Lithium battery insulating film and preparation method thereof

By using a mixed heating process of composite insulating mold additives such as glass fiber and mica and polypropylene, a lithium battery insulation film with high temperature resistance is prepared, and an electrolyte storage structure is set on the film to solve the problem of poor high temperature resistance of the lithium battery insulation film. problems and improve the safety and service life of lithium batteries.

CN118745259APending Publication Date: 2024-10-08广东瑞浦兰钧能源有限公司
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202410821115.0
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-06-24
Publication Date
2024-10-08

AI Technical Summary

Technical Problem

The insulating film of lithium batteries has poor high-temperature resistance and is prone to failure under high-temperature conditions, and may even cause explosion or heat spread.

Method used

Using composite insulation mold additives, including glass fiber and mica, combined with polypropylene for mixing and heating and curing, a lithium battery insulation film with improved high temperature resistance is prepared, and an electrolyte storage structure is set on the film to optimize the distribution of the electrolyte.

Benefits of technology

It effectively improves the high temperature resistance of the lithium battery insulation film, enhances the safety and life of the lithium battery, and avoids failure and safety hazards caused by high temperature.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118745259A_ABST
    Figure CN118745259A_ABST
Patent Text Reader

Abstract

The invention belongs to the technical field of lithium batteries, and discloses a lithium battery insulating film and a preparation method thereof.The preparation method of the lithium battery insulating film comprises the steps that S1, a composite insulating film additive accounting for 5%-20% of the weight of raw materials and polypropylene accounting for 80%-95% of the weight of the raw materials are weighed, mixing the weighed composite insulation mold additive and polypropylene; s2, heating and curing the mixed composite insulating film additive and polypropylene to form an insulating film of the lithium battery, wherein the composite insulating mold additive comprises one or two of glass fibers and mica. According to the preparation method of the lithium battery insulating film provided by the invention, the composite insulating film additive and the polypropylene are mixed, so that the high temperature resistance of the lithium battery insulating film is effectively improved, the safety of a lithium battery is further improved, and the service life of the lithium battery is further prolonged.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention belongs to the technical field of lithium batteries, and in particular relates to a lithium battery insulating film and a preparation method thereof. Background Art

[0002] As an indispensable component of new energy equipment, lithium battery products have the advantages of high energy density, good cycle performance, small size, high voltage and environmental friendliness, and are widely used in fields such as electric vehicles, household energy storage, portable batteries, digital batteries, etc. The lithium battery core uses low-melting-point polymer materials such as polyethylene and polypropylene, with a melting point of less than 200°C, while the melting point of polyethylene terephthalate is about 250°C. The failure of lithium batteries will exceed the above temperature, and serious failure may even cause explosion or heat spread.

[0003] Therefore, how to improve the high temperature resistance of lithium battery insulating films is a technical problem that needs to be solved urgently. Summary of the invention

[0004] In order to solve the technical problem that the high temperature resistance of the above-mentioned lithium battery insulating film is poor, the present invention provides a lithium battery insulating film and a preparation method thereof.

[0005] In a first aspect, the present invention provides a method for preparing a lithium battery insulating film, comprising:

[0006] Step S1, weighing 5%-20% of the raw material weight percentage of the composite insulation mold additive and 80-95% of the raw material weight percentage of polypropylene, and mixing the weighed composite insulation mold additive and polypropylene;

[0007] Step S2, heating and curing the mixed composite insulating mold additive and polypropylene to form an insulating film of a lithium battery;

[0008] The composite insulating mold additive includes one or two of glass fiber and mica.

[0009] Preferably, in step S1, 15%-20% by weight of the composite insulating mold additive and 80%-85% by weight of the polypropylene are weighed.

[0010] Preferably, if the composite insulating film additive includes two of the glass fiber and the mica, the respective proportions of the glass fiber and the mica are 25%-75% of the composite insulating film additive.

[0011] Preferably, an antioxidant is also added in step S2.

[0012] Preferably, after step S2, the method further includes: providing a plurality of electrolyte storage structures on the lithium battery insulating film.

[0013] In a second aspect, the present invention further provides a lithium battery insulating film, which uses a method for preparing a lithium battery insulating film as described in any one of the first aspects above, wherein the lithium battery insulating film includes a base film for wrapping the bottom surface of a bare battery cell, a first side film symmetrically arranged along the two long sides of the base film, and a second side film symmetrically arranged along the two short sides of the base film.

[0014] Preferably, it includes: a plurality of electrolyte storage structures are arranged on the lithium battery insulating film, and the electrolyte storage structures are arranged in an S shape on the first side film and the second side film.

[0015] Preferably, the lithium battery insulating film comprises: a composite insulating mold additive with a raw material weight percentage of 5%-20% and polypropylene with a raw material weight percentage of 80-95%, wherein the composite insulating mold additive comprises one or both of glass fiber and mica.

[0016] Preferably, the electrolyte storage structure is a flat pit.

[0017] Preferably, the diameter of the pit is 2mm-10mm.

[0018] Compared with the prior art, the preparation method of the lithium battery insulating film provided by the present invention forms an insulating film for a lithium battery by mixing, heating and curing a composite insulating mold additive having a raw material weight percentage of 5%-20% and polypropylene having a raw material weight percentage of 80-95%. The formed insulating film effectively improves the high temperature resistance of the lithium battery insulating film, and further improves the safety and life of the lithium battery. BRIEF DESCRIPTION OF THE DRAWINGS

[0019] In order to more clearly illustrate the embodiments of the present invention or the technical solutions in the prior art, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are only part of the embodiments of the present invention, rather than all of the embodiments. For ordinary technicians in this field, without paying creative work, other drawings obtained based on these drawings all fall within the scope of protection of the present invention.

[0020] Figure 1 A schematic diagram of a process for preparing a lithium battery insulating film according to an embodiment of the present invention;

[0021] Figure 2 A schematic diagram of the structure of a lithium battery insulating film provided by an embodiment of the present invention;

[0022] Figure 3 An enlarged schematic diagram of an electrolyte storage structure provided for an embodiment of the invention.

[0023] Among them, 10 is a bottom membrane, 20 is a first side membrane, 30 is a second side membrane, and 40 is an electrolyte storage structure. DETAILED DESCRIPTION

[0024] In order to make the purpose, technical solution and advantages of the present invention more clearly understood, the present invention is further described in detail below in conjunction with the accompanying drawings and specific embodiments. It should be understood that the specific embodiments described herein are only used to explain the present invention and are not used to limit the present invention.

[0025] In order to make the description of the content of the present invention more detailed and complete, the following is an illustrative description of the implementation method and specific examples of the present invention; however, this is not the only form of implementing or applying the specific embodiments of the present invention. The implementation method covers the features of multiple specific embodiments and the method steps and their sequence for constructing and operating these specific embodiments. However, other specific embodiments can also be used to achieve the same or equal functions and step sequences. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without making creative work are within the scope of protection of the present invention.

[0026] It should be noted that the terms "first", "second", etc. in the specification and claims of the present invention and the above-mentioned drawings are used to distinguish similar objects, and are not necessarily used to describe a specific order or sequence. It should be understood that the numbers used in this way can be interchanged where appropriate, so that the embodiments of the present invention described herein can be implemented in an order other than those illustrated or described herein.

[0027] In the description of the embodiments of the present invention, unless otherwise specified, “ / ” means or, for example, A / B can mean A or B; “and / or” in the text is merely a description of the association relationship of associated objects, indicating that three relationships may exist, for example, A and / or B can mean: A exists alone, A and B exist at the same time, and B exists alone. In addition, in the description of the embodiments of the present invention, “multiple” means two or more than two, and other quantifiers are similar. It should be understood that the preferred embodiments described herein are only used to illustrate and explain the present invention, and are not used to limit the present invention, and the embodiments of the present invention and the features in the embodiments may be combined with each other without conflict.

[0028] In order to solve the technical problem that the high temperature resistance of the above-mentioned lithium battery insulating film is poor, the present invention provides a method for preparing a lithium battery insulating film, please refer to Figure 1 , Figure 1A flow chart of a method for preparing a lithium battery insulating film provided for an embodiment of the invention, the method for preparing a lithium battery insulating film comprising: step S1, weighing a composite insulating mold additive with a raw material weight percentage of 5%-20% and polypropylene with a raw material weight percentage of 80-95%, and mixing the weighed composite insulating mold additive and polypropylene; step S2, heating and curing the mixed composite insulating mold additive and polypropylene to form an insulating film for a lithium battery; wherein the composite insulating mold additive comprises one or both of glass fiber and mica.

[0029] Specifically, in an embodiment of the present invention, 5%-20% of the composite insulating mold additive and 80-95% of polypropylene can be weighed according to the percentage of the weight of the raw materials, and the weighed composite insulating mold additive and polypropylene are mixed through a dispersion grinder. Finally, the mixed composite insulating mold additive and polypropylene are heated and cured in an oven to form an insulating film for a lithium battery.

[0030] It should be noted that the composite insulation mold additive includes one or two of glass fiber and mica. The composite insulation mold additive can be glass fiber, mica, or a mixture of glass fiber and mica. Among them, glass fiber is an inorganic non-metallic material with excellent performance, a wide variety, and has the advantages of good insulation, strong heat resistance, good corrosion resistance, and high mechanical strength. It is made of six kinds of minerals, namely pyrophyllite, quartz sand, limestone, dolomite, calcium borate, and magnesium borate, as raw materials through high-temperature melting, wire drawing, winding, weaving and other processes. The diameter of its monofilament is from several microns to more than twenty microns, which is equivalent to 1 / 20-1 / 5 of a hair. Each bundle of fiber raw fibers is composed of hundreds or even thousands of monofilaments. Due to its brittleness, the amount of addition alone cannot be higher than 20%, and the filaments are evenly distributed in the polypropylene material. The glass fiber used in the embodiment of the present invention can be alkali-free glass fiber or other types of glass fiber, which can be set according to actual needs, and the present invention does not make further restrictions.

[0031] As an implementation mode, in the step S1, a composite insulating mold additive with a raw material weight percentage of 15%-20% and polypropylene with a raw material weight percentage of 80%-85% are weighed. Specifically, in the embodiment of the present invention, when the insulating film is prepared by using the composite insulating mold additive with a raw material weight percentage of 15%-20% and polypropylene with a raw material weight percentage of 80%-85%, the use effect of the lithium battery insulating mold is better, and the prepared lithium battery insulating film is more thermally conductive and high temperature resistant.

[0032] As an implementation mode, if the composite insulating film additive includes two of the glass fiber and the mica, the ratio of the glass fiber and the mica is 25%-75% of the composite insulating film additive. Specifically, in the embodiment of the present invention, when the composite insulating film additive includes two materials, glass fiber and mica, 25-75% of the glass fiber and 25-75% of the mica can be weighed according to the weight percentage of the raw materials, and then the weighed glass fiber and mica are added to a dispersion grinder for mixing, so as to obtain a composite insulating film additive with thermal conductivity and high temperature resistance.

[0033] As an implementation method, an antioxidant is also added in step S2. Specifically, in the embodiment of the present invention, when preparing the lithium battery insulating film, an antioxidant is also added to enhance the oxidation resistance of the lithium battery insulating film, making the lithium battery insulating layer more stable, thereby increasing the service life of the lithium battery.

[0034] As an implementation mode, after step S2, it further includes: setting a plurality of electrolyte storage structures on the insulating film of the lithium battery. Specifically, in the embodiment of the present invention, a plurality of electrolyte storage structures can be set on the insulating film of the lithium battery. Generally, the electrolyte will be concentrated at the bottom of the battery cell due to gravity. The present invention sets a plurality of electrolyte storage structures with pit structures on the insulating film, which can more evenly release the electrolyte originally stored in the pits to replenish the battery cell body, so that the electrolyte can be more easily migrated from the pits to the inside of the battery cell in the later stage, so as to improve the capacity attenuation caused by the drying of the electrolyte in the battery cell cycle.

[0035] The present invention discloses a lithium battery insulating film and a preparation method thereof, wherein the preparation method of the lithium battery insulating film comprises: step S1, weighing a composite insulating mold additive with a raw material weight percentage of 5%-20% and a polypropylene with a raw material weight percentage of 80-95%, and mixing the weighed composite insulating mold additive and polypropylene; step S2, heating and curing the mixed composite insulating mold additive and polypropylene to form an insulating film of the lithium battery; wherein the composite insulating mold additive comprises one or two of glass fiber and mica. The preparation method of the lithium battery insulating film provided by the present invention effectively improves the high temperature resistance of the lithium battery insulating film by mixing the composite insulating mold additive and polypropylene, and further improves the safety and life of the lithium battery.

[0036] The present invention also provides a lithium battery insulating film, please refer to Figure 2 , Figure 2The present invention provides a schematic structural diagram of a lithium battery insulating film provided in an embodiment of the present invention. The lithium battery insulating film is applied with the above-mentioned method for preparing the lithium battery insulating film. The lithium battery insulating film includes a base film 10 for wrapping the bottom surface of a bare battery cell, a first side film 20 symmetrically arranged along the two long sides of the base film, and a second side film 30 symmetrically arranged along the two short sides of the base film. Specifically, in an embodiment of the present invention, the lithium battery insulating film includes a base film for wrapping the bottom surface of a bare battery cell and a first side film 20 and a second side film 30 for wrapping the side surfaces of the bare battery cell. The lithium battery insulating film can isolate the positive and negative electrodes of the lithium battery to prevent short circuits, and also absorb the electrolyte solution necessary for the electrochemical reaction in the lithium battery, ensuring high ionic conductivity and stopping the reaction when an abnormality occurs in the lithium battery, thereby improving the safety of the lithium battery.

[0037] As an implementation mode, a plurality of electrolyte storage structures 40 are provided on the lithium battery insulating film, and the electrolyte storage structures are arranged in an S shape on the first side film 20 and the second side film 30. Specifically, in the embodiment of the present invention, a plurality of electrolyte storage structures 40 are provided on the lithium battery insulating film, and the electrolyte in the electrolyte storage structure 40 overflows to the surface of the battery cell after being squeezed to replenish the consumed electrolyte, so that the electrolyte can be more easily migrated from the pit to the inside of the battery cell later, thereby avoiding the consumption of electrolyte during the battery cycle and causing lithium deposition in the battery cell, and effectively improving the safety performance and service life of the battery.

[0038] As an embodiment, the lithium battery insulating film includes: a composite insulating mold additive with a raw material weight percentage of 5%-20% and a polypropylene with a raw material weight percentage of 80-95%, wherein the composite insulating mold additive includes one or two of glass fiber and mica. Specifically, in an embodiment of the present invention, 5%-20% of the composite insulating mold additive and 80-95% of the polypropylene can be weighed according to the weight percentage of the raw materials, and the weighed composite insulating mold additive and polypropylene are mixed through a dispersion grinder. Finally, the mixed composite insulating mold additive and polypropylene are heated and cured in an oven to form an insulating film for a lithium battery. It should be noted that when the raw materials of the insulating film are 15%-20% of the composite insulating mold additive and 80-85% of the polypropylene, the lithium battery insulating mold prepared is more thermally conductive and high temperature resistant.

[0039] As an implementation method, please refer to Figure 3 , Figure 3 An enlarged schematic diagram of an electrolyte storage structure provided in an embodiment of the invention, wherein the electrolyte storage structure is a flat pit. Specifically, in an embodiment of the invention, the electrolyte storage structure is a pit structure, and the pit is flattened to make it easier for the electrolyte to migrate out of the pit to the inside of the battery cell in the later stage, thereby improving the capacity attenuation caused by the drying of the electrolyte during the battery cell cycle.

[0040] As an implementation, the diameter of the pit is 2 mm to 10 mm. Specifically, in the embodiment of the present invention, the diameter of the pit can be 2 mm to 10 mm, which is specifically set according to the size of the lithium battery and the lithium battery insulating film, and the embodiment of the present invention does not make any specific restrictions.

[0041] In the several embodiments provided by the present invention, it should be understood that the disclosed devices and methods can be implemented in other ways. For example, the device embodiments described above are only schematic, for example, the division of units is only a logical function division, and there may be other division methods in actual implementation, such as multiple units or components can be combined or integrated into another system, or some features can be ignored or not executed. Another point is that the mutual coupling or direct coupling or communication connection shown or discussed can be through some interfaces, indirect coupling or communication connection of devices or units, which can be electrical, mechanical or other forms.

[0042] In addition, each functional unit in each embodiment of the present invention may be integrated into one processing unit, or each unit may exist physically separately, or two or more units may be integrated into one unit. The above integrated unit may be implemented in the form of hardware or in the form of software functional units. The above is only an implementation mode of the present invention, and does not limit the patent scope of the present invention. Any equivalent structure or equivalent process transformation made by using the contents of the present invention specification and drawings, or directly or indirectly used in other related technical fields, are also included in the patent protection scope of the present invention.

[0043] The above are only preferred embodiments of the present invention, and are not intended to limit the present invention in any form. Although the present invention has been disclosed as above in the form of preferred embodiments, it is not intended to limit the present invention. Any technical personnel in the field can make some changes or modify the technical contents disclosed above into equivalent embodiments without departing from the scope of the technical solution of the present invention. However, any brief modifications, equivalent changes and modifications made to the above embodiments based on the technical essence of the present invention without departing from the content of the technical solution of the present invention are still within the scope of the technical solution of the present invention.

Claims

1. A method for preparing a lithium battery insulating film, characterized in that: include: Step S1, weighing 5%-20% of the raw material weight percentage of the composite insulation mold additive and 80-95% of the raw material weight percentage of polypropylene, and mixing the weighed composite insulation mold additive and polypropylene; Step S2, heating and curing the mixed composite insulating mold additive and polypropylene to form an insulating film of a lithium battery; The composite insulating mold additive includes one or two of glass fiber and mica.

2. The method for preparing a lithium battery insulating film according to claim 1, characterized in that: In the step S1, 15%-20% of the composite insulating mold additive and 80%-85% of the polypropylene are weighed.

3. The method for preparing a lithium battery insulating film according to claim 2, characterized in that: If the composite insulating film additive includes two of the glass fiber and the mica, the respective proportions of the glass fiber and the mica are 25%-75% of the composite insulating film additive.

4. The method for preparing a lithium battery insulating film according to claim 3, characterized in that: An antioxidant is also added in step S2.

5. The method for preparing a lithium battery insulating film according to claim 1, characterized in that: After step S2, the method further includes: providing a plurality of electrolyte storage structures on the lithium battery insulating film.

6. A lithium battery insulating film, characterized in that: The method for preparing a lithium battery insulating film as described in any one of claims 1 to 5 is applied, wherein the lithium battery insulating film includes a base film for wrapping the bottom surface of a bare battery cell, a first side film symmetrically arranged along the two long sides of the base film, and a second side film symmetrically arranged along the two short sides of the base film.

7. The lithium battery insulating film according to claim 6, characterized in that: include: A plurality of electrolyte storage structures are arranged on the lithium battery insulating film, and the electrolyte storage structures are arranged in an S shape on the first side film and the second side film.

8. The lithium battery insulating film according to claim 7, characterized in that: The lithium battery insulating film comprises: a composite insulating mold additive with a raw material weight percentage of 5%-20% and polypropylene with a raw material weight percentage of 80-95%, wherein the composite insulating mold additive comprises one or two of glass fiber and mica.

9. The lithium battery insulating film according to claim 8, characterized in that: The electrolyte storage structure is a flat pit.

10. The lithium battery insulating film according to claim 9, characterized in that: The diameter of the pit is 2mm-10mm.