Welding method

Through wet sandblasting or chemical agent rust removal and drying treatment, combined with copper pad and water transport heat dissipation technology, the problem of solder joint grooves after welding is solved, the welding strength and safety are improved, and the stability and stability of the welding process are ensured. Security.

CN118768705APending Publication Date: 2024-10-15FOSHAN SANYOU AUTOMOTIVE PARTS MFG CO LTD
View PDF 1 Cites 0 Cited by

Patent Information

Application Number
CN202310351142.1
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2023-04-04
Publication Date
2024-10-15

AI Technical Summary

Technical Problem

Existing welding methods can easily lead to solder joint grooves on the surface of the welded parts after welding, which affects product quality. In addition, there are safety hazards such as burns, electric shock, and visual impairment during the welding process.

Method used

Use wet sandblasting or chemical agents to remove rust and clean the surface of the welded parts. After combined with drying treatment, add a copper pad and water transport heat dissipation mechanism to the fixture to reduce solder joint depression through heat conduction and heat dissipation.

Benefits of technology

Effectively remove rust on the surface of welded parts, improve welding strength and safety, reduce the occurrence of solder joint grooves, and enhance the safety of the welding process.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118768705A_ABST
    Figure CN118768705A_ABST
Patent Text Reader

Abstract

The invention discloses a welding method. Comprising the following welding steps that S1, the welding surface of a welding part is cleaned; s2, the welding surface of the welding part is dried; s3, the welding part is clamped and fixed, and precise attachment of the welding surface is kept; s4, a welding clamp is transformed; s5, conducting heat conduction and heat dissipation treatment on the welding part; and S6, welding treatment on the welding part is achieved. According to the method, firstly, the surface of the welding part is cleaned, rust on the surface of the welding part is removed, the rust is prevented from influencing the welding strength during welding, the metal welding part is dried, residual water on the surface of the metal welding part is prevented from influencing the welding process, then the clamp is modified, and the welding quality is improved. The copper base plate is additionally arranged on the welding clamp, heat conduction and heat dissipation treatment is carried out on a welding part, the welding part is effectively treated, and welding spot grooves in the surface of the welding part are effectively reduced.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of welding, and in particular relates to a welding method. Background Art

[0002] Welding, also known as fusion, is a manufacturing process and technology that joins metals or other thermoplastic materials such as plastics by heating, high temperature or high pressure.

[0003] There are many sources of energy for modern welding, including gas flame, arc, laser, electron beam, friction and ultrasound. In addition to being used in factories, welding can also be performed in a variety of environments, such as outdoors, underwater and in space. Welding can be dangerous to operators wherever they are, so appropriate protective measures must be taken when welding. The possible harm caused by welding to the human body includes burns, electric shock, visual impairment, inhalation of toxic gases, excessive ultraviolet radiation, etc. When producing automotive parts, some parts need to be welded, but various welding methods on the market still have various problems.

[0004] For example, a welding method disclosed in the authorization announcement number CN111774702A realizes the use of tungsten inert gas shielded welding for base welding, and the use of metallurgical electrode gas shielded welding for filling welding and capping welding of the weld after base welding, which effectively ensures that the root of the weld is fully penetrated. However, it does not solve the problem that there will be grooves of welding points on the surface of the welded part after existing welding, which has a certain impact on the product. For this reason, we propose a welding method. Summary of the invention

[0005] The object of the present invention is to provide a welding method to solve the problems raised in the above background technology.

[0006] To achieve the above object, the present invention provides the following technical solution: a welding method, comprising the following welding steps: S1. Cleaning the welding surface of the welded parts: Clean the surface of the welded parts, that is, clean the rust on the surface of the welded parts, use wet sandblasting or chemical rust removal to clean the welding surface of the welded parts; S2. Drying the welding surface of the welded parts: Drying the cleaned welding surface of the welded parts to remove moisture from the welded parts during rust removal, so as to keep the welding surface of the welded parts dry for subsequent welding. S3. Clamp and fix the welded parts to keep the welded surfaces precisely fitted: fit the surfaces of the welded parts to be welded together, and then precisely clamp and fix them with a fixture to keep the welded surfaces fitted together; S4. Modify the welding fixture: add a copper backing plate to the welding fixture, and connect the copper backing plate to the fixture with bolts; S5. Conduct heat conduction and heat dissipation for welded parts: add a flat heat conduction plate to the welding fixture, and then add a water heat dissipation mechanism to keep the heating energy at the concentrated heating position unchanged, and transfer the heat energy to the product through the flat heat conduction plate, that is, heat dissipation is achieved by cooling with water; S6. Welding the welded parts: The welding parts are then welded by welding guns. The electrode cap size of the spot welding robot is Ф16*23, and the end face is 6 mm. The flat heat conducting plate and water heat dissipation mechanism are used to reduce the depression of the welding points.

[0007] Preferably, when the wet sandblasting in S1 is performed for rust removal, the welded parts are first clamped and fixed by a clamp, and when the wet sandblasting is performed for rust removal, the welded parts are clamped and fixed inside the rust removal box to prevent environmental pollution during rust removal.

[0008] By adopting the above technical solution, wet sandblasting is used for rust removal and clamping is performed by a clamp, which can protect the operator's hands and improve environmental protection.

[0009] Preferably, when the rust removal and sandblasting are being used, moisture may cause the welded parts to still rust during subsequent use, so 1%-15% of a rust inhibitor and an emulsifier or soapy water is added to the water, wherein the rust inhibitor includes trisodium phosphate, sodium carbonate and sodium nitrite, and sand collecting equipment is used to collect the sand to prevent splashing and polluting the environment.

[0010] By adopting the above technical solution, the moisture in wet sandblasting will cause rust on metal welded parts. In order to prevent rust, 1%-15% of rust inhibitor and emulsifier or soapy water is added to the water, and the sand dust is collected to prevent air pollution.

[0011] Preferably, the acid used for chemical rust removal in S1 includes sulfuric acid, hydrochloric acid, nitric acid, phosphoric acid, hydrofluoric acid, chromic anhydride, citric acid, oxalic acid and aminosulfuric acid. When the chemical rust removal is used, a corrosion inhibitor needs to be added to prevent excessive corrosion of the substrate of the metal weldment.

[0012] By adopting the above technical solution, chemical rust removal is used to achieve rust removal treatment on metal welded parts, effectively removing rust on the surface of metal welded parts, and in order to prevent excessive corrosion, corrosion inhibitors are added to protect the metal welded parts.

[0013] Preferably, in the cleaning process of chemical rust removal, in order to improve the cleaning rate and efficiency, ultrasonic wave is used for auxiliary cleaning, and the mechanical energy of ultrasonic oscillation is used to generate countless small bubbles in the rust removal liquid. These small bubbles generate strong mechanical force when they are formed, grown and closed, so that the oxide scale and rust dirt on the surface of the workpiece are quickly detached, thereby accelerating the rust removal process and making the rust removal more thorough.

[0014] By adopting the above technical solution and combining it with ultrasonic rust removal and cleaning, the surface of metal welded parts can be effectively cleaned, the cleaning efficiency can be improved, and the rust removal can be more thorough.

[0015] Preferably, before the drying treatment in S2, that is, after the weld is derusted, the surface of the weld is cleaned, especially the rust removal is carried out by chemical agents, and the chemical agents remaining on the surface of the weld are cleaned with distilled water to prevent the chemical agents from corroding the metal weld, and the number of cleaning times with distilled water is three times, or ultrasonic cleaning is performed in combination.

[0016] By adopting the above technical solution, the residual chemical agent will corrode the surface of the metal welded parts, affecting the welding strength and the strength of the welded parts. It can be effectively removed by distilled water, and the residual chemical agent in the gap can be removed by ultrasound.

[0017] Preferably, the drying process in S2 is hot air drying or open flame baking. The hot air drying uses a hot air blower to dry the surface of the weldment, and the open flame baking uses a flamethrower to directly dry the weldment.

[0018] By adopting the above technical scheme, open flame baking can be used for metal welds with high strength and high temperature resistance, which can not only dry the surface of the metal welds, but also process the surface of the metal welds to improve the welding strength. For metal welds with low strength and not resistant to high temperature, hot air drying can be used to effectively dry the surface of the metal welds.

[0019] Preferably, when the copper pad in S4 is installed and connected by bolts, a groove is opened on the end face of the copper pad, so that the end of the bolt can be snap-fitted and connected inside the groove, and the excess part of the end of the bolt is cut off by a cutting machine to keep the surface of the bolt and the copper pad flush, which is convenient for clamping and fixing the welded parts.

[0020] By adopting the above technical solution, the setting of the copper pad should reduce the obstacles to the clamping of the metal welded parts, and should increase the connectivity while maintaining flatness, so as to facilitate the clamping and fixing of the metal welded parts.

[0021] Preferably, the flat heat conducting plate in S5 is a metal heat conducting plate made of copper or aluminum, and is used to conduct the heat from the concentrated heating position to the welded part to improve the welding effect. The flat heat conducting plate is arranged between the clamp and the welded part to achieve the conduction of heat energy.

[0022] By adopting the above technical solution, the heat at the heating position is conducted using a metal heat conducting plate, so that the temperature of the entire metal welding part surface is kept uniform, which facilitates the welding process.

[0023] Preferably, the water transport and heat dissipation mechanism in S5 includes a water pump, a water tank, a circulating water pipe and a control valve. The water pump is arranged inside or outside the water tank to extract cooling water from the water tank and then transport it to the circulating water pipe. The circulating water pipe is used to cool and dissipate heat for the welded parts. The control valve is used to control the on / off and flow rate of the water flow.

[0024] By adopting the above technical solution, the water-dissipating heat dissipation mechanism is used to cool down the temperature of the welding point, thereby preventing the temperature of the welding point from being too high, thereby causing grooves in the welding point on the surface of the welded part.

[0025] Compared with the prior art, the present invention has the following beneficial effects: When the present invention is used, the surface of the welding part is first cleaned to effectively remove the rust on the surface of the welding part, so as to prevent the rust from affecting the welding strength during welding, and a variety of rust removal methods are selected and used according to the characteristics, shape and material of the metal welding part to improve the safety of the metal welding part. After cleaning, the metal welding part is dried to prevent the residual moisture on the surface of the metal welding part from affecting the welding process, preventing the welding process from being loose or welding through the metal welding part. Then, the clamp is modified, a copper pad is added to the welding clamp, and the welding part is heat-conducting and heat-dissipating. A flat heat-conducting plate is added to the welding clamp, and then a water-transporting heat-dissipating mechanism is added to keep the heating energy at the concentrated heating position unchanged, and transfer the heat energy to the product through the flat heat-conducting plate, that is, the heat dissipation is achieved by cooling with water, so that the welding part is effectively processed and the welding point grooves on the surface of the welding part are effectively reduced. BRIEF DESCRIPTION OF THE DRAWINGS

[0026] Figure 1 It is a schematic diagram of the steps of the present invention. Implementation

[0027] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0028] See also Figure 1 The present invention provides a technical solution: a welding method, comprising the following welding steps: S1. Cleaning the welding surface of the welded parts: Clean the surface of the welded parts, that is, clean the rust on the surface of the welded parts, use wet sandblasting or chemical rust removal to clean the welding surface of the welded parts; S2. Drying the welding surface of the welded parts: Drying the cleaned welding surface of the welded parts to remove moisture from the welded parts during rust removal, so as to keep the welding surface of the welded parts dry for subsequent welding. S3. Clamp and fix the welded parts to keep the welded surfaces precisely fitted: fit the surfaces of the welded parts to be welded together, and then precisely clamp and fix them with a fixture to keep the welded surfaces fitted together; S4. Modify the welding fixture: add a copper backing plate to the welding fixture, and connect the copper backing plate to the fixture with bolts; S5. Conduct heat conduction and heat dissipation for welded parts: add a flat heat conduction plate to the welding fixture, and then add a water heat dissipation mechanism to keep the heating energy at the concentrated heating position unchanged, and transfer the heat energy to the product through the flat heat conduction plate, that is, heat dissipation is achieved by cooling with water; S6. Welding the welded parts: The welding parts are then welded by welding guns. The electrode cap size of the spot welding robot is Ф16*23, and the end face is 6 mm. The flat heat conducting plate and water heat dissipation mechanism are used to reduce the depression of the welding points.

[0029] In the present embodiment, preferably, when the wet sandblasting in S1 is used for rust removal, the weldment is first clamped and fixed by a clamp, and when the wet sandblasting is used for rust removal, the weldment is clamped and fixed inside the rust removal box to prevent environmental pollution during rust removal. The wet sandblasting is used for rust removal by clamping with a clamp, which can protect the operator's hands and improve environmental protection.

[0030] In this embodiment, preferably, when the rust removal and sandblasting are in use, moisture will cause the welded parts to rust during subsequent use, and 1%-15% of rust inhibitors and emulsifiers or soapy water are added to the water. The rust inhibitor includes trisodium phosphate, sodium carbonate and sodium nitrite, and sand collecting equipment is used to collect the sand to prevent splashing and polluting the environment. The moisture in wet sandblasting and rust removal will cause metal welded parts to rust. In order to prevent rust, 1%-15% of rust inhibitors and emulsifiers or soapy water are added to the water, and the sand and dust are collected to prevent air pollution.

[0031] In this embodiment, preferably, the acid used for the chemical rust removal in S1 includes sulfuric acid, hydrochloric acid, nitric acid, phosphoric acid, hydrofluoric acid, chromic anhydride, citric acid, oxalic acid and aminosulfuric acid. When the chemical rust removal is used, it is necessary to add a corrosion inhibitor to prevent excessive corrosion of the substrate of the metal welded parts. The chemical rust removal is used to achieve rust removal treatment on the metal welded parts, effectively remove the rust on the surface of the metal welded parts, and in order to prevent excessive corrosion, a corrosion inhibitor is added to protect the metal welded parts.

[0032] In the present embodiment, preferably, in the cleaning process of chemical rust removal, in order to improve the cleaning rate and efficiency, ultrasonic wave is used for auxiliary cleaning, and the mechanical energy of ultrasonic oscillation is used to generate countless small bubbles in the rust removal liquid. These small bubbles generate strong mechanical force when they are formed, grown and closed, so that the oxide scale and rust dirt on the surface of the workpiece are quickly separated, thereby accelerating the rust removal process and making the rust removal more thorough. The rust removal cleaning is carried out in combination with ultrasonic wave, which can effectively realize the cleaning of the surface of metal welded parts, improve the cleaning efficiency, and make the volume rust removal more thorough.

[0033] In this embodiment, preferably, before the drying treatment in S2, that is, after the rust removal of the weld, the surface of the weld is cleaned, especially the rust removal by chemical agent, and the residual chemical agent on the surface of the weld is cleaned with distilled water to prevent the chemical agent from corroding the metal weld, and the distilled water is cleaned three times, or ultrasonic cleaning is used. The residual chemical agent will corrode the surface of the metal weld, affecting the welding strength and the strength of the weld, which can be effectively removed by distilled water, and the ultrasonic wave can remove the residual chemical agent in the gap.

[0034] In this embodiment, preferably, the drying treatment in S2 adopts hot air drying or open flame baking treatment. The hot air drying adopts a hot air blower to dry the surface of the weldment, and the open flame baking treatment adopts a flamethrower to directly dry the weldment. For metal weldments with high strength and high temperature resistance, open flame baking can be used, which can not only dry the surface of the metal weldment, but also process the surface of the metal weldment to improve the welding strength. For metal weldments with low strength and not resistant to high temperature, hot air drying is used to effectively dry the surface of the metal weldment.

[0035] In this embodiment, preferably, when the copper pad in S4 is installed and connected by bolts, a groove is opened on the end face of the copper pad, so that the end of the bolt can be snap-fitted and connected inside the groove, and the excess part of the end of the bolt is cut off by a cutting machine to keep the surface of the bolt and the copper pad flush, which is convenient for clamping and fixing the welded parts. The setting of the copper pad should reduce obstacles to the clamping of metal welded parts, and should increase connectivity while maintaining flatness, which is convenient for clamping and fixing metal welded parts.

[0036] In this embodiment, preferably, the flat heat conductive plate in S5 is a metal heat conductive plate, and the metal heat conductive plate is made of copper or aluminum, and is used to conduct the heat from the concentrated heating position to the weldment to improve the welding effect. The flat heat conductive plate is arranged between the clamp and the weldment to achieve the conduction of heat energy. The metal heat conductive plate is used to conduct the heat from the heating position, which is convenient for maintaining the uniform temperature of the entire metal weldment surface and facilitating the welding process.

[0037] In this embodiment, preferably, the water transport and heat dissipation mechanism in S5 includes a water pump, a water tank, a circulating water pipe and a control valve. The water pump is arranged inside or outside the water tank to extract cooling water from the water tank and then transport it to the circulating water pipe. The circulating water pipe is used to cool and dissipate heat of the welded parts. The control valve is used to control the on-off and flow rate of the water flow. The water transport and heat dissipation mechanism is arranged to cool the temperature of the welding point to prevent the temperature of the welding point from being too high, which causes grooves in the welded parts on the surface of the welded parts.

[0038] The working principle and use process of the present invention: The first step is to clean the welding surface of the welded parts: clean the surface of the welded parts, that is, clean the rust on the surface of the welded parts, use wet sandblasting or chemical rust removal to clean the welding surface of the welded parts; The second step is to dry the welding surface of the welded parts: dry the cleaned welding surface of the welded parts, dry the moisture present in the rust removal of the welded parts, keep the welding surface of the welded parts dry, and facilitate the subsequent welding process; The third step is to clamp and fix the welded parts to keep the welded surface precisely fitted: fit the welded parts to be welded, and then use the fixture to clamp and fix them precisely to keep the welded surface fitted; Step 4: Modify the welding fixture: add a copper backing plate to the welding fixture, and connect the copper backing plate to the fixture with bolts; Step 5: Heat conduction and heat dissipation treatment of welded parts: add a flat heat conduction plate to the welding fixture, and then add a water heat dissipation mechanism to keep the heating energy at the concentrated heating position unchanged, and transfer the heat energy to the product through the flat heat conduction plate, that is, heat dissipation is achieved by water cooling; Step 6: Welding the welded parts: Use a welding gun to weld the welded parts. The spot welding robot electrode cap size is Ф16*23, and the end face is 6 mm. Use a flat heat conducting plate and a water heat dissipation mechanism to reduce the depression of the weld.

[0039] Although embodiments of the present invention have been shown and described, it will be appreciated by those skilled in the art that various changes, modifications, substitutions and variations may be made to the embodiments without departing from the principles and spirit of the present invention, and that the scope of the present invention is defined by the appended claims and their equivalents.

Claims

1. A welding method, characterized in that: The welding steps include: S1. Clean the welding surface of the welded parts: clean the surface of the welded parts, that is, clean the rust on the surface of the welded parts, use wet sandblasting or chemical rust removal to clean the welding surface of the welded parts; S2. Drying the welding surface of the welded parts: Drying the cleaned welding surface of the welded parts to remove moisture from the welded parts during rust removal, so as to keep the welding surface of the welded parts dry for subsequent welding. S3. Clamp and fix the welded parts to keep the welded surfaces precisely fitted: fit the surfaces of the welded parts to be welded together, and then precisely clamp and fix them with a fixture to keep the welded surfaces fitted together; S4. Modify the welding fixture: add a copper backing plate to the welding fixture, and connect the copper backing plate to the fixture with bolts; S5. Conduct heat conduction and heat dissipation for welded parts: add a flat heat conduction plate to the welding fixture, and then add a water heat dissipation mechanism to keep the heating energy at the concentrated heating position unchanged, and transfer the heat energy to the product through the flat heat conduction plate, that is, heat dissipation is achieved by cooling with water; S6. Welding the welded parts: The welding parts are then welded by welding guns. The electrode cap size of the spot welding robot is Ф16*23, and the end face is 6 mm. The flat heat conducting plate and water heat dissipation mechanism are used to reduce the depression of the welding points.

2. A welding method according to claim 1, characterized in that: When the wet sandblasting rust removal in S1 is performed, the welded parts are first clamped and fixed by a clamp, and when the wet sandblasting rust removal is performed, the welded parts are clamped and fixed inside the rust removal box to prevent environmental pollution during rust removal.

3. A welding method according to claim 2, characterized in that: When the rust removal and sandblasting are in use, moisture will cause the welded parts to still rust during subsequent use. In this case, 1%-15% of a rust inhibitor and an emulsifier or soapy water is added to the water. The rust inhibitor includes trisodium phosphate, sodium carbonate and sodium nitrite, and sand is collected using a sand collecting device to prevent splashing and polluting the environment.

4. A welding method according to claim 1, characterized in that: The acid used for chemical rust removal in S1 includes sulfuric acid, hydrochloric acid, nitric acid, phosphoric acid, hydrofluoric acid, chromic anhydride, citric acid, oxalic acid and aminosulfuric acid. When the chemical rust removal is used, a corrosion inhibitor needs to be added to prevent excessive corrosion of the substrate of the metal weldment.

5. A welding method according to claim 4, characterized in that: In the cleaning process of chemical rust removal, in order to improve the cleaning rate and efficiency, ultrasonic wave is used for auxiliary cleaning, and the mechanical energy of ultrasonic oscillation is used to generate countless small bubbles in the rust removal liquid. These small bubbles generate strong mechanical force when they are formed, grown and closed, so that the oxide scale and rust dirt on the surface of the workpiece are quickly separated, thereby accelerating the rust removal process and making the rust removal more thorough.

6. A welding method according to claim 1, characterized in that: Before the drying treatment in S2, that is, after the weld is derusted, the surface of the weld is cleaned, especially by chemical derusting. Distilled water is used to clean the residual chemicals on the surface of the weld to prevent the chemicals from corroding the metal weld. The number of distilled water cleanings is three times, or ultrasonic cleaning is used.

7. A welding method according to claim 1, characterized in that: The drying process in S2 is hot air drying or open flame baking. The hot air drying uses a hot air blower to dry the surface of the weldment, and the open flame baking uses a flamethrower to directly dry the weldment.

8. A welding method according to claim 1, characterized in that: When the copper pad in S4 is installed and connected by bolts, a groove is opened on the end face of the copper pad, so that the end of the bolt can be snap-fitted and connected inside the groove, and the excess part of the end of the bolt is cut off by a cutting machine to keep the surface of the bolt and the copper pad flush, which is convenient for clamping and fixing the welded parts.

9. A welding method according to claim 1, characterized in that: The flat heat-conducting plate in S5 is a metal heat-conducting plate made of copper or aluminum, which is used to conduct the heat from the concentrated heating position to the welded part to improve the welding effect. The flat heat-conducting plate is arranged between the clamp and the welded part to achieve heat conduction.

10. A welding method according to claim 1, characterized in that: The water transport and heat dissipation mechanism in S5 includes a water pump, a water tank, a circulating water pipe and a control valve. The water pump is arranged inside or outside the water tank to extract cooling water from the water tank and then transport it to the circulating water pipe. The circulating water pipe is used to cool and dissipate heat for the welded parts. The control valve is used to control the on / off and flow rate of the water flow.

Citation Information

Patent Citations

  • Welding method

    CN111774702A