Powder coating device

By using multiple scrapers in dry powder coating technology for high-frequency vibration and staggered arrangement, the problem of weight deviation per unit area of ​​the powder layer is solved, and a powder coating effect with high performance and low environmental burden is achieved.

CN118765218APending Publication Date: 2024-10-11PANASONIC INTELLECTUAL PROPERTY MANAGEMENT CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202280092920.3
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Priority Date
2022-03-11
Filing Date
2022-12-08
Publication Date
2024-10-11

AI Technical Summary

Technical Problem

In the existing dry powder coating technology, the unit area weight of the powder layer has a large deviation in the width direction, resulting in coating unevenness.

Method used

Multiple scrapers are used to perform natural vibration at frequencies above 2 kHz and below 300 kHz. The first scraper is located in front of the second scraper, and the second scraper is staggered by four points along the width direction of the powder layer relative to the first scraper. One wavelength, through high-frequency vibration near the ultrasonic band, the fluidity of the powder is improved to ensure uniform supply and adjustment of the powder layer.

Benefits of technology

It effectively reduces the weight deviation per unit area of ​​the powder layer, improves the uniformity and quality of coating, reduces the uneven structure of the powder layer, and forms a powder layer with high performance and low environmental burden.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118765218A_ABST
    Figure CN118765218A_ABST
Patent Text Reader

Abstract

The powder coating device is provided with a first-stage blade (11) and a second-stage blade (12) for adjusting the thickness of the supplied powder (3), and the first-stage blade (11) and the second-stage blade (12) perform natural vibration at a frequency of 2 kHz or more and 300 kHz or less. The second-stage blade (12) is shifted from the first-stage blade (11) by a quarter wavelength of the natural vibration in the width direction of the powder (3) supplied to the surface of the sheet (4).
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to a powder coating device. Background Art

[0002] In recent years, compared with the wet coating method in which the powder is dispersed in a solvent and then applied, the dry coating method in which the powder is directly applied has attracted attention as a method for forming a powder layer with high performance and low environmental burden. This is because according to the dry coating method, a powder layer can be obtained in which material damage caused by the solvent is less, high performance can be maintained, the solvent does not need to be dried, and energy consumption can be greatly reduced.

[0003] As a method of dry-coating powder, there is conventionally known a technique of conveying a member such as a metal foil by a conveying device and coating the powder on the surface of the member.

[0004] For example, a technique for applying powder on the surface of a long metal foil is disclosed in Patent Document 1. Patent Document 1 describes that after the powder is supplied onto the surface of the metal foil, the powder is flattened with a scraper to adjust the thickness of the powder to be uniform. Figure 5 2 is a diagram showing a scraper 26 of a conventional powder coating device 21. Figure 6 The figures show how the scraper 26 of the conventional powder coating device 21 is viewed from above, and how the applied powder layer 25 is viewed from the front. Figure 6 (a) is a diagram showing a state in which the scraper 26 is naturally vibrating with a sinusoidal standing wave (showing a state in which it is viewed from the front) when the scraper 26 is viewed from above. Figure 6 (b) is a diagram showing a state where the powder layer 25 applied to the sheet 24 is viewed from the front.

[0005] like Figure 5 As shown, the scraper 26 vibrates at a high frequency near the ultrasonic band (frequency is 2 kHz to 300 kHz), and the vibration is transmitted to the powder 23 to improve the fluidity of the powder 23, thereby achieving coating without powder clogging.

[0006] like Figure 6 As shown in (a) of FIG. 1 , when the scraper 26 is vibrated at a high frequency, the scraper 26 vibrates as a sinusoidal standing wave due to the natural vibration. Figure 6 As shown in (b) of FIG. 1 , a concavo-convex structure cut into a sinusoidal standing wave shape is formed in the powder layer 25 that has passed through the gap of the scraper 26 .

[0007] Prior art literature

[0008] Patent Literature

[0009] Patent Document 1: Japanese Patent Application Publication No. 2021-178271 Summary of the invention

[0010] The powder coating device of the present invention comprises: a driving device, which moves a component in a specified direction; a powder supplying device, which supplies powder to the surface of the component; and a first scraper and a second scraper, which are arranged in a manner to form a gap with the component, and adjust the thickness of the powder supplied to the surface of the component by the powder supplying device, the first scraper and the second scraper perform natural vibration at a frequency of not less than 2 kHz and not more than 300 kHz, the first scraper is located at a position closer to the supply side of the powder than the second scraper, and the second scraper is offset relative to the first scraper by a quarter wavelength of the natural vibration along the width direction of the powder supplied to the surface of the component. BRIEF DESCRIPTION OF THE DRAWINGS

[0011] Figure 1 This is a schematic diagram showing a powder coating apparatus according to one embodiment of the present invention.

[0012] Figure 2 This is a schematic diagram showing a part of a powder coating apparatus and a powder layer according to an embodiment of the present invention.

[0013] Figure 3 This is a schematic diagram showing a part of a powder coating apparatus and a powder layer according to an embodiment of the present invention.

[0014] Figure 4 This is a schematic diagram showing a part of a powder coating apparatus according to an embodiment of the present invention.

[0015] Figure 5 This is a schematic diagram showing a part of a conventional powder coating device.

[0016] Figure 6 This is a schematic diagram showing a part of a conventional powder coating apparatus and a powder layer. DETAILED DESCRIPTION

[0017] In the technique disclosed in Patent Document 1, the weight per unit area of ​​the powder layer varies in the coating width direction, and there is room for improvement when achieving uniformity.

[0018] An object of the present invention is to provide a powder coating apparatus capable of reducing the variation in weight per unit area caused by a concavo-convex structure cut into a sinusoidal standing wave shape on the surface of a powder layer.

[0019] It should be noted that the embodiments described below all show general or specific examples. The numerical values, shapes, materials, constituent elements, configuration positions and connection methods of constituent elements, steps, and the order of steps shown in the following embodiments are examples, and their purpose is not to limit the present invention. In addition, the constituent elements of the following embodiments that are not recorded in the independent technical solutions are described as arbitrary constituent elements.

[0020] In addition, each figure is a schematic diagram, and does not necessarily illustrate the figure strictly. In addition, in each figure, the same reference numeral is attached to the same structural member.

[0021] (summary)

[0022] The powder coating device of the present invention comprises: a driving device that moves a component in a predetermined direction; a powder supply device that supplies powder to the surface of the component; and a plurality of scrapers that are arranged in a manner to form a gap (hereinafter, also referred to as a gap) between the component and the powder supply device to adjust the thickness and unit area weight of the powder supplied to the surface of the component by the powder supply device. In addition, the plurality of scrapers vibrate naturally at a frequency of 2 kHz or more and 300 kHz or less. In the case where the plurality of scrapers include a first scraper and a second scraper, the first scraper is located at a position closer to the supply side of the powder than the second scraper. In addition, the second scraper is offset relative to the first scraper by a quarter wavelength of the natural vibration along the width direction of the powder supplied to the surface of the component.

[0023] Thus, the first scraper and the second scraper vibrate at a high frequency near the ultrasonic band (frequency of 2 kHz to 300 kHz), and the vibration is transmitted to the powder to improve the fluidity of the powder, thereby achieving coating without powder clogging.

[0024] In addition, when the first scraper and the second scraper are vibrated at a high frequency, the first scraper and the second scraper vibrate naturally with a sinusoidal standing wave. As a result, the surface of the powder layer that has passed through the gap between the first scraper and the component and the gap between the second scraper and the component is cut into a sinusoidal standing wave shape. Therefore, by setting the second scraper to be offset from the first scraper by a quarter wavelength of the natural vibration and arranging the first scraper and the second scraper in the traveling direction and in two stages, the second scraper can scrape off the portion with more unit area weight due to the first scraper. As a result, the deviation of the unit area weight of the powder layer in the width direction can be reduced.

[0025] Hereinafter, embodiments of the present invention will be described with reference to the drawings.

[0026] (Implementation Method)

[0027] Below, refer to Figure 1~Figure 4 An implementation method will be described.

[0028] Figure 1 1 is a schematic diagram showing a powder coating device 1 according to an embodiment of the present invention. Figure 2 as well as Figure 3 1 is a schematic diagram showing a part of a powder coating device 1 and a powder layer 5 according to an embodiment of the present invention. Figure 4 This is a schematic diagram showing a part of a powder coating apparatus 1 according to an embodiment of the present invention. Figure 2 (a) is a diagram showing a state where the first-stage scraper 11 and the second-stage scraper 12 are naturally vibrating with a sinusoidal standing wave when the first-stage scraper 11 and the second-stage scraper 12 are viewed from above (the diagram shows a state when viewed from the front). Figure 2 (b) is a diagram showing a state when the powder layer 5 applied to the sheet 4 is observed from the front. Figure 3 (a) is a diagram showing the first-stage scraper 11, the second-stage scraper 12, and the powder layer 5 when viewed from the lateral direction. Figure 3 (b) is a diagram showing a state when the powder layer 5 applied to the first-stage scraper 11, the second-stage scraper 12, and the sheet 4 is observed from the front. Figure 4 This is a diagram showing the situation where the first-level scraper 11, the second-level scraper 12, the third-level scraper 13 and the fourth-level scraper 14 are naturally vibrating with a sinusoidal standing wave when the first-level scraper 11, the second-level scraper 12, the third-level scraper 13 and the fourth-level scraper 14 are observed from above (the diagram shows the situation when observed from the front).

[0029] [Powder coating equipment]

[0030] like Figure 1 As shown, the powder coating device 1 includes: a conveying device (not shown) as a driving device, a powder supply device (not shown), a first-stage scraper 11 vibrating at a high frequency, and a second-stage scraper 12 vibrating at a high frequency. The first-stage scraper 11 is an example of a first scraper. The second-stage scraper 12 is an example of a second scraper.

[0031] A sheet-shaped member (hereinafter also referred to as a sheet 4) is conveyed along a traveling direction by a conveying device. The powder coating device 1 uses a powder supply device to continuously supply powder 3 to the surface of the conveyed sheet 4. In addition, the powder coating device 1 uses a first-stage scraper 11 and a second-stage scraper 12 to adjust the film thickness and filling rate of the powder 3 supplied to the surface of the sheet 4, so that the powder layer 5 has a desired unit area weight and reduces the deviation of the unit area weight.

[0032] The powder 3 is first conditioned by the first-stage scraper 11 and then conditioned by the second-stage scraper 12 .

[0033] Here, the weight per unit area refers to the value expressing the amount of powder per unit area in terms of weight. The unit of the weight per unit area is, for example, g / cm 2 express.

[0034] It should be noted that the conveying device may be any device as long as it can convey the sheet 4 , and is not particularly limited. The conveying device may be, for example, a conveying device that can continuously deliver the sheet 4 wound in a roll, or a conveying device that can intermittently deliver the sheet 4 .

[0035] It should be noted that guide rollers that rotate as the sheet 4 moves, a control device that corrects the meandering of the sheet 4, and the like may be provided on the conveyance path of the sheet 4 .

[0036] In the present embodiment, the sheet 4 is a long strip-shaped thin plate and is wound. It should be noted that the sheet 4 is not limited to a long strip-shaped thin plate. For example, after the sheet 4 of the desired shape is sent out from the conveying device and the coating of the powder 3 on the sheet 4 is completed, a new sheet 4 can be sent out from the conveying device. In addition, the sheet 4 may not be wound into a roll. In other words, the sheet 4 can be in a shape that can be coated with the powder 3 using the powder coating device 1. Therefore, the shape of the sheet 4 is not particularly limited. In addition, in the present embodiment, the sheet 4 is a collector including a metal foil, but the material of the component is not particularly limited. In other words, any component can be used as long as the sheet 4 is a component that can be coated with the powder 3 using the powder coating device 1.

[0037] The powder 3 may be any material as long as it is in powder form. That is, the raw material of the powder, the composition of the powder 3 and the particle shape of the powder 3 are not particularly limited. In the present embodiment, the powder 3 is a particle group containing a solid electrolyte.

[0038] The average particle size (D50) of the powder 3 is preferably 0.005 μm or more and 30 μm or less. In this case, the fluidity of the powder 3 is easily reduced, but since the retention and aggregation of the powder 3 are suppressed by the vibration of the first-stage scraper 11 and the second-stage scraper 12, a powder layer 5 with less deviation in weight per unit area can be formed. Here, the average particle size (D50) refers to the volume-based median particle size calculated from the measured value of the particle size distribution obtained by the laser diffraction / scattering method. The average particle size (D50) can be measured using a commercially available laser analysis / scattering particle size distribution measuring device.

[0039] In addition, the powder 3 may contain only one type of powder, or may contain two or more types of powder.

[0040] In the present embodiment, a hopper is used as a powder supply device. The hopper stores powder 3 inside and supplies powder 3 to the surface of the sheet 4. The hopper is arranged on the upstream side of the first-stage scraper 11 and the second-stage scraper 12 in the traveling direction of the sheet 4. The powder 3 supplied to the surface of the sheet 4 reaches the second-stage scraper 12 via the first-stage scraper 11 as the sheet 4 moves. It should be noted that in the present embodiment, a hopper is used as a powder supply device, but it is not limited to this. As a powder supply device, any device that can supply powder 3 to the surface of the sheet 4 can be used.

[0041] A predetermined gap is formed between the first scraper 11 and the second scraper 12 and the sheet 4. The powder 3 supplied to the surface of the sheet 4 passes through the gap. When the powder 3 passes through the gap, the first scraper 11 and the second scraper 12 adjust the film thickness and filling rate of the powder 3 supplied to the surface of the sheet 4, thereby reducing the deviation of the unit area weight of the powder layer 5.

[0042] (High frequency vibration near the ultrasonic band)

[0043] The first-stage scraper 11 and the second-stage scraper 12 vibrate at a frequency of 2 kHz or more and 300 kHz or less. That is, the first-stage scraper 11 and the second-stage scraper 12 vibrate at a high frequency near the ultrasonic band. Specifically, when the powder 3 supplied to the surface of the sheet 4 passes through the gap between the first-stage scraper 11 and the second-stage scraper 12 and the sheet 4, the first-stage scraper 11 and the second-stage scraper 12 vibrate at a high frequency near the ultrasonic band, thereby improving the fluidity of the powder 3 in the powder layer 5. Therefore, powder clogging is suppressed.

[0044] The fluidity of the powder 3 tends to be improved more easily as the frequency of the vibration of the first-stage scraper 11 and the second-stage scraper 12 is higher. Therefore, by vibrating the first-stage scraper 11 and the second-stage scraper 12 at a frequency of 2 kHz or more in the high-frequency region near the ultrasonic band, the fluidity of the powder 3 can be sufficiently improved. However, if the frequency is too high, the high frequency near the ultrasonic band is easily attenuated, so the vibration of the first-stage scraper 11 and the second-stage scraper 12 is not easily transmitted to the powder 3, but if the frequency is 300 kHz or less, the fluidity of the powder 3 can be sufficiently improved. By vibrating the first-stage scraper 11 and the second-stage scraper 12 at a high frequency near the ultrasonic band, the powder 3 in contact with the first-stage scraper 11 and the second-stage scraper 12 is not easily subjected to the friction resistance caused by the powder pressure, so that the fluidity is improved, thereby suppressing the retention and aggregation of the powder 3.

[0045] In addition, for the powder 3 located near the first scraper 11 and the second scraper 12, the friction between the powder particles is also reduced due to the vibration effect of the first scraper 11 and the second scraper 12, so that the fluidity is improved, thereby suppressing the aggregation of the powder 3.

[0046] Therefore, even if the powder 3 with a particle size of 30 μm or less and having low fluidity is used, the powder 3 passes through the above-mentioned gap without being retained or agglomerated by the vibrating first-stage scraper 11 and second-stage scraper 12 .

[0047] (Natural Vibration of the First-Stage Scraper 11 and the Second-Stage Scraper 12, and Configuration of the First-Stage Scraper 11 and the Second-Stage Scraper 12)

[0048] When the first-stage scraper 11 and the second-stage scraper 12 are vibrated at a high frequency near the ultrasonic band, the first-stage scraper 11 and the second-stage scraper 12 vibrate in a natural vibration (resonance state), and the first-stage scraper 11 and the second-stage scraper 12 vibrate in a sinusoidal standing wave.

[0049] like Figure 2 As shown in (a), when viewed from the front, the first-stage scraper 11 and the second-stage scraper 12 are arranged in such a manner that the antinode portion of the sine standing wave of the first-stage scraper 11 corresponds to the node portion of the sine standing wave of the second-stage scraper 12. In other words, the first-stage scraper 11 and the second-stage scraper 12 are arranged in such a manner that the node portion of the sine standing wave of the first-stage scraper 11 corresponds to the antinode portion of the sine standing wave of the second-stage scraper 12.

[0050] Specifically, a first-stage scraper 11 and a second-stage scraper 12 of the same shape are prepared, and they are made to vibrate in the same natural vibration state. Here, the same natural vibration state refers to a state in which the positions of the antinode part and the node part correspond to each other at the same position. For example, this state can be achieved by operating the first-stage scraper 11 and the second-stage scraper 12 at the same frequency. Specifically, this state can be achieved by arranging the first-stage scraper 11 and the second-stage scraper 12 in parallel in this order along the traveling direction of the powder layer 5, and arranging the second-stage scraper 12 in a manner that is offset by a quarter wavelength of the natural vibration relative to the first-stage scraper 11 along the width direction of the powder 3, that is, the width direction of the powder layer 5. The width direction of the powder layer 5 is a direction orthogonal to the traveling direction.

[0051] Therefore, if Figure 2 As shown in (b), the powder layer 5 can be applied with less variation in weight per unit area than in the past. As a result, a powder layer 5 with good quality can be formed.

[0052] The reason is explained. First, the powder layer 5 is applied by the first-stage scraper 11 in a manner that the surface is scraped off in the shape of a sinusoidal standing wave. Compared with the node portion of the first-stage scraper 11, where the amplitude of the sinusoidal standing wave is almost non-existent, the antinode portion vibrates greatly. Therefore, compared with the powder layer 5 corresponding to the node portion, the powder layer 5 corresponding to the antinode portion is scraped off more when passing through the gap between the first-stage scraper 11 and the sheet 4.

[0053] However, the second-stage scraper 12 scrapes off the portion of the powder layer 5 where the weight per unit area of ​​the powder is high due to the first-stage scraper 11, that is, the portion of the powder layer 5 that has passed through the node of the first-stage scraper 11 (hereinafter, also referred to as the peak portion). The scraped-off peak portion of the powder layer 5 supplements the portion where the weight per unit area of ​​the powder is low due to the first-stage scraper 11, that is, the portion of the powder layer 5 that has passed through the antinode of the first-stage scraper 11 (hereinafter, also referred to as the valley portion). Therefore, coating with a small deviation in the weight per unit area of ​​the powder layer 5 can be performed.

[0054] In addition, the amplitudes of the first-stage scraper 11 and the second-stage scraper 12 are preferably in the relationship of first-stage scraper 11 ≥ second-stage scraper 12. That is, the amplitude of the first-stage scraper 11 is greater than the amplitude of the second-stage scraper 12. This is because by making the amplitude of the second-stage scraper 12 the same as the amplitude of the first-stage scraper 11, or making the amplitude of the second-stage scraper 12 smaller than the amplitude of the first-stage scraper 11, the coating result of the first-stage scraper 11 will not be completely reset. As a result, the effects of both the first-stage scraper 11 and the second-stage scraper 12 can be used to reduce the deviation in the unit weight of the powder layer 5.

[0055] Furthermore, the amplitude of the second-stage scraper 12 is preferably one-quarter to three-quarters of the amplitude of the first-stage scraper 11. By setting the amplitude of the second-stage scraper 12 to one-quarter to three-quarters of the amplitude of the first-stage scraper 11, the second-stage scraper 12 scrapes off the peak portion of the powder layer 5 after the first-stage scraper 11, and the powder 3 scraped off from the peak portion is supplemented to the valley portion of the powder layer 5. As a result, the balance between the peak portion after scraping and the valley portion after supplementing is improved. As a result, the deviation in the unit weight of the powder layer 5 can be further reduced.

[0056] Next, the gap between the first-stage scraper 11 and the second-stage scraper 12 and the sheet 4 will be described.

[0057] like Figure 3As shown in (a), if the first gap between the first-stage scraper 11 and the sheet 4 is set to h1, and the second gap between the second-stage scraper 12 and the sheet 4 is set to h2, then the relationship of h1≤h2 is preferably satisfied. That is, the first gap between the first-stage scraper 11 and the sheet 4 is less than the second gap between the second-stage scraper 12 and the sheet 4. This is because by making the second gap of the second-stage scraper 12 the same as the first gap of the first-stage scraper 11, or making the second gap of the second-stage scraper 12 larger than the first gap of the first-stage scraper 11, the coating result of the first-stage scraper 11 will not be completely reset. As a result, the effects of both the first-stage scraper 11 and the second-stage scraper 12 can be used to reduce the deviation in the unit area weight of the powder layer 5.

[0058] Furthermore, when the amplitudes of the sinusoidal standing waves of the first-stage scraper 11 and the second-stage scraper 12 are made the same, the second gap of the second-stage scraper 12 is preferably larger than the first gap of the first-stage scraper 11 by one-quarter to three-quarters of the amplitude. By making the amplitude of the second-stage scraper 12 larger than that of the first-stage scraper 11 by one-quarter to three-quarters, the second-stage scraper 12 scrapes off the peak portion of the powder layer 5 after the first-stage scraper 11, and the powder 3 scraped off from the peak portion is supplemented to the valley portion of the powder layer 5. As a result, the balance between the peak portion after scraping and the valley portion after supplementing becomes better. As a result, the deviation of the unit weight of the powder layer 5 can be further reduced.

[0059] In addition, if Figure 2 As shown in (b), if the powder 3 with a large unit area weight of the powder layer 5 that has passed through the gaps of the first-stage scraper 11 and the gaps of the second-stage scraper 12 is scraped off and the powder 3 is replenished to the part with a small unit area weight, the deviation in the unit area weight of the powder layer 5 can be further reduced.

[0060] It should be noted that a preliminary scraper for roughly adjusting the thickness of the powder layer 5 may be provided in front of the first-stage scraper 11 (on the powder supply device side), and the gap between the scraper and the sheet may be larger in the front (on the powder supply unit side). This is because, as a stage for roughly adjusting the thickness of the powder layer 5 and adjusting the weight per unit area, the thickness of the powder layer 5 is usually reduced and the weight per unit area is reduced.

[0061] And, if Figure 4 As shown, a third-stage scraper 13 may also be provided behind the second-stage scraper 12. That is, the third-stage scraper 13 may be arranged on the side of the second-stage scraper 12 opposite to the first-stage scraper 11. In this case, the third-stage scraper 13 is arranged in a manner that is offset by one eighth of the wavelength of the natural vibration relative to the second-stage scraper 12 along the width direction of the powder 3, that is, the width direction of the powder layer 5. The third-stage scraper 13 is an example of a third scraper.

[0062] In this way, the third scraper 13 can scrape off every other portion of the powder layer 5 with a large unit weight after passing through the gaps of the first scraper 11 and the second scraper 12, thereby replenishing the portion with a small unit weight with powder 3.

[0063] Furthermore, a fourth-stage scraper 14 may be provided behind the third-stage scraper 13. That is, the fourth-stage scraper 14 may be arranged on the side of the third-stage scraper 13 opposite to the side of the second-stage scraper 12. In this case, the fourth-stage scraper 14 is arranged to be offset by one-eighth of the wavelength of the natural vibration relative to the second-stage scraper 12 in the width direction of the powder layer 5 in a manner opposite to the direction in which the third-stage scraper 13 is arranged to be offset by one-eighth of the wavelength of the natural vibration relative to the second-stage scraper 12. The fourth-stage scraper 14 is an example of a fourth scraper.

[0064] In this way, the fourth scraper 14 can scrape off all the parts with high unit weight of the powder layer 5 after passing through the gaps of the first scraper 11 and the second scraper 12, so as to further replenish the parts with low unit weight with powder 3.

[0065] Specifically, the first-stage scraper 11, the second-stage scraper 12, the third-stage scraper 13, and the fourth-stage scraper 14 having the same shape are prepared, and they are made to vibrate naturally at the same frequency, and the scrapers are arranged so as to be staggered as described above.

[0066] (Direction, size, and scraper shape of high-frequency vibrations near the ultrasonic band)

[0067] The high-frequency vibration direction of the scraper near the ultrasonic wave section includes at least one of the components in the vertical direction and the components in the horizontal direction. That is, the scraper vibrates in at least one of the vertical direction and the horizontal direction. It should be noted that the scraper mentioned here is a collective name for the first-stage scraper 11, the second-stage scraper 12, the third-stage scraper 13, and the fourth-stage scraper 14 mentioned above.

[0068] The vertical direction refers to the direction perpendicular to the main surface of the scraper (the surface of the scraper in contact with the powder). Vibration in the vertical direction easily transmits longitudinal waves (waves in the vibration direction of the scraper approaching and moving away from the powder 3) to the powder 3.

[0069] The vertical component has a greater effect on reducing the frictional resistance between the powders 3. This is because the vibration in the vertical direction is the vibration direction in which the scraper approaches and moves away from the powders 3, so the powders 3 collide with each other repeatedly, and the vibration is easily transmitted to the powders 3. Since the high frequency near the ultrasonic band is high, the vibration between the powders 3 may be difficult to transmit, but if it is a vertical vibration, the vibration is particularly easy to transmit to the powder 3.

[0070] Here, the horizontal direction refers to a direction parallel to the main surface of the scraper and parallel to the axis of the scraper. Vibration in the horizontal direction easily transmits transverse waves (waves in the direction in which the scraper vibrates due to friction with the powder 3) to the powder 3. Here, the axis of the scraper refers to an axis in a direction parallel to the width direction of the sheet 4. The axis of the scraper may also be parallel to the long side direction of the scraper.

[0071] The horizontal component of the high-frequency vibration near the ultrasonic band of the scraper not only helps to reduce the friction resistance between the powder 3, but also greatly helps to reduce the friction between the scraper and the powder 3. If the vibration component in the vertical direction is too large, it is possible that the vibration is excessively transmitted to the powder 3, so that the powder 3 vibrates greatly and the film thickness deviation becomes larger. However, the vibration component in the horizontal direction can reduce the friction between the scraper and the powder 3, so it can especially improve the fluidity of the powder 3. It should be noted that the vibration of the scraper in the horizontal direction can be achieved by installing a high-frequency transducer in the axial direction of the scraper and using a bearing to support the end of the scraper, so compared with the vibration in the surface direction, the device structure can be simplified.

[0072] The direction of the high-frequency vibration near the ultrasonic band of the scraper may be only in the vertical direction or only in the horizontal direction. However, if the high-frequency vibration near the ultrasonic band in both the vertical direction and the horizontal direction is used, the fluidity of the powder 3 can be further improved. This is because, for example, when focusing on one powder 3, the vibration direction of the powder 3 becomes random, and the vibration is applied to the entire surface of the powder 3, so there is no longer a surface that does not transmit vibration and has a high friction resistance, and the fluidity of the powder 3 is improved.

[0073] When the scraper is vibrated at a high frequency near the ultrasonic band in the vertical and horizontal directions, the magnitude of the horizontal vibration of the scraper is preferably greater than the magnitude of the vertical vibration of the scraper. That is, for the scraper, the magnitude of the vibration of the transverse wave component of the powder 3 (the direction in which the scraper vibrates frictionally with respect to the powder 3) is preferably greater than the magnitude of the vibration of the longitudinal wave component of the powder 3 (the direction in which the scraper vibrates toward and away from the powder 3). In this case, the friction resistance at the interface between the scraper and the powder 3, where the friction resistance is particularly likely to increase, can be reduced by the horizontal vibration of the scraper, and the friction resistance between the powders 3 can also be reduced. Therefore, the fluidity of the powder 3 can be further improved.

[0074] The magnitude of the vertical vibration of the scraper is preferably 2 μm or more. That is, the vertical amplitude of the scraper is preferably 2 μm or more. In this case, the frictional resistance between the powders 3 can be sufficiently reduced, thereby further improving the fluidity of the powders 3. In this case, the vertical amplitude of the scraper is preferably, for example, 20 μm or less. Thus, it is possible to suppress the excessive vibration of the powder 3, thereby preventing the powder 3 from becoming dust and scattering and contaminating the surroundings.

[0075] The magnitude of the horizontal vibration of the scraper is preferably 4 μm or more. That is, the amplitude of the horizontal vibration of the scraper is preferably 4 μm or more. In this case, the friction resistance of the interface between the scraper and the powder 3 can be sufficiently reduced, thereby further improving the fluidity of the powder 3. In this case, the amplitude of the horizontal vibration of the scraper is preferably, for example, 40 μm or less. Thus, it is possible to suppress the excessive vibration of the powder 3, thereby preventing the powder 3 from becoming dust and scattering and polluting the surroundings.

[0076] The scraper is, for example, cylindrical, and is configured in such a manner that the axial direction of the cylinder (the height direction of the cylinder) is parallel to the upper surface of the sheet 4 and crosses (for example, is orthogonal) the moving direction of the sheet 4. The cylindrical scraper is configured by fixing the two ends of the axial direction of the cylinder of the scraper with a support with a bearing in such a manner that the two ends slide in the horizontal direction. The amount of sliding in the horizontal direction can be adjusted by providing a stopper on the scraper. In addition, by setting the axis of the scraper to the shape of the diameter of the circular bearing to be inserted and adjusting the difference between the scraper diameter and the bearing diameter, the amount of vibration in the vertical direction can be adjusted. As a result, a relationship in which the amplitude in the horizontal direction is greater than the amplitude in the vertical direction can be formed.

[0077] [Method for producing powder layer]

[0078] Hereinafter, a method for producing the powder layer 5 will be described. The powder layer 5 can be produced by using the powder coating apparatus 1 .

[0079] The method for manufacturing the powder layer 5 includes the following steps: supplying powder 3 to the surface of the sheet 4 while moving the sheet 4 such as a current collector in a prescribed direction (powder supplying step); and adjusting the thickness and unit area weight of the powder 3 supplied to the surface of the sheet 4 using the first-stage scraper 11 and the second-stage scraper 12 (powder arranging step).

[0080] First, a powder 3 is prepared. The raw material of the powder 3 is not particularly limited, and for example, a particle group containing an active material can be used. The active material and the binder are mixed with a suitable additive (for example, a conductive material) to prepare the powder 3. As a mixing method, there is a method of mixing using a mortar, a ball mill, a mixer, etc. In particular, a method of mixing the powder 3 without using a solvent or the like is preferred because there is no material degradation.

[0081] In the powder supplying step, the powder 3 is supplied to the surface of the sheet 4 using a powder supplying device such as a hopper while the sheet 4 is moved in a predetermined direction. The sheet 4 may be in a shape other than a sheet, such as a plate or a block. In this case, the sheet or the block may be intermittently flowed.

[0082] The powder alignment process is a process of aligning the powder 3 on the surface of the sheet 4 using the first-stage scraper 11 and the second-stage scraper 12 of the powder coating device 1. That is, in the powder alignment process, the thickness and unit area weight of the powder 3 supplied to the surface of the sheet 4 are adjusted using the first-stage scraper 11 and the second-stage scraper 12. At this time, the first-stage scraper 11 and the second-stage scraper 12 vibrate at a frequency of 2 kHz or more and 300 kHz or less. The first-stage scraper 11 and the second-stage scraper 12 are respectively arranged in a positional relationship that is offset by a quarter wavelength of the natural vibration in the coating width direction.

[0083] The method for producing the powder layer 5 may further include a powder sheeting step. The powder sheeting step is a step of compressing the powder 3 arranged on the sheet 4 using a roller press of the powder coating device 1. Thus, a compressed powder layer 5 is formed on the surface of the sheet 4.

[0084] As described above, in the method for manufacturing the powder layer 5, by sequentially performing the powder supply step and the powder aligning step, a powder layer 5 composed of the powder 3 is formed on the surface of the sheet 4. Such a laminate of the sheet 4 and the powder layer 5 can be used for energy devices. For example, when a current collector is used as the sheet 4 and an active material is used as the powder 3, an electrode for an energy device can be manufactured.

[0085] The energy device manufactured using the powder coating apparatus 1 can be directly coated with the powder 3 with fluidity, and has a powder layer 5 with a small deviation in weight per unit area. Therefore, according to the manufacturing method of the powder layer 5, the process of directly coating the powder 3 is not used, instead of dispersing the powder 3 in a solvent or the like, coating it, and then drying it, so that the deterioration of the material caused by the solvent can be prevented, and the cost increase can be suppressed. In addition, since the weight per unit area of ​​the powder layer 5 is uniform, the quality of the electrode in the energy device can be improved, so that a good quality energy device can be manufactured at a low cost.

[0086] It should be noted that the powder layer 5 may be a compressed powder layer that has been further subjected to a roll pressing step.

[0087] [Powder layer]

[0088] The powder layer 5 of the energy device according to one embodiment of the present invention has a film thickness of 30 μm or more formed on the current collector as the sheet 4. In addition, the powder layer 5 contains powder composed of at least one particle material. In addition, the concentration of the solvent contained in the powder layer 5 is 50 ppm or less, and the weight per unit area has a small deviation.

[0089] Thus, a powder layer 5 having a small deviation in weight per unit area and suppressed deterioration due to the solvent is realized. In addition, since there is no need to dry the solvent, the energy consumption for drying the solvent can be reduced, so that the environmental burden can be suppressed and the increase in manufacturing cost can be suppressed. Therefore, by using such a powder layer 5 in energy equipment, the output and quality of the energy equipment can be improved, the environmental burden can be reduced, and the cost can be reduced.

[0090] The powder layer 5 of the present embodiment can be used in, for example, an all-solid-state battery.

[0091] The powder layer 5 will be described in detail below.

[0092] The powder layer 5 is formed on the current collector as the sheet 4. The powder layer composite is the powder layer 5 of the energy device. For example, the powder layer composite is used as an electrode of the energy device, or is used in an all-solid-state battery. It should be noted that the current collector may further include other layers located between the current collector and the powder layer 5. For example, the other layers are connection layers including conductive carbon materials, etc.

[0093] The film thickness of the powder layer 5 is 30 μm or more. The upper limit of the film thickness of the powder layer 5 is not particularly limited, but is, for example, 2000 μm or less.

[0094] In addition, the powder layer 5 includes powder 3 composed of at least one type of particle material.

[0095] The concentration of the solvent contained in the powder layer 5 is 50 ppm or less. That is, the powder layer 5 does not substantially contain the solvent. Here, substantially not containing means the case where the solvent is not contained at all and the case where the solvent is inevitably contained at 50 ppm or less as impurities. The concentration of the solvent is a concentration based on weight.

[0096] The size of the powder layer 5 in plan view is, for example, 30 mm×30 mm or more. The upper limit of the size of the powder layer 5 in plan view is not particularly limited, but is, for example, 300 mm×500 mm or less.

[0097] In an arbitrary 30 mm×30 mm region on the surface of the powder layer 5 , the weight per unit area of ​​the powder layer 5 has a variation of 8% or less.

[0098] As a method for measuring the weight per unit area, for example, the following method is used. First, the powder layer 5 and the current collector are pressed from the top and bottom to perform compression, and then the powder layer 5 and the current collector are punched into a circle with a diameter of 5 mm or more and 9 mm or less, and the total weight of the punched powder layer 5 and the current collector is measured. Then, the weight of the current collector of the same batch punched with a diameter of 5 mm or more and 9 mm or less, which is measured in advance, is subtracted from the above total weight to obtain the weight of the powder layer 5. The weight is divided by the area of ​​the circle with a diameter of 5 mm or more and a diameter of 9 mm or less, thereby obtaining the weight per unit area.

[0099] In addition, the measurement of the deviation of the unit area weight is performed, for example, by the following method. First, select any 30 mm × 30 mm area on the surface of the powder layer 5 when viewed from above. The area may be an area in the central part of the surface of the powder layer 5, or an area including the end of the powder layer 5. Then, within the range of the area, for example, five or more parts are punched out in a circular shape with a diameter of more than 5 mm and less than 9 mm, and the unit area weight is measured using the above method. From the perspective of improving the accuracy of the measurement of the deviation, nine or more parts may be punched out. The average value of the unit area weight of all punched parts and the difference (in detail, the absolute value of the difference) between the unit area weight of the part with the largest difference from the average value among the unit area weights of the punched parts are divided by the average value, thereby calculating the unit area weight deviation. That is, a unit area weight deviation of less than 8% means that the difference between the unit area weight and the average value is less than 8% of the average value at any punched part.

[0100] The powder layer 5 is formed, for example, by imparting high-frequency vibration to the powder 3 supplied to the surface of the sheet 4, thereby imparting fluidity to the powder 3 and aligning the powder 3 in the powder layer 5, which will be described in detail later. Since the weight per unit area deviation in the width direction is also small, the powder layer 5 having a size of 30 mm×30 mm or more and a thickness of 30 μm or more can be produced with high quality. Therefore, the powder layer 5 can be used for large-scale high-capacity energy devices.

[0101] In addition, the powder layer 5 is produced, for example, by a coating process that does not substantially contain a solvent. Therefore, it is possible to form a powder layer 5 that does not substantially contain a solvent. As a result, there is no damage to the powder layer 5 caused by the solvent. Therefore, since the deterioration of the powder layer 5 is suppressed and the weight per unit area of ​​the powder 3 in the powder layer 5 is less varied, it is possible to form a powder layer 5 of a large-scale, high-capacity energy device with high output and excellent quality.

[0102] In addition, the powder layer 5 can be used, for example, as a positive electrode, a negative electrode, or a solid electrolyte layer of an energy device such as an all-solid-state battery.

[0103] When the powder layer 5 is used for the positive electrode, for example, the sheet 4 is a positive electrode current collector, and the powder layer 5 containing the powder 3 is a positive electrode mixture layer. That is, the positive electrode mixture layer is formed on the positive electrode current collector. The powder 3 in the positive electrode mixture layer contains a positive electrode active material and a solid electrolyte having ion conductivity as at least one particle material.

[0104] When the powder layer 5 is used for the negative electrode, for example, the sheet 4 is a negative electrode current collector, and the powder layer 5 containing the powder 3 is a negative electrode mixture layer. That is, the negative electrode mixture layer is formed on the negative electrode current collector. The powder 3 in the negative electrode mixture layer contains a negative electrode active material and a solid electrolyte having ion conductivity as at least one particle material.

[0105] When the powder layer 5 is used as a solid electrolyte layer, for example, the powder layer 5 including the powder 3 is a solid electrolyte layer. The solid electrolyte layer is formed on the surface of the powder layer 5 in the positive electrode or the surface of the powder layer 5 in the negative electrode. The powder 3 in the solid electrolyte layer contains a solid electrolyte having ion conductivity as at least one particle material.

[0106] The concentration of the solvent contained in the positive electrode mixture layer, the negative electrode mixture layer and the solid electrolyte layer is 50 ppm or less. That is, the positive electrode mixture layer, the negative electrode mixture layer and the solid electrolyte layer do not substantially contain a solvent. Here, substantially not containing a solvent means that these layers do not contain a solvent at all and that these layers inevitably contain a solvent of 50 ppm or less as an impurity.

[0107] It should be noted that the solvent refers to, for example, an organic solvent. In addition, the determination method of the solvent is not particularly limited, and for example, it can be determined using gas chromatography and mass change method. As the organic solvent, for example, non-polar organic solvents such as heptane, xylene and toluene, tertiary amine solvents, ether solvents, polar organic solvents such as thiol solvents and ester solvents, and combinations thereof are included. Examples of tertiary amine solvents include triethylamine, tributylamine and tripentylamine. Examples of ether solvents include tetrahydrofuran and cyclopentyl methyl ether. Examples of thiol solvents include ethyl mercaptan. Examples of ester solvents include butyl butyrate, ethyl acetate and butyl acetate.

[0108] Next, the materials used in the positive electrode mixture layer, the negative electrode mixture layer, and the solid electrolyte layer will be described in detail.

[0109] The positive electrode active material is a material in which metal ions such as lithium (Li) are inserted or removed from the crystal structure at a higher potential than the negative electrode and oxidized or reduced along with the insertion or removal of metal ions such as lithium. The type of positive electrode active material is appropriately selected according to the type of all-solid-state battery, and examples thereof include oxide active materials, sulfide active materials, etc.

[0110] The positive electrode active material in this embodiment uses, for example, an oxide active material (lithium-containing transition metal oxide). Examples of the oxide active material include LiCoO2, LiNiO2, LiMn2O4, LiCoPO4, LiNiPO4, LiFePO4, LiMnPO4, and compounds obtained by replacing the transition metals of these compounds with one or two different elements. As compounds obtained by replacing the transition metals of the above compounds with one or two different elements, LiNi can be used. 1 / 3 Co 1 / 3 Mn 1 / 3 O2、LiNi 0.8 Co 0.15 Al 0.05 O2、LiNi 0.5 Mn 1.5 O2 and other known materials. The positive electrode active material may be used alone or in combination of two or more.

[0111] As the shape of the positive electrode active material, for example, a particle shape and a thin film shape can be listed. When the positive electrode active material is in a particle shape, the particle size of the positive electrode active material is, for example, in the range of 50 nm or more and 30 μm or less, or in the range of 1 μm or more and 15 μm or less. If the particle size of the positive electrode active material is set to be greater than 50 nm, the handling property is improved. On the other hand, if the particle size is set to be less than 30 μm, the surface area becomes larger by using an active material with a small particle size, and a high-capacity positive electrode is easily obtained. It should be noted that the particle size of the material contained in the positive electrode mixture layer or the negative electrode mixture layer in this specification is, for example, the above-mentioned average particle size (D50).

[0112] The content of the positive electrode active material in the positive electrode mixture layer is not particularly limited, and may be, for example, in the range of 40% by weight or more and 99% by weight or less, or 70% by weight or more and 95% by weight or less.

[0113] The surface of the positive electrode active material may also be covered with a coating. This is because the reaction between the positive electrode active material (e.g., an oxide active material) and the solid electrolyte (e.g., a sulfide-based solid electrolyte) can be suppressed. Examples of materials for the coating include LiNbO3, Li3PO4, LiPON and other Li ion conductive oxides. The average thickness of the coating is, for example, in the range of 1 nm to 20 nm, or in the range of 1 nm to 10 nm.

[0114] When the ratio of the positive electrode active material and the solid electrolyte contained in the positive electrode mixture layer is set to positive electrode active material / solid electrolyte=weight ratio in terms of weight conversion, the weight ratio may be in the range of 1 to 19 or in the range of 2.3 to 19. By being within the range of this weight ratio, it is easy to ensure both the lithium ion conduction path and the electron conduction path in the positive electrode mixture layer.

[0115] The negative electrode active material is a material in which metal ions such as lithium are inserted into or removed from the crystal structure at a lower potential than that of the positive electrode, and is oxidized or reduced accompanying the insertion or removal of metal ions such as lithium.

[0116] As the negative electrode active material in this embodiment, for example, metals that are easily alloyed with lithium, such as lithium, indium, tin, and silicon, carbon materials such as hard carbon and graphite, and Li4Ti5O 12 、SiO x As the negative electrode active material, a composite obtained by appropriately mixing the above-mentioned negative electrode active materials can also be used.

[0117] The particle size of the negative electrode active material is, for example, 30 μm or less. By using an active material with a small particle size, the surface area becomes large, and a high capacity can be achieved.

[0118] When the ratio of the negative electrode active material and the solid electrolyte contained in the negative electrode mixture layer is set to negative electrode active material / solid electrolyte=weight ratio in terms of weight conversion, for example, the weight ratio is in the range of 0.6 to 19, or in the range of 1 to 5.7. Within this weight ratio range, it is easy to ensure both the lithium ion conduction path and the electron conduction path in the negative electrode mixture layer.

[0119] The solid electrolyte may be appropriately selected according to the type of conductive ions (eg, lithium ions), and can be roughly divided into, for example, sulfide-based solid electrolytes, oxide-based solid electrolytes, and halide-based solid electrolytes.

[0120] The type of sulfide-based solid electrolyte in the present embodiment is not particularly limited. As sulfide-based solid electrolytes, for example, Li2S-SiS2, LiI-Li2S-SiS2, LiI-Li2S-P2S5, LiI-Li2S-P2O5, LiI-Li3PO4-P2S5 and Li2S-P2S5 can be listed. In particular, from the perspective of excellent lithium ion conductivity, the sulfide-based solid electrolyte can contain Li, P and S. One sulfide-based solid electrolyte can be used, or two or more can be used in combination. In addition, the sulfide-based solid electrolyte can be crystalline, amorphous, or glass ceramic. It should be noted that the above-mentioned "Li2S-P2S5" record indicates a sulfide-based solid electrolyte composed of raw materials containing Li2S and P2S5, and the same is true for other records.

[0121] In the present embodiment, one scheme of the sulfide-based solid electrolyte is a sulfide glass ceramic containing Li2S and P2S5, and when the ratio of Li2S and P2S5 is set to Li2S / P2S5=molar ratio in terms of molar conversion, for example, the molar ratio is in the range of 2.3 to 4, or in the range of 3 to 4. By being within the range of this molar ratio, it is possible to set a crystal structure with high ion conductivity while maintaining the lithium concentration that affects the battery characteristics.

[0122] As the shape of the sulfide-based solid electrolyte in this embodiment, for example, a particle shape such as a true sphere and an ellipsoidal sphere, a thin film shape, etc. can be listed. When the sulfide-based solid electrolyte material is in a particle shape, the particle size of the sulfide-based solid electrolyte is not particularly limited, but in order to easily increase the filling rate in the positive electrode or the negative electrode, it can be 30 μm or less, or 20 μm or less, or 10 μm or less. On the other hand, the particle size of the sulfide-based solid electrolyte can be 0.001 μm or more, or 0.01 μm or more.

[0123] Next, the oxide-based solid electrolyte in this embodiment is described. The type of oxide-based solid electrolyte is not particularly limited, and examples thereof include LiPON, Li3PO4, Li2SiO2, Li2SiO4, Li 0.5 La 0.5 TiO3、Li 1.3 Al 0.3 Ti 0.7 (PO4)3, La 0.51 Li 0.34 TiO 0.74 , Li 1.5 Al 0.5 Ge 1.5(PO4)3, etc. The oxide-based solid electrolyte may be used alone or in combination of two or more.

[0124] Next, the positive electrode current collector and the negative electrode current collector are described in detail.

[0125] The positive electrode in this embodiment has a positive electrode collector composed of, for example, metal foil, etc. The positive electrode collector may be, for example, a foil, plate, mesh, etc. composed of aluminum, gold, platinum, zinc, copper, SUS, nickel, tin, titanium, or an alloy of two or more thereof.

[0126] The thickness and shape of the positive electrode current collector can be appropriately selected according to the application of the positive electrode.

[0127] The negative electrode in this embodiment has a negative electrode current collector composed of, for example, metal foil, etc. The negative electrode current collector may be, for example, a foil, plate, mesh, etc. composed of SUS, gold, platinum, zinc, copper, nickel, titanium, tin, or an alloy of two or more thereof.

[0128] The thickness and shape of the negative electrode current collector can be appropriately selected according to the application of the negative electrode.

[0129] It should be noted that the powder layer 5 may also be a compressed powder layer formed by compressing the powder layer 5 .

[0130] (Example)

[0131] Hereinafter, the present invention will be specifically described by the following examples. It should be noted that the present invention is not limited to the following examples.

[0132] In Examples 1 and 2 and Comparative Example 1, the shape of the scraper was set to a cylindrical shape, and simulation was performed at a vibration frequency of 2.5 kHz to analyze the deviation in the weight per unit area of ​​the powder layer 5 after the scraper passed.

[0133] The results are shown in Table 1 below.

[0134] In Example 1, the second scraper 12 is arranged on the traveling direction side relative to the first scraper 11 , and the first scraper 11 and the second scraper 12 are arranged to be offset by a quarter wavelength of the natural vibration in the powder layer width direction.

[0135] In the second embodiment, in addition to the structure of the first embodiment, the second-stage scraper 12 is further vibrated so that the amplitude of the second-stage scraper 12 becomes half of the amplitude of the first-stage scraper 11 .

[0136] Comparative Example 1 used only the first-stage scraper 11. Here, the weight per unit area deviation in Table 1 is obtained by standardizing the value of the standard deviation of the weight per unit area distribution in the width direction of the powder layer to the value of Comparative Example 1. In addition, the amplitude is standardized to the amplitude of the first-stage scraper 11 as 1.

[0137] In Example 1, by adopting a structure in which the second-stage scraper 12 is arranged to be offset by a quarter of the wavelength of the natural vibration relative to the first-stage scraper 11, stable coating with less deviation in weight per unit area can be achieved. In addition, in Example 2, by setting the amplitude of the second-stage scraper 12 to half of that of the first-stage scraper 11, stable coating with less deviation in weight per unit area can be achieved.

[0138]

Table 1

[0139]

[0140] (Other variations)

[0141] As mentioned above, although the powder coating apparatus according to the present invention has been described based on the embodiment, the present invention is not limited to the above-mentioned embodiment.

[0142] In addition, various modifications that can be conceived by those skilled in the art to the above-described embodiments and embodiments achieved by arbitrarily combining the components and functions in the above-described embodiments without departing from the gist of the present disclosure are also included in the present invention.

[0143] According to the powder coating apparatus of the present invention, it is possible to form a powder layer with high performance and low environmental impact, in which the variation in weight per unit area caused by the surface of the powder layer being cut into a sinusoidal standing wave-shaped concavo-convex structure is reduced.

[0144] Industrial Applicability

[0145] The powder coating apparatus of the present invention forms a uniform powder layer with little variation in film thickness without using a solvent, and therefore can also be used for applications such as a mixture layer of a high-quality all-solid-state battery.

[0146] Description of Reference Numerals

[0147] 1: powder coating device, 3: powder, 4: sheet, 5: powder layer, h1: gap between the first-stage scraper and the sheet, h2: gap between the second-stage scraper and the sheet, 11: first-stage scraper (first scraper), 12: second-stage scraper (second scraper), 13: third-stage scraper (third scraper), 14: fourth-stage scraper (fourth scraper).

Claims

1. A powder coating device, comprising: A drive device that moves the member in a specified direction; a powder supply device for supplying powder to the surface of the member; and The first scraper and the second scraper are arranged to form a gap with the member, and adjust the thickness of the powder supplied to the surface of the member by the powder supply device. The first scraper and the second scraper perform natural vibration at a frequency of 2 kHz or more and 300 kHz or less. The first scraper is located closer to the supply side of the powder than the second scraper. The second scraper is offset from the first scraper by a quarter wavelength of the natural vibration in the width direction of the powder supplied to the surface of the member.

2. The powder coating device according to claim 1, wherein: The vibration amplitude of the first scraper is greater than the vibration amplitude of the second scraper.

3. The powder coating device according to claim 1 or 2, wherein: The distance between the second scraper and the member is equal to or greater than the distance between the first scraper and the member.

4. The powder coating device according to any one of claims 1 to 3, wherein: The powder coating device further includes a third scraper disposed on a side of the second scraper opposite to the first scraper side. The third scraper is disposed so as to be offset from the second scraper by one eighth of the wavelength of the natural vibration in the width direction of the powder supplied to the surface of the member.

5. The powder coating device according to claim 4, wherein: The powder coating device further includes a fourth scraper disposed on a side of the third scraper opposite to the second scraper side. The fourth scraper is arranged in a direction opposite to the direction in which the third scraper is arranged relative to the second scraper by an amount one-eighth of the wavelength of the natural vibration, and is arranged relative to the second scraper along the width direction of the powder supplied to the surface of the component by an amount one-eighth of the wavelength of the natural vibration.

6. The powder coating device according to any one of claims 1 to 5, wherein: The average particle size (D50) of the powder is 0.005 μm or more and 30 μm or less.