Method for preparing alkali by using sodium sulfate

By mixing sodium sulfate, activated calcium oxide, sodium metaaluminate and calcium aluminate cement according to a specific ratio to generate a sodium hydroxide solution, the problem of processing the sodium salt flue gas desulfurization product Na2SO4 is solved, and the regeneration and regeneration of the sodium salt desulfurization product are realized. Recycling relieves environmental pollution pressure and improves economic benefits.

CN118754155APending Publication Date: 2024-10-11SHENYANG INSTITUTE OF CHEMICAL TECHNOLOGY
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202410976957.3
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-22
Publication Date
2024-10-11

AI Technical Summary

Technical Problem

The sodium salt flue gas desulfurization product Na2SO4 is difficult to process and forms industrial waste causing environmental pollution.

Method used

Sodium sulfate, activated calcium oxide, sodium metaaluminate and/or calcium aluminate cement are added to water according to a specific ratio, stirred and filtered to generate a sodium hydroxide solution, thereby realizing the regeneration and recycling of sodium salt desulfurization products.

Benefits of technology

It effectively solves the problem of safe handling of sodium salt desulfurization products, reduces environmental pollution, increases the economic income of enterprises, and realizes the high value-added utilization of sodium salt desulfurization products.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader

Abstract

The invention discloses a method for preparing alkali by using sodium sulfate, and relates to a desulfurization and denitrification alkali preparation method for treating a sodium-based desulfurization product. According to the method, sodium sulfate, active calcium oxide and sodium metaaluminate and / or calcium aluminate cement are dissolved in water to form an aqueous solution, NaOH is prepared through full reaction, and filter residues can be continuously desulfurized; according to the invention, the cyclic comprehensive utilization of the sodium salt desulfurization product is realized, the safe treatment problem of the sodium salt desulfurization product is effectively solved, and the environmental protection pressure is relieved. The method not only increases the economic income of enterprises, but also solves the problem of pollution caused by sodium salt desulfurization products, more importantly protects the environment, and brings better economic benefits to the enterprises.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to a method for preparing alkali, in particular to a method for preparing alkali by utilizing sodium sulfate. Background Art

[0002] Sodium salt flue gas desulfurization has high desulfurization efficiency and good desulfurization effect, so it is widely used in industrial flue gas desulfurization. However, the desulfurization product Na2SO4 generated is difficult to handle, forming industrial waste and causing environmental pollution. Summary of the invention

[0003] The object of the present invention is to provide a method for preparing alkali using sodium sulfate. The method comprises adding sodium sulfate, active calcium oxide, sodium metaaluminate and / or calcium aluminate cement to an appropriate amount of water according to an appropriate ratio, stirring for a period of time and filtering, and the filtrate is a sodium hydroxide solution. The problem of Na2SO4 forming industrial waste is solved, and it is prepared into high value-added NaOH. The present invention realizes the regeneration and cyclic comprehensive utilization of sodium salt desulfurization products, effectively solves the problem of safe treatment of sodium salt desulfurization products, and alleviates environmental pressure.

[0004] The objective of the present invention is achieved through the following technical solutions: A method for preparing alkali by using sodium sulfate. The method comprises the following steps: adding sodium sulfate, active calcium oxide, sodium aluminate and / or calcium aluminate cement into water according to a proportion, stirring and filtering, and the filtrate is a sodium hydroxide solution. The mass ratio of the sodium sulfate, active calcium oxide and sodium aluminate is 46:20-28:7-9. The calcium aluminate cement includes C3A, CA-50, CA-60, CA-70 and CA-80 cements. The mass ratio of the sodium sulfate:active calcium oxide:calcium aluminate cement is 46:20-28:4-16. The mass ratio of the sodium sulfate:active calcium oxide:calcium aluminate cement+sodium aluminate is 46:20-28:6-12.

[0005] The advantages and effects of the present invention are: The present invention realizes the regeneration and recycling comprehensive utilization of sodium salt desulfurization products, effectively solves the problem of safe treatment of sodium salt desulfurization products, and alleviates environmental pressure. It not only increases the economic income of the enterprise, but also solves the problem of pollution of sodium salt desulfurization products. More importantly, it protects the environment, brings better economic benefits to the enterprise, and fulfills the social responsibility of the enterprise. DETAILED DESCRIPTION

[0006] The present invention is described in detail below with reference to the embodiments.

[0007] Example 1 Sodium sulfate, active calcium oxide, sodium aluminate and / or calcium aluminate cement are added into a proper amount of water in a mass ratio of 46:20-28:7-9, stirred for 10-60 minutes and then filtered, and the filtrate is a sodium hydroxide solution.

[0008] Example 2 Sodium sulfate, activated calcium oxide and CA-50 calcium aluminate cement are added into a proper amount of water in a mass ratio of 46:20-28:8-16, stirred for 10-60 minutes and then filtered, and the filtrate is a sodium hydroxide solution.

[0009] Example 3 Sodium sulfate, activated calcium oxide and CA-60 calcium aluminate cement are added into a proper amount of water in a mass ratio of 46:20-28:8-16, stirred for 10-60 minutes and then filtered, and the filtrate is a sodium hydroxide solution.

[0010] Example 4 Sodium sulfate, activated calcium oxide and CA-70 calcium aluminate cement are added into a proper amount of water in a mass ratio of 46:20-28:6-12, stirred for 10-60 minutes and then filtered, and the filtrate is a sodium hydroxide solution.

[0011] Example 5 Sodium sulfate, activated calcium oxide and CA-80 calcium aluminate cement are added into a proper amount of water in a mass ratio of 46:20-28:4-10, stirred for 10-60 minutes and then filtered, and the filtrate is a sodium hydroxide solution.

[0012] Example 6 Sodium sulfate, active calcium oxide, sodium aluminate + CA-80 calcium aluminate cement are added into a proper amount of water in a mass ratio of 46:20-28:4-9, stirred for 10-60 minutes and then filtered, and the filtrate is a sodium hydroxide solution.

[0013] Example 7 Sodium sulfate, activated calcium oxide and C3A calcium aluminate cement are added into a proper amount of water in a mass ratio of 46:20-28:10-16, stirred for 10-60 minutes and then filtered, and the filtrate is a sodium hydroxide solution.

Claims

1. A method for preparing alkali using sodium sulfate, characterized in that: The method comprises adding sodium sulfate, active calcium oxide, sodium aluminate and / or calcium aluminate cement into water according to a proportion, stirring and filtering, and the filtrate is a sodium hydroxide solution; the mass ratio of the sodium sulfate, active calcium oxide and sodium aluminate is 46:20-28:7-9; the calcium aluminate cement includes C3A, CA-50, CA-60, CA-70 and CA-80 cement; The mass ratio of sodium sulfate: active calcium oxide: calcium aluminate cement is 46:20-28:4-16; the mass ratio of sodium sulfate: active calcium oxide: calcium aluminate cement + sodium metaaluminate is 46:20-28:6-12.