An integrated extrusion-filling-encapsulation method for processing phase change cooled metal phase change cells.
Through continuous processing steps and automated equipment, the complexities of metal phase transformation cell production have been solved, achieving efficient and stable production and quality control.
Patent Information
- Application Number
- CN202411066346.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-05
- Publication Date
- 2026-11-17
- Estimated Expiration
- 2044-08-05
AI Technical Summary
The existing metal phase transformation unit cell processing is complex, requires skilled operation and experience, has low production efficiency, and is difficult to achieve high-efficiency production.
The process involves continuous steps including smelting, die casting, grinding, filling, and freezing. Partial automation is achieved using vibratory feeders and automatic filling lines, and product quality is strictly controlled to ensure quality and performance at each stage.
This technology enables the efficient production of metal phase transformation cells, reduces production time, improves production efficiency and consistency, reduces operational difficulty, and ensures product quality and performance.
Abstract
Description
Technical Field
[0001] This invention relates to the technical field of cold storage material preparation methods, and in particular to an integrated extrusion-filling-encapsulation method for processing phase change cooling metal phase change cells. Background Technology
[0002] A metal phase change cell is a device that utilizes the latent heat storage properties of phase change materials (PCMs) to achieve cooling and preservation effects. A phase change material is a substance that can absorb or release a large amount of latent heat at a specific temperature. Through this property, metal phase change cells can rapidly allow the food temperature to cross the crystallization zone, forming fine ice crystals, while simultaneously creating a relatively stable low-temperature environment around the food or item, effectively extending its shelf life.
[0003] Specifically, the working principle of a metal phase transformation unit cell is as follows:
[0004] 1. In its initial state, the phase change material exists in solid form within the metal phase change cell. When the ambient temperature rises, the phase change material begins to absorb heat and gradually changes from solid to liquid. During this process, it absorbs a large amount of latent heat, thereby lowering the temperature of the food or object and its surrounding environment.
[0005] 2. When the ambient temperature decreases, the phase change material begins to release heat and gradually changes from liquid to solid, releasing the latent heat stored previously.
[0006] The existing technology for processing phase change cooled metal phase change cells involves multiple steps, including material preparation, extrusion molding, filling and sealing, cooling and demolding, and subsequent inspection and packaging. The process is relatively complex and requires skilled operation and experience. Summary of the Invention
[0007] To address the aforementioned problems, this invention provides an integrated extrusion-filling-encapsulation method for processing phase change cooled metal phase change cells. This method achieves highly efficient production of metal phase change cells through continuous steps, including melting, die casting, grinding, filling, and freezing. Each step is meticulously designed to minimize production time and maximize production efficiency. The details of this invention are as follows:
[0008] The purpose of this invention is to provide an integrated extrusion-filling-encapsulation method for processing phase change cooled metal phase change cells, the technical point of which is that it includes the following steps:
[0009] Step 1: The metal phase change cell shell composition is placed in a high-temperature furnace for melting, so that the metal phase change cell shell composition is melted into a metal solution;
[0010] Step 2: The molten metal from Step 1 is cooled or stamped using a die-casting mold to form a metal phase transformation cell shell;
[0011] Step 3: Grind the surface of the metal phase change cell shell to remove burrs. After passing the first inspection, it is transported to the automatic filling line by a vibratory feeder for filling of the metal phase change cell core material composition.
[0012] Step 4: After the metal phase change cell core material composition is filled, welded and sealed, polished, and then placed in a freezer for freezing, the composition is inspected for leakage, phase change, and expansion deformation, and then it is released from the warehouse.
[0013] To better achieve the above technical solution, the metal phase change cell shell composition in the extrusion-filling-encapsulation integrated phase change cooling metal phase change cell processing method of the present invention includes, by weight, 8-10 parts of nickel powder, 3-6 parts of tin powder, 1-3 parts of silicon powder, 0.25-0.4 parts of vanadium powder and 0.02-0.05 parts of aluminum powder.
[0014] To better achieve the above technical solution, the freezing point of the metal phase change cell core material composition in the extrusion-filling-encapsulation integrated phase change cooling metal phase change cell processing method of the present invention is -30 to -40°C.
[0015] To better achieve the above technical solution, the metal phase change cell core material composition in the extrusion-filling-encapsulation integrated phase change cooling metal phase change cell processing method of the present invention includes, by weight, 20-28 parts of glycerol, 20-22 parts of ethanol, 45-55 parts of nanofluid, 50-60 parts of deionized water, 4-6 parts of modified silica nanoparticles, and 4-6 parts of nucleating agent.
[0016] To better achieve the above technical solution, the nanofluid in the extrusion-filling-encapsulation integrated phase change cooling metal phase change cell processing method of the present invention is at least one of nanoparticle suspension, magnetic nanofluid, nanogel and graphene liquid.
[0017] To better achieve the above technical solution, the nucleating agent in the extrusion-filling-encapsulation integrated phase change cooling metal phase change cell processing method of the present invention is at least one of carbon nanotubes, boron carbide and boron nitride.
[0018] To better achieve the above technical solution, in step one of the extrusion-filling-encapsulation integrated phase change cooling metal phase change cell processing method of the present invention, the temperature of the metal phase change cell shell composition in the high-temperature furnace is 1500-2000℃, and the melting time is 3-10h.
[0019] Compared with the prior art, the integrated extrusion-filling-encapsulation method for processing phase change cooled metal phase change cells of the present invention has the following advantages:
[0020] The integrated extrusion-filling-encapsulation method for processing phase-change cooled metal phase-change cells of the present invention achieves efficient production of metal phase-change cells through continuous steps, including melting, die casting, grinding, filling, and freezing. Each step is carefully designed to minimize production time and maximize efficiency, and product quality is strictly controlled at each stage. The initial inspection ensures the surface quality of the metal phase-change cell shell; while freezing and inspection after filling ensure that the performance and structure of the core material composition meet predetermined requirements, effectively avoiding problems such as leakage, poor phase transformation, and expansion deformation. This processing method utilizes equipment such as vibratory feeders and automated filling lines to automate some operations, reduce manual intervention, lower operational difficulty, and improve production consistency and stability. Detailed Implementation
[0021] To make the objectives, technical solutions, and advantages of this invention clearer, the technical solutions of this invention will be clearly and completely described below in conjunction with specific embodiments. Obviously, the described embodiments are only a part of the embodiments of this invention, and not all of them. Based on the embodiments of this invention, all other embodiments obtained by those skilled in the art without creative effort are within the scope of protection of this invention.
[0022] Example 1
[0023] An integrated extrusion-filling-encapsulation method for processing phase change cooled metal phase change cells includes the following steps:
[0024] Step 1: The metal phase change cell shell composition is placed in a high-temperature furnace for melting, so that the metal phase change cell shell composition is melted into a metal solution;
[0025] Step 2: The molten metal from Step 1 is cooled or stamped using a die-casting mold to form a metal phase transformation cell shell;
[0026] Step 3: Grind the surface of the metal phase change cell shell to remove burrs. After passing the first inspection, it is transported to the automatic filling line by a vibratory feeder for filling of the metal phase change cell core material composition.
[0027] Step 4: After the metal phase change cell core material composition is filled, it is sealed by welding and polished, and then placed in a freezer to freeze. After the leakage, phase change and expansion deformation of the metal phase change cell core material composition are inspected and found to be qualified, it is released from the warehouse.
[0028] Furthermore, the metal phase change cell shell composition in the extrusion-filling-encapsulation integrated phase change cooling metal phase change cell processing method of this embodiment includes 9 kg of nickel powder, 4.5 kg of tin powder, 2 kg of silicon powder, 0.3 kg of vanadium powder and 0.03 kg of aluminum powder.
[0029] Furthermore, the freezing point of the metal phase change core material composition in this embodiment is -35°C.
[0030] Furthermore, the metal phase change cell core material composition in the extrusion-filling-encapsulation integrated phase change cooling metal phase change cell processing method of this embodiment includes, by weight, 28 kg of glycerol, 22 kg of ethanol, 55 kg of nanofluid, 60 kg of deionized water, 5 kg of modified silica nanoparticles, and 5 kg of nucleating agent.
[0031] Furthermore, in this embodiment, the nanofluid in the integrated extrusion-filling-encapsulation phase change cooling metal phase change cell processing method is a nanoparticle suspension.
[0032] Furthermore, in this embodiment, the nucleating agent in the integrated extrusion-filling-encapsulation phase change cooling metal phase change cell processing method is carbon nanotubes.
[0033] Furthermore, in step one of the extrusion-filling-encapsulation integrated phase change cooling metal phase change cell processing method of this embodiment, the temperature of the metal phase change cell shell composition in the high-temperature furnace is 1750°C, and the melting time is 6 hours.
[0034] The phase change cooling metal phase change cell prepared in this embodiment is unaffected in a high-temperature environment of 100°C, and the phase change material does not leak or fail. When the phase change cooling metal phase change cell is exposed to a low-temperature environment of -40°C, its performance is unaffected, the phase change material does not crystallize, and it does not lose its phase change properties.
[0035] Example 2
[0036] An integrated extrusion-filling-encapsulation method for processing phase change cooled metal phase change cells includes the following steps:
[0037] Step 1: The metal phase change cell shell composition is placed in a high-temperature furnace for melting, so that the metal phase change cell shell composition is melted into a metal solution;
[0038] Step 2: The molten metal from Step 1 is cooled or stamped using a die-casting mold to form a metal phase transformation cell shell;
[0039] Step 3: Grind the surface of the metal phase change cell shell to remove burrs. After passing the first inspection, it is transported to the automatic filling line by a vibratory feeder for filling of the metal phase change cell core material composition.
[0040] Step 4: After the metal phase change crystal cell core material composition is filled and frozen, it is inspected for leakage, phase change and expansion deformation before it is released from the warehouse.
[0041] Furthermore, the metal phase change cell shell composition in the extrusion-filling-encapsulation integrated phase change cooling metal phase change cell processing method of this embodiment includes 8 kg of nickel powder, 3 kg of tin powder, 1 kg of silicon powder, 0.25 kg of vanadium powder and 0.02 kg of aluminum powder.
[0042] Furthermore, the freezing point of the metal phase change core material composition in this embodiment is -30°C.
[0043] Furthermore, the metal phase change cell core material composition in the extrusion-filling-encapsulation integrated phase change cooling metal phase change cell processing method of this embodiment includes, by weight, 24 kg of glycerol, 21 kg of ethanol, 50 kg of nanofluid, 55 kg of deionized water, 4 kg of modified silica nanoparticles, and 4 kg of nucleating agent.
[0044] Furthermore, in this embodiment, the nanofluid in the integrated extrusion-filling-encapsulation phase change cooling metal phase change cell processing method is a magnetic nanofluid.
[0045] Furthermore, in this embodiment, the nucleating agent in the integrated extrusion-filling-encapsulation phase change cooling metal phase change cell processing method is boron carbide.
[0046] Furthermore, in step one of the extrusion-filling-encapsulation integrated phase change cooling metal phase change cell processing method of this embodiment, the temperature of the metal phase change cell shell composition in the high-temperature furnace is 2000°C, and the melting time is 3 hours.
[0047] The phase change cooling metal phase change cell prepared in this embodiment is unaffected in a high-temperature environment of 100°C, and the phase change material does not leak or fail. When the phase change cooling metal phase change cell is exposed to a low-temperature environment of -40°C, its performance is unaffected, the phase change material does not crystallize, and it does not lose its phase change properties.
[0048] Example 3
[0049] An integrated extrusion-filling-encapsulation method for processing phase change cooled metal phase change cells includes the following steps:
[0050] Step 1: The metal phase change cell shell composition is placed in a high-temperature furnace for melting, so that the metal phase change cell shell composition is melted into a metal solution;
[0051] Step 2: The molten metal from Step 1 is cooled or stamped using a die-casting mold to form a metal phase transformation cell shell;
[0052] Step 3: Grind the surface of the metal phase change cell shell to remove burrs. After passing the first inspection, it is transported to the automatic filling line by a vibratory feeder for filling of the metal phase change cell core material composition.
[0053] Step 4: After the metal phase change crystal cell core material composition is filled and frozen, it is inspected for leakage, phase change and expansion deformation before it is released from the warehouse.
[0054] Furthermore, the metal phase change cell shell composition in the extrusion-filling-encapsulation integrated phase change cooling metal phase change cell processing method of this embodiment includes 10 kg of nickel powder, 6 kg of tin powder, 3 kg of silicon powder, 0.4 kg of vanadium powder and 0.05 kg of aluminum powder.
[0055] Furthermore, the freezing point of the metal phase change core material composition in this embodiment is -40°C.
[0056] Furthermore, the metal phase change cell core material composition in the extrusion-filling-encapsulation integrated phase change cooling metal phase change cell processing method of this embodiment includes, by weight, 20 kg of glycerol, 20 kg of ethanol, 45 kg of nanofluid, 50 kg of deionized water, 6 kg of modified silica nanoparticles, and 6 kg of nucleating agent.
[0057] Furthermore, in this embodiment, the nanofluid in the integrated extrusion-filling-encapsulation phase change cooling metal phase change cell processing method is a graphene liquid.
[0058] Furthermore, in this embodiment, the nucleating agent in the integrated extrusion-filling-encapsulation phase change cooling metal phase change cell processing method is boron nitride.
[0059] Furthermore, in the integrated phase change cooling metal phase change cell processing method of extrusion-filling-encapsulation in this embodiment, the temperature of the metal phase change cell shell composition in step one is 1500°C and the melting time is 10h.
[0060] The phase change cooling metal phase change cell prepared in this embodiment is unaffected in a high-temperature environment of 100°C, and the phase change material does not leak or fail. When the phase change cooling metal phase change cell is exposed to a low-temperature environment of -40°C, its performance is unaffected, the phase change material does not crystallize, and it does not lose its phase change properties.
[0061] The above description is merely an embodiment of the present invention and is not intended to limit the invention. Various modifications and variations can be made to the present invention by those skilled in the art. Any modifications, equivalent substitutions, improvements, etc., made within the spirit and principle of the present invention should be included within the scope of the claims of the present invention.
Claims
1. An integrated extrusion-impregnation-encapsulation phase change cooling metal phase cell processing method, characterized in that, Includes the following steps: Step 1: The metal phase change cell shell composition is placed in a high-temperature furnace for smelting, so that the metal phase change cell shell composition is melted into a metal solution; the metal phase change cell shell composition includes 8-10 parts by weight of nickel powder, 3-6 parts by weight of tin powder, 1-3 parts by weight of silicon powder, 0.25-0.4 parts by weight of vanadium powder and 0.02-0.05 parts by weight of aluminum powder; Step 2: The molten metal from Step 1 is cooled or stamped using a die-casting mold to form a metal phase transformation cell shell; Step 3: Grind the surface of the metal phase change cell shell to remove burrs. After passing the first inspection, it is conveyed to the automatic filling line via a vibratory feeder for filling of the metal phase change cell core material composition. The freezing point of the metal phase change cell core material composition is -30~-40℃. The metal phase change cell core material composition includes, by weight, 20-28 parts of glycerol, 20-22 parts of ethanol, 45-55 parts of nanofluid, 50-60 parts of deionized water, 4-6 parts of modified silica nanoparticles, and 4-6 parts of nucleating agent. Step 4: After the metal phase change cell core material composition is filled, it is sealed by welding and polished, and then placed in a freezer to freeze. After the leakage, phase change and expansion deformation of the metal phase change cell core material composition are inspected and found to be qualified, it is released from the warehouse.
2. The method of claim 1, wherein the method is characterized by: The nanofluid is at least one of nanoparticle suspension, magnetic nanofluid, nanogel, and graphene liquid.
3. The integrated extrusion-filling-encapsulation method for processing phase change cooled metal phase change cells according to claim 2, characterized in that, The nucleating agent is at least one of carbon nanotubes, boron carbide, and boron nitride.
4. The integrated extrusion-filling-encapsulation method for processing phase change cooled metal phase change cells according to claim 1, characterized in that, In step one, the temperature of the metal phase transformation cell shell composition in the high-temperature furnace is 1500-2000℃, and the melting time is 3-10h.
Citation Information
Patent Citations
Chloroplast-imitated base grain high-efficiency phase change heat storage capsule
CN117229758A
Copper-based phase change capsule packaging method for long-term high-temperature heat storage
CN117884583A
Phase change capsule preparation tool
CN218609303U