Preparation method of high-purity ethylene sulfate
By using a topological titanium-silicon molecular sieve catalyst and a vacuum sublimation purification process, the problems of catalyst activity loss and purity improvement in the synthesis of vinyl sulfate are solved, efficient and low-cost vinyl sulfate preparation is achieved, and environmental pollution is reduced.
Patent Information
- Application Number
- CN202310346782.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2023-04-03
- Publication Date
- 2024-10-15
- Estimated Expiration
- 2043-04-03
AI Technical Summary
The existing vinyl sulfate synthesis method has problems such as high cost of precious metal catalysts, rapid loss of catalyst activity, difficulty in improving product purity, and environmental pollution and high costs caused by solvent methods.
A catalyst composed of topologically structured titanium-silicon molecular sieves, binders, carriers and titanium-containing additives is used to improve the activity and purity of the catalyst through roasting and modification with alkaline compounds, combined with a vacuum sublimation purification process.
The catalyst activity and the conversion rate of vinyl sulfate are improved, the production cost is reduced, the operation is simplified, the yield and purity of the product are improved, and the bottleneck problem of purity improvement in the existing technology is solved.
Smart Images

Figure CN118767983A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the field of synthesis and purification of vinyl sulfate, and in particular to a method for preparing high-purity vinyl sulfate. Background Art
[0002] Dithiothreitol (DTD) is the most comprehensive additive among the sulfur-containing additives in lithium battery electrolytes. However, the conventional synthesis method has the following problems: 1. The use of precious metal catalyst ruthenium trichloride is costly and produces many by-products; 2. Titanium silicon molecular sieve powder is used for production. The molecular sieve powder is too fine, which leads to high requirements for filtering and separation equipment, and the catalyst activity is lost quickly, making it difficult to maintain the catalytic effect; 3. In the existing synthesis route, the yield of the product is generally around 80-90%, and the purity is around 99.5%, which is difficult to further improve.
[0003] Patent CN202210580354.2 proposes to use 90-120°C dry hot gas to sublimate and purify vinyl sulfate, but vinyl sulfate has poor thermal stability and begins to decompose and discolor above 80°C, producing easily sublimable impurities, which has a great impact on sublimation purification.
[0004] The existing purification process is mainly the solvent method, but the solvent method purification has the following problems: high cost, environmental pollution, difficulty in recovering organic solvents, complex operation (often requiring repeated operations), and residual organic solvents will lead to low product purity, which in turn affects its performance as a lithium battery electrolyte additive added to lithium batteries. Summary of the invention
[0005] In order to improve the above technical problems, the present invention provides a catalyst, wherein the catalyst components include: a titanium silicon molecular sieve having a topological structure, a binder, a carrier, a titanium-containing auxiliary agent, a basic compound and water;
[0006] The mass ratio of the titanium silicon molecular sieve with topological structure, the solid component in the binder, the carrier, and the titanium-containing auxiliary agent is 100:(1-1000):(1-4000):(0.5-1000);
[0007] The molar mass ratio of the alkaline compound, the titanium silicon molecular sieve with a topological structure and water is (0.01-100) (mol): 100 (g): (10-3000) (g).
[0008] According to an embodiment of the present invention, the titanium silicon molecular sieve with a topological structure is one or more of a titanium silicon molecular sieve with an MFI structure (such as TS-1), a titanium silicon molecular sieve with a MEL structure (such as TS-2), a titanium silicon molecular sieve with a BEA structure (such as Ti-Beta), a titanium silicon molecular sieve with an MWW structure (such as Ti-MCM-22), a titanium silicon molecular sieve with a hexagonal structure (such as Ti-MCM-41, Ti-SBA-15), a titanium silicon molecular sieve with a MOR structure (such as Ti-MOR), a titanium silicon molecular sieve with a TUN structure (such as Ti-TUN) and a titanium silicon molecular sieve with other structures (such as Ti-ZSM-48); preferably, the titanium silicon molecular sieve with a topological structure is in powder form.
[0009] According to an embodiment of the present invention, the binder is one or more of silica sol, pseudo-boehmite, etc. The mass concentration of silicon dioxide in the silica sol is 1 to 80%, exemplarily 1%, 5%, 10%, 20%, 30%, 40%, 50%, 60%, 70%, 80%.
[0010] According to an embodiment of the present invention, the carrier is one or a mixture of silicon dioxide, silicon carbide, SBA-15, activated alumina, glass fiber, ceramic, layered graphite, quartz glass, natural clay, expanded perlite, activated carbon.
[0011] According to an embodiment of the present invention, the titanium-containing additive is titanium tetrachloride, titanium trichloride, titanium sulfate, titanium hydroxide, titanium oxychloride, organic titanate R4TiO4, wherein R is the same or different, and is independently selected from an alkyl group of 2 to 4 carbon atoms, titanium dioxide, or a mixture of one or more thereof. Preferably, the organic titanate is selected from tetrabutyl titanate, tetrapropyl titanate, and methyl triethyl titanate. The titanium-containing additive is preferably one or more of titanium tetrachloride, titanium hydroxide, and tetrabutyl titanate.
[0012] According to an embodiment of the present invention, the shape of the catalyst is one or more of a spherical shape, an elongated strip shape, a clover shape, an irregular shape, etc.
[0013] According to an embodiment of the present invention, the equivalent particle size of the catalyst is 0.1 mm to 30 mm, preferably 2 mm to 10 mm, further preferably 2 mm to 5 mm, and more preferably 2 mm to 3 mm.
[0014] According to an embodiment of the present invention, the alkaline compound is one or more of an organic quaternary ammonium base, aliphatic alcohol amines (triethanolamine, ethanolamine, etc.), aliphatic amines (hexamethylenediamine, butanediamine, etc.), an inorganic alkaline substance (ammonia water, sodium hydroxide, sodium carbonate, etc.), etc.
[0015] Furthermore, the organic quaternary ammonium base is R a4NOH, where R a The alkyl groups may be the same or different and independently selected from alkyl groups having 1 to 5 carbon atoms, or may be a mixture of a quaternary ammonium salt and a strong base (eg, tetramethylammonium chloride and sodium hydroxide, tetrapropylammonium bromide and tetramethylammonium hydroxide, tetrapropylammonium bromide and aqueous ammonia).
[0016] According to an embodiment of the present invention, the mass ratio of the titanium silicon molecular sieve with a topological structure, the solid component in the binder, the carrier, and the titanium-containing auxiliary agent is 100: (10-400): (1-400): (0.5-100).
[0017] According to an embodiment of the present invention, the molar mass ratio of the basic compound, the titanium silicalite having a topological structure and water is (0.1-10) (mol): 100 (g): (50-1000) (g).
[0018] The present invention also provides a method for preparing the above catalyst, the method comprising:
[0019] The catalyst is prepared by mixing a titanium silicon molecular sieve with a topological structure, a binder, a carrier and a titanium-containing auxiliary agent, calcining the mixture, and then subjecting the mixture to modification treatment with an alkaline compound aqueous solution.
[0020] According to an embodiment of the present invention, the aqueous solution of the alkaline compound is an alkaline compound dissolved in water.
[0021] According to an embodiment of the present invention, the equivalent particle size of the mixture is 0.1 mm to 30 mm, preferably 2 mm to 10 mm, further preferably 2 mm to 5 mm, and more preferably 2 mm to 3 mm.
[0022] According to an embodiment of the present invention, the calcination temperature is 400-900°C, exemplarily 400°C, 500°C, 550°C, 600°C, 700°C, 800°C, 850°C or 900°C, and the calcination time is 2-24h, exemplarily 2h, 5h, 6h, 10h, 12h, 16h, 18h, 20h, 24h.
[0023] According to an embodiment of the present invention, the modification treatment condition is: the calcined product is crystallized at 140-240°C for 2-120 hours. For example, it is placed in a stainless steel crystallization kettle with a polytetrafluoroethylene lining for crystallization treatment; illustratively, the crystallization treatment temperature is 140°C, 150°C, 160°C, 170°C, 180°C, 190°C, 200°C, 210°C, 220°C, 230°C, 240°C. The crystallization treatment time is 2h, 5h, 10h, 30h, 40h, 60h, 80h, 100h, 120h.
[0024] According to an embodiment of the present invention, after the modification, the product can be washed with water until it is neutral and / or dried. Preferably, the drying temperature is 60 to 700° C. In the present invention, the water content is not particularly limited, as long as the product is neutral.
[0025] As an exemplary embodiment of the present invention, the preparation method of the catalyst specifically includes:
[0026] A titanium silicon molecular sieve with a topological structure, a binder, a carrier and a titanium-containing auxiliary agent are mixed to prepare a large solid particle, which is then roasted, modified with an alkaline compound aqueous solution, washed with water to neutrality and dried to prepare a catalyst.
[0027] The present invention also provides an application of the catalyst in the preparation of vinyl sulfate.
[0028] The present invention also provides a method for preparing vinyl sulfate, the method comprising:
[0029] The vinyl sulfite, the oxidant and the above catalyst are mixed and reacted, and the prepared intermediate product is sublimated and condensed and crystallized to obtain the vinyl sulfate.
[0030] According to an embodiment of the present invention, the molar mass ratio of the vinyl sulfite, the oxidant and the catalyst is 1 mol:(0.1-20) mol:(0.1-5000) g, preferably 1 mol:(0.5-10) mol:(1-500) g; and also preferably 1 mol:(0.8-2) mol:(10-200) g.
[0031] According to an embodiment of the present invention, the reaction is carried out in a solvent; the solvent is one or more of water, halogenated alkanes (dichloromethane, dichloroethane, chloroform, dibromomethane, dibromoethane, etc.), ester solvents (ethyl acetate, butyl acetate, dimethyl carbonate, diethyl carbonate, ethyl methyl carbonate, ethylene carbonate, propylene carbonate, etc.), benzene solvents (toluene, ethylbenzene, xylene, nitrobenzene, etc.), ether solvents (ethyl ether, propyl ether, isopropyl ether, etc.), alcohols (methanol, ethanol, propanol, isopropanol, butanol, pentanol, propylene glycol, etc.), ketones (butanone, acetone, etc.), nitrile solvents (acetonitrile, propionitrile, etc.), acids (formic acid, acetic acid, etc.), tetrahydrofuran, pyridine, DMF, DMSO, alkanes (cyclohexane, n-hexane, n-pentane, n-octane, isooctane, n-nonane, isononane, etc.).
[0032] According to an embodiment of the present invention, the molar ratio of the vinyl sulfite to the solvent is 1:(0.1-20); preferably 1:(5-16).
[0033] According to an embodiment of the present invention, the oxidant is one or more of aqueous hydrogen peroxide solution (mass concentration of hydrogen peroxide ≥1%, for example, 1wt%-50wt%), tert-butyl hydroperoxide, urea peroxide, potassium persulfate, ammonium persulfate, cumene hydroperoxide, ethylbenzene hydroperoxide, cyclohexyl hydroperoxide, peracetic acid, peroxypropionic acid, benzoyl peroxide, potassium permanganate, hypochlorite, percarbonate, and dichromate.
[0034] According to an embodiment of the present invention, the reaction temperature is -10°C to 50°C, illustratively -10°C, 0°C, 10°C, 20°C, 30°C, 40°C, 50°C.
[0035] According to an embodiment of the present invention, the reaction time is 10 to 500 min, preferably 30 to 120 min, illustratively 30 min, 60 min, 80 min, 100 min, 120 min.
[0036] According to an embodiment of the present invention, vinyl sulfite, a solvent, and an oxidant are mixed and continuously fed into a reactor loaded with a catalyst for reaction. The reactor is at least one of a tubular reactor, a fixed bed reactor, a fluidized bed reactor, etc., and the reaction device used can limit the activity of the catalyst within a certain range.
[0037] According to an embodiment of the present invention, the reaction pressure (gauge pressure) is -0.02 MPa to 1 MPa, exemplarily -0.02 MPa, -0.01 MPa, 0, 0.01 MPa, 0.05 MPa, 0.2 MPa, 0.5 MPa, 1 MPa.
[0038] According to an embodiment of the present invention, before the intermediate product is sublimated, the solvent in the intermediate product can be removed. Preferably, the pressure (gauge pressure) of the solvent removal is -0.1 MPa to 0.5 MPa. Exemplarily, -0.1 MPa, -0.09 MPa, -0.05 MPa, 0, 0.2 MPa, 0.4 MPa, 0.5 MPa.
[0039] Preferably, the temperature for removing the solvent is 0 to 150° C., illustratively 0° C., 10° C., 20° C., 30° C., 40° C., 50° C., 60° C., 80° C., 100° C., 120° C., 140° C., 150° C.
[0040] Preferably, when removing the solvent, the solvent layer with the highest mass content of vinyl sulfate is subjected to solvent removal treatment; wherein the solvent layer with the highest mass content of vinyl sulfate refers to the solvent layer which needs to be separated first and then the mass contents are measured respectively according to the mass contents and the total mass of the solution, and then the solvent layer with the highest mass of vinyl sulfate is subjected to subsequent desolventizing treatment.
[0041] According to an embodiment of the present invention, the sublimation temperature is 0 to 80°C, exemplarily 0°C, 10°C, 20°C, 30°C, 40°C, 50°C, 60°C, 80°C.
[0042] According to an embodiment of the present invention, the sublimation pressure (gauge pressure) is -0.1 MPa to 0.01 MPa, exemplarily -0.1 MPa, -0.08 MPa, -0.06 MPa, 0, 0.02 MPa, 0.05 MPa, 0.08 MPa, 0.1 MPa.
[0043] According to an embodiment of the present invention, the temperature of the desublimation crystallization is -20°C to 50°C, exemplarily -20°C, -10°C, 0°C, 5°C, 7°C, 10°C, 20°C, 30°C, 40°C, 50°C.
[0044] According to an embodiment of the present invention, the sublimation step is carried out in a sublimator, and the sublimator is one or more of a flash sublimator, a stirring sublimator, a rotary drum sublimator, an air flow sublimator, a fluidized bed sublimator, a box sublimator, a spray sublimator and a belt sublimator.
[0045] As an exemplary embodiment of the present invention, the method for preparing vinyl sulfate specifically comprises:
[0046] After vinyl sulfite, solvent and oxidant are mixed and fully dispersed, they are continuously fed into a catalyst-loaded device for reaction; after the reaction is completed, the solvent layer containing the most vinyl sulfate is subjected to solvent removal treatment to obtain a solid crude product, and the solid crude product is added to a vacuum sublimator for sublimation and condensation crystallization to obtain pure vinyl sulfate.
[0047] Beneficial effects of the present invention:
[0048] 1. The present invention adopts titanium-containing additives to increase titanium sources, further improve catalyst activity, and improve vinyl sulfate conversion rate; 2. The present invention adopts carriers to better load the catalyst to improve catalyst strength and heat transfer performance, improve its service life, and reduce catalyst cost; 3. The present invention directly saves filtering operation by making it into large-particle solid, making the operation simpler and reducing production cost; 4. The present invention adopts alkaline compounds for modification treatment to expose more active sites, and also promotes further generation of active components on the catalyst surface, thereby enhancing catalytic activity; 5. The present invention adopts reduced pressure sublimation for purification, reduces product decomposition, solvent use and residues in the product, and improves product yield and purity; 6. The method of the present invention can better exert the properties of each component, achieve synergistic effect, improve catalytic ability, and is particularly suitable for the preparation of DTD products, solves the bottleneck problem that the yield and purity cannot be improved in DTD production, and reduces production cost. BRIEF DESCRIPTION OF THE DRAWINGS
[0049] Figure 1 is the NMR image of vinyl sulfate in Example 1;
[0050] Figure 2 This is a gas chromatographic detection chart of vinyl sulfate in Example 1. DETAILED DESCRIPTION
[0051] The technical scheme of the present invention will be further described in detail below in conjunction with specific embodiments. It should be understood that the following embodiments are only exemplary descriptions and explanations of the present invention and should not be construed as limiting the scope of protection of the present invention. All technologies implemented based on the above content of the present invention are included in the scope that the present invention is intended to protect.
[0052] Unless otherwise specified, the raw materials and reagents used in the following examples are commercially available or can be prepared by known methods.
[0053] Example 1
[0054] (i) 20 g of silicon carbide, 80 g of 30% (mass concentration of silica) silica sol, 20 g of tetrabutyl titanate, and 120 g of TS-1 powder were fully mixed, and then extruded into strip catalysts with a diameter of about 2-3 mm using an extruder, calcined at 550° C. for 6 hours, naturally cooled to room temperature, and then mixed with 0.15 mol of tetrapropylammonium hydroxide and 200 g of deionized water and placed in a stainless steel crystallization kettle lined with polytetrafluoroethylene, crystallized at 170° C. for 10 hours, taken out and washed with deionized water until neutral, and then placed in an oven to dry at 80° C. for 6 hours, and then dried at 600° C. for 6 hours to prepare a catalyst, which was loaded into a fixed bed reactor with a jacket.
[0055] (ii) 200 g of vinyl sulfite, 230 g of 30% hydrogen peroxide solution and 1000 g of ethylene dichloride solution were mixed at a mixing temperature of 20° C. After being uniformly dispersed, the mixture was fed into a fixed bed reactor. The temperature of the jacket coolant in the fixed bed was maintained at 20° C. The continuous feeding time was 60 min and the reaction pressure was 0.01 MPa. After all the materials had passed through the catalyst, they were layered and the lower layer of ethylene dichloride phase was removed under heating conditions of -0.09 MPa and 20° C. to remove the solvent to obtain a white powdery crude product. The obtained powder was then placed in a stirred sublimator at a heating temperature of 30° C. and a pressure of -0.1 MPa for sublimation. The desublimation temperature was 5° C. to obtain 223 g of a white product (molar yield of 97.0%, the molar yield being the molar amount of the final product vinyl sulfate divided by the theoretical molar amount calculated based on the complete reaction of vinyl sulfite) with a purity of 99.95%.
[0056] Figure 1is the NMR of vinyl sulfate in Example 1; Figure 1 It can be seen that: 1 H-NMR,δ4.766(s,4H)×10 -6 This is consistent with the chemical shift 1H-NMR: δ4.76 (s, 4H)×10-6 of the H NMR spectrum of DTD in the literature.
[0057] Figure 2 This is a gas chromatographic detection chart of vinyl sulfate in Example 1. Figure 2 These are the gas chromatography test data after the DTD product was dissolved in dimethyl carbonate, a solvent. After deducting the solvent peak, only two substances remain - vinyl sulfite and vinyl sulfate. The peak area is used to represent the content.
[0058] Comparative Example 1
[0059] (i) 20 g of silicon carbide, 80 g of 30% (mass concentration of silicon dioxide) silica sol, 20 g of tetrabutyl titanate, and 120 g of TS-1 powder were fully mixed, and then extruded into strip catalysts with a diameter of about 2-3 mm using an extruder, calcined at 550° C. for 6 hours, and naturally cooled to room temperature to prepare the catalyst, which was loaded into a fixed bed reactor with a jacket.
[0060] (ii) 200 g of vinyl sulfite, 230 g of 30% hydrogen peroxide solution and 1000 g of dichloroethane solution were mixed at a mixing temperature of 20° C. After being uniformly dispersed, the mixture was fed into a fixed bed reactor. The temperature of the jacket coolant in the fixed bed was maintained at 20° C. The continuous feeding time was 60 min and the reaction pressure was 0.01 MPa. After all the materials had passed through the catalyst, they were layered and the lower dichloroethane phase was removed under heating conditions of -0.09 MPa and 20° C. to remove the solvent to obtain a white powdery crude product. The obtained powder was then placed in a stirred sublimator at a heating temperature of 30° C. and a pressure of -0.1 MPa for sublimation. The sublimation temperature was 5° C. to obtain 212 g of a white product (molar yield 92.1%) with a purity of 99.71%.
[0061] Comparative Example 2
[0062] (i) 20 g of silicon carbide, 80 g of 30% (mass concentration of silica) silica sol, 20 g of tetrabutyl titanate, and 120 g of TS-1 powder were fully mixed, and then extruded into strip catalysts with a diameter of about 2-3 mm using an extruder, calcined at 550° C. for 6 hours, naturally cooled to room temperature, and then mixed with 0.15 mol of tetrapropylammonium hydroxide and 200 g of deionized water and placed in a stainless steel crystallization kettle lined with polytetrafluoroethylene, crystallized at 170° C. for 10 hours, taken out and washed with deionized water until neutral, and then placed in an oven to dry at 80° C. for 6 hours, and then dried at 600° C. for 6 hours to prepare a catalyst, which was loaded into a fixed bed reactor with a jacket.
[0063] (ii) 200 g of vinyl sulfite, 230 g of 30% hydrogen peroxide solution and 1000 g of ethylene dichloride solution were mixed at a mixing temperature of 20° C. After being uniformly dispersed, the mixture was fed into a fixed bed reactor. The temperature of the jacket coolant in the fixed bed was maintained at 20° C. The continuous feeding time was 60 min. The reaction pressure was 0.01 MPa. After all the materials had passed through the catalyst, they were layered. The lower layer of ethylene dichloride phase was removed under heating conditions of -0.09 MPa and 20° C. to remove the solvent to obtain a powdery solid. The powdery solid was then placed in a glass jacket reactor and heated to 110° C. to melt it into a liquid state. Then, a heat preservation pump was used to heat the mixture. It is sent to a spray sublimator to be atomized into small droplets, which are mixed with dry carbon dioxide at a temperature of 120°C in the atomizer and then flow downstream. Vinyl sulfate is heated and sublimated to obtain a mixed sublimation gas containing vinyl sulfate, which is then purified. The purified mixed sublimation gas enters a three-stage rotary drum scraper desublimation crystallizer, and cooling circulating water is introduced into the drum jacket to cool it to 30°C. Vinyl sulfate desublimates and crystallizes on the surface of the drum. When the drum rotates and passes through the scraper, it is scraped off and collected to obtain 214g of white fine needle-like product (molar yield 93.0%) with a purity of 99.51%.
[0064] Comparative Example 3
[0065] (i) 20 g of silicon carbide, 80 g of 30% (mass concentration of silicon dioxide) silica sol, and 120 g of TS-1 powder were fully mixed, and then extruded into strip catalysts with a diameter of about 2-3 mm using an extruder, calcined at 550° C. for 6 hours, naturally cooled to room temperature, and then mixed with 0.15 mol of tetrapropylammonium hydroxide and 200 g of deionized water and placed in a stainless steel crystallization kettle lined with polytetrafluoroethylene, crystallized at 170° C. for 10 hours, taken out and washed with deionized water until neutral, and then placed in an oven to dry at 80° C. for 6 hours, and then dried at 600° C. for 6 hours to prepare the catalyst, which was loaded into a fixed bed reactor with a jacket.
[0066] (ii) 200 g of vinyl sulfite, 230 g of 30% hydrogen peroxide solution and 1000 g of dichloroethane solution were mixed at a mixing temperature of 20° C. After being uniformly dispersed, the mixture was fed into a fixed bed reactor. The temperature of the jacket coolant in the fixed bed was maintained at 20° C. The continuous feeding time was 60 min and the reaction pressure was 0.01 MPa. After all the materials had passed through the catalyst, they were layered and the lower dichloroethane phase was removed under heating conditions of -0.09 MPa and 20° C. to remove the solvent to obtain a white powdery crude product. The obtained powder was then placed in a stirred sublimator at a heating temperature of 30° C. and a pressure of -0.1 MPa for sublimation. The sublimation temperature was 5° C. to obtain 210 g of a white fine needle-like product (molar yield 91.3%) with a purity of 99.62%.
[0067] Comparative Example 4
[0068] (i) 80 g of 30% (mass concentration of silica) silica sol, 20 g of tetrabutyl titanate, and 120 g of TS-1 powder were fully mixed, and then extruded into strip catalysts with a diameter of about 2-3 mm using an extruder, calcined at 550° C. for 6 hours, naturally cooled to room temperature, and then mixed with 0.15 mol of tetrapropylammonium hydroxide and 200 g of deionized water and placed in a stainless steel crystallization kettle lined with polytetrafluoroethylene, crystallized at 170° C. for 10 hours, taken out and washed with deionized water until neutral, and then placed in an oven to dry at 80° C. for 6 hours, and then dried at 600° C. for 6 hours to prepare the catalyst, which was loaded into a fixed bed reactor with a jacket.
[0069] (ii) 200 g of vinyl sulfite, 230 g of 30% hydrogen peroxide solution and 1000 g of dichloroethane solution were mixed at a mixing temperature of 20° C. After being uniformly dispersed, the mixture was fed into a fixed bed reactor. The temperature of the jacket coolant in the fixed bed was maintained at 20° C. The continuous feeding time was 60 min and the reaction pressure was 0.01 MPa. After all the materials had passed through the catalyst, they were layered and the lower dichloroethane phase was removed under heating conditions of -0.09 MPa and 20° C. to remove the solvent to obtain a white powdery crude product. The obtained powder was then placed in a stirred sublimator at a heating temperature of 30° C. and a pressure of -0.1 MPa for sublimation. The desublimation temperature was 5° C. to obtain 213 g of a white fine needle-like product (molar yield 92.6%) with a purity of 99.73%.
[0070] Comparative Example 5
[0071] (i) 1 g of silicon carbide, 80 g of 30% (mass concentration of silica) silica sol, 0.1 g of tetrabutyl titanate, and 120 g of TS-1 powder were fully mixed, and then extruded into strip catalysts with a diameter of about 2-3 mm using an extruder, calcined at 550° C. for 6 hours, naturally cooled to room temperature, and then mixed with 0.15 mol of tetrapropylammonium hydroxide and 200 g of deionized water and placed in a stainless steel crystallization kettle lined with polytetrafluoroethylene, crystallized at 170° C. for 10 hours, taken out and washed with deionized water until neutral, and then placed in an oven to dry at 80° C. for 6 hours, and then dried at 600° C. for 6 hours to prepare the catalyst, which was loaded into a fixed bed reactor with a jacket.
[0072] (ii) 200 g of vinyl sulfite, 230 g of 30% hydrogen peroxide solution and 1000 g of dichloroethane solution were mixed at a mixing temperature of 20° C. After being uniformly dispersed, the mixture was fed into a fixed bed reactor. The temperature of the jacket coolant in the fixed bed was maintained at 20° C. The continuous feeding time was 60 min and the reaction pressure was 0.01 MPa. After all the materials had passed through the catalyst, they were layered and the lower dichloroethane phase was removed under heating conditions of -0.09 MPa and 20° C. to remove the solvent to obtain a white powdery crude product. The obtained powder was then placed in a stirred sublimator at a heating temperature of 30° C. and a pressure of -0.1 MPa for sublimation. The sublimation temperature was 5° C. to obtain 209 g of a white product (molar yield 90.9%) with a purity of 99.55%.
[0073] Example 2
[0074] (i) 30 g of silicon dioxide, 90 g of 30% (mass concentration of silicon dioxide) silica sol, 20 g of titanium tetrachloride, and 120 g of TS-1 powder were fully mixed, and then extruded into strip catalysts with a diameter of about 2-3 mm using an extruder, calcined at 550° C. for 6 hours, naturally cooled to room temperature, and then mixed with 0.15 mol of tetrapropylammonium hydroxide and 200 g of deionized water and placed in a stainless steel crystallization kettle lined with polytetrafluoroethylene, crystallized at 170° C. for 10 hours, taken out and washed with deionized water until neutral, and then placed in an oven to dry at 80° C. for 6 hours, and then dried at 600° C. for 6 hours to prepare a catalyst, which was loaded into a fixed bed reactor with a jacket.
[0075] (ii) 200 g of vinyl sulfite, 230 g of 30% hydrogen peroxide solution and 1200 g of dichloromethane solution were mixed at a mixing temperature of 20° C. After being uniformly dispersed, the fixed bed reactor was fed. The temperature of the jacket coolant in the fixed bed was maintained at 20° C. The continuous feeding time was 60 min and the reaction pressure was 0.01 MPa. After all the materials had passed through the catalyst, they were layered, and the lower dichloromethane phase was removed by heating at -0.09 MPa and 15° C. to remove the solvent to obtain a white powdery crude product. The obtained powder was then placed in a stirred sublimator at a heating temperature of 30° C. and a pressure of -0.1 MPa for sublimation. The sublimation temperature was 5° C. to obtain 219 g of a white product (molar yield 95.2%) with a purity of 99.83%.
[0076] Example 3
[0077] (i) 20 g of silicon carbide, 80 g of 30% (mass concentration of silica) silica sol, 20 g of tetrabutyl titanate, and 120 g of TS-1 powder were fully mixed, and then extruded into strip catalysts with a diameter of about 2-3 mm using an extruder, calcined at 550° C. for 6 hours, naturally cooled to room temperature, and then mixed with 0.15 mol of tetrabutylammonium hydroxide and 200 g of deionized water and placed in a stainless steel crystallization kettle lined with polytetrafluoroethylene, crystallized at 170° C. for 10 hours, taken out and washed with deionized water until neutral, and then placed in an oven to dry at 80° C. for 6 hours, and then dried at 600° C. for 6 hours to prepare a catalyst, which was loaded into a fixed bed reactor with a jacket.
[0078] (ii) 200 g of vinyl sulfite, 230 g of 30% hydrogen peroxide solution and 1200 g of ethylene dichloride solution were mixed at a mixing temperature of 20° C. After being uniformly dispersed, the mixture was fed into a fixed bed reactor. The temperature of the jacket coolant in the fixed bed was maintained at 20° C. The continuous feeding time was 60 min and the reaction pressure was 0.01 MPa. After all the materials had passed through the catalyst, they were layered and the lower layer of ethylene dichloride phase was removed under heating conditions of -0.09 MPa and 20° C. to remove the solvent to obtain a white powdery crude product. The obtained powder was then placed in a stirred sublimator at a heating temperature of 35° C. and a pressure of -0.095 MPa for sublimation. The sublimation temperature was 7° C. to obtain 216 g of a white product (molar yield 93.9%) with a purity of 99.78%.
[0079] Example 4
[0080] (i) 20 g of silicon carbide, 80 g of 30% (mass concentration of silica) silica sol, 20 g of tetrabutyl titanate, and 120 g of TS-1 powder were fully mixed, and then extruded into strip catalysts with a diameter of about 2-3 mm using an extruder, calcined at 550° C. for 6 hours, naturally cooled to room temperature, and then mixed with 0.15 mol of tetrapropylammonium hydroxide and 200 g of deionized water and placed in a stainless steel crystallization kettle lined with polytetrafluoroethylene, crystallized at 170° C. for 10 hours, taken out and washed with deionized water until neutral, and then placed in an oven to dry at 80° C. for 6 hours, and then dried at 600° C. for 6 hours to prepare a catalyst, which was loaded into a fixed bed reactor with a jacket.
[0081] (ii) 200 g of vinyl sulfite, 230 g of 30% hydrogen peroxide solution, and 1000 g of acetonitrile solution were mixed at a mixing temperature of 20° C. After being uniformly dispersed, the fixed bed reactor was fed, and the temperature of the jacket coolant in the fixed bed was maintained at 20° C. The continuous feeding time was 60 min, and the reaction pressure was 0.01 MPa. After all the materials passed through the catalyst, the solution phase was removed from the solvent under heating conditions of -0.095 MPa and 30° C. to obtain a white powdery crude product. The obtained powder was then placed in a stirred sublimator at a heating temperature of 45° C. and a pressure of -0.088 MPa for sublimation. The sublimation temperature was 15° C. to obtain 218 g of a white product (molar yield 94.8%) with a purity of 99.61%.
[0082] Example 5
[0083] (i) 55 g of spherical silica with a diameter of about 2 mm was added to a ball rolling machine, and a mixed solution of 80 g of 30% concentration (mass concentration of silica) of silica sol and 20 g of tetrabutyl titanate was continuously sprayed, and 120 g of TS-1 powder was slowly added to roll the catalyst into a spherical catalyst with a diameter of about 3 mm, calcined at 550° C. for 6 hours, naturally cooled to room temperature, and then mixed with 0.15 mol of tetrapropylammonium hydroxide and 200 g of deionized water and placed in a stainless steel crystallization kettle lined with polytetrafluoroethylene, crystallized at 170° C. for 10 hours, taken out and washed with deionized water until neutral, and then placed in an oven to dry at 80° C. for 6 hours, and then dried at 600° C. for 6 hours to prepare a catalyst, which was loaded into a fixed bed reactor with a jacket.
[0084] (ii) 200 g of vinyl sulfite, 230 g of 30% hydrogen peroxide solution and 1000 g of ethylene dichloride solution were mixed at a mixing temperature of 20° C. After being uniformly dispersed, the mixture was fed into a fixed bed reactor. The temperature of the jacket coolant in the fixed bed was maintained at 20° C. The continuous feeding time was 60 min and the reaction pressure was 0.01 MPa. After all the materials had passed through the catalyst, they were layered and the lower layer of ethylene dichloride phase was removed under heating conditions of -0.09 MPa and 20° C. to remove the solvent to obtain a white powdery crude product. The obtained powder was then placed in a stirred sublimator at a heating temperature of 30° C. and a pressure of -0.1 MPa for sublimation. The sublimation temperature was 5° C. to obtain 226 g of a white product (molar yield 98.3%) with a purity of 99.96%.
[0085] Example 6
[0086] (i) 15 g of activated alumina, 120 g of 30% (mass concentration of silica) silica sol, 15 g of titanium hydroxide and 120 g of TS-2 powder were fully mixed, and then extruded into strip catalysts with a diameter of about 2-3 mm using an extruder, calcined at 550° C. for 6 hours, naturally cooled to room temperature, and then mixed with 0.15 mol of hexamethylenediamine and 200 g of deionized water and placed in a stainless steel crystallization kettle lined with polytetrafluoroethylene, crystallized at 170° C. for 10 hours, taken out and washed with deionized water until neutral, and then placed in an oven to dry at 80° C. for 6 hours, and then dried at 600° C. for 6 hours to prepare the catalyst, which was loaded into a fixed bed reactor with a jacket.
[0087] (ii) 200 g of vinyl sulfite, 250 g of 70% tert-butyl hydroperoxide, and 1200 g of DMF were mixed at a mixing temperature of 20° C. After being uniformly dispersed, the fixed bed reactor was fed, and the temperature of the jacket coolant in the fixed bed was maintained at 30° C. The continuous feeding time was 60 min, and the reaction pressure was 0.01 MPa. After all the materials passed through the catalyst, the solvent was removed under heating conditions of -0.09 MPa and 20° C. to obtain a white powdery crude product. The obtained powder was then placed in a stirred sublimator at a heating temperature of 50° C. and a pressure of -0.09 MPa for sublimation. The sublimation temperature was -5° C. to obtain 217.8 g of a white product (molar yield 94.3%) with a purity of 99.62%.
[0088] The above is an exemplary description of the embodiments of the present invention. However, the protection scope of the present invention is not limited to the above embodiments. Any modification, equivalent substitution, improvement, etc. made by those skilled in the art within the spirit and principle of the present invention shall be included in the protection scope of the present invention.
Claims
1. A catalyst, characterized in that The catalyst components include: a titanium silicon molecular sieve with a topological structure, a binder, a carrier, a titanium-containing auxiliary agent, a basic compound and water; The mass ratio of the titanium silicon molecular sieve with topological structure, the solid component in the binder, the carrier, and the titanium-containing auxiliary agent is 100:(1-1000):(1-4000):(0.5-1000); The molar mass ratio of the alkaline compound, the titanium silicon molecular sieve with a topological structure and water is (0.01-100) mol:100 g:(10-3000) g.
2. The catalyst according to claim 1, characterized in that The titanium silicon molecular sieve with a topological structure is one or more of a titanium silicon molecular sieve with an MFI structure, a titanium silicon molecular sieve with a MEL structure, a titanium silicon molecular sieve with a BEA structure, a titanium silicon molecular sieve with an MWW structure, a titanium silicon molecular sieve with a hexagonal structure, a titanium silicon molecular sieve with a MOR structure, a titanium silicon molecular sieve with a TUN structure, and a titanium silicon molecular sieve with other structures; Preferably, the binder is one or more of silica sol, pseudo-boehmite, etc.; the mass concentration of silicon dioxide in the silica sol is 1 to 80%. Preferably, the carrier is one or a mixture of silicon dioxide, silicon carbide, SBA-15, activated alumina, glass fiber, ceramic, layered graphite, quartz glass, natural clay, expanded perlite, activated carbon. Preferably, the titanium-containing additive is titanium tetrachloride, titanium trichloride, titanium sulfate, titanium hydroxide, titanium oxychloride, organic titanate R4TiO4, wherein R is the same or different and is independently selected from an alkyl group of 2 to 4 carbon atoms, titanium dioxide, or a mixture of several thereof. Preferably, the organic titanate is selected from tetrabutyl titanate, tetrapropyl titanate, and methyl triethyl titanate. The titanium-containing additive is preferably one or several of titanium tetrachloride, titanium hydroxide, and tetrabutyl titanate. Preferably, the equivalent particle size of the catalyst is 0.1 mm to 30 mm. Preferably, the alkaline compound is one or more of an organic quaternary ammonium base, an aliphatic alcohol amine, an aliphatic amine, and an inorganic alkaline substance. Preferably, the organic quaternary ammonium base is R a 4NOH, where R a The same or different alkyl groups are independently selected from alkyl groups with 1 to 5 carbon atoms, or a mixture of a quaternary ammonium salt and a strong base substance.
3. The catalyst according to claim 1, characterized in that The mass ratio of the titanium silicon molecular sieve with a topological structure, the solid component in the binder, the carrier, and the titanium-containing auxiliary agent is 100: (10-400): (1-400): (0.5-100). Preferably, the molar mass ratio of the basic compound, the titanium silicalite molecular sieve having a topological structure and water is (0.1-10) (mol): 100 (g): (50-1000) (g).
4. The method for preparing the catalyst according to any one of claims 1 to 3, characterized in that: The method comprises: The catalyst is prepared by mixing a titanium silicon molecular sieve with a topological structure, a binder, a carrier and a titanium-containing auxiliary agent, calcining the mixture, and then subjecting the mixture to modification treatment with an alkaline compound aqueous solution.
5. The method according to claim 4, characterized in that The calcination temperature is 400-900° C., and the calcination time is 2-24 hours. Preferably, the modification treatment condition is: crystallizing the calcined product at 140-240° C. for 2-120 hours.
6. Use of the catalyst according to any one of claims 1 to 3 in the preparation of vinyl sulfate.
7. A method for preparing vinyl sulfate, characterized in that: The method comprises: Vinyl sulfite, an oxidant and the catalyst according to any one of claims 1 to 3 are mixed and reacted, and the prepared intermediate product is sublimated and condensed and crystallized to obtain the vinyl sulfate.
8. The method according to claim 7, characterized in that The molar mass ratio of the vinyl sulfite, the oxidant and the catalyst is 1 mol: (0.1-20) mol: (0.1-5000) g. Preferably, the oxidant is one or more of aqueous hydrogen peroxide, tert-butyl hydroperoxide, urea peroxide, potassium persulfate, ammonium persulfate, cumene hydroperoxide, ethylbenzene hydroperoxide, cyclohexyl hydroperoxide, peracetic acid, peroxypropionic acid, benzoyl peroxide, potassium permanganate, hypochlorite, percarbonate, and dichromate. Preferably, the reaction temperature is -10°C to 50°C; the reaction time is 10 to 500 min; and the reaction pressure is -0.02 MPa to 1 MPa.
9. The method according to claim 7, characterized in that: The sublimation temperature is 0-80°C. Preferably, the sublimation pressure is -0.1 MPa to 0.01 MPa.
10. The method according to claim 7, characterized in that The temperature of the desublimation crystallization is -20°C to 50°C.
Citation Information
Patent Citations
Extrusion molding method for high-strength TS-1 (Titanium Silicalite-1) catalyst
CN103041850A
Propylene epoxidation catalyst, as well as preparation method and application thereof
CN103464197A
Method for modifying extrusion moulding titanium silicalite molecular sieve
CN106238094A
Preparation method of cyclic sulfate
CN107353277A
Preparation method of cyclic sulfates
CN109422719A
Cited By
Preparation method of ethylene sulfate and derivatives thereof
CN119707913A