Device and method for identifying phase purity of narrow-band-gap semiconductor material through infrared variable-temperature PL spectrum
Through the infrared temperature-changing PL spectroscopy method, using pulse pump lasers and Fourier transform infrared spectrometers, the photoluminescence spectrum of narrow bandgap semiconductor materials is measured, which solves the problem of identifying the phase purity of semiconductor materials in the existing technology and achieves rapid, accurate and Non-destructive test, suitable for phase purity analysis of narrow band gap semiconductor materials.
Patent Information
- Application Number
- CN202411082165.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-08
- Publication Date
- 2024-10-08
AI Technical Summary
Existing technologies are difficult to quickly and accurately identify the phase purity of semiconductor materials, especially narrow bandgap materials, and traditional methods require multiple experiments and special sample preparation, making it difficult to achieve in-situ characterization and non-destructive testing.
The infrared variable temperature PL spectroscopy method is used to measure the photoluminescence spectrum of narrow bandgap semiconductor materials at different temperatures through pulse pump lasers, Fourier transform infrared spectrometers and lock-in amplifiers, extract the luminescence peak energy and draw a temperature change curve. According to the curve Analyze the phase purity of the material.
It achieves rapid, accurate and non-destructive reflection of the phase purity of semiconductor materials, simplifies the testing process, has wide applicability, and the materials can still be used for device preparation after testing.
Smart Images

Figure CN118746566A_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the technical field of semiconductor material phase purity identification, and specifically relates to a device and method for identifying the phase purity of narrow-bandgap semiconductor materials by using infrared variable-temperature PL spectroscopy. Background Art
[0002] Semiconductor materials are the basis for manufacturing semiconductor devices, but semiconductor materials are prone to produce multiple crystal phases during the growth process, becoming a multiphase mixture. Semiconductor materials with different crystal phases have different electronic structures and optoelectronic properties, which will lead to a decrease in the overall performance of the material. The methods currently used to identify the phase purity of semiconductor materials mainly include X-ray diffraction, transmission electron microscopy, etc., but the information about phase purity obtained by these methods is one-sided, which is not convenient for materials that need to screen specific band gap values. If a comprehensive characterization of the material is required, samples that meet the test requirements must be prepared and multiple different experiments must be conducted, which will greatly increase the test time and make it difficult to achieve in-situ characterization. It is also difficult for samples that meet the test requirements to continue to prepare devices. These deficiencies indicate that it is necessary to find a non-destructive, convenient and accurate method to reflect the phase purity of semiconductor materials. Summary of the invention
[0003] In view of the above problems, the purpose of the present invention is to provide a device and method for identifying the phase purity of narrow-bandgap semiconductor materials by infrared variable temperature PL spectroscopy, so as to quickly and truly reflect the phase purity of the material being tested.
[0004] The specific technical solution for achieving the purpose of the present invention is: A device for identifying the phase purity of narrow-bandgap semiconductor materials by infrared variable temperature PL spectroscopy, comprising a pulse pump laser, a first and a second off-axis reflector, a cold head, a sample holder, a temperature controller, a compression refrigerator, a vacuum pump, a phase-locked amplifier, a Fourier infrared spectrometer and a computer for controlling the Fourier infrared spectrometer, and the device is characterized in that: the Fourier infrared spectrometer is connected to the computer, the Fourier infrared spectrometer contains a Michelson interferometer and a detector, and the signal output end of the detector is connected to the signal input end of the phase-locked amplifier through a circuit; the temperature controller, the compression refrigerator and the vacuum pump are respectively connected to the cold head, the cold head is provided with a sample holder, the sample is fixed on the sample holder, and the pulse pump laser is connected to the reference signal input end of the phase-locked amplifier through a circuit; the first off-axis reflector is arranged between the pulse pump laser and the cold head, and the second off-axis reflector is arranged in front of the light inlet of the Fourier infrared spectrometer and is located directly below the first off-axis reflector; The laser emitted by the pulse pump laser passes through the central hole of the first off-axis reflector and irradiates the sample on the sample holder. The modulated photoluminescence signal emitted by the sample is reflected by the first off-axis reflector and the second off-axis reflector in turn and enters the light inlet of the Fourier infrared spectrometer. The light signal after interference by the Michelson interferometer enters the detector. The frequency signal emitted by the pulse pump laser is fed into the reference signal input end of the phase-locked amplifier as the reference signal of the phase-locked amplifier. The phase-locked amplifier pre-processes the modulated photoluminescence signal, extracts the light signal from the sample and feeds it back to the detector, and finally displays the photoluminescence spectrum on the computer.
[0005] Furthermore, the reference signal fed into the phase-locked amplifier is a frequency signal for periodically switching between a high-energy pulse output state and a pump pause state generated by the pulse pump laser.
[0006] A method for identifying the phase purity of narrow-bandgap semiconductor materials by infrared variable-temperature PL spectroscopy based on the above device comprises: Measure the PL spectra of narrow bandgap semiconductor materials at different temperatures; Extract the luminescence peak energy of the PL spectrum at each temperature and draw a curve of the relationship between the peak energy and temperature; The purity of the narrow bandgap semiconductor material phase under test is identified based on the relationship curve between the peak energy and temperature; The measuring of the PL spectra of the narrow bandgap semiconductor material at different temperatures specifically includes: S1. Fix the narrow bandgap semiconductor material to be tested, i.e. the sample, on the sample holder in the cold head with vacuum grease, turn on the vacuum pump to evacuate the cold head, and when the pressure in the cold head reaches 10 -4 After reaching the specified level, turn on the compression refrigerator to cool the cold head and set the target temperature to 3K on the temperature controller. The temperature displayed on the temperature controller is the real-time temperature inside the cold head. Wait until the temperature inside the cold head drops to 3K. S2, adjust the height and position of the first off-axis reflector and the cold head, ensure that the height of the center hole of the first off-axis reflector, the height of the sample holder in the cold head and the height of the light outlet of the pulse pump laser are the same and in a straight line, set the excitation wavelength of the pulse pump laser to 600-1000nm, adjust the height of the second off-axis reflector to be consistent with the height of the first off-axis reflector, and adjust the angle of the second off-axis reflector to ensure that the modulated photoluminescence signal emitted by the sample to be tested can enter the spectrometer; S3, connecting the reference signal input terminal of the phase-locked amplifier to the pulse pump laser, and connecting the signal input terminal of the phase-locked amplifier to the signal output terminal of the detector; S4. Select CaF2 as the beam splitter of the Michelson interferometer, select InSb as the detector, set the aperture size to 0.5-8mm and the resolution to 8cm in the computer.-1 , the scanning time is 5-20min, and the PL spectra are collected when the temperature in the cold head is 3K, 4K, 5K, 8K, 10K, 15K, 20K, 30K, 40K, 50K, 60K, 77K, 90K, 110K, 130K, 150K, 180K, 210K, 240K, 270K, and 290K respectively. The temperature in the cold head is set by the temperature controller. After reaching the set temperature and stabilizing for two minutes, click to start the test in the computer; The method of identifying the purity of the narrow bandgap semiconductor material phase under test according to the relationship curve between the peak energy and the temperature is specifically as follows: As the temperature increases, the peak energy increases first and then decreases, indicating that the sample under test is a multiphase mixture with low phase purity; As the temperature increases, the peak energy changes slightly but the half-width increases, indicating that the phase purity of the narrow bandgap semiconductor material tested is high.
[0007] Compared with the traditional method of characterizing phase purity, the advantages of the present invention are: 1. This method is simple and easy to operate, has no special requirements for samples, and has wide applicability; 2. This method is convenient, economical and accurate. The phase purity of the narrow bandgap semiconductor material under test can be analyzed based on the relationship curve between the peak energy and temperature, and the true bandgap value can be obtained. If traditional characterization methods are used, this requires a combination of multiple experiments to achieve; 3. This method is non-destructive. If the material tested by infrared variable temperature PL spectrum meets the requirements, it can still be further used in the preparation of devices.
[0008] 4. Compared with the traditional mid-infrared band weak signal PL spectrum test, the present invention does not need to use mechanical chopping and the step scanning mode of the Fourier transform infrared spectrometer, but directly uses the frequency of the pulse pump laser as the reference signal of the phase-locked amplifier, which can achieve the same signal-to-noise ratio in a shorter scanning time. BRIEF DESCRIPTION OF THE DRAWINGS
[0009] Figure 1 This is a schematic diagram of the infrared variable temperature PL spectrum test experimental device; Figure 2 The temperature-variable PL principle diagram of the multiphase heterojunction structure; Figure 3 The theoretical prediction of the α-Te crystal structure diagram and energy band structure diagram is as follows: the theoretical band gap value calculated by PBE+SOC (solid line) is 1.08eV, and the theoretical band gap value calculated by HSE06+SOC (dotted line) is 1.69eV; Figure 4The theoretical prediction of the β-Te crystal structure diagram and energy band structure diagram is shown in Figure 2. The theoretical band gap value calculated by PBE+SOC (solid line) is 1.01eV, and the theoretical band gap value calculated by HSE06+SOC (dotted line) is 1.41eV. Figure 5 This is the temperature-dependent PL experimental result diagram of the narrow bandgap semiconductor material Te; Figure 6 This is the curve of the peak energy of the photoluminescence spectrum of the narrow bandgap semiconductor material Te changing with temperature. DETAILED DESCRIPTION
[0010] The present invention is described in detail below with reference to the accompanying drawings and embodiments. Example
[0011] This embodiment uses the narrow bandgap semiconductor material tellurium (Te) as the material to be tested and combines the accompanying drawings to fully and detailedly describe the technical solution of the present invention. Obviously, the described embodiment is only a part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0012] Tellurium has a band gap of 0.34 eV and is a narrow band gap semiconductor material with broad application prospects in the mid-infrared band. Tellurium has a special spiral chain structure, and the chains are bound together by Van Der Waals (VDW) interactions. Therefore, tellurium crystals are highly anisotropic in structure and have a strong one-dimensional growth tendency. However, external conditions have a huge impact on the anisotropic growth and shape evolution of tellurium. For example, when tellurium is prepared by PVD, the heating temperature and inert gas flow rate will affect the nucleation and growth of tellurium atoms, thereby producing other crystalline phases with different structures. Theoretical workers have predicted the crystal structure diagram and band structure diagram of α-Te and β-Te, as shown below: Figure 3 and Figure 4 As shown, the theoretical band gap value of α-Te calculated based on PBE+SOC (solid line) is 1.08eV, and the theoretical band gap value calculated based on HSE06+SOC (dotted line) is 1.69eV. The theoretical band gap value of β-Te calculated based on PBE+SOC (solid line) is 1.01eV, and the theoretical band gap value calculated based on HSE06+SOC (dotted line) is 1.41eV, indicating that the band gap of α-Te is larger than that of β-Te.
[0013] A method and device for identifying the phase purity of narrow-bandgap semiconductor materials by infrared variable temperature PL spectroscopy. The method takes the analysis of the phase purity of tellurium crystals prepared by PVD as an example. The tellurium crystals may contain one or more crystal phases of α-Te or β-Te, and the band gap values of these two crystal phases are different.
[0014] A device for identifying the phase purity of narrow-bandgap semiconductor materials by infrared variable temperature PL spectroscopy comprises a pulse pump laser, a first and a second off-axis reflector, a cold head, a sample holder, a temperature controller, a compression refrigerator, a vacuum pump, a lock-in amplifier, a Fourier transform infrared spectrometer and a computer for controlling the Fourier transform infrared spectrometer.
[0015] Figure 1 This is a schematic diagram of the infrared variable temperature PL spectrum test experimental device of this embodiment. The temperature controller, the compression refrigerator and the vacuum pump are connected to the cold head where the sample is placed. The Fourier infrared spectrometer, the phase-locked amplifier, the pulse pump laser, the first and second off-axis reflectors, and the off-axis reflector are all arranged on a vibration-damping table. The pulse pump laser emits a high-frequency modulated laser and is incident on the sample holder in the cold head through the small hole of the first off-axis reflector. The modulated photoluminescence signal emitted by the sample enters the Fourier infrared spectrometer after being reflected by the two off-axis reflectors. The frequency signal emitted by the pulse pump laser is fed into the reference signal input end of the phase-locked amplifier as a reference signal. The signal input end of the phase-locked amplifier is connected to the signal output end of the detector. The modulated photoluminescence signal is preprocessed, and the light signal from the sample is extracted and the photoluminescence spectrum is displayed on the computer.
[0016] The high-energy pulse output generated by the pulse pump laser can be released in a short time, and then a pump pause state appears, and these two states are switched periodically.
[0017] The frequency of the periodic switching is the reference signal fed into the lock-in amplifier.
[0018] A method for identifying the phase purity of narrow-bandgap semiconductor materials by infrared variable temperature PL spectroscopy, comprising: Measure the PL spectra of narrow bandgap semiconductor materials at different temperatures; Extract the luminescence peak energy of the PL spectrum at each temperature and draw a curve of the relationship between the peak energy and temperature; The phase purity of the narrow bandgap semiconductor material being tested is analyzed based on the relationship curve between the peak energy and the temperature.
[0019] The basic principle of the method of this embodiment is as follows: When laser light shines on semiconductor materials, electrons in the semiconductor materials can absorb the energy of photons and transition from low energy levels to high energy levels, forming non-equilibrium carriers. This is unbalanced, so electrons at high energy levels will return to a lower energy state and release excess energy in the form of light, which is photoluminescence.
[0020] Due to the differences in crystal structures of different crystalline phases of semiconductor materials, lattice parameters, lattice symmetry and defects will directly affect the arrangement and energy state of electrons in the crystal, resulting in differences in band structures and band gaps among these different crystalline phases. These differences can be reflected in the PL spectrum.
[0021] When a semiconductor material contains two or more different crystalline phases at the same time, a multiphase heterojunction structure will be formed. Due to the differences in the band structure and the Fermi level, in order to achieve an equilibrium state where the Fermi level is equal everywhere, the electrons will be rearranged. At this time, the band structure is the result of the interaction and equilibrium between the crystalline phases.
[0022] Figure 2 This is the temperature-dependent PL principle diagram of a multiphase heterojunction structure. At low temperatures, the thermal kinetic energy of carriers is very small, and electrons and holes are localized in localized states with lower energy. Under the excitation of external lasers, carriers are more inclined to transition to the vicinity of the ground state of the conduction band, and are not easy to transition to excited states with higher energy. Therefore, for semiconductor materials that contain two or more crystalline phases at the same time, at low temperatures, the PL spectrum only reflects the luminescence process of the crystalline phase with a smaller band gap. As the temperature rises, the thermal kinetic energy increases, and carriers can escape from these localized states and fill in free states or near-free states with higher energy, causing the luminescence peak position to move toward the high-energy direction. At this time, the crystalline phase with a larger band gap also begins to partially or fully participate in the luminescence process and is reflected in the PL spectrum. When the crystalline phase with a larger band gap accounts for a large proportion, there may even be two obvious luminescence peaks.
[0023] The method of measuring the PL spectra of the narrow-bandgap semiconductor material at different temperatures is based on the device for identifying the phase purity of the narrow-bandgap semiconductor material using infrared variable-temperature PL spectra, and specifically includes the following steps: S1. Fix the sample to be tested on the sample holder in the cold head with vacuum grease, turn on the vacuum pump to evacuate the cold head, and when the pressure in the cold head reaches 10 -4 After reaching the specified level, turn on the compression refrigerator to cool the cold head and set the target temperature to 3K on the temperature controller. The temperature displayed on the temperature controller is the real-time temperature inside the cold head. Wait until the temperature inside the cold head drops to 3K. S2, adjust the height and position of the off-axis reflector 1 and the cold head, ensure that the height of the center hole of the first off-axis reflector, the height of the sample holder in the cold head and the height of the light outlet of the pulse pump laser are the same and in a straight line, set the excitation wavelength of the pulse pump laser to 800nm, adjust the height of the second off-axis reflector to be consistent with the height of the first off-axis reflector, and adjust the angle of the second off-axis reflector to ensure that the modulated photoluminescence signal emitted by the narrow-bandgap semiconductor material to be measured can enter the spectrometer; S3, connecting the reference signal input terminal of the phase-locked amplifier to the pulse pump laser, and connecting the signal input terminal of the phase-locked amplifier to the signal output terminal of the detector; S4, select CaF2 as the beam splitter of the Michelson interferometer, select InSb as the detector, set the aperture size to 8mm and the resolution to 8cm in the computer -1 , the scanning time is 15min, and the PL spectra are collected when the temperature in the cold head is 3K, 4K, 5K, 8K, 10K, 15K, 20K, 30K, 40K, 50K, 60K, 77K, 90K, 110K, 130K, 150K, 180K, 210K, 240K, 270K, and 290K respectively. The temperature in the cold head is set by the temperature controller. After reaching the set temperature and stabilizing for two minutes, click to start the test in the computer. The variable temperature PL experimental results of this embodiment are shown in the figure Figure 5 shown.
[0024] The phase purity of the narrow bandgap semiconductor material under test is analyzed according to the relationship curve between the peak energy and the temperature, specifically: As the temperature increases, the peak energy increases first and then decreases, indicating that the narrow bandgap semiconductor material under test is a multiphase mixture with low phase purity; As the temperature increases, the peak energy changes slightly but the half-width increases, indicating that the phase purity of the narrow bandgap semiconductor material tested is high.
[0025] Figure 6 The curve of the variation of the peak energy of the photoluminescence spectrum of the narrow bandgap semiconductor material Te with temperature in this embodiment is as follows. As the temperature increases, the peak energy of the PL spectrum of the narrow bandgap semiconductor material Te increases first and then decreases. According to the above method for judging phase purity, the following conclusions can be drawn: The increase in peak energy is because the crystalline phase with a larger band gap begins to participate in luminescence. However, since no obvious two peaks appear in the process of increasing peak energy, it means that the crystalline phase with a larger band gap accounts for a small proportion. However, the narrow band gap semiconductor material Te being tested is still a multiphase mixture with low phase purity.
[0026] At 3K, the peak energy of the PL spectrum of the semiconductor material tellurium is about 0.3348eV. At this time, the PL spectrum only reflects the luminescence process of the crystal phase with a smaller band gap. Combined with the theoretical prediction of the band gaps of different crystal phases of tellurium materials, 0.3348eV is the band gap value of β-Te.
Claims
1. A device for identifying the phase purity of narrow-bandgap semiconductor materials by infrared variable temperature PL spectroscopy, comprising a pulsed pump laser, a first and a second off-axis reflector, a cold head, a sample holder, a temperature controller, a compression refrigerator, a vacuum pump, a lock-in amplifier, a Fourier transform infrared spectrometer and a computer for controlling the Fourier transform infrared spectrometer, characterized in that: The Fourier infrared spectrometer is connected to a computer, and includes a Michelson interferometer and a detector in the Fourier infrared spectrometer, and the signal output end of the detector is connected to the signal input end of the phase-locked amplifier through a circuit; the temperature controller, the compression refrigerator and the vacuum pump are respectively connected to a cold head, and a sample holder is arranged in the cold head, and the pulse pump laser is connected to the reference signal input end of the phase-locked amplifier through a circuit; the first off-axis reflector is arranged between the pulse pump laser and the cold head, and the second off-axis reflector is arranged in front of the light inlet of the Fourier infrared spectrometer and is located directly below the first off-axis reflector; The laser emitted by the pulse pump laser passes through the central hole of the first off-axis reflector and irradiates the sample on the sample holder. The modulated photoluminescence signal emitted by the sample is reflected by the first off-axis reflector and the second off-axis reflector in turn and enters the light inlet of the Fourier infrared spectrometer. The light signal after interference by the Michelson interferometer enters the detector. The frequency signal emitted by the pulse pump laser is fed into the reference signal input end of the phase-locked amplifier as the reference signal of the phase-locked amplifier. The phase-locked amplifier pre-processes the modulated photoluminescence signal, extracts the light signal from the sample and feeds it back to the detector, and finally displays the photoluminescence spectrum on the computer.
2. The device according to claim 1, characterized in that The reference signal fed into the phase-locked amplifier is a frequency signal for periodically switching between a high-energy pulse output state and a pump pause state generated by the pulse pump laser.
3. A method for identifying the phase purity of narrow-bandgap semiconductor materials by infrared variable temperature PL spectroscopy based on the device of claim 1, characterized in that: include: Measure the PL spectra of narrow bandgap semiconductor materials at different temperatures; Extract the luminescence peak energy of the PL spectrum at each temperature and draw a curve of the relationship between the peak energy and temperature; The purity of the narrow bandgap semiconductor material phase under test is identified based on the relationship curve between the peak energy and temperature; The measuring of the PL spectra of the narrow bandgap semiconductor material at different temperatures specifically includes: S1. Fix the narrow bandgap semiconductor material to be tested, i.e. the sample, on the sample holder in the cold head with vacuum grease, turn on the vacuum pump to evacuate the cold head, and when the pressure in the cold head reaches 10 -4 After reaching the specified level, turn on the compression refrigerator to cool the cold head and set the target temperature to 3K on the temperature controller. The temperature displayed on the temperature controller is the real-time temperature inside the cold head. Wait until the temperature inside the cold head drops to 3K. S2, adjust the height and position of the first off-axis reflector and the cold head, ensure that the height of the center hole of the first off-axis reflector, the height of the sample holder in the cold head and the height of the light outlet of the pulse pump laser are the same and in a straight line, set the excitation wavelength of the pulse pump laser to 600-1000nm, adjust the height of the second off-axis reflector to be consistent with the height of the first off-axis reflector, and adjust the angle of the second off-axis reflector to ensure that the modulated photoluminescence signal emitted by the sample to be tested can enter the spectrometer; S3, connecting the reference signal input terminal of the phase-locked amplifier to the pulse pump laser, and connecting the signal input terminal of the phase-locked amplifier to the signal output terminal of the detector; S4. Select CaF2 as the beam splitter of the Michelson interferometer, select InSb as the detector, set the aperture size to 0.5-8mm and the resolution to 8cm in the computer. -1 , the scanning time is 5-20min, and the PL spectra are collected when the temperature in the cold head is 3K, 4K, 5K, 8K, 10K, 15K, 20K, 30K, 40K, 50K, 60K, 77K, 90K, 110K, 130K, 150K, 180K, 210K, 240K, 270K, and 290K respectively. The temperature in the cold head is set by the temperature controller. After reaching the set temperature and stabilizing for two minutes, click to start the test in the computer; The method of identifying the purity of the phase of the narrow bandgap semiconductor material to be measured according to the relationship curve between the peak energy and the temperature is specifically as follows: As the temperature increases, the peak energy increases first and then decreases, indicating that the sample under test is a multiphase mixture with low phase purity; As the temperature increases, the peak energy changes slightly but the half-width increases, indicating that the phase purity of the tested samples is high.