Stress sensor prepared by laser activated chemical plating and preparation method thereof
Using laser-activated electroless plating technology, combined with flexible polymers and light-activated catalysts, a stress sensor with high sensitivity and large stretchability is prepared, which solves the contradiction between sensitivity and stretchability of traditional stress sensors and reduces production costs. , achieving low-cost, large-scale manufacturing and patterned design.
Patent Information
- Application Number
- CN202410815343.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-06-24
- Publication Date
- 2024-10-08
AI Technical Summary
Existing stretchable metal strain sensors have problems such as high manufacturing cost and complex large-scale manufacturing when balancing high sensitivity and large stretching range, which limits their application.
Laser-activated electroless plating technology is used to prepare a multi-layered stress sensor through a substrate composed of a flexible polymer and a photoactivated catalyst and a metal conductive layer formed by laser catalysis. The device is adjusted by combining the curing agent ratio, substrate thickness and laser processing method. performance, enabling low-cost, large-scale manufacturing and patterned design.
It achieves high sensitivity, large stretchability, low cost, and is suitable for large-scale manufacturing and pattern design. It solves the contradiction between sensitivity and stretchability of traditional stress sensors and reduces production costs.
Smart Images

Figure CN118745569A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the technical field of flexible electronic device preparation, and more specifically, to a stress sensor prepared by laser activated chemical plating and a preparation method thereof. Background Art
[0002] Flexible electronics is a new transformative technology that has emerged in recent years. It is the process of depositing electronic materials and devices on flexible substrates, thereby giving traditional electronic materials and devices novel properties such as bendability, foldability, and stretchability. In recent years, with the research of new materials and new processes, it has been vigorously developed in academia and industry at home and abroad.
[0003] Stretchable strain sensors are essential for the emerging field of soft electronics, including wearable and implantable devices, humanoid robots with artificial skin, and biomimetic sensory systems. For example, they can be used to treat movement disorders, detect microstrain in implanted artificial blood vessels for aortic dissection treatment, neural interface electrodes, and heartbeat monitoring. In addition, stretchable strain sensors play a key role in the construction of robotic artificial sensory systems in terms of touch sensing, joint motion control, and thermal expansion monitoring.
[0004] However, current stretchable metal strain sensors have problems such as the contradiction between high stretchability and high sensitivity, high manufacturing cost, and complex large-scale manufacturing, making it difficult for the device to have both high sensitivity and a large stretchable range. In addition, the high production cost and equipment requirements have greatly restricted the development of stress sensors.
[0005] Therefore, developing a stress sensor that can achieve both high stretchability and high sensitivity and can be mass-produced and controllably patterned at low cost is of great significance for the practical application of stress sensors. Summary of the invention
[0006] Based on the above-mentioned problems existing in the prior art, the purpose of the embodiments of the present application is to provide a stress sensor prepared by laser-activated chemical plating and a preparation method thereof. Through the laser-activated chemical plating technology, a multi-layer structure arrangement of the device is realized, which has both high sensitivity and high stretchability and is low in cost and easy for large-scale preparation and pattern design.
[0007] The technical solution adopted by the present application to solve its technical problems is: a stress sensor prepared by laser-activated chemical plating, including a sensor, the sensor including an upper layer, a substrate is arranged on the lower side of the upper layer, the substrate is composed of a flexible polymer and a light-activated catalyst, and the upper layer is a metal conductive layer formed by laser-catalyzed chemical plating and is closely connected to the bottom layer.
[0008] Furthermore, the light-activated catalyst in the substrate contains a catalyst that can undergo a replacement reaction with a chemical plating solution after being activated by light.
[0009] Furthermore, the shape and thickness of the metal layer on the surface of the sensor are affected by the laser processing method.
[0010] Furthermore, the tensile properties of the sensor are determined by the curing agent ratio and the substrate thickness.
[0011] Furthermore, the working range of the sensor is determined by the thickness of the metal layer, the doping ratio of the substrate, the laser processing method of the metal layer and the device size.
[0012] Furthermore, the flexible polymer of the substrate contains a polymer as a doped supporting substrate.
[0013] A method for preparing a stress sensor by laser activated chemical plating comprises the following steps:
[0014] S1. Mix the flexible polymer and the photoactivated catalyst in a certain proportion and stir them evenly to make the dopant evenly distributed in the substrate to form a flexible polymer colloid doped with the photoactivated catalyst. Then add a certain amount of curing agent, stir evenly and evacuate until no bubbles are generated.
[0015] S2, spraying a silicon release agent on a glass sheet, heating and drying it on a drying table, and then spin-coating the prepared polymer colloid on the glass sheet on a coating machine to form a uniformly distributed colloid, and then placing it on a drying table to heat and cure to form a film with uniform thickness;
[0016] S3, treating the film with laser as required, and cleaning the film surface with clean water after the treatment;
[0017] S4, prepare the solution required for chemical plating in proportion and stir it thoroughly, put the laser-treated film into the solution, seal it with tin foil, and put it into a constant temperature box for chemical plating;
[0018] S5. Take out the thin film, wash it with clean water and dry it, peel the thin film off the glass sheet to obtain the required sensor, and complete the preparation of the metal stress sensor.
[0019] Furthermore, in step S1, the weight ratio of the photoactivated catalyst ATO to the flexible polymer PDMS is 3%-6%, and the ratio of the curing agent to PDMS is 1:10.
[0020] Furthermore, in step S2, the silicon release agent is dried on a drying table at a temperature of 150° for 10 minutes, and the spin coating step is carried out on a coating machine at a speed of 400 r / min for 2 minutes. During heating and curing, the drying table temperature is 150° and the heating time is 5 minutes.
[0021] Furthermore, the laser processing in step S3 is to use ultraviolet laser at a laser frequency of 60kHz and a speed of 2000mm / s to perform laser activation processing on several 40mm×100mm areas on the film with a filling interval of 0.01, and then use a 20kHz laser to perform cutting processing on the edge of the area at a speed of 10mm / s;
[0022] Furthermore, in step S4, the chemical plating solution is composed of water, copper plating solution component A, and copper plating solution component B in a ratio of 15:2:1, the temperature of the thermostat is set to 30° and the humidity is set to 20%, and the chemical plating time is 4 hours.
[0023] The beneficial effects of the present invention are as follows: the present invention provides a design method for a metal stress sensor prepared by laser-activated chemical plating, the stress sensor has large stretchability and high sensitivity, and the device performance can be adjusted according to the laser processing parameters and substrate parameters, and has the characteristics of low cost and easy large-scale manufacturing and patterning. BRIEF DESCRIPTION OF THE DRAWINGS
[0024] The accompanying drawings constituting a part of the present invention are used to provide a further understanding of the present invention. The exemplary embodiments of the present invention and their descriptions are used to explain the present invention and do not constitute an improper limitation of the present invention. In the accompanying drawings:
[0025] Figure 1 This is a doped film substrate image after curing;
[0026] Figure 2 This is a picture of the doped thin film substrate after laser treatment;
[0027] Figure 3 The laser processing image is drawn using AutoCAD;
[0028] Figure 4 This is a picture of the completed device after stripping off the excess parts;
[0029] Figure 5 It is a curve diagram of device pull-up performance and resistance change; DETAILED DESCRIPTION
[0030] It should be noted that, in the absence of conflict, the embodiments and features in the embodiments of the present application may be combined with each other. The present invention will be described in detail below with reference to the accompanying drawings and in combination with the embodiments.
[0031] It should be noted that, unless otherwise specified, all technical and scientific terms used in this application have the same meanings as commonly understood by ordinary technicians in the technical field to which this application belongs.
[0032] In the present invention, unless otherwise specified, the directions used, such as "up" and "down", usually refer to the directions shown in the drawings, or to the vertical, perpendicular or gravity directions; similarly, for ease of understanding and description, "left" and "right" usually refer to the left and right shown in the drawings; "inside" and "outside" refer to the inside and outside relative to the outline of each component itself, but the above-mentioned directions are not used to limit the present invention.
[0033] like Figure 1-5 As shown, the present application provides a stress sensor prepared by laser-activated chemical plating, including a sensor, wherein the sensor includes an upper layer, a substrate is arranged on the lower side of the upper layer, the substrate is composed of a flexible polymer and a light-activated catalyst, and the upper layer is a metal conductive layer formed by laser-catalyzed chemical plating and is closely connected to the bottom layer.
[0034] The photoactivated catalyst in the substrate includes catalysts such as nano-tin antimony oxide that can undergo a replacement reaction with a chemical plating solution after being activated by laser light; the flexible polymer in the substrate includes polymers such as polydimethylsiloxane and styrene polymer that can serve as a doped supporting substrate.
[0035] The shape and thickness of the metal layer on the sensor surface are affected by the laser processing method.
[0036] The tensile properties of the sensor are determined by the curing agent ratio and substrate thickness.
[0037] The working range of the sensor is determined by the thickness of the metal layer, the substrate doping ratio, the laser processing method of the metal layer and the device size.
[0038] The mechanism of the present invention is: using laser activated chemical plating, a metal layer tightly connected to the substrate is grown on the original doped substrate according to the laser processing mode, so that when the device is stretched, cracks are generated in the surface metal layer due to stretching, causing the device resistance to produce corresponding resistance changes according to the stretching size, thereby achieving the effect of measuring the stretching degree of the device by measuring the resistance change.
[0039] Laser activated chemical plating;
[0040] The laser-activated chemical plating process includes using a laser to treat a base film doped with a photoactivated catalyst such as ATO, and placing the film in a chemical plating solution to plate a metal layer. By controlling the pattern, power, speed of the laser processing and the time, temperature, humidity and other parameters of the chemical plating, the thickness, state, position and other performance parameters of the metal layer growth can be controlled.
[0041] A method for preparing a stress sensor by laser activated chemical plating comprises the following steps:
[0042] S1. Mix PDMS and ATO in a weight ratio of 100:5 and stir them thoroughly to make the dopant evenly distributed in the substrate to form a flexible polymer colloid doped with a photoactivated catalyst. Then add a curing agent with a weight ratio of 10% of PDMS, evacuate and continue stirring until no bubbles are generated.
[0043] S2. Spray the silicone release agent on the glass sheet, heat it on a 150° drying table for 10 minutes to dry it, then spin-coat the prepared polymer colloid on a glue spreader at a speed of 400r / min for two minutes to form a uniformly distributed colloid base, and then heat it on a 150° drying table for 5 minutes to solidify it into Figure 1 A film of uniform thickness is shown.
[0044] S3, press the conductive film as Figure 2 The pattern is processed with a 60kHz laser at a speed of 2000mm / s, and then the edge of the image is cut with a 20kHz laser at a speed of 20mm / s. After processing, the film surface is cleaned with clean water. Figure 3 shown.
[0045] S4. Prepare the solution required for chemical plating by mixing water, copper plating solution component A and copper plating solution component B in a weight ratio of 15:2:1 and stir well. Put the laser-treated film into the solution, seal it with tin foil and put it into a constant temperature box set at a temperature of 30° and a humidity of 30% for chemical plating for 4 hours.
[0046] S5. Take out the film and wash it with clean water and then wipe it dry. Figure 4 As shown, the film is peeled off from the glass sheet to obtain Figure 5 The sensor shown in the figure is consistent with the preset laser pattern, and the preparation of the multi-layer stress sensor is completed. After electrical testing, the data of the sensor changing with the stretching resistance is as follows Figure 5 shown.
[0047] Obviously, the above-described embodiments are only a part of the embodiments of the present invention, rather than all the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work should fall within the scope of protection of the present invention.
[0048] It should be noted that the terms used herein are only for describing specific embodiments and are not intended to limit the exemplary embodiments according to the present application. As used herein, unless the context clearly indicates otherwise, the singular form is also intended to include the plural form. In addition, it should be understood that when the terms "comprise" and / or "include" are used in this specification, it indicates the presence of features, steps, operations, devices, components and / or combinations thereof.
[0049] It should be noted that the terms "first", "second", etc. in the specification and claims of the present application and the above-mentioned drawings are used to distinguish similar objects, and are not necessarily used to describe a specific order or sequence. It should be understood that the numbers used in this way can be interchanged where appropriate, so that the embodiments of the present application described herein can be implemented in an order other than those illustrated or described herein.
[0050] The above description is only a preferred embodiment of the present invention and is not intended to limit the present invention. For those skilled in the art, the present invention may have various modifications and variations. Any modification, equivalent replacement, improvement, etc. made within the spirit and principle of the present invention shall be included in the protection scope of the present invention.
[0051] The above is only a preferred embodiment of the present invention, and the protection scope of the present invention is not limited to the above embodiments. All technical solutions under the concept of the present invention belong to the protection scope of the present invention. It should be pointed out that for ordinary technicians in this technical field, some improvements and modifications without departing from the principle of the present invention should also be regarded as the protection scope of the present invention.
Claims
1. A stress sensor prepared by laser activated chemical plating, characterized in that: The sensor comprises an upper layer, a substrate is arranged on the lower side of the upper layer, the substrate is composed of a flexible polymer and a light-activated catalyst, and the upper layer is a metal conductive layer formed by laser catalytic chemical plating and closely connected with the bottom layer.
2. A stress sensor prepared by laser activated chemical plating according to claim 1, characterized in that: The light-activated catalyst in the substrate contains a catalyst which can undergo a replacement reaction with a chemical plating solution after being activated by light.
3. A stress sensor prepared by laser activated chemical plating according to claim 1, characterized in that: The shape and thickness of the metal layer on the sensor surface are affected by the laser processing method.
4. A stress sensor prepared by laser activated chemical plating according to claim 1, characterized in that: The tensile properties of the sensor are determined by the curing agent ratio and the substrate thickness.
5. The stress sensor prepared by laser activated chemical plating according to claim 1, characterized in that: The working range of the sensor is determined by the thickness of the metal layer, the doping ratio of the substrate, the laser processing method of the metal layer and the device size.
6. The stress sensor prepared by laser activated chemical plating according to claim 1, characterized in that: The flexible polymer of the substrate contains a polymer as a doped supporting substrate.
7. A method for preparing a stress sensor by laser activated chemical plating, characterized in that: The following steps are involved: S1. Mix the flexible polymer and the photoactivated catalyst in a certain proportion and stir them evenly to make the dopant evenly distributed in the substrate to form a flexible polymer colloid doped with the photoactivated catalyst. Then add a certain amount of curing agent, stir evenly and evacuate until no bubbles are generated. S2, spraying a silicon release agent on a glass sheet, heating and drying it on a drying table, and then spin-coating the prepared polymer colloid on the glass sheet on a coating machine to form a uniformly distributed colloid, and then placing it on a drying table to heat and cure to form a film with uniform thickness; S3, treating the film with laser as required, and cleaning the film surface with clean water after the treatment; S4, prepare the solution required for chemical plating in proportion and stir it thoroughly, put the laser-treated film into the solution, seal it with tin foil, and put it into a constant temperature box for chemical plating; S5. Take out the thin film, wash it with clean water and dry it, peel the thin film off the glass sheet to obtain the required sensor, and complete the preparation of the metal stress sensor.
8. A stress sensor prepared by laser activated chemical plating and a preparation method thereof according to claim 7, characterized in that: In the step S1, the weight ratio of the photo-activated catalyst ATO to the flexible polymer PDMS is 3%-6%, and the ratio of the curing agent to PDMS is 1:
10.
9. A stress sensor prepared by laser activated chemical plating and a preparation method thereof according to claim 7, characterized in that: The drying of the silicone release agent in step S2 is carried out by heating on a drying table at a temperature of 150° for 10 minutes, and the spin coating step is carried out on a coating machine at a speed of 400 r / min for 2 minutes. During heating and curing, the drying table temperature is 150° and the heating time is 5 minutes.
10. A stress sensor prepared by laser activated chemical plating and a preparation method thereof according to claim 7, characterized in that: The laser treatment in step S3 is to use ultraviolet laser at a laser frequency of 60kHz and a speed of 2000mm / s to perform laser activation treatment on several 40mm×100mm areas on the film with a filling interval of 0.01, and then use a 20kHz laser at a speed of 10mm / s to cut the edge of the area; In step S4, the chemical plating solution is composed of water, copper plating solution component A, and copper plating solution component B in a ratio of 15:2:
1. The temperature of the thermostat is set to 30° and the humidity is set to 20%. The chemical plating time is 4 hours.