the pattern of the counter side convex portion, such as Figure 6C The pattern of the second photoresist film is used as an etching mask, and the sidewall insulating film 22 is selectively etched using a dry etching technique (such as RIE) until the top surface of the counter electrode base 11 is exposed, forming Figure 6C The second damascene groove portion is shown in medium gray. The counter electrode substrate 11 serves as an etching stopper.

[0171] Then, a second conductive film such as W is formed by a CVD method to embed the second inlay groove portion. The first and second conductive films can use the same conductive material. Then, the film is flattened by a CMP method thin film polishing method until the top surface of the side wall insulating film 22 is exposed, thereby embedding the second conductive film into the second inlay groove portion, such as Figure 6B The partial cross-section structure is shown in Figure 2. Figure 6B The cross-sectional structure of the outer cross section shown is the second conductive film embedded in the second inlay groove portion, and the opposite step side wall portion 11a0 and the opposite step side wall portion 11a0 constitute the outermost side wall structure, becoming the first layer of hexagonal ring on the inner side, namely the first pair of side protrusions 11a1.

[0172] In practice, Figure 6C The planar pattern shown in FIG. 1 is a planar counter electrode base 11 having a flat main surface, and the counter convex portion 11a is p-1 , 11a p , 11a p+1 , ...form a pattern of multiple concentric hexagonal rings that are periodically and repeatedly connected to form a stepped electrode structure. Figure 6C It should be noted that the convex portion 11a on the opposite side p-1 , 11a p , 11a p+1, ..., etc. are not continuous and complete hexagonal rings, but discontinuous hexagonal rings with breakpoints (gaps). p-1 , 11a p , 11a p+1 The cutouts in the plane patterns of the respective hexagonal rings of , ... are radially continuous and form three corrosion medium channels (channels). Figure 6C In the figure, two dotted lines are used to schematically represent three corrosion medium channels (channels) 151, 152 and 153, but this figure does not mean that the side convex portion 11a p-1 , 11a p , 11a p+1 , ..., the patterns of the gap portion and the groove portion are different. As described below, the "etching medium channel" is a medium path for introducing an etchant (etching medium) during the process of removing the sacrificial film. Therefore, in the case where the etching medium is a liquid, the opposite side convex portion 11a p-1 , 11a p , 11a p+1 In a micro-integrated structure consisting of about 150 channels with a spacing of 400 nm, the number of the etching medium channels (channels) 151, 152, 153 may be less than three, in which case the channels are radially distributed in a spider web shape. In the case where the etching medium is a gas, the etching medium channels 151, 152, 153 may be omitted.

[0173] In addition, between the side wall insulating film 22 and the opposite side protrusion 11a p-1 , 11a p , 11a p+1 , ..., and the third photoresist film is spin-coated on the entire surface of the side wall structure, and the third photoresist film is applied to the outermost opposite step side wall portion 11a0 as the side wall structure by using the photolithography technology, and the top surface of the side wall insulation film 22 located at the periphery of the opposite step side wall portion 11a0 is exposed and developed to form a pattern for protecting the top surface of the side wall insulation film 22. After the pattern of the third photoresist film is formed, it also covers the top surfaces of the pipeline ends 141, 142, 143 as the peripheral portion, and the etching medium channels 151, 152, 153, which are continuous with the pipeline ends 141, 142, 143 on the side of the side wall through the side wall insulation film 22. Then, using the pattern of the third photoresist film as an etching mask, the top surface of the counter electrode base 11 is etched by using the etching selectivity ratio, for example, by wet etching technology, until the top surface of the counter electrode base 11 is exposed, forming a sacrificial film embedded in the groove portion. However, if the etching selectivity ratio can be ensured, wet etching is not necessary. As a result of etching using this etching selectivity ratio, the side protrusion 11a p-1 , 11a p , 11a p+1 , ... and the surface without the opposite side protrusion 11ap-1 , 11a p , 11a p+1 , ..., the surface of the opposite electrode base portion 11 is exposed. Figure 6C The surface of the electrode base 11 corresponding to the corrosion medium channels 151, 152, 153 shown in FIG. 1 and the opposite side protrusion 11a cut by the corrosion medium channels 151, 152, 153 p-1 , 11a p , 11a p+1 , ..., the end portion in the direction perpendicular to the wall surface of the hexagonal ring (radial direction) is also exposed.

[0174] Then, between the side wall insulating film 22 and the opposite side protrusion 11a p-1 , 11a p , 11a p+1 , ..., a fourth photoresist film is spin-coated on the entire surface to fill the sacrificial film embedding groove, and form Figure 6C The patterns for opening the pipe ends 141, 142, 143 shown in the figure, and the patterns for opening the etching medium channels (pipes) 151, 152, 153, which continuously pass through the side wall insulating film 22 to the pipe ends 141, 142, 143. And the patterns for opening the etching medium channels (pipes) 151, 152, 153, which continuously pass through the side wall insulating film 22 to the pipe ends 141, 142, 143, are exposed and developed to form the peripheral area. Then, using the pattern of the fourth layer of photoresist film as an etching mask, the side wall insulating film 22 is selectively etched by dry etching technology such as RIE to form vertical hole-shaped (well-shaped) pipe ends 141, 142, 143 and pipe ends 141, 142, 143 horizontal to the side wall insulating film 22. U-shaped groove segments 151, 152, 153 forming the flow channel of the corrosive medium penetrate downward from the side where the sacrificial film is embedded in the groove segment and are continuous.

[0175] Then, by using a CVD method or the like, a dielectric layer 54 on the opposite side composed of a dielectric film such as a silicon nitride film is formed so as to cover the opposite side protrusion 11a. p-1 , 11a p , 11a p+1 , ... and the surface of the opposite electrode base 11 exposed at the bottom of the sacrificial film embedded groove, and its thickness is 50nm. The opposite dielectric layer 54 also covers the Figure 6C The surface of the electrode base 11 corresponding to the corrosion medium channels 151, 152, 153 shown in FIG. 1 and the opposite side protrusion 11a cut by the corrosion medium channels 151, 152, 153 p-1 , 11a p , 11a p+1, .... In addition, the inner wall and bottom surface of the vertical hole pattern that becomes the pipe end 141, 142, 143, and the inner wall and bottom surface of the U-shaped groove that is the continuous etching medium channel 151, 152, 153 from the sacrificial film embedding groove side to the pipe end 141, 142, 143, are also covered with the opposite side dielectric layer 54.

[0176] Next, a sacrificial film 16 made of a material film (e.g., W) having sacrificial etching adaptability is formed on the entire surface of the opposite dielectric layer 54 by using a method such as CVD. For example, the thickness of the sacrificial film formed along the side profile of the sacrificial film embedded groove segment is about 20-100 nm, and the sacrificial film embedded groove segment is filled. The sacrificial film 16 also fills the inside of the pipeline ends 141, 142, 143 (vertical holes (wells)), and the inside of the etching medium channels 151, 152, 153 (U-shaped groove portions that are continuous with the corresponding pipeline ends 141, 142, 143, respectively). Subsequently, a fifth layer of photoresist film is spin-coated on the entire surface of the sacrificial film 16, and is exposed and developed to selectively expose the top side position of the peripheral sidewall insulating film 22. Then, the pattern of the fifth layer of photoresist film is used as an etching mask, and the sacrificial film 16 is selectively etched by dry etching technology (e.g., RIE) to expose the top surface of the opposite dielectric layer 54 located on the top surface of the peripheral sidewall insulating film 22. In the process of exposing the top surface of the opposite dielectric layer 54 located on the top surface of the sidewall insulating film 22 of the peripheral part, the sacrificial film 16 can also be embedded in the pipeline ends 141, 142, 143 and the corrosion medium channels 151, 152, 153 respectively connected to the corresponding pipeline ends 141, 142, 143 to become plugs.

[0177] In addition, if Fig.6D As shown, a vibration side dielectric layer 55 composed of a dielectric film such as a silicon nitride film is formed on the entire surface of the sacrificial film 16 and the opposite side dielectric layer 54 using a CVD method or the like, and has a thickness of about 50 nm. Fig.6D As shown, the counter-side dielectric layer 54, the vibration-side dielectric layer 55, and the sacrificial film 16 are formed along the periodic continuous uneven shape of the sacrificial film embedded in the groove composed of the counter-side step side wall portion 11a0, the counter electrode base portion 11, and the first counter-side convex portion 11a1. Therefore, the cross-sectional shape of the counter-side dielectric layer 54, the vibration-side dielectric layer 55, and the sacrificial film 16 has a periodically repeated concave-convex shape between the multiple hexagonal rings of the counter-side step side wall portion 11a0, the first counter-side convex portion 11a1, etc., forming a stepped counter electrode.

[0178] Next, a third conductive film (eg, a W film) is formed with a thickness of about 100 nm on the entire surface of the vibration-side dielectric layer 55 by using a CVD method or the like so as to embed grooves in the vibration-side dielectric layer 55. Fig. 6EAs shown, CMP is used to completely embed the third conductive film into the groove of the vibration side dielectric layer 55. Alternatively, instead of using CMP, a sixth photoresist film is spin-coated on the entire surface to cover the third conductive film, and is exposed and developed to selectively expose the top side of the peripheral side wall insulating film 22. The pattern of the sixth photoresist film is then used as an etching mask to selectively etch the third conductive film by dry etching techniques such as RIE to expose the top surface of the vibration side dielectric layer 55 located on the top surface of the peripheral side wall insulating film 22. After removing the sixth photoresist film, the third conductive film is etched back. As shown in FIG. Fig. 6E As shown, after etching, the patterns of the first vibration side convex portion 12a1 and the second vibration side convex portion 12a2 are formed. The patterns of the first vibration side convex portion 12a1 and the second vibration side convex portion 12a2 are embedded in the groove of the sacrificial film 16 in a rectangular cross-sectional shape. The sacrificial film 16 passes through the vibration side dielectric layer 55, and its shape is along the periodically repeated concave-convex shape, as shown in FIG. Fig. 6E shown.

[0179] because Fig. 6E It is a partial cross-sectional view focusing on the periphery of the vibration cavity, showing the rectangular cross-section of two convex parts, the outermost first vibration side convex part 12a1 and the inner second vibration side convex part 12a2. Fig. 6E On the left side, the residue 12a2 of the third conductive film buried in the corner of the step formed by the sacrificial film 16 and the vibration side dielectric layer 55 also remains in a triangular pattern. As can be seen from FIG. 2, as an overall structure, the vibration side convex portion 12a q-1 , 12a q , 12a q+1 , ... are periodically formed, for example, with a pitch of 400nm and repeated 150 times. After the third conductive film is patterned, a fourth conductive film such as a W film is formed on the vibration side dielectric layer 55 and inside the first vibration side convex portion 12a1 and the second vibration side convex portion 12a2 using a CVD method, etc., and the thickness is about 100nm. The third conductive film and the fourth conductive film can use the same conductive material.

[0180] Then, the seventh photoresist film is spin-coated on the entire surface to cover the top of the fourth conductive film, and exposure and development are performed to selectively expose the position of the top side surface of the sidewall insulating film 22 in the peripheral region. Then, using the pattern of the seventh photoresist film as an etching mask, the fourth conductive film is selectively etched by a dry etching technique such as RIE, thereby exposing the top surface of the vibration side dielectric layer 55 located on the top surface of the sidewall insulating film 22 in the peripheral region. Fig. 6F As shown, a plate-shaped vibrating electrode base 12 having a flat main surface in a non-vibrating state is formed, which is connected to the upper end of the first vibration side convex portion 12a1 and the upper end of the second vibration side convex portion 12a2, respectively.

[0181] like Fig. 6F The partial cross-sectional view of the periphery of the vibration cavity shown in the figure shows the cross-sectional structure in which two convex parts, the outermost first vibration side convex part 12a1 and the inner second vibration side convex part 12a2, are connected to the lower surface of the vibration electrode base 12. Fig. 6F On the left side, the etching edge of the fourth conductive film is connected to the residue 12a2 of the third conductive film, thereby forming a vertical side on the left side of the step formed by the sacrificial film 16 and the vibration-side dielectric layer 55. Fig. 6F The vertical sidewalls of the etching edges composed of the third and fourth conductive films shown on the left constitute the outer diameter of the regular hexagon shown in FIG2. As for the overall structure, as can be seen from FIG2, the lower surface of the plate-shaped vibration electrode base 12 having a flat main surface when not vibrating is formed with 150 vibration side convex portions 12a at a pitch of 400 nm, for example. q-1 , 12a q , 12a q+1 , ... inserted into the opposite side convex portion 11a p-1 , 11a p , 11a p+1 ,...in such a way as to form a stepped vibration electrode with a suspension structure.

[0182] Next, a vibration electrode protection film base such as a silicon oxide film is formed on the entire surface of the vibration side dielectric layer 55 and the vibration electrode base portion 12 using a CVD method or the like, with a thickness of about 50 nm. Figure 6G As shown, the eighth photoresist film is spin-coated on the entire surface to cover the bottom layer of the vibration electrode protection film, and the pattern of the holes 161, 162, 163 forming the cavity is aligned with the pattern mask of the pipe ends 141, 142, 143 for exposure and development. Then, the pattern of the eighth photoresist film is used as an etching mask, and a dry etching technique such as RIE is used to selectively etch through the bottom layer of the vibration electrode protection film, the vibration side dielectric layer 55, and the opposite side dielectric layer 54. Figure 6G As shown, by selective etching, cavity forming holes 161, 162, 163 are opened to reach the surface of the sacrificial film 16 buried in the pipe end portions 141, 142, 143 in a plug shape.

[0183] Then, by Figure 6G As shown, when a corrosive medium such as a hydrogen peroxide (H2O2) solution enters as an etchant through the cavity forming holes 161, 162 and 163, the corrosive medium enters the corresponding corrosive medium channels 151, 152 and 153 through the corresponding pipe ends 141, 142 and 143, respectively. Figure 6D-6F As shown, the corrosive medium (etchant) will etch away the sacrificial film 16, and the cross-sectional shape of the sacrificial film 16 is a periodic non-uniform shape. Figure 6HAs shown, when the sacrificial film 16 is etched away, a vibration cavity 18 is formed between the counter electrode base 11, the driving side wall counter electrode 11a0 and the first pair of side protrusions 11a1 and the vibration electrode base 12, the first vibration side protrusion 12a1 and the second vibration side protrusion 12a2.

[0184] Figure 6H It is a cross-sectional view showing the periphery of the vibration cavity 18, the vibration cavity 18 meandering in a wave shape between the first vibration side convex parts 12a0, the first vibration side convex parts 12a1 are inserted from above, and the space of the concave part composed of the outermost opposite side stepped side wall part 11a0 and the first opposite side convex part 11a1 as the side wall structure is offset. In addition, Figure 6H As shown on the right side of the paper, the concave space on the inner peripheral side of the first relative side convex portion 11a2 is a part of the wave-shaped meandering vibration cavity 18 between the second vibration side convex portion 12a2 inserted from above. As for the overall structure, as shown in FIG. 2, the corresponding vibration side convex portion 12a q-1 , 12a q , 12a q+1 , ... inserted into the adjacent pair of convex parts 11a p-1 , 11a p , 11a p+1 , ..., inserted in a nested configuration, wherein the bellows is on the opposite side convex portion 11a p-1 , 11a p , 11a p+1 , ... and the vibration side convex portion 12a q-1 , 12a q , 12a q+1 ,...winding between them to form a vibration cavity 18.

[0185] When the etching medium is a liquid (such as a hydrogen peroxide solution), after the removal process of the sacrificial film 16 is completed, the etching medium cleaning process is transferred to the etching medium cleaning process using a cleaning liquid. After the etching medium cleaning process is completed, the cleaning liquid is dried by methods such as isopropyl alcohol (IPA) vapor drying. After the cleaning liquid is dried, a main protective layer, that is, the remaining part of the vibration electrode top protective film 56, is deposited on the bottom layer of the vibration electrode protective film with a thickness of 150-1000nm on the entire surface using a reduced pressure CVD method or the like. By depositing the main protective layer on the bottom layer of the vibration electrode protective film under reduced pressure, plugs can be set at the entrances of the holes 161, 162, and 163 that form the cavity, and the vibration cavity 18 is vacuum sealed. For example, using He gas as the main carrier gas, the main protective layer is deposited by reduced pressure CVD, so that the interior of the vibration cavity 18 is in a reduced pressure state of about 1kPa, and plugs are set at the entrances of the holes 161, 162, and 163 that form the cavity. The composite film of the lower layer of the vibration electrode protective film and the main protective layer constitutes Figure 6HThe protective film 56 on top of the vibration electrode is shown to complete the acoustic element in the first embodiment.

[0186] In the above series of manufacturing processes, for example, assuming that the thickness of the dielectric layer 54 is 50 nm, the thickness of the vibration side dielectric layer 55 is 50 nm, the thickness of the side wall insulating film 22 is 250 nm, and the thickness of the sacrificial film 16 is 100 nm, the vibration side convex portion 12a q-1 , 12a q , 12a q+1 , ... and the opposite convex portion 11a p-1 , 11a p , 11a p+1 , ..., the initial crossover is 50%. However, if Figure 3 to Figure 5 As shown, the acoustic element with an initial crossover rate of 0% has higher stored electrical energy and transmitted acoustic energy than the acoustic element with an initial crossover rate of 50%.

[0187] In order to manufacture an acoustic element with an initial crossover rate of 0% by partially utilizing the structure based on the above series of manufacturing processes, a second vibration cavity is further provided in the protective film 56 on the top surface of the vibration electrode, and a vibration electrode suction electrode is provided above the second vibration cavity, which is parallel to and opposite to the vibration electrode base 12, and the suction electrode is deflected upward. If a voltage of, for example, -90V to -180V is applied to the vibration electrode suction electrode, so that the vibration electrode base 12 at the ground potential is deflected upward in the second vibration cavity, the vibration side convex portion 12a q-1 , 12a q , 12a q+1 , ... can be from the opposite side convex part 11a along the vibration direction p-1 , 11a p , 11a p+1 , ... are pulled out to an initial state of 0% initial crossover. Then, based on this initial state, a voltage of 90V to 180V is applied to the electrode base 11. In addition, there is another manufacturing method in which the initial crossover is 0% at the end of the manufacturing process. This manufacturing method will be described in the variation section of the second embodiment.

[0188] As described previously, the plane pattern of the acoustic element of the first embodiment is not limited to a regular hexagon. Fig. 7A The structure of the acoustic element according to the first variation of the first embodiment includes a plurality of concentric octagonal rings on the electrode side, focusing on a plurality of opposite side convex portions 71a. p-1 , 71a p , 71a p+1 ,........ The corresponding cross-sectional diagram is omitted, but Figure 2B Similar to the example shown in the cross-sectional view, a plurality of opposite side protrusions 71a p-1 , 71ap , 71a p+1 ,.......respectively have vertical side walls, and their cross-sections are rectangular (oblong). Fig. 7A The base of the electrode is also omitted in the figure, but a plurality of concentric octagonal rings are formed on the opposite sides of the convex portion 71a. p-1 , 71a p , 71a p+1 Each of the convex portions in , ....... is arranged on the counter electrode base as a convex portion having a rectangular cross section. A flat plate-shaped counter electrode base having a flat main surface and a plurality of counter side convex portions 71a on the counter electrode base p-1 , 71a p , 71a p+1 The overall structure of ,....... constitutes a stepped counter electrode. Fig. 7A The figure is omitted, and each vibration side convex portion composed of a plurality of concentric octagonal rings is inserted as a convex portion into the opposite side convex portion 71a p-1 , 71a p , 71a p+1 In the internal space of the groove defined by ,......., a structure of multiple concentric octagonal rings that can be nested with each other is formed.

[0189] Fig. 7A This is a schematic diagram showing the number of concentric octagonal rings at intervals to make the structure easier to understand. If the outermost side wall structure, that is, the opposite stepped side wall part, is an octagonal ring, Fig. 7A The simplified structure shown is six octagonal rings surrounding a central octagonal column as a concentric octagonal ring. Figure 2A As in the case of the multiple concentric hexagonal rings shown, in the structure described by the simplified model, for example, 151 opposite convex portions 71a p-1 , 71a p , 71a p+1 ,.......and 150 pairs of concave and convex parts of the vibration side convex parts are arranged alternately with a gap of 20nm.

[0190] exist Fig. 7A It should be noted that the convex portion 71a on the opposite side p-1 , 71a p , 71a p+1 ,.......each pattern is not a continuous and complete octagonal ring, but a discontinuous octagonal ring with a gap. That is, each of the opposite side protrusions 71a p-1 , 71a p , 71a p+1 The grooves in the octagonal ring plane pattern are radially continuous, indicating that there are four corrosion medium channels. The corrosion medium channel is removed Figure 6HThe sacrificial membrane and the medium channel for introducing the corrosive agent (corrosive medium) in the process of forming the vibration cavity are shown. The four corrosive medium channels are respectively connected to the pipe ends 144, 145, 146, and 147 of the peripheral area which are arranged in a vertical hole-shaped (tic-tac-toe) structure. They are arranged radially. If the corrosive medium is a gas, the corrosive medium channel can be omitted.

[0191] Fig. 7A The acoustic element of the first variant of the first embodiment is shown as Figure 7B As shown, when the element array is partially arranged, the regular octagonal unit cell X can be fully covered. (i-1),(j+1) , X i,(j+1) , X (i+1),(j+1) , …, X (i-1),j , X i,j , X (i+1),j , …, X (i-1),(j-1) , X i,(j-1) , X (i+1),(j-1) , .... However, for a regular octagon, it is not possible to perform plane filling (tessellation) on the same plane (same surface). That is, Figure 7B As shown, a quadrilateral Y will appear between the regular octagons (i -2) ,(j+1) , Y (i-1),(j+1) , Y i,(j+1) , Y (i+1) ,(j+1),..., resulting in low area efficiency. For example, the regular octagonal unit cell X (i-1),(j+1) , X i,(j+1) , X (i+1) ,(j+1),…,X (i-1),j , X i,j , X (i+1) ,j,…,X (i-1),(j-1) , X i,(j-1) , X (i+1) ,(j-1),…as the sending unit, and the gap quadrilateral Y (i -2) ,(j+1) , Y (i-1),(j+1) , Y i,(j+1) , Y (i+1) ,(j+1),... as a receiving unit, can be used to form an acoustic element integrated circuit. On the contrary, the regular octagonal unit cell X (i-1),(j+1) , X i,(j+1) , X (i+1) ,(j+1),…,X (i-1),j , X i,j , X (i+1) ,j,…,X (i-1),(j-1) , X i,(j-1) , X (i+1) ,(j-1),…as receiving units, and the gap quadrilateral Y (i -2),(j+1) , Y (i-1),(j+1) , Y i,(j+1) , Y (i+1) ,(j+1),... as the sending unit. Although the quadrilateral Y (i -2) ,(j+1) , Y (i-1),(j+1) , Y i,(j+1) , Y (i+1) ,(j+1),...area efficiency is low, but they can also be arranged into multiple hexagonal or multiple octagonal rings in the sending unit.

[0192] Fig. 8A The structure of the acoustic element of the second variation of the first embodiment is shown in FIG. 1 , which includes a plurality of concentric dodecagonal rings on the electrode side, focusing on a plurality of opposite side convex portions 71a. p-1 , 71a p , 71a p+1 ,........like Figure 2B In the example shown in the cross-sectional view, although not shown in the figure, the plurality of opposite side protrusions 71a p-1 , 71a p , 71a p+1 , ....... respectively have vertical side walls, and their cross-sections are rectangular (rectangular). Not shown in the figure, a plurality of opposite side protrusions 71a forming concentric dodecagonal rings p-1 , 71a p , 71a p+1 Each of the protrusions in , ..... is arranged on the base of the counter electrode as a protrusion having a rectangular cross-section.

[0193] Depend on Fig. 8A It can be seen that the dodecagonal ring is almost a circle. Even if the pattern of the dodecagonal ring is constructed in the mask layer, the finished pattern after processes such as photolithography and etching is almost a circle. Therefore, regular polygons with more angles than the regular dodecagon, such as concentric 15-angle rings and concentric 20-angle rings, can be approximated as circles. The stepped counter electrode is composed of a counter electrode base with a flat main surface and a plurality of opposite side protrusions 71a on the counter electrode base. p-1 , 71a p , 71a p+1 Each vibration side convex portion (omitted in the figure) composed of a plurality of concentric dodecagonal rings is arranged as a convex portion and inserted into the opposite side convex portion 71a. p-1 , 71a p , 71a p+1 In the internal space of the groove defined by ,......., a structure of multiple concentric twelve-angle rings that can be nested with each other is formed.

[0194] Fig. 8AThis is a schematic diagram showing the number of concentric dodecagonal rings at intervals, making the structure easier to understand. If the outermost sidewall structure, that is, the opposite stepped sidewall part, is a dodecagonal ring, Fig. 8A Showing a simplified structure, 6 dodecagonal rings surround a central dodecagonal column as concentric dodecagonal rings. However, unlike Figure 2A As in the case of the multiple concentric hexagonal rings shown in FIG. 1 , the structure described in the simplified model, for example, 151 pairs of convex portions 71a p-1 , 71a p , 71a p+1 ,.......and 150 pairs of concave and convex parts of the vibration side convex parts are arranged alternately with a gap of 20nm.

[0195] like Fig. 8A As shown, each of the opposite side protrusions 71a p-1 , 71a p , 71a p+1 The pattern of , ....... is not a continuous and complete dodecagonal ring, but a discontinuous dodecagonal ring with a gap. That is, the convex portion 71a on the opposite side p-1 , 71a p , 71a p+1 ,........the notches in the plane pattern of the respective dodecagonal rings are illustrated as three radially continuous etching medium channels. The three etching medium channels are arranged radially and are respectively connected to the pipe ends 144, 145, 146, and 147 arranged in a well-like structure at the peripheral portion. If the etching medium is a gas, the etching medium channel can be omitted.

[0196] when Fig. 8A The acoustic element of the second variation of the first embodiment shown in Figure 8B As shown, when the element array is partially arranged, the regular dodecagonal unit cell X can be fully covered. (i-1),(j+1) , X i,(j+1) , X (i+1) ,(j+1),…,X (i-1),j , X i,j , X (i+1) ,j,…,X (i-1),(j-1) , X i,(j-1) , X (i+1) ,(j-1),…. However, for a regular dodecagon, plane filling cannot be performed on the same plane. That is, Figure 8B As shown, a concave octagon Y will appear between the regular dodecagons (i-1),(j+1) , Y i,(j+1) , …, Y (i-1),j , Y i,j , ..., resulting in low area efficiency. For example, a regular dodecagonal unit cell X (i-1),(j+1) , X i,(j+1) , X(i+1) ,(j+1),…,X (i-1),j , X i,j , X (i+1) ,j,…,X (i-1),(j-1) , X i,(j-1) , X (i+1) ,(j-1),…as the sending unit, the concave octagon Y (i-1),(j+1) , Y i,(j+1) , …, Y (i-1),j , Y i,j , ... as receiving units. On the contrary, the regular dodecagonal unit cell X (i-1),(j+1) , X i,(j+1) , X (i+1) ,(j+1),…,X (i-1),j , X i,j , X (i+1) ,j,…,X (i-1),(j-1) , X i,(j-1) , X (i+1) ,(j-1),…as receiving units, and the concave octagon Y in the gap (i-1),(j+1) , Y i,(j+1) , …, Y (i-1),j , Y i,j , ... can be used as a transmission unit. Although the area efficiency is low, it can be used in the concave octagon Y (i-1),(j+1) , Y i,(j+1) , …, Y (i-1),j , Y i,j , … and a plurality of hexagonal, octagonal and dodecagonal rings are arranged inside.

[0197] If the corrosive medium used in manufacturing the vibration cavity is liquid, in the micro-integrated structure, Figure 2A The opposite side convex portion 11a shown in p-1 , 11a p , 11a p+1 , ... In a cavity with a width of 120 μm, there are about 150 channels (pipes) 151, 152, 153 at a pitch of 400 nm. The number of the corrosion medium channels (pipes) 151, 152, 153 may be less than 3. Similarly, if Fig. 7A As shown, in the case of a regular octagon, four channels for the corrosive medium will not be enough, while Fig. 8A As shown in FIG. 1 , in the case of a regular dodecagon, three etching medium channels will not be enough. In this case, it is necessary to form etching medium channels in a spider web-like radial pattern. As the number of spider web-like radial additional channels increases, the facing length between the first step side wall of the step vibration electrode and the second step side wall of the step counter electrode becomes longer, and the facing area cannot be increased. In addition, in the spider web-like planar pattern, the unit cell X i,j The area efficiency of the spider web pattern in the image will be worse because sharp corners will be generated in the spider web mesh and half-sized mesh portions will be generated.

[0198] In the acoustic element of the third variation of the first embodiment, as Fig.9A As shown, the downward protruding portion of the step vibration electrode 74 having a lattice shape is Fig. 9B The square pin 74a on the counter electrode side is shown ij The upward projections of the Fig. 9B In the embodiment, the pipe ends 171, 172, 173 are configured as vertical holes at the positions of the peripheral side wall insulation films. Fig.9A In the figure, holes 181, 182, 183 for forming cavities are arranged at positions of the peripheral side wall insulating film corresponding to the positions of the pipe ends 171, 172, 173, so that the liquid corrosive medium can be introduced through the holes 181, 182, 183 for forming cavities. The lattice-shaped step vibration electrode 74 is arranged at the bottom of the flat plate vibration electrode base with a flat main surface, which is omitted in the figure. Fig. 9B The square prism needle 74a shown in ij The sword-shaped square column needles 74a that constitute the stepped counter electrode are arranged on the counter electrode base like a sword mountain to form a stepped counter electrode, which is omitted in the figure. ij The step counter electrode and the step vibration electrode are nested in the space formed by the lattice groove on one side of the vibration electrode, thereby maximizing the relative area between the step counter electrode and the step vibration electrode. Therefore, the acoustic element according to the third variation of the first embodiment can achieve the same driving voltage in the unit cell X. i,j Increase the sending output of ultrasonic signals.

[0199] (Second embodiment)

[0200] The acoustic element integrated circuit of the second embodiment of the present invention is different from the acoustic element integrated circuit of the first embodiment. Figure 1 Similarly, in the element array part, the regular hexagonal unit cell X (i-1),(j+1) , X i,(j+1) , X (i+1) ,(j+1),…,X (i-1),j , X i,j , X (i+1) ,j,…,X (i-1),(j-1) , X i,(j-1) , X (i+1) , (j-1), ..., etc. are arranged in the same plane (on the same surface) to form a two-dimensional matrix according to the plane layout. Fig.10 As shown, the stepped counter electrode of the acoustic element of the second embodiment includes a counter-side convex portion (second electrode side convex portion) 13a p-1 , 13a p , 13a p+1,.......consists of a plurality of wall-shaped conductors, forming a plurality of concentric hexagonal rings in a cavity, and its plane layout is a regular hexagon, arranged at equal intervals. However, as an example, it is not always necessary to form a plurality of concentric hexagonal rings with the same gap and a certain spacing. By making the gaps and spacings of the plurality of concentric hexagonal rings uneven, the frequency band of the acoustic element integrated circuit of the second embodiment can be widened. Therefore, the gaps or spacings of the plurality of concentric hexagonal rings can be changed to achieve the purpose of widening the frequency bandwidth. Multiple opposite side protrusions 13a p-1 , 13a p , 13a p+1 Each of the , ....... has a vertical side wall, Fig.12 The opposite side convex portion 13a shown in p and Fig.13 The cross-sectional structures of the pair of stepped side wall portions 13a0 and the first pair of convex portions 13a1 shown in FIG. 1 are the same.

[0201] like Fig.11 As shown in FIG. 1 , focusing on the plan view of the stepped counter electrode, a plurality of counter-side protrusions 13a p-1 , 13a p , 13a p+1 , ....... are arranged on the first pair of electrode bases 111, the second pair of electrode bases 112 and the third pair of electrode bases 113 respectively, which are divided into three parts, Figure 2A and Figure 2E The acoustic element of the first embodiment shown in FIG. 1 is different from the structure of the single pair of electrode bases 11 of the acoustic element of the first embodiment, which is characterized by being electrically connected to each other. In the acoustic element of the second embodiment, there are three flat plate-shaped first pair of electrode bases 111, second pair of electrode bases 112, and third pair of electrode bases 113 with flat main surfaces, which are divided into three parts and have the same potential, and a plurality of pairs of side protrusions 13a connected to the three first pair of electrode bases 111, second pair of electrode bases 112, and third pair of electrode bases 113. p-1 , 13a p , 13a p+1 ,.......the overall structure is called "step counter electrode".

[0202] However, it is not limited to three partitions, and may be divided into two or four or more other partitions. p-1 , 13a p , 13a p+1 , .......a vibration side convex portion (first electrode side convex portion) 12a composed of a plurality of wall-shaped conductors forming another plurality of concentric hexagonal rings with gaps between them q-1 , 12a q , 12a q+1, ... having equally spaced gaps arranged at a certain pitch, with a plurality of opposite side convex portions 13a p-1 , 13a p , 13a p+1 ,........The structure of the acoustic element of the first embodiment is the same as that of the acoustic element of the first embodiment in that the cross-sectional structure is formed. Fig.12 The structure shown is the same, with multiple vibration side convex parts 12a q-1 , 12a q , 12a q+1 , ...having vertical side walls.

[0203] In the acoustic element of the first embodiment, the etching medium passages 151, 152 and 153 for introducing the etching medium when forming the vibration chamber are flat-topped structures, and the plurality of side protrusions 11a are flat-topped structures. p-1 , 11a p , 11a p+1 , ... are arranged on the same horizontal plane. In contrast, in the acoustic element of the second embodiment, Fig.11 and Fig.12 As shown, the corrosion medium channels 151b, 152b, and 153b for introducing the corrosion medium are three-dimensional structures, which are divided into three parts, namely, three flat underground pits with flat main surfaces having the same electric potential as the first pair of electrode bases 111, the second pair of electrode bases 112, and the third pair of electrode bases 113, which is different from the acoustic element involved in the first embodiment.

[0204] By configuring the corrosive medium channels 151b, 152b, 153b in the underground tunnel below the vibration chamber 18, the corrosive medium channels 151b, 152b, 153b have a three-dimensional structure, that is, the number of the corrosive medium channels 151b, 152b, 153b is increased and arranged in a dense spider web structure, and the plurality of opposite side protrusions 13a p-1 , 13a p , 13a p+1 , ....... and vibration side convex portion 12a q-1 , 12a q , 12a q+1 , ..., it is possible to avoid the relative length reduction between the plurality of hexagonal rings. That is, even in the case where the cavity width is 120 μm, the opposite side protrusions 13a are arranged at a pitch of 400 nm. p-1 , 13a p , 13a p+1 , ....... and vibration side convex portion 12a q-1 , 12a q , 12a q+1,... The microstructure can effectively form a corrugated vibration cavity by increasing the number of corrosion medium channels 151b, 152b, 153b and the cross-sectional area of ​​the fluid channel formed in the pit, and avoid the reduction of relative length.

[0205] exist Figure 2E and Figure 6C In the acoustic element of the first embodiment shown in FIG. 1 , the dielectric layer 31 covers the electrode base 11 and the side protrusion 11a. p-1 , 11a p , 11a p+1 , ... surfaces. In contrast, in the acoustic element of the second embodiment, Fig.12 and Fig.13 As shown, the opposite side protrusion 13a is formed by a low resistivity dielectric such as an impurity-doped semiconductor. p-1 , 13a p , 13a p+1 , ......., so that the opposite side convex portion 13a p-1 , 13a p , 13a p+1 ,.......surfaces are exposed inside the vibration chamber 18, which is similar to Figure 2E As described above, in the present invention, on the surface of the opposite regions with different potentials, the portion where the positive charge as the starting point of the electric force line in the vibration cavity and the negative true charge as the end point of the electric force line in the vibration cavity are induced according to Gauss's law is defined as an "electrode". Figure 2E The normal direction capacitor C is shown udv1 , C udv2 and the non-linear capacitor C udh The symbol is marked with Figure 2E Same, in Fig.13 In the cross-sectional structure shown in FIG. 1 , the surface of the opposite step side wall portion 11a0 and the surface of the first opposite side convex portion 11a1, the surface of the first vibration side convex portion 12a1 and the surface of the second vibration side convex portion 12a2 are on the surface of the vibration cavity 18. According to Gauss's law, these surfaces are the starting point and the end point of the electric line, and the true charge is induced on them, forming a normal direction capacitor C udv1 , C udv2 and the non-linear capacitor C udh . Normal direction capacitor C udv1 , C udv2 It indicates that the electric field lines extend in the normal direction of the main surfaces of the first electrode base (vibration electrode base) 12 and the second electrode base (counter electrode base) 11. Fig.13 In the non-linear direction, the capacitor C udh The direction in which the electric lines of force extend is perpendicular to the electric lines of force in the normal direction of the main surfaces of the first and second electrode bases.

[0206] That is, the low resistivity dielectric surface of the convex portion that forms the same potential as the first pair of electrode bases 111, the second pair of electrode bases 112, and the third pair of electrode bases 113 induces true charge according to Gauss's law, so the "opposite side convex portion" plays the role of an element that constitutes a part of the electrode. Fig.13 As shown, the surface of the third pair of electrode bases 113 is coated with a counter-side dielectric layer 31. The vibration side convex portion 12a q-1 , 12a q , 12a q+1 , ... are made of metal. When the vibration side convex portion 12a q-1 , 12a q , 12a q+1 , ... are made of metal, and the convex portion 13a on the opposite side p-1 , 13a p , 13a p+1 ,.......When it is made of solid dielectric, through the opposite side convex part 13a p-1 , 13a p , 13a p+1 ,.......set length longer than the vibration side convex portion 12a q-1 , 12a q , 12a q+1 , ..., so that the vibration side convex portion 12a q-1 , 12a q , 12a q+1 , ... and the opposite side convex portion 13a p-1 , 13a p , 13a p+1 ,.......can prevent short circuits between metal electrodes.

[0207] The surface of the vibration electrode base (first electrode base) 12 is coated with a vibration side dielectric layer 55. Even if the vibration side dielectric layer 55 is destroyed, there will be a large contact resistance between the dielectric and the metal, and the dielectric also has resistance. Therefore, the opposite side convex portion 13a made of a solid dielectric p-1 , 13a p , 13a p+1 ,.......can play the role of a baffle. In addition, similar to the structure described in the first embodiment, a vibration electrode side convex portion made of an insulating material can be provided at the center position of the vibration electrode side, and a counter electrode side convex portion made of an insulating material can be provided at the center position of the counter electrode side, so that the top of the counter electrode side convex portion collides with the top of the vibration electrode side convex portion, thereby playing the role of a stopper. In this case, if one of the counter electrode side convex portion and the vibration electrode side convex portion is made of an insulator, at least one of them can play a blocking role. In addition, the vibration side convex portion 12aq-1 , 12a q , 12a q+1 , ... are made of metal, and the convex portion 13a on the opposite side p-1 , 13a p , 13a p+1 ,.......When made of solid dielectric material, the length of the opposite convex part near the center of the vibration cavity has a large deflection. Only the length of the opposite convex part of the vibration cavity can play a blocking role, even if its local setting is longer than the vibration convex part.

[0208] Fig.12 is along the orthogonal direction of the corrosive medium channel 152b ( Fig.11 A local cross-sectional view of the XII-XII direction). Fig.12 The structure of the partial cross-sectional view shown in is based on a three-layer structure, that is, a bottom insulating film 52 such as a silicon oxide film is deposited on a component bottom plate 51 such as a single crystal silicon substrate, and a protective film 53 such as a silicon nitride film is deposited on the bottom insulating film 52. The bottom protective film 53 of the electrode is the top layer of the three-layer structure, and the second electrode base 112 and the third electrode base 113 are two of the three segmented electrodes, which are spaced apart and embedded on both sides of the three-layer structure. Fig.11 It can be seen from the plan view that the corrosion medium channel 152b is Fig.12 The dielectric layer 31 covers the second pair of electrode bases 112 and the third pair of electrode bases 113 which are formed separately. p The opposite side dielectric layer 31 bridges both sides of the second pair of electrode bases 112 and the third pair of electrode bases 113. Through the contact hole on the opposite side dielectric layer 31, the opposite side protrusion 13a p The second pair of electrode bases 112 and the third pair of electrode bases 113 are electrically connected to form a partial structure of a portion of the step pair of electrodes (13a p , 112, 113). Fig.12 In the middle, the opposite side convex part 13a p The lower surface of the p Irregular shape of the selective removal film 33 residue on the lower surface. According to the design, the selective removal film 33 residue is an unnecessary structure and can be ignored.

[0209] Fig.13 The cross-sectional structure of the acoustic element of the second embodiment is shown, with emphasis on the structure on the outer periphery of the vibration chamber. Fig.12Similarly, it is based on a three-layer structure, in which a bottom insulating film 52 is deposited on the element substrate 51, and a bottom electrode protection film 53 is further deposited on the top of the bottom insulating film 52. The outermost first vibration side convex portion 12a1 is inserted between the groove formed by the outermost opposite side stepped side wall portion 13a0 and the first pair of side convex portions 13a1, which is the side wall structure of the acoustic element of the first embodiment, and the second vibration side convex portion 12a2 is inserted into the groove inside the first pair of side convex portions 13a1, forming a normal direction capacitor C udv1 , C udv2 and the non-linear capacitance C udh Increase (such as Figure 2E Shown C udv1 , C udv2 and capacitor C udh ).

[0210] The third pair of electrode bases 113 as one of the three segmented electrodes is placed on the pair of electrode bottom protection film 53, and a common driving potential V is applied to the third pair of electrode bases 113 together with the other first pair of electrode bases 111 and the second pair of electrode bases 112. dr For example, the driving potential V dr Can be V dr =30V or more. The third pair of electrode bases 113 may be composed of a conductor such as W. The opposite side stepped side wall portions 13a0 and the first pair of side protrusions 13a1 are arranged above the third pair of electrode bases 113, forming a structure protruding upward from the third pair of electrode bases 113, and they are composed of a low resistivity dielectric (such as a DOPOS film). The acoustic element in the second embodiment illustrates a structure having a protrusion of a conductive material. However, more generally, as described in the sixth embodiment, the opposite side stepped side wall portions 13a0 and the first pair of side protrusions 13a1, etc. may be a dielectric that is an insulator with a resistivity ρ≈∞.

[0211] like Fig.13 As shown, the upper surface of the third pair of electrode bases 113 where the opposite-side stepped sidewalls 13 a 0 and the first pair of side protrusions 13 a 1 are not provided is covered with an opposite-side dielectric layer 31 such as a silicon oxide film. 1212 Similarly, the surfaces of the first vibration side protrusion 12a and the second vibration side protrusion 12a and the bottom surface of the vibration electrode base 12 where the first vibration side protrusion 12a and the second vibration side protrusion 12a are not configured are covered with a vibration side dielectric layer 55 composed of a dielectric film such as a silicon nitride film. The opposite side dielectric layer 54 and the vibration side dielectric layer 55 can be made of various high dielectrics, ferroelectrics, normal dielectrics, etc., as described in the latter part of the basic concept explanation at the beginning of this section. The upper surface of the vibration electrode has a protective film 56, such as a silicon oxide film, which is arranged on the vibration electrode base 12. Fig.13In the example structure of , the sidewall of the cavity includes a composite structure of a sidewall insulating film base layer 21 (e.g., a silicon oxide film) and a sidewall insulating film 22 (e.g., a silicon oxide film) deposited on the sidewall insulating film base layer 21. The sidewall insulating film base layer 21 is deposited on the upper surface of the underlying insulating film 52 in a manner embedded in the third pair of electrode bases 113, while the sidewall insulating film 22 is deposited on the sidewall insulating film base layer 21, including the upper surface of the edge of the third pair of electrode bases 113.

[0212] like Fig.13 FIG. 1 is a schematic cross-sectional view of the outer portion of the vibration chamber 18, showing the first vibration side convex portion 12a1 inserted from above and the waveform-shaped vibration chamber 18 formed by the concave space formed by the outermost opposite side stepped side wall portion 13a0 and the first pair of side convex portions 13a1 as the side wall structure. In addition, Fig.13 The portion of the vibration cavity 18 shown on the right side of the paper is wavy and meandering between the second vibration side convex portion 12a2 inserted from above and the concave space inside the first pair of side convex portions 13a1. As for the overall structure, as shown in FIG. 2, the corresponding vibration side convex portion 12a q-1 , 12a q , 12a q+1 , ... are inserted into the adjacent opposite side protrusions 13a in a nested configuration p-1 , 13a p , 13a p+1 ,........ The concave space between the convex part 13a on the opposite side p-1 , 13a p , 13a p+1 , ....... and vibration side convex portion 12a q-1 , 12a q , 12a q+1 , ...in a nested configuration, a vibration chamber 18 similar to a bellows is formed.

[0213] =Acoustic element manufacturing method according to the second embodiment of the present invention=

[0214] The following will refer to Figures 14A-14IThe manufacturing method of the acoustic element of the second embodiment of the present invention is described. First, a bottom insulating film 52 (such as a silicon oxide film) is formed on an element substrate 51 (such as a single crystal silicon substrate) using a CVD method or the like, and the thickness of the entire surface is about 100nm. Next, a bottom electrode protection film 53 such as a silicon nitride film is formed on the bottom insulating film 52 using a CVD method or the like, and the thickness thereof is about 50nm. In addition, a side wall insulating film bottom layer 21 such as a silicon oxide film is formed on the entire surface of the bottom electrode protection film 53 using a CVD method or the like, and the thickness thereof is about 100nm. Then, a first photoresist film is spin-coated on the entire surface of the side wall insulating film base layer 21, and the first photoresist film is exposed and developed using a photolithography technique to open the pattern of the first embedded groove portion embedded in the third electrode base 113. Using the pattern of the first photoresist film as an etching mask, the side wall insulating film base layer 21 is selectively etched to a desired depth by a dry etching technique (such as RIE), thereby forming a first embedded groove portion.

[0215] like Fig.14A As shown in FIG. 1 , after forming a first conductive film (such as W) to embed the first embedded groove portion using a film forming method (such as a CVD method), the film is polished using a film forming polishing method (such as a CMP method) until the top surface of the protective film 53 on the bottom surface of the counter electrode is exposed. The first conductive film embedded in the first embedded groove becomes the second counter electrode base 112 and the third counter electrode base 113 with a flat main surface. The remaining counter electrode base 111 (which is divided into three parts at other locations but Fig.14A (not shown) is embedded simultaneously with the second pair of electrode bases 112 and the third pair of electrode bases 113.

[0216] Then, if Fig. 14B As shown, a counter-side dielectric layer 31, such as a silicon oxide film, having a thickness of about 50 nm is formed on the entire surface of the sidewall insulating film bottom layer 21 and the third counter electrode substrate 113 using a CVD method or the like. Then, a second photoresist film is spin-coated on the entire surface of the counter-side dielectric layer 31, and the second photoresist film is exposed and developed using a photolithography technique to open a groove pattern for the second inlay. Using the pattern of the second photoresist film as an etching mask, a dry etching technique (such as RIE) is used to selectively etch the counter-side dielectric layer 31 to a desired depth to form a second inlay. Fig. 14C The second setting groove 59 is shown.

[0217] Then, if Fig.14D As shown in FIG. 1 , a second conductive film 32 (eg, W) is formed by a film forming method (eg, CVD method) to embed the second damascene groove 59. The first conductive film and the second conductive film 32 may use the same conductive material. Fig.14EAs shown in FIG. 1 , the reverse side of the dielectric layer 31 is polished by a thin film polishing method (such as a CMP method) until the top surface of the dielectric layer 31 is exposed, and then further etched back. Next, a selective removal film 33 is formed on the entire surface by a CVD method or a similar method, such as Fig.14F As shown, the etching selectivity ratio of the film to a specific etchant is different from that of the opposite dielectric layer 31. When the opposite dielectric layer 31 is a silicon oxide film, a silicon nitride film can be used as the selective removal film 33.

[0218] like Figure 14G As shown, the opposite dielectric layer 31 is planarized by a thin film polishing method (such as a CMP method) until the surface of the opposite dielectric layer 31 is exposed, and then a selective removal film 33 is embedded on the top surface of the W film embedded in the second inlay groove 59. Next, a sidewall insulating film 22, such as a silicon oxide film, is formed on the entire surface of the opposite dielectric layer 31 and the selective removal film 33 by a CVD method or a similar method, with a thickness of about 250-900 nm. Then, a third layer of photoresist film is spin-coated on the entire surface of the top of the sidewall insulating film 22, and the third layer of photoresist film is exposed and developed by a photolithography technique to open the sidewall insulating film 22. Fig.10 The pattern of the sidewall insulating film 22 is shown to remain in the peripheral region. Using the pattern of the third photoresist film as an etching mask, the sidewall insulating film 22 is selectively etched using a dry etching technique (such as RIE) until the top surface of the opposite dielectric layer 31 is exposed.

[0219] Then, a fourth photoresist film is spin-coated on the entire surface of the opposite-side dielectric layer 31, and the fourth photoresist film is exposed and developed using a photolithography technique to form a pattern of contact holes for the second pair of electrode bases 112 and the third pair of electrode bases 113. Using the pattern of the fourth photoresist film as an etching mask, a dry etching technique (such as RIE) is used to selectively etch the opposite-side dielectric layer 31 to form contact holes, exposing a portion of the surface of the second and third pair of electrode bases 112 and 113.

[0220] Then, a dielectric film such as a DOPOS film having a thickness of 250nm-1000nm is deposited on the entire surface by a doping CVD method or the like. Then, a fifth layer of photoresist film is spin-coated on the entire surface on the basis of the dielectric film, and the fifth layer of photoresist film is exposed and developed using a photolithography technique to form a convex shell pattern on the reverse side. The pattern of the fifth layer of photoresist film is used as an etching mask, and the dielectric film is selectively etched to a desired depth using a dry etching technique (such as RIE) to form the opposite side convex portion 13a. p ,like Fig.14H As shown. The opposite side convex portion 13a p The second and third electrode bases 112 and 113 may be electrically connected through contact holes on the dielectric layer 31 on the opposite side. Fig.14HThe opposite side convex portion 13a is shown p At the same time, a plurality of opposite side convex portions 13a are formed in other parts such as the depth of the paper surface. p-1 , 13a p+1 , ... and other patterns are electrically connected to the corresponding first pair of electrode bases 111 , second pair of electrode bases 112 and third pair of electrode bases 113 via contact holes provided in the opposite-side dielectric layer 31 .

[0221] Then, on the plurality of opposite side protrusions 13a p-1 , 13a p+1 ,.......spin-coat the sixth photoresist film on the entire surface of the opposite dielectric layer 31 and the sidewall insulating film 22, and apply the sixth photoresist film to the mask using photolithography technology to form a window, selectively opening the area above the etching medium channels 151b, 152b and 153b. Use the pattern of the sixth photoresist film as an etching mask, use dry etching technology (such as RIE) to selectively etch a portion of the opposite dielectric layer 31 until a window is formed, exposing the pattern on the top surface of the film 33 for selective removal in the window. In addition, on the plurality of opposite convex portions 13a p-1 , 13a p+1 A seventh photoresist film is spin-coated on the entire surface of the sidewall insulating film 22, and the seventh photoresist film is applied to the pipe end portions 141b, 142b, and 143b as a mask having a hole pattern using a photolithography technique.

[0222] The pattern of the seventh photoresist film is used as an etching mask, and the sidewall insulating film 22 is selectively etched using a dry etching technique (such as RIE) until the top surface of the selective removal film 33 is exposed. Next, when the entire surface is etched using a hot phosphoric acid (H3PO4) solution, the selective removal film 33 embedded in the second embedding groove 59 is selectively removed, and the selective removal film 33 is selectively removed on the plurality of opposite side protrusions 13a. p-1 , 13a p , 13a p+1 , ........, the surface of the embedded second conductive film 32 between the patterns is exposed. Even if there is a deviation in the mask alignment in the photolithography process using the sixth photoresist film, the desired area on the upper part of the etching medium channel 151b, 152b, 153b can be selectively opened by the selective removal process using the selective removal film 33. In addition, the selective removal film 33 exposed at the bottom of the pipe end 141b, 142b, 143b can also be selectively removed.

[0223] Then, using a CVD method or the like, a sacrificial film 16 made of a thin film of a material having sacrificial etching adaptability (such as W) is deposited on the entire surface to a thickness of about 20-200 nm and Fig.6DAs shown in FIG. 1 , a plurality of opposite side protrusions 13a p-1 , 13a p , 13a p+1 ,......., the pattern is vertical steps along the side wall covering the side wall. Fig.14I The manner in which the sacrificial film 16 is deposited along the vertical sidewalls of the opposite side protrusions is also schematically shown. With the complete deposition of the sacrificial film 16, the wells at the open channel ends 141b, 142b and 143b in the peripheral sidewall insulating film 22 are also blocked and filled.

[0224] Furthermore, a vibration-side dielectric layer 55 composed of a dielectric film such as a silicon nitride film is formed on the entire surface of the sacrificial film 16 by using a CVD method or the like, and the thickness thereof is about 50 nm. Fig.6D The same as shown in . Next, using a CVD method or the like, a third conductive film (such as a W film) with a thickness of about 100 nm is formed on the entire surface of the vibration side dielectric layer 55 so as to completely fill the grooves in the vibration side dielectric layer 55. Then, an eighth photoresist film is spin-coated on the entire surface to cover the third conductive film, and exposure and development are performed to selectively expose the position of the top surface of the opposite side dielectric layer 31 in the peripheral area. The pattern of the eighth photoresist film is then used as an etching mask, and the third conductive film is selectively etched by a dry etching technique (such as RIE) to expose the top surface of the vibration side dielectric layer 55 located on the top surface of the opposite side dielectric layer 31 in the peripheral part. After removing the eighth photoresist film, the third conductive film is etched again. After etching, the pattern of the first vibration side convex portion 12a1 and the second vibration side convex portion 12a2 is formed, which is the same as Figure 1 The same structure as shown in E.

[0225] After etching, a fourth conductive film, such as a W film, having a thickness of about 100 nm is formed on the entire surface using CVD or the like, and the conductive film is located on the vibration side dielectric layer 55 and on the first vibration side convex portion 12a1 and the second vibration side convex portion 12a2 of the inner and outer peripheries. Then, a ninth photoresist film is spin-coated on the entire surface to cover the fourth conductive film, and exposure and development are performed to selectively expose the position of the top surface of the dielectric layer 31 on the opposite side of the periphery. Then, using the pattern of the ninth photoresist film as an etching mask, the fourth conductive film is selectively etched by dry etching technology (such as RIE) to expose the top surface of the vibration side dielectric layer 55 located on the top surface of the dielectric layer 31 on the opposite side of the peripheral portion. Therefore, as Fig.13 As shown, a planar vibrating electrode base 12 having a flat main surface in a non-vibrating state is formed, which is connected to the upper end of the first vibration side convex portion 12a1 and the upper end of the second vibration side convex portion 12a2, respectively.

[0226] Next, a vibration electrode protection film base layer having a thickness of about 50 nm is formed on the entire surface of the vibration electrode by using a CVD method or the like, such as a silicon oxide film formed on the vibration side dielectric layer 55 and the vibration electrode base 12. A tenth layer of a photoresist film is spin-coated on the entire surface to cover the vibration electrode protection film base layer, such as Fig.10 As shown, a mask whose pattern of the hole for forming the cavity matches the pattern of the pipe end portions 141b, 142b, and 143b is exposed and developed. Then, using the pattern of the 10th layer of the photoresist film as an etching mask, selective etching is performed by dry etching techniques such as RIE to penetrate the vibration electrode protection film base layer and the 55 vibration side dielectric layer. Fig.10 As shown, holes for forming cavities are opened in the channel ends 141b, 142b, 143b by selective etching, and these cavities can reach the surface of the sacrificial film 16 embedded in the form of a plug.

[0227] When a corrosive medium such as hydrogen peroxide solution is introduced as an etchant through the cavity forming hole, the corrosive medium is introduced into the corrosive medium channels 151b, 152b, 153b, which are connected by Fig.10 The pipe ends 141b, 142b, 143b shown are arranged in a three-dimensional structure in the lower layer. Therefore, the sacrificial film 16 will be etched away by the corrosive medium (etchant). When the sacrificial film 16 is etched away, as shown in FIG. Fig.12 and Fig.13 As shown, a vibration cavity 18 is formed between the third pair of electrode bases 113, the driving side wall pair of electrodes 13a0 and the first pair of side protrusions 13a1 and the vibration electrode base 12, the first vibration side protrusion 12a1 and the second vibration side protrusion 12a2.

[0228] If the etching medium is a liquid, such as a hydrogen peroxide solution, after the sacrificial film 16 removal process is completed, the etching medium is moved to a cleaning process using a cleaning solution. After the cleaning process is completed, the cleaning solution is dried by IPA steam drying or other methods. During the drying process of the cleaning solution, vacuum heat treatment can be combined to make the convex portion 13a p-1 , 13a p , 13a p+1,.......siliconized and alloyed with the first pair of electrode bases 111, the second pair of electrode bases 112 and the third pair of electrode bases 113. After the cleaning solution is dried, a thin film deposition technique under reduced pressure such as reduced pressure CVD, plasma CVD or vacuum deposition is used to deposit a main protective layer on the entire surface with a thickness of 150-1000nm on the base layer of the vibration electrode protection film. The main protective layer is the remaining part of the vibration electrode top protection film 56. By depositing the main protective layer on the bottom layer of the vibration electrode protection film under reduced pressure, a plug can be set at the entrance of the cavity forming hole, and the vibration cavity 18 can be vacuum sealed. For example, using He gas as the main carrier gas, the main protective layer is deposited by reduced pressure CVD, so that the interior of the vibration cavity 18 is in a reduced pressure state of about 1kPa, and the entrance of the cavity forming hole is blocked. The composite film of the lower layer of the vibration electrode protection film and the main protective layer constitutes Fig.13 The protective film 56 on the upper surface of the vibration electrode is shown to complete the acoustic element of the second embodiment.

[0229] (Variation of the Second Embodiment)

[0230] In the description of the acoustic element of the second embodiment, as Figure 3-Figure 5 As shown, the acoustic element with an initial crossover rate of 0% has greater stored electrical energy and greater transmitted acoustic energy than the acoustic element with an initial crossover rate of 50%. Figure 6A-6H In the acoustic element manufacturing method of the first embodiment shown, there is a problem that the structure at the end of the manufacturing process has an initial crossover rate exceeding 50%. In the following manufacturing method of the acoustic element according to the variation of the second embodiment, it is described that the W film and the film 33 for selective removal are embedded in the above Figure 14G After the process in the second setting groove 59 shown, the initial crossover can be 0% at the end of the manufacturing process.

[0231] That is to say, Fig.15A Shown in Figure 14G After the process shown, the contact hole 31c is opened on the opposite dielectric layer 31 using the pattern of the fourth photoresist film as an etching mask to expose a portion of the upper surface of the first pair of electrode bases 111 which is one of the three-part pair of electrode base parts. Fig. 15B A state is shown in which a dielectric film 13p (eg, DOPOS film) is deposited on the entire surface of the counter-side dielectric layer 31 so that the dielectric film 13p is electrically connected to a portion of the upper surface of the first counter electrode base 111 through the contact hole 31c.

[0232] In the method for manufacturing an acoustic element according to a modification of the second embodiment, Fig. 15CAs shown, a first sacrificial film 16a having a sacrificial etching suitability such as W is further deposited on the entire surface of the dielectric film 13p by a film forming method such as a CVD method, and its vertical block height is h. Then, a fifth photoresist film is spin-coated on the entire surface of the first sacrificial film 16a, and the fifth photoresist film is exposed and developed using a photolithography technique to form a pattern of the opposite side protrusion (second electrode side protrusion). Using the pattern of the fifth photoresist film as an etching mask, the first sacrificial film 16a and the dielectric film 13p are etched using a highly directional dry etching technique (such as RIE) until the top surface of the opposite side dielectric layer 31 is exposed, as shown in FIG. Fig.15D As shown, a convex portion 13a having a vertical side wall is formed. p-2 , 13a p-1 , 13a p , 13a p+1 When the fifth photoresist film is used for selective etching, the first sacrificial film 16a and the dielectric film 13p on the peripheral area sidewall insulating film are also removed.

[0233] Then, on the plurality of opposite side convex portions 13a p-1 , 13a p , 13a p+1 , ......., the sixth photoresist film is spin-coated on the entire surface of the opposite dielectric layer 31 and the sidewall insulating film 22, and the sixth photoresist film is used as the Fig.10 and Fig.11 The mask of the upper opening of the etching medium channels 151b, 152b, and 153b is used. The pattern of the sixth photoresist film is used as an etching mask, and the opposing dielectric layer 31 is etched using a dry etching technique (such as RIE) until an opening is selectively opened to expose the top surface of the film 33 for selective removal. In addition, on the plurality of opposite side protrusions 13a p-1 , 13a p+1 ,......., the seventh photoresist film is spin-coated on the entire surface of the opposite dielectric layer 31 and the side wall insulating film 22, and the seventh photoresist film is applied to the pipe ends 141b, 142b, 143b, 143b as a mask with a hole pattern by photolithography. The pattern of the seventh photoresist film is used as an etching mask, and the side wall insulating film 22 is selectively etched by dry etching technology until the top surface of the film 33 for selective removal is exposed, and vertical holes (wells) of the pipe ends 141b, 142b, 143b are dug on the side wall insulating film 22.

[0234] Next, hot phosphoric acid solution is used to perform full surface etching to selectively remove the plurality of side protrusions 13a. p-1 , 13a p , 13a p+1The selectively removed film 33 is exposed in the opening of a portion of the opposite dielectric layer 31 at the bottom of the concave pattern formed. Due to the selective removal of the film 33, the surface of the second conductive film 32 embedded in the second inlay groove 59 is exposed to the plurality of opposite convex portions 13a. p-1 , 13a p , 13a p+1 ,.......a portion of the bottom of the concave pattern formed. Even if there is a slight deviation in mask alignment during the photolithography process of the exposed top surface of the selective removal film 33, the desired area on the top of the etching medium channel 151b, 152b, 153b can be selectively opened by the selective removal process using the selective removal film 33. In addition, the selective removal film 33 exposed at the bottom of the pipe terminal 141b, 142b, 143b is also selectively removed.

[0235] Next, highly directional thin film deposition techniques such as ultra-high vacuum electron beam deposition or molecular beam deposition are used, such as Fig.15E As shown, it is not attached to the opposite side convex portion 13a p-2 , 13a p-1 , 13a p , 13a p+1 , ..., on the vertical side wall, on the opposite side convex portion 13a p-2 The opposite side convex part 13a p-1 The groove bottom and the opposite side convex part 13a p-1 The opposite side convex part 13a p The groove bottom and the opposite side convex part 13a p The opposite side convex part 13a p+1 The second sacrificial film 16b is deposited vertically at the bottom of the groove between the first and second sacrificial films 16a and 16b. The first sacrificial film 16a and the second sacrificial film 16b should be made of materials with almost the same etching characteristics for the same etchant. Fig.15E In the highly directional vertical deposition technology shown in FIG. 1 , if the convex portion 13a on the opposite side p-2 , 13a p-1 , 13a p , 13a p+1 ,.......forms an eave (overhang), then the deposit shape at the bottom of the groove in the cross-sectional view is a trapezoid. One factor in the formation of the eaves is the accumulation of charge on the deposits, so the second pair of electrode bases 112 are grounded to prevent the deposits from being charged. In addition, while back etching is used, the formation of the eaves can also be prevented. The second sacrificial film 16b is also deposited in the vertical holes of the pipe ends 141b, 142b, 143b that penetrate the sidewall insulating film 22, but the cross-sectional shape of the deposits in the pipe ends 141b, 142b, 143b can be a trapezoid.

[0236] Fig.15EThe highly directional vertical deposition technique shown, the cornice removal process is repeatedly implemented, such as Fig.15F As shown, on the opposite side convex portion 13a p-2 The opposite side convex part 13a p-1 The groove bottom between the two sides and the convex part 13a on the opposite side p-1 The opposite side convex part 13a p The groove bottom between the two sides and the convex part 13a on the opposite side p The opposite side convex part 13a p+1 On the bottom of the groove between ..., the second sacrificial film 16b is deposited with a vertical volume h2 orientation. p-2 , 13a p-1 , 13a p , 13a p+1 , ..., the upper end of the second sacrificial film 16b is also deposited with a vertical volume h2, so when the designed vertical volume h2 is reached, the side convex portion 13a is removed by CMP or other methods. p-2 , 13a p-1 , 13a p , 13a p+1 Then, a good film forming method such as reduced pressure CVD, etc., is used to form a step cover layer. Figure 15G As shown, the third sacrificial film 16 c is deposited on the entire surface in such a manner that the gap thickness Δ=20 to 100 nm.

[0237] The gap thickness Δ is determined by the position of the opposite convex portion 13a. p-2 , 13a p-1 , 13a p , 13a p+1 , ....... and the vibration side convexities (first electrode side convexities) 12a respectively opposite thereto q-2 , 12a q-1 , 12a q , 12a q+1 ,........ The first sacrificial film 16a, the second sacrificial film 16b and the third sacrificial film 16c must be thin films of materials with chemical properties that have almost the same etching selectivity to the same etchant, even though the deposition techniques may be different. The complete deposition of the third sacrificial film 16c will also block the tops of the wells of the pipe ends 141b, 142b, 143b opened in the peripheral sidewall insulating film 22.

[0238] In addition, if Figure 15GAs shown, a vibration side dielectric layer 55 composed of a dielectric film such as a silicon nitride film is formed on the entire surface of the third sacrificial film 16c using a CVD method or the like, and the thickness thereof is about 50nm. A third conductive film (such as a W film) having a thickness of about 100nm is continuously formed on the entire surface of the vibration side dielectric layer 55 by a CVD method or the like to completely fill the grooves in the vibration side dielectric layer 55. In addition, an eighth layer of photoresist film is spin-coated on the entire surface to cover the third layer of conductive film, and exposure and development are performed to selectively expose the position of the top surface of the opposite side dielectric layer 31 in the peripheral area. The pattern of the eighth photoresist film is then used as an etching mask, and the third conductive film is selectively etched by dry etching technology to expose the top surface of the vibration side dielectric layer 55 located on the top surface of the dielectric layer 31 on the opposite side of the peripheral part. After removing the eighth layer of photoresist film, the third layer of conductive film is etched back.

[0239] After etching, a fourth conductive film, such as a W film, is formed on the entire surface of the vibration side dielectric layer 55 and the third conductive film using a CVD method or the like, with a thickness of about 100 nm. Furthermore, the pattern of the ninth photoresist film is used as an etching mask, and the fourth conductive film is selectively etched by dry etching technology, so that the top surface of the vibration side dielectric layer 55 is exposed on the top surface of the opposite side dielectric layer 31 located in the peripheral area. In this way, the process is completed as shown in FIG. Fig.15I The structure of the step-type vibration electrode 12p is shown. Fig.15J As shown, the step vibration electrode 12p includes a plate-shaped vibration electrode base (first electrode base) 12 and a plurality of vibration side protrusions 12a suspended on the lower surface of the vibration electrode base 12. q-2 , 12a q-1 , 12a q , 12a q+1 ,........ Then, a tenth photoresist film is spin-coated on the entire surface to cover the step counter electrode 12p, and exposure and development are performed to selectively expose the position on one side of the upper surface of the peripheral counter-side dielectric layer 31.

[0240] Next, a vibration electrode protection film base layer such as a silicon oxide film with a thickness of about 50 nm is formed on the vibration-side dielectric layer 55 and the vibration electrode substrate 12 by using a CVD method or the like. Fig.10 As shown, the 10th layer of photoresist film is spin-coated on the entire surface to cover the vibration electrode protection film base layer, and is exposed and developed through a mask matching the pattern of the pipe ends 141b, 142b and 143b to form the pattern of the cavity hole. The pattern of the 10th layer of photoresist film is then used as an etching mask to selectively etch the vibration electrode protection film base layer and the 55 vibration side dielectric layer by dry etching technology. Fig.10 As shown, holes are selectively etched to form cavities, reaching the surface of the third sacrificial film 16c embedded in the conduit ends 141b, 142b, 143b.

[0241] When a corrosive medium such as a hydrogen peroxide solution is introduced as an etchant through the cavity forming hole, the corrosive medium passes through Fig.10 The pipe ends 141b, 142b, 143b shown enter the corresponding corrosive medium channels 151b, 152b, 153b respectively. As a result, the first sacrificial film 16a, the second sacrificial film 16b and the third sacrificial film 16c are etched away by the corrosive medium (etchant). After the first sacrificial film 16a, the second sacrificial film 16b and the third sacrificial film 16c are etched away, Fig.15J The first pair of electrode bases 111 and the side protrusions 13a are shown p-2 , 13a p-1 , 13a p , 13a p+1 , ....... and the vibration electrode base 12, the vibration side convex portion 12a q-2 , 12a q-1 , 12a q , 12a q+1 , .... a vibration cavity 18 is formed between them. The subsequent steps have been introduced above and will not be repeated here.

[0242] According to the acoustic element manufacturing method of the second embodiment of the modification, Fig.15J As shown, by adjusting the vertical volume height h1 of the first sacrificial film 16a, the vertical volume height h2 of the second sacrificial film 16b, and the gap thickness Δ of the third sacrificial film 16c, an initial crossover of 0% can be achieved at the end of the manufacturing process. By reducing the initial crossover amount of the structure at the end of the manufacturing process stage, the stored electrical energy and transmitted acoustic energy can be increased.

[0243] (Third Embodiment)

[0244] The acoustic element integrated circuit of the third embodiment of the present invention is different from the acoustic element integrated circuit described in the first embodiment. Figure 1 Similarly, in the element array section, the X (i-1),(j+1) , X i,(j+1) , X (i+1),(j+1) , …, X (i-1),j , X i,j , X (i+1),j , …, X (i-1),(j-1) , X i,(j-1) , X (i+1),(j-1) , etc., are arranged on the same plane to form a two-dimensional matrix layout. Fig.17A As shown, focusing on the structure of the stepped vibration electrode, the stepped vibration electrode of the acoustic element of the third embodiment has a plurality of wall-shaped vibration side protrusions (first electrode side protrusions) 14a. q-2 , 14a q-1 , 14a q , 14aq+1 , ..., they form multiple concentric hexagonal rings in a cavity, and their plane pattern is a regular hexagon, arranged at a constant pitch, with equal spacing (in Fig.17A In the vibration side convex part 14a q-2 , 14a q-1 , 14a q , 14a q+1 , ... are omitted. ). However, as an example, it is not always necessary to construct a plurality of concentric hexagonal rings with the same gap and constant pitch. By making the gaps and pitches of the plurality of concentric hexagonal rings uneven, the frequency bandwidth of the acoustic element integrated circuit of the third embodiment can be widened. q-2 , 14a q-1 , 14a q , 14a q+1 , ... respectively have vertical side walls parallel to the vibration direction, and Fig.16 The cross-sectional structures of the outermost first vibration side protrusion 14a1 and the second vibration side protrusion 14a2 in the cross-sectional view of the structure close to the side wall insulation film 22 are the same.

[0245] like Fig.17A As shown, a plurality of vibration side protrusions 14a q-2 , 14a q-1 , 14a q , 14a q+1 , ...are suspended under the array of the first vibration electrode base 185, the second vibration electrode base 186 and the third vibration electrode base 187 which are divided into three parts, and are arranged in an electrically connected manner. The structural features are similar to Figure 2B The acoustic element of the first embodiment shown in FIG. 1 is provided on a single vibration electrode base 12. In the acoustic element of the third embodiment, three flat-plate-shaped first vibration electrode bases 185, second vibration electrode bases 186, and third vibration electrode bases 187 are divided into three parts, have the same potential, and have flat main surfaces, and a plurality of vibration side protrusions 14a suspended and connected on the lower surfaces of the three first vibration electrode bases 185, second vibration electrode bases 186, and third vibration electrode bases 187. q-1 , 14a q , 14a q+1 The overall structure of , ... is called a "step-type vibration electrode". However, the three-division is just a simple example, and other divisions such as two-division or four-division or more may also be used.

[0246] like Fig.17A As shown, the plurality of vibration side convex portions 14a q-2 , 14a q-1 , 14a q , 14a q+1, ..., each of which is sandwiched by a gap, to form a plurality of wall-shaped opposite side protrusions (second electrode side protrusions) 14a of another plurality of concentric hexagonal rings. p-2 , 14a p-1 , 14a p , 14a p+1 , ....... have equal intervals, are arranged at a certain pitch, and are in contact with a plurality of vibration side convex portions 14a q-2 , 14a q-1 , 14a q , 14a q+1 , ... forming a cross-sectional structure, the structure is the same as that of the acoustic element of the first embodiment ( Fig.17A This is a schematic diagram centered on the stepped vibration electrode, so the opposite side convex portion 14a is omitted. p-2 , 14a p-1 , 14a p , 14a p+1 ,.......picture). Fig.16 The cross-sectional view shows the outermost pair of stepped side wall portions 14a0 and the first pair of side convex portions 14a1 on the inner side thereof, but the other pair of side convex portions 14a p-2 , 14a p-1 , 14a p , 14a p+1 ,.......'s respective structures are also Fig.16 The structure of the insulating film 22 near the side wall is the same, and has a vertical side wall parallel to the vibration direction.

[0247] In the acoustic element of the first embodiment, the corrosion medium passages 151, 152, 153 for introducing the corrosion medium when forming the vibration cavity and the plurality of side protrusions 11a are connected. p-1 , 11a p , 11a p+1 , ... are arranged on the same horizontal plane, i.e., a flat-top structure. In contrast, in the acoustic element of the third embodiment, Fig.16 , Fig.17A and Fig. 17B As shown in FIG. 1 , the three first etching medium passages 175b, the second etching medium passages 176b and the third etching medium passages 177b for introducing the etching medium are arranged on the same horizontal plane as the first vibration electrode base 185, the second vibration electrode base 186 and the third vibration electrode base 187, and are different from the acoustic element in the first embodiment because they are a three-dimensional structure formed on the top surface of the vibration cavity 18. The three separated first vibration electrode bases 185, the second vibration electrode bases 186 and the third vibration electrode bases 187 are at the same potential and have a flat plate shape with a flat main surface.

[0248] By configuring three first corrosion medium channels 175b, second corrosion medium channels 176b and third corrosion medium channels 177b on the ceiling above the vibration chamber 18 to form a three-dimensional structure, the number of the first corrosion medium channels 175b, second corrosion medium channels 176b and third corrosion medium channels 177b is increased to four or more, and the conductivity of the fluid can be improved. In addition, even in the case where the spider web is densely arranged, the plurality of vibration side protrusions 14a q-2 , 14a q-1 , 14a q , 14a q+1 , ... and the opposite side convex portion 14a p-1 , 14a p , 14a p+1 ,........ can avoid reducing the length of the surface. That is, even if the vibration side convex portion 14a q-2 , 14a q-1 , 14a q , 14a q+1 , ... and the opposite side convex portion 14a p-1 , 14a p , 14a p+1 ,.......In the microstructure arranged at a spacing of 400nm within a cavity width of 120μm, by increasing the number of the first corrosion medium channel 175b, the second corrosion medium channel 176b and the third corrosion medium channel 177b and the cross-sectional area of ​​the fluid channel configured in the ceiling, a bellows-shaped vibration cavity can also be effectively formed and the reduction of the opposite side length can be avoided.

[0249] exist Figure 2E and Figure 6C In the acoustic element of the first embodiment shown in FIG. 1 , the vibration-side dielectric layer 55 covers the surface of the vibration electrode base 12 and the vibration-side convex portion 12a. q-1 , 12a q , 12a q+1 , ... In contrast, in the acoustic element of the third embodiment, as Fig.16 and Fig. 17B As shown, the vibration side convex portion 14a q-2 , 14a q-1 , 14a q , 14a q+1 , ... is composed of a low resistivity dielectric (such as a semiconductor doped with impurities), the vibration side convex portion 14a q-2 , 14a q-1 , 14a q , 14a q+1 The surfaces of , ... are exposed inside the vibration cavity 18, which is similar to Figure 2EIn addition, the acoustic element in the third embodiment exemplifies a structure having a conductive convex portion, but more generally, the vibration side convex portion 14a q-2 , 14a q-1 , 14a q , 14a q+1 , ..., etc., as described in the sixth embodiment, are dielectrics of an insulator having a resistivity ρ≈∞.

[0250] Fig.16 The normal direction capacitor C is omitted udv1 , C udv2 and the non-linear capacitor C udh The symbol, but Figure 2E As shown, the surfaces of the opposite step side wall portion 11a0 and the first pair of side convex portions 11a1 and the surfaces of the first vibration side convex portion 14a1 and the second vibration side convex portion 14a2 induce true charges that become the starting point and the end point of the electric line of the vibration cavity 18 according to Gauss's law, forming a normal direction capacitor C udv1 , C udv2 and the non-linear capacitor C udh . Normal direction capacitor C udv1 , C udv2 It means that the electric field lines extend in the normal direction of the main surfaces of the first electrode base (vibrating electrode base) 12 and the second electrode base (opposite electrode base) 11. Fig.16 In the non-linear direction, the capacitor C udh The direction in which the electric lines of force extend is perpendicular to the electric lines of force in the normal direction of the main surfaces of the first and second electrode bases.

[0251] That is, as described above, in the present invention, the portion that induces positive charge and negative true charge on the surface of the area with different potentials relative to each other according to Gauss's law is defined as an "electrode". Therefore, since the low-resistivity dielectric surface that forms the convex portion with the same potential electrically connected to the first vibration electrode base 185, the second vibration electrode base 186, and the third vibration electrode base 187 respectively induces true charge according to Gauss's law, the "vibration side convex portion" is equivalent to a component that functions as a part of the electrode. Although omitted in the figure, the side convex portion 11a p-2 , 11a p-1 , 11a p , 11a p+1 , ... are made of metal. On the vibration side convex portion 14a q-2 , 14a q-1 , 14a q , 14a q+1 , ... is made of solid dielectric, and the opposite side protrusion 11a p-2 , 11a p-1 , 11a p, 11a p+1 , ... When the vibration side convex portion 14a is made of metal, q-2 , 14a q-1 , 14a q , 14a q+1 , ... is set to be longer than the opposite side protrusion 11a p-2 , 11a p-1 , 11a p , 11a p+1 , ... long, can prevent the vibration side convex portion 14a q-2 , 14a q-1 , 14a q , 14a q+1 , ... opposite side protrusions 11a p-2 , 11a p-1 , 11a p , 11a p+1 ,...the metal electrodes are short-circuited to each other.

[0252] The surface of the counter electrode base (second electrode base) 11 is coated with a counter dielectric layer 54, but even if the counter dielectric layer 54 is destroyed, there is still a large contact resistance between the dielectric and the metal, and the dielectric also has resistance. Therefore, the vibration side convex portion 14a made of a solid dielectric q-2 , 14a q-1 , 14a q , 14a q+1 , ... can play the role of a baffle. Similar to the structures described in the first and second embodiments, a vibration electrode side convex portion of an insulator can be set at the center position of the vibration electrode side, and an opposite electrode side convex portion of an insulator can be set at the center position of the opposite electrode side, so that the top of the opposite electrode side convex portion collides with the top of the vibration electrode side convex portion, playing the role of a stopper. In this case, if the opposite electrode side convex portion and the vibration electrode side convex portion are composed of an insulator, at least one of them can play a blocking role. In addition, when the vibration side convex portion 14a q-2 , 14a q-1 , 14a q , 14a q+1 , ... are made of solid dielectric, and the side convex portion 11a p-2 , 11a p-1 , 11a p , 11a p+1 , ...When it is made of metal, even if the length of the vibration-side convex portion near the center of the vibration cavity with large deflection is set longer than the local opposite-side convex portion, it can still play a blocking role.

[0253] Fig.16The cross-sectional structure of the acoustic element of the third embodiment is shown, with the focus on the peripheral side structure of the vibration chamber. That is, the outermost first vibration side convex portion 14a1, which becomes the side wall structure, is inserted between the groove formed by the outermost opposite side step side wall portion 11a0 and the first pair of side convex portions 11a1, and the second vibration side convex portion 14a2 is inserted into the groove on the inner periphery of the first pair of side convex portions 11a1, so as to increase the normal direction capacitor C udv1 , C udv2 and the non-linear capacitor C udh (C udv1 , C udv2 And quantity C udh Reference Figure 2E ).like Fig.16 As shown, the opposite side stepped side wall 11a0 exposed to the partial surface of the vibration cavity 18 and the surface of the first pair of side protrusions 11a1, as well as the top surface of the opposing electrode base 11 where the opposite side stepped side wall portion 11a0 and the first pair of side protrusions 11a1 are not located, are covered by an opposite side dielectric layer 54 composed of a dielectric film such as a silicon nitride film.

[0254] On the other hand, the surfaces of the first vibration side protrusion 14a1 and the second vibration side protrusion 14a2 formed of solid dielectric are exposed, and in the area where the first vibration side protrusion 14a1 and the second vibration side protrusion 14a2 are not arranged, the bottom surface of the third vibration electrode base 187 is covered by the vibration side dielectric layer 55 composed of a dielectric film such as a silicon nitride film. The opposite side dielectric layer 54 and the vibration side dielectric layer 55 can be various high dielectrics, ferroelectrics, normal dielectrics, etc., as described in the latter part of the basic concept at the beginning of this section. A protective film 56 of the top surface of the vibration electrode, such as a silicon oxide film, is arranged on the third vibration electrode base 187. The side wall insulation film base 21 is deposited on the upper surface of the bottom insulation film 52 in a manner of embedding the opposite electrode base 11, and the side wall insulation film 22 is deposited on the side wall insulation film base 21, including the upper surface of the edge of the opposite electrode base 11. Fig.16 The focus is on the third vibration electrode base 187, even if Fig.16 Area not shown, but from Fig.17A and Fig. 17B As can be seen in FIG. 1 , the lower surfaces of the first and second vibration electrode bases 185 and 186 are also coated with the vibration-side insulating layer 55 .

[0255] Fig. 17B is along the orthogonal direction of the second corrosive medium channel 176b ( Fig.17A In other words, Fig. 17B The qth vibration side convex portion 14a is q A cross-sectional view with the center at . Fig.17A In the example, the q-th vibration side convex portion 14a q The hexagonal ring is formed by the qth opposite side protrusion 11aq As concentric hexagonal rings, the qth pair of side protrusions 11a q Not shown in the plan view. Fig. 17B In the cross-sectional view, around the q-th vibration side convex portion 14a q The qth relative side convexity 11a q Appears on the lower side of the paper. Fig.16 As shown, although not on the paper surface, it is on the q-th side convex portion 11a. q There is a three-layer structure below, in which the element substrate 51, the bottom insulating film 52 and the protective film 53 for the bottom surface of the electrode are deposited. Fig.16 In the figure, the qth pair of side protrusions 11a are shown. q The top surface of the first pair of side protrusions 14a1 is covered with a dielectric layer 54 on the opposite side, and Fig. 17B In the figure, the qth pair of side protrusions 11a are shown. q The top surface of the paper is covered with a dielectric layer 54 on the opposite side, and the two sides of the qth opposite side convex portion 11a are separated. q It is a whole structure connected together.

[0256] The second corrosion medium channel 176b is one of the three medium channels and is disposed on the qth vibration side convex portion 14a in the vibration cavity 18. q On the same level as the second etching medium channel 176b, among the three segmented vibration electrode bases on both sides of the second etching medium channel 176b, the second vibration electrode base 186 and the third vibration electrode base 187 are separated from each other. Fig.17A As can be seen from the plan view in FIG. 1 , between the second vibration electrode base 186 and the third vibration electrode base 187, the second corrosion medium channel 176b is perpendicular to Fig. 17B The vibration-side dielectric layer 55 covers the bottom surfaces of the second vibration electrode base 186 and the third vibration electrode base 187 formed separately. Fig.17A It can be inferred that in Fig. 17B The back side of the paper surface, the qth vibration side convex part 14a q The q-th vibration side protrusion 14a is connected to the lower surfaces of the second vibration electrode base 186 and the third vibration electrode base 187. q The lower surfaces of the second vibration electrode base 186 and the third vibration electrode base 187 are electrically connected via contact holes in the vibration-side dielectric layer 55 covering the lower surfaces of the second vibration electrode base 186 and the third vibration electrode base 187. q The second vibration electrode base 186 and the third vibration electrode base 187 constitute a part of the stepped vibration electrode (14a q, 186, 187).

[0257] =Method for manufacturing acoustic element according to the third embodiment=

[0258] Fig.18A In the description of the method for manufacturing the acoustic element showing the first embodiment, Fig.6D The stage of the process shown in FIG. 18 is a state where the sacrificial film 16 is deposited on the opposite dielectric layer 54 to a thickness of about 20-100 nm. As shown in FIG. 18a, the opposite dielectric layer 54 and the sacrificial film 16 are formed along the opposite convex portion 11a. p The concave and convex shapes are formed by patterns, and the concave parts are sandwiched between the convex parts 11a on both sides. p As in the method for manufacturing the acoustic element of the first embodiment, thereafter, Fig.18B As shown, by using the fifth photoresist film and the photolithography process of the dry etching technology, the top surface of the opposite side dielectric layer 54 located on the top surface of the peripheral side wall insulating film 22 is exposed, and then using the doping CVD method, etc., as shown in FIG. Fig.18B As shown, a dielectric film 19, such as a DOPOS film, having a thickness of about 250 nm to 1000 nm is formed on the entire surface of the sacrificial film 16 and the opposite dielectric layer 54. Fig.18B As shown, the opposite side dielectric layer 54, the sacrificial film 16 and the dielectric film 19 are connected along the opposite side protrusion 11a. p The concave-convex shape formed by the pattern of the like forms a concave shape in the center, and the dielectric film 19 is embedded in the convex parts 11a on both sides. p The concave part between the patterns.

[0259] Subsequently, the surface of the sacrificial film 16 is flattened by CMP or other techniques until the surface is exposed, and then the dielectric film 19 is embedded in the groove formed by the sacrificial film 16, and the vibration side convex portion 14a is cut out. q Although omitted in the figure, the other vibration side convex portion 14a q-2 , 14a q-1 , 14a q+1 , ..., etc. are formed in the same way. Fig. 18C As shown, a vibration side dielectric layer 55 (eg, silicon nitride film) having a thickness of about 50 nm is formed on the entire surface of the sacrificial film 16 by using a CVD method or the like, covering the vibration side convex portion 14a. q-2 , 14a q-1 , 14a q , 14a q+1 ,…pattern. Fig. 18C The stages of the process cross-sectional view shown correspond to the stages of the process cross-sectional view described in the method for manufacturing the acoustic component of the first embodiment. Fig.6D The state of the cross-section diagram is shown.

[0260] Subsequently, a sixth photoresist film is spin-coated on the entire surface to cover the vibration side dielectric layer 55, and exposure and development are performed to form a pattern of the corrosive medium channel and the contact hole. The pattern of the sixth photoresist film is then used as an etching mask to selectively etch the vibration side dielectric layer 55 by dry etching technology to selectively expose the vibration side convex portion 14a. q Part of the top surface, such as Fig.18D As shown. Fig.18D Other vibration side convex parts 14a not shown q-2 , 14a q-1 , 14a q+1 , ..., and similarly, selectively expose a portion of the top surface. Fig.18D Although not shown in the figure, a contact hole is formed in the vibration side dielectric layer 55, which is located at the vibration side convex portion 14a on the far side of the paper. q on the top surface. Fig.18E As shown, after removing the sixth photoresist film, a third conductive film 191, such as a W film, is formed on the entire surface with a thickness of 100-1000nm. Fig.18D Although not shown, the third conductive film 191 is connected to the vibration side convex portion 14a through a contact hole opened in the vibration side dielectric layer 55 on the back side of the paper surface. q The top surface of the device is electrically connected.

[0261] Then, a seventh photoresist film is spin-coated on the entire surface to cover the third conductive film 191, and as shown in FIG17a, the three first vibration electrode bases 185, the second vibration electrode bases 186, and the third vibration electrode bases 187, as well as the three first etching medium channels 175b, the second etching medium channels 176b, and the third etching medium channels 177b are exposed and developed to separate the third conductive film 191. Then, the third conductive film 191 is selectively etched by dry etching technology using the pattern of the seventh photoresist film as an etching mask, as shown in FIG17a. Fig.18F As shown, the second vibration electrode base 186 and the third vibration electrode base 187 are separated into a second etching medium passage forming pattern 192 , and the second etching medium passage forming pattern 192 is sandwiched between the second vibration electrode base 186 and the third vibration electrode base 187 .

[0262] Next, if Figure 18GAs shown, a vibrating electrode protective film bottom layer, such as a silicon oxide film, having a thickness of about 50 nm is formed on the entire surface by using a CVD method or the like, covering the dielectric film 19 and the second vibrating electrode base 186 and the third vibrating electrode base 187. The vibrating electrode protective film bottom layer is an insulating film, and constitutes the vibrating electrode top protective film 56 as a composite film in the subsequent process. In order to cover the vibrating electrode protective film bottom layer, an eighth layer of photoresist film is spin-coated on the entire surface, and the pattern of the hole for forming the cavity is matched by a mask, and exposure and development are performed. Then, using the pattern of the eighth layer of photoresist film as an etching mask, the vibrating electrode protective film bottom layer is opened by dry etching technology, exposing a portion of the upper surface of the second etching medium channel forming pattern 192, and opening the hole for forming the cavity.

[0263] When a corrosive medium such as hydrogen peroxide solution is used as an etchant to form a hole through the cavity, the second corrosive medium channel forming pattern 192 is etched away to form a second corrosive medium channel 176b. Figure 18G At the far end of the paper, the first etching medium channel 175b and the third etching medium channel 177b are formed in the same manner. After the second etching medium channel 176b is formed, the sacrificial film 16 is etched away through the second etching medium channel 176b to form Fig. 17B The vibration chamber 18 is shown.

[0264] If the etching medium is a liquid, after the process of removing the sacrificial film 16 is completed, the etching medium cleaning process is transferred to the etching medium cleaning process using a cleaning liquid. After the etching medium cleaning process is completed, the cleaning liquid is evaporated. After the cleaning liquid evaporates, use CVD, etc. to deposit a main protective layer, that is, the remaining part of the vibration electrode top protective film 56, with a thickness of 150-1000nm on the entire surface of the vibration electrode protective film base layer. By depositing the main protective layer on the vibration electrode protective film bottom layer under reduced pressure, a plug is set at the entrance of the cavity forming hole, and the vibration cavity 18 is vacuum sealed. The composite film of the vibration electrode protective film bottom layer and the main protective layer constitutes the protective film 56 on the top surface of the vibration electrode shown in Figure 18H, completing the process as shown in Figure 18H. Fig. 17B A cross-sectional structure of an acoustic element according to a third embodiment is shown.

[0265] (Fourth embodiment)

[0266] As mentioned in the introduction, the fourth embodiment of the present invention is mainly described with respect to the case where both the side protrusion and the vibration side protrusion are conductive bodies. Fig.19 The cross-sectional structure of the acoustic element of the fourth embodiment is shown, with emphasis on the structure on the outer periphery of the vibration chamber. Figure 2E , Fig.13 and Fig.16As shown in Figures 1 and 2, it is based on a three-layer structure, in which a bottom insulating film 52 is deposited on the element substrate 51, and a bottom electrode protective film 53 is deposited on the top of the bottom insulating film 52. As the side wall structure of the acoustic element of the fourth embodiment, the outermost opposite step side wall portion 13a0 and the first pair of side protrusions 13a1 are composed of a low-resistivity dielectric (such as a DOPOS film). The outermost first vibration side protrusion 14a1 is inserted between the groove formed by the opposite step side wall 13a0 and the first pair of side protrusions 13a1, and the second vibration side protrusion 14a2 is inserted into the inner groove of the first pair of side protrusions 13a1. The first vibration side protrusion 14a1 and the second vibration side protrusion 14a2 are also composed of a low-resistivity dielectric such as a DOPOS film.

[0267] Fig.19 The normal direction capacitor C is omitted udv1 , C udv2 and the non-linear capacitor C udh The symbol mark, but with Figure 2E Similarly, the surfaces of the opposite step side wall portion 13a0 and the first opposite side convex portion 13a1, as well as the surfaces of the first vibration side convex portion 14a1 and the second vibration side convex portion 14a2, are normal to the capacitor C according to Gauss's law. udv1 , C udv2 and the non-linear capacitor C udh It is composed of induced true charges, which are the starting point and end point of the electromotive force line of the vibration cavity 18. Normal direction capacitor C udv1 , C udv2 It means that the electric field lines extend in the normal direction of the main surfaces of the first electrode base (vibration electrode base) 12 and the second electrode base (counter electrode base) 11. Fig.19 In the non-linear direction, the capacitor C udh The direction in which the electric lines of force extend is perpendicular to the electric lines of force in the normal direction of the main surfaces of the first and second electrode bases.

[0268] like Fig.19As shown, the surfaces of the opposite step side wall portion 13a0 and the first pair of side protrusions 13a1 are exposed, but a dielectric layer 54, such as a silicon oxide film, is plated on the upper surface of the electrode base 11 at the positions of the opposite step side wall 13a0 and the first pair of side protrusions 13a1. The surfaces of the first vibration side protrusion 14a1 and the second vibration side protrusion 14a2 made of solid dielectric are exposed, while the lower surface of the vibration electrode base 12 at the position where the first vibration side protrusion 14a1 and the second vibration side protrusion 14a2 are not arranged is covered with a vibration side dielectric layer 55 composed of a dielectric film such as a silicon nitride film. A vibration electrode top protective film 56 (such as a silicon oxide film) is arranged on the vibration electrode base 12. The side wall of the cavity has a composite structure, including a side wall insulating film base 21 (such as a silicon oxide film) and a side wall insulating film 22 (such as a silicon oxide film) deposited on the side wall insulating film base 21.

[0269] As described above, when the vibration side convex portion 12a q-1 , 12a q , 12a q+1 , ... and the opposite side convex portion 11a p-1 , 11a p , 11a p+1 When the metal electrodes are made of metal, there is a risk of short circuit between the metal electrodes. q-1 , 12a q , 12a q+1 The surface of the vibrating side dielectric layer 55 is covered, and the opposite side convex portion 11a p-1 , 11a p , 11a p+1 The surface of , ... must be covered with the opposite dielectric layer 54. Fig.19 As shown, when the opposite stepped side wall portions 13a0, the first pair of side protrusions 13a1, the first vibration side protrusions 14a1 and the second vibration side protrusions 14a2 are made of solid low-resistivity dielectrics, the surface of the low-resistivity dielectric can be exposed in the vibration cavity 18.

[0270] In the description of the first and second embodiments, the side convex portion 11a is described. p-1 , 11a p , 11a p+1 , ... and the opposite side convex portion 13a p-1 , 13a p , 13a p+1 , .... A case where a dielectric having a resistivity ρ ≤ 3Ω·cm is used as the conductor. In the description of the first and third embodiments, the vibration side convex portion 12a is described. q-1 , 12a q , 12a q+1 , ... and the vibration side convex portion 14a q-1, 14a q , 14a q+1 , ... a case where a dielectric having a resistivity ρ≤3Ω·cm is used as a conductor. The acoustic element of the fourth embodiment is an example of a case where the opposite step side wall portion 13a0, the first pair of side protrusions 13a1, the first vibration side protrusion 14a1, and the second vibration side protrusion 14a2 all use a dielectric having a resistivity ρ≤3Ω·cm as a conductor.

[0271] That is, the acoustic element of the fourth embodiment is composed of a first electrode base, a convex portion composed of a dielectric, a convex portion composed of a dielectric (a first step side wall composed of a dielectric is composed of a plane inclined at an angle of less than 45° to the vibration direction and is arranged on the first electrode base), a convex portion composed of a conductor, a convex portion composed of a conductor (a second step side wall composed of a conductor is composed of a plane with the same inclination angle as the first step side wall, faces the first electrode base to form a capacitor), and a convex portion composed of a second electrode base (the second step side wall is composed of a plane inclined at an angle of less than 45° to the vibration direction, faces the first electrode base to form a capacitor). The convex portion composed of a conductor has a second step side wall composed of a plane, and a second electrode base opposite to the first electrode base, and the convex portion is composed of a conductor and faces the first electrode base. The first electrode base may be the above-mentioned vibration electrode base 12 , first vibration electrode base 185 , second vibration electrode base 186 and third vibration electrode base 187 , or may be the electrode base 11 , first pair of electrode bases 111 , second pair of electrode bases 112 and third pair of electrode bases 113 .

[0272] In the acoustic element of the fourth embodiment, when the first electrode base is the vibration electrode base 12 or the first vibration electrode base 185, the second vibration electrode base 186, and the third vibration electrode base 187, the second electrode base is the counter electrode base 11 or the first counter electrode base 111, the second counter electrode base 112, and the third counter electrode base 113. Conversely, if the first electrode base is the counter electrode base 11, the first counter electrode base 111, the second counter electrode base 112, and the third counter electrode base 113, the second electrode base is the vibration electrode base 12, the first vibration electrode base 185, the second vibration electrode base 186, and the third vibration electrode base 187. The voltage applied between the first and second electrode bases causes the first or second electrode base to vibrate in the vibration direction.

[0273] In addition, if Figure 1As shown, a specific number of transmitting units can be distributed, wherein the protrusion is composed of a dielectric having a specific resistance ρ≤3Ω·cm, even if multiple units (each unit is distributed with a unit number of capacitive acoustic elements) are arranged in a two-dimensional manner on the same curved surface, as described above in the acoustic element integrated circuit. Each of the multiple transmitting units includes: a first electrode base; a protrusion composed of a dielectric with a resistivity ρ≤3Ω·cm, the dielectric having a first stepped side wall composed of a plane with an inclination angle within 45° to the vibration direction, and facing the first electrode base to form a capacitor; a protrusion composed of a dielectric, the protrusion having a second stepped side wall composed of a plane inclined at the same inclination angle as the first stepped side wall, and having a resistivity ρ≤3Ω·cm; and a second electrode base opposite to the first electrode base, the second electrode base being arranged with a protrusion composed of a dielectric and facing the first electrode base. In each transmitting unit of the acoustic element integrated circuit of the fourth embodiment, the first or second electrode base vibrates along the vibration direction by applying a voltage between the first and second electrode bases.

[0274] (Fifth Embodiment)

[0275] As described in the basic concept of the present invention, the vibration side convex portion (first electrode side convex portion) and the opposite side convex portion (second electrode side convex portion) can be a conductor with a low resistivity ρ, or can be an almost complete insulator (ρ≈∞). Therefore, as described at the beginning, the first to fourth embodiments of the present invention are mainly described for the case where the opposite side convex portion and the vibration side convex portion are conductors, and the fifth embodiment of the present invention will be mainly described for the case where the opposite side convex portion and the vibration side convex portion are almost complete insulators. Figure 3-Figure 5 As shown, the vibration-side protrusion and the opposite-side protrusion may also be composed of an almost perfect insulator having a low resistivity ρ≈∞.

[0276] Fig.19 The cross-sectional structure mentioned in the acoustic element related to the fourth embodiment focuses on the structure on the outer side of the vibration cavity, but in the acoustic element related to the fifth embodiment, the relative side convex part and the vibration side convex part are almost completely insulated. Since the relative side convex part and the vibration side convex part are made of different materials, they are described with reference to each other. Figure 2E In the structure of the acoustic element of the fifth embodiment shown in FIG. 1 , the thickness of the side wall of the dielectric layer 54 on the opposite side and the dielectric layer 55 on the vibration side may be increased, and the width of the convex portion on the vibration side and the convex portion on the opposite side (see FIG. Fig. 22 The convex width x0 defined in (a) is reduced to the limit. Figure 2E , Fig.13 and Fig.16 The same structure as the conductive protrusions, such as Fig.19The acoustic element of the fifth embodiment shown is based on a three-layer structure in which a bottom insulating film 52 is deposited on an element substrate 51, and a bottom electrode protective film 53 is further deposited on the bottom insulating film 52. However, the difference from the acoustic element of the fourth embodiment is that the outermost pair of stepped side wall portions 13a0 and the first pair of side protrusions 13a1, which are the side wall structures of the acoustic element of the fifth embodiment, are composed of an almost perfect insulator with a low resistivity ρ≈∞. The outermost first vibration side protrusion 14a1 is inserted between the groove formed by the opposite side stepped side wall portion 13a0 and the first pair of side protrusions 13a1, and the second vibration side protrusion 14a2 is inserted into the inner groove of the first pair of side protrusions 13a1, but the first vibration side protrusion 14a1 and the second vibration side protrusion 14a2 are also composed of an almost perfect insulator with a low resistivity ρ≈∞.

[0277] Fig.19 The normal direction capacitor C is omitted udv1 , C udv2 The symbol mark, but with Figure 2E Similarly, according to Gauss's law, the true charges at the starting point and the end point of the electric lines of force of the vibration cavity 18 are induced to form a normal direction capacitor C. udv1 , C udv2 . If the relative dielectric constant of the opposite stepped side wall portion 13a0, the first pair of side convex portions 13a1, the first vibration side convex portion 14a1 and the second vibration side convex portion 14a2 is ε1, and the relative dielectric constant of the vibration cavity 18 is ε2, as described in the basic concept, if ε2<<ε1, the electric field inside the opposite stepped side wall portion 13a0, the first pair of side convex portions 13a1, the first vibration side convex portion 14a1 and the second vibration side convex portion 14a2 will be weakened by ε1 / ε2, and the distribution profile of the equipotential lines will be distorted.

[0278] If ε2<<ε1, when the gap between the opposite step side wall portion 13a0 and the first vibration side convex portion 14a1, the gap between the first pair of side convex portions 13a1 and the first vibration side convex portion 14a1, or the gap between the first pair of side convex portions 13a1 and the second vibration side convex portion 14a2 is narrow, the distribution profile of the equipotential lines will be distorted, and the slope of the equipotential lines of the relative dielectric constant ε2 will become a steep slope close to the vertical direction. Since the direction of the electric flux is consistent with the normal direction of the equipotential lines, the electric flux and the electric field lines will be inclined in a direction close to the horizontal, and the electric field lines will be bent, between the opposite step side wall portion 13a0 and the first vibration side convex portion 14a1, between the first pair of side convex portions 13a1 and the first vibration side convex portion 14a1, or between the first pair of side convex portions 13a1 and the second vibration side convex portion 14a2. That is, inclined electric force lines are generated between the opposite stepped side wall portions 13a0 and the first vibration side convex portion 14a1, between the first pair of side convex portions 13a1 and the first vibration side convex portion 14a1, or between the first pair of side convex portions 13a1 and the second vibration side convex portion 14a2, and these electric force lines pass through the opposite stepped side wall portions 13a0 and the first pair of side convex portions 13a1, enter the vibration cavity, and reach the first vibration side convex portions 14a1 and the second vibration side convex portions 14a2, where the paths of the internal electric force lines are bent. That is, in the power element of the fifth embodiment, a capacitor in a non-normal direction is formed inside the vibration cavity by means of the electric force lines bent relative to the normal direction of the main surfaces of the first and second electrode bases. The slope of the partial electric force lines provided by the capacitor in the non-normal direction formed in the power element of the fifth embodiment is the same as that of the capacitor in the non-normal direction. Figure 2E The slopes of the capacitor electric lines of force in the non-normal direction are almost similar in the case of the conductor shown. Figure 3-Figure 5 As described above, even in the case of an almost perfect insulator (ρ≈∞), the electrostatic energy in the vibration cavity of the capacitor containing the non-normal direction can be increased, and the attraction can also be increased, so that the transmitted sound pressure can be increased like the acoustic elements using the protrusions of the conductor in the first to fourth embodiments.

[0279] like Fig.19As shown, the surfaces of the opposite step side wall portion 13a0 and the first pair of side protrusions 13a1 are exposed, but the upper surface of the opposite electrode base (second electrode base) 11 where the opposite step side wall portion 13a0 and the first pair of side protrusions 13a1 are not arranged is covered with an opposite side dielectric layer 54 such as a silicon oxide film. In addition, the surfaces of the first vibration side protrusion 14a1 and the second vibration side protrusion 14a2 made of solid dielectric are exposed, while the lower surface of the vibration electrode base (first electrode base) 12 where the first vibration side protrusion 14a1 and the second vibration side protrusion 14a2 are not arranged is covered with a vibration side dielectric layer 55 (such as a dielectric film such as a silicon nitride film). A protective film 56 such as a silicon oxide film is provided on the upper surface of the vibration electrode base 12. The side wall of the cavity has a composite structure, namely, a side wall insulating film bottom layer 21 (such as a silicon oxide film) and a side wall insulating film 22 (such as a silicon oxide film) deposited on the side wall insulating film bottom layer 21. In the acoustic element of the fifth embodiment, the vibrating electrode base 12 is referred to as the "first electrode base 12", the counter electrode base 11 is referred to as the "second electrode base 11", the vibrating side convex portion is referred to as the "first electrode side convex portion", and the counter electrode side convex portion is referred to as the "second electrode side convex portion", but these are names selected for convenience of explanation. It is also possible to select the vibrating electrode base defined in the acoustic element of the fifth embodiment as the "second electrode base", the counter electrode base as the "first electrode base", the vibrating side convex portion as the "second electrode side convex portion", and the counter convex portion as the "first electrode side convex portion".

[0280] As described in the first to fourth embodiments, when the vibration side convex portion 12a q-1 , 12a q , 12a q+1 , ... and the opposite side convex portion 11a p-1 , 11a p , 11a p+1 When the metal electrodes are made of metal, the metal electrodes may short-circuit with each other. Due to the risk of short-circuiting between the metal electrodes, the vibration side convex portion 12a q-1 , 12a q , 12a q+1 The surface of the convex portion 11a is covered with a vibration-side dielectric layer 55. p-1 , 11a p , 11a p+1 The surface of , ... must cover the opposite dielectric layer 54. Fig.19 As shown, when the opposite stepped side walls 13a0 , the first pair of side protrusions 13a1 , the first vibration side protrusion 14a1 and the second vibration side protrusion 14a2 are made of solid dielectric material, the surface of the solid dielectric material can be exposed in the vibration cavity 18 .

[0281] Furthermore, if Figure 1As shown, the transmitting units distributed in a specific number, wherein the dielectric constituting the convex part is composed of an almost perfect insulator (ρ≈∞), and even in the acoustic element integrated circuit, multiple units are distributed in a two-dimensional array on the same curved surface, and each unit has a unit number of capacitive acoustic elements. Each of the multiple transmitting units includes: a vibrating electrode base; a vibrating side convex part, which is arranged on the vibrating electrode base and is composed of a dielectric having a first step side wall part composed of a plane inclined at an angle within 45° relative to the vibration direction; a counter-side convex part, which is opposite to the vibrating electrode base in a capacitor-forming manner and is composed of a dielectric having a second step side wall part composed of a plane inclined at the same angle as the first step side wall part; and the counter-side convex part is configured to have a counter-electrode base opposite to the vibrating electrode base.

[0282] Here, the vibrating side convex portion formed by the dielectric having the first stepped side wall and the opposite side convex portion formed by the dielectric having the second stepped side wall can be almost perfect insulators (ρ≈∞) respectively. In each transmitting unit of the acoustic device integrated circuit of the fifth embodiment, the voltage applied between the first and second electrode bases causes the first or second electrode base to vibrate in the vibration direction.

[0283] (Sixth embodiment)

[0284] The exemplary description of the acoustic element of the sixth embodiment of the present invention mainly describes the case where the opposite convex portion or the vibration convex portion is an almost perfect insulator (ρ≈∞), or equivalent to a perfect insulator. Fig.13 The contralateral convex part or Fig.16 The case where the vibrating protrusion shown is replaced by an almost perfect insulator, or Fig.13 The contralateral convex part or Fig.16 The vibrating protrusion shown corresponds to the electrical connection of a perfect insulator. Fig.16 The case where the vibration side convex part shown is replaced by a complete insulator is similar to the case described at the beginning of this section. Fig.23 The structure corresponds.

[0285] For example, in Fig.13 In the structure shown, the opposite side protrusion made of a low resistivity dielectric is electrically connected to the third opposite side electrode base 113 as one of the split electrodes through the contact hole (assuming that Fig.16 On the outside or back side of the paper, the vibration side convex part of the hexagonal ring structure is also connected to the first pair of electrode bases 111 and the second pair of electrode bases 112 as other segmented electrodes). In contrast, "the situation equivalent to a perfect insulator" means that there is no contact hole between the side convex parts that is electrically connected, that is, the low resistivity dielectric is in a suspended state, etc. Similarly, in Fig.16In the structure shown, the vibration side convex part composed of the low resistivity dielectric is electrically connected to the first vibration electrode base 185 as one of the split electrodes through the contact hole, that is, the vibration side convex part has no contact hole for electrical connection, and the low resistivity dielectric is in a floating state. (Assuming that Fig.16 The vibration side convex portion of the hexagonal ring structure is also connected to the second vibration electrode base 186 and the third vibration electrode base 187 as other segmented electrodes on the outer side or back side of the paper). That is, even a low-resistivity dielectric will exhibit characteristics equivalent to an insulator if it is in an electrically floating state. In the case of a low-resistivity dielectric, since no electric field is generated or is extremely small inside, the distance is actually equivalent to a reduction in distance. However, in order to express behavior equivalent to an insulator, it is more preferable that the resistivity ρ of the dielectric as the opposite side convex portion or the vibration side convex portion is 1 kΩ·cm or more, which is a relatively high resistivity that facilitates dielectric polarization.

[0286] The acoustic element of the sixth embodiment includes: a first electrode base; a first electrode side protrusion, which is arranged on the first electrode base and is composed of a dielectric having a first step side wall composed of a plane inclined at an angle within 45° relative to the vibration direction; a second electrode side protrusion, which is composed of a conductor having a second step side wall composed of a plane inclined at the same angle as the first step side wall; and a second electrode side protrusion composed of the conductor is arranged so that the second electrode base opposite to the first electrode base can be used as a main component. In other words, the case where either the vibration side protrusion or the opposite side protrusion that becomes the first electrode side protrusion is a substantially complete insulator with a low resistivity ρ≈∞, and the opposite second electrode side protrusion is a structure composed of a conductor.

[0287] like Fig.23 As shown, when the vibration side convex portion 12c ij When the insulator protrusion is formed, the electric flux flows from the protrusion side wall (opposite side protrusion) of the step counter electrode 1a through the vibration side protrusion 12c. ij The inside of the vibrating electrode base 12 reaches the vibrating electrode base 12 . Fig.23 In the case of ε1≒ε2, it can be observed that the electric flux passes from the side wall of the opposite side convex part through the vibration side convex part 12c. ij The vibration side convex part 12c reaches the vibration electrode base part 12. When ε1<<ε2, the vibration side convex part 12c ij The internal equipotential lines extend in the longitudinal direction, and the distribution curve of the equipotential lines is deformed, extending from the side wall of the opposite side convex portion through the vibration side convex portion 12c. ij The electric flux reaching the vibration electrode base 12 increases, and the electric flux slope between the gaps with the relative dielectric constant ε2 becomes close to horizontal. ij Oblique electric field lines are generated between the side walls.

[0288] Apart from Fig.23 The normal direction capacitor C between the vibration electrode base 12 and the opposite convex top shown in FIG. udv1 and the insulator 12c of the vibration side protrusion 12c inserted between the groove of the step counter electrode 1a and the vibration electrode base 12. ij The normal direction of the capacitor C udv2 In addition, it also relies on the electric lines that are at least partially inclined at a certain angle to the normal direction to form a non-normal line capacitor. Fig.23 Likewise, in Fig.13 In the case where the opposite side protrusion is replaced by a complete insulator, in addition to the normal direction capacitor between the opposite side electrode base and the top of the vibration side protrusion, the insulator inserted between the stepped vibration electrode groove and the opposite side electrode base, and the insulator inserted between the side wall of the opposite side protrusion and the side wall of the vibration side protrusion constitute a non-normal direction capacitor, which at least partially relies on the oblique electromotive force lines generated between the side wall of the opposite side protrusion and the side wall of the vibration side protrusion to increase the electrostatic energy. The increase in electrostatic energy will increase the attraction between the vibration electrode base and the opposite electrode base, thereby increasing the transmission pressure.

[0289] In the acoustic element of the sixth embodiment, the first electrode base may be the single vibration electrode base 12 described in the acoustic element of the first embodiment, or may be a separate structure of the first vibration electrode base 185, the second vibration electrode base 186, and the third vibration electrode base 187 described in the acoustic element of the third embodiment. Fig.13 The split-type electrodes, namely the first pair of electrode bases 111, the second pair of electrode bases 112 and the third pair of electrode bases 113, are shown in the figure, but a single pair of electrode bases may also be used. The pair of electrode bases may be the single pair of electrode bases 11 described in the acoustic element of the first embodiment, or may be the split structure of the first pair of electrode bases 111, the second pair of electrode bases 112 and the third pair of electrode bases 113 described in the acoustic element of the third embodiment. However, in Fig.16 In the structure shown, the split electrode is electrically connected to the first vibration electrode base 185, the second vibration electrode base 186, and the third vibration electrode base 187, but it may be a single vibration electrode base.

[0290] In the acoustic element of the sixth embodiment, when the first electrode base is the vibration electrode base 12 or the first vibration electrode base 185, the second vibration electrode base 186, and the third vibration electrode base 187, the second electrode base is the counter electrode base 11 or the first counter electrode base 111, the second counter electrode base 112, and the third counter electrode base 113. Conversely, if the first electrode base is the counter electrode base 11, the first counter electrode base 111, the second counter electrode base 112, and the third counter electrode base 113, the second electrode base is the vibration electrode base 12, the first vibration electrode base 185, the second vibration electrode base 186, and the third vibration electrode base 187. The voltage applied between the first and second electrode bases causes the first or second electrode base to vibrate in the vibration direction.

[0291] In addition, if Figure 1 As shown, even if the multiple units of the capacitive acoustic element are respectively allocated in units in the above-mentioned acoustic element integrated circuit, they are distributed on the same curved surface in the form of a two-dimensional array, wherein the dielectric constituting the convex portion is composed of an almost perfect insulator (ρ≈∞), and the transmitting unit is distributed in a specific number of units. Each of the multiple transmitting units includes: a first electrode base, a convex portion composed of a dielectric having a first step side wall formed by a plane arranged on the first electrode base and inclined at an angle within 45° relative to the vibration direction; a convex portion composed of a conductor having a second step side wall formed by a plane opposite to the first electrode base in a capacitor manner and inclined at the same angle as the first step side wall; a convex portion composed of the conductor and having a second electrode base opposite to the first electrode base, but the convex portion composed of a dielectric having a first step side wall can also be a substantially complete insulator (ρ≈∞). In each transmitting unit of the acoustic device integrated circuit of the sixth embodiment, the voltage applied between the first and second electrode bases causes the first or second electrode base to vibrate in the vibration direction.

[0292] (Other embodiments)

[0293] As described above, the present invention is described by the 1st to the 6th embodiment, but the description and drawings constituting a part of the present disclosure should not be understood as limiting the present invention. For those skilled in the art, various optional embodiments, examples and operation techniques will be apparent from the present disclosure.

[0294] like Figure 2C and 2D As shown in Figure 1, the deflection shape of the step vibration electrode in the vibration direction is not uniform. Figure 2DAs shown, near the center of the vibration cavity 18, the stepped vibration electrode and the stepped counter electrode can achieve a cross topology and have a sufficient facing area, but in the periphery where the deflection is small, a sufficient facing area cannot be achieved. The calculation method of the "secondary moment of cross section I" is: divide the cross section into countless micro-section areas dA, and multiply each micro-section area by the square of the distance y from a certain rotation axis. 2 , then add (I = ∑ (y 2 dA)), whose size is the fourth power of the length. The so-called "specific rotation axis" refers to the central axis of the bar when it is bent, although its cross section is slightly rotated. The second-order moment of the cross section represents the geometric resistance to deformation during bending. It is well known that the second-order section moment of a rectangular cross-section material with width b and thickness h is

[0295] I=bh 3 / 12.........(14)

[0296] It is expressed in the form of being inversely proportional to the cube of the thickness h. Young's modulus Y represents the deformation resistance in a mechanical sense.

[0297] The deflection (bending) of the beam can be calculated from the neutral surface radius ρ. The larger the neutral surface radius, the smaller the deflection, which means that the larger the YI, the smaller the deflection of the beam. Therefore, YI is also called the bending stiffness K of the beam.

[0298] K=YI=Ybh 3 / 12.........(15)

[0299] The deformation of the plate is divided into flexure (bending), elongation (compression) and shear (torsion). The bending stiffness K of the plate also uses Poisson's ratio σ,

[0300] K=YI=Yh 3 / 12(1-σ 2 ).........(16)

[0301] Therefore, the bending stiffness K is related to Young's modulus Y and the cubic value of the plate thickness (h 3 ) is proportional to the product of .

[0302] For various materials, if α is a proportionality constant, then

[0303] k / h 3 =α(Y / (1-σ 2 )).........(17)

[0304] That is, the main body of the spring constant k of the step vibration electrode side structure is the bending stiffness shown in formula (16). Theoretically, the Poisson's ratio σ can only take a value below 0.5. Table 1 gives some examples. The Poisson's ratio σ of many materials is between 0.3 and 0.4. The square of the Poisson's ratio σ (σ 2 ) The value obtained after the addition is about 0.09-0.16. The Young's modulus (longitudinal elastic modulus) of silicon oxide film is about 66-68GPa, while the Young's modulus of silicon nitride film is about 210-310GPa, so the rigidity of silicon nitride film is higher than that of silicon oxide film.

[0305] Formula (16) shows that a silicon nitride film (Si3N4 film) having a large Young's modulus Y has a high plate bending rigidity K. Therefore, the rigidity can be enhanced by using a silicon nitride film as a protective film 56 on the top surface of the vibration electrode and increasing the thickness of the central portion of the silicon nitride film.

[0306] (Table 1)

[0307] Material Poisson's ratio W 0.28 Al 0.345 Cu 0.343 Pb 0.44 Au 0.44 Sn 0.36 <![CDATA[SiO2]]> 0.2 <![CDATA[Si3N4]]> 0.27~0.25

[0308] Fig. 20 (a) and Fig. 20 The dotted line in (b) represents the deflection profile of the vibration electrode base 12 in the vibration direction. Figure 2C and Figure 2D same. Fig. 20 The vertical axis of (a) represents the displacement (absolute amount) of the vibrating electrode base 12, and Fig. 20 The vertical axis of (b) represents Fig. 20 (a) is the relative value of the displacement of the vibrating electrode base 12 when the maximum displacement is normalized to -1. Fig. 20 The horizontal axis of (a) and (b) is the horizontal position coordinate in the vibration cavity.

[0309] In the above Figure 2E In the example shown in FIG. 1 , a protective film 56 structure on the upper surface of the vibration electrode is formed of a silicon nitride film having a uniform plate thickness, so the rigidity is enhanced to a certain extent by using the silicon nitride film. Fig. 20 In (a) and 20(b), the "no rigidity enhancement" acoustic element structure indicated by the dotted line means that the protective film 56 on the upper surface of the vibration electrode is composed of a planar silicon nitride film with a uniform plate thickness of about 5 μm. Fig. 20 The structure of the "rigidity-enhanced" acoustic element shown by the solid lines in (a) and 20 (b) means that the protective film 56 on the top surface of the vibration electrode has a structure in which the central portion has a silicon nitride film with a thickness of about 13.8 μm, and the peripheral portion has a silicon nitride film with a thickness of about 3.8 μm, which surrounds the central portion in a concentric manner. The thickness of the structure varies.

[0310] like Fig. 20 In the structure with "rigidity reinforcement" shown by the solid lines in (a) and (b), the flattening of the deflection profile can be achieved. Fig. 20 In the transmission capacity simulation shown in (c), Fig. 20 The cavity width of the structure without rigid reinforcement shown by the dotted line and the structure with rigid reinforcement shown by the solid line in (a) and (b) is 120 μm. For the structure with rigid reinforcement, the width of the thicker part of the central part of the protective film 56 on the upper surface of the vibration electrode is set to 60 μm. The transmission energy of the acoustic element is given by Fig. 20 The radial coordinate integral of the transmitted sound pressure distribution shown in (c) gives Fig. 20 The area enclosed under the transmitted sound pressure distribution curve shown in (c) is the transmitted energy. Fig. 20 The area of ​​the acoustic element with rigid reinforcement shown by the solid line in (c) is larger than the area of ​​the acoustic element without rigid reinforcement shown by the dotted line. Fig. 20 The area enclosed by the curve (c) below is 58% (integer value) for the acoustic element without rigid reinforcement as shown by the dotted line, while the area of ​​the acoustic element with rigid reinforcement as shown by the solid line is 62% (integer value). Therefore, in the peripheral structure of the stepped vibration electrode, the rigidity of the central part is enhanced. This shows that by enhancing the rigidity of the central part of the peripheral structure of the stepped vibration electrode, the transmission energy of the acoustic element can be increased.

[0311] There are many other ways to make the deflection shape profile of the step vibration electrode side of the acoustic element uniform. For example, due to the relative dielectric constant ε of the silicon nitride film r =7.0-7.8, and the relative dielectric constant of silicon oxide film ε r =3.9-4.5, so silicon nitride film can be used as the material of the side wall of the vibration cavity 18 to strengthen the electric field in the peripheral area. As the electric field enhancement layer for strengthening the peripheral electric field, in addition to silicon nitride film, the high dielectric material introduced at the beginning of this article, such as HfSi x O y In addition, the peripheral electric field enhancement structure and the rigidity enhancement structure of thickening the central portion of the protective film 56 on the upper surface of the vibration electrode may be used simultaneously.

[0312] exist Fig.17A , the vibration electrode base portion is divided into three parts: the first vibration electrode base portion 185, the second vibration electrode base portion 186, and the third vibration electrode base portion 187. Fig.21As shown in FIG. 1 , the six-part structure on the vibration electrode side of the first central vibration electrode base 185i, the second central vibration electrode base 186i, the third central vibration electrode base 187i, the first peripheral vibration electrode base 185o, the second peripheral vibration electrode base 186o, and the third peripheral vibration electrode base 187o of the vibration electrode base can also effectively flatten the deflection curve. That is, if the rigidity of the conductive material used for the first central vibration electrode base 185i, the second central vibration electrode base 186i, and the third central vibration electrode base 187i is stronger than the rigidity of the conductive material used for the first peripheral vibration electrode base 185o, the second peripheral vibration electrode base 186o, and the third peripheral vibration electrode base 187o, the deflection curve can be flattened. Alternatively, the driving voltage applied to the first central vibrating electrode base 185i, the second central vibrating electrode base 186i, and the third central vibrating electrode base 187i is lower than the driving voltage applied to the first peripheral vibrating electrode base 185o, the second peripheral vibrating electrode base 186o, and the third peripheral vibrating electrode base 187o, and the deflection profile may also be flattened.

[0313] In addition, in the acoustic element of the second embodiment, it is described that the side protrusion is connected to the split electrode, the first pair of electrode bases 111, the second pair of electrode bases 112 and the third pair of electrode bases 113, but this is only an example. As with the acoustic element of the first embodiment, as long as the flow path of the etching medium and other manufacturing technology issues are not considered, the three split electrodes can also be a single, continuous pair of electrode bases. Similarly, in the acoustic element of the third embodiment, the vibration side protrusion is electrically connected to the split electrode, the first vibration electrode base 185, the second vibration electrode base 186 and the third vibration electrode base 187, but this is only an example. As long as the flow path of the etching medium is not considered, the three split electrodes can be a continuous vibration electrode base, such as the acoustic element in the first embodiment.

[0314] The height of each pair of convex parts does not have to be the same, and the height of the vibration side convex parts does not have to be the same. Figure 2C In the cross-sectional structure shown, the opposite convex portion 11a p-1 , 11a p , 11a p+1 , ... and the vibration side convex portion 12a q-1 , 12a q , 12a q+1 , ... intersect in the central part of the vibration cavity, but do not intersect in the periphery. Figure 2C In the case shown, crossing becomes difficult at the periphery, and the height of the contralateral convex portion or the vibration-side convex portion may be higher at the periphery than at the center.

[0315] Therefore, the present invention is not limited to the description of the above-mentioned first to sixth embodiments, but various changes can be made, and these changes are also included in the scope of the present invention. Therefore, according to the above description, the technical scope of the present invention is determined only by the invention details related to the description of the claims.

[0316] Explanation of symbols

[0317] 11: a counter electrode base (a second electrode base), 11a p-1 , 11a p , 11a p+1 ...side convex portion (second electrode side convex portion), 111 ...first pair of electrode bases, 112 ...second pair of electrode bases, 113 ...third pair of electrode bases, 12 ...vibrating electrode base (first electrode base), 12a p-1 , 12a p , 12a p+1 ...vibration side convex portion (first electrode side convex portion), 13p...dielectric film, 141, 142, 143, 141b, 142b, 143b, 144, 145, 146, 147, 171, 172, 173...pipe end portion, 151, 152, 153, 151b, 152b, 153b...etching medium channel, 16...sacrificial film, 16a...first sacrificial film, 16b...second sacrificial film, 16c...third sacrificial film, 161, 162, 163, 181, 182, 183...hole forming a cavity, 175b...first etching medium channel, 176b...second etching medium channel, 177b...third etching medium channel, 18...vibration cavity, 185...first vibration electrode base, 185i...first central vibration electrode base, 185o...first peripheral vibration electrode base, 1 86...second vibration electrode base, 186i...second central vibration electrode base, 186o...second peripheral vibration electrode base, 187...third vibration electrode base, 187i...third central vibration electrode base, 187o...third peripheral vibration electrode base, 19...dielectric film, 191...third conductive film, 192...second etching medium flow path forming pattern, 21...side wall insulating film bottom layer, 22...side wall insulating film, 23...cavity side wall portion, 25...counter electrode supporting layer, 31, 54...counter side dielectric layer, 31c...contact hole, 32...second conductive film, 33...selective removal film, 51...element substrate, 52...bottom layer insulating film, 53...counter electrode bottom protective film, 55...vibration side dielectric layer, 56...vibration electrode top protective film, 59...second embedding groove

Claims

1. An acoustic element, characterized in that a first electrode base having a flat main surface and a flat plate shape, A second electrode base having a flat main surface and parallel to and opposite to the first electrode base, The first electrode side protrusion is provided on the first electrode base and has a first stepped side wall formed by a plane having an inclination angle within 45° relative to the vibration direction. a second electrode side protrusion, which is arranged on the second electrode base, at least a part of which is opposite to the first electrode side protrusion in a cross manner, and has a second step side wall composed of a plane inclined at the same inclination angle as the first step side wall, By applying a voltage between the first electrode base and the second electrode base, the first electrode base or the second electrode base vibrates in the vibration direction, generating a capacitor at least partially dependent on the electric lines between the first step side wall and the second step side wall, and the electrostatic energy in the vibration cavity clamped by the first electrode base and the second electrode base is increased.

2. The acoustic element according to claim 1, characterized in that The electric lines of force between the first step side wall and the second step side wall are inclined relative to the normal direction of the first electrode base main surface and the second electrode base main surface.

3. The acoustic element according to claim 1 or 2, characterized in that: At least one of the first electrode-side protrusion and the second electrode-side protrusion is an electrical conductor.

4. The acoustic element according to claim 1 or 2, characterized in that: At least one of the first electrode-side protrusion and the second electrode-side protrusion is a dielectric.

5. The acoustic element according to claim 1, characterized in that The inclination angle between the inclination angle and the vibration direction does not exceed 10°.

6. The acoustic element according to claim 1, characterized in that The inclination angle relative to the vibration direction is 0°, and the relative areas of the first step side wall and the second step side wall vary with the voltage applied between the step-type vibration electrode and the step-type counter electrode.

7. An acoustic element integrated circuit, characterized in that: It includes multiple units, each unit has a unit number of capacitive acoustic elements, which are distributed on the same surface in the form of a two-dimensional array. Each unit is distributed in a specific amount, a first electrode base having a flat main surface and a flat plate shape, A second electrode base having a flat main surface and parallel to and opposite to the first electrode base, The first electrode side protrusion is provided on the first electrode base and has a first stepped side wall formed by a plane having an inclination angle within 45° relative to the vibration direction. a second electrode side protrusion, which is arranged on the second electrode base, at least a part of which is opposite to the first electrode side protrusion in a cross manner, and has a second step side wall composed of a plane inclined at the same inclination angle as the first step side wall, By applying a voltage between the first electrode base and the second electrode base, the first electrode base or the second electrode base vibrates along the vibration direction, generating a capacitor that at least partially depends on the electric lines between the first step side wall and the second step side wall, and the electrostatic energy in the vibration cavity clamped by the first electrode base and the second electrode base increases.

8. The acoustic element integrated circuit according to claim 7, characterized in that The plurality of units distributed by other specific unit numbers are units for receiving.