Fundamental frequency gain and nonlinear frequency conversion integrated single crystal optical fiber and preparation method and application thereof

By adopting coupling-free design and femtosecond laser processing technology of single-crystal fiber integrating fundamental frequency gain and nonlinear frequency conversion in the laser, the problems of coupling loss and spatial walk-off effect in the laser are solved, and efficient energy conversion and beam processing are achieved. Improved quality, suitable for portable and space-constrained scenarios.

CN118763489AActive Publication Date: 2024-10-11SHANDONG UNIV
View PDF 6 Cites 0 Cited by

Patent Information

Application Number
CN202411032159.1
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-30
Publication Date
2024-10-11
Estimated Expiration
2044-07-30

AI Technical Summary

Technical Problem

Coupling losses and spatial walk-off effects exist in the fundamental frequency gain and nonlinear frequency conversion process in existing lasers, making it difficult to improve energy utilization and beam quality. Moreover, traditional bulk crystals have limited utilization in portable or space-constrained scenarios.

Method used

The fundamental frequency gain and nonlinear frequency conversion integrated single crystal fiber is used. The fundamental frequency gain single crystal fiber and the nonlinear single crystal fiber are connected in cascade to form a coupling-free integrated structure. The optical waveguide characteristics of the single crystal fiber are used to optimize energy conversion. efficiency, and a low refractive index microstructure cladding is formed through femtosecond laser processing to compensate for the spatial walk-off effect.

Benefits of technology

It significantly improves energy conversion efficiency and beam quality, reduces material waste and cost, enhances system integration and miniaturization capabilities, and solves the limitations of traditional lasers in conversion efficiency and volume.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118763489A_ABST
    Figure CN118763489A_ABST
Patent Text Reader

Abstract

The invention discloses a fundamental frequency gain and nonlinear frequency conversion integrated single crystal optical fiber and a preparation method and application thereof, and belongs to the technical field of laser. The single-crystal optical fiber comprises a fundamental frequency gain single-crystal optical fiber and one or more nonlinear single-crystal optical fibers, a coupling-free integrated structure is prepared in the mode that bulk crystal bonding is conducted firstly and then integrated drawing is conducted, and the single-crystal optical fiber can be applied to miniature visible light, ultraviolet or intermediate infrared lasers. The influence of the space walk-off effect in the nonlinear process of the bulk crystal can be remarkably reduced, the energy conversion efficiency is improved, the advantages of miniaturization, high efficiency and stable performance are presented, the limitation of a traditional laser in the aspects of conversion efficiency and size is thoroughly broken through, and the energy conversion efficiency is improved. The method has the advantages of good practicability, high universality and excellent market application prospect.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the fields of laser technology and material science, and further to a single-crystal optical fiber integrating fundamental frequency gain and nonlinear frequency conversion, and a preparation method and application thereof. Background Art

[0002] Laser technology, as one of the key tools of national industry, plays an irreplaceable role in many fields such as industrial manufacturing, medical treatment, national defense, scientific research, communication, cleaning and space technology. With the deepening of technology application, the requirements for laser performance are increasing, including increasing power, increasing energy, shortening pulse width, optimizing spectrum, expanding band and improving beam quality, etc., to meet a wider range of professional needs.

[0003] Nonlinear optical frequency conversion is an effective means to expand the laser band. It uses the second-order nonlinear effect of materials and derives a variety of lasers of different wavelengths through energy exchange between light waves of different frequencies, including visible blue-green light, ultraviolet light, and mid-infrared lasers. Each laser has its own unique application scenarios and advantages: visible blue-green lasers are mainly used for precision measurement, special material welding, optical data storage, and biomedical imaging; ultraviolet lasers, with their short wavelengths, can provide higher resolution and are suitable for laser lithography, semiconductor manufacturing, micromachining, and photochemical processing; mid-infrared lasers are particularly suitable for spectral analysis, medical diagnosis, and nonlinear optical research because their wavelengths are within the range of molecular vibration frequencies. However, this type of laser technology still faces some key issues, mainly: blue-green lasers face challenges in power enhancement and stability; the generation efficiency and equipment cost of ultraviolet lasers are relatively high; and mid-infrared lasers need to be further optimized in terms of light source availability and beam quality.

[0004] Gain crystals and nonlinear crystals are the core components of nonlinear frequency conversion lasers, and currently they are mainly in bulk form. Bulk crystals are widely used due to their high optical quality, large physical size, and good physical and chemical stability. However, the effective beam mode field in the laser is generally only tens to hundreds of microns, resulting in very limited utilization of bulk materials, limiting the applicability of certain portable or space-constrained scenarios, and the spatial walk-off effect in the nonlinear frequency conversion process cannot be effectively compensated, making it difficult to further improve energy utilization and beam quality.

[0005] Single-crystal optical fiber has a unique slender crystal structure and excellent optical waveguide confinement transmission capability, demonstrating its dual advantages in the field of laser amplification media. This structure not only optimizes heat dissipation efficiency and ensures high beam quality under high-power operating conditions, but also, compared with traditional bulk crystals, the excellent optical waveguide properties can significantly improve energy extraction efficiency and amplification gain. In addition, the simple traveling wave amplification structure of single-crystal optical fiber can further simplify the system integration process. These advantages of single-crystal optical fiber make it an ideal choice for high-power, high-energy ultrashort pulse laser amplification technology. It is widely used in key areas such as scientific research and industrial processing, showing its great potential in promoting technological innovation and application expansion.

[0006] Therefore, how to provide a single crystal optical fiber that supports nonlinear frequency conversion is an urgent problem to be solved by those skilled in the art. Summary of the invention

[0007] In view of the problems existing in the prior art, the purpose of the present invention is to provide a single crystal fiber integrating fundamental gain and nonlinear frequency conversion and its preparation method and application. A coupling-free integrated single crystal fiber is formed by cascading a fundamental gain single crystal fiber and one or more nonlinear single crystal fibers, wherein the fundamental gain single crystal fiber is used to generate fundamental frequency oscillation laser, and the nonlinear single crystal fiber is used to introduce nonlinear frequency conversion to expand the wavelength. The coupling-free integrated structure can effectively solve the coupling loss problem between the fundamental gain single crystal fiber and the nonlinear single crystal fiber, reduce the influence of the spatial walk-off effect of the nonlinear process, and improve the energy conversion efficiency. Using an integrated single crystal fiber instead of the traditional bulk crystal combination can significantly improve the heat management capability, improve the energy extraction efficiency, reduce material waste and reduce costs, and improve the system integration and miniaturization capability.

[0008] In order to achieve the above object, the present invention provides the following technical solutions: A single crystal fiber integrating fundamental frequency gain and nonlinear frequency conversion comprises a fundamental frequency gain single crystal fiber and one or more nonlinear single crystal fibers; one end of the fundamental frequency gain single crystal fiber is cascade-connected with one end of the one or more nonlinear single crystal fibers to form a coupling-free integrated structure; the fundamental frequency gain single crystal fiber is a doped single crystal fiber; the doped single crystal fiber comprises a matrix and luminescent ions; the one or more nonlinear single crystal fibers are single crystal fibers that can absorb the fundamental frequency laser and generate nonlinear frequency conversion.

[0009] In some embodiments, the matrix of the fundamental frequency gain single crystal optical fiber is yttrium vanadate (chemical formula: YVO4), gadolinium vanadate (chemical formula Gd(VO3)3), lutetium vanadate (chemical formula LuVO4), scandium vanadate (chemical formula ScVO4), yttrium aluminum garnet (chemical formula Y3Al5O 12 , referred to as YAG), lutetium aluminum garnet (chemical formula Lu3Al5O12 , referred to as LuAG), gadolinium aluminum garnet (chemical formula Gd3Al5O 12 , referred to as GAG or GdAG), gadolinium gallium garnet (chemical formula Gd3Ga5O 12 , referred to as GGG), lutetium yttrium aluminum garnet (chemical formula Lu 3-x Y x Al5O 12 , referred to as LuYAG), lutetium gadolinium aluminum garnet (chemical formula Lu 3-x G x Al5O 12 , referred to as LuGdAG), gadolinium yttrium aluminum garnet (chemical formula (Gd 1-x Y x )3Al5O 12 , referred to as GYAG or GdYAG), yttrium aluminum perovskite (chemical formula YAlO3, referred to as YAP), lutetium aluminate (chemical formula LuAlO3, referred to as LuAP), lutetium yttrium aluminum perovskite (chemical formula (Lu x Y 1-x )AlO3, referred to as LuYAP or (Lu,Y)AP), lutetium-scandium aluminum perovskite (chemical formula LuScAlO4, referred to as LuScAP), yttrium-scandium aluminum perovskite (chemical formula YAl 1-x Sc x O3, referred to as YScAP), sapphire (chemical formula Al2O3), lutetium oxide (chemical formula Lu2O3), yttrium oxide (chemical formula Y2O3), gadolinium oxide (chemical formula Gd2O3), lutetium yttrium mixed sesquioxide (chemical formula (Lu x Y 1-x )2O3, referred to as LuYO or Lu:Y2O3), lutetium-scandium mixed sesquioxide (chemical formula (Lu x Sc 1-x )2O3, referred to as LuScO or Lu:Sc2O3), yttrium-scandium mixed sesquioxide (chemical formula (Y x Sc 1-x )2O3, referred to as YScO or Y:Sc2O3), gallium fluoride (chemical formula GaF2), strontium fluoride (chemical formula SrF2), lanthanum fluoride (chemical formula LaF3), cerium fluoride (chemical formula CeF3), yttrium lithium fluoride (chemical formula LiYF4, referred to as YLF), lutetium lithium fluoride (chemical formula LiLuF4, referred to as LLF), lanthanum lithium fluoride (chemical formula LiLaF4, referred to as LLF), zinc selenide (chemical formula ZnSe), zinc sulfide (chemical formula ZnS), potassium gadolinium tungstate (chemical formula K2Gd(WO4)3, referred to as KGW), yttrium calcium oxyborate (chemical formula YCa4O(BO3)3, referred to as YCOB).

[0010] In some embodiments, the luminescent ion of the fundamental frequency gain single crystal optical fiber is cerium (Ce 3+ ), praseodymium (Pr 3+ ), Neodymium (Nd 3+ ), Samarium (Sm 3+ ), Europium (Eu 3+ ), terbium (Tb 3+ ), Dysprosium 3+ ), holmium (Ho 3+ ), Erbium 3+ ), Thulium (Tm 3+ ), Ytterbium (Yb 3+ )、Vanadium(V 3+ / V 2+ ), Lu 3+ )、Ti 3+ ), chromium (Cr 3+ / Cr 4+ ), cobalt (Co 2+ ), bismuth (Bi 3+ ), manganese (Mn 2+ / Mn 3+ ), iron (Fe 2+ / Fe 3 + ), copper (Cu 3+ ) elements.

[0011] The nonlinear single crystal optical fiber supports nonlinear frequency conversion processes, mainly including frequency doubling, sum frequency, difference frequency, optical parametric oscillation / amplification, etc.

[0012] In some embodiments, the one or more nonlinear single crystal optical fibers are potassium dihydrogen phosphate (chemical formula KH2PO4, referred to as KDP), ammonium dihydrogen phosphate (chemical formula NH4H2PO4, referred to as ADP), lithium triborate (chemical formula LiB3O5, referred to as LBO), cesium borate (chemical formula CsB3O5, referred to as CBO), barium metaborate (chemical formula BaB2O4, referred to as BBO), potassium titanium phosphate (chemical formula KTiOPO4, referred to as KTP), lithium yttrium fluoride (chemical formula LiYF4, referred to as YLF), lithium neodymium fluoride (referred to as Nd:YLF), zinc selenide (chemical formula ZnSe), zinc sulfide (chemical formula ZnS), lithium niobate (chemical formula LiNbO3), yttrium aluminum garnet (chemical formula: Y3Al5O 12, referred to as YAG), gadolinium vanadate (chemical formula GdVO4), lutetium fluoride (chemical formula LuLiF4, referred to as LLF), gallium arsenide (chemical formula GaAs), gallium phosphide (chemical formula GaP), silver gallium sulfide (chemical formula AgGaS2), silver gallium selenide (chemical formula AgGaSe2), cadmium selenide (chemical formula CdSe), yttrium calcium oxyborate (chemical formula YCa4O(BO3)3, referred to as YCOB), neodymium aluminum garnet (chemical formula NdAlO4, referred to as Nd:YAP), neodymium gadolinium oxyborate (chemical formula Nd 3-x G x Ca4O(BO3)3, referred to as Nd:GdCOB).

[0013] In some embodiments, the diameter of the single crystal optical fiber integrating fundamental frequency gain and nonlinear frequency conversion is 0.01-1 mm.

[0014] Preferably, the side of the single-crystal optical fiber integrating fundamental frequency gain and nonlinear frequency conversion is induced and modified by femtosecond laser processing to form a low-refractive index microstructure cladding structure, thereby enhancing the light guiding ability of the single-crystal optical fiber and compensating for the spatial walk-off effect in the nonlinear frequency conversion process.

[0015] Preferably, the end faces of both sides of the fundamental frequency gain and nonlinear frequency conversion integrated single crystal optical fiber are coated with optical films, one end of the fundamental frequency gain single crystal optical fiber is coated with a pump light anti-reflection film and a fundamental frequency light total reflection film, and one end of the nonlinear single crystal optical fiber is coated with a fundamental frequency light total reflection film and a frequency conversion light high transmittance film.

[0016] The present invention includes a method for preparing the single crystal optical fiber integrating fundamental frequency gain and nonlinear frequency conversion, comprising the following steps: S1 preparing a crystal rod: cascading and bonding a fundamental frequency gain bulk crystal and one or more nonlinear bulk crystals by bonding to form a rod suitable for growth; S2 single crystal optical fiber growth: adopting any one of a laser heating pedestal method, a pedestal method, a guided mode method, and a micro-pull-down method to prepare the single crystal optical fiber integrating fundamental frequency gain and nonlinear frequency conversion.

[0017] In some embodiments, the fundamental frequency gain bulk crystal and one or more nonlinear bulk crystals are ground and polished, and then cleaned and coated with photoresist, and then placed in a vacuum hot press furnace for heat treatment to complete cascade crystal bonding and manufacture into a material rod suitable for growth.

[0018] In some embodiments, when the growth method is a laser heating susceptor method, the following steps are included: S21 equipment setting: select a high-purity material rod made by bonding, set the laser, focusing system, pulling mechanism and temperature control system; S22 laser heating: generate a stable annular heat source through the laser and optical components to melt the top of the material rod to form a stable molten zone; S23 seed crystal introduction: place the seed crystal above the molten zone, accurately position the seed crystal and the melt, and start crystal growth; S24 crystal growth: synchronously control the pulling speed and material rod feeding to form a single crystal optical fiber; S25 growth parameter control: dynamically adjust the laser power and growth rate to ensure the quality of the single crystal optical fiber; S26 crystal quality monitoring: implement optical monitoring to ensure defect-free growth; S27 end of growth: terminate laser heating in time to accurately control the crystal length; S28 post-processing: perform annealing, precision machining and coating post-processing to complete the preparation of the single crystal optical fiber with integrated fundamental gain and nonlinear frequency conversion. The advantages of the laser heating susceptor method are that it does not require a crucible, has high growth efficiency, and is suitable for preparing single crystal optical fibers with a high aspect ratio.

[0019] The present invention also provides a miniaturized, high-conversion-efficiency nonlinear single-crystal fiber laser, which can change the problems of low conversion efficiency and large size of traditional lasers. The nonlinear single-crystal fiber laser adopts a linear cavity design, comprising a semiconductor laser, a coupling lens group, and the single-crystal fiber integrated with fundamental gain and nonlinear frequency conversion. The semiconductor laser is used to provide pump light, and the central wavelength corresponds to the absorption peak of the fundamental gain single-crystal fiber; the pump light is shaped by the coupling lens group and coupled into the single-crystal fiber integrated with fundamental gain and nonlinear frequency conversion in a matching mode field, and partially excites the fundamental laser in the fundamental gain single-crystal fiber, and further excites the nonlinear process in the nonlinear single-crystal fiber to generate frequency conversion laser; the single-crystal fiber integrated with fundamental gain and nonlinear frequency conversion is coated at both ends to form a resonant cavity, thereby obtaining a stable laser output. This type of laser has the characteristics of miniaturization, high efficiency, and stable performance.

[0020] Compared with the prior art, the present invention can bring the following beneficial effects: The present invention provides a single crystal fiber with integrated fundamental gain and nonlinear frequency conversion, and a preparation method and application thereof. The uncoupled integrated design of the single crystal fiber effectively eliminates the laser coupling loss between traditional single crystal fibers, thereby significantly improving the energy conversion efficiency. Compared with the traditional bulk crystal combination, the use of integrated single crystal fiber greatly enhances the heat management capability, improves the energy extraction efficiency, and reduces material consumption and costs. In addition, by processing the microstructure on the side of the single crystal fiber to form a low refractive index cladding, the optical waveguide capability is enhanced, and the spatial walk-off effect in the nonlinear frequency conversion process is effectively compensated. The single crystal fiber is prepared by a laser heating base method, which has the characteristics of no need to use a crucible and high growth efficiency, and is particularly suitable for preparing single crystal fibers with a high aspect ratio. Nonlinear single crystal fiber lasers show the advantages of miniaturization, high efficiency and performance stability, and completely solve the limitations of traditional lasers in conversion efficiency and volume. In summary, the integrated single crystal fiber and related technologies provided by the present invention, with its excellent practicality, wide applicability and broad market application prospects, represent a major advancement in the field of laser technology.

[0021] The preferred implementation modes will be described below in a clearer and easier to understand manner with reference to the accompanying drawings to further illustrate the characteristics, technical features, advantages and implementation methods of the present invention. BRIEF DESCRIPTION OF THE DRAWINGS

[0022] The drawings that constitute a part of this application are used to provide further understanding of this application. The illustrative embodiments of this application and their descriptions are used to explain this application and do not constitute improper limitations on this application.

[0023] In addition, the terms "installed", "set", "provided with", "connected", "connected", and "socketed" should be understood in a broad sense. For example, it can be a fixed connection, a detachable connection, or an integral structure; it can be a mechanical connection or an electrical connection; it can be a direct connection, or an indirect connection through an intermediate medium, or it can be an internal connection between two devices, elements, or components. For those of ordinary skill in the art, the specific meanings of the above terms in this application can be understood according to specific circumstances.

[0024] In the attached picture: Figure 1 This is a schematic diagram of the structure of a single-crystal optical fiber integrating fundamental frequency gain and nonlinear frequency conversion according to the present invention; Figure 2 This is a flow chart of preparing a double-crystal series-connected integrated single-crystal optical fiber by the laser heating base method in Example 3; Figure 3 This is a flow chart of preparing three-crystal series-connected integrated single-crystal optical fiber by laser heating base method in Example 3; Figure 4 This is a schematic diagram of the structure of the nonlinear single-crystal fiber laser of the present invention. DETAILED DESCRIPTION

[0025] The following will be combined with specific embodiments to clearly and completely describe the technical solutions in the present invention. The following embodiments are only used to more clearly illustrate the preferred technical solutions of the present invention, and cannot be used to limit the protection scope of the present invention. Example

[0026] Nd:YAG fundamental frequency gain and LBO nonlinear frequency conversion integrated single crystal fiber and its application Figure 1 The single crystal fiber structure of Nd:YAG fundamental frequency gain and LBO nonlinear frequency conversion integrated provided by this embodiment is shown. The structure of the traditional bulk crystal combination in the prior art has the advantages of high laser damage threshold, high optical surface quality and mature technology, but the volume and weight are relatively large and heavy, and the optical alignment is relatively complicated; although the conventional single crystal fiber structure brings the characteristics of high thermal conductivity, compact size and easy integration, there is a large coupling light loss between the single crystal fibers; the single crystal fiber integrated with fundamental frequency gain and nonlinear frequency conversion provided by the present invention is a coupling-free structure, which avoids coupling light loss, and also has the advantages of convenient heat management and easy integration.

[0027] The fundamental frequency gain and nonlinear frequency conversion integrated single crystal fiber 130 of this embodiment includes a fundamental frequency gain single crystal fiber 107 and a nonlinear single crystal fiber 108, which are connected to form an integrated structure without coupling, such as Figure 1 The fundamental frequency gain single crystal fiber 107 is a doped single crystal fiber, including a matrix and luminescent ions; the nonlinear single crystal fiber 108 is a single crystal fiber that can absorb fundamental frequency laser and generate nonlinear frequency conversion.

[0028] In this embodiment, the matrix of the fundamental frequency gain single crystal optical fiber 107 is YAG (yttrium aluminum garnet, chemical formula: Y3Al5O 12 ), the luminescent ion is Nd 3+ (neodymium ion), the nonlinear single crystal fiber 108 is LBO (lithium triborate, chemical formula LiB3O5).

[0029] It should be noted that the matrix and luminescent ion elements listed in this embodiment are only a preferred embodiment of the present invention, and the purpose is to further illustrate the present invention. It should not be understood as limiting the scope of the single crystal optical fiber material system integrating fundamental frequency gain and nonlinear frequency conversion of the present invention. Some non-essential improvements and adjustments made by technicians in this field based on the above content of the present invention all fall within the scope of protection of the present invention.

[0030] In this embodiment, the diameter of the single crystal optical fiber 130 integrating Nd:YAG fundamental frequency gain and LBO nonlinear frequency conversion is 0.1 mm.

[0031] Preferably, this embodiment uses femtosecond laser to process the Nd:YAG fundamental frequency gain single crystal fiber 107 and the LBO nonlinear single crystal fiber 108 to induce their modification, forming a low refractive index microstructure cladding structure to enhance the single crystal fiber light field confinement capability, with the purpose of compensating for the spatial walk-off effect in the nonlinear frequency conversion process.

[0032] Preferably, in this embodiment, one end of the Nd:YAG fundamental frequency gain single crystal fiber 107 is coated with an 808 nm anti-reflection film and a 1064 nm total reflection film 111 , and one end of the LBO nonlinear single crystal fiber 108 is coated with a 1064 nm total reflection film and a 532 nm high transmittance film 112 .

[0033] On this basis, this embodiment provides a specific application method of the above-mentioned Nd:YAG fundamental frequency gain and LBO nonlinear frequency conversion integrated single crystal optical fiber 130, namely Figure 4 The miniature green light single crystal fiber laser shown in FIG. The laser adopts a simple and compact linear cavity design, and its components include: semiconductor laser 114, coupling lens group 115, and integrated single crystal fiber 130. Among them, the semiconductor laser 114 adopts butterfly packaging and pigtail output, and can stably emit 808nm laser radiation through temperature control, and the output laser mode field area is about 105 microns; the coupling lens group 115 is composed of a pair of coupling lenses with a focusing ratio of 2:1, and its function is to collimate and focus the pump light to less than 100 microns.

[0034] In specific implementation, the 808nm pump light first passes through the coupling lens group 115, is focused into the Nd:YAG fundamental frequency gain single crystal fiber 107, is absorbed and radiates the 1064nm fundamental frequency light, and part of the 1064nm fundamental frequency light is then generated into 532nm frequency conversion light through the frequency doubling effect of the LBO nonlinear single crystal fiber 108. Since the light-incoming and light-outgoing surfaces of the single crystal fiber are both coated with 1064nm high-reflection films 111 and 112, the integrated single crystal fiber 130 is a 1064nm fundamental frequency light resonant cavity, and only 532nm frequency conversion light can be emitted. This wavelength is in the green light range, that is, a green light laser. This type of laser has the characteristics of miniaturization, high efficiency, and stable performance, and can change the problems of low conversion efficiency and large size of traditional bulk crystal lasers. Example

[0035] Nd:YVO4 fundamental frequency gain and double BBO nonlinear frequency conversion integrated single crystal fiber and its application Figure 1The single crystal fiber structure of Nd:YVO4 fundamental frequency gain and double BBO nonlinear frequency conversion integrated provided by this embodiment is shown. The structure of the traditional bulk crystal combination in the prior art, especially the difference in phase matching between the frequency doubling and sum frequency bulk crystals, will bring about serious spatial walk-off effect, which will eventually affect the conversion efficiency and the beam quality of the nonlinear laser; the present invention provides a single crystal fiber with a coupling-free structure that integrates fundamental frequency gain and nonlinear frequency conversion. The microstructure cladding structure can provide a perfect energy field confinement effect, avoid coupling light loss, and well compensate for the spatial walk-off effect, thereby improving the energy conversion efficiency.

[0036] The fundamental frequency gain and nonlinear frequency conversion integrated single crystal fiber 170 of this embodiment includes a fundamental frequency gain single crystal fiber 107, a first nonlinear single crystal fiber 108 and a second nonlinear single crystal fiber 109, which are connected to form an integrated structure without coupling, such as Figure 1 As shown. The fundamental frequency gain single crystal fiber 107 is a doped single crystal fiber, including a matrix and luminescent ions; the first nonlinear single crystal fiber 108 is a single crystal fiber that can absorb fundamental frequency laser, stimulate nonlinear frequency conversion and generate first frequency conversion light; the second nonlinear single crystal fiber 109 is a single crystal fiber that can absorb fundamental frequency laser and first frequency conversion light, stimulate nonlinear frequency conversion and generate second frequency conversion light.

[0037] In this embodiment, the matrix of the fundamental frequency gain single crystal optical fiber 107 is YVO4 (yttrium vanadate), and the luminescent ion is Nd 3+ (neodymium ion), the first nonlinear single crystal fiber 108 is BBO (barium borate, chemical formula BaB2O4), and the second nonlinear single crystal fiber 109 is BBO (barium borate, chemical formula BaB2O4).

[0038] It should be noted that the matrix and luminescent ion elements listed in this embodiment are only a preferred embodiment of the present invention, and the purpose is to further illustrate the present invention. It should not be understood as limiting the scope of the single crystal optical fiber material system integrating fundamental frequency gain and nonlinear frequency conversion of the present invention. Some non-essential improvements and adjustments made by technicians in this field based on the above content of the present invention all fall within the scope of protection of the present invention.

[0039] In this embodiment, the diameter of the single crystal optical fiber 170 integrating the Nd:YVO4 fundamental frequency gain and double BBO nonlinear frequency conversion is 0.1 mm.

[0040] Preferably, this embodiment uses femtosecond laser to process the Nd:YVO4 fundamental frequency gain single crystal fiber 107, the BBO first nonlinear single crystal fiber 108 and the BBO second nonlinear single crystal fiber 109 to induce their side modifications to form a low refractive index microstructure cladding structure to enhance the single crystal fiber light field confinement capability, with the aim of compensating for the spatial walk-off effect during the nonlinear frequency conversion process.

[0041] Preferably, in this embodiment, one end of the Nd:YVO4 fundamental frequency gain single crystal fiber 107 is coated with an 808nm anti-reflection film, a 1064nm total reflection film and a 532nm total reflection film 111, and one end of the BBO second nonlinear single crystal fiber 109 is coated with a 355nm high-transmittance film, a 532nm total reflection film and a 1064nm total reflection film 113.

[0042] On this basis, this embodiment provides a specific application method of the above-mentioned Nd:YVO4 fundamental frequency gain and double BBO nonlinear frequency conversion integrated single crystal optical fiber 170, namely Figure 4 The miniature ultraviolet single-crystal fiber laser shown in FIG. The laser adopts a simple and compact linear cavity design, and its components include: semiconductor laser 114, coupling lens group 115, and integrated single-crystal fiber 170. Among them, the semiconductor laser 114 adopts a butterfly package and a pigtail output, and can stably emit 808nm laser radiation through temperature control, and the output laser mode field area is about 105 microns; the coupling lens group 115 is composed of a pair of coupling lenses with a focusing ratio of 2:1, and its function is to collimate and focus the pump light to less than 100 microns.

[0043] In specific implementation, the 808nm pump light first passes through the coupling lens group 115, is focused into the Nd:YVO4 fundamental frequency gain single crystal fiber 107, is absorbed and radiates the 1064nm fundamental frequency light, and part of the 1064nm fundamental frequency light is then subjected to the frequency doubling effect of the BBO first nonlinear single crystal fiber 108 to generate the 532nm first frequency conversion light, and the remaining 1064nm fundamental frequency light and the 532nm first frequency conversion light are finally subjected to the sum frequency effect of the BBO second nonlinear single crystal fiber 109 to generate the 355nm second frequency conversion light. Since the light-incoming and light-outgoing surfaces of the single crystal fiber are both coated with 1064nm and 532nm high-reflection films 111 and 113, the integrated single crystal fiber 170 is a resonant cavity of the 1064nm fundamental frequency light and the 532nm first frequency conversion light, and only the 355nm second frequency conversion light can be emitted, and this wavelength is in the ultraviolet range, that is, an ultraviolet laser. This type of laser has the characteristics of miniaturization, high efficiency and stable performance, and can change the problems of low conversion efficiency and large size of traditional bulk crystal lasers. Example

[0044] Preparation method of single crystal optical fiber with integrated fundamental frequency gain and nonlinear frequency conversion On the basis of Examples 1 and 2, the present invention further provides a method for preparing the above-mentioned single crystal optical fiber 130, 170 integrating fundamental frequency gain and nonlinear frequency conversion, such as Figure 2 , 3 As shown, the following steps are included: (the LBO nonlinear single crystal fiber 108 and the BBO first nonlinear single crystal fiber 108 in embodiments 1 and 2 are collectively referred to as the first nonlinear single crystal fiber 108): Step S1: preparing the material rod: grinding and polishing the fundamental frequency gain bulk crystal 101, the first nonlinear bulk crystal 102 and the second nonlinear bulk crystal 103, and then cleaning and photoresisting them, and then putting them into a vacuum hot press furnace for heat treatment to complete cascade crystal bonding and make material rods 100 and 140 suitable for growth; Step S2: Optical fiber growth: Use any one of the laser heating pedestal method, pedestal method, guided mode method, and micro-pull-down method to prepare the single crystal optical fiber with integrated fundamental frequency gain and nonlinear frequency conversion. Specifically, the growth method of this embodiment is the laser heating pedestal method, which is as follows: Step S21 Equipment setting: fix the bonded crystal rods 100 and 140 on a laser heating base device, the device including a laser source, a focusing system, a lifting mechanism, a temperature control system, etc.; Step S22: Introducing the seed crystal: placing the seed crystal cut into a specific shape above the crystal rods 100 and 140. Since the fundamental frequency gain bulk crystal 101, the first nonlinear bulk crystal 102 and the second nonlinear bulk crystal 103 on the rods have been bonded and connected in sequence, the other end of the fundamental frequency gain bulk crystal 101 is fixed on the lower rod, and the seed crystal containing the single crystal optical fiber matrix material is fixed on the seed crystal rod, while the other end of the second nonlinear bulk crystal 103 faces the seed crystal. At the same time, the positions of the crystal rods 100 and 140 and the seed crystal are adjusted so that they are on the same straight line as the laser focusing point.

[0045] Step S23: Laser heating: the furnace chamber is sealed and evacuated, nitrogen is introduced to adjust the furnace chamber pressure to 1.008 MPa, and the heat generated by the CO2 laser is used to form a ring heat source through a focusing system to heat the top of the material rod to melt it and form a stable melting zone. After the melting zone forms a hemispherical melt, the seed crystal is contacted with the melt; Step S24: crystal growth: after the seed crystal contacts the melt, the power is adjusted and observed for 2 minutes until the connection is stable, and then the seed crystal is slowly pulled up at a pulling speed of 20 mm / h, while the material rod feeding speed is controlled at 6.98 mm / h, so that the melt crystallizes at the seed crystal to form single crystal optical fibers 110 and 150; Step S25 Growth parameter control: accurately control the pulling speed, laser power, feeding speed and other parameters to ensure the quality and diameter uniformity of the single crystal optical fiber; Step S26 Crystal quality monitoring: Use an optical microscope or a CCD camera to monitor the growth process in real time to ensure that the crystal grows without defects; Step S27 Growth end: When the expected length is reached, the laser power is gradually reduced, the time is set to 1 hour, the pulling and feeding are stopped, the growth is ended, and the optical fiber is taken out after the temperature of the single crystal optical fiber 110, 150 and the cavity of the heating base furnace drops to room temperature; Step S28 Post-processing: Annealing the single crystal optical fiber to eliminate stress Step S29 Cladding processing: femtosecond laser is used to process the side surfaces of the single crystal optical fibers 110 and 150 to induce modification thereof, thereby forming a low refractive index microstructure cladding structure, and obtaining single crystal optical fibers 120 and 160 with strong light field confinement capability.

[0046] Step S30: End face coating: performing post-processing such as cutting, grinding, polishing and coating on the single crystal optical fibers 120 and 160 to form the single crystal optical fibers 130 and 170 integrating fundamental frequency gain and nonlinear frequency conversion.

[0047] The specific embodiments of the present invention are described in detail above, but they are only examples, and the present invention is not limited to the specific embodiments described above. For those skilled in the art, any equivalent modifications and substitutions made to the present invention are also within the scope of the present invention. Therefore, the equalization changes and modifications made without departing from the spirit and scope of the present invention should be included in the scope of the present invention.

Claims

1. A single crystal optical fiber with integrated fundamental frequency gain and nonlinear frequency conversion, It is characterized in that It includes a fundamental frequency gain single crystal fiber and one or more nonlinear single crystal fibers; One end of the fundamental frequency gain single crystal optical fiber is cascade-connected with one end of the one or more nonlinear single crystal optical fibers to form a coupling-free integrated structure; The fundamental frequency gain single crystal optical fiber is a doped single crystal optical fiber; The doped single crystal optical fiber includes a matrix and luminescent ions; The one or more nonlinear single crystal optical fibers are single crystal optical fibers that can absorb the fundamental frequency laser and stimulate nonlinear frequency conversion; The matrix of the fundamental frequency gain single crystal optical fiber is YVO 4 、Gd(VO 3 ) 3 、LuVO 4 ScVO 4 , YAG, LuAG, GAG, GGG, LuYAG, LuGdAG, GYAG, YAP, LuAP, LuYAP, LuScAP, YScAP, Al 2 O 3 、Lu 2 O 3 , Y 2 O 3 , Gd 2 O 3 、LuYO、LuScO、YScO、GaF 2 , SrF 2 、LaF 3 , CeF 3 , any one of YLF, LLF, ZnSe, ZnS, KGW, YCOB; The luminescent ion of the fundamental frequency gain single crystal optical fiber is Ce 3+ , Pr 3+ 、Nd 3+ 、Sm 3+ 、Eu 3+ , Tb 3+ 、Dy 3+ 、Ho 3+ , Er 3+ 、Tm 3 + , Yb 3+ 、V 3+ / V 2+ 、Lu 3+ 、Ti 3+ Cr 3+ / Cr 4+ 、Co 2+ 、Bi 3+ , Mn 2+ / Mn 3+ , Fe 2+ / Fe 3+ , Cu 3+ Any one or more of the following.

2. The single crystal optical fiber integrating fundamental frequency gain and nonlinear frequency conversion according to claim 1, It is characterized in that The nonlinear single crystal optical fiber supports nonlinear frequency conversion processes, mainly including frequency doubling, sum frequency, difference frequency, optical parametric oscillation / amplification processes, etc.

3. The single crystal optical fiber integrating fundamental frequency gain and nonlinear frequency conversion according to claim 1, It is characterized in that The one or more nonlinear single crystal optical fibers are KDP, ADP, LBO, CBO, BBO, KTP, YLF, Nd:YLF, ZnSe, ZnS, LiNbO 3 、YAG、GdVO 4 、LLF、GaAs、GaP、AgGaS 2 、AgGaSe 2 , CdSe, YCOB, Nd:YAP, Nd:GdCOB.

4. The single crystal optical fiber integrating fundamental frequency gain and nonlinear frequency conversion according to claim 1, It is characterized in that The diameter of the single crystal optical fiber integrating fundamental frequency gain and nonlinear frequency conversion is 0.01-1 mm.

5. The single crystal optical fiber integrating fundamental frequency gain and nonlinear frequency conversion according to claim 1, It is characterized in that The baseband gain and nonlinear frequency conversion integrated single crystal optical fiber is modified by femtosecond laser processing on its side surface to form a low refractive index microstructure cladding structure, thereby enhancing the light guiding ability of the single crystal optical fiber and compensating for the spatial walk-off effect in the nonlinear frequency conversion process.

6. The single crystal optical fiber integrating fundamental frequency gain and nonlinear frequency conversion according to claim 1, It is characterized in that The fundamental frequency gain and nonlinear frequency conversion integrated single crystal optical fiber has optical film coated on both end faces, one end of the fundamental frequency gain single crystal optical fiber is coated with a pump light anti-reflection film and a fundamental frequency light total reflection film, and one end of the nonlinear single crystal optical fiber is coated with a fundamental frequency light total reflection film and a frequency conversion light high transmittance film.

7. A method for preparing a single crystal optical fiber integrating fundamental frequency gain and nonlinear frequency conversion according to any one of claims 1 to 6, It is characterized in that The steps include: Step S1: preparing a crystal rod: bonding a fundamental frequency gain bulk crystal and one or more nonlinear bulk crystals in cascade connection to form a rod suitable for growth; Step S2: Single crystal optical fiber growth: adopt any one of a laser heating pedestal method, a pedestal method, a guided mode method, and a micro-pull-down method to prepare the single crystal optical fiber integrating fundamental frequency gain and nonlinear frequency conversion.

8. The preparation method according to claim 7, It is characterized in that When the growth method is a laser heating susceptor method, the method comprises the following steps: Step S21: Equipment setting: Select the high-purity material rod made by bonding, and set the laser, focusing system, lifting mechanism and temperature control system; Step S22: Laser heating: A stable annular heat source is generated by a laser and an optical component to melt the top of the material rod to form a stable molten zone; Step S23: Seed crystal introduction: placing the seed crystal above the melting zone, accurately positioning the seed crystal and the melt, and starting crystal growth; Step S24: Crystal growth: synchronously controlling the pulling speed and the feeding of the material rod to form a single crystal optical fiber; Step S25: Growth parameter control: dynamically adjust the laser power and growth rate to ensure the quality of the single crystal optical fiber; Step S26: Crystal quality monitoring: optical monitoring is performed to ensure defect-free growth; Step S27: End of growth: terminate laser heating at an appropriate time and precisely control the crystal length; Step S28: Post-processing: annealing the single crystal optical fiber to eliminate stress; Step S29: Cladding processing: using femtosecond laser to process the side of the single crystal optical fiber to induce modification, forming a low refractive index microstructure cladding structure; Step S30: Coating treatment: After cutting, grinding, polishing and coating treatment, the single crystal optical fiber integrating fundamental frequency gain and nonlinear frequency conversion is obtained.

9. Application of a single crystal optical fiber integrating fundamental frequency gain and nonlinear frequency conversion, It is characterized in that The single crystal optical fiber with integrated fundamental frequency gain and nonlinear frequency conversion as described in any one of claims 1 to 6 or prepared by the preparation method in claims 7 to 8 can be applied to nonlinear single crystal optical fiber lasers; The nonlinear single crystal fiber laser adopts a linear cavity design and comprises a semiconductor laser, a coupling lens group and a single crystal fiber integrating fundamental frequency gain and nonlinear frequency conversion.

10. Application of the single crystal optical fiber integrating fundamental frequency gain and nonlinear frequency conversion according to claim 9, It is characterized in that The semiconductor laser is used to provide pump light, and the central wavelength corresponds to the absorption peak of the fundamental frequency gain single crystal fiber; the pump light is shaped by the coupling lens group and coupled into the fundamental frequency gain single crystal fiber in a matching mode field to partially excite the fundamental frequency laser, and further excites the nonlinear process in the nonlinear single crystal fiber to generate frequency conversion laser.

Citation Information

Patent Citations

  • Infrared laser in self-optical parametric oscillation of double-cavity composite unsteady cavity mode selection pump

    CN107528197A

  • All-crystal optical fiber and cladding making technology

    CN108418085A

  • Sesquioxide monocrystal optical fibers and preparation method and application thereof

    CN108977882A

  • Rare earth doped (LuaScbYc)2O3 (a + b + c = 1)single crystal optical fiber, and preparation method and application thereof

    CN112281213A

  • Crystal fiber pump light coupling system and method and application thereof

    CN116131080A