Support-free additive manufacturing method
Through the support-free additive manufacturing method, the database and finite element simulation are used to optimize the processing plan, and the topological method and porous design are combined to dynamically adjust the processing parameters, solving the problems of support structure and residual stress in additive manufacturing, and achieving high-precision and high-performance products. Create effects.
Patent Information
- Application Number
- CN202410699387.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-05-31
- Publication Date
- 2024-10-11
AI Technical Summary
Existing additive manufacturing technology requires the addition of additional support structures when manufacturing suspended structures, resulting in material waste, complex processes, and reduced part quality. The laser melting process also produces large residual stress, which affects the dimensional accuracy and mechanical properties of the parts.
Using support-free additive manufacturing methods, by combining database, simulation prediction, real-time monitoring and feedback optimization, finite element simulation experiments and topology methods or porous design are used to optimize the processing plan, dynamically adjust processing parameters to control residual stress, and reduce it through annealing treatment stress to ensure part quality.
Effectively control residual stress during the additive manufacturing process, improve the dimensional accuracy and mechanical properties of parts, and achieve support-free, high-precision, and high-performance additive manufacturing.
Smart Images

Figure CN118761252A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the technical field of additive manufacturing, and in particular to a support-free additive manufacturing method. Background Art
[0002] Laser powder bed fusion (LPBF), as an additive manufacturing technology, has shown broad application prospects in aerospace, automotive, medical, and electronics industries. However, when manufacturing parts with overhanging sections, this technology requires the addition of additional support structures, which leads to material waste, complex processes, and reduced part quality.
[0003] Currently, multi-laser additive and subtractive manufacturing methods, which combine ultrafast lasers and continuous lasers for additive and subtractive composite manufacturing, can improve part manufacturing accuracy and surface quality to a certain extent. However, existing technologies still have the following shortcomings:
[0004] 1. Support structure problem. Traditional additive manufacturing technology still needs to add support structures when manufacturing suspended structures, which cannot completely solve the problems caused by the support structures.
[0005] 2. Residual stress problem: The laser melting process will produce large residual stress, which will affect the dimensional accuracy and mechanical properties of the parts.
[0006] Chinese patent document CN115488349A discloses a powder bed subtractive manufacturing device for in-situ tomographic reconstruction and imaging detection and its use method. The method uses X-rays to in-situ scan the current layer being printed. The X-ray signal receives the irradiation signal to reconstruct the tomographic scan, which can monitor the interior of the subtractive manufacturing sample in situ during the printing process.
[0007] Chinese patent document CN115488349A discloses a support-free laser selective melting additive manufacturing method. This method pre-lays powder in the overhang area. When processing the overhang structure, the laser is used to melt or sinter the powder surface. Without disturbing the original position of the powder, connections are established between the powder particles to form a relatively loose overhang layer. The overhang layer is then remelted to improve the connection quality and density, forming a continuous single-layer part cross-section slice.
[0008] Although the solution in the above document solves the support structure problem, it fails to solve the residual stress problem in additive manufacturing.
[0009] Therefore, a new support-free additive manufacturing method needs to be developed to overcome the shortcomings of existing technologies. Summary of the Invention
[0010] In order to overcome the problems existing in the related art, the purpose of the present invention is to provide a support-free additive manufacturing method, which overcomes the problems existing in the prior art by combining database, simulation prediction, real-time monitoring and feedback optimization.
[0011] A support-free additive manufacturing method, comprising:
[0012] S1: Obtain a database of different processing parameters and their corresponding forming conditions, corresponding residual stress conditions, and workpiece parameters;
[0013] S2: determining an initial processing plan for the support layer according to the parameters of the workpiece and the database, and performing a finite element simulation experiment on the initial processing plan;
[0014] S3: Optimizing the initial processing plan through topological optimization or multi-hole design method according to the experimental results to generate an actual processing plan;
[0015] S4: performing additive processing on the workpiece according to the actual processing plan, while monitoring the residual stress of the workpiece, and performing annealing treatment if the residual stress is too large;
[0016] S5: generating an initial processing plan for subsequent layers according to the residual stress of the workpiece, and performing a simulation experiment on the processing plan for the subsequent layers;
[0017] Repeat steps S3 to S5.
[0018] By establishing a database of different processing parameters, forming conditions, and residual stress data, and optimizing the processing plan through finite element simulation, we can effectively control the residual stress during the additive manufacturing process. Furthermore, by monitoring the residual stress in real time and performing annealing treatments, we can further reduce the residual stress and improve part quality. Based on the residual stress of the workpiece, we can dynamically adjust the processing plan for subsequent layers to ensure the stability and controllability of the entire additive manufacturing process.
[0019] The topology optimization method and the porous design method optimization are optimized by combining the actual stress situation of the previous layer and the stress simulation of the current layer, and the support structure is redesigned and optimized to better disperse and reduce stress concentration.
[0020] Preferably, the processing scheme includes heat treatment type, laser type, laser power, scanning speed, defocus amount, laser pulse, single pulse energy, repetition frequency, spot overlap rate, number of scans and spot diameter.
[0021] Combining workpiece parameters and databases, the initial processing plan can determine a more reasonable heat treatment type, laser parameter combination, and scanning strategy, which can be verified and optimized through finite element simulation to more effectively predict and reduce residual stress caused by support structures.
[0022] Preferably, the topology optimization method specifically includes:
[0023] Perform single-layer modeling;
[0024] performing stress-deformation simulation on the single-layer modeling model according to the residual stress;
[0025] The optimization criterion method is used for optimization according to the stress-deformation simulation.
[0026] By modeling a single layer, we focus on its deformation under residual stress. Based on the stress-deformation simulation results, we use an optimization algorithm to automatically find the optimal support structure topology, thereby minimizing residual stress and deformation.
[0027] Preferably, the optimization of the porous design method specifically includes:
[0028] Use design software to perform single-layer modeling;
[0029] Performing stress simulation analysis on the single-layer model to obtain the optimal pore size, pore shape and pore distribution;
[0030] The pore size range is 100 μm-10 mm.
[0031] By simulating models with different hole diameters, hole shapes, and hole distributions through methods such as finite element analysis, it is possible to predict the impact of different design schemes on residual stress, thereby finding the optimal hole design scheme to minimize residual stress while ensuring the strength and stability of the support structure.
[0032] Preferably, the annealing treatment specifically includes:
[0033] A large spot diameter heat treatment laser is used for treatment, wherein the heat treatment laser power is 200W-8000W and the spot diameter is 1mm-10mm.
[0034] The large spot can cover a larger area at one time, improving annealing efficiency while ensuring more uniform heat distribution, reducing local stress concentration, and lowering the risk of deformation.
[0035] Preferably, the heat treatment types include melting molding and sintering molding, and the optimized thin layer includes an optimized part and a complementary part.
[0036] Preferably, the laser types include continuous laser, thermal treatment laser, nanosecond laser and ultrafast laser;
[0037] The power of the continuous laser is 10W-200W, the scanning speed is 20mm / s-7000mm / s, the defocus is 0.1mm-30mm, the pulse width of the pulse laser is 1ns-10ps, the single pulse energy is 1μJ-10mJ, the repetition frequency is 100KHz-5000KHz, the spot overlap rate is 10%-99%, the number of scans is 1-20 times, and the spot diameter is 30μm;
[0038] The power of the heat treatment laser is 10W-8000W, the spot diameter is 1mm-10mm, and the scanning speed is 10mm / s-7000mm / s.
[0039] By providing a variety of laser types and detailed parameter ranges, the processing strategy can be flexibly adjusted according to different application requirements and material properties, achieving fine control over the additive manufacturing process and ultimately obtaining high-quality support-free structures.
[0040] Preferably, when the single layer is modeled, the missing parts are completed.
[0041] In the actual processing process, the laser scanning path does not completely cover the entire area, and there are some unprocessed vacancies. When modeling, these vacancies need to be reasonably filled to ensure the integrity and accuracy of the model.
[0042] Preferably, the database contains information on forming conditions, residual stress, molten pool depth and width, and powder sticking corresponding to different materials, different laser parameters, different layer thicknesses, and different numbers of layers, and the data in the database are obtained through full-factor or orthogonal experiments.
[0043] Full-factorial experiments test all factor and level combinations to obtain the most comprehensive data, but the experimental cost is high. Orthogonal experiments obtain representative data with fewer experiments, balancing experimental cost and data comprehensiveness.
[0044] The beneficial effects of the present invention are:
[0045] The present invention provides a method for unsupported additive manufacturing, which establishes a database of different processing parameters, molding conditions and residual stress data, and uses finite element simulation experiments to optimize the processing scheme using a topological method or a porous design method. The topological method optimization and the porous design method optimization are optimized in combination with the actual stress conditions of the previous layer and the stress simulation conditions of the current layer, and the support structure is redesigned and optimized to better disperse and reduce stress concentration. It can effectively control the residual stress in the additive manufacturing process and avoid the degradation of the dimensional accuracy and mechanical properties of the parts due to excessive residual stress. At the same time, by real-time monitoring of the residual stress and performing annealing treatment, the residual stress can be further reduced and the quality of the parts can be improved. In addition, according to the residual stress conditions of the workpiece, the processing plan of the subsequent layer is dynamically adjusted to ensure the stability and controllability of the entire additive manufacturing process, and ultimately achieve unsupported, high-precision, and high-performance additive manufacturing. BRIEF DESCRIPTION OF THE DRAWINGS
[0046] Figure 1 is a flow chart of a support-free additive manufacturing method provided in an embodiment of the present application;
[0047] Figure 2 is a schematic diagram of an unoptimized layer provided in an embodiment of the present application;
[0048] Figure 3 is a schematic diagram of a porous optimization layer provided in an embodiment of the present application;
[0049] Figure 4 This is a flow chart of a topology optimization layer provided in an embodiment of the present application;
[0050] Figure 5 is a schematic diagram of a manufacturing process provided in an embodiment of the present application;
[0051] Figure 6 is a schematic diagram of another manufacturing process provided in an embodiment of the present application;
[0052] Figure 7 This is an experimental diagram of a topology-optimized unsupported additive manufacturing method provided in an embodiment of the present application;
[0053] Figure 8 This is an experimental diagram of a non-optimized unsupported additive manufacturing method provided in an embodiment of the present application; DETAILED DESCRIPTION
[0054] The preferred embodiments of the present invention will be described in more detail below with reference to the accompanying drawings. Although preferred embodiments of the present invention are shown in the accompanying drawings, it should be understood that the present invention can be implemented in various forms and should not be limited by the embodiments described herein. Rather, these embodiments are provided to make the present invention more thorough and complete and to fully convey the scope of the present invention to those skilled in the art.
[0055] Example 1
[0056] like Figures 1-8 As shown, this embodiment provides a method for unsupported additive manufacturing, which includes
[0057] Step S1: obtaining a database of different processing parameters and their corresponding forming conditions, corresponding residual stress conditions, and workpiece parameters;
[0058] Step S2: determining an initial processing plan for the support layer according to the parameters of the workpiece and the database, and performing a finite element simulation experiment on the initial processing plan;
[0059] Step S3: Optimizing the initial processing plan through topological optimization or multi-hole design method according to the experimental results to generate an actual processing plan;
[0060] Step S4: performing additive processing on the workpiece according to the actual processing plan, while monitoring the residual stress of the workpiece. If the residual stress is too large, annealing treatment is performed;
[0061] Step S5: generating an initial processing plan for subsequent layers according to the residual stress of the workpiece, and performing a simulation experiment on the processing plan for the subsequent layers;
[0062] Repeat steps S3 to S5.
[0063] The topology optimization method and the porous design method optimization are optimized by combining the actual stress situation of the previous layer and the stress simulation of the current layer, and the support structure is redesigned and optimized to better disperse and reduce stress concentration.
[0064] Specifically, the processing plan includes heat treatment type, laser type, laser power, scanning speed, defocus amount, laser pulse, single pulse energy, repetition frequency, spot overlap rate, number of scans and spot diameter.
[0065] More specifically, the laser parameters of pulsed laser are mainly: single pulse energy, repetition frequency, spot overlap rate, scanning speed, laser power, spot diameter, and defocus.
[0066] More specifically, the laser parameters of continuous laser are mainly: laser power, scanning speed, defocus, spot diameter, etc.
[0067] More specifically, the laser parameters of the heat treatment laser are mainly: laser power, scanning speed, defocus, spot diameter, etc. Compared with continuous laser, the power of the heat treatment laser can be very high.
[0068] The scanning strategy refers to the planning of the scanning path, including the scanning angle, scanning path shape (straight line scanning, S-shaped scanning, U-shaped scanning, etc.) and laser types and parameters in different areas.
[0069] Combining workpiece parameters and databases, the initial processing plan can determine a more reasonable heat treatment type, laser parameter combination, and scanning strategy, which can be verified and optimized through finite element simulation to more effectively predict and reduce residual stress caused by support structures.
[0070] Specifically, the topology optimization method includes:
[0071] Perform single-layer modeling;
[0072] performing stress-deformation simulation on the single-layer modeling model according to the residual stress;
[0073] The optimization criterion method is used for optimization according to the stress-deformation simulation.
[0074] By modeling a single layer, we focus on its deformation under residual stress. Based on the stress-deformation simulation results, we use an optimization algorithm to automatically find the optimal support structure topology, thereby minimizing residual stress and deformation.
[0075] Specifically, the optimization of the porous design method includes:
[0076] Use design software to perform single-layer modeling;
[0077] Performing stress simulation analysis on the single-layer model to obtain the optimal pore size, pore shape and pore distribution;
[0078] The pore size range is 100 μm-10 mm.
[0079] By simulating models with different hole diameters, hole shapes, and hole distributions through methods such as finite element analysis, it is possible to predict the impact of different design schemes on residual stress, thereby finding the optimal hole design scheme to minimize residual stress while ensuring the strength and stability of the support structure.
[0080] Specifically, the annealing treatment includes:
[0081] A large spot diameter heat treatment laser is used for treatment, wherein the heat treatment laser power is 200W-8000W and the spot diameter is 1mm-10mm.
[0082] The large spot can cover a larger area at one time, improving annealing efficiency while ensuring more uniform heat distribution, reducing local stress concentration, and lowering the risk of deformation.
[0083] Specifically, the heat treatment types include melting molding and sintering molding, and the optimized thin layer includes an optimized part and a supplemented part.
[0084] Specifically, the laser types include continuous laser, thermal treatment laser, nanosecond laser and ultrafast laser;
[0085] The power of the continuous laser is 10W-200W, the scanning speed is 20mm / s-7000mm / s, the defocus is 0.1mm-30mm, the pulse width of the pulse laser is 1ns-10ps, the single pulse energy is 1μJ-10mJ, the repetition frequency is 100KHz-5000KHz, the spot overlap rate is 10%-99%, the number of scans is 1-20 times, and the spot diameter is 30μm;
[0086] The power of the heat treatment laser is 10W-8000W, the spot diameter is 1mm-10mm, and the scanning speed is 10mm / s-7000mm / s.
[0087] By providing a variety of laser types and detailed parameter ranges, the processing strategy can be flexibly adjusted according to different application requirements and material properties, achieving fine control over the additive manufacturing process and ultimately obtaining high-quality support-free structures.
[0088] Specifically, when the single layer modeling is performed, the missing parts are completed.
[0089] In the actual processing process, the laser scanning path does not completely cover the entire area, and there are some unprocessed vacancies. When modeling, these vacancies need to be reasonably filled to ensure the integrity and accuracy of the model.
[0090] Specifically, the database contains information on forming conditions, residual stress, molten pool depth and width, and powder sticking corresponding to different materials, different laser parameters, different layer thicknesses, and different numbers of layers. The data in the database are obtained through full-factor or orthogonal experiments.
[0091] Full-factorial experiments test all factor and level combinations to obtain the most comprehensive data, but the experimental cost is high. Orthogonal experiments obtain representative data with fewer experiments, balancing experimental cost and data comprehensiveness.
[0092] Example 2
[0093] like Figures 1-8 As shown, this embodiment provides a method for unsupported additive manufacturing, which includes
[0094] Step S1: obtaining a database of different processing parameters and their corresponding forming conditions, corresponding residual stress conditions, and workpiece parameters;
[0095] Step S2: determining an initial processing plan for the support layer according to the parameters of the workpiece and the database, and performing a finite element simulation experiment on the initial processing plan;
[0096] Step S3: Optimizing the initial processing plan through topological optimization or multi-hole design method according to the experimental results to generate an actual processing plan;
[0097] Step S4: performing additive processing on the workpiece according to the actual processing plan, while monitoring the residual stress of the workpiece. If the residual stress is too large, annealing treatment is performed;
[0098] Step S5: generating an initial processing plan for subsequent layers according to the residual stress of the workpiece, and performing a simulation experiment on the processing plan for the subsequent layers;
[0099] Repeat steps S3 to S5.
[0100] In this embodiment, if Figure 5 As shown, the first layer is sintered using a continuous laser beam, with selected continuous laser sintering parameters to form a powder sintered layer. The second layer is optimized using a porous design method to form a porous optimized layer. This porous optimized layer is then melted using a continuous laser beam, with corresponding melting parameters selected to melt the second layer while simultaneously connecting it to the first sintered layer.
[0101] In the missing parts of the porous optimization layer, modeling is performed to fill them, and the filled parts are formed using the sintering parameters of the first layer so as not to affect the bending resistance of the porous structure and the formation of the third layer.
[0102] In the formation of the third layer, the same porous optimized structure as the second layer is used. In the optimized part corresponding to the second layer, since the second layer is already connected to the first layer, the third layer in this area can be formed with less energy, and the corresponding low energy parameters of the third layer are used.
[0103] In the second layer of the completed part, since the first and second layers are both sintered, a higher energy is used for forming, and the third layer is formed with a higher energy parameter in order to connect the three-layer structure.
[0104] After forming three layers, subsequent layers are optimized. If online monitoring and simulation indicate excessive residual stress in subsequent layers, a heat treatment laser is used for annealing. After annealing, optimization continues until the part is complete.
[0105] Specifically, when the first layer is sintered, continuous laser or pulsed laser can be used for sintering, and low energy density can be used for sintering. The continuous laser can use a power of 10W-80W and a scanning speed of 100mm / s-800mm / s.
[0106] If it is a pulse laser, a single pulse energy of 1μJ-50μJ, a repetition frequency of 100KHz-1000KHz, a spot overlap rate of 10%-70% and heat treatment laser sintering can also be used.
[0107] The second layer is formed by continuous laser melting with medium energy density, laser power of 50W-150W, and scanning speed of 20mm / s-500mm / s. While the second layer is melting, the first and second layers can also be fused.
[0108] The third layer is formed by continuous laser high-energy melting, with a laser power of 60W-200W and a scanning speed of 20mm / s-300mm / s, which can fully fuse the three layers.
[0109] During the melting and forming of the second and third layers, pulsed laser can also be used to shape the powder layer. The single pulse energy is 30μJ-10mJ, the repetition frequency is 1000KHz-5000KHz, and the spot overlap rate is 50%-90%.
[0110] More specifically, XRD or warpage method can be used to measure the residual stress of the sample, and the depth and width of the molten pool and the powder sticking situation can be measured to obtain data including sintering parameters, melting parameters, sintering-melting ratio and thickness.
[0111] Example 3
[0112] As shown in the figure, this embodiment provides a method for unsupported additive manufacturing, which includes:
[0113] Step S1: obtaining a database of different processing parameters and their corresponding forming conditions, corresponding residual stress conditions, and workpiece parameters;
[0114] Step S2: determining an initial processing plan for the support layer according to the parameters of the workpiece and the database, and performing a finite element simulation experiment on the initial processing plan;
[0115] Step S3: Optimizing the initial processing plan through topological optimization or multi-hole design method according to the experimental results to generate an actual processing plan;
[0116] Step S4: performing additive processing on the workpiece according to the actual processing plan, while monitoring the residual stress of the workpiece. If the residual stress is too large, annealing treatment is performed;
[0117] Step S5: generating an initial processing plan for subsequent layers according to the residual stress of the workpiece, and performing a simulation experiment on the processing plan for the subsequent layers;
[0118] Repeat steps S3 to S5.
[0119] like Figure 6As shown, the first layer is sintered by using a pulsed laser, and the pulsed laser sintering parameters are selected to form a powder sintered layer.
[0120] The second layer is optimized into a topology optimized layer by a topology method, and the topology optimized layer is formed by continuous laser melting. Using continuous laser melting parameters, the second layer is melted and connected to the first sintered layer at the same time.
[0121] In the missing parts of the topology optimization layer, the modeling is completed and the first layer sintering parameters are used for forming so as not to affect the bending resistance of the topology optimization structure and the forming of the third layer.
[0122] In the forming of the third layer, the same topological optimization structure as the second layer is used. In the optimized part corresponding to the second layer, since the second layer is already connected to the first layer, the third layer in this area can be formed with a smaller energy. In the complementary part corresponding to the second layer, since both the first and second layers are sintered, a higher energy is used to form the three-layer structure in order to connect them.
[0123] After forming three layers, subsequent layers are optimized. If online monitoring and simulation indicate excessive residual stress in subsequent layers, a heat treatment laser is used for annealing. After annealing, optimization continues until the part is complete.
[0124] In this embodiment, the laser types include continuous laser, thermal treatment laser, nanosecond laser and ultrafast laser;
[0125] The power of the continuous laser is 10W-200W, the scanning speed is 20mm / s-7000mm / s, the defocus is 0.1mm-30mm, the pulse width of the pulse laser is 1ns-10ps, the single pulse energy is 1μJ-10mJ, the repetition frequency is 100KHz-5000KHz, the spot overlap rate is 10%-99%, the number of scans is 1-20 times, and the spot diameter is 30μm;
[0126] The power of the heat treatment laser is 10W-8000W, the spot diameter is 1mm-10mm, and the scanning speed is 10mm / s-7000mm / s.
[0127] Example 4
[0128] As shown in the figure, this embodiment provides a method for unsupported additive manufacturing, which includes:
[0129] Step S1: obtaining a database of different processing parameters and their corresponding forming conditions, corresponding residual stress conditions, and workpiece parameters;
[0130] Step S2: determining an initial processing plan for the support layer according to the parameters of the workpiece and the database, and performing a finite element simulation experiment on the initial processing plan;
[0131] Step S3: Optimizing the initial processing plan through topological optimization or multi-hole design method according to the experimental results to generate an actual processing plan;
[0132] Step S4: performing additive processing on the workpiece according to the actual processing plan, while monitoring the residual stress of the workpiece. If the residual stress is too large, annealing treatment is performed;
[0133] Step S5: generating an initial processing plan for subsequent layers according to the residual stress of the workpiece, and performing a simulation experiment on the processing plan for the subsequent layers;
[0134] Repeat steps S3 to S5.
[0135] The processing scheme includes heat treatment type, laser type, laser power, scanning speed, defocusing amount, laser pulse, single pulse energy, repetition frequency, spot overlap rate, number of scans and spot diameter.
[0136] The heat treatment types include melting molding and sintering molding, and the optimized thin layer includes an optimized part and a supplemented part.
[0137] The parameters are adjusted in different zones and layers by sintering first and then melting and forming, and the melt layer is stabilized by heat treatment.
[0138] During the sintering and melting process, according to the stress and deformation characteristics of unsupported forming, the structure is porous designed or topologically optimized, the forming shape of each layer is optimized, the order of regional scanning is adjusted, and the interlayer distribution is optimized, so as to achieve the purpose of reducing residual stress, reducing support structure, and improving forming quality and efficiency.
[0139] The first layer is sintered by using a pulsed laser, and pulsed laser sintering parameters are selected to form a powder sintered layer.
[0140] The second layer is optimized into a topology optimized layer by a topology method, and the topology optimized layer is formed by continuous laser melting. Using continuous laser melting parameters, the second layer is melted and connected to the first sintered layer at the same time.
[0141] In the missing parts of the topology optimization layer, the modeling is completed and the first layer sintering parameters are used for forming so as not to affect the bending resistance of the topology optimization structure and the forming of the third layer.
[0142] In the forming of the third layer, the same topological optimization structure as the second layer is used. In the optimized part corresponding to the second layer, since the second layer is already connected to the first layer, the third layer in this area can be formed with a smaller energy. In the complementary part corresponding to the second layer, since both the first and second layers are sintered, a higher energy is used to form the three-layer structure in order to connect them.
[0143] After forming three layers, subsequent layers are optimized. If online monitoring and simulation indicate excessive residual stress in subsequent layers, a heat treatment laser is used for annealing. After annealing, optimization continues until the part is complete.
[0144] In this embodiment, the melting forming is performed by collaborative forming using pulsed laser and heat treatment flat-top light mode. After forming using pulsed laser, the heat treatment laser large-spot flat-top light mode is used for stable forming. The parameters use pulsed laser forming parameters, and the heat treatment laser spot diameter is controlled at 3 mm.
[0145] Unless otherwise specifically stated, the relative arrangement, numerical expression and numerical value of the parts and steps set forth in these embodiments do not limit the scope of the application. In all examples shown and discussed here, any specific value should be interpreted as merely exemplary, rather than as a restriction. Therefore, other examples of exemplary embodiments can have different values. It should be noted that: similar reference numerals and letters represent similar items in the accompanying drawings below, and therefore, once a certain item is defined in an accompanying drawing, it does not need to be further discussed in the accompanying drawings subsequently.
[0146] In addition, it should be noted that the use of terms such as "first" and "second" for limitation is only for the convenience of distinction. Unless otherwise stated, the above terms have no special meaning and therefore cannot be understood as limiting the scope of protection of this application.
[0147] The foregoing description is merely a preferred embodiment of the present invention and is not intended to limit the present invention. Those skilled in the art will readily appreciate that various modifications and variations of the present invention are possible. Any modifications, equivalent substitutions, or improvements made within the spirit and principles of the present invention are intended to be within the scope of protection of the present invention.
Claims
1. A method for unsupported additive manufacturing, It is characterized in that include: S1: Obtain a database of different processing parameters and their corresponding forming conditions, corresponding residual stress conditions, and workpiece parameters; S2: determining an initial processing scheme for the support layer according to the parameters of the workpiece and the database, and performing a finite element simulation experiment on the initial processing scheme; S3: Optimizing the initial processing plan by topological optimization or multi-hole design method according to the experimental results to generate an actual processing plan; S4: performing additive processing on the workpiece according to the actual processing plan, while monitoring the residual stress of the workpiece, and performing annealing treatment if the residual stress is too large; S5: generating an initial processing plan for a subsequent layer according to the residual stress of the workpiece, and performing a simulation experiment on the processing plan for the subsequent layer; Repeat steps S3 to S5.
2. The method for unsupported additive manufacturing according to claim 1, It is characterized in that The processing scheme includes heat treatment type, laser type, laser power, scanning speed, defocusing amount, laser pulse, single pulse energy, repetition frequency, spot overlap rate, scanning times and spot diameter.
3. The method for unsupported additive manufacturing according to claim 1, It is characterized in that The topology method optimization specifically includes: Perform single-layer modeling; performing stress-deformation simulation on the single-layer modeling model according to the residual stress; The optimization is performed using the optimization criterion method according to the stress-deformation simulation.
4. The method for unsupported additive manufacturing according to claim 1, It is characterized in that The optimization of the porous design method specifically includes: Single-layer modeling is performed through design software; Performing stress simulation analysis on the single-layer modeling model to obtain the optimal pore size, pore shape and pore distribution; The pore size range is 100 μm-10 mm.
5. The method for unsupported additive manufacturing according to claim 1, It is characterized in that The annealing treatment specifically includes: A large spot diameter heat treatment laser is used for treatment, wherein the heat treatment laser power is 200W-8000W and the spot diameter is 1mm-10mm.
6. The method for unsupported additive manufacturing according to claim 2, It is characterized in that The heat treatment types include melting molding and sintering molding, and the optimized thin layer includes an optimized part and a complementary part.
7. The unsupported additive manufacturing method according to claim 2, It is characterized in that The laser types include continuous laser, thermal treatment laser, nanosecond laser and ultrafast laser; The power of the continuous laser is 10W-200W, the scanning speed is 20mm / s-7000mm / s, the defocus is 0.1mm-30mm, the pulse width of the pulse laser is 1ns-10ps, the single pulse energy is 1μJ-10mJ, the repetition frequency is 100KHz-5000KHz, the spot overlap rate is 10%-99%, the number of scans is 1-20 times, and the spot diameter is 30μm; The power of the heat treatment laser is 10W-8000W, the spot diameter is 1mm-10mm, and the scanning speed is 10mm / s-7000mm / s.
8. The unsupported additive manufacturing method according to claim 3 or 4, It is characterized in that When the single layer is modeled, the missing parts are completed.
9. The method for unsupported additive manufacturing according to claim 1, It is characterized in that The database contains information on forming conditions, residual stress, molten pool depth and width, and powder sticking conditions corresponding to different materials, different laser parameters, different layer thicknesses, and different numbers of layers. The data in the database are obtained through full factor or orthogonal experiments.
Citation Information
Cited By
Horizontal support-free forming method for laser powder bed melting
CN119609153A