AP / layered hydroxide compound as well as preparation method and application thereof
By mixing AP and layered hydroxide precursor solution under the acoustic resonance platform, the AP/layered hydroxide composite is prepared, which solves the problems of uneven mixing and unsafe preparation in the existing technology, and improves the combustion performance. and security.
Patent Information
- Application Number
- CN202410818434.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-06-24
- Publication Date
- 2024-10-11
AI Technical Summary
The existing ammonium perchlorate (AP) catalyst in the solid propellant is mixed unevenly, the preparation process is unsafe, and the energy release is unstable, which affects the combustion performance.
An acoustic resonance platform is used to mix AP and layered hydroxide precursor solution. By adjusting the resonance frequency and acceleration, a uniform shear force field is formed to prepare the AP/layered hydroxide composite to improve energy release efficiency and safety. sex.
The uniform mixing of AP/layered hydroxide composite materials is achieved, the energy release efficiency and safety performance are improved, the shear force of the reaction materials is reduced, and the preparation safety is enhanced.
Smart Images

Figure CN118754791A_ABST
Abstract
Description
Technical Field
[0001] The embodiments of the present application relate to an energetic material and a preparation technology thereof, and in particular to an AP / layered hydroxide composite and a preparation method and use thereof. Background Art
[0002] Ammonium perchlorate (AP) is the most commonly used oxidant in composite solid propellants such as nitrate ester plasticized polyether (NEPE) propellants and modified double-base propellants. It is an important component of energetic materials such as pyrotechnics, accounting for more than 70% of the total. Ammonium perchlorate has good compatibility, low hygroscopicity, high gas generation and low cost, and plays a very important role in solid propellants. By adding some catalysts to change the decomposition characteristics, the combustion performance of the propellant can be significantly improved. The addition of catalysts mostly adopts the method of physical mixing, which has hidden dangers such as uneven mixing, unsafe preparation process, and unstable energy release. Summary of the invention
[0003] In view of this, the embodiments of the present application provide an AP / layered hydroxide composite and a preparation method and use thereof, so as to at least solve the above technical problems.
[0004] According to a first aspect of the present application, a method for preparing an AP / layered hydroxide composite is provided, comprising: Adding AP to ethyl acetate to obtain an AP solution with a first set concentration; Dissolving the soluble metal salt, the intercalated organic matter and sodium hydroxide in deionized water respectively to obtain a metal salt solution with a second set concentration, an intercalated organic matter solution with a third set concentration and a sodium hydroxide solution with a fourth set concentration; Adding an intercalation organic solution to a soluble metal salt solution, and then slowly adding a sodium hydroxide solution to prepare a mixed solution, and adjusting the pH value of the mixed solution to maintain at a first set value to obtain a layered hydroxide precursor solution; After the reaction container is mounted on the acoustic resonance platform, the resonance frequency and phase difference of the acoustic resonance reaction platform are adjusted to keep the acceleration of the acoustic resonance reaction platform within a first set range, the AP solution and the layered hydroxide precursor solution are added to the reaction container, the air in the reaction container is exhausted with nitrogen, and then the circulating nitrogen is slowly injected; The temperature of the reaction container is maintained at a first set temperature, the reaction is carried out for a first set time, and the ammonium bicarbonate solution is slowly added dropwise during the reaction; The reactants are filtered, washed and dried to obtain an AP / layered hydroxide composite material.
[0005] In some optional embodiments, the intercalated organic matter includes at least one of the following: The intercalated organic matter comprises at least one of the following: Sodium salicylate, potassium salicylate, sodium benzoate, potassium benzoate, pyridinium acetate, sodium acetylide, alkyl amino acids, glutamic acid, threonine, L-propyl glutathione and glutathione.
[0006] In some optional embodiments, the soluble metal salt includes at least one of the following: Copper acetate, copper nitrate, lead acetate, lead nitrate, cadmium acetate, cadmium nitrate, iron nitrate, nickel nitrate, cobalt nitrate, calcium nitrate, zinc nitrate.
[0007] In some optional embodiments, the pH value ranges from 3 to 12.
[0008] In some optional embodiments, the resonance frequency of the acoustic resonance reaction platform is adjusted to be maintained at 53 Hz to 69 Hz, and the phase difference is maintained at 0.01 to 0.4.
[0009] In some optional embodiments, the acceleration of the acoustic resonance reaction platform is maintained at 12g to 166g.
[0010] In some optional embodiments, the first set time is 4 minutes to 94 minutes, and the first set temperature is 2° C. to 100° C.
[0011] In some optional embodiments, the AP / layered hydroxide composite has a layered hydroxide content of 0.03 wt % to 49 wt %, and an AP content of 51 wt % to 99.97 wt %.
[0012] According to a second aspect of the present application, an AP / layered hydroxide composite is provided. The AP / layered hydroxide composite is prepared by the above-mentioned method for preparing the AP / layered hydroxide composite.
[0013] According to a third aspect of the present application, there is provided a use of an AP / layered hydroxide composite, wherein the AP / layered hydroxide composite is used as a propellant.
[0014] Compared with the traditional stirring paddle preparation method, the mixed preparation technology of the embodiment of the present application is more fully mixed with the stirring paddle synthesis method, and the organic-inorganic layered hydroxide has the characteristics of simple preparation, environmental protection, low cost, rich functions, and rich catalytic active sites. Monometallic / bimetallic hydroxides can be selected to be compounded with AP, which can effectively improve the energy release efficiency of AP / layered hydroxide. The AP / layered hydroxide composite material has lower sensitivity performance and faster energy release rate. The shear force on the reaction materials during mixing is reduced, the friction between the materials, stirring paddles, and reaction vessels is avoided, and the intrinsic safety of the reaction is improved. Compared with pure AP, the AP / layered copper hydroxide composite has a faster heat release rate (sharper heat release peak) and improves the energy release efficiency of AP, and the layered copper hydroxide makes the AP thermal decomposition 114.1°C earlier; compared with pure AP, the impact sensitivity of AP / layered copper hydroxide is reduced from 93.7cm to 112cm, which greatly improves its safety performance. BRIEF DESCRIPTION OF THE DRAWINGS
[0015] Figure 1 A schematic diagram of a process for preparing an AP / layered hydroxide composite provided in an embodiment of the present application; Figure 2 Schematic diagram showing the heat release rate comparison between the AP / layered copper hydroxide composite and pure AP according to an embodiment of the present application. DETAILED DESCRIPTION
[0016] The essence of the technical solution of the embodiment of the present application is explained in detail below.
[0017] Figure 1 A schematic diagram of the process for preparing the AP / layered hydroxide composite provided in the embodiments of the present application is shown in FIG. Figure 1 As shown, the preparation method of the AP / layered hydroxide composite provided in the embodiment of the present application comprises the following steps: Step 101: adding AP to ethyl acetate to obtain an AP solution with a first set concentration.
[0018] In the embodiment of the present application, the first set concentration may be 11wt% to 15.1wt%. As an example, the concentration of the ADN solution may be 11.3wt%, 11.5wt%, 11.8wt%, 12.0wt%, 12.5wt%, 13wt%, 13.1wt%, 13.2wt%, 13.5wt%, 13.8wt%, 14.1wt%, 14wt%, 14.5wt%, 14.8wt%, or 15wt%, etc.
[0019] Step 102, dissolving the soluble metal salt, the intercalated organic matter and sodium hydroxide in deionized water respectively to obtain a metal salt solution with a second set concentration, an intercalated organic matter solution with a third set concentration and a sodium hydroxide solution with a fourth set concentration.
[0020] In the embodiment of the present application, the intercalated organic matter includes at least one of the following: Sodium salicylate, potassium salicylate, sodium benzoate, potassium benzoate, pyridinium acetate, sodium acetylide, alkyl amino acids, glutamic acid, threonine, L-propyl glutathione and glutathione.
[0021] The soluble metal salt of the embodiment of the present application includes at least one of the following: copper acetate, copper nitrate, lead acetate, lead nitrate, cadmium acetate, cadmium nitrate, iron nitrate, nickel nitrate, cobalt nitrate, calcium nitrate, zinc nitrate. As a preferred embodiment, the soluble metal salt is copper nitrate.
[0022] In the embodiment of the present application, the second set concentration may be 3.3 wt % to 4.1 wt %. As an example, the concentration of the soluble metal salt solution may be 3.4 wt %, 3.5 wt %, 3.6 wt %, 3.7 wt %, 3.8 wt %, 3.9 wt %, or 4.0 wt %.
[0023] The third set concentration may be 2.0 wt% to 2.5 wt%. As an example, the concentration of the intercalated organic solution may be 2.1 wt%, 2.2 wt%, 2.3 wt%, or 2.4 wt%.
[0024] The fourth set concentration may be 1.7 wt % to 2.1 wt %. As an example, the concentration of the sodium hydroxide solution may be 1.8 wt %, 1.9 wt %, 2.0 wt %, or 2.08 wt %.
[0025] Step 103, adding the intercalation organic solution to the soluble metal salt solution, and then slowly adding the sodium hydroxide solution to prepare a mixed solution, adjusting the pH value of the mixed solution to maintain at a first set value, and obtaining a layered hydroxide precursor solution.
[0026] In the embodiment of the present application, the pH value ranges from 3 to 12. As an example, by adding sodium hydroxide solution to the mixed solution, the pH value of the mixed solution is adjusted to be maintained at 4, 5, 6, 7, 8, 9, 10, 11 or 11.5. As a preferred embodiment, the pH value of the mixed solution is adjusted to be maintained at 7.1 to 7.9.
[0027] Step 104, after the reaction container is installed on the acoustic resonance platform, the resonance frequency and phase difference of the acoustic resonance reaction platform are adjusted to keep the acceleration of the acoustic resonance reaction platform within a first set range, the AP solution and the layered hydroxide precursor solution are added to the reaction container, the air in the reaction container is exhausted with nitrogen, and then the circulating nitrogen is slowly injected.
[0028] In the embodiment of the present application, the phase difference of the acoustic resonance reaction platform is adjusted to maintain a value range of 0.01 to 0.4. As an implementation method, the phase difference of the first acoustic resonance reaction platform can be 0.02, 0.03, 0.05, 0.08, 0.10, 0.12, 0.15, 0.18, 0.20, 0.24, 0.27, 0.29, 0.31, 0.34, 0.36, 0.38, or 0.40, etc. As a preferred method, the phase difference of the acoustic resonance reaction platform is adjusted to maintain 0.14 to 0.25. The resonant frequency of the acoustic resonance reaction platform is adjusted to 53 Hz to 69 Hz. As an implementation method, the resonance frequency of the acoustic resonance reaction platform is set to 53.5Hz, 54.5Hz, 56.3Hz, 57.4Hz, 58.6Hz, 59.5Hz, 60.4Hz, 61.8Hz, 62Hz, 62.6Hz, 63.1Hz, 63.5Hz, 64.5Hz, 64.8Hz, 65.5Hz, 65.6Hz, 67.4Hz, 68.2Hz, or 68.8Hz, etc. As a preferred method, the resonance frequency of the acoustic resonance reaction platform is preferably 59Hz to 62Hz. The acceleration of the acoustic resonance reaction platform is maintained at 12g to 166g. Specifically, the acceleration of the acoustic resonance reaction platform can be 15g, 18g, 20g, 25g, 30g, 35g, 45g, 50g, 55g, 60g, 65g, 70g, 75g, 80g, 85g, 90g, 95g, 100g, 105g, 115g, 120g, 125g, 130g, 135g, 145g, 150g, 155g, or 158g, etc. As a preferred embodiment, the acceleration of the acoustic resonance reaction platform is set to 64g-80g.
[0029] Step 105, maintaining the temperature of the reaction container at a first set temperature, reacting for a first set time, and slowly adding ammonium bicarbonate solution while reacting.
[0030] In an embodiment of the present application, the first set time length can be 4min to 94min. Specifically, the first set time length can be 7min, 10min, 16min, 21min, 25min, 29min, 35min, 44min, 49min, 55min, 60min, 65min, 70min, 75min, 80min, 85min, 89min, or 93min.
[0031] The first set temperature can be 2°C to 100°C. As an example, the first set temperature can be 5°C, 10°C, 15°C, 20°C, 25°C, 30°C, 35°C, 38°C, 45°C, 50°C, 55°C, 58°C, 60°C, 65°C, 70°C, 75°C, 80°C, 85°C, 90°C, 95°C, 96°C, or 98°C, etc.
[0032] Step 106, filtering, washing, and drying the reactants to obtain an AP / layered hydroxide composite material.
[0033] In the embodiment of the present application, the washing times can be 6 times, such as washing the filtered material 3 times with deionized water and washing the filtered material 3 times with ethanol. The washing method can also be alternating between deionized water and ethanol.
[0034] The AP / layered hydroxide composite of the embodiment of the present application has a layered hydroxide content of 0.01 wt % to 55 wt %, and an ADN content of 45 wt % to 99.99 wt %.
[0035] The technical scheme of the embodiments of the present application is described below in conjunction with specific embodiments, but the conditions and results described in the implementation do not limit the scope of protection of the present application. The embodiments of the present application only illustrate the preparation of related solutions, etc. for example. For industrial use or other preparation amounts, the amount can be expanded in proportion accordingly. The preparation device used is also only an exemplary description. In industrial production, alternative container equipment can be used, or the corresponding container equipment can be enlarged in proportion.
[0036] The technical solution of this application is further illustrated by using specific examples below. Example
[0037] In this example, 3.78 g AP was weighed and dissolved in 28 mL ethyl acetate to obtain an AP solution; 0.179 g intercalation organic matter, 0.224 g sodium hydroxide, and 0.432 g copper nitrate were weighed and dissolved in 8 mL, 11 mL, and 11 mL distilled water, respectively, to obtain an intercalation organic matter solution, a sodium hydroxide solution, and a copper salt solution. The intercalation organic matter solution was added to the copper salt solution, and then the sodium hydroxide solution was slowly added to adjust the pH of the system to 8 to obtain a layered hydroxide precursor solution. After the reaction container is installed on the acoustic resonance platform, the reaction container is fixed, the resonance frequency is set to 63.8 Hz, the phase difference is set to 0.02, the acceleration G1 is 60 g, and the above-configured layered hydroxide precursor solution and AP dispersion are added to the reaction container respectively by a metering pump. After the air in the reaction container is exhausted by nitrogen, the circulating nitrogen is slowly injected to increase the temperature of the reaction system to 85°C, and the reaction is carried out at 85°C for 60 minutes. Ammonium bicarbonate solution (NH4HCO3, 0.4 mol / L) is slowly added during the reaction; after the reaction is completed, the reaction is filtered, and the obtained product is washed with deionized water and ethanol in turn, and placed in a vacuum drying oven for drying to obtain a dry AP / layered hydroxide composite material product.
[0038] According to conversion rate = mass of reacting substance / total mass of reactants × 100%, the conversion rate is calculated to be 89%. Example
[0039] In this example, 4.78 g AP was weighed and dissolved in 28 mL ethyl acetate to obtain an AP solution; 0.179 g intercalation organic matter, 0.224 g sodium hydroxide, and 0.432 g copper nitrate were weighed and dissolved in 8 mL, 11 mL, and 11 mL distilled water, respectively, to obtain an intercalation organic matter solution, a sodium hydroxide solution, and a copper salt solution. The intercalation organic matter solution was added to the copper salt solution, and then the sodium hydroxide solution was slowly added to adjust the pH of the system to 8 to obtain a layered hydroxide precursor solution. After the reaction container is installed on the acoustic resonance platform, the reaction container is fixed, the resonance frequency is set to 63.8 Hz, the phase difference is set to 0.02, the acceleration G1 is 60 g, and the above-configured layered hydroxide precursor solution and AP dispersion are added to the reaction container respectively by a metering pump. After the air in the reaction container is exhausted by nitrogen, the circulating nitrogen is slowly injected to increase the temperature of the reaction system to 85°C, and the reaction is carried out at 85°C for 60 minutes. Ammonium bicarbonate solution (NH4HCO3, 0.4 mol / L) is slowly added during the reaction; after the reaction is completed, the reaction is filtered, and the obtained product is washed with deionized water and ethanol in turn, and placed in a vacuum drying oven for drying to obtain a dry AP / layered hydroxide composite material product.
[0040] According to conversion rate = mass of reacting substance / total mass of reactants × 100%, the conversion rate is 91%. Example
[0041] In this example, 4.78 g AP was weighed and dissolved in 28 mL ethyl acetate to obtain an AP solution; 0.179 g intercalation organic matter, 0.224 g sodium hydroxide, and 0.432 g copper nitrate were weighed and dissolved in 8 mL, 11 mL, and 11 mL distilled water, respectively, to obtain an intercalation organic matter solution, a sodium hydroxide solution, and a copper salt solution. The intercalation organic matter solution was added to the copper salt solution, and then the sodium hydroxide solution was slowly added to adjust the pH of the system to 8 to obtain a layered hydroxide precursor solution. After the reaction container is installed on the acoustic resonance platform, the reaction container is fixed, the resonance frequency is set to 63.8 Hz, the phase difference is set to 0.02, the acceleration G1 is 60 g, and the above-configured layered hydroxide precursor solution and AP dispersion are added to the reaction container respectively by a metering pump. After the air in the reaction container is exhausted by nitrogen, the circulating nitrogen is slowly injected to increase the temperature of the reaction system to 85°C, and the reaction is carried out at 85°C for 30 minutes. Ammonium bicarbonate solution (NH4HCO3, 0.4 mol / L) is slowly added during the reaction; after the reaction is completed, the reaction is filtered, and the obtained product is washed with deionized water and ethanol in turn, and placed in a vacuum drying oven for drying to obtain a dry AP / layered hydroxide composite material product.
[0042] According to conversion rate = mass of reacting substance / total mass of reactants × 100%, the conversion rate is calculated to be 89%. Example
[0043] In this example, 4.78 g AP was weighed and dissolved in 28 mL ethyl acetate to obtain an AP solution; 0.179 g intercalation organic matter, 0.224 g sodium hydroxide, and 0.432 g copper nitrate were weighed and dissolved in 8 mL, 11 mL, and 11 mL distilled water, respectively, to obtain an intercalation organic matter solution, a sodium hydroxide solution, and a copper salt solution. The intercalation organic matter solution was added to the copper salt solution, and then the sodium hydroxide solution was slowly added to adjust the pH of the system to 8 to obtain a layered hydroxide precursor solution. After the reaction container is installed on the acoustic resonance platform, the reaction container is fixed, the resonance frequency is set to 63.8 Hz, the phase difference is set to 0.02, the acceleration G1 is 60 g, and the above-configured layered hydroxide precursor solution and AP dispersion are added to the reaction container respectively by a metering pump. After the air in the reaction container is exhausted by nitrogen, the circulating nitrogen is slowly injected to increase the temperature of the reaction system to 90°C, and the reaction is carried out at 90°C for 30 minutes. Ammonium bicarbonate solution (NH4HCO3, 0.4 mol / L) is slowly added during the reaction; after the reaction is completed, the reaction is filtered, and the obtained product is washed with deionized water and ethanol in turn, and placed in a vacuum drying oven for drying to obtain a dry AP / layered hydroxide composite material product.
[0044] According to conversion rate = mass of reacting substance / total mass of reactants × 100%, the conversion rate is 90%.
[0045] Figure 2 Schematic diagram of heat release rate comparison between the AP / layered copper hydroxide composite and pure AP in the embodiment of the present application. Figure 2 As shown, the AP / layered copper hydroxide composite has a faster heat release rate (sharper heat release peak) than pure AP, which improves the energy release efficiency of AP, and layered copper hydroxide makes the thermal decomposition of AP 114.1℃ earlier ( Figure 2 Compared with pure AP, the impact sensitivity of AP / layered copper hydroxide is reduced from 93.7cm to 112cm, which greatly improves its safety performance The substance concentrations and weights in the examples are only examples and should not be construed as limitations on the technical solutions of the present application.
[0046] The AP / layered hydroxide complex prepared by the technical solution of the embodiment of the present application uses low-frequency and high-intensity acoustic energy to induce resonance of the materials in the mixer, generate a uniform shear force field, fluidize the materials rapidly, and form a large number of micro-mixing zones, which can evenly mix the materials in a relatively short time, and is a new technology to replace the traditional stirring paddle mixing technology. The micro-mixing effect of the sound wave can be distributed throughout the entire mixing container, is dead-angle-free, all-round, and belongs to full-field mixing. Compared with the traditional preparation method of the stirring paddle, this mixing preparation technology has more complete mixing between the reaction materials, faster reaction speed, and better and more uniform quality of the reaction product. Layered hydroxide can be prepared by the method of acoustic resonance mixing and uniformly coated on the surface of AP. The coating of the layered hydroxide can improve the safety and energy release efficiency of AP.
[0047] The examples of the present application also describe an AP / layered hydroxide composite, which is prepared using the preparation method of the AP / layered hydroxide composite described in the above examples.
[0048] The examples of the present application also describe a use of an AP / layered hydroxide composite. The AP / layered hydroxide composite of the examples of the present application can be used as a propellant.
[0049] It should be understood that "one embodiment" or "an embodiment" mentioned throughout the specification means that specific features, structures or characteristics related to the embodiment are included in at least one embodiment of the present application. Therefore, "in one embodiment" or "in an embodiment" appearing throughout the specification does not necessarily refer to the same embodiment. In addition, these specific features, structures or characteristics can be combined in one or more embodiments in any suitable manner. It should be understood that in various embodiments of the present application, the size of the sequence number of the above-mentioned processes does not mean the order of execution. The execution order of each process should be determined by its function and internal logic, and should not constitute any limitation on the implementation process of the embodiment of the present application. The above-mentioned sequence numbers of the embodiments of the present application are for description only and do not represent the advantages and disadvantages of the embodiments.
[0050] It should be noted that, in this article, the terms "include", "comprises" or any other variations thereof are intended to cover non-exclusive inclusion, so that a process, method, article or device including a series of elements includes not only those elements, but also other elements not explicitly listed, or also includes elements inherent to such process, method, article or device. In the absence of further restrictions, an element defined by the sentence "comprises a ..." does not exclude the existence of other identical elements in the process, method, article or device including the element.
[0051] The above is only an implementation method of the present application, but the protection scope of the present application is not limited thereto. Any person skilled in the art who is familiar with the present technical field can easily think of changes or substitutions within the technical scope disclosed in the present application, which should be included in the protection scope of the present application. Therefore, the protection scope of the present application should be based on the protection scope of the claims.
Claims
1. A method for preparing an AP / layered hydroxide composite, characterized in that: The method comprises: Adding AP to ethyl acetate to obtain an AP solution with a first set concentration; Dissolving the soluble metal salt, the intercalated organic matter and sodium hydroxide in deionized water respectively to obtain a metal salt solution with a second set concentration, an intercalated organic matter solution with a third set concentration and a sodium hydroxide solution with a fourth set concentration; Adding an intercalation organic solution to a soluble metal salt solution, and then slowly adding a sodium hydroxide solution to prepare a mixed solution, and adjusting the pH value of the mixed solution to maintain at a first set value to obtain a layered hydroxide precursor solution; After the reaction container is mounted on the acoustic resonance platform, the resonance frequency and phase difference of the acoustic resonance reaction platform are adjusted to keep the acceleration of the acoustic resonance reaction platform within a first set range, the AP solution and the layered hydroxide precursor solution are added to the reaction container, the air in the reaction container is exhausted with nitrogen, and then the circulating nitrogen is slowly injected; The temperature of the reaction container is maintained at a first set temperature, the reaction is carried out for a first set time, and the ammonium bicarbonate solution is slowly added dropwise during the reaction; The reactants are filtered, washed and dried to obtain an AP / layered hydroxide composite material.
2. The preparation method according to claim 1, characterized in that: The intercalated organic matter comprises at least one of the following: Sodium salicylate, potassium salicylate, sodium benzoate, potassium benzoate, pyridinium acetate, sodium acetylide, alkyl amino acids, glutamic acid, threonine, L-propyl glutathione and glutathione.
3. The preparation method according to claim 1, characterized in that: The soluble metal salt comprises at least one of the following: Copper acetate, copper nitrate, lead acetate, lead nitrate, cadmium acetate, cadmium nitrate, iron nitrate, nickel nitrate, cobalt nitrate, calcium nitrate, zinc nitrate.
4. The preparation method according to claim 1, characterized in that: The pH value range is 3 to 12.
5. The preparation method according to claim 1, characterized in that: The resonance frequency of the acoustic resonance reaction platform is adjusted to be maintained at 53 Hz to 69 Hz, and the phase difference is maintained at 0.01 to 0.
4.
6. The preparation method according to claim 1, characterized in that: The acceleration of the acoustic resonance reaction platform is maintained at 12g to 166g.
7. The preparation method according to claim 1, characterized in that: The first set time is 4 minutes to 94 minutes, and the first set temperature is 2° C. to 100° C.
8. The preparation method according to claim 1, characterized in that: The AP / layered hydroxide composite has a layered hydroxide content of 0.03 wt % to 49 wt %, and an AP content of 51 wt % to 99.97 wt %.
9. An AP / layered hydroxide composite, characterized in that The AP / layered hydroxide composite is prepared by the preparation method of the AP / layered hydroxide composite according to any one of claims 1 to 8.
10. Use of the AP / layered hydroxide composite according to claim 9, characterized in that: The AP / layered hydroxide composite is used as a propellant.
Citation Information
Cited By
Method for synergistically improving energy release and safety performance of energetic material at low cost
CN122749240A