Machining method for large-depth wedge-shaped inner cavity with irregular square contour

The one-time forming processing of the wedge-shaped inner cavity with a special square profile and a large depth through a wire cutting machine tool solves the problems of long processing time and high cost in the existing technology, improves production efficiency and quality traceability, and adapts to the trend of automated production.

CN118752018AActive Publication Date: 2024-10-11SHANXI NORTH MACHINE BUILDING
View PDF 7 Cites 0 Cited by

Patent Information

Application Number
CN202411007862.7
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-25
Publication Date
2024-10-11
Estimated Expiration
2044-07-25

AI Technical Summary

Technical Problem

The existing technology has the problems of long processing time, low production efficiency, high production cost and poor quality traceability when processing irregular square contours and large depth wedge-shaped inner cavities, especially due to the need for multiple clamping, alignment and design of special fixtures. This results in high operating intensity and high cost.

Method used

A wire cutting machine tool is used for one-time forming processing. By calculating the slope angle of the part and the guide rail slope, the processing program and trajectory are designed, and the molybdenum wire is used to cut the cavity at different movement rates, thereby achieving complete processing of the slope and straight surfaces and reducing transportation and clamping times.

Benefits of technology

It improves production efficiency, reduces production costs and labor costs, and the remaining materials after wire cutting can be completely preserved, improving quality traceability.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118752018A_ABST
    Figure CN118752018A_ABST
Patent Text Reader

Abstract

The invention relates to a machining method for a large-depth wedge-shaped inner cavity with a special-square outline, and belongs to the technical field of machining. Comprising the following steps: S1, analyzing the structure of the large-depth wedge-shaped inner cavity with the irregular square outline; s2, determining a machining original point, and calculating the position relationship among the projection contour of the cavity, the appearance of the part and the machining original point; S3, designing a machining program and a machining track according to the coordinate point parameters; according to the machining method, machining of the large-depth wedge-shaped inner cavity with the special-square outline is changed into linear cutting one-time forming machining, the labor hour consumption of transferring, repeated clamping and alignment in the original multi-procedure production process of milling, lineation, rough insertion and fine insertion is reduced, and the production efficiency is improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of mechanical processing, and in particular relates to a processing method for a wedge-shaped inner cavity with a square profile and a large depth. Background Art

[0002] The wedge-shaped cavity is a structure in a part that is used to accommodate the mating part and seal it together with the mating part. It has an irregular square outline and a wedge-shaped cavity structure. Figure 1 The whole is composed of 3 straight surfaces and 1 inclined surface. The left and right straight surfaces have a set of inclined guide surfaces with a certain angle to the longitudinal axis, which are used for the up and down sliding of the mating parts in the cavity.

[0003] The usual processing method is: milling combined with slotting, first rough-machine the bottom hole on a vertical milling machine to remove a large amount of machining allowance; then use a special marking template to draw a square outline on the upper plane of the part to be processed; then clamp a part on the slotting machine, slot the left and right sides and the front of the cavity, a total of 3 straight surfaces; then install the part on a special fixture, adjust the inclined surface of the cavity to be parallel to the main axis of the slotting machine, and slot the inclined surface and the inclined guide surface. The above processing methods have the following disadvantages:

[0004] 1) Due to the high strength of the material of a certain part and the deep depth of the cavity, in order to ensure the processing quality, the slotting process needs to be divided into rough slotting and fine slotting processes, which involves multiple clamping and alignment preparations, and the processing takes a long time and has low production efficiency;

[0005] 2) When slotting the inclined surface of the cavity, the inclined surface should be tilted according to the inclination angle α (see Figure 2 ) Make special fixtures. Facing cavity structures at different angles, it is necessary to design and make multiple sets of special fixtures. The demand is large and the scope of use is single. It is also necessary to regularly inspect and maintain the fixtures, resulting in high production costs;

[0006] 3) During slotting, the operator has high labor intensity and the parts are heavy, about 1 to 2 tons. Before rough and fine slotting, it is necessary to manually load and unload materials, turn over goods, clamp and align them many times. During the processing, the operator needs to continuously pay attention to the position line of the cavity's irregular square contour processing, which leads to high labor intensity for the workers.

[0007] 4) The quality traceability is poor. The materials removed during cavity processing become scrap iron filings during the process and have no quality traceability.

[0008] Therefore, in the absence of special fixtures and special machine tools, it is urgent to invent a processing method for a wedge-shaped cavity with a square profile and a large depth to solve the above problems. Summary of the invention

[0009] 1. Technical issues to be resolved

[0010] The technical problem to be solved by the present invention is to provide a processing method for a wedge-shaped inner cavity with a square profile and a large depth to solve the problem that the rough and fine insertion processing of the wedge-shaped inner cavity with a square profile and a large depth takes a long time and the production efficiency is low.

[0011] (II) Technical solution

[0012] In order to solve the above technical problems, the present invention provides a method for processing a wedge-shaped inner cavity with a square profile and a large depth, comprising the following steps:

[0013] S1: According to the wedge-shaped inner cavity structure of the part to be processed, the inner cavity inclined surface, the guide rail inclined surface inclination angle α and the projection contour of the inner cavity irregular square contour on the lower plane 103 are calculated with the upper plane 105 of the part as the reference;

[0014] S2: Place the part horizontally on the worktable 201 of the wire cutting machine, with the lower plane 103 of the part in close contact with the worktable 201 of the machine, and align the molybdenum wire with the front end face 101 and the left side face 102 of the part, and determine the machining origin as the center of the projection contour of the inner cavity on the upper plane 105 according to the relative coordinate positions of the front end face 101, the left side face 102 and the worktable 201;

[0015] S3: Take the machining origin as the coordinate origin, the axis of the front and rear end faces of the part passing through the coordinate origin as the X-axis, the axis of the left and right end faces of the part passing through the coordinate origin as the Y-axis, and the axis passing through the coordinate origin and perpendicular to the XOY plane as the Z-axis, establish a rectangular coordinate system, and design the machining program and machining trajectory according to the parameters of each coordinate point;

[0016] S4. Adjust the molybdenum wire on the wire cutting machine to the processing origin. According to the processing program and processing trajectory in S3 and the two projection contours of the irregular square contour of the inner cavity on the upper plane 105 and the lower plane 103 of the part, design the inclination angle of the molybdenum wire to cut the cavity, and complete the processing of the inner cavity from a straight cavity to a tapered cavity.

[0017] The inclination angle α of the guide rail slope in step S1 is measured by the projection dimension L1 of the inner cavity slope in the upper plane 105 , the projection dimension L2 in the lower plane 103 , and the cutting depth H.

[0018] Among them, the coordinate point parameters in step S3 include: the vertical distance H2 between the upper guide wheel center 202 and the lower guide wheel center 203 of the wire cutting machine, the distance H1 between the lower guide wheel center 203 of the wire cutting machine and the machine tool worktable 201, and the cutting depth H.

[0019] Among them, the cutting trajectory in step S3 is set as: taking the processing origin determined in step S2 as the starting point, the intersection of the front straight surface 104 of the cavity and the right side surface 106 as the initial cutting point, and processing along the trajectory of front straight surface 104 → left straight surface → left inclined guide surface → left straight surface → rear inclined surface → right straight surface → right inclined guide surface → right straight surface.

[0020] Wherein, the inclination angle of the molybdenum wire in step S4 is obtained by calculating the offset position A of the upper guide wheel and the offset position B of the lower guide wheel of the cutting machine tool;

[0021] Among them, A = (H2-H1) × tanα, B = H1 × tanα;

[0022] When wire cutting an inclined surface, the upper and lower guide wheels of the wire cutting machine are controlled to move at different speeds to positions A and B respectively, thereby controlling the inclination of the molybdenum wire. Then the upper and lower guide wheels are cut along the OX direction axis at the same speed until the inclined surface cutting is completed.

[0023] Among them, in step 4, when the bevel cutting is completed and the cutting is converted to straight cutting, the upper guide wheel and the lower guide wheel move to the direction perpendicular to the OX axis and cut along the X direction at the same speed until the straight cutting is completed.

[0024] (III) Beneficial effects

[0025] Compared with the prior art, the present invention has the following beneficial effects:

[0026] 1) The present invention changes the processing of the wedge-shaped inner cavity with a square profile and a large depth into a one-step forming process by wire cutting, thereby reducing the time consumption of transportation, repeated clamping and alignment in the original production process of multiple processes such as milling, scribing, rough insertion and fine insertion, and improving production efficiency;

[0027] 2) It solves the problem that the fixtures cannot be used universally when processing different structures, reduces the cost of special fixtures, and can greatly save production costs in scientific research and multi-variety, small-batch production;

[0028] 3) Adapting to the trend of automated production, workers do not need to operate the whole process, only one clamping and alignment are required, which improves labor productivity and reduces labor cost consumption;

[0029] 4) The cavity residue after wire cutting can be completely preserved, improving the quality traceability of parts production. BRIEF DESCRIPTION OF THE DRAWINGS

[0030] Figure 1 It is a schematic diagram of the parts structure;

[0031] Figure 2 for Figure 1 A cross-sectional view of

[0032] Figure 3 for Figure 1 A top view of

[0033] Figure 4 It is a schematic diagram of the cavity bevel cutting;

[0034] Among them, 1-a certain part; 2-a wedge-shaped inner cavity with a square profile and a large depth; 101-the front face of part 1; 102-the left side of part 1; 103-the bottom plane of part 1; 104-the front straight face of the wedge-shaped inner cavity with a square profile and a large depth; 105-the upper plane of part 1; 106-the right side of the wedge-shaped inner cavity with a square profile and a large depth; 107-the right side of part 1; 201-the worktable of the wire cutting machine; 202-the center of the upper guide wheel of the wire cutting machine; 203-the center of the lower guide wheel of the wire cutting machine; 204-the molybdenum wire for wire cutting. DETAILED DESCRIPTION

[0035] In order to make the purpose, content, and advantages of the present invention more clear, the specific implementation methods of the present invention are further described in detail below in conjunction with the accompanying drawings and examples.

[0036] This embodiment provides a method for processing a wedge-shaped inner cavity with a square profile and a large depth, comprising the following steps:

[0037] S1: According to the wedge-shaped inner cavity structure of the part to be processed, the inner cavity inclined surface, the guide rail inclined surface inclination angle α and the projection contour of the inner cavity irregular square contour on the lower plane 103 are calculated with the upper plane 105 of the part as the reference;

[0038] S2: Place the part horizontally on the worktable 201 of the wire cutting machine, with the lower plane 103 of the part in close contact with the worktable 201 of the machine, and align the molybdenum wire with the front end face 101 and the left side face 102 of the part, and determine the machining origin as the center of the projection contour of the inner cavity on the upper plane 105 according to the relative coordinate positions of the front end face 101, the left side face 102 and the worktable 201;

[0039] S3: Take the machining origin as the coordinate origin, the axis of the front and rear end faces of the part passing through the coordinate origin as the X-axis, the axis of the left and right end faces of the part passing through the coordinate origin as the Y-axis, and the axis passing through the coordinate origin and perpendicular to the XOY plane as the Z-axis, establish a rectangular coordinate system, and design the machining program and machining trajectory according to the parameters of each coordinate point;

[0040] S4. Adjust the molybdenum wire on the wire cutting machine to the processing origin. According to the processing program and processing trajectory in S3 and the two projection contours of the irregular square contour of the inner cavity on the upper plane 105 and the lower plane 103 of the part, design the inclination angle of the molybdenum wire to cut the cavity, and complete the processing of the inner cavity from a straight cavity to a tapered cavity.

[0041] The inclination angle α of the guide rail slope in step S1 is measured by the projection dimension L1 of the inner cavity slope in the upper plane 105 , the projection dimension L2 in the lower plane 103 , and the cutting depth H.

[0042] The coordinate point parameters in step S3 include: the vertical distance H2 between the upper guide wheel center 202 and the lower guide wheel center 203 of the wire cutting machine, the distance H1 between the lower guide wheel center 203 of the wire cutting machine and the machine tool worktable 201, and the cutting depth H;

[0043] Among them, the cutting trajectory in step S3 is set as: taking the processing origin determined in step S2 as the starting point, the intersection of the front straight surface 104 of the cavity and the right side surface 106 as the initial cutting point, and processing along the trajectory of front straight surface 104 → left straight surface → left inclined guide surface → left straight surface → rear inclined surface → right straight surface → right inclined guide surface → right straight surface.

[0044] Wherein, the inclination angle of the molybdenum wire in step S4 is obtained by calculating the offset position A of the upper guide wheel and the offset position B of the lower guide wheel of the cutting machine tool;

[0045] Among them, A = (H2-H1) × tanα, B = H1 × tanα;

[0046] When wire cutting an inclined surface, the upper and lower guide wheels of the wire cutting machine are controlled to move at different speeds to positions A and B respectively, thereby controlling the inclination of the molybdenum wire. Then the upper and lower guide wheels are cut along the OX direction axis at the same speed until the inclined surface cutting is completed.

[0047] Among them, in step 4, when the bevel cutting is completed and the cutting is converted to straight cutting, the upper guide wheel and the lower guide wheel move to the direction perpendicular to the OX axis and cut along the X direction at the same speed until the straight cutting is completed.

[0048] In step S2, the length L3 of the front straight surface 104 of the inner cavity from the front end surface 101 of the part and the width L6 of the part are measured, and the positional relationship between the projection contour of the inner cavity on the lower plane 103 of the part and the part shape and the processing origin is calculated;

[0049] The projection profile of the irregular square shape of the inner cavity in the lower plane 103 is calculated by the size of the guide rail wide inclined surface L4 and the guide rail narrow inclined surface L5.

[0050] The above is only a preferred embodiment of the present invention. It should be pointed out that for ordinary technicians in this technical field, several improvements and modifications can be made without departing from the technical principles of the present invention. These improvements and modifications should also be regarded as the scope of protection of the present invention.

Claims

1. A method for processing a wedge-shaped inner cavity with a square profile and a large depth, characterized in that: The following steps are involved: S1: According to the wedge-shaped inner cavity structure of the part to be processed, the inner cavity inclined surface, the guide rail inclined surface inclination angle α and the projection contour of the inner cavity irregular square contour on the lower plane 103 are calculated with the upper plane 105 of the part as the reference; S2: Place the part horizontally on the worktable 201 of the wire cutting machine, with the lower plane 103 of the part in close contact with the worktable 201 of the machine, and align the molybdenum wire with the front end face 101 and the left side face 102 of the part, and determine the machining origin as the center of the projection contour of the inner cavity on the upper plane 105 according to the relative coordinate positions of the front end face 101, the left side face 102 and the worktable 201; S3: Take the machining origin as the coordinate origin, the axis of the front and rear end faces of the part passing through the coordinate origin as the X-axis, the axis of the left and right end faces of the part passing through the coordinate origin as the Y-axis, and the axis passing through the coordinate origin and perpendicular to the XOY plane as the Z-axis, establish a rectangular coordinate system, and design the machining program and machining trajectory according to the parameters of each coordinate point; S4. Adjust the molybdenum wire on the wire cutting machine to the processing origin. According to the processing program and processing trajectory in S3 and the two projection contours of the irregular square contour of the inner cavity on the upper plane 105 and the lower plane 103 of the part, design the inclination angle of the molybdenum wire to cut the cavity and complete the processing of the inner cavity.

2. The method for processing a wedge-shaped inner cavity with a square profile and a large depth as claimed in claim 1, characterized in that: In step S1 , the inclination angle α of the guide rail inclined surface is measured by the projection dimension L1 of the inner cavity inclined surface in the upper plane 105 , the projection dimension L2 in the lower plane 103 , and the cutting depth H.

3. The method for processing a wedge-shaped inner cavity with a square profile and a large depth as claimed in claim 2, characterized in that: The coordinate point parameters in step S3 include: the vertical distance H2 between the upper guide wheel center 202 and the lower guide wheel center 203 of the wire cutting machine, the distance H1 between the lower guide wheel center 203 of the wire cutting machine and the machine tool worktable 201, and the cutting depth H.

4. The method for processing a wedge-shaped inner cavity with a square profile and a large depth as claimed in claim 3, characterized in that: The cutting trajectory in step S3 is set as follows: taking the processing origin determined in step S2 as the starting point, the intersection of the front straight surface 104 and the right side surface 106 of the cavity as the initial cutting point, and processing along the trajectory of front straight surface 104 → left straight surface → left inclined guide surface → left straight surface → rear inclined surface → right straight surface → right inclined guide surface → right straight surface.

5. The method for processing a wedge-shaped inner cavity with a square profile and a large depth as claimed in claim 4, characterized in that: In step S4, the inclination angle of the molybdenum wire is obtained by calculating the offset position A of the upper guide wheel and the offset position B of the lower guide wheel of the cutting machine; Among them, A = (H2-H1) × tanα, B = H1 × tanα; When wire cutting an inclined surface, the upper and lower guide wheels of the wire cutting machine are controlled to move at different speeds to positions A and B respectively, thereby controlling the inclination of the molybdenum wire. Then the upper and lower guide wheels are cut along the OX direction axis at the same speed until the inclined surface cutting is completed.

6. The method for processing a wedge-shaped inner cavity with a square profile and a large depth as claimed in claim 5, characterized in that: In step 4, when the bevel cutting is completed and the cutting is converted to straight cutting, the upper guide wheel and the lower guide wheel move to a direction perpendicular to the OX axis and cut along the X direction at the same speed until the straight cutting is completed.

Citation Information

Patent Citations

  • Wire electric discharge machine which performs taper cutting

    CN104096928A

  • Method for accurately controlling central symmetry of inner hole key groove and tooth parts or tooth groove of bevel gear

    CN110369773A

  • Guide hole machining method

    CN113245647A

  • Linear cutting tool and machining method for canard base body

    CN113579382A

  • Irregular casting machining method based on vector projection deviation compensation

    CN115816167A