Manufacturing process of aluminum shell and production system of aluminum shell
Patent Information
- Application Number
- CN202410775599.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-06-17
- Publication Date
- 2024-10-15
Smart Images

Figure CN118768869A_ABST
Abstract
Description
Technical Field
[0001] The present application relates to a manufacturing technology of an aluminum shell, and in particular to a manufacturing process of an aluminum shell and a production system of an aluminum shell. Background Art
[0002] The aluminum shell of the power battery needs to have good sealing performance, so the manufacturing process of the aluminum shell of the power battery is very important. In order to produce aluminum shells with different wall thicknesses, in the relevant technology, multiple sheet metal parts of different thicknesses are generally welded together. The weld formed by welding will run through the entire product, and the weld is long, resulting in a higher risk of leakage in the power battery manufactured using the aluminum shell. Summary of the invention
[0003] The present application aims to solve at least one of the technical problems existing in the prior art. To this end, the present application proposes a manufacturing process of an aluminum shell, which can manufacture an integrally formed aluminum shell.
[0004] The present application also provides a production system of an aluminum shell having the above-mentioned manufacturing process of the aluminum shell.
[0005] According to the first aspect of the present application, the manufacturing process of the aluminum shell includes the following steps:
[0006] Obtaining blanks;
[0007] The blank is extruded into a first semi-finished product by an extrusion device; wherein the extrusion device includes a first molding structure and a first force-applying structure, the first molding structure forms a molding groove, the molding groove has two opposite first groove walls and two opposite second groove walls, the first force-applying structure has two opposite first side walls and two opposite second side walls, and the size of the cross section of the first force-applying structure is smaller than the size of the cross section of the molding groove; when the first force-applying structure enters the molding groove, a first gap is formed between the first groove wall and the first side wall, a second gap is formed between the second groove wall and the second side wall, and the spacing of the first gap is smaller than the spacing of the second gap ; The blank is placed in the molding groove, the first force-applying structure moves toward the molding groove along the first direction, the first force-applying structure squeezes the blank in the molding groove, the blank is deformed and flows around to the first gap and the second gap and extends in the opposite direction of the first direction, so that the blank forms a first semi-finished product, the first semi-finished product includes an integrated shell part and an end cover part, the first gap corresponds to forming a first shell wall of the shell part, the second gap corresponds to forming a second shell wall of the shell part, the thickness of the first shell wall is less than the thickness of the second shell wall, and the end cover part is formed between the bottom of the molding groove and the bottom end of the first force-applying structure;
[0008] The first semi-finished product is thinned by a thinning device to form a second semi-finished product;
[0009] The second semi-finished product is cut to form an aluminum shell.
[0010] According to the manufacturing process of the aluminum shell of the first embodiment of the present application, at least the following beneficial effects are achieved: the present application uses an extrusion device to extrude a blank to form a first semi-finished product with different wall thicknesses, then uses a thinning device to thin the first shell wall and the second shell wall of the first semi-finished product to form a second semi-finished product, and then shortens the second semi-finished product to form an aluminum shell with different wall thicknesses, and the first wall body and the second wall body of the aluminum shell are integrally formed, thereby, the aluminum shell manufactured by the manufacturing process of the aluminum shell of the present application is integrally formed, and has good sealing performance, thereby the power battery manufactured using the aluminum shell has good sealing performance. And because the wall thickness of the aluminum shell is different, the volume, weight and production cost of the aluminum shell can be reduced.
[0011] According to some embodiments of the present application, the step of thinning the first semi-finished product to form the second semi-finished product by a thinning device comprises the following steps:
[0012] The thinning device includes a second force-applying structure and at least two second molding structures, the second molding structures are distributed along the second direction, and the second molding structures are provided with molding holes that penetrate the second molding structures along the second direction, and the molding holes of adjacent second molding structures are connected; along the second direction, the inner diameter of the molding holes shows a decreasing trend; the second force-applying structure is inserted into the interior of the shell part, abuts against the end cover part, and pushes the first semi-finished product along the second direction, so that the first semi-finished product passes through each of the molding holes in turn, the first shell wall and the second shell wall abut and slide against the inner wall of the molding hole, so that the first shell wall and the second shell wall become thinner and longer and are correspondingly formed into the third shell wall and the fourth shell wall, so that the first semi-finished product forms the second semi-finished product, wherein the wall thickness of the first shell wall is a1, the wall thickness of the second shell wall is b1, the wall thickness of the third shell wall is a2, and the wall thickness of the fourth shell wall is b2, a1 is greater than a2, and b1 is greater than b2.
[0013] According to some embodiments of the present application, a difference in wall thickness between the first shell wall and the third shell wall is e1, and a difference in wall thickness between the second shell wall and the fourth shell wall is e2, wherein e2 is greater than e1.
[0014] According to some embodiments of the present application, a blocking groove is formed at the bottom end of the first force-applying structure, and the blocking groove extends in a direction parallel to the first side wall.
[0015] According to some embodiments of the present application, the choke groove includes a plurality of choke grooves.
[0016] According to some embodiments of the present application, two ends of the flow-blocking groove close to the second side wall form flow-guiding slopes.
[0017] According to some embodiments of the present application, the set length of the aluminum shell is h1, and the length of the second semi-finished product formed by the thinning device is h2, and h2 is greater than h1;
[0018] The cutting of the second semi-finished product to form an aluminum shell comprises the following steps:
[0019] The end portion and the tail portion of the second semi-finished product are cut, and the middle portion of the second semi-finished product forms the aluminum shell.
[0020] According to some embodiments of the present application, after the blank is extruded by the extrusion device to form the first semi-finished product, the first semi-finished product has heat, and the thinning device thins the first semi-finished product with heat to form the second semi-finished product.
[0021] According to some embodiments of the present application, a baffle is provided on one end of the first force-applying structure away from the first molding structure, and when the first force-applying structure squeezes the blank in the molding groove, the blank extends toward the baffle.
[0022] According to the production system of the aluminum shell of the second embodiment of the present application, the aluminum shell is manufactured by applying the manufacturing process of the aluminum shell of the first embodiment.
[0023] The production system of the aluminum shell according to the second aspect of the present application has at least the following beneficial effects: including all the beneficial effects of the manufacturing process of the aluminum shell of the first aspect, which will not be repeated here.
[0024] Additional aspects and advantages of the present application will be given in part in the description below, and in part will become apparent from the description below, or will be learned through the practice of the present application. BRIEF DESCRIPTION OF THE DRAWINGS
[0025] The present application is further described below with reference to the accompanying drawings and embodiments, wherein:
[0026] Figure 1 A three-dimensional diagram of an extrusion device for a manufacturing process of an aluminum shell according to an embodiment of the first aspect of the present application;
[0027] Figure 2 for Figure 1 A partial structural schematic diagram of the first force-applying structure;
[0028] Figure 3 for Figure 1 A cross-sectional view of the extrusion device;
[0029] Figure 4 A schematic diagram of the steps of extruding a blank into a first semi-finished product by an extrusion device in a manufacturing process of an aluminum shell according to an embodiment of the first aspect of the present application;
[0030] Figure 5 A schematic diagram of the steps of extruding a blank into a first semi-finished product from another perspective in the manufacturing process of the aluminum shell according to the first aspect of the present application;
[0031] Figure 6 A schematic diagram of the steps of thinning a first semi-finished product to form a second semi-finished product by a thinning device in a manufacturing process of an aluminum shell according to an embodiment of the first aspect of the present application, wherein a portion of the first semi-finished product enters a molding hole of a first second molding structure;
[0032] Figure 7 A schematic diagram of the steps of thinning a first semi-finished product to form a second semi-finished product by a thinning device in a manufacturing process of an aluminum shell according to an embodiment of the first aspect of the present application, wherein the first semi-finished product completely enters the molding hole of the first second molding structure;
[0033] Figure 8 A schematic diagram of the steps of thinning a first semi-finished product to form a second semi-finished product by a thinning device in a manufacturing process of an aluminum shell according to an embodiment of the first aspect of the present application, wherein the first semi-finished product enters a molding hole of a second second molding structure;
[0034] Fig. 9 A schematic diagram of the steps of thinning a first semi-finished product to form a second semi-finished product by a thinning device in a manufacturing process of an aluminum shell according to an embodiment of the first aspect of the present application, wherein the first semi-finished product passes through a forming hole of a second second forming structure;
[0035] Fig.10 is a structural schematic diagram of the first semi-finished product;
[0036] Fig.11 is a schematic structural diagram of the second semi-finished product;
[0037] Fig.12 Schematic diagram of the structure of the aluminum shell.
[0038] Reference numerals:
[0039] A first molding structure 100, a first groove wall 110, a second groove wall 120, a molding groove 130, a first gap 140, and a second gap 150;
[0040] A first force-applying structure 200, a first side wall 210, a second side wall 220, a flow-blocking groove 230, a flow-guiding inclined surface 231, and a baffle 240;
[0041] A second force applying structure 300;
[0042] A second molding structure 400 and a molding hole 410;
[0043] A first semi-finished product 500, an end cover portion 500a, a housing portion 500b, a first housing wall 510, and a second housing wall 520;
[0044] A second semi-finished product 600, a third shell wall 610, and a fourth shell wall 620;
[0045] Aluminum shell 700 , first wall 710 , second wall 720 . DETAILED DESCRIPTION
[0046] The embodiments of the present application are described in detail below, and examples of the embodiments are shown in the accompanying drawings, wherein the same or similar reference numerals throughout represent the same or similar elements or elements having the same or similar functions. The embodiments described below with reference to the accompanying drawings are exemplary and are only used to explain the present application, and cannot be understood as limiting the present application.
[0047] In the description of the present application, it should be understood that descriptions involving orientation, such as up, down, front, back, left, right, etc., indicating orientations or positional relationships, are based on the orientations or positional relationships shown in the accompanying drawings, and are only for the convenience of describing the present application and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore should not be understood as a limitation on the present application.
[0048] In the description of this application, "several" means more than one, "more" means more than two, "greater than", "less than", "exceed", etc. are understood to exclude the number itself, and "above", "below", "within", etc. are understood to include the number itself. If there is a description of "first" or "second", it is only used for the purpose of distinguishing technical features, and cannot be understood as indicating or implying relative importance or implicitly indicating the number of the indicated technical features or implicitly indicating the order of the indicated technical features.
[0049] In the description of this application, unless otherwise clearly defined, terms such as setting, installing, connecting, etc. should be understood in a broad sense, and technicians in the relevant technical field can reasonably determine the specific meanings of the above terms in this application based on the specific content of the technical solution.
[0050] In the description of the present application, the description with reference to the terms "one embodiment", "some embodiments", "illustrative embodiments", "examples", "specific examples", or "some examples" means that the specific features, structures, materials, or characteristics described in conjunction with the embodiment or example are included in at least one embodiment or example of the present application. In this specification, the schematic representation of the above terms does not necessarily refer to the same embodiment or example. Moreover, the specific features, structures, materials, or characteristics described may be combined in any one or more embodiments or examples in a suitable manner.
[0051] According to the manufacturing process of the aluminum shell of the first embodiment of the present application, it should be noted that the manufacturing process of the aluminum shell of the present application is used to manufacture an aluminum shell 700 of a power battery, referring to Fig.12, wherein the cross section of the aluminum shell 700 is rectangular, and the aluminum shell 700 includes a first wall 710 and a second wall 720 relative to each other, and the thickness of the first wall 710 and the second wall 720 are inconsistent, and the thickness of the first wall 710 is less than the thickness of the second wall 720. It should be understood that the second wall 720 is used for welding the explosion-proof valve, so the second wall 720 needs to be designed to be thicker, and the first wall 710 can be designed to be the minimum value required by the bursting pressure. It can be understood that making the aluminum shell 700 with different wall thicknesses to reduce the size of the first wall 710 can reduce the overall size of the power battery using the aluminum shell 700, and can reduce the weight of the power battery, and at the same time, can reduce the production cost.
[0052] The manufacturing process of the aluminum shell includes the following steps:
[0053] Step 1: Obtain the blank.
[0054] It is understandable that, in some embodiments, the blank can be a long section of raw material punched into small blocks, and then annealed and saponified. Of course, in some other embodiments, the blank can also be an aluminum block.
[0055] Step 2, extruding the blank into a first semi-finished product 500 by an extrusion device; wherein, referring to Figure 1 and 3 The extrusion device includes a first molding structure 100 and a first force-applying structure 200, wherein the first molding structure 100 forms a molding groove 130, wherein the molding groove 130 has two opposite first groove walls 110 and two opposite second groove walls 120, and the first force-applying structure 200 has two opposite first side walls 210 and two opposite second side walls 220, and the cross-sectional dimension of the first force-applying structure 200 is smaller than the cross-sectional dimension of the molding groove 130; Figure 3 When the first force-applying structure 200 enters the molding groove 130, a first gap 140 is formed between the first groove wall 110 and the first side wall 210, and a second gap 150 is formed between the second groove wall 120 and the second side wall 220. The spacing of the first gap 140 is smaller than the spacing of the second gap 150. Figures 3 to 5 The blank is placed in the molding groove 130, the first force-applying structure 200 moves toward the molding groove 130 along the first direction, the first force-applying structure 200 squeezes the blank in the molding groove 130, the blank is deformed and flows along the periphery to the first gap 140 and the second gap 150 and extends in the opposite direction of the first direction, so that the blank forms a first semi-finished product 500, referring to Fig.10The first semi-finished product 500 includes an integrated shell part 500b and an end cover part 500a. The first gap 140 corresponds to the first shell wall 510 of the shell part 500b, and the second gap 150 corresponds to the second shell wall 520 of the shell part 500b. The thickness of the first shell wall 510 is less than the thickness of the second shell wall 520. The end cover part 500a is formed between the bottom of the forming groove 130 and the bottom end of the first force-applying structure 200.
[0056] It is understood that in step 2, referring to Figures 3 to 5 , the blank is placed in the molding groove 130 of the first molding structure 100, and then the first force-applying structure 200 moves toward the blank in the molding groove 130 and squeezes the blank. Under the squeezing action of the first force-applying structure 200 and the limiting action of the bottom wall of the molding groove 130, the blank will deform and flow along the gap between the groove wall of the molding groove 130 and the first force-applying structure 200, so that the blank flows in the opposite direction of the force-applying direction of the first force-applying structure 200, that is, flows in the opposite direction of the first direction to the gap between the groove wall of the molding groove 130 and the first force-applying structure 200. Subsequently, the blank flowing between the groove wall of the molding groove 130 and the peripheral side of the first force-applying structure 200 will form a shell part 500b, and the blank squeezed and thinned between the groove bottom of the molding groove 130 and the bottom end of the first force-applying structure 200 will form an end cover part 500a, wherein the shell part 500b and the end cover part 500a are integrally formed. Specifically, a first gap 140 is formed between the first groove wall 110 and the first side wall 210, a second gap 150 is formed between the second groove wall 120 and the second side wall 220, and a first shell wall 510 of the shell portion 500b is formed corresponding to the first gap 140, and a second shell wall 520 of the shell portion 500b is formed corresponding to the second gap 150, and because the first gap 140 is smaller than the second gap 150, the thickness of the first shell wall 510 will be smaller than the thickness of the second shell wall 520. It should be understood that the first shell wall 510 corresponds to the first wall body 710 of the aluminum shell 700, and the second shell wall 520 corresponds to the second wall body 720 of the aluminum shell 700, and at this time, the size of the first shell wall 510 is larger than the first wall body 710, and the size of the second shell wall 520 is larger than the second wall body 720, and the first shell wall 510 and the second shell wall 520 need to be further thinned.
[0057] Step 3: Thinning the first semi-finished product 500 by a thinning device to form a second semi-finished product 600.
[0058] It is understandable that, referring to Figures 6 to 9 , through step 3, the first shell wall 510 and the second shell wall 520 are thinned, referring to Fig.11 and Fig.12, so that the first shell wall 510 and the second shell wall 520 of the first semi-finished product 500 are thinned to form the third shell wall 610 and the fourth shell wall 620 of the second semi-finished product 600, wherein the third shell wall 610 and the fourth shell wall 620 correspond to the first wall body 710 and the second wall body 720 respectively, and at this time, the thickness of the third shell wall 610 and the thickness of the fourth shell wall 620 are respectively equal to the thickness of the first wall body 710 and the thickness of the second wall body 720. However, the length of the third shell wall 610 is greater than the length of the first wall body 710, and the length of the fourth shell wall 620 is greater than the length of the second wall body 720, thus, the length of the third shell wall 610 and the fourth shell wall 620 needs to be cut.
[0059] It can also be understood that the outer sides of the first shell wall 510 and the second shell wall 520 formed in step 2 may be relatively rough. In the process of forming the third shell wall 610 and the fourth shell wall 620 by thinning the first shell wall 510 and the second shell wall 520, the outer sides of the third shell wall 610 and the fourth shell wall 620 can be made relatively smoother.
[0060] Step 4: cutting the second semi-finished product 600 to form an aluminum shell 700.
[0061] It is understandable that, referring to Fig.11 and Fig.12 , the third shell wall 610 and the fourth shell wall 620 of the second semi-finished product 600 are cut in step 4 to cut off the size of the third shell wall 610 and the fourth shell wall 620 to form the aluminum shell 700. It should be understood that in this embodiment, the aluminum shell 700 is hollow, so the end cover part 500a also needs to be cut off in step 4. Of course, in some other embodiments, the end cover part 500a can also be retained.
[0062] In summary, the present application forms a first semi-finished product 500 with different wall thicknesses through step 2, and then through step 3, the first shell wall 510 and the second shell wall 520 of the first semi-finished product 500 are thinned to form a second semi-finished product 600, and then the third shell wall 610 and the fourth shell wall 620 of the second semi-finished product 600 are shortened to form an aluminum shell 700 with different wall thicknesses, and the first wall 710 and the second wall 720 of the aluminum shell 700 are integrally formed, so that the power battery manufactured using the aluminum shell 700 has better sealing performance. And because the thickness of the first wall 710 and the second wall 720 of the aluminum shell 700 is different, the volume, weight and production cost of the aluminum shell 700 can be reduced.
[0063] It should also be noted that there is also a process for producing the aluminum shell 700 in the prior art, in which a long section of metal shell is extruded by aluminum extrusion, and then the long section of metal shell is cut to form a single aluminum shell 700. However, in the process of extruding the long section of metal shell, stress will accumulate, resulting in uneven thickness at the rear end of the long section of metal shell, and even a risk of breakage, resulting in uneven quality of the aluminum shell 700 products produced at the front and rear ends of the metal shell, and the aluminum shell 700 formed at the rear end of the metal shell is of poor quality.
[0064] Therefore, compared with the aluminum shell 700 produced by the above-mentioned aluminum extrusion process, in the manufacturing process of the aluminum shell of the present application, a single blank corresponds to the production of a single aluminum shell 700. Therefore, there will be no problem of excessive stress accumulation leading to uneven quality of the aluminum shell 700 and poor quality of the aluminum shell 700.
[0065] Specifically, according to some embodiments of the present application, referring to Figures 6 to 9 The thinning of the first semi-finished product 500 to form the second semi-finished product 600 by the thinning device includes the following steps:
[0066] Reference Figures 6 to 9 The thinning device includes a second force-applying structure 300 and at least two second molding structures 400, the second molding structures 400 are distributed along the second direction, and the second molding structures 400 are provided with molding holes 410 that penetrate the second molding structures 400 along the second direction, and the molding holes 410 of adjacent second molding structures 400 are connected; along the second direction, the inner diameter of the molding holes 410 shows a decreasing trend; the second force-applying structure 300 is inserted into the interior of the shell part 500b, abuts against the end cover part 500a, and pushes the first semi-finished product 500 along the second direction, so that the first semi-finished product 500 passes through each of the molding holes 410 in turn, and the first shell wall 510 and the second shell wall 520 abut against and slide against the inner wall of the molding hole 410, refer to Fig.10 and Fig.11 , making the first shell wall 510 and the second shell wall 520 thinner and longer and correspondingly forming the third shell wall 610 and the fourth shell wall 620, so that the first semi-finished product 500 forms the second semi-finished product 600, wherein the wall thickness of the first shell wall 510 is a1, the wall thickness of the second shell wall 520 is b1, the wall thickness of the third shell wall 610 is a2, and the wall thickness of the fourth shell wall 620 is b2, a1 is greater than a2, and b1 is greater than b2.
[0067] It can be understood that the first semi-finished product 500 formed by step 1 has a shell part 500b and an end cover part 500a, the shell part 500b is hollow inside, the second molding structure 400 can be inserted into the shell part 500b, and the bottom end of the second molding structure 400 can abut against the inner side of the end cover part 500a, so as to push the first semi-finished product 500 to move along the second direction. During the movement of the first semi-finished product 500 along the second direction, it can pass through the molding holes 410 of each second molding structure 400 in sequence. It should be understood that the cross-sectional size of the first molding hole 410 is smaller than the cross-sectional size of the first semi-finished product 500, and the cross-sectional size of the second molding hole 410 is smaller than the cross-sectional size of the first molding hole 410, and so on. In the second direction, the cross-sectional size of the molding hole 410 located on the rear side is smaller than the cross-sectional size of the molding hole 410 on the front side, so that in the process of the second molding structure 400 pushing the first semi-finished product 500 to move along the second direction, the first shell wall 510 and the second shell wall 520 of the first semi-finished product 500 will abut and squeeze the inner wall of the molding hole 410. , and can slide relative to the inner wall of the forming hole 410, so that the first shell wall 510 and the second shell wall 520 are gradually thinned and elongated to form the second semi-finished product 600. Specifically, the first shell wall 510 is correspondingly thinned and elongated to form the third shell wall 610 of the second semi-finished product 600, and the second shell wall 520 is correspondingly thinned and elongated to form the fourth shell wall 620 of the second semi-finished product 600, that is, a1 is greater than a2, b1 is greater than b2, and the length of the third shell wall 610 is longer than the first shell wall 510, and the length of the fourth shell wall 620 is longer than the second shell wall 520.
[0068] It should also be understood that by repeatedly passing through the forming holes 410 with gradually smaller sizes, the process of thinning and stretching the first shell wall 510 and the second shell wall 520 is progressive, thereby reducing the risk of tearing of the first shell wall 510 and the second shell wall 520, so that the thickness of the third shell wall 610 and the fourth shell wall 620 of the formed second semi-finished product 600 is uniform.
[0069] According to some embodiments of the present application, a difference in wall thickness between the first shell wall 510 and the third shell wall 610 is e1, and a difference in wall thickness between the second shell wall 520 and the fourth shell wall 620 is e2, wherein e2 is greater than e1.
[0070] It can be understood that in the process of thinning the first shell wall 510 and the second shell wall 520 through step 3, the thickness of the first shell wall 510 and the second shell wall 520 are inconsistent. Specifically, the wall thickness difference between the first shell wall 510 and the third shell wall 610 is e1, and the wall thickness difference between the second shell wall 520 and the fourth shell wall 620 is e2, wherein e2 is greater than e1, that is, the thickness of the second shell wall 520 is thinned more than the thickness of the first shell wall 510. It should be understood that the first wall 710 of the aluminum shell 700 is thinner than the second wall 720. Therefore, in step 2, the first shell wall 510 is extruded to a thickness closer to the first wall 710, and the first shell wall 510 is made thinner than the second shell wall 520. Therefore, in step 3, when the first shell wall 510 needs to be thinned to form the third shell wall 610, it can be thinned less than the second shell wall 520 to form the fourth shell wall 620, so as to reduce the risk of the first shell wall 510 being cracked due to its thin thickness. In addition, the second shell wall 520 is relatively thick and can be thinned to a larger size. During the process of extruding the blank in step 2, the second gap 150 can be designed to be larger, and the blank can have better fluidity in the second gap 150, and can better fill the second gap 150 to avoid forming pits. The second shell wall 520 formed by the second gap 150 has better structural strength, which is more conducive to the installation of an explosion-proof valve on the second wall body 720 of the aluminum shell 700 formed by the second shell wall 520.
[0071] It should be noted that, since the sizes of the first gap 140 and the second gap 150 are inconsistent, the flow speeds of the blank in the first gap 140 and the second gap 150 after being extruded are inconsistent. Specifically, since the spacing of the first gap 140 is smaller than the spacing of the second gap 150, the blank flows faster in the first gap 140, which may cause the first shell wall 510 formed by the first gap 140 and the second shell wall 520 formed by the second gap 150 to form a wavy structure at the end away from the end cover portion 500a, which will lead to poor quality of the aluminum shell 700 product formed in the end. In order to avoid quality problems of the aluminum shell 700 caused by inconsistent flow rates. According to some embodiments of the present application, referring to Figure 2 A blocking groove 230 is formed at the bottom end of the first force-applying structure 200 , and the blocking groove 230 extends in a direction parallel to the first side wall 210 .
[0072] It is understandable that the blocking groove 230 is provided at the bottom end of the first force-applying structure 200, and the blocking groove 230 is parallel to the first side wall 210, that is, it can be parallel to the first gap 140. It is understandable that when the stock is squeezed and flows around, when it flows toward the second gap 150, the stock can flow along the blocking groove 230, without being hindered by the blocking groove 230 or being less affected by the blocking groove 230, while when the stock flows toward the first gap 140, the flow of the stock will be hindered by the inner wall of the blocking groove 230. Thus, the flow speed of the stock in the first gap 140 and the second gap 150 is balanced, so that the flow speed of the stock in the first gap 140 and the second gap 150 is consistent or similar, so as to avoid product quality problems caused by inconsistent flow speed.
[0073] Specifically, refer to Figure 2 The blocking grooves 230 include a plurality of blocking grooves 230 which are arranged in parallel and distributed along both ends of the first side wall 210 of the first force-applying structure 200 , thereby improving the blocking effect on the blank flowing along the first gap 140 .
[0074] In some other embodiments, a plurality of convex strips may be disposed at the bottom end of the first force-applying structure 200 , and the convex strips are disposed parallel to the first side wall 210 .
[0075] It should be understood that in the first semi-finished product 500 formed by the blocking groove 230 , the end cover portion 500 a is thicker, has better structural strength, and is not easy to break.
[0076] According to some embodiments of the present application, referring to Figure 2 The two ends of the blocking groove 230 close to the second side wall 220 form a guide slope 231.
[0077] It can be understood that in order to reduce the impact of the blocking groove 230 on the blank flowing to the second gap 150, a guide slope 231 is formed at both ends of the blocking groove 230 close to the second side wall 220. Specifically, the guide slope 231 is inclined in the direction close to the second side wall 220 so that the blocking groove 230 expands outward toward both ends of the second side wall 220. The blank can flow out of the blocking groove 230 along the guide slope 231, thereby increasing the speed at which the blank flows to the second gap 150.
[0078] According to some embodiments of the present application, referring to Fig.11 and Fig.12 , the set length of the aluminum shell 700 is h1, and the length of the second semi-finished product 600 formed by the thinning device is h2, and h2 is greater than h1;
[0079] The step of cutting the second semi-finished product 600 to form the aluminum shell 700 includes the following steps:
[0080] The end and tail of the second semi-finished product 600 are cut, and the middle portion of the second semi-finished product 600 forms the aluminum shell 700 .
[0081] It can be understood that the second semi-finished product 600 formed by the thinning device is stretched to a length longer than the aluminum shell 700, so that the second semi-finished product 600 has a length margin for cutting. Among them, the end of the second semi-finished product 600 can be cut off to cut off the end cover part 500a formed in step 2; the tail of the second semi-finished product 600 can be cut off to form a wavy structure due to the inconsistent flow rate of the blank in the first gap 140 and the second gap 150 in step 2, and the inconsistent thinning thickness of the first shell wall 510 and the second shell wall 520 in step 3 will cause the tail end of the second semi-finished product 600 to correspond to the third shell wall 610 and the fourth shell wall 620. There is a situation of inconsistent length, thus, cutting off the tail of the second semi-finished product 600 can make the tail of the second semi-finished product 600 neat.
[0082] Specifically, refer to Fig.10 and Fig.12 The length of the first semi-finished product 500 is h3, and h3 should be smaller than h1 to ensure the strength of the first semi-finished product 500 when it is thinned.
[0083] According to some embodiments of the present application, after the blank is extruded by the extrusion device to form the first semi-finished product 500 , the first semi-finished product 500 has heat, and the thinning device thins the first semi-finished product 500 having heat to form the second semi-finished product 600 .
[0084] It can be understood that in the process of the extrusion device extruding the blank into the first semi-finished product 500, the first semi-finished product 500 will have heat. The first semi-finished product 500 with heat has better plasticity. In step 3, the thinning device thins the first semi-finished product 500 with heat into the second semi-finished product 600, so that the first shell wall 510 and the second shell wall 520 can be better thinned and elongated during the thinning process.
[0085] According to some embodiments of the present application, referring to Figure 4 and Figure 5 A baffle 240 is provided on one end of the first force-applying structure 200 away from the first molding structure 100 . When the first force-applying structure 200 squeezes the blank in the molding groove 130 , the blank extends toward the baffle 240 .
[0086] It can be understood that in step 2, after the first force-applying structure 200 extrude the blank, the blank will extend in the opposite direction of the first direction, that is, the blank will extend in the direction away from the first molding structure 100. It should be understood that a baffle 240 is provided on the end of the first force-applying structure 200 away from the first molding structure 100, so as to limit the flow and extension of the blank, thereby limiting the length of the first shell wall 510 and the second shell wall 520 of the first semi-finished product 500.
[0087] According to the production system of the aluminum shell of the second embodiment of the present application, the aluminum shell 700 is manufactured by applying the manufacturing process of the aluminum shell of the first embodiment.
[0088] The production system of the aluminum shell according to the second aspect of the present application has at least the following beneficial effects: including all the beneficial effects of the manufacturing process of the aluminum shell of the first aspect, which will not be repeated here.
[0089] Specifically, the production system of the aluminum shell includes an extrusion device and a thinning device.
[0090] Reference Figures 1 to 3 The extrusion device includes a first molding structure 100 and a first force-applying structure 200, wherein the first molding structure 100 forms a molding groove 130, wherein the molding groove 130 has two opposite first groove walls 110 and two opposite second groove walls 120, wherein the first force-applying structure 200 has two opposite first side walls 210 and two opposite second side walls 220, and the cross-sectional size of the first force-applying structure 200 is smaller than the cross-sectional size of the molding groove 130; when the first force-applying structure 200 enters the molding groove 130, a first gap 140 is formed between the first groove wall 110 and the first side wall 210, and a second gap 150 is formed between the second groove wall 120 and the second side wall 220, and the spacing of the first gap 140 is smaller than the spacing of the second gap 150.
[0091] Reference Figures 6 to 9 The thinning device includes a second force-applying structure 300 and at least two second molding structures 400, wherein the second molding structures 400 are distributed along the second direction, and the second molding structures 400 are provided with molding holes 410 penetrating the second molding structures 400 along the second direction, and the molding holes 410 of adjacent second molding structures 400 are connected; along the second direction, the inner diameter of the molding holes 410 presents a decreasing trend; the second force-applying structure 300 can be inserted into the interior of the shell part 500b of the first semi-finished product 500, abut against the end cover part 500a, and push the first semi-finished product 500 along the second direction, so that the first semi-finished product 500 passes through each of the molding holes 410 in turn.
[0092] Furthermore, the aluminum shell production system further includes a cutting device, which is used to cut off the end and tail of the second semi-finished product 600 .
[0093] The embodiments of the present application are described in detail above in conjunction with the accompanying drawings, but the present application is not limited to the above embodiments. Various changes can be made within the knowledge of ordinary technicians in the relevant technical field without departing from the purpose of the present application. In addition, the embodiments of the present application and the features in the embodiments can be combined with each other without conflict.
Claims
1. The manufacturing process of the aluminum shell is characterized by: The steps include: Obtaining blanks; The blank is extruded into a first semi-finished product by an extrusion device; wherein the extrusion device includes a first molding structure and a first force-applying structure, the first molding structure forms a molding groove, the molding groove has two opposite first groove walls and two opposite second groove walls, the first force-applying structure has two opposite first side walls and two opposite second side walls, and the size of the cross section of the first force-applying structure is smaller than the size of the cross section of the molding groove; when the first force-applying structure enters the molding groove, a first gap is formed between the first groove wall and the first side wall, a second gap is formed between the second groove wall and the second side wall, and the spacing of the first gap is smaller than the spacing of the second gap ; The blank is placed in the molding groove, the first force-applying structure moves toward the molding groove along the first direction, the first force-applying structure squeezes the blank in the molding groove, the blank is deformed and flows around to the first gap and the second gap and extends in the opposite direction of the first direction, so that the blank forms a first semi-finished product, the first semi-finished product includes an integrated shell part and an end cover part, the first gap corresponds to forming a first shell wall of the shell part, the second gap corresponds to forming a second shell wall of the shell part, the thickness of the first shell wall is less than the thickness of the second shell wall, and the end cover part is formed between the bottom of the molding groove and the bottom end of the first force-applying structure; The first semi-finished product is thinned by a thinning device to form a second semi-finished product; The second semi-finished product is cut to form an aluminum shell.
2. The manufacturing process of the aluminum shell according to claim 1, characterized in that: The step of thinning the first semi-finished product to form the second semi-finished product by a thinning device comprises the following steps: The thinning device includes a second force-applying structure and at least two second molding structures, the second molding structures are distributed along the second direction, and the second molding structures are provided with molding holes that penetrate the second molding structures along the second direction, and the molding holes of adjacent second molding structures are connected; along the second direction, the inner diameter of the molding holes shows a decreasing trend; the second force-applying structure is inserted into the interior of the shell part, abuts against the end cover part, and pushes the first semi-finished product along the second direction, so that the first semi-finished product passes through each of the molding holes in turn, the first shell wall and the second shell wall abut and slide against the inner wall of the molding hole, so that the first shell wall and the second shell wall become thinner and longer and are correspondingly formed into the third shell wall and the fourth shell wall, so that the first semi-finished product forms the second semi-finished product, wherein the wall thickness of the first shell wall is a1, the wall thickness of the second shell wall is b1, the wall thickness of the third shell wall is a2, and the wall thickness of the fourth shell wall is b2, a1 is greater than a2, and b1 is greater than b2.
3. The manufacturing process of the aluminum shell according to claim 2, characterized in that: The difference in wall thickness between the first shell wall and the third shell wall is e1, and the difference in wall thickness between the second shell wall and the fourth shell wall is e2, wherein e2 is greater than e1.
4. The manufacturing process of the aluminum shell according to claim 1, characterized in that: A flow-blocking groove is formed at the bottom end of the first force-applying structure, and the flow-blocking groove extends in a direction parallel to the first side wall.
5. The manufacturing process of the aluminum shell according to claim 4, characterized in that: The choke grooves include a plurality of choke grooves.
6. The manufacturing process of the aluminum shell according to claim 4, characterized in that: Two ends of the blocking groove close to the second side wall form flow guiding inclined surfaces.
7. The manufacturing process of the aluminum shell according to claim 1, characterized in that: The set length of the aluminum shell is h1, and the length of the second semi-finished product formed by the thinning device is h2, and h2 is greater than h1; The cutting of the second semi-finished product to form an aluminum shell comprises the following steps: The end portion and the tail portion of the second semi-finished product are cut, and the middle portion of the second semi-finished product forms the aluminum shell.
8. The manufacturing process of the aluminum shell according to claim 1, characterized in that: After the blank is extruded by the extrusion device to form the first semi-finished product, the first semi-finished product has heat, and the thinning device thins the first semi-finished product having heat to form the second semi-finished product.
9. The manufacturing process of the aluminum shell according to claim 1, characterized in that: A baffle is provided on one end of the first force-applying structure away from the first molding structure. When the first force-applying structure squeezes the blank in the molding groove, the blank extends toward the baffle.
10. A production system for an aluminum shell, characterized in that: The aluminum shell is manufactured using the aluminum shell manufacturing process described in any one of claims 1 to 9.
Citation Information
Patent Citations
Extrusion forming method for variable-wall-thickness shell
CN114535332A
Square battery container, method of manufacturing the container, and square battery using the container
CN1406395A
Manufacturing method of metal square can by backward extrusion forming
JP2002178096A
Method for obtaining a shell with a variable wall thickness along the perimeter
RU2761569C1